TY - CONF A1 - Niederleithinger, Ernst T1 - Concepts from seismic interferometry transferred to sonic and ultrasonic concrete inspection and monitoring N2 - Seismic interferometry (SI) deals either with the sensible detection of changes in the subsurface or with the reconstruction of virtual signals between two receivers by crosscorrelation of signals from diffuse sources. These concepts can be applied in NDT in civil engineering for various purposes, e. g. to detect changes in bridges. Here it is demonstrated using data from a reference structure on our test site. Practical applications can be expected in the very near future. T2 - European Conference on Non-Destructive Testing (ECNDT) CY - Gothenburg, Sweden DA - 11.6.2018 KW - Ultrasound KW - Monitoring KW - Concrete KW - Interferometry KW - Coda PY - 2018 AN - OPUS4-46844 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wilsch, Gerd T1 - Fast quantitave chemical analysis of concrete using LIBS N2 - Overview about LIBS applications for investigation of building materials. T2 - NDT&E Advanced Training Workshop CY - Berlin, Germany DA - 27.06.2018 KW - LIBS KW - Concrete KW - Damage processes KW - Chlorid KW - Sulfate KW - Alkalies PY - 2018 AN - OPUS4-46821 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wilsch, Gerd T1 - Application of LIBS for the chemical investigation of concrete infrastructure N2 - Concrete is often used in combination with steel as reinforced concrete. Environmental influences, especially the ingress of harmful ions in combination with the ingress of water, trigger different damage processes which reduce the designed lifetime of a structure. The ingress of chlorides from de-icing salt or sea water leads to corrosion of the reinforcement. Also the carbonation of the concrete may trigger the corrosion of the reinforcement. The ingress of alkalis from de-icing salts may cause the expansion of the amorphous silica aggregates (alkali-silica reaction) through formation of a swelling gel of calcium silicate hydrate if water is present. The ingress of sulfates may cause spalling of the concrete surface due to ettringite formation. BAM has developed the LIBS technique for automated laboratory use with high numbers of samples to investigate transport processes of harmful species (Cl-, CO2, SO42- and alkalis) in concrete. Information about ingress depth and the quantitative values are important to estimate the remaining lifetime of the infrastructure. To get information about the ingress depth, a core has to be taken and cut in the middle. The measurements are carried out at the cross section. The main advantages of LIBS are the direct measurement on the surface of the concrete, fast analysis (sample rate 100 Hz) with a spatial resolution of up to 100 µm, the consideration of the heterogeneity of the concrete. The possibility of automated measurements saves a lot of manpower and time. At the same time a 2D-evaluation provides information about hot spots of elemental concentration which may not be found by standard methods. Typical results of 2D investigation of concrete in laboratory will be presented. The performance is also demonstrated by examples for onsite applications using a mobile LIBS system. The road map to standardization is presented as well. T2 - 12th ECNDT CY - Gothenburg, Sweden DA - 11.06.2018 KW - LIBS KW - Concrete KW - Chloride KW - Sulfates KW - Heterogeneity PY - 2018 AN - OPUS4-46828 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wilsch, Gerd T1 - Application of LIBS for the chemical investigation of concrete infrastructure N2 - The majority of the built infrastructure is made of concrete, which is a multiphase system made of cement, aggregates, water and pores. Concrete is often used in combination with steel as reinforced concrete. Environmental influences, especially the ingress of harmful ions in combination with the ingress of water, trigger different damage processes which reduce the designed lifetime of a structure. The ingress of chlorides from de-icing salt or sea water leads to corrosion of the reinforcement. Also the carbonation of the concrete may trigger the corrosion of the reinforcement. The ingress of alkalis from de-icing salts may cause the expansion of the amorphous silica aggregates (alkali-silica reaction) through formation of a swelling gel of calcium silicate hydrate if water is present. The ingress of sulfates may cause spalling of the concrete surface due to ettringite formation. For the standard procedure in civil engineering cores are taken, cut in slices, grinded and the obtained homogenized powder is solved in acid and investigated by standard procedures. BAM has developed the LIBS technique for the 2D evaluation of the chemical composition of concrete [1-11]. The technique is established for automated laboratory use with high numbers of samples to investigate transport processes of harmful species (Cl-, CO2, SO42- and alkalis) in concrete. Information about ingress depth and the quantitative values are important to estimate the remaining lifetime of the infrastructure. LIBS is a surface technique. To get information about the ingress depth, a core has to be taken and cut in the middle. The measurements are carried out at the cross section. The main advantages of LIBS are the direct measurement on the surface of the concrete, fast analysis (sample rate 100 Hz) with a spatial resolution of up to 100 µm, the consideration of the heterogeneity of the concrete and the possibility of automated measurements which save a lot of manpower and time. As an example the investigation of ingress profiles for standard diffusion and migration tests in civil engineering takes hours in comparison to