TY - CONF A1 - Rhode, Michael T1 - Evaluation of the wear protection of modified NiMoCrSi alloy and machinability using ultrasonic-assisted milling N2 - The development of technologies for climate-neutral energy generation is an important contribution to reducing CO2 emissions, whereby the efficient use of material systems is a key factor. Wear-resistant coatings are required for highly efficient and economical steel components in energy, process and power plant engineering in order to withstand the high corrosive, tribological, thermal and mechanical loads. Considering price and supply risks as well as the increasing demands on corrosive resistance at high temperatures, conventional cobalt alloys are to be replaced by nickel alloys. In addition, there is a growing demand for defined surfaces of high quality or functional surfaces of these protective coatings. The milling required for this is often not economically feasible, especially for SMEs, due to high tool wear. A joint project of BAM and ISAF of TU Clausthal (Fosta P1550/IGF 21959 N) investigates the optimization of these challenging machining conditions by means of alloy modifications of the welding powder for plasma transferred arc cladding, without reducing the wear protection potential and using innovative ultrasonic assisted milling process for better machinability without reducing wear resistance. This article presents the results of investigations into the relationships between different alloy modifications (Ti, Al, Nb Mo and Hf with wX ≤ 0.01), the resulting microstructure and precipitation morphology, the machinability and the wear protection properties using a NiCrMoSiFeB alloy (trade name: Colmonoy 56 PTA). Tests using cast samples have already shown that the addition of Nb leads to a finer distribution of the hard phases and that this results in a reduction in cutting forces and tool wear during ultrasonic-assisted milling. The change in the microstructure morphology through the addition of Al, on the other hand, causes a significant increase in the cutting forces that occur. T2 - IIW Intermediate meeting of Commission II-A CY - Online meeting DA - 12.03.2024 KW - Ultrasonic assisted milling KW - Surface integrity PY - 2024 AN - OPUS4-61924 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hübner, Martin T1 - Effects of weld seam design on the fatigue strength of welded components with LTT welding filler N2 - Low Transformation Temperature (LTT) welding fillers offer an innovative approach to increase the compressive residual stresses in weld seams which have a positive impact on the fatigue strength of welded structures. LTT welding fillers exhibit a martensitic phase transformation close to ambient temperature which generates compressive residual stresses through a volume expansion in the weld seam and the heat affected zone (HAZ). This article focuses on the punctually placement of additional LTT layers to generate compressive residual stresses in fatigue-critical areas of conventional weld joints. This enables an economical solution without effecting the integrity of welded joints. For this, longitudinal stiffeners made of high-strength steel were gas metal arc welded using conventional welding consumable in the first layer. Afterwards, a chromium-nickel alloyed LTT welding consumable was applied on front sides of the stiffeners. By varying the welding parameters, three different weld geometries of the LTT weld bead could be realized. The effects of additional LTT layers were investigated with regards to dilution, residual stresses, and fatigue strength. The dilution does not exhibit much difference regards to the chemical composition. Therefore, it can be assumed that all three variants have a similar martensite start temperature. X-ray residual stresses measurements show that the residual stresses at the critical weld toe are significantly reduced by using LTT welding filler. While the conventional weld is characterized by tensile residual stresses, compressive residual stresses can be detected at the LTT weld. The level of residual stresses is influenced by the geometry of the LTT layer. LTT layers with a high offset to the conventional weld generate more compressive residual stresses in the HAZ than with a low offset. Therefore, the weld geometry has a considerable impact on the residual stress profile. The fatigue testing results shows that the LTT layers in all three variants has a positive impact to the fatigue strength. T2 - MPA Seminar Stuttgart 2024 CY - Stuttgart, Germany DA - 08.10.2024 KW - LTT (Low Transformation Temperature) KW - Fatigue strength KW - Weld geometry KW - Residual stress PY - 2024 AN - OPUS4-61615 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröpfer, Dirk T1 - Evaluation of the wear protection of modified Nimocrsi alloy and machinability using ultrasonic-assisted milling N2 - The targets for reducing CO2 emissions are closely linked to the development of highly efficient and economical steel components in plant, process and power plant technology, which require wear protection coatings tailored to the application and steel material for high combined corrosive, tribological, thermal and mechanical stresses. There is a growing demand in industry for defined functional surfaces of high quality for these coatings. Milling is a standard process for finish machining. The desired properties of wear resistant alloys imply significant challenges for the milling process due to high tool wear and surface defects. Besides the hardness of the coating materials, especially due to the precipitations, inhomogeneous, anisotropic weld structures of the claddings lead to further deteriorations of milling processes due to unstable milling conditions and process forces. A joint project of BAM and ISAF of TU Clausthal (Fosta P1550/IGF 21959 N) investigates the optimization of these challenging machining conditions by means of alloy modifications of the welding powder for plasma transferred arc cladding, without reducing the wear protection potential and using ultrasonic assisted milling process. T2 - 6th European Symposium on Friction, Wear and Wear Protection CY - Oberhof, Germany DA - 26.02.2024 KW - Ultrasonic assisted milling KW - Surface integrity PY - 2024 AN - OPUS4-61927 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Einfluss Spanender Bearbeitungsschritte auf die Eigenspannungen in additiv gefertigten Bauteilen aus hochfestem Stahl N2 - Der Vortrag gibt einen Überblick über den Einfluss der Prozessparameter auf die Eigenspannungen sowie die Härte in additiv gefertigten Bauteilen aus hochfestem stahl. Des Weiteren wird dargestellt, wie sich das Bauteildesign und trennende Fertigungsschritte auf die Eigenspannungen der Bauteile auswirken. T2 - Fachausschuss für Eigenspannungen AWT CY - Wolfsburg, Germany DA - 20.03.2024 KW - Hochfester Stahl KW - Additive Fertigung KW - Eigenspannungen PY - 2024 AN - OPUS4-61624 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Becker, Amadeus T1 - Adequate repair concepts for high-strength steel weld joints considering design influences N2 - The sustainable and resource-efficient production of wind energy plants requires the use of modern high-strength fine-grain structural steels. This applies to both foundation and erection structures. During the assembly of steel structures, unacceptable defects can occasionally be found in the weld area. In most cases, the economical solution would be local thermal gouging of the affected areas and re-welding. Due to the high shrinkage restraint of the joint groove in the overall structure, the superposition of design and welding-induced residual stress can lead to crack formation and ultimately to component failure, particularly in interaction with the degradation of the microstructure and mechanical properties high-strength steels during the repair process. In this context, component-related investigations (FOSTA-P1311/IGF-Nr. 20162 N) focusing on welding residual stress evolution during local thermal gouging and rewelding of S500MLO and S960QL are carried out using in-situ digital image correlation (DIC) and ex-situ X-ray diffraction methods (XRD). Therefore, self-restrained specimens were systematically gouged and rewelded with defined welding heat control (heat input, working temperature) and parameters. By means of structural mechanics calculations, geometries of self-restrained specimens were identified, that represent defined rigidity conditions of repair welds of real components. It could be shown that with increasing restraint intensity significantly higher residual stresses occur in the weld metal and heat affected zone. Furthermore, it revealed that the transverse stresses along the weld seam decrease at the weld seam ends leading to different stress state during gouging and welding. XRD analysis of the local residual stresses after cooling to RT longitudinal and transverse to the weld direction showed a good comparability with global DIC analyses. T2 - Bachelor-, Master-, Doktoranden-Kolloquium der Otto-von-Guericke Universität Magdeburg CY - Magdeburg, Germany DA - 20.10.2021 KW - High-strength steels KW - Repair welding KW - X-ray diffraction KW - Digital image correlation PY - 2021 AN - OPUS4-53640 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Engelking, Lorenz T1 - Regelwerke aus Forschungsvorhaben der Forschungsvereinigung des DVS: „Herstellung beanspruchungsgerechter Oberflächen durch Kombination innovativer additiver und abtragender Fertigungsschritte an hochbelasteten Komponenten“ N2 - In vielen Anwendungen werden aufgrund zunehmender Anforderungen an den Widerstand gegenüber hohen, kombinierten mechanischen, tribologischen, thermischen und korrosiven Beanspruchungen Hochleistungsle¬gierungen eingesetzt. Den vielfach komplexen Bauteilstrukturen, herausfordernden Fertigungseigenschaften und der Erhöhung der Ressourceneffizienz lässt sich heute mit der additiven Fertigung (AM) begegnen, dem oftmals noch unzureichende Kenntnisse über die resultierende Homogenität und Anisotropie der speziellen Gefüge und den damit verbundenen Eigenschaften entgegensteht. Viele Anwendungen benötigen zudem definierte Oberflächen mit hohen Anforderungen an die Oberflächenintegrität, dem durch komplementären Einsatz von additiven und abtragenden Fertigungsschritten Rechnung getragen wird. Hochleistungslegierungen auf der Basis von Nickel oder Kobalt sind infolge der niedrigen Wärmeleitfähigkeit verbunden mit hoher Festigkeit und Zähigkeit äußerst herausfordernd mit Blick auf eine wirtschaftliche Zerspanung mit geometrisch bestimmter Schneide. Ein Vorhaben (IGF-Nr. 20.979 N/DVS-Nr. 1.3211) der BAM und TU Clausthal/ISAF befasst sich mit der Lösung dieser Problemstellung durch gezielte Beeinflussung des Gefüges mittels Modifikation der Schweißzusatzwerkstoffe und den Einsatz des ultraschallunterstützten Fräsens (US), bei gleichzeitiger Sicherstellung der geforderten Eigenschaften der untersuchten Werkstoffe. Es werden die Ergebnisse der Mikrostruktur und der Zerspanbarkeit der Modifikationen der FeNi36-Referenzlegierung mit 0,33 Gew.-% Ti, Zr sowie Hf und der Modifikationen der CoCr-Referenzlegierung mit 1 Gew.-% Ti, Zr sowie Hf vorgestellt. Abschließend werden aus den Ergebnissen Handlungsempfehlungen abgeleitet. T2 - Sitzung der Arbeitsgruppe (AG) V 12 „Additive Fertigung“ CY - Online meeting DA - 23.11.2022 KW - Legierungsmodifikation KW - Ultraschallunterstütztes Fräsen KW - Additive Fertigung PY - 2022 AN - OPUS4-56610 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Engelking, Lorenz T1 - Bericht zum Fortschritt des laufenden Projekts: „Herstellung beanspruchungsgerechter Oberflächen durch Kombination innovativer additiver und abtragender Fertigungsschritte an hochbelasteten Komponenten“ N2 - Das DVS-Vorhaben 01.3211 „Herstellung beanspruchungsgerechter Oberflächen durch Kombination innovativer additiver und abtragender Fertigungsschritte an hochbelasteten Komponenten“ ist ein Kooperationsprojekt der Bundesanstalt für Materialforschung und -prüfung (BAM) und dem Institut für Schweißtechnik und Trennende Fertigungsverfahren (ISAF) der Technischen Universität Clausthal. Das Übergeordnete Projektziel ist das Erlangen von Erkenntnissen für eine sichere und wirtschaftliche, kombinierte additive und abtragende Fertigung aus kostenintensiven Werkstoffen hochbelasteter Komponenten insbesondere für KMU. Dabei stehe die beiden Werkstoffe CoCr26Ni9Mo5W (2.4681) und FeNi36 (1.3912) im Fokus. Mittels Modifikation der Schweißzusätze sind homogen und isotrop ausgeprägte Werkstoffeigenschaften und eine Erhöhung der Prozessstabilität und Fertigungsfreiheitsgrade bei der additiven Fertigung erzielbar. Darüber hinaus wird der Einfluss nachfolgender abtragender Bearbeitungsschritte des ultraschallunterstützen und des konventionellen Fräsprozesses untersucht. Die mit dem Forschungsvorhaben verbundenen Nutzen für KMU sind die Stärkung der Innovationsfähigkeit und der Wirtschaftlichkeit sowie die Erhöhung der Wettbewerbsfähigkeit. In AP-2 wurden die Legierungsmodifikationen des CoCr-Ausgangswerkstoffes sowie des FeNi36-Ausgangswerkstoffes abgeschlossen. In AP-4 wurden Zerspanversuche an den Modifikationen des FeNi36-Ausgangswerkstoffes sowie des CoCr-Ausgangswerkstoffes gefahren. Ferner wurden die zur Übertragung auf den MSG-Prozess ausgewählten Modifikationen beider Ausgangswerkstoffe vorgestellt. T2 - Sitzung des Fachausschusses 01 „Schweißmetallurgie und Werkstoffverhalten“ des DVS CY - Magdeburg, Germany DA - 09.11.2022 KW - Legierungsmodifikation KW - Ultraschallunterstütztes Fräsen KW - Additive Fertigung PY - 2022 AN - OPUS4-56609 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Eissel, A. T1 - Bericht zum Fortschritt des laufenden Projekts:„Herstellung beanspruchungsgerechter Oberflächen durch Kombination innovativer additiver und abtragender Fertigungsschritte an hochbelasteten Komponenten“ N2 - In vielen Anwendungen werden aufgrund zunehmender Anforderungen an den Widerstand gegenüber hohen, kombinierten mechanischen, tribologischen, thermischen und korrosiven Beanspruchungen Hochleistungsle¬gierungen eingesetzt. Den vielfach komplexen Bauteilstrukturen, herausfordernden Fertigungseigenschaften und der Erhöhung der Ressourceneffizienz lässt sich heute mit der additiven Fertigung (AM) begegnen, dem oftmals noch unzureichende Kenntnisse über die resultierende Homogenität und Anisotropie der speziellen Gefüge und den damit verbundenen Eigenschaften entgegensteht. Viele Anwendungen benötigen zudem definierte Oberflächen mit hohen Anforderungen an die Oberflächenintegrität, dem durch komplementären Einsatz von additiven und abtragenden Fertigungsschritten Rechnung getragen wird. Hochleistungslegierungen auf der Basis von Nickel oder Kobalt sind infolge der niedrigen Wärmeleitfähigkeit verbunden mit hoher Festigkeit und Zähigkeit äußerst herausfordernd mit Blick auf eine wirtschaftliche Zerspanung mit geometrisch bestimmter Schneide. Ein Vorhaben (IGF-Nr. 20.979 N/DVS-Nr. 1.3211) der BAM und TU Clausthal/ISAF befasst sich mit der Lösung dieser Problemstellung durch gezielte Beeinflussung des Gefüges mittels Modifikation der Schweißzusatzwerkstoffe und den Einsatz des ultraschallunterstützten Fräsens (US), bei gleichzeitiger Sicherstellung der geforderten Eigenschaften der untersuchten Werkstoffe. Im vorliegenden Beitrag werden für die beiden untersuchten FeNi und CoCr-Legierungen wesentliche Zusammenhänge zwischen ver¬schiedenen Legierungsmodifikationen, der entstehenden Gefüge¬morphologie und den Zerspanungseigenschaften von mittels PTA additiv gefertigter Proben dargestellt. Hierbei ließen sich Ti, Zr und Hf pulvermetallurgisch zu den jeweiligen Ausgangsschweißzusätzen hinzulegieren. T2 - #additivefertigung: Metall in bestForm CY - Essen, Germany DA - 26.10.2022 KW - Legierungsmodifikation KW - Ultraschallunterstütztes Fräsen KW - Additive Fertigung PY - 2022 AN - OPUS4-56613 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Engelking, Lorenz T1 - Untersuchungen zum Einfluss der Amplitude beim ultraschallunterstützten Schlichtfräsen schwer spanbarer FeNi Legierungen N2 - Es werden erzielte Ergebnisse des ultraschallunterstützen Schlichtfräsens einer schwer spanbaren FeNi-Legierung vorgestellt. Dabei wird der Einfluss der Amplitude der Ultraschallunterstützung auf die Zerspankraft sowie die Oberflächenintegrität untersucht, wobei ein besonderer Fokus auf die Passivkraft gelegt wird. Die Ultraschallunterstützung bedingt beim Schlichtfräsen der Alloy 36 im Vergleich zum konventionellen Fräsprozess eine signifikante Reduzierung der resultierenden Zerspankraft sowie der Rauheit. Außerdem werden oberflächennahen Druckeigenspannungen induziert. Eine Angehobene Osziallations-Amplitude beim ultraschallunterstützten Fräsen bewirkt eine Erhöhung des Anteils der Passivkraft an der resultierenden Zerspankraft sowie eine Erhöhung der oberflächennahen Druckeigenspannungen und eine Verringerung von Oberflächendefekten und Rauheitskennwerten. T2 - Bachelor-, Master-, Doktoranden-Kolloquium CY - Magdeburg, Germany DA - 30.11.2022 KW - Ultraschallunterstütztes Fräsen KW - Alloy 36 KW - Oberflächenintegrität PY - 2022 AN - OPUS4-56612 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Fügetechnik für die neue Wasserstoffökonomie – Werkstoffe, Schweißtechnologien, Perspektiven – N2 - Die Studie gibt einen Überblick über die Aspekte der Fügetechnik und ihrer Bedeutung in Wasserstofftechnologien. Dazu werden die Grundlagen der Technologiefelder Wasserstofferzeugung, -speicherung, -transport und -nutzung vorgestellt und der Stand der Technik der fügetechnischen Fertigung von Komponenten in Wasserstofftechnologien zusammengefasst. Dabei werden nicht nur exklusiv Metalle betrachtet. Anhand repräsentativer Beispiele aus der Praxis, Forschung und Entwicklung wird die Bedeutung der Fügetechnik in Wasserstofftechnologien klar herausgestellt und mögliche Perspektiven für die Zukunft abgeleitet. Hier ist ersichtlich, dass Fügetechnologien wesentliche Bedeutung für die erfolgreiche Umsetzung von technischen Komponenten der Wasserstofftechnologien haben, von der Erzeugung bis zur Anwendung. Aus gesamtwirtschaftlicher Sicht umfassen die Schwerpunkte bzw. Trends der Fügetechnik dabei: die Erstellung neuer Infrastruktur für Wasserstoffspeicherung und -transport sowie die sichere Umnutzung der bestehenden Erdgasinfrastruktur. Bei der Wasserstoffanwendung wird die effiziente massentaugliche Produktion von Brennstoffzellen immer wichtiger. Es ist zudem klar ersichtlich, dass die additive Fertigung bereits jetzt ein hohes Potential für Komponenten von Wasserstofftechnologien besitzen und dieses wachsen wird. Aus den perspektivischen Anwendungen ergeben sich zudem Herausforderungen und Forschungsbedarfe für die notwendigen nationalen und internationalen Regelwerke und technischen Normen. Schwerpunktmäßig sind hierbei die bereits bestehenden Empfehlungen und kodifizierten Regeln vollständig zu adaptieren und in die Aus- und Weiterbildung von fügetechnischem Fachpersonal einzubetten. KW - Fügetechnik KW - Wasserstoff KW - Werkstoffe KW - Prozesse KW - Perspektiven PY - 2021 UR - https://www.dvs-media.eu/de/neuerscheinungen/4425/dvs-studie-zur-fuegetechnik-fuer-die-neue-wasserstoffoekonomie-werkstoffe-schweisstechnologien-perspektiven SN - 978-3-96144-157-0 SN - 978-3-96144-158-7 VL - 373 SP - 1 EP - 59 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-53498 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Becker, Amadeus T1 - Beanspruchungsgerechte Reparatur beim Bauteilschweißen hochfester Feinkornbaustähle N2 - Eine nachhaltige und ressourceneffiziente Fertigung und Errichtung von Windenergieanlagen, sowohl auf See als auch an Land, erfordert zunehmend den Einsatz moderner hochfester Feinkornbaustähle. Werden nach dem Schweißen dieser hochfesten Konstruktionen unzulässige Defekte detektiert, sind nach geltenden Verarbeitungsrichtlinien die defekten Bereiche durch lokales Ausfugen und anschließendes Schweißen zu reparieren. Fehlende Informationen zu adäquaten Reparaturkonzepten in den Regelwerken bedingen oftmals eine unzureichende Berücksichtigung dabei auftretender zusätzlicher Beanspruchungen durch die erhöhte Schrumpfbehinderung der Ausfugenuten. Zusätzlich haben die ausführenden Betriebe vielfach kaum Kenntnis über die Degradation angrenzender Gefüge durch thermische Ausfugeprozesse und erneutes Schweißen, die in diesem Zusammenhang besonders bei den hochfesten Stählen als kritisch anzusehen sind. Das aktuelle Forschungsvorhaben der BAM (FOSTA P1311/IGF-Nr.20162N) fokussiert hierfür systematisch bauteilrelevante Untersuchungen zu den schweißbedingten Beanspruchungen und Gefügeveränderungen bei der Reparatur von hochfesten Schweißverbindungen. Wesentlich sind hierbei der Einfluss der Schrumpfbehinderung, der Wärmeführung beim Schweißen und Ausfugen sowie der Reparaturzyklenanzahl und die metallurgischen Aspekte bei den hochfesten Güten S500MLO für zukünftige Offshore-Anwendungen und S960QL für aktuelle Mobilkrananwendungen. Aufbauend auf einigen Studien zur schweißbedingten Beanspruchung hochfester Stähle zeigt der vorliegende Beitrag die Identifikation geeigneter Probengeometrien und Schweißdetails mittels numerischer und experimenteller Analysen. Dadurch wird die Übertragbarkeit der vorgestellten Schweißexperimente und Ergebnisse hinsichtlich der resultierenden Schweißeigenspannungen auf reale Reparaturfälle im Bereich des hochfesten Stahlbaus sichergestellt. Es zeigt sich in Übereinstimmung mit früheren Ergebnissen eine signifikante Erhöhung der Beanspruchungen an den variierten schlitzförmigen Prüfnähten. Das Eigenspannungsniveau sowohl im Schweißgut als auch in der WEZ korreliert mit dem Einspanngrad. Mit dem Ziel beanspruchungs- und werkstoffgerechte Reparaturkonzepte zu erarbeiten, sind zum einen geringere Wärmeinbringungen, besonders durch niedrige Zwischenlagentemperaturen und Einspannbedingungen anzustreben, um hohe Beanspruchungen