Thermoresponsive poly(N-C3 glycine)s

  • Ring-opening polymerization of N-substituted glycine N-carboxyanhydrides (NCAs) was applied to prepare a series of well-defined poly(N-C3 glycine)s (C3 = n-propyl, allyl, propargyl, and isopropyl), polypeptoids, with molecular weights in the range of 1.8–6.6 kg mol–1. Poly(N-isopropyl glycine), a previously unreported polypeptoid, could be obtained by bulk polymerization of the corresponding NCA in the melt. The samples were characterized by spectroscopy (NMR and FT-IR), size exclusion chromatography (SEC), and matrix-assisted laser desorption/ionization time-of-flight mass spectroscopy (MALDI–ToF MS). The polymers could be dispersed in water up to 20–40 g L–1; the poly(N-propargyl glycine) was not soluble in water. Turbidity measurements of the three water-soluble polypeptoids illustrated cloud point temperatures dependent on structural and electronic properties of the side chain. The cloud point temperatures were found to increase in the order C3 = n-propyl (15–25 °C) < allyl (27–54Ring-opening polymerization of N-substituted glycine N-carboxyanhydrides (NCAs) was applied to prepare a series of well-defined poly(N-C3 glycine)s (C3 = n-propyl, allyl, propargyl, and isopropyl), polypeptoids, with molecular weights in the range of 1.8–6.6 kg mol–1. Poly(N-isopropyl glycine), a previously unreported polypeptoid, could be obtained by bulk polymerization of the corresponding NCA in the melt. The samples were characterized by spectroscopy (NMR and FT-IR), size exclusion chromatography (SEC), and matrix-assisted laser desorption/ionization time-of-flight mass spectroscopy (MALDI–ToF MS). The polymers could be dispersed in water up to 20–40 g L–1; the poly(N-propargyl glycine) was not soluble in water. Turbidity measurements of the three water-soluble polypeptoids illustrated cloud point temperatures dependent on structural and electronic properties of the side chain. The cloud point temperatures were found to increase in the order C3 = n-propyl (15–25 °C) < allyl (27–54 °C) < isopropyl (47–58 °C). Long-term annealing of the aqueous solution of poly(N-{n-propyl} glycine) and poly(N-allyl glycine) above the cloud point temperature resulted in the formation of crystalline microparticles with melting points of 188–198 and 157–165 °C (differential scanning calorimetry, DSC), respectively, and rose bud type morphology (scanning electron microscopy, SEM).zeige mehrzeige weniger

Volltext Dateien herunterladen

  • ma302412v.pdf
    eng

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:J.W. Robinson, C. Secker, Steffen WeidnerORCiD, H. Schlaad
Dokumenttyp:Zeitschriftenartikel
Veröffentlichungsform:Verlagsliteratur
Sprache:Englisch
Titel des übergeordneten Werkes (Englisch):Macromolecules
Jahr der Erstveröffentlichung:2013
Verlag:American Chemical Society
Verlagsort:Washington, DC
Jahrgang/Band:46
Ausgabe/Heft:3
Erste Seite:580
Letzte Seite:587
DOI:10.1021/ma302412v
ISSN:0024-9297
ISSN:1520-5835
Verfügbarkeit des Dokuments:Datei im Netzwerk der BAM verfügbar ("Closed Access")
Datum der Freischaltung:20.02.2016
Referierte Publikation:Ja
Datum der Eintragung als referierte Publikation:18.02.2013
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.