just a few minutes using LIBS. At the same time a 2D-evaluation provides information about hot spots of elemental concentration which may not be found by standard methods. Ingress of chlorides due to a crack in a repair mortar. Left: Photo of the cross section of a concrete core and the surface investigated by LIBS (area 70 mm x 70 mm). Right: Color coded chlorine intensity on the cross section of a concrete core, dark red represents high chlorine content. The state of the art of LIBS technique for applications in civil engineering will be presented, including typical results of 2D investigation of concrete in laboratory. The performance is also demonstrated by examples for onsite applications using a mobile LIBS system. The road map to standardization is presented as well. T2 - ICCRRR2018, 5th international conference on Concrete Repair, Rehabilitation and Retrofitting CY - Cape Town, South Africa DA - 19.11.2018 KW - LIBS KW - Chlorid KW - Alkalies KW - Concrete KW - Damage PY - 2018 AN - OPUS4-46781 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wilsch, Gerd T1 - Detection of ion ingress by LIBS for Evaluation of the remaining lifetime of a concrete structure N2 - The majority of the built infrastructure is made of concrete, which is a multiphase system made of cement, aggregates, water and pores. Concrete is often used in combination with steel as reinforced concrete. Environmental influences, especially the ingress of harmful ions in combination with the ingress of water, trigger different damage processes which reduce the designed lifetime of a structure. The ingress of chlorides from de-icing salt or sea water leads to corrosion of the reinforcement. Also the carbonation of the concrete may trigger the corrosion of the reinforcement. The ingress of alkalis from de-icing salts may cause the expansion of the amorphous silica aggregates (alkali-silica reaction) through formation of a swelling gel of calcium silicate hydrate if water is present. The ingress of sulfates may cause spalling of the concrete surface due to ettringite formation. For the standard procedure in civil engineering cores are taken, cut in slices, grinded and the obtained homogenized powder is solved in acid and investigated by standard procedures. BAM has developed the LIBS technique for the 2D evaluation of the chemical composition of concrete [1-11]. The technique is established for automated laboratory use with high numbers of samples to investigate transport processes of harmful species (Cl-, CO2, SO42- and alkalis) in concrete. Information about ingress depth and the quantitative values are important to estimate the remaining lifetime of the infrastructure. LIBS is a surface technique. To get information about the ingress depth, a core has to be taken and cut in the middle. The measurements are carried out at the cross section. The main advantages of LIBS are the direct measurement on the surface of the concrete, fast analysis (sample rate 100 Hz) with a spatial resolution of up to 100 µm, the consideration of the heterogeneity of the concrete and the possibility of automated measurements which save a lot of manpower and time. As an example the investigation of ingress profiles for standard diffusion and migration tests in civil engineering takes hours in comparison to just a few minutes using LIBS. At the same time a 2D-evaluation provides information about hot spots of elemental concentration which may not be found by standard methods. Ingress of chlorides due to a crack in a repair mortar. Left: Photo of the cross section of a concrete core and the surface investigated by LIBS (area 70 mm x 70 mm). Right: Color coded chlorine intensity on the cross section of a concrete core, dark red represents high chlorine content. The state of the art of LIBS technique for applications in civil engineering will be presented, including typical results of 2D investigation of concrete in laboratory. The performance is also demonstrated by examples for onsite applications using a mobile LIBS system. The road map to standardization is presented as well. T2 - ASNT SMT/NDT-CE 2018 CY - New Brunswick, NJ, USA DA - 27.08.2018 KW - Damage processes KW - LIBS KW - Concrete KW - Chloride PY - 2018 AN - OPUS4-46782 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Niederleithinger, Ernst T1 - The LAUS: First applications of a new system for ultrasonic imaging of very concrete structures N2 - The LAUS (Large Aperture Ultrasonic System) has been developed to image very thick concrete structures, which are not accessible for commercial systems. The device and the corresponding software is the result of joint research of BAM, an ultrasonic instrument manufacturer and University of Kassel, Germany. It consists of 12 separate arrays of 32 point-contact shear wave transducers each, which can be deployed in flexible configurations. Each array is combined with battery and transmitter, receiver and wireless communication electronics. Three case histories are presented. First the system was deployed on a 5-m thick heavily reinforced foundation slab. The reflection of the slab’s bottom was imaged clearly. In addition, a multiple reflection was registered, thus giving hope that even thicker elements might be imaged by the instrument. Second, the LAUS was used to investigate a massive bridge girder where a heavy rainstorm during concreting had led to imperfections that were visible after removing the formwork was removed. The LAUS could image tendon ducts in 1.8m depth and the backwall closely behind them. Some limited areas showed blurred reflections and were checked by drill holes; these areas were affected by diffuse damage which could be repaired by