Comparison of the stress crack resistance of polyethylene grades with the test performance behaviour of packagings for the transport of dangerous goods

  • Resistance to stress cracking by wetting solution is one of the selected properties together with the corresponding test method FNCT and tolerances for a comparison of polyethylene grades of one design type in the procedural rule on suitability proof for alternative plastic resins used for packagings and intermediate bulk containers (IBCs) for the transport of dangerous goods. The environmental stress crack resistance determined by Full Notch Creep Test (FNCT) represents the impacts from the stacking tests at 40 °C performed with standard liquid wetting solution (without pre-storage) and with normal butyl acetate saturated wetting solution (pre-storage with normal butyl acetate). Environmental stress crack resistance determined with FNCT for the polyethylene grades was related to the times to failure of different jerrican samples made of these grades in stacking tests with 5% wetting solution and a n-butyl acetate saturated wetting solution (pre-storage with n-butyl acetate) at 40 °C.Resistance to stress cracking by wetting solution is one of the selected properties together with the corresponding test method FNCT and tolerances for a comparison of polyethylene grades of one design type in the procedural rule on suitability proof for alternative plastic resins used for packagings and intermediate bulk containers (IBCs) for the transport of dangerous goods. The environmental stress crack resistance determined by Full Notch Creep Test (FNCT) represents the impacts from the stacking tests at 40 °C performed with standard liquid wetting solution (without pre-storage) and with normal butyl acetate saturated wetting solution (pre-storage with normal butyl acetate). Environmental stress crack resistance determined with FNCT for the polyethylene grades was related to the times to failure of different jerrican samples made of these grades in stacking tests with 5% wetting solution and a n-butyl acetate saturated wetting solution (pre-storage with n-butyl acetate) at 40 °C. The FNCT is suitable for comparison of polyethylene grades in relation to environmental stress crack resistance independent of their use as drum, IBC or jerrican material. The stiffness of polyethylene grades should be taken into account to the comparison as jerricans are not only chemically but also mechanically stressed.zeige mehrzeige weniger

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:Margit Weltschev, Ute Niebergall
Dokumenttyp:Beitrag zu einem Tagungsband
Veröffentlichungsform:Graue Literatur
Sprache:Englisch
Titel des übergeordneten Werkes (Englisch):EUROCORR 2010 - From the earth´s depths to space heights
Jahr der Erstveröffentlichung:2010
Herausgeber (Institution):European Federation of Corrosion
Verlag:DECHEMA
Verlagsort:Moscow
Ausgabe/Heft:324
Erste Seite:1
Letzte Seite:6
Freie Schlagwörter:Gefahrgutverpackungen; Polyethylenformstoffe; Spannungsrissbeständigkeit; Stapeldruckprüfungen
Veranstaltung:EUROCORR 2010
Veranstaltungsort:Moscow, Russia
Beginndatum der Veranstaltung:2010-09-13
Enddatum der Veranstaltung:2010-09-17
Bemerkung:
Serientitel: EFC-Event – Series title: EFC-Event
Verfügbarkeit des Dokuments:Physisches Exemplar in der Bibliothek der BAM vorhanden ("Hardcopy Access")
Bibliotheksstandort:Sonderstandort: Publica-Schrank
Datum der Freischaltung:19.02.2016
Referierte Publikation:Nein
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.