Safety assessment of aged metal seals

  • With our experiments we want to simulate a load situation which can result from a cask vertical drop test. The lid can lift a little for a very short moment and that can perhaps result in a little movement of the seal, a little rotation or a little lateral movement, so that the contact section can change. The aim of the project is to learn more about the sealing efficiency after the seal is compressed again. What we know from former component tests with non-aged seals is, that the leakage rate measured after one or more decompression /compression cycles with seal movement becomes significant higher. And this result is considered for specification of design leakage rates for release calculation in safety cases. In the recent years we all have learned more about the significant influence of temperature and time on seal behavior and so the plan was to do similar experiments with aged seals, just to get an idea about seal behavior and achievable leakage rates. What we did in detailWith our experiments we want to simulate a load situation which can result from a cask vertical drop test. The lid can lift a little for a very short moment and that can perhaps result in a little movement of the seal, a little rotation or a little lateral movement, so that the contact section can change. The aim of the project is to learn more about the sealing efficiency after the seal is compressed again. What we know from former component tests with non-aged seals is, that the leakage rate measured after one or more decompression /compression cycles with seal movement becomes significant higher. And this result is considered for specification of design leakage rates for release calculation in safety cases. In the recent years we all have learned more about the significant influence of temperature and time on seal behavior and so the plan was to do similar experiments with aged seals, just to get an idea about seal behavior and achievable leakage rates. What we did in detail is: We compressed Helicoflex-seals of both design types, with Aluminum and Silver outer jackets, in testflanges and aged them in an oven at a temperature of 125°C for 3 months to produce seal properties comparable with properties after several years use at more typical operating temperatures between 90 and 100°C. After this ageing procedure we opened the flanges completely, moved the seal a little to vary the contact area and compressed the flanges again. What we measured during all compression and decompression cycles was the load, the deformation and -as long as possible- the leakage rates.zeige mehrzeige weniger

Volltext Dateien herunterladen

  • IRSN _BAM workshop Cadarache_Ro.pdf
    eng

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:Annette Rolle
Koautor*innen:Tino Neumeyer, Frank Wille
Dokumenttyp:Vortrag
Veröffentlichungsform:Präsentation
Sprache:Englisch
Jahr der Erstveröffentlichung:2022
Organisationseinheit der BAM:3 Gefahrgutumschließungen; Energiespeicher
3 Gefahrgutumschließungen; Energiespeicher / 3.3 Sicherheit von Transportbehältern
DDC-Klassifikation:Technik, Medizin, angewandte Wissenschaften / Ingenieurwissenschaften / Angewandte Physik
Freie Schlagwörter:Ageing; Radioactive; Seal behavior; Transport
Themenfelder/Aktivitätsfelder der BAM:Energie
Energie / Kerntechnische Entsorgung
Veranstaltung:Workshop IRSN/BAM
Veranstaltungsort:Cadarache, France
Beginndatum der Veranstaltung:12.10.2022
Enddatum der Veranstaltung:14.10.2022
Verfügbarkeit des Dokuments:Datei im Netzwerk der BAM verfügbar ("Closed Access")
Datum der Freischaltung:31.10.2022
Referierte Publikation:Nein
Eingeladener Vortrag:Nein
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.