injections. Third, a large retaining wall was checked for thickness. Meanwhile, the LAUS has been used in underground waste deposits (nuclear and other) for quality assurance of sealing plugs. A confirmed penetration depth of about 7 m has been reached. T2 - ASNT SMT/NDT-CE 2018 CY - New Brunswick, NJ, USA DA - 27.8.2018 KW - LAUS KW - Ultrasound KW - Imaging KW - Concrete PY - 2018 AN - OPUS4-45828 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Cunningham, Patrick A1 - Wang, L. A1 - Kane, S. A1 - Kim, A. A1 - Jenkins, B. M. A1 - Miller, S. A. T1 - Lifecycle implications and mechanical properties of carbonated biomass ashes as carbon-storing supplementary cementitious materials N2 - Methods to sequester and store atmospheric CO2 are critical to combat climate change. Alkaline-rich bioashes are potential carbon fixing materials. This work investigates potential co-benefits from mineralizing carbon in biomass ashes and partially replacing high embodied greenhouse gas (GHG) Portland cement (PC) in cement-based materials with these ashes. Specifically, rice hull ash (RHA), wheat straw ash (WSA), and sugarcane bagasse ash (SBA) were treated to mineralize carbon, and their experimental carbon content was compared to modeled potential carbonation. To understand changes in the cement-based storage materials, mortars made with CO2-treated WSA and RHA were experimentally compared to PC-only mortars and mortars made with ashes without prior CO2 treatment. Life cycle assessment methodology was applied to understand potential reductions in GHG emissions. The modeled carbonation was ∼18 g-CO2/kg-RHA and ∼180 g-CO2/kg-WSA. Ashes oxidized at 500 °C had the largest measured carbon content (5.4 g-carbon/kg-RHA and 35.3 g-carbon/kg-WSA). This carbon appeared to be predominantly residual from the biomass. Isothermal calorimetry showed RHA-PC pastes had similar heat of hydration to PC-pastes, while WSA-PC pastes exhibited an early (at ∼1.5 min) endothermic dip. Mortars with 5 % and 15 % RHA replacement had 1–12 % higher compressive strength at 28 days than PC-only mortars, and milled WSA mortars with 5 % replacement had 3 % higher strength. A loss in strength was noted for the milled 15 % WSA, the CO2-treated 5 %, and the 15 % WSA mortars. Modeled reductions in GHG emissions from CO2-treated ashes were, however, marginal (<1 %) relative to the untreated ashes. KW - CO2 sequestration KW - CO2 storage KW - Biomass ash KW - Supplementary cementitious materials KW - Concrete PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-626959 DO - https://doi.org/10.1016/j.biombioe.2025.107772 SN - 1873-2909 VL - 197 SP - 1 EP - 13 PB - Elsevier CY - Amsterdam AN - OPUS4-62695 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Vogler, Nico A1 - Drabetzki, Philipp A1 - Lindemann, Mathias A1 - Kühne, Hans-Carsten T1 - Description of the concrete carbonation process with adjusted depth resolved thermogravimetric analysis N2 - The thermal gravimetric analysis (TG) is a common method for the examination of the carbonation progress of cement-based materials. Unfortunately, the thermal properties of some components complicate the evaluation of TG results. Various hydrate phases, like ettringite (AFt), C-S-H and AFm decompose almost simultaneously in the temperature range up to 200 °C. Additionally, physical bound water is released in the same temperature range. In the temperature range between 450 °C and 600 °C the decomposition of calcium hydroxide and amorphous or weakly bound carbonates takes place simultaneously. Carbonates, like calcite, from limestone powder or other additives may be already contained in the noncarbonated sample material. For this research an attempt was made to minimise the influence of these effects. Therefore, differential curves from DTG-results of non-carbonated areas and areas with various states of carbonation of the same sample material were calculated and evaluated. Concretes based on three different types of cement were produced and stored under accelerated carbonation conditions (1 % CO2 in air). The required sample material was obtained by cutting slices from various depth of previously CO2-treated specimen and subsequent grinding. During the sample preparation, a special attention was paid that no additional carbonation processes took place. As reference method for the determination of the carbonation depth the sprayed application of phenolphthalein solution was carried out. Microscopic analysis where examined to confirm the assumptions made previously. Furthermore, the observed effect of encapsulation of calcium hydroxide by carbonates caused by the accelerated carbonation conditions was examined more closely. KW - Microscopy KW - Accelerated carbonation KW - Carbonation behaviour KW - Concrete KW - Thermal Analysis PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-530571 DO - https://doi.org/10.1007/s10973-021-10966-1 VL - 147 IS - 11 SP - 1 EP - 14 PB - Springer AN - OPUS4-53057 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Deresse, N. E. A1 - Thiele, Marc A1 - Pirskawetz, Stephan A1 - Sarem, M. A1 - Francois, St. A1 - Verstrynge, E. T1 - Evaluation of Concrete Fatigue Damage with Elastic Wave-based Measurement Techniques N2 - The fatigue damage evolution and the fatigue life of quasi-brittle materials such as concrete are not yet completely understood. Accordingly to get better insights, researchers have recently been incorporating advanced measuring techniques in their fatigue experiments. In this research, acoustic emission techniques (AET), active ultrasonic, and deformation measurements are used to track the damage evolution of concrete samples subjected to fatigue loading. The samples are