und kritische Gefügedegradationen im Reparaturbereich zu vermeiden. Dies wird durch systematische Untersuchungen zum Ausfugen und Schweißen sowie letztlich dem Transfer von Verarbeitungsempfehlungen für die Anwender und Richtlinien erreicht. T2 - DVS Congress 2021 CY - Essen, Germany DA - 14.09.2021 KW - Eigenspannungen KW - Hochfest KW - Feinkornbaustahl KW - Reparatur KW - Schweißen PY - 2021 AN - OPUS4-53317 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Becker, Amadeus T1 - Consideration of design influences to provide adequate repair concepts for high-strength steel weld joints in offshore support structures N2 - The sustainable and resource-efficient production of offshore wind turbines requires the use of modern high-strength fine-grained structural steels (Martin and Schroeter, 2005). This applies to wind turbines in terms of increasing turbine sizes as well as to maintenance and installation vessels and equipment (Ummenhofer et al., 2013). Without the demanded high load-bearing capacities and boom lengths, the economic realization of these goals would be inconceivable. During the assembly of high-strength steel structures, unacceptable defects can occasionally be found in the weld area, although the welding process was executed in accordance with the specifications. In most cases, the economical solution would be local thermal gouging of the affected areas and re-welding. Corresponding standards hardly provide any information on adequate repair concepts, and there is no uniform scientific data on which to base such concepts. This applies particularly to the consideration and optimization of welding-induced stresses due to the high shrinkage hindrance of the gouging grooves and degradation of the adjacent microstructures by gouging and re-welding. The result, especially in the case of high-strength steel grades, are frequently recurring imperfections as well as a missing consideration of the additionally induced welding stresses in the design of the structure. In this context, at BAM component-relevant investigations focused on welding residual stress evolution and microstructural degradation during repair of weld joints due to local thermal gouging and re-welding are carried out within the scope of a FOSTA project (P1311, IGF 20162N). In this study, several relevant findings are discussed based on examples of structural engineering focusing on mechanical-technological properties and residual stresses, for instance found by (Schasse, 2017). Also experimental and numerical work as conducted by (Wongpanya, 2008) and weld tests under defined shrinkage restraint in special weld test-setups for research projects, e. g. FOSTA-P922 (Kannengiesser and Schroepfer, 2015) and P1011 (Kannengiesser and Schroepfer, 2017) have shown that an optimization of the welding-induced stresses of high-strength structural steels is specifically achievable by means of adapted heat control concepts (Schroepfer, 2017). The present research involves systematic investigations of influences of shrinkage restraint, the number of repair cycles and heat control during repair welding of the relatively new developed offshore-relevant high-strength steel S500MLO (EN 10225-1). For the quantification of the shrinkage restraint of weld joints, the concept of restraint intensity established by (Satho et al., 1973) was applied analogous to recent research, e. g. (Schwenk et al., 2008). By means of structural mechanics calculations, geometries of self-strained specimens were identified, that represent different defined rigidity conditions of repair welds of real components, cf. Fig. 1. It could be shown that with increasing weld joint restraint intensity significantly higher residual stresses in the weld metal and heat affected zone up to 80 % of the nominal yield strength occur, cf. Fig. 2. In relation to existing results, it has been shown that a safe repair of such welds can only be achieved by means of appropriate repair concepts and heat control taking the high welding stresses and special microstructures of high-strength steels into account. Finally, the aim of this research is to derive recommendations for repair concepts appropriate to the stresses and materials involved providing a basis for standards and guidelines, especially for SMEs, in order to avoid damage and, in most cases, expensive reworking and to improve the full utilization of the potential of high-strength steels. T2 - Wind Energy Science Conference 2021 CY - Online meeting DA - 25.05.2021 KW - High-strength structural steels KW - Welding KW - Repair KW - Residual stresses KW - Restraint PY - 2021 AN - OPUS4-53319 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Nietzke, Jonathan T1 - Diffusionsmessungen in UP-Mehrlagenschweißgut als effektives Tool gegen verzögerte Kaltrissbildung in Dickblechschweißungen N2 - Offshore-Windenergieanlagen bilden einen zentralen Bestandteil der zukünftigen Energieerzeugung. Hierzu notwendige Gründungs- und Turmstrukturen werden vorrangig aus UP-geschweißten Blechen aus hochfesten niedriglegierten Stählen mit Dicken bis zu 200 mm hergestellt. Die großen Blechdicken begünstigen hohe Schweißeigenspannungen und lange Diffusionswege für z.B. über den Schweißprozess eingebrachten Wasserstoff. Damit steigt das Risiko für eine wasserstoffunterstützte Kaltrissbildung (WKB) an. Zum sichereren Ausschluss von WKB in den geschweißten Komponenten wird in Abhängigkeit der Nahtgröße, Wärmeeinbringung und Stahlsorte eine Mindestwartezeit (MWZ) von bis zu 48 h empfohlen, bevor die zerstörungsfreie Prüfung durchgeführt wird. Es ist allerdings offen, ob die empfohlene MWZ zu konservativ ist. Einflüsse sind hier bspw. die schwierige Bewertung des Wasserstoffdiffusionsverhaltens im heterogenen UP-Mehrlagen-Schweißgut (SG) im Vergleich zum Grundwerkstoff (GW). Zudem sind nur sehr begrenzt H-Diffusions-koeffizienten für UP-Mehrlagen-SG als Grundlage zur Abschätzung des Zeitintervalls einer möglichen verzögerten Kaltrissbildung (somit MWZ) oder auch für Nachwärmprozeduren zur Wasserstoffreduktion (keine MWZ) verfügbar. Verlässliche H-Diffusionskoeffizienten sind daher ein adäquates Tool zur Bewertung des Risikos einer verzögerten WKB. Dieser Beitrag beschreibt Untersuchungen zur Charakterisierung der Wasserstoffdiffusionsverhalten in UP-Mehrlagen-SG eines 60 mm dicken Bleches einer Offshore-Stahlgüte. Dazu wurden Proben unterschiedlicher Dicke aus dem reinen Schweißgut extrahiert und über elektrochemische Permeation und Trägergasheißextraktion im Temperaturbereich bis 400 °C sehr interessante Ergebnisse zu den korrespon-dierenden Diffusionskoeffizienten erarbeitet. Es zeigte sich, dass: 1. Diffusionskoeffizienten bei Umgebungstemperatur als Tool zur Bewertung einer MWZ geeignet sind. Jedoch veränderte sich der Diffusionskoeffizient mit der untersuchten Probendicke um bis zu einer Größenordnung, d. h. daraus abgeleitete Wartezeiten differieren dementsprechend. 2. Dies deutet darauf hin, dass MWZs von bis zu 48 h einerseits möglicherweise zu konservativ gewählt sind, da der Wasserstoff schneller aus der Naht diffundiert. Andererseits muss aber auch die schnellere Diffusion in weitere potenziell risskritische Nahtbereiche, wie die WEZ, berücksichtigt werden. Daher ist noch keine direkte Aussage auf eine verallgemeinerte WKB-Anfälligkeit (ja/nein) innerhalb der MWZ möglich. 3. Im Fall einer konservativen Prävention der WKB durch Wasserstoffarmglühen (Vermeidung der MWZ) sind die Diffusionskoeffizienten bei erhöhten Temperaturen bis 400 °C zur Abschätzung der notwendigen Haltezeiten geeignet, z. B. über die numerische Simulation der Wasserstoffdiffusion. T2 - DVS Congress 2021 CY - Essen, Germany DA - 14.09.2021 KW - UP-Schweißen KW - Offshore KW - Windturbine KW - Wasserstoff KW - Diffusion PY - 2021 AN - OPUS4-53322 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Richter, Tim T1 - Characterization of Hydrogen Diffusion in a Thick-walled Submerged Arc Multi-Layer Weld Joint N2 - The energy production of the future will be dominated by CO2-emission free techniques like wind turbines and become essential in scope of the planned hydrogen economy. As onshore installation capacity is limited, the in-crease of the number of offshore wind turbines (OWT) is a major goal. In that connection, the OWTs continuously increase in size and weight and demand adequate foundations concepts like monopiles or tripods. These compo-nents are typically manufactured from welded mild steel plates with thickness up to 200 mm. The predominant welding technique is submerged arc welding (SAW) with up to five wires. In accordance with the standards, the occurrence of delayed hydrogen assisted cracking is anticipated by either a hydrogen removal heat treatment (HRHT) or a so-called minimum waiting time (MWT) before non-destructive testing (NDT) of the respective weld joint is allowed. The reason for the MWT is the necessary time for the hydrogen diffusion at ambient temperature due the high plate thickness. Both the effectiveness of a HRHT at elevated temperatures or the MWT at ambient temperature can be estimated by calculation of the diffusion time. This time depends on reliable hydrogen diffu-sion coefficients and these are rare in literature. For that reason, this study presents the hydrogen diffusion coef-ficients obtained from a multi-layer SAW joint of an offshore steel grade. Two different experimental techniques were used to identify the respective diffusion behavior: (1) hydrogen desorption experiments with a carrier gas hot extraction analyzer at elevated temperatures for the characterization of a HRHT and (2) the electrochemical permeation technique at ambient temperature for the characterization of an MWT. From both experiments, the respective diffusion coefficients were calculated. The obtained DCs are different from those reported in literature, i.e., the duration or applicability of a HRHT or MWT must be critically discussed. T2 - European Congress and Exhibition on Advanced Materials and Process - Euromat 2021 CY - Online meeting DA - 13.09.2021 KW - Welding KW - Offshore KW - Wind turbine KW - Hydrogen KW - Cracking PY - 2021 AN - OPUS4-53296 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröpfer, Dirk T1 - Process-related influences and correlations in wire arc additive manufacturing of high-strength steels N2 - High-strength fine-grained structural steels have great potential for weight-optimized, efficient structures in many modern steel applications. Further advances in efficiency can be achieved through additive manufacturing and bionic design. Commercial high-strength filler materials for wire arc additive manufacturing (WAAM) are already provided by the consumable producers. Today, application would be strictly limited due to absence of quantitative findings or any guidelines for the industry regarding welding-related stresses and component safety during manufacturing and service. Hence, process- and material-related influences and design-related restraint conditions associated with formation of residual stresses and cold cracking risk are investigated. The aim is the accessibility of special WAAM self-restraining cold cracking tests and easy applicable processing recommendations, enabling an economical, fit-for-purpose and crack-safe WAAM of high-strength steels. This first study focuses on determination of interactions between WAAM process parameters, resulting layer geometry, microstructure and residual stresses, analyzed via X-ray diffraction. Defined reference specimens are automated welded using a special WAAM solid wire (yield strength >820 MPa). Geometric properties can be specifically adjusted by wire feed and welding speed, but cannot be varied arbitrarily, since a high heat input causes local overheating, inadmissible changes of microstructure and mechanical properties, defects and comparable high tensile residual stresses. T2 - 22. Werkstofftechnischen Kolloquium der TU Chemnitz CY - Online meeting DA - 24.03.2021 KW - Additive Manufacturing KW - High-strength steel KW - Residual stresses PY - 2021 AN - OPUS4-53328 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Becker, Amadeus T1 - Konstruktive Einflüsse bei der beanspruchungsgerechten Reparatur geschweißter Bauteile aus hochfesten Feinkornbaustählen N2 - Bei der Montage von Stahlkonstruktionen kommt es trotz anforderungsgerechter schweißtechnischer Fertigung vereinzelt zur Detektion von unzulässigen Unregelmäßigkeiten im Schweißbereich. Die Verarbeitungsregelwerke empfehlen das lokale thermische Ausfugen betroffener Bereiche und erneutes Schweißen, geben aber aufgrund fehlender wissenschaftlich fundierter Untersuchungen kaum Informationen zu adäquaten Reparaturkonzepten. Dies betrifft insbesondere die Berücksichtigung und Optimierung resultierender schweißbedingter Beanspruchungen durch hohe Schrumpfbehinderungen der Ausfugenuten sowie der Gefügedegradation angrenzender Bereiche durch das Ausfugen und erneute Schweißen. Gerade bei hochfesten Stahlgüten ergeben sich dadurch häufig reduzierte mechanische Eigenschaften und zusätzliche schweißbedingte Beanspruchungen sowie erneut auftretende Nahtdefekte. Deshalb sind für das Forschungsvorhaben systematische bauteilrelevante Untersuchungen der schweißbedingten Beanspruchungen und Gefügeveränderungen reparierter Schweißnähte in Abhängigkeit von der Schrumpfbehinderung und Wärmeführung beim Schweißen und Ausfugen sowie von der Reparaturzyklenanzahl geplant, mit dem Ziel Empfehlungen für beanspruchungs- und werkstoffgerechte Reparaturkonzepte abzuleiten. Hierfür sind gerade Analysen an hochfesten Stahlgüten S500 für den Offshore-Bereich und S960QL für den Mobilkranbau interessant, die zur Errichtung und Fertigung hocheffizienter Konstruktionen wie Windenergieanlagen notwendig sind. Die Erkenntnisse bieten eine Grundlage für entsprechende Normen und Regelwerke. Damit können letztlich Schäden und zumeist teure Nacharbeiten verhindert und eine verbesserte Ausnutzung des hohen Festigkeitspotentials hochfester Stähle erreicht werden. Gerade auch KMU können mit Blick auf die Kosten für Fertigung, Schweißarbeit und Material von den Erkenntnissen beim Einsatz hochfester Stähle, die für eine effiziente Realisierung der Energiewende in Deutschland notwendig sind, profitieren. T2 - Bachelor-, Master-, Doktoranden-Kolloquium der Otto-von-Guericke Universität Magdeburg CY - Online meeting DA - 17.06.2021 KW - Eigenspannungen KW - Hochfest KW - Feinkornbaustahl KW - Reparatur KW - Schweißen PY - 2021 AN - OPUS4-53318 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baeßler, Matthias A1 - Kannengießer, Thomas T1 - Aktivitäten in Forschung und Zulassung im Bereich Windenergie N2 - Die vielfältigen Tätigkeiten der BAM im Bereich technischer Sicherheit von Windenergieanlagen werden vorgestellt und im Bereich aktueller Entwicklungen in der Fügetechnik detailliert. T2 - Arbeitskreis Gründungsstrukturen und Stahlbau der WAB CY - Online meeting DA - 13.04.2021 KW - BAM Windenergie Fügetechnik PY - 2021 AN - OPUS4-53026 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Erste Untersuchungen auf dem Weg zum WAAM-Kaltrisstest für hochfeste Stähle N2 - Hochfeste Feinkornbaustähle verfügen über ein großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. In dieser Präsentation werden erste Analysen des Einflusses der Fertigungsstrategie auf die Härte in additiv gefertigten Bauteilen aus hochfestem Stahl vorgestellt. T2 - NA 092-00-05 GA (DVS AG Q 4/Q 4.1) CY - Online meeting DA - 10.03.2021 KW - Additive Fertigung KW - Hochfester Stahl KW - Härteprüfung nach Vickers PY - 2021 AN - OPUS4-53327 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Engelking, Lorenz T1 - Bericht zum Fortschritt des laufenden Projekts: „Herstellung beanspruchungsgerechter Oberflächen durch Kombination innovativer additiver und abtragender Fertigungsschritte an hochbelasteten Komponenten“ N2 - Das DVS-Vorhaben 01.3211 „Herstellung beanspruchungsgerechter Oberflächen durch Kombination innovativer additiver und abtragender Fertigungsschritte an hochbelasteten Komponenten“ ist ein Kooperationsprojekt der Bundesanstalt für Materialforschung und -prüfung (BAM) und dem Institut für Schweißtechnik und Trennende Fertigungsverfahren (ISAF) der Technischen Universität Clausthal. Das Übergeordnete Projektziel ist das Erlangen von Erkenntnissen für eine sichere und wirtschaftliche, kombinierte additive und abtragende Fertigung aus kostenintensiven Werkstoffen hochbelasteter Komponenten insbesondere für KMU. Dabei stehe die beiden Werkstoffe CoCr26Ni9Mo5W (2.4681) und FeNi36 (1.3912) im Fokus. Mittels Modifikation der Schweißzusätze sind homogen und isotrop ausgeprägte Werkstoffeigenschaften und eine Erhöhung der Prozessstabilität und Fertigungsfreiheitsgrade bei der additiven Fertigung erzielbar. Darüber hinaus wird der Einfluss nachfolgender abtragender Bearbeitungsschritte des ultraschallunterstützen und des konventionellen Fräsprozesses untersucht. Die mit dem Forschungsvorhaben verbundenen Nutzen für KMU sind die Stärkung der Innovationsfähigkeit und der Wirtschaftlichkeit sowie die Erhöhung der Wettbewerbsfähigkeit. In AP-3 wurden die Mikrostruktur der MSG-Schweißung der CoCr-Referenzlegierung untersucht. In AP-4 wurden Zerspanversuche an der MSG-Schweißung der CoCr-Referenzlegierung durchgeführt. T2 - Sitzung des Fachausschusses 01 „Schweißmetallurgie und Werkstoffverhalten“ des DVS CY - Aachen, Germany DA - 22.02.2023 KW - Legierungsmodifikation KW - Ultraschallunterstütztes Fräsen KW - Additive Fertigung KW - Oberflächenintegrität PY - 2023 AN - OPUS4-57175 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schroeder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Ausscheidungsverhalten und Eigenschaften der schweißbedingten Wärmeeinflusszonen hochfester Stähle in Abhängigkeit der Mikrolegierungsroute N2 - Für eine signifikante Festigkeitssteigerung von vergüteten, hochfesten Feinkornbaustäh-len mit einer Nominalstreckgrenze ≥ 690 MPa, ist die Zugabe von Mikrolegierungselementen, wie Nb und Ti, unerlässlich. Die Normvorgaben zur chemischen Zusammensetzung dieser Stähle (bspw. in DIN EN 10025-6) geben zur Erzielung der vorgeschriebenen Eigenschaften dabei oft nur Grenzgehalte für die Hersteller vor. Die Wirkung der Legierungselemente in der WEZ ist teilweise komplett konträr. Somit wird eine adäquate Vorhersage der Chargenabhängigkeit hinsichtlich der Schweißeignung und des Tragver-haltens der Schweißverbindung erschwert. Neben metallographischen Untersuchungen einzelner WEZ-Bereiche wurden unter Variation der chemischen Zusammensetzung, thermodynamische Phasenberech-nungen mittels ThermoCalc durchgeführt. Hierdurch wird ein Verständnis zur Phasentransformation, Aus-scheidungswachstum und -auflösung während des Schweißens in Abhängigkeit von Temperatur und Ab-kühlbedingungen geschaffen. T2 - Forschungsseminar BAM, BMDK CY - Magdeburg, Germany DA - 05.12.2022 KW - WEZ-Erweichung KW - Thermodynamische Simulation KW - Mikrolegierungseinfluss KW - Hochfester Feinkornbaustahl KW - Modifizierter Sprühlichtbogen PY - 2023 AN - OPUS4-56837 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schroeder, Nina T1 - Influence of microalloying on precipitation behavior and notched impact strength of welded high-strength structural steels N2 - This presentation summarizes the latest results on the microalloying influence on the preciptitation behavior on the mechanical properties of welded high-strength steel with a design yield strength of 690 MPa and above. For that reason, Charpy tests were performed for the pure weld metal and different heat-affected zones. Thermodynamic phase field modeling showed the usefulness of calculations in Thermocalc to predict the preciptiation behavior and (finally) to conclude the mechanistic behavior of the welded joint. T2 - IIW Intermediate meeting of Commission II-A CY - Garching, Germany DA - 06.03.2023 KW - Welding KW - High-strength steel KW - Phase field modeling KW - Preciptiates KW - Microstructure characterization PY - 2023 AN - OPUS4-57107 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten A1 - Schröpfer, Dirk A1 - Scharf-Wildenhain, R. A1 - Hälsig, A. A1 - Kromm, Arne A1 - Kannengießer, Thomas T1 - WAAM process influences on local microstructure and residual stresses in high-strength steels N2 - High-strength fine-grain structural steels have great potential for weight optimization of many modern engineering structures. Efficient manufacturing can be achieved here above all by Wire Arc Additive Manufacturing (WAAM). First commercial high-strength welding consumables for WAAM are already available. Due to a lack of knowledge and guidelines for the industry regarding welding residual stresses and component safety in manufacturing and operation, their application is still severely limited. Residual stresses play a crucial role here, as the special microstructure of high-strength steels is sensitive to cold cracking. For this reason, process- and material-related influences, as well as the design effects on residual stress formation, are being investigated in a project funded by the AiF (FOSTA P1380/IGF 21162 BG). This study focuses on determining the interactions between heat control during WAAM process, resulting hardness, microstructure, and residual stresses, analyzed by X-ray diffraction. Welding experiments using geometrically similar AM specimens show that, with regard to the heat input, the energy per unit length in particular leads to significantly affected cooling times and microstructures and causes pronounced localized effects in terms of residual stresses in the upper weld beads. T2 - 46th MPA-Seminar CY - Stuttgart, Germany DA - 12.10.2021 KW - Wire Arc Additive Manufacturing KW - High-strength structural steels KW - Vickers hardness KW - Residual stresses PY - 2021 VL - 46 SP - 296 EP - 306 PB - MPA-Stuttgart AN - OPUS4-53571 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kannengießer, Thomas A1 - Rhode, Michael T1 - Fügetechnik in Wasserstofftechnologien - Forschungsbedarf für die Branche N2 - Die Studie gibt einen kurzen Überblick über die jetzige Bedeutung der Fügetechnik in Wasserstofftechnologien und über zukünftige Forschungsbedarfe für die Branche in den einzelnen Technologiefeldern Wasserstofferzeu-gung, -speicherung, -transport und -nutzung. Fügetechnologien haben dabei wesentliche Bedeutung für die er-folgreiche Umsetzung von technischen Komponenten der Wasserstofftechnologien. Die Schwerpunkte bzw. For-schungsbedarfe ergeben sich bspw. durch die Erstellung neuer Infrastruktur für Wasserstoffspeicherung und -transport sowie durch Umnutzung der bestehenden Erdgasinfrastruktur. Bei der Wasserstofferzeugung und -anwendung wird z.B. die Entwicklung effiziente Massenproduktionsmethoden von Elektrolyseuren und Brennstoff-zellen einen wichtigen Meilenstein bilden und laserbasierte Fügetechnologien sind hier zum Teil schon etabliert. Die additive Fertigung nimmt dabei eine Querschnittsposition ein und besitzt hohes Anwendungspotential für die Zukunft z.B. für die Fertigung von Komponenten in Gasturbinen. Aus den technischen Fragestellungen und For-schungsbedarfen ergeben sich zudem Herausforderungen für die notwendige Neu- und Weiterentwicklung von technischen Regelwerken und Normen und den Eingang in die Aus- und Weiterbildung von fügetechnischem Fachpersonal. T2 - DVS Congress 2021 CY - Essen, Germany DA - 14.09.2021 KW - Wasserstoff KW - Fügetechnik KW - Forschung KW - Technologie PY - 2021 AN - OPUS4-53321 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Joining Processes in Hydrogen Technologies - Current need and future R&D activites, a review N2 - This study gives an overview on the important field of joining processes for component fabrication in hydrogen technologies. For that reason, the current need and future research and developement activites are highlighted for the different technological field of hydrogen generation, storage, transport and use. In addition, the emerging field of additive manufacturing is included. Finally, some remarks are given for necessary changes in the standardization and its challenges. T2 - 46th Seminar - Additive Manufacturing, Hydrogen, Energy, Integrity CY - Online meeting DA - 12.10.2021 KW - Hydrogen KW - Joining process KW - Welding KW - Review KW - Research and Development PY - 2021 AN - OPUS4-53554 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scharf-Wildenhain, R. A1 - Hälsig, A. A1 - Wandtke, Karsten A1 - Schröpfer, Dirk A1 - Kromm, Arne A1 - Kannengießer, Thomas T1 - Einfluss der Wärmeführung auf die Eigenschaften und fertigungsbedingten Beanspruchungen additiv geschweißter hochfester Feinkornbaustähle N2 - Hochfeste Feinkornbaustähle verfügen über ein großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. Kommerzielle hochfeste Zusatzwerkstoffe für additives MSG-Schweißen (engl.: Wire Arc Additive Manufacturing, WAAM) sind bereits von den Schweißzusatzherstellern lieferbar. Derzeit ist jedoch eine breite industrielle Anwendung insbesondere für KMU aufgrund fehlender quantitativer Erkenntnisse und Richtlinien bezüglich schweißbedingter Beanspruchungen und Bauteilsicherheit während der Herstellung und des Betriebs stark limitiert. In einem gemeinsamen Forschungsprojekt (FOSTA-P1380/IGF21162BG) der BAM und der TU Chemnitz werden die mit Eigenspannungsausbildung und der Gefahr einer Kaltrissbildung verbundenen prozess- und werkstoffbedingten sowie konstruktiven Einflüsse untersucht. Im Fokus dieser Analysen steht die Bestimmung der Wechselwirkungen zwischen WAAM-Prozessparametern bzw. der Wärmeführung auf das Gefüge und die Eigenspannungen. Hierfür werden Referenzproben als offene Hohlquader mit definierten Abmessungen vollautomatisiert mit einem speziellen, hochfesten WAAM-Massivdraht (Streckgrenze >790 MPa) geschweißt. Die gezielte Einstellung der geometrischen Eigenschaften erfolgt durch Schweißparameter und Nahtaufbau bei ca. 4 kg/h mittlerer Abschmelzleistung. Die Wärmeführung wird innerhalb eines statistischen Versuchsplanes mittels Streckenenergie (200 kJ/m bis 650 kJ/m) und Zwischenlagentemperatur (100 °C bis 300 °C) so variiert, dass die t8/5-Abkühlzeiten dem empfohlenen Verarbeitungsbereich entsprechen (ca. 5 s bis 20 s). Ziel ist es bei konstanten geometrisch-konstruktiven Randbedingungen, den Einfluss der Wärmeführung auf Gefüge und resultierende Eigenspannungen zu analysieren. Für die Streckenenergie können neben den Gefügeeinflüssen aufgrund der resultierenden Abkühlzeit deutliche Effekte insbesondere auf die lokalen Eigenspannungen im Bauteil belegt werden. Das Schweißen mit zu hoher Wärmeeinbringung bzw. Abschmelzleistung kann zu ungünstigen Gefüge- und Bauteileigenschaften führen, gleichzeitig jedoch niedrigere Zugeigenspannungsniveaus bewirken. Solche komplexen Wechselwirkungen gilt es letztlich mit diesen Untersuchungen zu klären, um leicht anwendbare Verarbeitungsempfehlungen und Normvorgaben für ein wirtschaftliches, anforderungsgerechtes und risssicheres WAAM von hochfesten Stählen den Anwendern zur Verfügung zu stellen. T2 - DVS Congress 2021 CY - Online meeting DA - 14.09.2021 KW - MAG-Schweißen KW - Hochfester Stahl KW - Eigenspannungen KW - Additive Fertigung KW - Kaltrisssicherheit PY - 2021 SN - 978-3-96144-146-4 VL - 371 SP - 16 EP - 22 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-56669 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Becker, Amadeus A1 - Schröpfer, Dirk A1 - Kannengießer, Thomas T1 - Beanspruchungsgerechte Reparatur beim Bauteilschweißen hochfester Feinkornbaustähle N2 - Eine nachhaltige und ressourceneffiziente Fertigung und Errichtung von Windenergieanlagen, sowohl auf See als auch an Land, erfordert zunehmend den Einsatz moderner hochfester Feinkornbaustähle. Werden nach dem Schweißen dieser hochfesten Konstruktionen unzulässige Defekte detektiert, sind nach geltenden Verarbeitungsrichtlinien die defekten Bereiche durch lokales Ausfugen und anschließendes Schweißen zu reparieren. Fehlende Informationen zu adäquaten Reparaturkonzepten in den Regelwerken bedingen oftmals eine unzureichende Berücksichtigung dabei auftretender zusätzlicher Beanspruchungen durch die erhöhte Schrumpfbehinderung der Ausfugenuten. Zusätzlich haben die ausführenden Betriebe vielfach kaum Kenntnis über die Degradation angrenzender Gefüge durch thermische Ausfugeprozesse und erneutes Schweißen, die in diesem Zusammenhang besonders bei den hochfesten Stählen als kritisch anzusehen sind. Das aktuelle Forschungsvorhaben der BAM (FOSTA P1311/IGF-Nr.20162N) fokussiert hierfür systematisch bauteilrelevante Untersuchungen zu den schweißbedingten Beanspruchungen und Gefügeveränderungen bei der Reparatur von hochfesten Schweißverbindungen. Wesentlich sind hierbei der Einfluss der Schrumpfbehinderung, der Wärmeführung beim Schweißen und Ausfugen sowie der Reparaturzyklenanzahl und die metallurgischen Aspekte bei den hochfesten Güten S500MLO für zukünftige Offshore-Anwendungen und S960QL für aktuelle Mobilkrananwendungen. Aufbauend auf einigen Studien zur schweißbedingten Beanspruchung hochfester Stähle zeigt der vorliegende Beitrag die Identifikation geeigneter Probengeometrien und Schweißdetails mittels numerischer und experimenteller Analysen. Dadurch wird die Übertragbarkeit der vorgestellten Schweißexperimente und Ergebnisse hinsichtlich der resultierenden Schweißeigenspannungen auf reale Reparaturfälle im Bereich des hochfesten Stahlbaus sichergestellt. Es zeigt sich in Übereinstimmung mit früheren Ergebnissen eine signifikante Erhöhung der Beanspruchungen an den variierten schlitzförmigen Prüfnähten. Das Eigenspannungsniveau sowohl im Schweißgut als auch in der WEZ korreliert mit dem Einspanngrad. Mit dem Ziel beanspruchungs- und werkstoffgerechte Reparaturkonzepte zu erarbeiten, sind zum einen geringere Wärmeinbringungen, besonders durch niedrige Zwischenlagentemperaturen und Einspannbedingungen anzustreben, um hohe Beanspruchungen und kritische Gefügedegradationen im Reparaturbereich zu vermeiden. Dies wird durch systematische Untersuchungen zum Ausfugen und Schweißen sowie letztlich dem Transfer von Verarbeitungsempfehlungen für die Anwender und Richtlinien erreicht. T2 - DVS Congress 2021 CY - Online meeting DA - 14.09.2021 KW - MAG-Schweißen KW - Reparatur KW - Eigenspannungen KW - Hochfester Stahl KW - Thermisches Ausfugen KW - Windenergie KW - Gefügedegradation PY - 2021 SN - 978-3-96144-146-4 VL - 371 SP - 285 EP - 292 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-56666 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scharf-Wildenhain, R. A1 - Hälsig, A. A1 - Härtel, S. A1 - Wandtke, Karsten A1 - Schröpfer, Dirk A1 - Kromm, Arne A1 - Kannengießer, Thomas T1 - Einfluss der Wärmeführung auf die Eigenschaften und fertigungsbedingten Beanspruchungen additiv geschweißter hochfester Feinkornbaustähle N2 - Hochfeste Feinkornbaustähle verfügen über ein großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. Kommerzielle hochfeste Zusatzwerkstoffe für additives MSG-Schweißen (engl.: Wire Arc Additive Manufacturing, WAAM) sind bereits von den Schweißzusatzherstellern lieferbar. Derzeit ist jedoch eine breite industrielle Anwendung insbesondere für KMU aufgrund fehlender quantitativer Erkenntnisse und Richtlinien bezüglich schweißbedingter Beanspruchungen und Bauteilsicherheit während der Herstellung und des Betriebs stark limitiert. In einem gemeinsamen Forschungsprojekt (FOSTA-P1380/IGF21162BG) der BAM und der TU Chemnitz werden die mit Eigenspannungsausbildung und der Gefahr einer Kaltrissbildung verbundenen prozess- und werkstoffbedingten sowie konstruktiven Einflüsse untersucht. Im Fokus dieser Analysen steht die Bestimmung der Wechselwirkungen zwischen WAAM-Prozessparametern bzw. der Wärmeführung auf das Gefüge und die Eigenspannungen. Hierfür werden Referenzproben als offene Hohlquader mit definierten Abmessungen vollautomatisiert mit einem speziellen, hochfesten WAAM-Massivdraht (Streckgrenze >790 MPa) geschweißt. Die gezielte Einstellung der geometrischen Eigenschaften erfolgt durch Schweißparameter und Nahtaufbau bei ca. 4 kg/h mittlerer Abschmelzleistung. Die Wärmeführung wird innerhalb eines statistischen Versuchsplanes mittels Streckenenergie (200 kJ/m bis 650 kJ/m) und Zwischenlagentemperatur (100 °C bis 300 °C) so variiert, dass die t8/5-Abkühlzeiten dem empfohlenen Verarbeitungsbereich entsprechen (ca. 5 s bis 20 s). Ziel ist es bei konstanten geometrisch-konstruktiven Randbedingungen, den Einfluss der Wärmeführung auf Gefüge und resultierende Eigenspannungen zu analysieren. Darüber hinaus erfolgt die Bestimmung des Einflusses der t8/5-Abkühlzeit auf die mechanisch-technologischen Eigenschaften des speziellen, hochfesten WAAM-Massivdrahts mithilfe von Dilatometeranalysen. Für die Streckenenergie können neben den Gefügeeinflüssen aufgrund der resultierenden Abkühlzeit deutliche Effekte insbesondere auf die lokalen Eigenspannungen im Bauteil belegt werden. Das Schweißen mit zu hoher Wärmeeinbringung bzw. Abschmelzleistung kann zu ungünstigen Gefüge- und Bauteileigenschaften führen, gleichzeitig jedoch niedrigere Zugeigenspannungsniveaus bewirken. Die Dilatometeranalysen zeigen für den untersuchten WAAM-Schweißzusatzwerkstoff eine großes t8/5-Zeitfenster mit einer vergleichsweise geringen Abnahme der Zugfestigkeit mit zunehmender t8/5-Abkühlzeit. Solche komplexen Wechselwirkungen gilt es letztlich mit diesen Untersuchungen zu klären, um leicht anwendbare Verarbeitungsempfehlungen und Normvorgaben für ein wirtschaftliches, anforderungsgerechtes und risssicheres WAAM von hochfesten Stählen den Anwendern zur Verfügung zu stellen. T2 - 42. Assistentenseminar Fügetechnik CY - Brunswick, Germany DA - 06.10.2021 KW - MAG-Schweißen KW - Hochfester Stahl KW - Eigenspannungen KW - Additive Fertigung KW - Kaltrisssicherheit PY - 2022 SN - 978-3-96144-210-2 VL - 385 IS - 42 SP - 94 EP - 101 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-56642 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scharf-Wildenhain, R. T1 - Einfluss von Wärmeführung und Bauteildesign auf die Beanspruchungen additiv geschweißter hochfester Feinkornbaustähle N2 - Hochfeste Feinkornbaustähle verfügen über großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. Hochfeste Zusatzwerkstoffe für additives MSG-Schweißen (engl.: Wire Arc Additive Manufacturing, WAAM) sind bereits von den Schweißzusatzherstellern lieferbar. Eine breite industrielle Anwendung insbesondere für KMU ist aufgrund fehlender quantitativer Erkenntnisse und Richtlinien bezüglich schweißbedingter Beanspruchungen und Bauteilsicherheit während der Herstellung und des Betriebs derzeit stark limitiert. In einem gemeinsamen Forschungsprojekt (FOSTA-P1380/IGF21162BG) der BAM und der TU Chemnitz werden daher die mit Eigenspannungsausbildung und der Gefahr einer Kaltrissbildung verbundenen prozess- und werkstoffbedingten sowie konstruktiven Einflüsse beim WAAM hochfester Stähle untersucht. Der vorliegende Beitrag fokussiert die Analyse der Auswirkungen von Schweißwärmeführung und Design der WAAM-Bauteile auf die Abkühlbedingungen, Gefüge, mechanisch-technologischen Eigenschaften und Eigenspannungen. Hierfür werden geometrisch definierte Probenkörper (Hohlquader) vollautomatisiert mit einem speziellen, hochfesten WAAM-Massivdraht (Streckgrenze >790 MPa) geschweißt. Die Wärmeführung und Probenabmessungen werden innerhalb eines statistischen Versuchsplans variiert. Die Schweißwärmeführung wird dabei so eingestellt, dass die t8/5-Abkühlzeiten im empfohlenen Verarbeitungsbereich (ca. 5 s bis 20 s) sichergestellt sind. Hierzu ließen sich über zusätzliche thermo-physikalische Umformsimulationen mittels Dilatometer die komplexen Wärmezyklen abbilden und die resultierende Zugfestigkeit des Schweißgutes bestimmen. Das WAAM-Schweißen komplexer Geometrien mit variierenden Schweißwärmeführungen und geometrischen Verhältnissen bzw. Wanddicken bedingt neben den Auswirkungen auf die Abkühlbedingungen, Abkühlzeiten und Gefüge deutliche Einflüsse auf die konstruktiven Steifigkeitsverhältnisse beim Schweißen. Es zeigen sich anhand der Schweißexperimente signifikante Auswirkungen durch Probenskalierung und Wärmeeinbringung auf die resultierenden lokalen Eigenspannungen. Die Folge können ungünstige Bauteileigenschaften und risskritische Zugeigenspannungen sein. T2 - DVS Congress 2022 CY - Koblenz, Germany DA - 19.09.2022 KW - WAAM KW - Eigenspannungen KW - Additive Fertigung KW - Hochfester Stahl KW - Kaltrisssicherheit KW - Windenergie KW - Wärmeführung PY - 2022 AN - OPUS4-56718 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Influence of the WAAM process and design aspects on residual stresses in high-strength structural steels N2 - High-strength fine-grain structural steels have great potential for weight optimization of many modern engineering structures. Efficient manufacturing can be achieved here above all by Wire Arc Additive Manufacturing (WAAM). First commercial high-strength welding consumables for WAAM are already available. However, due to a lack of knowledge and guidelines for the industry regarding welding residual stresses and component safety in manufacturing and operation, their application is still severely limited. Residual stresses play a crucial role here, as the sensitive microstructure of high-strength steels carries a high risk of cold cracking. For this reason, process- and material-related influences, as well as the design aspects on residual stress formation and the risk of cold cracking, are being investigated in a recent project (FOSTA-P1380/IGF21162BG). This high strength of the WAAM welding consumables is adjusted via a martensitic phase transformation. The volume expansion associated with martensite formation has a significant influence on residual stress evolution. However, this has not yet been investigated in relation to the processing of high-strength steels by WAAM. The aim of this work is to establish a WAAM cold crack test and easy-to-apply processing recommendations that will allow economical, expedient, and crack-resistant fabrication of high-strength steels, especially for SME. This paper focuses on the analysis of the effects of welding heat control and design of WAAM components on cooling conditions, microstructure, mechanical-technological properties and residual stresses. For this purpose, geometrically defined specimens (hollow cuboids) are welded fully automatically with a special, high-strength WAAM solid wire (yield strength >790 MPa). The heat control and specimen dimensions are varied within a statistical experimental design. The weld heat control is adjusted in such a way that the t8/5 cooling times are ensured within the recommended processing range (approx. 5–20 s). For this purpose, additional thermo-physical forming simulations using a dilatometer allowed the complex heat cycles to be reproduced and the resulting ultimate tensile strength of the weld metal to be determined. The WAAM welding of complex geometries with varying welding heat control and geometric factors or wall thicknesses not only has an effect on the cooling conditions, cooling times and microstructure, but also has a significant influence on the structural restraint conditions during welding. Hence, the welding experiments show significant effects of specimen scaling and heat input on the welding residual stresses, which may be detrimental regarding component properties and crack-critical tensile residual stresses. These complex interactions are analyzed within this investigation T2 - 75th IIW Annual Assembly (Subcomission IIA) CY - Online meeting DA - 17.07.2022 KW - WAAM KW - Residual Stresses KW - High-strength Steels KW - Cold cracking safety KW - Wind energy KW - Heat control PY - 2022 AN - OPUS4-56715 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Engelking, Lorenz A1 - Schröpfer, Dirk A1 - Kannengießer, Thomas A1 - Eissel, A. A1 - Treutler, K. A1 - Wesling, V. T1 - Herstellung beanspruchungsgerechter Oberflächen durch Kombination innovativer additiver und abtragender Fertigungsschritte an hochbelasteten Komponenten N2 - Die additive Fertigung mittels Schweißverfahren bietet große ökonomische Vorteile für eine ressourceneffiziente Bauteilherstellung. Offene Fragen bezüglich Homogenität, Anisotropie der Schweißgefüge und den damit verbundenen Bauteileigenschaften stehen einer wirtschaftlichen Verarbeitung oftmals im Wege. Finale Bauteilgeometrie und Oberflächengüte erfordern meist komplementäre subtraktive Fertigungsschritte. Werkstoffe für hochbelastbare Komponenten sind oftmals schwer spanbar. In einem Vorhaben der BAM und des ISAF wurde untersucht, wie die Modifikation der AM-Schweißzusätze und das ultraschallunterstützte Fräsen (US) die Zerspanungssituation verbessern. Der vorliegende Artikel stellt wesentliche Zusammenhänge zwischen Legierung, Gefüge und Zerspanung zweier schwer spanbarer Hochleistungslegierungen (FeNi und CoCr) dar. Großes Potenzial zeigte neben dem US die Modifikation mit Zr und Hf bei Zulegierung in das Schweißgut mittels Beschichtung von Massivdrähten bzw. Herstellung von Fülldrähten. KW - Legierungsmodifikation KW - Ultraschallunterstütztes Fräsen KW - Additive Fertigung KW - Oberflächenintegrität KW - Metallschutzgasschweißen PY - 2024 VL - 76 IS - 1-2 SP - 8 EP - 13 PB - DVS-Media GmbH CY - Düsseldorf AN - OPUS4-59463 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Liepold, Philipp ED - Kromm, Arne ED - Kannengießer, Thomas T1 - Anwendung von Convolutional Neural Networks (CNNs) bei der Erkennung von Rissen im Modifizierten Varestraint-Transvarestraint-Heißrisstest (MVT-Test) N2 - Der Modifizierte Varestraint-Transvarestraint-Test wird an der Bundesanstalt für Materialforschung und -prüfung als Variante des Varestraint-Tests verwendet. Die Auswertung dieser Tests findet klassisch durch Abmessungen der entstandenen Risse unter dem Lichtmikroskop statt. Eine solche Auswertung ist aufwendig und fehleranfällig. Convolutional Neural Networks können trainiert werden, um die Risse auf digitalen Bildern zu segmentieren, wodurch der menschliche Fehler in der Auswertung eliminiert werden kann. Die Ergebnisse können durch Overlay mit den Originalbildern verglichen werden. T2 - DVS-Congress, Große Schweißtechnische Tagung CY - Essen, Germany DA - 11.09.2023 KW - CNN KW - MVT KW - KI PY - 2023 SN - 978-3-96144-231-7 SN - 978-3-96144-230-0 VL - 2023 SP - 153 PB - Print Media Group GmbH & Co. KG CY - Hamm AN - OPUS4-59336 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröpfer, Dirk T1 - Residual stress formation in DED-arc manufactured high strength steel components N2 - Additive manufacturing (AM) processes enable the efficient production of advanced constructions. New developments in topology optimization are leading to weight-optimized designs of increasing complexity. Direct energy deposition processes (DED) such as wire and arc-based additive manufacturing are an important method of additive manufacturing. The wire filler metals enable a wide range of materials, while the arc process provides a high deposition rate compared to laser and powder-based processes. Combined with the use of high-strength steels, the thickness of walls or components can be significantly reduced in the context of lightweight construction, which results in significant savings in energy, costs, time and resources. Suitable high-strength steel filler metals are commercially available for DED-arc AM processes. However, guidelines and quantitative knowledge about welding stresses and cold cracking issues during component production and service are lacking. This limits the industrial application considerably. In a joint project of BAM and Chemnitz University of Technology, the main influences and complex interactions of material, production process, design and processing steps on the residual stress level are investigated. The aim is to develop processing recommendations and a cold cracking test for economical