Supercritical CO2-corrosion in pipe steels during carbon capture and storage CCS

  • The CCS technique involves the compression of emission gasses in deep geological layers. To guarantee the safety of the site, CC>2-corrosion of the injection pipe steels has to be given special attention when engineering CCS-sites. To get to know the corrosion behaviour samples of the heat treated Steel 1.72252CrMo4, used for casing, and the stainless injection-pipe Steel 1.4034 X46Crl3 were kept at T=60 °C and ambient pressure as well as p=100 bar for 700 h - 8000 h in a CC>2-saturated synthetic aquifer environment similar to possible geological onshore CCS-sites in the northern German Basin. The isothermal corrosion behaviour obtained by mass gain of the steels in the gas phase, the liquid phase and the intermediate phase gives surface corrosion rates around 0.1 to 0.8 mm/year at ambient pressure and much lower about 0.02 to 0.2 mm/year at 100 bar where the CO2 is in its supercritical state. Severe pit corrosion with pit heights around 4.5 mm are only located on the 42CrMo4 Steel.The CCS technique involves the compression of emission gasses in deep geological layers. To guarantee the safety of the site, CC>2-corrosion of the injection pipe steels has to be given special attention when engineering CCS-sites. To get to know the corrosion behaviour samples of the heat treated Steel 1.72252CrMo4, used for casing, and the stainless injection-pipe Steel 1.4034 X46Crl3 were kept at T=60 °C and ambient pressure as well as p=100 bar for 700 h - 8000 h in a CC>2-saturated synthetic aquifer environment similar to possible geological onshore CCS-sites in the northern German Basin. The isothermal corrosion behaviour obtained by mass gain of the steels in the gas phase, the liquid phase and the intermediate phase gives surface corrosion rates around 0.1 to 0.8 mm/year at ambient pressure and much lower about 0.02 to 0.2 mm/year at 100 bar where the CO2 is in its supercritical state. Severe pit corrosion with pit heights around 4.5 mm are only located on the 42CrMo4 Steel. Main phase of the continuous complicated multi-layered carbonate/oxide structure is siderite FeCCh in both types of Steel.zeige mehrzeige weniger

Volltext Dateien herunterladen

  • Supercritical CO2-corrosion in pipe steels during carbon capture and storage CCS_Malaysia.pdf
    eng

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:Anja Pfennig, Barbara Linke, Sabrina Schulz, Axel KranzmannORCiD
Dokumenttyp:Beitrag zu einem Tagungsband
Veröffentlichungsform:Graue Literatur
Sprache:Englisch
Titel des übergeordneten Werkes (Englisch):3rd International congress on green process engineering (GPE 2011)
Jahr der Erstveröffentlichung:2011
Erste Seite:1
Letzte Seite:6
Freie Schlagwörter:CCS; CO2-storage; Carbonate layer; Corrosion; Pipeline; Steel; Supercritical CO2-
Veranstaltung:3rd International congress on green process engineering (GPE 2011)
Veranstaltungsort:Kuala-Lumpur, Malaysia
Beginndatum der Veranstaltung:06.12.2011
Enddatum der Veranstaltung:08.12.2011
Verfügbarkeit des Dokuments:Datei im Netzwerk der BAM verfügbar ("Closed Access")
Datum der Freischaltung:19.02.2016
Referierte Publikation:Nein
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.