subjected to constant amplitude and stepwise fatigue loading in Brazilian splitting test set-ups. Initially, a good agreement is observed between the deformation and the ultrasonic measurements in capturing the crack propagation during Brazilian splitting tests. The three fatigue damage phases could be identified with all of the three techniques. The Phase II damage rates quantified by deformation measurements and AET in stepwise fatigue tests were used to predict the number of cycles to failure at various stress levels. The predictions were validated using the number of cycles to failure of the constant amplitude fatigue tests. T2 - 36th Conference of the European Working Group on Acoustic Emission CY - Potsdam, Germany DA - 18.09.2024 KW - Concrete KW - Acoustic emission KW - Ultrasonic testing KW - Fatigue PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-615677 DO - https://doi.org/10.58286/30228 SN - 1435-4934 VL - 29 IS - 10 SP - 1 EP - 10 PB - NDT.net AN - OPUS4-61567 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Küttenbaum, Stefan A1 - Taffe, A. A1 - Braml, T. A1 - Maack, Stefan ED - Alexander, M. G. ED - Beushausen, H. ED - Dehn, F. ED - Moyo, P. T1 - Reliability assessment of existing bridge constructions based on results of non-destructive testing N2 - The non-destructive testing methods available for civil engineering (NDT-CE) enable the measurements of quantitative parameters, which realistically describe the characteristics of existing buildings. In the past, methods for quality evaluation and concepts for validation expanded into NDT-CE to improve the objectivity of measured data. Thereby, a metrological foundation was developed to collect statistically sound and structurally relevant information about the inner construction of structures without destructive interventions. More recently, the demand for recalculations of structural safety was identified. This paper summarizes a basic research study on structural analyses of bridges in combination with NDT. The aim is to use measurement data of nondestructive testing methods as stochastic quantities in static calculations. Therefore, a methodical interface between the guide to the expression of uncertainty in measurement and probabilistic approximation procedures (e.g. FORM) has been proven to be suitable. The motivation is to relate the scientific approach of the structural analysis with real information coming from existing structures and not with those found in the literature. A case study about the probabilistic bending proof of a reinforced concrete bridge with statistically verified data from ultrasonic measurements shows that the measuring results fulfil the requirements concerning precision, trueness, objectivity and reliability. T2 - International Conference on Concrete Repair, Rehabilitation and Retrofitting (ICCRRR 2018) CY - Cape Town, South Africa DA - 19.11.2018 KW - NDT KW - Concrete KW - Probabilistic reassessment KW - Bridge PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-467898 DO - https://doi.org/10.1051/matecconf/201819906001 SN - 2261-236X VL - 199 SP - 06001, 1 EP - 9 PB - MATEC Web of Conferences AN - OPUS4-46789 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Klimek, André A1 - Stelzner, Ludwig A1 - Hothan, Sascha A1 - Zehfuß, Jochen T1 - Influence of thermal strain on concrete spalling N2 - Understanding the susceptibility to spalling of concrete members in case of fire is important to evaluate the residual load-bearing capacity. The investigations of the spalling phenomenon of a concrete mixture using real scale members are necessary but expensive to carry out. Reducing the specimen size leads to an increase of boundary effects that can result in a reduced spalling or absence of spalling. In this study, fire tests were carried out on unrestrained, single-sided exposed, cuboid shaped specimens (0.6 m x 0.6 m x 0.29 m) as well as unrestrained and steel ring restrained cylindrical specimens (Ø = 0.47 m, h = 0.29 m), which induce different boundary conditions. These fire tests were carried out on two ordinary concrete mixtures. The two mixtures differ only in the type of aggregates (quartz gravel and basalt grit) and were used to investigate the influence of the thermal expansion of the aggregate on the spalling behaviour of the concrete. The results show a significant increase of the spalling depth due to the restrained thermal expansion achieved by the applied steel rings. Additionally, the type of aggregate has a direct influence on the spalling behaviour of a concrete mixture. The reduction of the boundary effects by the steel rings recreate the test conditions in the centre of a large concrete member. Thus, this type of specimen is suitable to determine the susceptibility to spalling of a material (screening-tests) as preliminary investigations to full scale fire tests. KW - Spalling KW - Concrete KW - Fire test KW - Restraint KW - Screening test PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-593350 DO - https://doi.org/10.1617/s11527-023-02274-x VL - 57 SP - 1 EP - 14 PB - Springer AN - OPUS4-59335 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sigrüner, M. A1 - Hüsken, Götz A1 - Pirskawetz, Stephan A1 - Herz, J. A1 - Muscat, D. A1 - Strübbe, N. T1 - Pull-out behavior of polymer fibers in concrete N2 - The bond between polymer fibers and the surrounding cementitious matrix is essential for the development of concrete reinforcement. The single fiber pull-out test (SFPT) is the standard characterization technique for testing the bond strength. However, the different phases of debonding cannot be distinguished by the SFPT. This study investigates the debonding of different polymer fibers from the surrounding cementitious matrix with a modified SFPT and proposes methods to change the SFPT setup to generate more valuable information on the debonding mechanism. The SFPT was equipped with linear variable differential transformers (LVDT), digital image correlation (DIC) and acoustic emission (AE) analysis. The results demonstrate that the modified SFPT allows a better understanding of the different phases of debonding during fiber pull-out. Furthermore, bond strength values calculated by different methods reveal that the chemical bond of the investigated polymers is not different as reported by previous studies. Deformation measurements performed using LVDTs and DIC are suitable measuring techniques to characterize the debonding mechanism in SFPT. A correlation between recorded AE and debonding phases was not found. KW - Polymer Fibres KW - Concrete KW - Pull-Out Behaviour KW - Debonding Mechanism PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-582918 DO - https://doi.org/10.1002/pol.20230264 SN - 2642-4169 SP - 1 EP - 13 PB - Wiley Periodicals, LLC. AN - OPUS4-58291 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pohl, Christoph A1 - Smilauer, V. A1 - Unger, Jörg F. T1 - A three-phase transport model for high-temperature concrete simulations validated with X-ray CT data N2 - Concrete exposure to high temperatures induces thermo-hygral phenomena, causing water phase changes, buildup of pore pressure and vulnerability to spalling. In order to predict these phenomena under various conditions, a three-phase transport model is proposed. The model is validated on X-ray CT data up to 320 ◦C, showing good agreement of the temperature profiles and moisture changes. A dehydration description, traditionally derived from thermogravimetric analysis, was replaced by a formulation based on data from neutron radiography. In addition, treating porosity and dehydration evolution as independent processes, previous approaches do not fulfil the solid mass balance. As a consequence, a new formulation is proposed that introduces the porosity as an independent variable, ensuring the latter condition. KW - Concrete KW - Porous media KW - Spalling KW - Dehydration KW - Moisture transport KW - Heat transfer KW - Pore pressure KW - Porosity KW - Finite elements PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-532840 UR - https://doi.org/10.5281/zenodo.4890635 DO - https://doi.org/10.3390/ma14175047 SN - 1996-1944 VL - 14 IS - 17 SP - 1 EP - 21 PB - MDPI CY - Basel AN - OPUS4-53284 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Unger, Jörg F. T1 - Concrete under cyclic loading a continuum damage model and a temporal multiscale approach N2 - The durability of concrete structures and its performance over the lifetime is strongly influenced by many interacting phenomena such as e.g. mechanical degradation due to fatigue loading, loss of prestress, degradation due to chemical reactions or creep and shrinkage. Failure due to cyclic loading is generally not instantaneous, but characterized by a steady damage accumulation. Many constitutive models for concrete are currently available, which are applicable for specific loading regimes, different time scales and different resolution scales. A key limitation is that the models often do not address issues related to fatigue on a structural level. Very few models can be found in the literature that reproduce deterioration of concrete under repeated loading-unloading cycles. The objective of this paper is the presentation of numerical methods for the simulation of concrete under fatigue loading using a temporal multiscale method. First, a continuum damage model for concrete is developed with a focus on fatigue under compressive stresses. This includes the possibility to model stress redistributions and capture size effects. In contrast to cycle based approaches, where damage is accumulated based on the number of full stress cycles, a strain based approach is developed that can capture cyclic degradation under variable loading cycles including different amplitudes and loading frequencies. Second, a multiscale approach in time is presented to enable structural computations of fatigue failure with a reduced computational effort. The damage rate within the short time scale corresponding to a single cycle is computed based on a Fourier based approach. This evolution equation is then solved on the long time scale using different time integration schemes. T2 - 6th European Conference on Computational Mechanics (ECCM 6) CY - Glasgow, UK DA - 11.06.2018 KW - Cycle jump KW - Fatigue damage KW - Concrete PY - 2018 AN - OPUS4-45696 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Unger, Jörg F. A1 - Kindrachuk, Vitaliy A1 - Hirthammer, Volker A1 - Titscher, Thomas A1 - Pohl, Christoph T1 - The importance of multiphysics and multiscale modelling of concrete to understand its complex macroscopic properties N2 - Concrete is a complex material. Its properties evolve over time, especially at early age, and are dependent on environmental conditions, i.e. temperature and moisture conditions, as well as the composition of the material. This leads to a variety of macroscopic phenomena such as hydration/solidification/hardening, creep and shrinkage, thermal strains, damage and inelastic deformations. Most of these phenomena are characterized by specific set of model assumptions and often an additive decomposition of strains into elastic, plastic, shrinkage and creep components is performed. Each of these phenomena are investigated separately and a number of respective independent models have been designed. The interactions are then accounted for by adding appropriate correction factors or additional models for the particular interaction. This paper discusses the importance of reconsider even in the experimental phase the model assumptions required to generalize the experimental data into models used in design codes. It is especially underlined that the complex macroscopic behaviour of concrete is strongly influenced by its multiscale and multiphyscis nature and two examples (shrinkage and fatigue) of interacting phenomena are discussed. T2 - International RILEM Conference on Materials, Systems and Structures in Civil Engineering CY - Lyngby, Denmark DA - 22.08.2016 KW - Concrete KW - Multiscale KW - Multiphysics PY - 2016 VL - 1 SP - 115 EP - 124 PB - International RILEM Conference on Materials, Systems and Structures in Civil Engineering, Conference segment on COST TU1404 AN - OPUS4-38651 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Titscher, Thomas T1 - Implicit/explicit (IMPL-EX) integration of the gradient enhanced damage model N2 - Isotropic damage models are widely used for the finite element simulation of softening materials, e.g. in mesoscale simulations of concrete. Regularization techniques must be employed to obtain a physically meaningful fracture energy upon mesh refinement. In regularized local damage models the strains localize in single elements allowing them to represent weak or strong discontinuities. In implicit integration schemes, these models can exhibit convergence Problems caused by an ill-conditioned tangent stiffness. This corresponds to the loss of ellipticity of the local rate equilibrium equations. Oliver et al. developed the implicit/explicit (IMPL-EX) integration scheme which overcomes These problems in local damage models. The internal damage driving variable is extrapolated based on previous implicitly determined values. This provides two main benefits: First, it always results in a symmetric positive semi-definite algorithmic stiffness matrix which precludes ill-posedness. Second, the system becomes incrementally linear and converges in one Newton-Raphson iteration. Even though the IMPL-EX algorithm, like explicit algorithms in general, requires smaller time steps than implicit schemes to obtain the same accuracy, it leads to a computational speedup. The gradient enhanced damage model by Peerlings is a nonlocal damage model that provides the regularization by limiting the curvature of the damage-driving strains. These models do not lose their ellipticity. However, structural instabilities often require tiny time steps and many iterations to obtain convergence. Here, the second aspect of the IMPL-EX scheme reduces the computational costs. This is shown in simulations of the complex geometry of concrete mesostructures, where only the gradient enhanced matrix material and linear elastic aggregates are considered. With regard to future mesoscale simulations, the remaining component of the mesoscopic structure, the interfacial transition zone and its degradation, has to be included. This adds a local damage model to the nonlocal problem. Thus, an IMPL-EX implementation has to be provided for both models to benefit from the increase of robustness and performance. T2 - ECCOMAS Congress 2016 CY - Crete, Greece DA - 05.06.2016 KW - Concrete KW - Mesoscale KW - IMPL-EX PY - 2016 AN - OPUS4-38671 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Unger, Jörg F. T1 - The importance of multiphysics and multiscale modeling of concrete to understand its complex macroscopic properties N2 - Concrete is a complex material. Its properties evolve over time, especially at early age, and are dependent on environmental conditions, i.e. temperature and moisture conditions, as well as the composition of the material. This leads to a variety of macroscopic phenomena such as hydration/solidification/hardening, creep and shrinkage, thermal strains, damage and inelastic deformations. Most of these phenomena are characterized by specific set of model assumptions and often an additive decomposition of strains into elastic, plastic, shrinkage and creep components is performed. Each of these phenomena are investigated separately and a number of respective independent models have been designed. The interactions are then accounted for by adding appropriate correction factors or additional models for the particular interaction. This paper discusses the importance of reconsider even in the experimental phase the model assumptions required to generalize the experimental data into models used in design codes. It is especially underlined that the complex macroscopic behaviour of concrete is strongly influenced by its multiscale and multiphyscis nature and two examples (shrinkage and fatigue) of interacting phenomena are discussed. T2 - International RILEM Conference on Materials, Systems and Structures in Civil Engineering CY - Lyngby, Denmark DA - 22.08.2016 KW - Multiscale KW - Concrete KW - Multiphysics PY - 2016 AN - OPUS4-38652 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Unger, Jörg F. T1 - Mechanics group at Federal Institute for Materials Research and Testing N2 - The poster presents the work of the mechanics group in BAM, department 7. The current projects deal with the simulation of concrete on different spatial and temporal scales - ranging from the creation of mesoscale geometries up to fatigue and high strain rate impact phenomena. T2 - COST Meeting 1404 CY - Ljubljana, Slovenia DA - 16.05.2015 KW - Mechanics KW - Contact KW - Multiscale KW - Concrete KW - Constitutive modelling PY - 2015 AN - OPUS4-38647 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hirthammer, Volker T1 - Modeling the interactions of creep, shrinkage and damage in a multiphysics simulation of concrete N2 - The time dependent, mechanical behavior of concrete is affected by multiple phenomena like creep, shrinkage and damage propagation. The interactions of these processes are supposed to have significant influence on the materials response to external loading. For example it can be observed that the compressive strength of concrete rises with lowering the moisture content [Dahms, 1968]. Most of the constitutive models for finite element methods are designed with just a single phenomena in mind. In multiphysics simulations it is quiet common to use a linear superposition, i.e. additive decomposition of the total strain into elastic shrinkage, creep or thermal strains. In this paper, the interactions of creep, shrinkage and damage models are investigated, in particular for cases where the assumption of linear superposition is questionable. A gradient enhanced damage model proposed by [Peerlings et al., 1996] is employed. Creep is modeled as a Kelvin chain as described in [Jirásek and Bažant, 2001]. Shrinkage is simulated by using two different approaches. The first model simulates shrinkage as an additional moisture dependent strain component. In the second model, shrinkage is simulated as a moisture dependent pore pressure applied to the solid bulk. The impact of model interactions will be discussed with a focus on simulating the influence of the moisture content on the macroscopic strength. The model is validated by comparison to experimental data. T2 - 6th European Conference on Computational Mechanics (ECCM 6) CY - Glasgow, UK DA - 11.06.2018 KW - Concrete KW - Damage KW - FEM KW - Multiphysics Problems KW - Shrinkage PY - 2018 AN - OPUS4-45692 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Klimek, André A1 - Stelzner, Ludwig A1 - Hothan, Sascha A1 - Rogge, Andreas T1 - Fire induced concrete spalling in combination with size effects N2 - The size effect has its origin in fracture mechanics and describes the formation as well as propagation of cracks in brittle and solid materials in dependence of the specimen size. However, the size effect in concrete spalling describes the damage behaviour on a macroscopic scale for different sized specimens in case of fire. Concrete spalling is a very complex and yet not fully understood phenomenon. To reduce the effort of fire tests to analyse the spalling behaviour of concrete mixtures, this study investigates the susceptibility to spalling for six different concrete mixtures and three specimen sizes. The sizes were divided in full scale slabs (1.8 m x 1.2 m x 0.3 m), intermediate scale cuboids (0.6 m x 0.6 m x 0.3 m) and small scale cylinders (Ø0.15 m x 0.3 m). For this purpose, a novel test set-up was built to test six intermediate scale or twelve small scale specimens simultaneously to ensure a similar heating regime for every specimen. All specimens were fire exposed on one side and remained unrestrained. A size effect occurred for four of the six concrete mixtures. Compared to the full scale specimens the spalling was reduced significantly for all smaller specimen sizes. Additionally, spalling did not occur for the small scale specimens. The results show that the specimen size is an essential parameter to investigate the susceptibility to spalling of a concrete mixture. For future investigations the testing conditions must be adjusted for the intermediate scale specimens to recreate the conditions of the slabs. KW - Concrete KW - Spalling KW - Size effect KW - Fire test PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-559231 DO - https://doi.org/10.1617/s11527-022-02051-2 VL - 55 IS - 8 SP - 1 EP - 14 PB - Springer AN - OPUS4-55923 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittrich, Tim A1 - Stelzner, Ludwig A1 - Weise, Frank T1 - Fire-induced spalling of normal strength concrete with different types of blended Portland cement N2 - The cement industry is looking to reduce its overall CO2 footprint. Greener manufacturing can be achieved by the introduction of more clinker-reduced cements. Concrete exposed to fire tends to show explosive spalling caused by thermomechanical and thermohydraulic processes. It is therefore essential to determine how concretes with clinker-reduced cements behave under fire exposure, especially for concretes containing calcined clays, as these are expected to be the supplementary cementitious material of the future. In this paper, normal strength concretes with four different cements (CEM I, CEM II/A-LL, CEM III/A and CEM II/B-Q) were examined for their fire-induced spalling behaviour. In addition, a mix with PP fibres was investigated for each concrete. The experiments were conducted on ring-restrained cylindrical specimens exposed to the hydrocarbon fire curve. The results showed that the cement type influences spalling behaviour. Samples with CEM I spalled the least, followed by CEM II/A-LL and CEM III/A. Finally, samples with CEM II/B-Q showed the most severe damage. It was found that the spalling behaviour of different concretes correlates with the moisture content before exposure to fire, meaning that higher moisture content leads to higher spalling susceptibility. The use of 2 kg/m³ PP fibres completely inhibited spalling regardless of the cement type used and therefore remains a successful avoidance strategy. T2 - Structures in Fire 2024 CY - Coimbra, Portugal DA - 19.06.2024 KW - Fire-induced concrete spalling KW - Concrete KW - Blended Portland cement KW - SCM KW - PP-fibres PY - 2024 SN - 978-989-35292-2-5 DO - https://doi.org/10.30779/cmm_SIF24 VL - 1st Edition SP - 461 EP - 471 AN - OPUS4-60809 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Johann, Sergej A1 - Strangfeld, Christoph