Research and development into a European code-of-practice for strain-controlled thermo-mechanical fatigue testing

  • Thermo-mechanical fatigue (TMF) testing plays an increasingly important role in the design, the reliability assessment and the lifecycle management of safety critical components used, for instance, for power generation, in the process industry and in aeronautical and automotive applications, with a view to increasing the fuel efficiency, safety and service intervals, while reducing production (and material) costs. In a European Commission funded research project (acronym: TMF-Standard) of the 5th Framework Programme, 20 European laboratories have undertaken a joint research effort to establish a validated code-of-practice (CoP) for strain-controlled TMF testing. Starting from a survey of the testing protocols and procedures previously used by the partners, a comprehensive pre-normative research activity into various issues has been completed, addressing the dynamic temperature control, the effects of deviations in nominal temperatures and phase angles, the influences of temperatureThermo-mechanical fatigue (TMF) testing plays an increasingly important role in the design, the reliability assessment and the lifecycle management of safety critical components used, for instance, for power generation, in the process industry and in aeronautical and automotive applications, with a view to increasing the fuel efficiency, safety and service intervals, while reducing production (and material) costs. In a European Commission funded research project (acronym: TMF-Standard) of the 5th Framework Programme, 20 European laboratories have undertaken a joint research effort to establish a validated code-of-practice (CoP) for strain-controlled TMF testing. Starting from a survey of the testing protocols and procedures previously used by the partners, a comprehensive pre-normative research activity into various issues has been completed, addressing the dynamic temperature control, the effects of deviations in nominal temperatures and phase angles, the influences of temperature gradients, as well as the practicalities of test interruption and restart procedures. Meaningful allowable tolerances for the various test parameters were identified and practical recommendations as to the test techniques were formulated. From this a preliminary CoP was compiled and used to guide an extensive round robin exercise among the project partners. From the statistical analysis of that exercise, a validated CoP was derived dealing with strain-controlled constant amplitude TMF of nominally homogeneous metallic materials subjected to spatially uniform temperature fields and uniaxial mechanical loading. It is intended to give advice and guidance on the appropriate test setup, testing procedures and the analysis of results, in particular for newcomers in the field of strain-controlled TMF. This paper highlights some of the results of the TMF-Standard project. Moreover, commonalities and differences of the present CoP with respect to the standard documents for strain-controlled TMF, which have been developed at ISO and ASTM levels, are presented in this paper.zeige mehrzeige weniger

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:P. Hähner, C. Rinaldi, V. Bicego, E. E. Affeldt, T. Brendel, H. Andersson, T. Beck, Hellmuth Klingelhöffer, Hans-Joachim Kühn, A. Köster, M. Loveday, M. Marchionni, C. Rae
Dokumenttyp:Zeitschriftenartikel
Veröffentlichungsform:Verlagsliteratur
Sprache:Englisch
Titel des übergeordneten Werkes (Englisch):International Journal of Fatigue
Jahr der Erstveröffentlichung:2008
Verlag:Elsevier
Verlagsort:Oxford
Jahrgang/Band:30
Ausgabe/Heft:2
Erste Seite:372
Letzte Seite:381
Freie Schlagwörter:Ni-base superalloy; Standardisation; Test methods; Thermo-mechanical fatigue
DOI:10.1016/j.ijfatigue.2007.01.052
ISSN:0142-1123
Verfügbarkeit des Dokuments:Physisches Exemplar in der Bibliothek der BAM vorhanden ("Hardcopy Access")
Bibliotheksstandort:Sonderstandort: Publica-Schrank
Datum der Freischaltung:19.02.2016
Referierte Publikation:Ja
Datum der Eintragung als referierte Publikation:05.06.2008
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.