Assessment of hot cracking behaviour in welds

  • Hot crack assessment during production and processing of metallic materials is an essential prerequisite for the safety of welded structures. The hot cracking investigations presented here were carried out as part of a study aimed at the development of Cr/Ni low transformation temperature filler materials. Low transformation temperature alloys open up the possibility for welding high strength steels. The externally loaded Modified Varestraint Transvarestraint hot cracking test was employed in the experiments described. The hot cracking resistance was evaluated with the help of light microscopy applied at the specimen surface. The proportionality between hot cracking susceptibility and Cr/Ni alloy content was explained by the altered solidification kinetics and by the enlarged solidification interval. The internal crack paths and the three-dimensional structure of the crack net in the material volume were examined using X-ray computer tomography. The total crack lengths for differentHot crack assessment during production and processing of metallic materials is an essential prerequisite for the safety of welded structures. The hot cracking investigations presented here were carried out as part of a study aimed at the development of Cr/Ni low transformation temperature filler materials. Low transformation temperature alloys open up the possibility for welding high strength steels. The externally loaded Modified Varestraint Transvarestraint hot cracking test was employed in the experiments described. The hot cracking resistance was evaluated with the help of light microscopy applied at the specimen surface. The proportionality between hot cracking susceptibility and Cr/Ni alloy content was explained by the altered solidification kinetics and by the enlarged solidification interval. The internal crack paths and the three-dimensional structure of the crack net in the material volume were examined using X-ray computer tomography. The total crack lengths for different material depths and circumjacent rectangular volumes, respectively, were be determined. An increasing hot cracking susceptibility with increasing Cr/Ni alloy content was also be established for the specimen volume.zeige mehrzeige weniger

Volltext Dateien herunterladen

  • Assessment of hot cracking behaviour in welds.pdf
    eng

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:Thomas KannengießerORCiD, Michael RethmeierORCiD, Pedro Dolabella PortellaORCiD, Uwe Ewert, Bernhard Redmer
Dokumenttyp:Zeitschriftenartikel
Veröffentlichungsform:Verlagsliteratur
Sprache:Englisch
Titel des übergeordneten Werkes (Englisch):International journal of materials research
Jahr der Erstveröffentlichung:2011
Herausgeber (Institution):Deutsche Gesellschaft für Materialkunde
Verlag:Carl Hanser
Verlagsort:München
Jahrgang/Band:102
Ausgabe/Heft:8
Erste Seite:1001
Letzte Seite:1006
Freie Schlagwörter:Hot cracking; Low transformation temperature (LTT) alloy; Modified varestraint transvarestraint (MVT) hot cracking test; X-ray computer tomography
DOI:10.3139/146.110545
ISSN:1862-5282
Verfügbarkeit des Dokuments:Datei im Netzwerk der BAM verfügbar ("Closed Access")
Datum der Freischaltung:19.02.2016
Referierte Publikation:Ja
Datum der Eintragung als referierte Publikation:29.09.2011
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.