A1 - Chahardehinejad, Omid A1 - Bartholmai, Matthias ED - Pastrama, S. D. ED - Constantinescu, D. M. T1 - Passive RFID Transponder – Low-Power Multi-Sensor Interface for Structural Health Monitoring in Concrete N2 - Structural Health Monitoring (SHM) has become very important in today's rapidly developing time. High buildings, large bridges and complex technical structures need to be monitored continuously and this over long periods. Visual monitoring cannot evaluate the internal condition of building structures. Thus, material embedded sensors are needed. Cable connection of these sensors pose the disadvantage of weak spots and water intrusion. For concrete embedded sensors the use of batteries is not convenient, because of limited lifetime, difficult charging, and generation of electrical waste.. Hence, monitoring should be implemented preferentially with firmly embedded passive RFID sensor modules. However, since the concrete structure forms an electromagnetically reflective and absorbing barrier, only limited energy can be transmitted to the module. This project requires a highly energy-saving system, which can record different sensor parameters at critical points. T2 - 35th Danubia - Adria Symposium on Advances in Experimental Mechanics CY - Sinaia, Romania DA - 25.09.2018 KW - RFID KW - Structural Health Monitoring KW - Passive sensor interface KW - Concrete PY - 2018 SN - 978-606-23-0874-2 SP - 141 EP - 142 AN - OPUS4-46097 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pimienta, Pierre A1 - McNamee, Robert A1 - Robert, Fabienne A1 - Boström, Lars A1 - Huang, Shan-Shan A1 - Mróz, Katarzyna A1 - Davie, Colin A1 - Mohaine, Siyimane A1 - Alonso, Maria Cruz A1 - Bodnarova, Lenka A1 - Bosnjak, Josipa A1 - Dal Pont, Stefano A1 - Dao, Vinh A1 - Dauti, Dorjan A1 - Dehn, Frank A1 - Felicetti, Roberto A1 - Hager, Izabela A1 - Hela, Rudolf A1 - Hozjan, Tomaz A1 - Juknat, Michael A1 - Jumppanen, Ulla-Maija A1 - Kirnbauer, Johannes A1 - Kolsek, Jerneja A1 - Korzen, Manfred A1 - Lakhani, Hitesh A1 - Lion, Maxime A1 - Lo Monte, Francesco A1 - Maluk, Cristian A1 - Meftah, Fekri A1 - Miah, Md Jihad A1 - Millard, Alain A1 - Mindeguia, Jean-Christophe A1 - Moreau, Bérénice A1 - Msaad, Yahia A1 - Ozawa, Mitsuo A1 - Pesavento, Francesco A1 - Pham, Duc Toan A1 - Pistol, Klaus A1 - Rickard, Ieuan A1 - Rodrigues, Joao Paulo Correia A1 - Roosefid, Mohsen A1 - Schneider, Martin A1 - Sharma, Umesh Kumar A1 - Sideris, Kosmas A1 - Stelzner, Ludwig A1 - Weber, Benedikt A1 - Weise, Frank T1 - Recommendation of RILEM TC 256-SPF on fire spalling assessment during standardised fire resistance tests: complementary guidance and requirements N2 - The recommendation is based on the co-authors’ work organized by the RILEM TC 256-SPF “Spalling of concrete due to fire: testing and modelling”. It aims to provide useful information, guidance and best practices in fire spalling assessment to laboratories that perform large-scale tests based on fire resistance test standards. It provides guidance on the spalling observation techniques during testing, as well as post-test spalling quantification/assessment methods. This document is intended to be used in conjunction with the fire resistance test standards, e.g. EN 1363-1 and ISO 834-1. KW - Concrete KW - Fire spalling KW - Large scale tests KW - Standardised fire resistance tests PY - 2024 DO - https://doi.org/10.1617/s11527-023-02248-z SN - 1871-6873 VL - 57 IS - 1 SP - 1 EP - 12 PB - Springer CY - Dordrecht AN - OPUS4-59288 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pimienta, Pierre A1 - McNamee, Robert A1 - Hager, Izabela A1 - Mróz, Katarzyna A1 - Boström, Lars A1 - Mohaine, Siyimane A1 - Huang, Shan-Shan A1 - Mindeguia, Jean-Christophe A1 - Robert, Fabienne A1 - Davie, Colin A1 - Felicetti, Roberto A1 - Miah, Md Jihad A1 - Lion, Maxime A1 - Lo Monte, Francesco A1 - Ozawa, Mitsuo A1 - Rickard, Ieuan A1 - Sideris, Kosmas A1 - Alonso, Maria Cruz A1 - Millard, Alain A1 - Jumppanen, Ulla-Maija A1 - Bodnarova, Lenka A1 - Bosnjak, Josipa A1 - Dal Pont, Stefano A1 - Dao, Vinh A1 - Dauti, Dorjan A1 - Dehn, Frank A1 - Hela, Rudolf A1 - Hozjan, Tomaz A1 - Juknat, Michael A1 - Kirnbauer, Johannes A1 - Kolsek, Jerneja A1 - Korzen, Manfred A1 - Lakhani, Hitesh A1 - Maluk, Cristian A1 - Meftah, Fekri A1 - Moreau, Bérénice A1 - Pesavento, Francesco A1 - Pham, Duc Toan A1 - Pistol, Klaus A1 - Correia Rodrigues, Joao Paulo A1 - Roosefid, Mohsen A1 - Schneider, Martin A1 - Sharma, Umesh Kumar A1 - Stelzner, Ludwig A1 - Weber, Benedikt A1 - Weise, Frank T1 - Recommendation of RILEM TC 256-SPF on the method of testing concrete spalling due to fire: material screening test N2 - The recommendation is based on the coauthors’ work organized by the RILEM TC 256-SPF ‘‘Spalling of concrete due to fire: testing and modelling’’. The Committee has defined two types of screening tests for characterization of concrete propensity to fire spalling: Material screening tests and Product screening tests. Definitions of both types of tests are given in the paper. The following recommendations apply to Material screening tests. The material screening tests described in these recommendations are a set of minimum requirements to test concrete spalling propensity (for example, the minimal specimen size). This document covers the aspects of concrete characterization, specimen geometries, storage conditions, test methods and measured parameters. KW - Concrete KW - Fire Spalling KW - Screening tests KW - High temperature PY - 2023 DO - https://doi.org/10.1617/s11527-023-02202-z VL - 56 IS - 9 SP - 1 EP - 12 PB - Springer Science and Business Media LLC AN - OPUS4-60635 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -