Zitieren Sie bitte immer diesen URN: urn:nbn:de:kobv:b43-545780
Assessment of the Solidification Cracking Susceptibility of Welding Consumables in the Varestraint Test by Means of an Extended Evaluation Methodology
- Various test methods are available for assessing the susceptibility of materials to solidification cracking during welding. In the widely used Varestraint test, the crack length is selected as a criterion as a function of the applied bending strain. Unfortunately, the crack length does not characterize the material behavior alone but depends to varying degrees on the individual test parameters used, which makes the interpretation of the results difficult. In addition, the crack length is not comparable under different test conditions. To overcome these disadvantages, we have developed a novel evaluation methodology that decouples the machine influence from the material behavior. The measured crack length is related to the maximum possible value specified by welding speed and deformation time. This relative crack length is calculated numerically, considering the orientation of the cracks. Experiments on two high-alloy martensitic welding consumables show that, in contrast to theVarious test methods are available for assessing the susceptibility of materials to solidification cracking during welding. In the widely used Varestraint test, the crack length is selected as a criterion as a function of the applied bending strain. Unfortunately, the crack length does not characterize the material behavior alone but depends to varying degrees on the individual test parameters used, which makes the interpretation of the results difficult. In addition, the crack length is not comparable under different test conditions. To overcome these disadvantages, we have developed a novel evaluation methodology that decouples the machine influence from the material behavior. The measured crack length is related to the maximum possible value specified by welding speed and deformation time. This relative crack length is calculated numerically, considering the orientation of the cracks. Experiments on two high-alloy martensitic welding consumables show that, in contrast to the conventional evaluation, a comparison of different welding parameters becomes possible. Furthermore, the strain rate proved to be a suitable crack criterion in agreement with Prokhorov's hot cracking model.…
Autor*innen: | Arne KrommORCiD, Maximilian ThomasORCiD, Thomas KannengießerORCiD, J. GibmeierORCiD, F. Vollert |
---|---|
Dokumenttyp: | Zeitschriftenartikel |
Veröffentlichungsform: | Verlagsliteratur |
Sprache: | Englisch |
Titel des übergeordneten Werkes (Englisch): | Advanced Engineering Materials |
Jahr der Erstveröffentlichung: | 2022 |
Organisationseinheit der BAM: | 9 Komponentensicherheit |
9 Komponentensicherheit / 9.4 Integrität von Schweißverbindungen | |
Veröffentlichende Institution: | Bundesanstalt für Materialforschung und -prüfung (BAM) |
Verlag: | Wiley online library |
Erste Seite: | 2101650 |
DDC-Klassifikation: | Technik, Medizin, angewandte Wissenschaften / Ingenieurwissenschaften / Angewandte Physik |
Freie Schlagwörter: | Solidification cracking; Varestraint test; Welding |
Themenfelder/Aktivitätsfelder der BAM: | Energie |
DOI: | 10.1002/adem.202101650 |
URN: | urn:nbn:de:kobv:b43-545780 |
ISSN: | 1438-1656 |
Verfügbarkeit des Dokuments: | Datei für die Öffentlichkeit verfügbar ("Open Access") |
Lizenz (Deutsch): | Creative Commons - CC BY - Namensnennung 4.0 International |
Datum der Freischaltung: | 04.04.2022 |
Referierte Publikation: | Ja |
Datum der Eintragung als referierte Publikation: | 20.04.2022 |
Paper des Monats: | Ja |
Schriftenreihen ohne Nummerierung: | Wissenschaftliche Artikel der BAM |