processing and stress-related design of high-strength steels with DED-arc. This study focuses on residual stress analysis by neutron diffraction (ND) and X-ray diffraction (XRD) on defined test specimens. The ND analysis were performed at the Paul Scherrer Institute- Villigen, Switzerland (PSI) and the XRD analysis at BAM. The study shows a quantitative and qualitative comparison of the residual stress magnitudes and distribution between the component bulk (ND) and surface (XRD) analyses. The ND analysis reveals that in DED-arc AM walls the residual stresses dominate in the direction of welding and are negligibly small in each case transverse to the direction of welding. The topology of the analyzed residual stresses shows almost identical residual stress maps compared to XRD. In addition, the residual stresses are significantly influenced by the solid phase transformation of the material due to low cooling times and less post heat treatment cycles of following AM layers in the area of the top layer. T2 - IIW Intermediate Meeting 2023 CII and CIX CY - Munich, Germany DA - 06.03.2023 KW - WAAM KW - Residual Stresses KW - High-strength Steels KW - Microstructure KW - Cold cracking safety KW - Wind energy PY - 2023 AN - OPUS4-59261 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Einfluss trennender Fertigungsschritte auf die Eigenspannungen in Bauteilen aus hochfestem Stahl N2 - Der Vortrag gibt einen Überblick über den Einfluss Trennender Fertigungsschritte auf die Eigenspannungen in einer Schweißverbindung und an additiv gefertigten Bauteilen aus hochfestem Stahl. Es wird dargestellt, wie die Spanende Bearbeitung in Wechselwirkung mit der lokalen Mikrostruktur die Eigenspannungen beeinflusst. T2 - Bachelor-, Master-, Doktoranden-Kolloquium OvGU Magdeburg CY - Magdeburg, Germany DA - 17.01.2024 KW - Hochfester Stahl KW - Additive Fertigung KW - Reparaturschweißen KW - Eigenspannungen PY - 2024 AN - OPUS4-59413 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Nietzke, Jonathan A1 - Mente, Tobias A1 - Kannengießer, Thomas T1 - Diffusionsmessungen in UP-Mehrlagenschweißgut als effektives Tool gegen verzögerte Kaltrissbildung in Dickblechschweißungen N2 - Offshore-Windenergieanlagen bilden einen zentralen Bestandteil der zukünftigen Energieerzeugung. Hierzu notwendige Gründungs- und Turmstrukturen werden vorrangig aus UP-geschweißten Blechen aus hochfesten niedriglegierten Stählen mit Dicken bis zu 200 mm hergestellt. Die großen Blechdicken begünstigen hohe Schweißeigenspannungen und lange Diffusionswege für z. B. über den Schweißprozess eingebrachten Wasserstoff. Damit steigt das Risiko für eine wasserstoffunterstützte Kaltrissbildung (WKB) an. Zum sichereren Ausschluss von WKB in den geschweißten Komponenten wird in Abhängigkeit der Nahtgröße, Wärmeeinbringung und Stahlsorte eine Mindestwartezeit (MWZ) von bis zu 48 h empfohlen, bevor die zerstörungsfreie Prüfung durchgeführt wird. Es ist allerdings offen, ob die empfohlene MWZ zu konservativ ist. Einflüsse sind hier bspw. die schwierige Bewertung des Wasserstoffdiffusionsverhaltens im heterogenen UP-Mehrlagen-Schweißgut (SG) im Vergleich zum Grundwerkstoff (GW). Zudem sind nur sehr begrenzt H-Diffusionskoeffizienten für UP-Mehrlagen-SG als Grundlage zur Abschätzung des Zeitintervalls einer möglichen verzögerten Kaltrissbildung (somit MWZ) oder auch für Nachwärmprozeduren zur Wasserstoffreduktion (keine MWZ) verfügbar. Verlässliche H-Diffusionskoeffizienten sind daher ein adäquates Tool zur Bewertung des Risikos einer verzögerten WKB. Dieser Beitrag beschreibt Untersuchungen zur Charakterisierung der Wasserstoffdiffusionsverhalten in UP-Mehrlagen-SG eines 60 mm dicken Bleches einer Offshore-Stahlgüte. Dazu wurden Proben unterschiedlicher Dicke aus dem reinen Schweißgut extrahiert und über elektrochemische Permeation und Trägergasheißextraktion im Temperaturbereich bis 400 °C sehr interessante Ergebnisse zu den korrespondierenden Diffusionskoeffizienten erarbeitet. T2 - DVS Congress 2021 CY - Online meeting DA - 14.09.2021 KW - UP-Schweißen KW - Wasserstoff KW - Kaltriss KW - Permeation KW - Diffusion PY - 2021 SN - 978-3-96144-146-4 VL - 371 SP - 448 EP - 459 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-53369 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Joining processes for components in hydrogen technologies: Current need and future importance N2 - This presentation gives an overview on the importance of joining processes for component fabrication in hydrogen technologies. For that reason, the current need and future research and developement activites are highlighted for the three technological fields: hydrogen storage, transport and use (in terms of the emerging field of additive manufacturing). Finally, some remarks are given for necessary changes in the standardization. T2 - IIW Intermediate Meeting, Comm. II-A "Welding Metallurgy" CY - Online meeting DA - 17.03.2022 KW - Hydrogen KW - Welding KW - Research KW - Review KW - Additive manufacturing PY - 2022 AN - OPUS4-54488 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kromm, Arne T1 - Residual stresses and hydrogen assisted cracking in thick walled submerged arc weld joints for offshore applications N2 - Offshore wind turbines continuously increase in size and weight and demand adequate offshore foundations concepts like monopiles, tripods or jackets. These components are typically submerged arc welded (SAW) high-strength thick steel plates like the S420ML. During welding, the occurrence of delayed hydrogen assisted cracking (HAC) must be anticipated. HAC is a critical combination of the local hydrogen concentration within a susceptible microstructure under certain mechanical load, i.e., the occurring (welding) residual stresses. The welding sequence of the thick-walled plates complicate the residual stress distribution due to the necessary repeated thermal cycling, i.e., welding seam / layer deposition to fill the joint. For that purpose, SAW with two-wire-technique was used to weld a specially designed and prototype-like mock-up of a real component with a thickness of 50 mm, filled with 22 passes and a seam length of 1,000 mm. Additional welded stiffeners simulated the effect of a high restraint, to stimulate critical HAC conditions. The residual stresses were determined by a robot XRD goniometer. A least square regression analysis of the sin²ψ-law by using multiple ψ- and φ-tilts was applied. Tensile residual stresses up to the yield limit are found both in the weld metal and in the heat-affected zone. Numerical modelling allowed the qualitative estimation of the hydrogen diffusion in the weld, enabling the determination of critical conditions for the formation of HAC. In a future step, a structural simulation will allow the assessment of the welding residual stresses and the comparison to the XRD-values. T2 - International Conference on Residual Stresses ICRS-11 CY - Nancy, France DA - 27.03.2022 KW - Welding KW - X-ray diffraction KW - Hydrogen KW - Cracking KW - Offshore steel PY - 2022 AN - OPUS4-54576 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Consideration of manufacturing-related stresses and cold crack avoidance in high-strength steels WAAM components N2 - High-strength steels offer great potential in weight-optimised modern steel structures. Additive manufacturing processes, such as Wire Arc Additive Manufacturing (WAAM), enable near-net-shape manufacturing of complex structures and more efficient manufacturing, offering significant savings in costs, time, and resources. Suitable filler materials for WAAM are already commercially available. However, the lack of knowledge or technical guidelines regarding welding residual stresses during manufacturing and operation in connection with cold cracking risk limit their industrial application significantly. In a project of BAM and TU Chemnitz, the influences and complex interactions of material, manufacturing process, design and processing steps on residual stress evolution are investigated. By developing process recommendations and a special cold cracking test, economic manufacturing, and stress-appropriate design of high-strength steel WAAM components are main objectives. The present study focuses on determining the influence of heat control (interpass temperature, heat input, cooling time) and the design aspects of the components on the hardness and residual stresses, which are analysed by X-ray diffraction. Defined reference specimens, i.e., hollow cuboids, are automatically welded with a special WAAM solid wire. The influences of wall length, wall thickness and wall height on the residual stresses are analysed. Geometric properties can be selectively adjusted by wire feed and welding speed but cannot be varied arbitrarily. This was addressed by adapted build-up strategies. The results indicate a significant influence of the heat control and the wall height on the residual stresses. The interpass temperature, wall thickness and wall length are not significant. These analyses allow recommendations for standards and manufacturing guidelines, enabling a safe and economic manufacturing of high-strength steel components. T2 - European Steel Technology and Application Days CY - Düsseldorf, Germany DA - 14.06.2023 KW - DED-arc KW - Additive manufacturing KW - Heat control KW - High-strength filler metals KW - Residual stress PY - 2023 AN - OPUS4-57691 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Einfluss trennender Fertigungsschritte auf die Eigenspannungen in additiv gefertigten Bauteilen aus hochfestem Stahl N2 - Additive Fertigungsverfahren wie das Wire Arc Additive Manufacturing (WAAM) ermöglichen die effiziente Fertigung von gewichtsoptimierten endkonturnahen Strukturen in modernen Stahlkonstruktionen. Ihre Effizienz kann weiter durch die Verwendung von hochfesten Stählen gesteigert werden. Dies erlaubt eine signifikante Einsparung von Kosten, Zeit und Ressourcen. Entsprechende Schweißzusatzwerkstoffe für Lichtbogenschweißverfahren sind kommerziell verfügbar. Fehlende Richtlinien und fehlende quantitative Kenntnisse über die schweißtechnische Beanspruchung während der Fertigung und im Betrieb limitieren den industriellen Einsatz stark. Daher werden in einem aktuellen Vorhaben (IGF-Nr. 21162 BG) der BAM und TU Chemnitz die wesentlichen Einflüsse und komplexen Interaktionen durch Werkstoff, Fertigungsprozess, Konstruktion und trennende Fertigungsschritte auf den Beanspruchungszustand untersucht. Der vorliegende Beitrag fokussiert hierfür die Auswirkungen trennender Fertigungsschritte auf Verzug und Eigenspannungen definierter WAAM-Prüfkörper. Die Eigenspannungsanalyse erfolgt mittels Röntgenbeugung. Die große Anzahl an Ergebnissen von zuvor untersuchten Referenzproben, die mit einem speziellen WAAM-Massivdraht (Streckgrenze >820 MPa) bei unterschiedlicher Wärmeführung und Geometrie vollautomatisiert geschweißt wurden, lässt eine Korrelation der Messdaten zu. Hierzu erfolgt die Analyse des Ausgangszustandes und abschließend des Zustandes nach trennender Bearbeitung, welche begleitend mittels digitaler Bildkorrelation hinsichtlich des Verzuges untersucht wurden. So ist zu beobachten, dass die Geometrie deutlichen Einfluss auf Relaxation und Umlagerung der Eigenspannungen hat und damit die Risssicherheit positiv beeinflussen kann. T2 - Bachelor-, Master-, Doktoranden-Kolloquium OvGU Magdeburg CY - Magdeburg, Germany DA - 31.05.2023 KW - Additive Fertigung KW - Hochfester Stahl KW - Eigenspannungen PY - 2023 AN - OPUS4-57689 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Neutronen- und Röntgendiffraktion zur Einflussanalyse des Bauteil-Designs auf die Eigenspannungen bei der additiven Fertigung mit hochfestem Stahl N2 - Vorstellung und Gegenüberstellung von Eigenspannungsanalysen mittels Röntgen- und Neutronenbeugung an einer additiven Prüfgeometrie aus hochfestem Stahl. Einflussanalyse des Designs (Länge, Höhe, Wandstärke) von additiv gefertigten Bauteilen aus hochfestem Stahl auf die Eigenspannungen. T2 - Bachelor-, Master-, Doktoranden-Kolloquium OvGU Magdeburg CY - Magdeburg, Germany DA - 25.01.2023 KW - Additive Fertigung KW - Hochfester Stahl KW - Eigenspannungen PY - 2023 AN - OPUS4-57688 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Neumann, Martin T1 - Friction coefficients for wood-wood and wood-steel interfaces in impact limiters for transport casks N2 - Wood is widely used in impact limiters of transport casks for radioactive material. Encapsulated by an outer and inner steel structure, spruce wood is often applied in layers of alternating direction. The friction at the interfaces between these layers is of crucial importance for the impact and energy absorption e.g., at an accidental impact of a cask against a hard target. In order to get detailed information for corresponding numerical calculations, in this study the friction coefficient for the combinations wood-wood and wood-steel was measured in the temperature range between -40°C and 90°C according to the relevant stress conditions for such casks. Results show decreasing friction with increasing temperature, ranging from 0.43 at -40°C to 0.22 for 90°C for wood-steel combinations and from 0.3 at -40°C to 0.24 at 90°C to for a wood-wood combination. T2 - 20th International Symposium on the Packaging and Transportation of Radioactive Materials (PATRAM 22) CY - Juan-les-Pins, France DA - 11.06.2023 KW - Wood KW - Friction KW - Transport cask PY - 2023 AN - OPUS4-57702 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scharf-Wildenhain, R. A1 - Hälsig, A. A1 - Hensel, J. A1 - Wandtke, Karsten A1 - Schröpfer, Dirk A1 - Kannengießer, Thomas T1 - Korrelation von Wärmeführung, Nahtgeometrie, Bauteildesign und Eigenspannungen bei DED-Arc mit hochfesten Zusatzwerkstoffen N2 - Hochfeste Feinkornbaustähle verfügen über großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. Hochfeste Zusatzwerkstoffe für formgebendes MSG-Schweißen (engl.: Wire Arc Additive Manufacturing, WAAM) sind bereits von den Schweißzusatzherstellern lieferbar. Eine breite industrielle Anwendung insbesondere für KMU ist aufgrund fehlender quantitativer Erkenntnisse und Richtlinien bezüglich schweißbedingter Beanspruchungen und Bauteilsicherheit während der Herstellung und des Betriebs derzeit stark limitiert. In einem gemeinsamen Forschungsprojekt (FOSTA-P1380/IGF21162BG) der BAM und der TU Chemnitz werden daher die mit Eigenspannungsausbildung und der Gefahr einer Kaltrissbildung verbundenen prozess- und werkstoffbedingten sowie konstruktiven Einflüsse beim WAAM hochfester Stähle untersucht. Der vorliegende Beitrag fokussiert die Analyse der Auswirkungen von Schweißwärmeführung und Design der WAAM-Bauteile auf Nahtgeometrie, Materialausnutzung und Eigenspannungen. Hierfür werden geometrisch definierte Probenkörper (Hohlquader) vollautomatisiert mit einem speziellen, hochfesten WAAM-Massivdraht (Streckgrenze >790 MPa) geschweißt. Die Wärmeführung wird innerhalb eines statistischen Versuchsplans so variiert, dass die Dt8/5-Abkühlzeiten im empfohlenen Verarbeitungsbereich (ca. 5 s bis 20 s) liegen. Das WAAM-Schweißen komplexer Geometrien mit variierenden Schweißwärmeführungen und geometrischen Verhältnissen bzw. Wanddicken bedingt neben den Auswirkungen auf die Abkühlbedingungen, Abkühlzeiten und Gefüge deutliche Einflüsse auf die konstruktiven Steifigkeitsverhältnisse beim Schweißen. Es zeigen sich anhand der Schweißexperimente signifikante Auswirkungen durch Probenskalierung und Wärmeeinbringung auf die resultierenden lokalen Eigenspannungen. Die Folge können ungünstige Bauteileigenschaften und risskritische Zugeigenspannungen sein. T2 - 43. Assistentenseminar Füge- und Schweißtechnik 2022 CY - Chemnitz, Germany DA - 27.09.2022 KW - Additive Fertigung KW - Hochfester Stahl KW - Eigenspannungen PY - 2023 VL - 386 SP - 1 EP - 7 PB - DVS Media CY - Düsseldorf AN - OPUS4-59232 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Einfluss trennender Fertigungsschritte auf die Eigenspannungen in additiv gefertigten Bauteilen aus hochfestem Stahl N2 - Additive Fertigungsverfahren wie das Wire Arc Additive Manufacturing (WAAM) ermöglichen die effiziente Fertigung von gewichtsoptimierten endkonturnahen Strukturen in modernen Stahlkonstruktionen. Ihre Effizienz kann weiter durch die Verwendung von hochfesten Stählen gesteigert werden. Dies erlaubt eine signifikante Einsparung von Kosten, Zeit und Ressourcen. Entsprechende Schweißzusatzwerkstoffe für Lichtbogenschweißverfahren sind kommerziell verfügbar. Fehlende Richtlinien und fehlende quantitative Kenntnisse über die schweißtechnische Beanspruchung während der Fertigung und im Betrieb limitieren den industriellen Einsatz stark. Daher werden in einem aktuellen Vorhaben (IGF-Nr. 21162 BG) der BAM und TU Chemnitz die wesentlichen Einflüsse und komplexen Interaktionen durch Werkstoff, Fertigungsprozess, Konstruktion und trennende Fertigungsschritte auf den Beanspruchungszustand untersucht. Der vorliegende Beitrag fokussiert hierfür die Auswirkungen trennender Fertigungsschritte auf Verzug und Eigenspannungen definierter WAAM-Prüfkörper. Die Eigenspannungsanalyse erfolgt mittels Röntgenbeugung. Die große Anzahl an Ergebnissen von zuvor untersuchten Referenzproben, die mit einem speziellen WAAM-Massivdraht (Streckgrenze >820 MPa) bei unterschiedlicher Wärmeführung und Geometrie vollautomatisiert geschweißt wurden, lässt eine Korrelation der Messdaten zu. Hierzu erfolgt die Analyse des Ausgangszustandes und abschließend des Zustandes nach trennender Bearbeitung, welche begleitend mittels digitaler Bildkorrelation hinsichtlich des Verzuges untersucht wurden. So ist zu beobachten, dass die Geometrie deutlichen Einfluss auf Relaxation und Umlagerung der Eigenspannungen hat und damit die Risssicherheit positiv beeinflussen kann. T2 - 23. Werkstofftechnisches Kolloquium CY - Chemnitz, Germany DA - 29.03.2023 KW - Additive Fertigung KW - Hochfester Stahl KW - Eigenspannungen KW - Residual stress PY - 2023 AN - OPUS4-59231 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Influence of machining on residual stresses in additive manufactured high-strength steel components N2 - Additive manufacturing processes such as direct energy deposition-arc (DED-Arc) welding or Wire Arc Additive Manufacturing (WAAM) enable the efficient production of weight-optimized near-net-shape components in modern steel constructions. Further increased efficiency can be achieved by using high-strength steels. This enables considerable savings in terms of costs, time and resources. Commercial filler metals are available for these arc welding processes, but a lack of guidelines and quantitative knowledge of the welding stresses during production and operation limit their industrial application. This study focuses on the effect of machining steps on the residual stresses and distortion of WAAM specimens. These specimens were welded fully automatically with a special WAAM solid wire (yield strength >820 MPa) with different geometric designs. The initial state and the state after cutting of the residual stresses were analyzed by means of X-ray diffraction on the surface and compared with data from three-dimens T2 - IIW Annual Assembly 2024 CY - Rhodos, Greece DA - 07.07.2024 KW - High strength steels KW - Additive manufacturing KW - Residual stress PY - 2024 AN - OPUS4-61951 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kromm, Arne A1 - Thomas, Maximilian A1 - Liepold, Philipp A1 - Kannengießer, Thomas A1 - Schröpfer, Dirk T1 - Einfluss der Schweiß- und Prüfparameter bei der Heißrissbewertung hochfester Schweißzusatzwerkstoffe N2 - Die Heißrissneigung beim Schweißen kann mittels einer ganzen Reihe von Prüfverfahren ermittelt werden. Eine etablierte Methode ist die sogenannte Varestraint-Prüfung, welche auch an der Bundesanstalt für Materialforschung und -prüfung (BAM) als modifizierter Varestraint/Transvarestraint-Test (MVT) zum Einsatz kommt. Die Ergebnisse von Varestraint-Prüfungen hängen jedoch stets in unter-schiedlichem Maße von der individuellen Prüfmaschinenauslegung und den verwendeten Prüfparametern ab. Dies kann zu einer uneinheitlichen Bewertung des Rissverhaltens führen, wenn die Risslänge konventionell als Kriterium für die Rissneigung herangezogen wird. Scheinbare Abhängigkeiten von Prozessparametern erschweren dann die Interpretation der Ergebnisse. Eine neuartige Bewertungsmethodik entkoppelt den Maschineneinfluss vom Materialverhalten und verwendet die Dehnrate als Risskriterium. T2 - 5. Symposium Materialtechnik CY - Clausthal-Zellerfeld, Germany DA - 23.02.2023 KW - Heißrisse KW - Varestraint-Test PY - 2023 SN - 978-3-8440-9105-2 SN - 2364-0804 VL - 12 SP - 357 EP - 365 PB - Shaker CY - Düren AN - OPUS4-57993 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kaiser, Sebastian T1 - Repair welding of pressurized in-service hydrogen pipelines: A review on current challenges and strategies N2 - As energy carrier of the future, green hydrogen can make a decisive contribution to a sustainable energy supply. In Europe concrete plans for a hydrogen pipeline grid already exist, as the so called “European Hydrogen backbone”. As building a completely new pipeline grid is economically not justifiable, a dual-way strategy of repurposing natural gas (NG) pipelines and newly built pipelines is intended. Long distance pipeline grids require regular maintenance and repairs. In that conection, for natural gas (NG) pipelines in-service welding is state of the art. Concepts such as hot-tapping (drilling into pressurized pipelines) and “stoppling” (sealing off pipeline sections after installing bypasses or pressure relieves) allow the repair of damaged pipeline sections or the installation of new branches without shutting the pipeline down. The EIGA 121/14 guideline already pointed out in 2014 that “a hydrogen hot-tap shall not be considered a routine procedure”. This shows that the determination of the transferability of these repair concepts to hydrogen pipelines is of utmost importance. Due to the degrading effects of hydrogen on mechanical proper-ties, commonly referred to as “hydrogen embrittlement” it is necessary to understand and investigate the occurring effects. In the special case of repair welding on in-service hydrogen pipelines an increased hydro-gen uptake due to a large heat input and microstructural changes in the material needs to be considered. For this reason, this paper gives an overview on existing weld repair concepts and its risks and limitations in terms of hydrogen absorption and possible embrittlement effects when transferred to hydrogen pipelines. The complexity lies in a large variety of materials (low alloyed steels), pipeline diameters and corresponding welded joints. The material compatibility of materials in used (repurposed NG-pipelines) and new condition must be investigated. Particularly for repurposed/used pipelines the effect of a pre-matured/corroded inner surface and sometimes insufficient documentation of the material “history” needs to be considered. An overview on ongoing and completed R&D-projects with respect to repair concepts for hydrogen pipelines and hydrogen effects on pipeline materials is given. T2 - 77th IIW Annual Assembly and International Conference, Meeting of Commission XI "Pressure Vessels and Piping" CY - Ixia, Rhodes, Greece DA - 07.07.2024 KW - Hydrogen KW - Repair welding KW - Pipelines KW - Study PY - 2024 AN - OPUS4-60673 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Reichel, Levin T1 - Effiziente Reparaturkonzepte mittels geregelter MSG Hochleistungsprozesse bei der Fertigung hochfester Dickblechverbindungen für Offshore Windenergieanlagen P1629 N2 - Der Bau von Gründungs- und Turmstrukturen für Windkraftanlagen erfordert den Einsatz moderner, nachhaltiger und ressourcenschonender hochfester Feinkornbaustähle. Durch den Schweißprozess verursachte Schweißnahtfehler sind nicht akzeptabel. Um diese zu beheben, ist das lokale thermische Fugenhobeln mit anschließendem Reparaturschweißen ein gängiges und wirtschaftliches Verfahren. Die hohe Schrumpfbehinderung um die ausgefugte Nut durch das umgebende Gefüge kann zu Rissbildung führen, wenn sich konstruktiv bedingte Spannungen und Eigenspannungen aus der Reparaturschweißung überlagern. Diese Gefahr wird durch die Verschlechterung der Mikrostruktur und der mechanischen Eigenschaften hochfester Stähle während des Schweißreparaturprozesses noch verstärkt. T2 - Bachelor-, Master-, Doktoranden-Kolloquium CY - Magdeburg, Germany DA - 16.05.2024 KW - Reparaturschweißen KW - Thermisches Ausfugen KW - Offshore KW - Sprühlichtbogen PY - 2024 AN - OPUS4-60050 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Fügetechnik in Wasserstofftechnologien Ein aktueller Überblick N2 - Der Vortrag gibt einen kurzen Überblick über die Bedeutung der Fügetechnik in Wasserstofftechnologien und über zukünftige Herausforderungen. Fügetechnologien, insbesondere die Schweißtechnik, haben dabei wesentliche Bedeutung für die Umsetzung von technischen Komponenten der Wasserstofftechnologien. Forschungsschwerpunkte ergeben sich insbesondere für die Erzeugung und den Transport des Wasserstoffs. T2 - Vortragsreihe des DVS Bezirksverbandes Mannheim-Ludwigshafen CY - Online meeting DA - 27.04.2023 KW - Wasserstoff KW - Schweißen KW - Studie PY - 2023 AN - OPUS4-57411 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Welding (and joining) technologies for the hydrogen economy - a short overview N2 - This study gives an overview on the important field of joining processes for component fabrication in hydrogen technologies. The current main issues and future perspectives are highlighted for the different technological field of hydrogen generation, storage, transport and use. In addition, the emerging field of additive manufacturing is included. Some remarks are given for standardization and regulations. T2 - Meeting of the European Welding Association (EWA), Executive Committee (EC) 1 CY - Frankfurt am Main, Germany DA - 22.03.2023 KW - Hydrogen KW - Welding KW - Research KW - Study PY - 2023 AN - OPUS4-57222 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Neumann, Martin A1 - Gleim, Tobias A1 - Gradt, Thomas A1 - Wille, Frank T1 - Friction coefficients for wood-wood and wood-steel interfaces in impact limiters for transport casks N2 - Wood is widely used in impact limiters of transport casks for radioactive material. Encapsulated by an outer and inner steel structure, spruce wood is often applied in layers of alternating direction. The friction at the interfaces between these layers is of crucial importance for the impact and energy absorption e.g., at an accidental impact of a cask against a hard target. In order to get detailed information for corresponding numerical calculations, in this study the friction coefficient for the combinations wood-wood and wood-steel was measured in the temperature range between -40°C and 90°C according to the relevant stress conditions for such casks. Results show decreasing friction with increasing temperature, ranging from 0.43 at -40°C to 0.22 for 90°C for wood-steel combinations and from 0.3 at -40°C to 0.24 at 90°C to for a wood-wood combination. T2 - 20th International Symposium on the Packaging and Transportation of Radioactive Materials CY - Juan-les-Pins, France DA - 11.06.2023 KW - Wood KW - Friction KW - Transport cask PY - 2023 SP - 1 EP - 11 AN - OPUS4-57334 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Bewertung und Vermeidung von schweißverarbeitungsbedingten Rissen in hochfesten Baustählen N2 - Die vorliegende Präsentation fasst die Ergebnisse von drei laufenden bzw. beendeten AiF/IGF-Projekten zusammen, die über die Forschungsvereinigung Stahlanwendung FOSTA e.V. an der BAM bearbeitet wurden zum Thema: Bewertung und Vermeidung von schweißverarbeitungsbedingten Rissen in hochfesten Baustählen. T2 - FOSTA Tagung: Hochfester Stahl im Stahl und Anlagenbau CY - Essen, Germany DA - 16.05.2023 KW - Studie KW - Schweißen KW - Hochfester Stahl KW - Riss KW - Forschung PY - 2023 AN - OPUS4-57517 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kromm, Arne T1 - Eigenspannungen in mittels DED-Arc gefertigten Bauteilen aus hochfestem Stahl N2 - Der Vortrag gibt einen Überblick über die mittels XRD und Neutronenbeugung ermittelten Eigenspannungen in additiv gefertigten Bauteilen. Zusätzlich wird der Einfluss der Prozessparameter auf die Härte betrachtet. T2 - Frühjahrssitzung des Fachausschusses 13 Eigenspannungen der AWT CY - Berlin, Germany DA - 28.03.2023 KW - Eigenspannungen KW - DED-arc KW - Hochfester Stahl KW - Neutronenbeugung PY - 2023 AN - OPUS4-57289 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kromm, Arne T1 - Hot Cracking Behavior of LTT Alloys under Variable Conditions in the Varestraint Test N2 - The use of Low Transformation Temperature (LTT) filler materials is an innovative way to reduce welding residual stresses. The generation of compressive residual stresses in the weld and heat-affected zone can lead to an improvement of the fatigue life of high-strength welds. However, high-alloy filler metals can be prone to solidification cracking. Two important LTT alloys were evaluated under variable welding and loading parameters using the Modified Varestraint/Transvarestraint (MVT) test. Initially conflicting results were interpreted using a newly developed image-based crack detection routine [1]. Based on the melt pool dimensions, the shape of the isotherms is reconstructed, and the theoretical crack growth along numerically determined crystallization paths is considered in relation to the cracks observed. Decreasing welding speeds with simultaneously higher heat input promote crack formation with increasing strain rate. T2 - International Joint Conference EMPOrIA 2023 CY - Aachen, Germany DA - 16.05.2023 KW - LTT KW - Solidification cracking KW - Varestraint test PY - 2023 AN - OPUS4-57546 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Czeskleba, Denis T1 - Experimental determination of hydrogen diffusion in high-strength submerged arc welded joints by electrochemical permeation N2 - High-strength structural steels are increasingly used in modern steel construction for economic and design reasons, e.g., in building, plant or mobile crane construction. By using steels with higher yield strengths (≥690 MPa), significant weight reductions and lower processing costs can be achieved by reducing the wall thickness. For example, substituting S235J2 with S960QL can reduce weight by up to 78%. Current efforts in lightweight design result from the goal of reducing greenhouse gas emissions by up to 65% by 2030 compared to 1990. These demands mean a significant reduction in process emissions in industry by increasing the efficiency of energy and raw materials. Submerged arc welding (SAW) offers high deposition rates and the welding of sheet thicknesses of up to 200 mm. Due to their special microstructure to achieve strength, high strength steels have reduced ductility and are susceptible to hydrogen-assisted cold cracking (HACC), which can also form with delay. In addition, large plate thicknesses lead to high residual welding stresses and long diffusion paths for hydrogen introduced via the welding process, for example. Furthermore, H-diffusion coefficients for submerged arc multi-layer weld metal are very limited as a basis for estimating the time interval of a possible delayed cold cracking (thus HACC) or for post-heating procedures for hydrogen reduction (no HACC). Reliable H-diffusion coefficients are therefore an adequate tool for assessing the risk of delayed HACC. This study characterizes the hydrogen diffusion behavior in submerged arc multi-pass weld metal, heat-affected zone and base metal of a two different S690 steels (TM and QT condition). Samples were extracted from the weld metal, heat-affected zone and base material to investigate the microstructure-specific influence on the diffusion of hydrogen. Using electrochemical permeation at room temperature and carrier gas hot extraction in the temperature range up to 400 °C, the corresponding diffusion coefficients were determined. From the experimental data, hydrogen diffusion coefficients and absorbed hydrogen concentrations had been calculated. In contrast e.g. to GMA welds, the hydrogen diffusion coefficients did not exhibit significant differences in the two base materials (TM and QT) or the heat-affected zone or weld metal, although quite different welding heat inputs were investigated. From the practical viewpoint, thick-walled SAW joints can be assessed for delayed hydrogen diffusion only by the base material coefficients. The calculated diffusion coefficients will be further used for numerical modelling of the hydrogen diffusion in welded joints. T2 - IIW Intermediate Meeting 2025 CY - Trollhätten, Sweden DA - 10.03.2025 KW - Hydrogen Cracking KW - Submerged Arc Welding KW - Hydrogen Diffusion KW - Cold Cracking PY - 2025 AN - OPUS4-63124 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Erxleben, Kjell T1 - Assessment of in-service welding conditions for pressurized hydrogen pipelines via component test N2 - Hydrogen is the energy carrier of tomorrow for a fossil-free future. This requires a reliable transport infrastructure capable of transporting large quantities of hydrogen. In addition to the construction of new pipelines, the conversion of existing natural gas (NG) networks is an essential part of global hydrogen strategies. The transport of hydrogen is fundamentally different from that of NG, as hydrogen can be absorbed into the pipeline material. Given the known effects of hydrogen embrittlement, the compatibility of the materials for the proposed pipelines (typically low alloy steels in a wide range of strengths and thicknesses) must be investigated. However, pipelines require frequent maintenance, repair, or the need to install additional outlets. In some cases, it is necessary to perform welding on or to the pipelines while they are in-service, i.e. with active gas flow under high pressure. This in-service welding poses challenges for hydrogen operations in terms of additional hydrogen absorption during welding and material compatibility. The challenge can be roughly divided into the possible austenitization of the inner pipe material exposed to hydrogen, which can lead to sufficient hydrogen absorption, and the welding itself, which causes an increased temperature range. Both lead to a significant increase in hydrogen solubility of the respective materials compared to room temperature. In this context, knowledge about welding on hydrogen pipelines is scarce due to the lack of operational experience. Fundamental experimental investigations are required to investigate the transferability from natural gas to hydrogen pipeline networks. For this reason, the present study presents a specially designed demonstrator concept for the realistic assessment of the welding process conditions. The demonstrator was designed ex-post sample extraction for quantification of the absorbed hydrogen concentration. For safety reasons, the required volume of pressurized hydrogen was limited by inserting a solid cylinder. Welding experiments on the DN50 and DN200 pressurized demonstrators showed an increased hydrogen uptake in the welded area of several ppm. T2 - Materials Week/Steel Innovation CY - Frankfurt am Main, Germany DA - 02.04.2025 KW - In-service KW - Hydrogen KW - Pipeline KW - Repair welding KW - Component test PY - 2025 AN - OPUS4-62941 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - Hybrid laser-arc welding of laser and plasma-cut 20 mm thick structural steels with AC magnetic support N2 - It is already known that the laser beam welding (LBW) or hybrid laser-arc welding (HLAW) processes are sensitive to manufacturing tolerances such as gaps and misalignment of the edges, especially at welding of thick-walled steels due to its narrow beam diameter. Therefore, the joining parts preferably have to be milled. The study deals with the influence of the edge quality, the gap and the misalignment of edges on the weld seam quality of hybrid laser-arc welded 20-mm-thick structural steel plates which were prepared by laser and plasma cutting. Single-pass welds were conducted in butt joint configuration. An AC magnet was used as a contactless backing. It was positioned under the workpiece during the welding process to prevent sagging. The profile of the edges and the gap between the workpieces were measured before welding by a profile scanner or a digital camera, respectively. With a laser beam power of just 13.7 kW, the single-pass welds could be performed. A gap bridgeability up to 1 mm at laser-cut and 2 mm at plasma-cut samples could be reached respectively. Furthermore, a misalignment of the edges up to 2 mm could be welded in a single pass. The new findings may eliminate the need for cost and time-consuming preparation of the edges. T2 - WAITRO-Workshop “Advanced Materials and Manufacturing Technologies for Africa and Middle East Development” CY - Cairo, Egypt DA - 01.06.2022 KW - Hybrid laser arc welding KW - Laser beam welding PY - 2022 AN - OPUS4-54950 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - Schweisstechnische Anwendungen von Hochleistungslasern für dickwandige Konstruktionen N2 - Der Beitrag befasst sich mit dem Potential der schweißtechnischen Anwendung von Hochleistungslasern für die moderne industrielle Fertigung. Die Ergebnisse eines abgeschlossenen IGF-Projektes werden präsentiert und im Hinblick auf die Vorteile des vorgeschlagenen EM-unterstützten Laser-MSG-Hybridschweißverfahrens ggü. konventionellen Schweißverfahren diskutiert. Vor allem die Eigenschaften des Verfahrens, wie eine bessere Spaltüberbrückbarkeit, eine bessere Durchmischung des Zusatzmaterials und gute mechanisch-technologische Eigenschaften der Schweißverbindungen werden hervorgehoben. T2 - Anwendertreffen des Laserverbundes Berlin-Brandenburg CY - Berlin, Germany DA - 25.11.2022 KW - Laserstrahlschweißen KW - Hybridschweißen KW - Elektromagnetische Schmelzbadkontrolle PY - 2022 AN - OPUS4-56571 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rethmeier, Michael T1 - Single pass laser vacuum welding of thick steel plates using electromagnetic support N2 - The increasing demand for renewable energy produced by offshore wind turbines goes along with an increased demand in the production of offshore wind turbine foundations, so called “monopiles”, which are made by joining thick metal sheets. The industrial standard of multi-layer submerged arc welding (SAW) for joining of thick metal sheets is the current bottleneck in the production of monopiles. A possible increase in productivity by the implementation of high-power laser welding in a newly developed mobile vacuum chamber (MoVac) and an electromagnetic root support is the subject of this study. Single run butt welds are performed in flat position on S355 mild steel of thicknesses up to 80 mm using a disc laser system with 1030 nm wavelength and a maximum output of 60 kW. The laser optic is fixed on the MoVac-System which is held and manipulated by an articulated robot. T2 - 13th CIRP Conference on Photonic Technologies [LANE 2024] CY - Fürth, Germany DA - 16.09.2024 KW - Laser beam welding KW - Laser welding with mobile vacuum PY - 2024 AN - OPUS4-62416 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Abilio, André T1 - Expert System for Screening Microbiologically Influenced Corrosion (MIC) as Internal Failure Cause in Oil and Gas Upstream Pipelines N2 - The analysis of pipeline failures due to Microbiologically Influenced Corrosion (MIC) is challenging due to the complex interaction of many influencing parameters including pipeline operation conditions, fluid chemistry and microbiology, as well as the analysis of corrosion features and products. To help address this challenge, an expert system was developed to assist non-specialists in screening internal pipeline corrosion failures due to MIC related threats. To accomplish this, 15 MIC subject matter experts (with a total of 355 man-years of accumulated MIC based experience) were recruited to evaluate a total of 65 MIC failure cases based on real-life scenarios. These case study parameters and the expert elicited results were input into an Artificial Neural Network (ANN) model to create a model system which can screen whether a given failure scenario is one of three outcomes: a) failure is likely due to MIC, b) failure is likely not due to MIC, or c) the conclusion is inconclusive (analysis needs more data/information). The model system had an overall accuracy of 74.8% and it showcases that knowledge from subject matter experts can be captured in a reasonably effective way to screen for possible MIC failures. Based on that, this presentation will provide details of the model development process and key results to date. Important considerations regarding the level of confidence of the diagnoses and variation between expert opinion will also be discussed alongside with ideas on how to improve the model for field applicability. T2 - ISMOS 9 CY - Edinburgh, United Kingdom DA - 27.06.2023 KW - Expert System KW - Microbiologically Influenced Corrosion (MIC) KW - Oil and Gas Upstream KW - Failure Investigation KW - Artificial neural networks (ANN) PY - 2023 AN - OPUS4-64603 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Scharf-Wildenhain, R. A1 - Engelking, Lorenz A1 - Hälsig, A. A1 - Schröpfer, Dirk A1 - Kannengießer, Thomas A1 - Hensel, J. T1 - Effect of heat control on mechanical properties and residual stresses at the transition zone of component and substrate in hybrid DED‑arc manufacturing N2 - In hybrid additive manufacturing, components or semi-finished products manufactured by conventional primary forming are enhanced or modified by additive manufactured structures. However, systematic investigations focusing on the critical transition area between the specific properties of the substrate (like high-strength) and the additively manufactured component, made of specific filler material, are still lacking. The focus of the present study was to determine the influence of heat control on the Δt8/5 cooling time, the distortion, the mechanical properties, and the residual stresses in the transition area of hybrid-additive components. This contributed to the knowledge regarding the safe avoidance of cold cracking, excessive distortion, a reduction in yield stress, and the implementation of hybrid DED-arc manufacturing. The heat control was varied by means of heat input and working temperature such that the Δt8/5 cooling times corresponded to the recommended processing range. The heat input has a greater influence on the cooling time in the transition area than the working temperature. Working temperature and the total energy applied per layer have a significant effect on component distortion. The lowest working temperature of 100 °C in combination with the highest total energy per layer leads to significantly greater distortion compared to manufacturing with a high working temperature of 300 °C and low total energy per layer. In addition, the longitudinal residual compressive stresses in the sensitive transition area are reduced from − 500 MPa to approx. − 200 MPa by adjusting the working temperature from 100 to 300 °C. Such complex interactions must be clarified comprehensively to provide users with easily applicable processing recommendations and standard specifications for an economical hybrid additive manufacturing of components made, for example, of high-strength steels in the transition area. T2 - IIW Annual Assembly and International Conference CY - Rhodes Island, Greece DA - 07.07.2024 KW - Hybrid additive manufacturing KW - DED-arc KW - Heat control KW - High-strength metals KW - Residual stress PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-630415 DO - https://doi.org/10.1007/s40194-025-02036-z SN - 1878-6669 SP - 1 EP - 15 PB - Springer AN - OPUS4-63041 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittner, Andreas T1 - Automated arc welding and quality assessment of large scale support structures for offshore wind turbines N2 - Offshore wind energy is a key driver in achieving a carbon dioxide-free industrial sector over the coming decades. However, the foundation systems for offshore wind plants significantly influence the overall installation process, alongside regulatory challenges. The adoption of lightweight design principles in steel construction, such as the use of dissolved load-bearing structures known as jacket foundations, holds substantial promise for reducing resource use, particularly the required volume of steel. This presentation focuses on the complete digitalization of the welding manufacturing and testing processes, enabling fully automated production and quality assessment of tubular nodes, which are critical components of jacket foundation structures. Additionally, the study examines the correlation between seam geometry and fatigue strength through numerical simulations inspired by bionic design principles. It demonstrates that tubular nodes can be welded entirely automatically while accommodating geometric tolerances. Moreover, seam geometries can be precisely manufactured according to the numerical models, significantly enhancing the service life of the structures. Finally, the resource efficiency and reduction in carbon dioxide emissions resulting from these advancements are analyzed through a life-cycle assessment, highlighting the environmental benefits of this approach. T2 - 77th IIW Annual Assembly and International Conference, C-XII: Arc Welding Processes and Production Systems CY - Rhodos, Greece DA - 07.07.2024 KW - Offshore wind KW - Support structures KW - Light-weight construction KW - Automated arc welding PY - 2024 AN - OPUS4-62016 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittner, Andreas A1 - Brauser, Stephan T1 - Herausforderungen und Lösungen für das robotergestützte Schweissen von Stahlrohrknoten für Offshore Wind Jackets N2 - Die Offshore-Windenergie spielt eine wichtige Rolle beim angestrebten Übergang zu einer emissionsfreien Industrie während der nächsten Jahrzehnte. Allerdings beeinflusst die Gründung der Offshore-Windanlagen den gesamten Installationsprozess. Die Anwendung von Leichtbauprinzipien im Stahlbau, wie beispielsweise die Verwendung von aufgelösten Tragstrukturen, sogenannten Jacket-Fundamenten, bietet ein großes Potenzial zur Reduzierung des Ressourcenverbrauchs, insbesondere im Hinblick auf die benötigte Stahlmenge. Der Vortrag befasst sich daher mit der vollständigen Digitalisierung der schweißtechnischen Fertigungs- und Prüfkette. Ziel ist es, eine vollautomatische Fertigung sowie Qualitätsprüfung von Rohrknoten zu ermöglichen. Diese stellen ein Schlüsselelement von Jacket-Fundamenten dar. Des Weiteren wird der Zusammenhang zwischen der Geometrie der Schweißnaht und der resultierenden Ermüdungsfestigkeit durch numerische Methoden unter Einbeziehung bionischer Prinzipien bewertet. Es wird gezeigt, dass rohrförmige Knoten unter Berücksichtigung von Geometrietoleranzen vollautomatisch geschweißt werden können. Die Schweißnahtform konnte gemäß den numerischen Modellen hergestellt werden, was ein großes Potenzial für eine verlängerte Lebensdauer bietet. Anschließend erfolgt eine Bewertung der Verbesserungen bei der Ressourceneffizienz und der Verringerung des CO2-Fußabdrucks durch ein Life Cycle Assessment. T2 - Schweissen in der maritimen Technik und im Ingenieurbau CY - Hamburg, Germany DA - 24.05.2023 KW - Offshore Windenergie KW - Fertigung KW - Leichtbau KW - Aufgelöste Tragstrukturen KW - Schweißen KW - Ermüdungsfestigkeit PY - 2023 AN - OPUS4-59498 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gook, Sergej A1 - El-Sari, Bassel A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael A1 - Biegler, Max T1 - Kombination des Laserhybridschweißens und UP-Engspaltschweißens für dickwandige Bauteile zur Erhöhung der Wirtschaftlichkeit N2 - Dieser Beitrag befasst sich mit der Entwicklung eines wirtschaftlichen und robusten Verfahrens zum Schweißen dicker Stahlbleche. Es werden Ergebnisse für das Fügen von Blechen im Dickenbereich von 25 mm bis 80 mm vorgestellt. Die 30 mm dicken Schweißnähte konnten im Stumpfstoß in zwei Durchgängen unter Verwendung des Laserhybridschweißens und des Unterpulverschweißens (UP) geschweißt werden. Das Laserhybridschweißen wird als Einschweißung mit einer Tiefe von ca. 25 mm ausgeführt. Die UP-Lagen werden auf der gegenüberliegenden Seite des Blechs aufgebracht. Bei richtiger Wahl der Schweißparameter wird der Nahtquerschnitt durch eine sichere Überlappung beider Lagen geschlossen. Bei Blechdicken über 30 mm ist eine Kantenvorbereitung erforderlich, die eine Ausführung der UP-Fülllagen in Engspalttechnik ermöglicht. Die Vorteile der vorgeschlagenen Prozesskombination liegen darin, dass die Nahtwurzel der Laserhybridnaht nicht geformt werden muss. Defekte in der Wurzel der Laserhybrideinschweißung können durch die UP-Lagen effektiv beseitigt werden. Das Verfahren bietet eine hohe Stabilität des Schweißprozesses in Bezug auf die Qualität der Blechkanten. Plasmageschnittene Kanten konnten ohne Bindefehler geschweißt werden. Die erreichte Nahtqualität wurde durch zerstörende und zerstörungsfreie Prüfungen bestätigt. T2 - Innovationstag 2024 CY - Düsseldorf, Germany DA - 10.04.2024 KW - Laserhybridschweißen KW - Windturm KW - Dickblech KW - Unterpulverschweißen PY - 2024 SN - 978-3-96144-253-9 VL - 391 SP - 186 EP - 194 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-60031 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittner, Andreas A1 - Fabry, Çağtay T1 - Automated welding of support structures for offshore wind turbines N2 - Offshore wind energy plays an important role for the desired transition towards a carbon dioxide free industry within the next decades. However, the grounding of the offshore wind plants governs the overall installation process besides bureaucratic bottlenecks. The application of lightweight principles in steel construction, e.g. the usage dissolved load-bearing structures, so called Jackets foundations, offer great potential in reducing the resource consumption, especially with respect to the needed amount of steel. In this context this paper focuses on a fully digitalization of the welding manufacturing and as well as testing chain to enable a fully automated manufacturing as well as quality assessment of tubular nodes as key element of Jackets foundation structures. Furthermore, the relationship between the seam shape geometry and resulting fatigue strength is evaluated by numerical methods incorporating bionic principles. It is shown that tubular nodes can be welded fully automatically taking geometry tolerances into account. Moreover, the seam shape could be manufactured as requested by the numerical models which offers great potential for an extended lifetime. Subsequently, the improvements in resource efficiency and reduction of carbon dioxide emissions are evaluated by a life-cycle-assessment. T2 - THERMEC'2023 International Conference on PROCESSING & MANUFACTURING OF ADVANCED MATERIALS: Processing, Fabrication, Properties, Applications CY - Vienna, Austria DA - 02.07.2023 KW - Offshore Wind energy KW - Automated welding KW - Life cycle assessment KW - Jacket foundations KW - Fatigue life PY - 2023 AN - OPUS4-59501 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Masoud Nia, Niloufar A1 - Nietzke, Jonathen A1 - Kannengiesser, Thomas T1 - Ti and Nb microalloying of HSLA steels and its effect on hydrogen diffusion and trapping N2 - Fine-grain, high-strength, low-alloy (HSLA) structural steels with yield strengths > 600 MPa are now the state of the art in construction applications such as mobile cranes and civil engineering. HSLA grades derive their strength from a combination of specific heat treatment and the underlying chemical composition. In this context, Ti or Nb are essential to obtain a fine-grained microstructure as well as the necessary carbides or nitrides for precipitation strengthening. In this context, the specific effect of Ti or Nb-rich compounds on hydrogen trapping and diffusion is well known for special laboratory cast alloys, but unknown for realistic steel compositions. For this reason, a series of S690Q-based alloys were synthesized, close to a real steel composition, but with well controlled Ti or Nb additions in different amounts. Specimens were obtained from these alloys by electrochemical discharge machining (EDM). The specimens were tested using the well-established electrochemical permeation technique. From the experimental results, the hydrogen diffusion coefficients and the analytical subsurface hydrogen concentration were calculated. In addition, the hydrogen trapping behavior at elevated temperatures was interpreted by thermal desorption analysis (TDA) using different heating rates of hydrogen charged samples. The results showed that in contrast to metallurgically "pure" laboratory cast alloys, realistic chemical compositions were similar in their hydrogen trapping behavior, despite some small differences. All investigated steel grades exhibited shallow and reversible hydrogen trapping, regardless of their chemical composition. Of course, the experiments only allowed the calculation of effective diffusion coefficients and trapping energies, which represent an average of the entire microstructure. Nevertheless, HSLA steels are typically joined by arc welding, which includes the risk of delayed hydrogen assisted cracking. From the point of view of welding practice, however, a more or less identical hydrogen diffusion behavior means that no special "metallurgically specific", justifiable measures need to be considered, despite the well-established processes such as "soaking" or dehydrogenation heat treatment. T2 - MPAC 2025 CY - Stuttgart, Germany DA - 06.10.2025 KW - HACC KW - Hydrogen KW - HSLA PY - 2025 AN - OPUS4-64337 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Reichel, Levin A1 - Schroepfer, Dirk A1 - Kromm, Arne A1 - Kannengiesser, Thomas T1 - Stress-Optimised Welding Repair for High-Strength Offshore Steel Joints N2 - The successful energy transition in Germany will require offshore wind turbines with outputs >10 MW in the future. To achieve these high outputs, turbines far from the coast are required, featuring large subsea jacket structures (30 m up to 50 m) and tall towers (up to 200 m). High-strength steels with a yield strengths up to 500 MPa and wall thicknesses of up to 120 mm are increasingly being used for these structures. During manufacture, weld defects detected by non-destructive testing (NDT) require localized repair (gouging and rewelding). To date, there is a lack of repair concepts and information in standards and guidelines. Therefore, BAM initiated the FOSTA project P1629 (IGF 01IF22746N) to investigate the stress-optimized repair (local gouging and welding) of high-strength thick plate joints made of offshore grades in the yield strength range off 355 to 460 MPa and similar weld metal. This research aims to develop a stress-optimized repair concept for thick plate joints, using controlled high-performance GMAW processes and optimized, narrow gouging grooves. Thermal and mechanical gouging are performed, allowing the groove configuration to be modified. Modern welding processes provide deep root penetration and focused energy input capable of welding narrow seams. The aimed residual stress reduction can be attributed to the lower input of weld metal due to the changes in groove configuration and to the reduction in heat input per layer due to the controlled arc process. The experimental analyses take into account the interaction of process, material, and design-related influences on the formation of weld induced stresses. Concluding with recommendations for guidelines elaborated for steel-processing SMEs. T2 - MPA Stuttgart 2025 CY - Stuttgart, Germany DA - 06.10.2025 KW - Repair welding KW - Residual stress KW - High-strength steels KW - Gouging KW - Modern welding processes PY - 2025 AN - OPUS4-64347 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas A1 - Kromm, Arne A1 - Kadoke, Daniel A1 - Kruse, Julius T1 - Effect of Ti microalloying on the local strain behavior of cross-weld tensile samples determined by digital image correlation N2 - High-strength low-alloyed (HSLA) steels with yield strength / proof stress ≥ 600 MPa are the basis of modern light-weight steel constructions. Indeed, the economic and ecological benefits strongly depend on their processability in terms of welding. In this context, the use of highly productive welding processes and suitable welding consumables is of vital interest and requires a fundamental understanding of the microstructural changes in the HSLA steel and especially the heat-affected zone (HAZ) of the welded joint. Microalloying elements, such as Ti or Nb, are essential to achieve the desired mechanical properties. To analyse the weldability, three-layer welds were performed using gas metal arc welding (GMAW) and critical microstructures, such as areas of the HAZ that exhibit significant softening or hardening, were identified. The effect of the softened HAZ region on failure was evaluated using cross-weld tensile specimens. Digital image correlation (DIC) was used for in-situ monitoring of the development and accumulation of the local strains in different HAZ regions during tensile testing. Using a specially designed mirror system, the local strains of the microstructure zones on the top and bottom of the weld were recorded simultaneously. In addition, the analysis of the local deformation helps to understand the effects of the softened HAZ on the global strain, the reduction in area, the fracture position, and the overall fracture behavior. KW - High-strength structural steel KW - Microalloying influences KW - HAZ-softening KW - Digital Image Correlation KW - Constraint effect KW - Thermodynamic simulation PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-643558 DO - https://doi.org/10.1007/s40194-025-02185-1 SP - 1 EP - 17 PB - Springer Nature AN - OPUS4-64355 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Component test for simulation of in-service welding on hydrogen pipelines N2 - Hydrogen is set as the energy carrier of tomorrow and most countries will achieve large-scale hydrogen transport through the conversion of the natural gas (NG) grid and the construction of new pipelines. The interaction between hydrogen and the pipeline materials differs fundamentally from that of NG, as hydrogen is readily absorbed into the material. Considering the possible hydrogen embrittlement (HE), the compatibility of the pipeline materials (low-alloyed steels with a wide strength/thickness range) must be investigated. However, pipelines require intervention for maintenance, repair, or grid expansion with welding on/onto the pipelines while in service, i.e. the well-known "hot tapping" and "stoppling". The challenges compared to NG can be broadly divided into the possible austenitization of the inner pipe material exposed to hydrogen and the welding itself. Both result in a significant increase in hydrogen solubility and could potentially pose challenges in terms of HE. Emphasis is placed on the word "could" because knowledge of "hot tapping" on hydrogen pipelines is scarce due a lack of service experience. To this end, this study proposes a concept for a component-like demonstrator with the objectives: (1) safe feasibility of "hot tapping" on pressurized model hydrogen pipeline sections, (2) facilitate ex-post sample extraction for the purpose of quantifying the absorbed hydrogen concentrations, and (3) ensure in-situ temperature measurement during welding to monitor the pipeline surface temperature. For safety reasons in the event of an unintentional "burn-through", a solid cylinder was inserted in the demonstrator to restrict the hydrogen gas volume to a small, pressurized layer. Reference pipeline surface temperature measurements were ensured on comparable, unpressurized geometries. The investigated range of welding conditions was investigated for representative material/thickness combinations (DN60 to DN300), suggesting the feasibility of the demonstrator for the determination of reliable in-service welding conditions for both installed and new pipelines for hydrogen service. T2 - 49th MPA Conference CY - Stuttgart, Germany DA - 06.10.2025 KW - Hydrogen KW - Pipeline KW - In-service welding KW - Component test PY - 2025 AN - OPUS4-64317 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Brunner-Schwer, Christian T1 - Hochleistungs-Lichtbogenschweißen von dicken Stahlblechen mit elektromagnetischer Schweißbadunterstützung N2 - Das Unterpulverschweißen (UP) ist das Lichtbogenschweißverfahren mit der höchsten Abschmelzrate. Beim Schweißen von dicken Blechen ist dieses Verfahren jedoch besonders für die Wurzellage von Nachteil. Voll-ständiges Umschmelzen ohne extremen Wurzeldurchhang oder ein Austropfen der Schmelze ist ohne weitere Hilfsmittel schwer zu erreichen. Aus diesem Grund werden Pulver-, Kupfer-, keramische Badstützen oder Ble-che zur Vermeidung des Wurzeldurchhangs verwendet. Bei der Verwendung von Kupfer- oder Keramikstützen beeinflusst beispielsweise die Diffusion chemischer Elemente in die Schweiß- oder Schmelzlinie die mecha-nischen Eigenschaften der Schweißnaht. All diese Badstützen erfordern zusätzliche Schritte zur Vorbereitung und Entfernung sowie zur Reinigung der Schweißwurzel. Die Verwendung einer elektromagnetischen Bad-stütze hat dagegen viele Vorteile. Der Magnet kommt nicht mit dem Werkstück in Kontakt, sodass ein zusätz-licher Schritt des Entfernens nicht erforderlich ist. Versuche mit Laserstrahlschweißen oder Laserhybrid-schweißen haben bereits erstmalig gezeigt, dass Blechdicken bis 30 mm einlagig einseitig geschweißt werden können und zusätzlich ein Spalt oder Kanterversatz von bis zu 2 mm überbrückt werden können. In dieser Arbeit wird die elektromagnetische Badstütze für den UP-Prozess eingesetzt. Die Wurzellage wird an 15 mm dicken Blechen mit einer Spaltgröße von 2 mm geschweißt. Die Verwendung eines elektromagnetischen Sys-tems stellt hier sicher, dass die Schmelze nach oben gedrückt und in Position gehalten wird. Ferner kann die Schweißtiefe entsprechend den magnetischen Parametern angepasst werden. Dieses Verfahren kann die Produktivität im Schweißbereich von vielen Betrieben deutlich steigern und Kosten gleichzeitig senken und kann dazu beitragen, diese Arbeitsplätze in Deutschland zu sichern. T2 - DVS CONGRESS 2024 Große Schweißtechnische Tagung CY - Erfurt, Germany DA - 16.09.2024 KW - Hochleistungs-Lichtbogenschweißen KW - Unterpulverschweißen PY - 2024 AN - OPUS4-62037 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rethmeier, Michael T1 - Kombination des Laserhybridschweißens und UP-Engspaltschweißens für dickwandige Bauteile zur Erhöhung der Wirtschaftlichkeit N2 - Dieser Beitrag befasst sich mit der Entwicklung eines wirtschaftlichen und robusten Verfahrens zum Schweißen dicker Stahlbleche. Es werden Ergebnisse für das Fügen von Blechen im Dickenbereich von 25 mm bis 80 mm vorgestellt. Die 30 mm dicken Schweißnähte konnten im Stumpfstoß in zwei Durchgängen unter Verwendung des Laserhybridschweißens und des Unterpulverschweißens (UP) geschweißt werden. Das Laserhybridschweißen wird als Einschweißung mit einer Tiefe von ca. 25 mm ausgeführt. Die UP-Lagen werden auf der gegenüberliegenden Seite des Blechs aufgebracht. Bei richtiger Wahl der Schweißparameter wird der Nahtquerschnitt durch eine sichere Überlappung beider Lagen geschlossen. Bei Blechdicken über 30 mm ist eine Kantenvorbereitung erforderlich, die eine Ausführung der UP-Fülllagen in Engspalttechnik ermöglicht. Die Vorteile der vorgeschlagenen Prozesskombination liegen darin, dass die Nahtwurzel der Laserhybridnaht nicht geformt werden muss. Defekte in der Wurzel der Laserhybrideinschweißung können durch die UP-Lagen effektiv beseitigt werden. Das Verfahren bietet eine hohe Stabilität des Schweißprozesses in Bezug auf die Qualität der Blechkanten. Plasmageschnittene Kanten konnten ohne Bindefehler geschweißt werden. Die erreichte Nahtqualität wurde durch zerstörende und zerstörungsfreie Prüfungen bestätigt. T2 - Innovationstag 2024 - Transfertage der Fügetechnik CY - Düsseldorf, Germany DA - 10.04.2024 KW - Laserhybridschweißen KW - Wirtschaftlichkeit KW - UP-Engspaltschweißen PY - 2024 AN - OPUS4-62222 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rethmeier, Michael T1 - AI-based welding process monitoring for quality control in the manufacture of large-diameter pipes N2 - The paper presents the experimental results into the development of a multi-channel system for monitoring and quality assurance of the multi-wire submerged arc welding (SAW) process for the manufacture of large diameter pipes. Process signals such as welding current, arc voltage and the acoustic signal emitted from the weld zone are recorded and processed to provide information on the stability of the welding process. It was shown by the experiments that the acoustic pattern of the SAW process in a frequency range between 30 Hz and 2.5 kHz contains the most diagnostic information. In the spectrogram of the acoustic signal, which represents the time course of the frequency spectrum of the welding process, the formation of weld irregularities such as undercuts could be reliably identified. The on-line quality assessment of the weld seam produced is carried out in combination with methods of artificial intelligence (AI). From the results obtained, it can be concluded that the use of the latest concepts in welding and automation technology, combined with the high potential of AI, can achieve a new level of quality assurance in pipe manufacturing. T2 - Pipeline Technology Conference 2024 CY - Berlin, Germany DA - 08.04.2024 KW - Process monitoring KW - Submerged arc welding KW - Acoustic signal KW - Artificial intelligence KW - Quality control PY - 2024 AN - OPUS4-62225 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kröll, Mirco T1 - Noch ein Normungsausschuss? Was hinter dem neuen Tribologie-Ausschuss beim DIN steckt N2 - Am 10. März fand die Gründungssitzung des neuen DIN-Ausschusses NA 062-10-21 AA "Tribologie" statt. Er fokussiert den praxisnahen Wissenstransfer zur Lösung aktueller Herausforderungen und beschäftigt sich mit Querschnittsthemen sowie übergreifenden Aspekten. Der Vortrag informiert über den Kontext der Gründung und stellt die ersten Normungsprojekte vor. T2 - 66. GfT Tribologie-Fachtagung 2025 CY - Wernigerode, Germany DA - 01.10.2025 KW - Tribologie KW - DIN KW - Normung KW - Standardisierung KW - Harmonisierung KW - FAIR KW - Verschleißermittlung KW - Oberflächencharakterisierung KW - Terminologie KW - Ontologie KW - Semantik KW - Datenbank KW - Dataspace PY - 2025 AN - OPUS4-64252 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rethmeier, Michael A1 - El-Sari, Bassel A1 - Biegler, Max A1 - Gook, Sergej T1 - AI-based welding process monitoring for quality control in the manufacture of large-diameter pipes N2 - The paper presents the experimental results into the development of a multi-channel system for monitoring and quality assurance of the multi-wire submerged arc welding (SAW) process for the manufacture of large diameter pipes. Process signals such as welding current, arc voltage and the acoustic signal emitted from the weld zone are recorded and processed to provide information on the stability of the welding process. It was shown by the experiments that the acoustic pattern of the SAW process in a frequency range between 30 Hz and 2.5 kHz contains the most diagnostic information. In the spectrogram of the acoustic signal, which represents the time course of the frequency spectrum of the welding process, the formation of weld irregularities such as undercuts could be reliably identified. The on-line quality assessment of the weld seam produced is carried out in combination with methods of artificial intelligence (AI). From the results obtained, it can be concluded that the use of the latest concepts in welding and automation technology, combined with the high potential of AI, can achieve a new level of quality assurance in pipe manufacturing. T2 - Pipeline Technology Conference 2024 CY - Berlin, Germany DA - 08.04.2024 KW - Process monitoring KW - Submerged arc welding KW - Acoustic signal KW - Artificial intelligence PY - 2024 UR - https://www.pipeline-conference.com/abstracts/ai-based-welding-process-monitoring-quality-control-large-diameter-pipe-manufacturing SP - 1 EP - 9 AN - OPUS4-62226 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Akyel, Fatma A1 - Gook, Sergej A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Brunner-Schwer, Christian A1 - Rethmeier, Michael T1 - Hochleistungs-Lichtbogenschweißen von dicken Stahlblechen mit elekt-romagnetischer Schweißbadunterstützung N2 - Das Unterpulverschweißen (UP) ist das Lichtbogenschweißverfahren mit der höchsten Abschmelzrate. Beim Schweißen von dicken Blechen ist dieses Verfahren jedoch besonders für die Wurzellage von Nachteil. Voll-ständiges Umschmelzen ohne extremen Wurzeldurchhang oder ein Austropfen der Schmelze ist ohne weitere Hilfsmittel schwer zu erreichen. Aus diesem Grund werden Pulver-, Kupfer-, keramische Badstützen oder Ble-che zur Vermeidung des Wurzeldurchhangs verwendet. Bei der Verwendung von Kupfer- oder Keramikstützen beeinflusst beispielsweise die Diffusion chemischer Elemente in die Schweiß- oder Schmelzlinie die mecha-nischen Eigenschaften der Schweißnaht. All diese Badstützen erfordern zusätzliche Schritte zur Vorbereitung und Entfernung sowie zur Reinigung der Schweißwurzel. Die Verwendung einer elektromagnetischen Bad-stütze hat dagegen viele Vorteile. Der Magnet kommt nicht mit dem Werkstück in Kontakt, sodass ein zusätz-licher Schritt des Entfernens nicht erforderlich ist. Versuche mit Laserstrahlschweißen oder Laserhybrid-schweißen haben bereits erstmalig gezeigt, dass Blechdicken bis 30 mm einlagig einseitig geschweißt werden können und zusätzlich ein Spalt oder Kanterversatz von bis zu 2 mm überbrückt werden können. In dieser Arbeit wird die elektromagnetische Badstütze für den UP-Prozess eingesetzt. Die Wurzellage wird an 15 mm dicken Blechen mit einer Spaltgröße von 2 mm geschweißt. Die Verwendung eines elektromagnetischen Sys-tems stellt hier sicher, dass die Schmelze nach oben gedrückt und in Position gehalten wird. Ferner kann die Schweißtiefe entsprechend den magnetischen Parametern angepasst werden. Dieses Verfahren kann die Produktivität im Schweißbereich von vielen Betrieben deutlich steigern und Kosten gleichzeitig senken und kann dazu beitragen, diese Arbeitsplätze in Deutschland zu sichern. T2 - DVS CONGRESS 2024 Große Schweißtechnische Tagung CY - Erfurt, Germany DA - 16.09.2024 KW - Unterpulverschweißen KW - Hochleistungs-Lichtbogenschweißen PY - 2024 SN - 978-3-96144-269-0 VL - 395 SP - 134 PB - DVS Media CY - Düsseldorf AN - OPUS4-61613 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Abilio, André T1 - Expert System for Screening Microbiologically Influenced Corrosion asInternal Failure Cause in Oil and Gas Upstream Pipelines N2 - The analysis of pipeline failures due to Microbiologically Influenced Corrosion (MIC) is challenging due to the complex interaction of many influencing parameters including pipeline operation conditions, fluid chemistry and microbiology, as well as the analysis of corrosion features and products. To help address this challenge, an expert system was developed to assist non-specialists in screening internal pipeline corrosion failures due to MIC related threats. To accomplish this, 15 MIC subject matter experts (with a total of 355 man-years of accumulated MIC based experience) were recruited to evaluate a total of 65 MIC failure cases based on real-life scenarios. These case study parameters and the expert elicited results were input into an Artificial Neural Network (ANN) model to create a model system which can screen whether a given failure scenario is one of three outcomes: a) failure is likely due to MIC, b) failure is likely not due to MIC, or c) the conclusion is inconclusive (analysis needs more data/information). The model system had an overall accuracy of 74.8%and it showcases that knowledge from subject matter experts can be captured in a reasonably effective way to screen for possible MIC failures. Based on that, this presentation will provide details of the model development process and key results to date. Important considerations regarding the level of confidence of the diagnoses and variation between expert opinion will also be discussed alongside with ideas on how to improve the model for field applicability. T2 - ISMOS 9 CY - Edinburgh, United Kingdom DA - 27.06.2023 KW - Expert System KW - Microbiologically Influenced Corrosion (MIC) KW - Oil and Gas Upstream KW - Artificial neural networks (ANNs) KW - Failure analysis PY - 2023 AN - OPUS4-64602 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Griesche, Axel T1 - In situ Measurement of Hydrogen in Steel using Laser-induced Breakdown Spectroscopy (LIBS) N2 - Laser-induced breakdown spectroscopy (LIBS) is an analysis technique that allows contactless and fast in situ measurements of hydrogen in welded steels. The surface does not need necessarily be prepared as the laser can ablate material before the measurement. Depth profiling, point measurements as well as scanning of areas (mapping) can be utilized and automated. The method can be used for quantitative measurements, which requires a calibration with standards of similar material containing known hydrogen concentrations. LIBS is a candidate for ISO 3690, determination of diffusible hydrogen in martensitic, bainitic, and ferritic steel weld metal using arc welding processes with filler material. The capability of the method is shown in a hydrogen diffusion experiment. T2 - Tagung Steel & Hydrogen 2025 CY - Genth, Belgium DA - 14.10.2025 KW - LIBS KW - Hydrogen measurement KW - Laser spectroscopy KW - Steel PY - 2025 AN - OPUS4-64451 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Koerdt, Andrea T1 - Wasserstofflagerung in unterirdischen geologischen Formationen und potenzielle Risiken durch Mikroorganismen N2 - Bei dem Vortrag werden die potentiellen mikrobiologischen Einflüsse im Falle der Lagerung von Wasserstofflagerung in unterirdischen geologischen Formationen vorgestellt, die Zusammenarbeit mit internen und auch externen Partnern. Der Fokus liegt dabei auf UGF; anaerobe Umgebungen, Sulfate reduzierenden Bakterien, methanogenen Archaea, weiterleitenden Systeme und die Kombination der Untersuchung abiotisch/biotische T2 - VDI-Schadensanalyse (49) CY - Würzburg, Germany DA - 17.10.2023 KW - MIC KW - Wasserstofflagerung KW - Unterirdische Speicher KW - Kontamination von H2 KW - H2-Abbau KW - Mikroorganismen KW - Biotische/abiotische Faktoren PY - 2023 AN - OPUS4-58645 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Reichel, Levin A1 - Schroepfer, Dirk A1 - Kromm, Arne A1 - Kannengiesser, Thomas T1 - Reduction of residual stress by narrowing the repair groove: Optimising repair welding with modern welding processes for high strength offshore steels N2 - The ongoing German energy transition will require offshore wind turbines with outputs of >10 MW in the future. Turbines with these high outputs must be located far from the coast, with up to 50 m large subsea jacket structures and tall towers. These structures are increasingly fabricated of high-strength steels with a yield strength up to 500 MPa and wall thicknesses of up to 120 mm. During production, weld defects identified through non-destructive testing (NDT) must be locally repaired by gouging and rewelding. Standards and guidelines lack sufficient concepts and information regarding such repair procedures. To address this gap, BAM launched the FOSTA project P1629 (IGF 01IF22746N) to explore stress-optimised repair concepts, specifically local gouging and welding, for high-strength thick plate joints made from offshore-grade steels with yield strengths between 355 MPa and 460 MPa, including matching weld metals. This research aims to develop a stress-optimised repair concept for thick plate joints, utilising controlled high-performance GMAW techniques and narrow gouging grooves. Both thermal and mechanical gouging methods are applied, enabling adjustments to the groove geometry. Modern welding processes offer deep root penetration and concentrated energy input, making them suitable for narrow seams. The intended reduction in residual stress results from the decreased weld metal volume, due to modified groove shapes and the lower heat input per layer achieved through controlled arc processes. Experimental investigations examine how process parameters, material properties, and design factors interact to influence the development of welding-induced stresses. The project concludes with practical recommendations for guidelines tailored to steel-processing SMEs. T2 - 4th International Conference on Advanced Joining Processes (AJP 2025) CY - Coimbra, Portugal DA - 16.10.2025 KW - Repair welding KW - Residual stress KW - Modern welding processes KW - High-strength offshore steel KW - Narrow groove PY - 2025 AN - OPUS4-64887 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröpfer, Dirk T1 - Influence of Ultrasonic-Assisted Milling on Surface Integrity of Additively Manufactured Components Using DED-Arc/GMAW N2 - Additive manufacturing (AM) is increasingly used for producing complex metallic com-ponents. Subsequent machining is essential to achieve final geometries and surface conditions. The resulting surface integrity, particularly the near-surface residual stress state, plays a crucial role in component performance and fatigue life. This study inves-tigates the potential of ultrasonic-assisted milling (USAM), a hybrid machining process, to improve surface integrity and machinability compared to conventional milling (CM). Three materials were investigated, two difficult-to-cut materials CoCr26Ni9Mo5W and FeNi36 and a low-alloy steel S355J2C. The CoCr26Ni9Mo5W and FeNi36 were addi-tively manufactured via DED-Arc and then machined with varying cutting speeds and feed rates within a Design of Experiments. USAM exhibited enhanced machinability and surface integrity, particularly at low cutting speeds, by reducing cutting forces up to 40% and shifting near-surface residual stresses from tensile to compressive. For S355J2C, USAM reduced cutting forces by approximately 45% and induced surface-near compressive residual stresses up to approximately -700 MPa, leading to a 11% higher fatigue strength compared to CM. These findings highlight the advantages of ultrasonic assistance in post-AM machining, offering enhanced fatigue performance and surface quality for various metallic materials. T2 - 4th International Conference on Advanced Joining Processes 2025 CY - Coimbra, Portugal DA - 16.10.2025 KW - Ultrasonic-assisted milling KW - Additive manufacturing KW - Surface integrity KW - Fatigue strength KW - Residual stress PY - 2025 AN - OPUS4-65051 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröpfer, Dirk T1 - Influence of Substrate Design on Properties and Residual Stresses in Hybrid AM/DED-Arc of High-Strength Steels N2 - High-strength, fine-grained structural steels are increasingly used in modern steel construction to meet economic and environmental demands through lightweight design and reduced material usage. Additive manufacturing (AM), in particularly direct energy deposition with gas metal arc welding (DED-Arc), offers significant advantages in flex-ibility, production speed, and cost efficiency. In hybrid AM, conventionally manufac-tured parts are extended or modified using AM processes. Welding-induced residual stresses, especially in the transition area, pose challenges to structural integrity. This study investigates the influence of substrate design and thermal pretreatment on the residual stress state of hybrid AM components made from base material steel S690QL and a welding filler, a modified solid wire G79. Two substrate geometries (I- and T-substrate) are analysed, which are additively and conventionally manufactured, re-spectively. Results show that substrate geometry significantly affects local residual stresses, microstructure and hardness, particularly in the transition are. The findings contribute to a better understanding of the evolution of welding stresses in hybrid AM components to achieve reliable, crack-resistant and economic high-strength steel structures. T2 - 4th International Conference on Advanced Joining Processes 2025 CY - Coimbra, Portugal DA - 16.10.2025 KW - DED-Arc KW - Residual stress KW - Hybrid additive manufacturing PY - 2025 AN - OPUS4-65048 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scharf-Wildenhain, R. T1 - Influence of build-up height on residual stresses in additive repair and modification of multi-material composites using DED-Arc N2 - The application of steels with a higher yield strength allows reductions in wall thickness, component weight and production costs. Hybrid additive manufacturing based on Gas Metal Arc Welding (GMAW) processes (DED-Arc) can be used to realise highly effi-cient component modifications and repairs on semi-finished products and additively manufactured structures. There are still a number of key issues preventing widespread implementation, particularly for SMEs. In addition to the manufacturing design, detailed information about assembly strategy and geometric adaptation of the component for modifications or repairs are missing. These include the welding-related stresses associ-ated with the microstructural influences caused by the additive manufacturing steps, particularly in the transition area of the substrate and filler material interface. The present research focuses the effect of component height on residual stress distribution. Defined specimens were welded fully automatically with a high-strength solid wire (yield strength > 790 MPa) especially adapted for DED-Arc on S690QL substrate. T2 - IIW intermediate meeting for commission IX CY - Trollhätten, Sweden DA - 12.03.2025 KW - DED-Arc KW - Residual stress KW - Component height PY - 2025 AN - OPUS4-65046 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hübner, Martin A1 - Dittmann, Florian A1 - Kromm, Arne A1 - Varfolomeev, Igor A1 - Kannengiesser, Thomas T1 - Improvement of Fatigue Resistance through the Application of a Low-Transformation-Temperature Welding Consumable N2 - Low transformation temperature (LTT) welding consumables are an innovative approach to reduce tensile residual stress in weld seams and the surrounding heat affected zone (HAZ). The reduced tensile stress can lead to an improvement in fatigue strength of welded components. LTT alloys are characterized by a chemical composition which reduce the martensite start temperature (Ms) close to room temperature. This article focuses on a hybrid use of LTT filler metals, where the LTT filler is applied as an additional layer to conventional welds on fatigue-critical spots. Conventional gas metal arc welded longitudinal stiffeners are used as specimens. At the face ends of the stiffeners, a second LTT layer was added with various modifications in weld shapes. These different shapes were achieved by changing the welding parameters such as welding speed and offset to the first layer. These samples were used to analyze shape, dilution, resulting Ms, residual stress and fatigue strength. The dilatometer verified Ms and dilution did not change significant, although the area of the 2nd LTT weld seam was varying clear with each modification. However, the weld modification had a significant effect on the residual stress state and the fatigue strength. The X-ray determined residual stress in the HAZ became lower when the weld toe of the LTT layer was further away from the stiffener. All samples with LTT weld exhibit significantly higher fatigue strength values than conventionally single and double-layer welded samples. The lower the residual stress at weld toe, the higher the fatigue strength. The results show that on the one hand LTT filler metals increase the fatigue strength, and on the other hand the impact of LTT fillers materials is not restricted to the dilution and Ms, the shape of the weld seam must also be considered. T2 - 4th international Conference on Advanced Joining Processes AJP CY - Combria, Portugal DA - 16.10.2025 KW - Low transformation temperature (LTT) KW - Residual stress reduction KW - Fatigue strength KW - Longitudenal stiffener PY - 2025 AN - OPUS4-65090 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hübner, Martin T1 - Bericht zum Fortschritt des laufenden Projekts: "Hybrider Einsatz von LTT-Schweißzusätzen zur Schwingfestigkeitsverbesserung hochfester Stahlbauteile" N2 - Low Transformation Temperature (LTT) Schweißzusätze erzeugen während der Abkühlung Druckeigenspannungen in die Schweißnaht und Wärmeeinflusszone durch eine Volumenexpansion, wodurch die Ermüdungsfestigkeit erhöht werden kann. Um das Potential dieser neuartigen Schweißzusätze besser zu quantifizieren, wurden konventionelle Längssteifen als Probenkörper verwendet, welche an den Stirnseiten mit einer LTT-Zusatznaht geschweißt wurden. Durch Variation der Schweißparameter konnten unterschiedliche Nahtformen realisiert werden. Es konnte, je nach Nahtausführung, eine Erhöhung der Ermüdungsfestigkeit bei 2 Millionen Lastwechseln von 140% festgestellt werden. Somit sind LTT-Zusätze grundsätzlich geeignet, um die Ermüdungsfestigkeit zu erhöhen. Weiterhin wurde festgestellt, dass das Reparaturschweißen mit LTT Schweißzusätzen als Decklage ebenfalls zu einem deutlichen Ermüdungsfestigkeitsanstieg führte. T2 - Sitzung des DVS Fachausschuss FA09 - Konstruktion und Festigkeit CY - Düsseldorf, Germany DA - 10.12.2025 KW - Low transformation temperature (LTT) KW - Eigenspannungen KW - Ermüdungsfestigkeit KW - hochfeste Stähle KW - Mikroproben PY - 2025 AN - OPUS4-65089 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - Effect of hydrogen pressure on the fretting behavior of elastomers N2 - In this study, the fretting behavior of several elastomer materials against 316L were evaluated in air and hydrogen environment up to 10 MPa. Furthermore, aging experiments were conducted for 7 days under static conditions in 100 MPa hydrogen and the physical and mechanical properties of the rubber materials were examined before and after hydrogen exposure. Fretting tests revealed that the wear of these compounds is significantly affected by the hydrogen environment compared to air, especially with NBR grades. After aging experiment, the friction response of HNBR grades is characterized by increased adhesion due to elastic deformation, leading to partial slip. T2 - ITC 2023: 9th International Tribology Conference 2023 CY - Fukuoka, Japan DA - 26.09.2023 KW - Hydrogen KW - Fretting KW - Elastomers PY - 2023 AN - OPUS4-61962 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Cano Murillo, Natalia A1 - Balasooriya, Winoj A1 - Theiler, Geraldine T1 - Effect of hydrogen environment on the physical and mechanical properties of elastomers N2 - The development of a robust hydrogen infrastructure poses challenges to materials exposed to high pressurized hydrogen environments. Polymeric materials, which are expected to perform as seals, gaskets, O-rings, hoses among other applications face high risk of damage due to rapid gas decompression (RGD) which might cause operational safety issues. In this study, we intend to assess the effects of a high pressurized hydrogen environment on carbon black filled (CB) elastomers. The materials were exposed to 100 MPa hydrogen atmosphere at room temperature and at 85°C. Ex-situ characterization was performed during the first 30 minutes after decompression and repeated two days after the exposure when total gas desorption has taken place. The physical and mechanical characteristics of the materials were determined by means of density and volume change, hardness and tensile tests, and dynamic mechanical analysis. T2 - EHEC, the European Hydrogen Energy Conference 2024 CY - Bilbao, Spain DA - 06.03.2024 KW - High pressurized Hydrogen KW - Sealing Materials KW - Carbon Black Filled Elastomers PY - 2024 AN - OPUS4-60706 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Theiler, Geraldine A1 - Cano Murillo, Natalia A1 - Halder, Karabi A1 - Balasooriya, Winoj A1 - Hausberger, Andreas A1 - Kaiser, Andreas T1 - Effect of high-pressure hydrogen environment on the physical and mechanical properties of elastomers N2 - This study presents the influence of high-pressure hydrogen environment on the physical and mechanical properties of two types of cross-linked hydrogenated acrylonitrile butadiene rubbers. Based on the CSA/ANSI standard, static exposures in hydrogen experiments were performed up to 100 MPa at 120 °C. Characterization before and after exposure was conducted by means of density and hardness measurements, dynamic mechanical analysis (DMA), tensile tests, compression set, FT-IR and AFM analyses to assess effects after decompression. While the effect of high-pressure exposure is significant immediately after exposure, most of the physical and mechanical properties recover after 48 hours. FT-IR, AFM, SEM and compression set results indicate, however, permanent effects. KW - Hydrogen KW - Mechanical properties KW - Elastomers KW - High-pressure hydrogen environment PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-597102 DO - https://doi.org/10.1016/j.ijhydene.2024.01.148 SN - 0360-3199 VL - 58 SP - 389 EP - 399 PB - Elsevier Ltd. AN - OPUS4-59710 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Theiler, Geraldine A1 - Cano Murillo, Natalia A1 - Hausberger, Andreas T1 - Effect of hydrogen pressure on the fretting behavior of rubber materials N2 - Safety and reliability are the major challenges to face for the development and acceptance of hydrogen technology. It is therefore crucial to deeply study material compatibility, in particular for tribological components that are directly in contact with hydrogen. Some of the most critical parts are sealing materials that need increased safety requirements. In this study, the fretting behavior of several elastomer materials were evaluated against 316L stainless steel in an air and hydrogen environment up to 10 MPa. Several grades of cross-linked hydrogenated acrylonitrile butadiene (HNBR), acrylonitrile butadiene (NBR) and ethylene propylene diene monomer rubbers (EPDM) were investigated. Furthermore, aging experiments were conducted for 7 days under static contions in 100 MPa of hydrogen followed by rapid gas decompression. Fretting tests revealed that the wear of these compounds is significantly affected by the hydrogen environment compared to air, especially with NBR grades. After the aging experiment, the friction response of the HBNR grades is characterized by increased adhesion due to elastic deformation, leading to partial slip. KW - Fretting wear KW - Rubbers KW - Hydrogen KW - High-pressure PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-608462 DO - https://doi.org/10.3390/lubricants12070233 VL - 12 IS - 7 SP - 1 EP - 17 PB - MDPI AN - OPUS4-60846 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kröll, Mirco T1 - Harmonized tribological testing of polymers in hydrogen N2 - To investigate typical polymer compounds and a potential alternative to be used in hydrogen compressors, tribological tests have been performed with several tribometers in hydrogen atmosphere. The compounds used were a commercially available PEEK matrix with 10 wt-% PTFE, graphite, and short carbon fibers each (supplied by company Polytron), a PPS matrix with 10 wt-% PTFE and graphite (supplied by company MOCOM) and an experimental PA12 matrix with PTFE, chemically coupled with an oleyl alcohol, as additive (supplied by the polymer research institute IPF). For all compounds a steel counter disc (type 316L / 1.4404) with a lapped surface was used in a cylinder on disc setup. The focus of this work is to study the tribological performance of the polymers in hydrogen atmosphere. Additionally, tests were carried out with up to three different tribometers at two institutions. The challenge to compare and harmonize equipment, procedures, and methods is an important part of the study. This naturally includes the determination of the wear volumes of the polymeric cylinders. Furthermore, selected results of the wear and the resulting change in the contact geometry were compared by FEM simulations and an analytical model. T2 - Colloquium H2Safety@BAM, Materials properties and compatibility CY - Online meeting DA - 14.05.2025 KW - Hydrogen KW - Polymers KW - Tribometer KW - Wear KW - Coefficient of Friction KW - Interlaboratory comparison KW - Comparability KW - Harmonisation KW - Standardisation KW - Tribology KW - Oil-coupled compounds PY - 2025 AN - OPUS4-63103 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Clute, C. A1 - Balasooriya, Winoj A1 - Cano Murillo, Natalia A1 - Theiler, Geraldine A1 - Kaiser, A. A1 - Fasching, M. A1 - Schwarz, Th. A1 - Hausberger, A. A1 - Pinter, G. A1 - Schloegl, S. T1 - Morphological investigations on silica and carbon-black filled acrylonitrile butadiene rubber for sealings used in high-pressure H2 applications N2 - Effects of NBR formulations on properties for high-pressure gas systems were tested. Functionalized silica enhances typical properties to a comparable range like CB. The balance of additives results in suitable RGD performance. Silica filled NBR shows lower H2 uptake compared to non-plasticized CB filled NBR. Morphology of CB filled NBR is less affected by H2 than silica filled grades. KW - High-pressure hydrogen gas KW - Sealing KW - Acrylonitrile butadiene rubber KW - Filler-rubber-interaction KW - Rapid gas decompression (RGD) PY - 2024 DO - https://doi.org/10.1016/j.ijhydene.2024.04.133 SN - 0360-3199 VL - 67 SP - 540 EP - 552 PB - Elsevier Ltd. AN - OPUS4-60559 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - Fretting behavior of elastomer materials in hydrogen N2 - This presentation deals with the fretting wear behavior of elastomer materials (two types of cross-linked hydrogenated acrylonitrile butadiene rubbers) against 316L steel ball in hydrogen environment. Furthermore, aging experiments were conducted for 7 days under static conditions in 100 MPa hydrogen. Fretting tests revealed the wear of the polymer decreases with increasing hydrogen pressure. After high pressure hydrogen exposure, the fretting process is characterized by increased adhesion due to elastic deformation, leading to partial slip. T2 - 63rd German Tribology Conference 2022 CY - Göttingen, Germany DA - 26.09.2022 KW - Fretting KW - Rubbers KW - Hydrogen PY - 2022 AN - OPUS4-62082 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kröll, Mirco T1 - Harmonized testing in hydrogen N2 - In this study, the tribological performance of conventional and alternative polymer compounds for compressors was investigated in gaseous hydrogen using several tribometers. The compounds used were a commercial PEEK matrix with 10 wt.% each of PTFE, graphite, and short carbon fibres (Polytron), a PPS matrix with 10 wt.% each of PTFE and graphite (MOCOM), and an experimental PA12 matrix with PTFE, chamically coupled with an oleyl alcohol, as additive (supplied by the polymer research institute IPF). For all compounds a steel counter disc (type 316L / 1.4404) with a lapped surface finish was used in a cylinder-on-disc setup. Next to the tribological performance of the polymer compounds in hydrogen atmosphere, a strong focus of the work was to compare the results obtained with different tribometer setups. The tests were carried out with three different tribometers at two institutions. The challenge to compare and harmonise equipment, procedures, test and evaluation methods was an important part of the study. This includes the determination of the wear volumes of the polymeric cylinders with different wear analysis workflows. Furthermore, selected results of the wear and the resulting change in the contact geometry were compared with an FEM simulation and an analytical model. T2 - 25th International Conference of Wear of Materials CY - Sitges, Spain DA - 14.04.2025 KW - Standardisation KW - Harmonisation KW - Hydrogen KW - Polymers KW - Wear KW - Coefficient of Friction KW - Interlaboratory comparison KW - Tribometer PY - 2025 AN - OPUS4-62992 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - On the way to sustainable and hydrogen compatible sealing materials N2 - In this contribution, the sliding performance of newly formulated polymer materials with improved sustainability are investigated and compared with conventional materials. Tribological tests were performed in hydrogen at ambient temperature as well as cryogenic medium. The samples were arranged in a pin-on-disk configuration with a flat pin sliding against a rotating austenitic steel disk. The friction and wear mechanisms are described and discussed by means of surface analyses. T2 - PolyTrib 2024 CY - Portoroz, Slowenia DA - 03.10.2024 KW - High-performance polymers KW - Sliding wear KW - Hydrogen KW - Cryogenic PY - 2024 AN - OPUS4-61419 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine A1 - Cano Murillo, Natalia A1 - Hashimoto, H. A1 - Aoyagi, A. A1 - Dobbelaar, E. T1 - On the way to sustainable and hydrogen compatible sealing materials N2 - In this contribution, the sliding performance of newly formulated polymer materials with improved sustainability are investigated and compared with conventional materials. Tribological tests were performed in hydrogen at ambient temperature as well as cryogenic medium. The samples were arranged in a pin-on-disk configuration with a flat pin sliding against a rotating austenitic steel disk. The friction and wear mechanisms are described and discussed by means of surface analyses. T2 - PolyTrib 2024 CY - Portoroz, Slowenia DA - 03.10.2024 KW - High-performance polymers KW - Sliding wear KW - Hydrogen KW - Cryogenic PY - 2024 SP - 1 EP - 2 AN - OPUS4-61421 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Sobol, Oded T1 - Metallic materials for the transport and storage of hydrogen N2 - Um die Absorption von Wasserstoff und dessen Verhalten in den Werkstoffen beim Einsatz unter Druck-H2 sowie die H- abhängigen Materialeigenschaften zu definieren, entwickelt die BAM mit ihrer langjährigen Erfahrung adäquate Prüfkonzepte, die einsatzrelevante Bedingungen und reale Beanspruchungen (Temperatur, Wasserstoff und mech. Beanspruchung) hierarchisch berücksichtigen. Der Vortrag gibt eine Einführung in das Thema von wasserstoffunterstützen Materialschäden durch die Problematik der Einspeisung von Wasserstoff in bestehende Erdgasnetze. Ferner wird auf die Hochdruck-Infrastruktur (sowie H2-Tankstellen) und die Entwicklung von Prüfkonzepten für die Gasinfrastruktur unter Druckwasserstoffbeaufschlagung eingegangen. T2 - Die Deutsche Physikalische Gesellschaft (DPG): Veranstaltung der Arbeitsgruppe Senior Expert Netzwerk CY - Berlin, Germany DA - 20.10.2021 KW - Hydrogen Embrittlement KW - Hydrogen assisted cracking KW - Gaseous hydrogen KW - Time-of-Flight Mass Spectrometry KW - Tensile test PY - 2021 UR - https://www.dpg-physik.de/veranstaltungen/2021/mhb-agsen-2021-10-20 AN - OPUS4-53599 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Sobol, Oded T1 - Challenges with metallic materials for the transport and storage of hydrogen N2 - The following presentation provides an overview on some of the challenges with metallic materials used as structural materials in the energy sector for the transport and storage of hydrogen. The presentation contains explanations about the methodologies utilized to characterize the susceptibility of these materials for hydrogen. T2 - Materials and Quality Assurance CY - Bergheim, Germany DA - 10.05.2023 KW - Hollow specimen KW - Slow strain tensile tests KW - Hydrogen assisted cracking PY - 2023 AN - OPUS4-57515 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Konert, Florian T1 - Die Hohlzugprobentechnik als Methodik zur Untersuchung der Materialverträglichkeit N2 - Die Hohlzugprobentechnik wird als Methodik zur Untersuchung der Materialverträglichkeit von metallischen Werkstoffen in Wasserstoffatmosphäre erläutert. T2 - Workshop Wasserstoffverträglichkeit CY - Bonn, Germany DA - 02.03.2023 KW - Wasserstoff KW - Hohlzugprobe KW - Materialkompatibilität KW - SSRT PY - 2023 AN - OPUS4-57171 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kromm, Arne T1 - Die Hohlzugprobentechnik - Eine neue Methodik zur Untersuchung der Materialverträglichkeit unter Wasserstoffeinfluss N2 - Die schädigende Wirkung von Wasserstoff auf die mechanischen Eigenschaften von Stählen ist zwar bekannt, aber noch immer nicht ausreichend erforscht. Die schnelle und sichere Markteinführung von Wasserstofftechnologien macht es erforderlich, dieses Thema genauer zu untersuchen. Im Allgemeinen wird dies oft als Wasserstoffversprödung bezeichnet. Daher ist es wünschenswert, eine Prüfmethode zu entwickeln, die auf einfache Weise die Materialeigenschaften unter Wasserstoffatmosphäre ermitteln kann. Derzeit werden mechanische Prüfungen unter Wasserstoffatmosphäre in Autoklaven durchgeführt. Für diese Technik ist eine aufwendige Hardware erforderlich, daher sind die Prüfungen teuer und die Prüfkapazitäten nur in geringem Umfang verfügbar. Die hier vorgestellte Prüfmethode verspricht einen zukunftsweisenden Ansatz zur Reduzierung von Kosten und Bearbeitungszeiten durch die Verwendung von Hohlkörpern, d.h. die Probe selbst stellt den Autoklav dar. T2 - Sitzung des DIN-Gemeinschaftsarbeitsausschusses NA 092 00 05 GA, NAS/NMP: Zerstörende Prüfung von Schweißverbindungen CY - Berlin, Germany DA - 15.03.2023 KW - Prüfung KW - Wasserstoff KW - Probengeometrie KW - Hochdruck PY - 2023 AN - OPUS4-57168 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröpfer, Dirk T1 - Bericht zum Fortschritt des laufenden Projekts: „Praktikable Prüfung geschweißter Ferngasleitungen aus niedrig-legierten Stählen für den sicheren Transport von Wasserstoff“ N2 - Das Vorhaben untersucht, wie geschweißte Ferngasleitungen aus niedriglegierten und höherfesten Stählen sicher für den Transport von Wasserstoff genutzt werden können. Im Fokus steht, in welchem Maß Wasserstoff unter verschiedenen Druck-, Temperatur- und Gaszusammensetzungen in Werkstoffe und Schweißverbindungen eindringt, deren Duktilität mindert und sprödbrüchiges Versagen verursachen kann. Dafür wird die Prüftechnik der Hohlzugproben in Kombination mit Slow-Strain-Rate-Tests weiterentwickelt, um reale Beanspruchungsbedingungen abzubilden und wirtschaftliche, praxisnahe Prüfungen zu ermöglichen. Untersucht werden insbesondere Schweißnahtgefüge, deren Interaktion, zyklische Belastungen sowie die Übertragbarkeit der Laborergebnisse auf reale Komponenten. Ziel ist ein praktikables Bewertungs- und Qualifizierungskonzept, das die H2-Readiness bestehender und neuer Rohrleitungen beschleunigt und in Normung und Industrieanwendung überführt werden kann. T2 - Herbstsitzung des Fachausschuss "FA 1 Schweißmetallurgie und Werkstoffverhalten" CY - Düsseldorf, Germany DA - 06.11.2025 KW - Wasserstoffversprödung KW - Hohlzugproben KW - Slow-Strain Rate Test KW - Schweißnahtgefüge PY - 2025 AN - OPUS4-65260 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Witte, Julien T1 - Bericht zum Fortschritt des laufenden Projekts: „Praktikable Prüfung geschweißter Ferngasleitungen aus niedrig-legierten Stählen für den sicheren Transport von Wasserstoff“ N2 - Das Vorhaben untersucht, wie geschweißte Ferngasleitungen aus niedriglegierten und höherfesten Stählen sicher für den Transport von Wasserstoff genutzt werden können. Im Fokus steht, in welchem Maß Wasserstoff unter verschiedenen Druck-, Temperatur- und Gaszusammensetzungen in Werkstoffe und Schweißverbindungen eindringt, deren Duktilität mindert und sprödbrüchiges Versagen verursachen kann. Dafür wird die Prüftechnik der Hohlzugproben in Kombination mit Slow-Strain-Rate-Tests weiterentwickelt, um reale Beanspruchungsbedingungen abzubilden und wirtschaftliche, praxisnahe Prüfungen zu ermöglichen. Untersucht werden insbesondere Schweißnahtgefüge, deren Interaktion, zyklische Belastungen sowie die Übertragbarkeit der Laborergebnisse auf reale Komponenten. Ziel ist ein praktikables Bewertungs- und Qualifizierungskonzept, das die H2-Readiness bestehender und neuer Rohrleitungen beschleunigt und in Normung und Industrieanwendung überführt werden kann. T2 - Frühjahrssitzung des Fachausschuss "FA 1 Schweißmetallurgie und Werkstoffverhalten" CY - Hamm, Germany DA - 26.03.2025 KW - Wasserstoffversprödung KW - Hohlzugproben KW - Slow-Strain Rate Test KW - Schweißnahtgefüge PY - 2025 AN - OPUS4-65259 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Sobol, Oded T1 - Challenges with metallic materials in H 2 technologies N2 - Increasing environmental problems with conventional energy technology are stimulating the demand for alternative energy solutions. With air quality reaching catastrophic levels in large cities worldwide, Fuel Cell Electric Vehicles offer the ideal combination of clean power with the amenities of electric drives. Hydrogen use on vehicles, nevertheless, also raises some issues about safe handling. As fuel cells and hydrogen applications, including vehicles, approach technological maturity, developing their business cases becomes crucial in introducing them to the consumer markets. The Joint European Summer School JESS 2021 addresses these issues by offering high quality graduate level courses on selected topics of vehicle technology, innovation & business development, safe handling of hydrogen, and modelling. This series of summer schools has been ongoing since 2004 and targets an audience of university students (MSc and PhD levels) and post-doctoral researchers. We also welcome more experienced researchers and engineers wishing to expand their general knowledge, for instance, to suit a newly acquired position or collect credits for Continuous Professional Development (CPD). The course content is tailored to the needs of a diverse audience: newcomers to the field, experienced students, and young professionals working at the forefront of fuel cell and hydrogen applications. T2 - Joint european summer school (JESS) CY - Online meeting DA - 06.09.2021 KW - Hydrogen Embrittlement KW - Hydrogen assisted cracking KW - Gaseous hydrogen PY - 2021 UR - https://www.jess-summerschool.eu/Week-2 SP - 1 EP - 41 AN - OPUS4-53402 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Reichel, Levin T1 - Reparaturschweißen in der schweißtechnischen Montage: Moderne Schweißverfahren für hochfeste Offshore-Stähle N2 - Der Ausbau der Offshore-Windenergie mit Anlagenleistungen von über 10 MW er-fordert zunehmend den Einsatz hochfester Stähle mit Streckgrenzen ab 460 MPa bei Wanddicken von bis zu 150 mm. Inakzeptable Defekte, die während bzw. nach der schweißtechnischen Montage solcher dickwandigen Verbindungen im Nahtbereich detektiert werden, können wirtschaftlich durch lokales Ausfugen und anschließendes Schweißen noch in der Fertigung repariert werden. Insbesondere bei hochfesten Baustählen stellt dies hohe Anforderungen an die schweißtechnische Fertigung, da bislang keine standardisierten Reparaturkonzepte oder normativen Vorgaben existie-ren. Praxisnahe Empfehlungen sind hier vor allem für kleine und mittlere Unterneh-men (KMU) notwendig, damit diese Reparaturschweißungen sicher und wirtschaft-lich durchführen können. Die laufende Untersuchung (FOSTA P1629/IGF 01IF22746N) legt daher den Schwerpunkt auf die Optimierung der Reparaturverfahren mit dem Ziel, schweißbe-dingte Beanspruchungen zu reduzieren, weil diese häufig zu erneuten Bildung Fehl-stellen führen. Hierfür werden hochfeste, dickwandige Verbindungen aus Offshore-Stahlgüten im Streckgrenzenbereich von 355 MPa bis 460 MPa untersucht. Die ex-perimentellen Analysen berücksichtigen dabei die komplexen Wechselwirkungen zwischen werkstoff- und prozess- sowie konstruktionsbedingten Einflüssen auf den Beanspruchungszustand nach dem Schweißzyklus (Verbindungsschweißen, Ausfu-gen, Reparaturschweißen). Diese Faktoren, wie z. B. die Steifigkeitsverhältnisse der Schweißnaht, sind von entscheidender Bedeutung für die resultierenden Eigenspan-nungen, die sich infolge der schweißtechnischen Reparatur ausbildet. Um die Bau-teilsicherheit und Leistungsfähigkeit zu gewährleisten, sind insbesondere risskriti-sche, mehrachsige Eigenspannungszustände zu vermeiden. So lassen sich moderne Hochleistungs-MAG-Schweißprozesse mit hierfür optimierten, schmaleren Fugen-geometrien in bauteilbezogenen Schweißversuchen auf Großprüfanlagen untersu-chen, um hierfür angepasste Prozess- und Wärmeführungsparameter zu identifizie-ren und angepasste Reparaturkonzepte abzuleiten. Ziel ist es, Handlungsempfehlun-gen für Richtlinien und Normen zu erarbeiten, die das Potenzial hochfester Stähle voll ausschöpfen und die Anwendbarkeit im Offshore-Stahlbau, insbesondere für KMU, substanziell stärken. Auf diese Weise leistet das Projekt einen entscheiden-den Beitrag zur erfolgreichen Umsetzung der Energiewende in Deutschland. T2 - Forschungsseminar OVGU-Magdeburg CY - Magdeburg, Germany DA - 18.06.2025 KW - Moderne Schweißprozesse KW - Offshore KW - Reparaturschweißen KW - Thermisches Ausfugen KW - Eigenspannungen KW - Gefügedegradation PY - 2025 AN - OPUS4-65238 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -