Oxidation of single crystal PWA 1483 at 950 °C in flowing air

  • The oxidation behaviour of single crystal PWA 1483 at 950 °C was investigated by means of XRD, SEM and EDS. The parabolic oxidation behaviour, as defined by mass gain and the respective oxide layer thicknesses, is characterized by a parabolic rate constant of about 4 × 10-6 mg²/(cm4 × s) and the formation of a multi-layered oxide scale. An outer scale contains a Ti-bearing thin film composed of TiO2 and NiTiO3 but mostly Cr in Cr2O3 and (Ni/Co)Cr2O4 besides NiTaO4. This outer scale is connected to a discontinuous layer of Al2O3 and an area of γ?'-depletion within the base material.

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:Anja Pfennig, Bernard FedelichORCiD
Dokumenttyp:Zeitschriftenartikel
Veröffentlichungsform:Verlagsliteratur
Sprache:Englisch
Titel des übergeordneten Werkes (Englisch):Corrosion science
Jahr der Erstveröffentlichung:2008
Verlag:Elsevier
Verlagsort:Orlando, Fla.
Jahrgang/Band:50
Ausgabe/Heft:9
Erste Seite:2484
Letzte Seite:2492
Freie Schlagwörter:A. Superalloys; B. Weight loss; C. High temperature corrosion; C. Kinetic parameters; C. Oxidation
DOI:10.1016/j.corsci.2008.06.033
ISSN:0010-938X
Verfügbarkeit des Dokuments:Physisches Exemplar in der Bibliothek der BAM vorhanden ("Hardcopy Access")
Bibliotheksstandort:Sonderstandort: Publica-Schrank
Datum der Freischaltung:19.02.2016
Referierte Publikation:Ja
Datum der Eintragung als referierte Publikation:18.09.2008
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.