TY - CONF A1 - Grimault de Freitas, Tomás T1 - Comprehensive standardization of the hollow specimen method for tests in high pressure hydrogen gas N2 - As the world moves towards a decarbonised economy, the demand for sustainable and low-carbon alternatives is rapidly increasing. Hydrogen plays an important role in this transition, but in order to make the most of hydrogen as an energy carrier, a comprehensive understanding of its impact on the integrity of structural materials is necessary. Metallic materials, mostly steels, are the most regularly used structural materials in various components throughout the hydrogen supply chain. Ensuring their sustainable and safe use in hydrogen technologies is a crucial factor in the development of the hydrogen economy. This is particularly important since hydrogen can promote crack formation and ultimately lead to premature failure in these materials when combined with mechanical load. This process is commonly known as Hydrogen Embrittlement and can occur in almost all the steels used for the hydrogen technologies. Extensive materials qualification is needed for the rapid implementation of hydrogen technologies, however, most accepted, and standardised test methods for determining the effect of gaseous hydrogen on metallic materials describe complex and costly procedures that are only available to a very limited extent worldwide. The hollow specimen technique is a simple and economical method that has the potential to overcome the limitations of the current methods and complement them for qualifying metallic materials under high-pressure hydrogen gas. In this method, an axial hole is drilled in a tensile specimen, which is then filled with hydrogen gas, sealed, and placed in a standard testing machine. This method requires significantly lower amounts of hydrogen, resulting in fewer safety measures and no need for complex equipment or a specialised laboratory, unlike the conventional autoclave technique. The technique's low investment and testing costs, simple operation, and shorter testing time make it optimal for widespread use around the world, thereby increasing the output of results. Initial studies have demonstrated the feasibility of assessing hydrogen effects in metallic materials using the hollow specimen technique. This led to the establishment of the committee ISO/TC 164/SC 1/WG 9 “Tensile testing, method in high-pressure hydrogen environment“ to standardise the method, however, there are open questions that currently prevent the technique from being standardised for hydrogen testing. These open questions relate to specimen geometry, inner hole surface and gas quality and are being addressed in the H2HohlZug project. Here, the aim is to systematically address and close the gaps towards the standardisation of this technique for tests with hydrogen. This contribution presents the structure and milestones of the project, followed by initial results regarding the optimisation of the specimen geometry, as well as the influence of different manufacturing and finishing processes on the inner hole surface of the hollow specimen and its response to hydrogen effects. T2 - TestXpo | 32nd International Expo for Materials Testing CY - Ulm, Germany DA - 21.10.2024 KW - Hydrogen KW - Hydrogen Embrittlement KW - High-Pressure Gaseous Gas KW - Hollow Specimen Technique KW - H2HohlZug KW - TransHyDE KW - Standardisation KW - Tensile Test PY - 2024 AN - OPUS4-61453 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Grimault de Freitas, Tomás A1 - Konert, Florian A1 - Nietzke, Jonathan A1 - Krzysch, Zephanja A1 - Böllinghaus, Thomas A1 - Michler, Thorsten A1 - Wackermann, Ken A1 - Oesterlin, Heiner A1 - Tlili, Mohamed A1 - Puthur, Alen A1 - Elsen-Humberg, Stephan A1 - Koenigs, Timo A1 - Ruchti, Peter A1 - Systermans, Thomas A1 - Sobol, Oded T1 - Hollow Specimen Method for Tests in High-Pressure Hydrogen Gas: The Role of Strain-Rate and Surface Quality N2 - The feasibility of the method for slow strain tensile tests has been demonstrated in several studies, leading to the establishment of the ISO/TC 164/SC 1/WG 9 ISO committee for its standardisation. Questions have emerged during this process, that currently prevent the method from being standardised for hydrogen testing. These questions relate to specimen geometry, specimen manufacturing and gas quality and are being systematically addressed in the TransHyDE-H2HohlZug project. The first results addressing the questions regarding specimen manufacturing are presented in this poster. T2 - TrasnsHyDE Abschlusskonferenz CY - Berlin, Germany DA - 25.03.2025 KW - Hydrogen KW - Hydrogen Embrittlement KW - Hollow Specimen Technique KW - High-Pressure Gaseous Hydrogen KW - TransHyDE KW - H2HohlZug PY - 2025 AN - OPUS4-62809 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Ekici, Nilsah T1 - Introduction of The SHIMMER Database for Safe Hydrogen Injection in The European Natural Gas Infrastructure N2 - An important step in the transportation strategy for hydrogen is its injection into the existing natural gas grid, which allows accelerating the transition to a low-carbon economy, in other words, hydrogen economy. The European Commission has established hydrogen roadmaps and strategies that emphasize the safe and efficient integration of hydrogen into the natural gas network to support this transition. In line with the objectives of the road map, several funded projects have been established, among others – the Safe Hydrogen Injection Modelling and Management for European Gas Network Resilience (SHIMMER) project. One of the main goals of this project is establishing a database containing a comprehensive repository of information regarding materials, standards, European pilot projects, and operational conditions parameters for the European gas network gathered from open sources as well as transmission and distribution system operators participating in the project. The SHIMMER database has an extensive structure consisting of 262 pipeline entries, each with details such as length, design pressure, inner diameter, and installation year and more. The following contribution elaborates on how the SHIMMER database was established as reliable source of information to be available for the public. The database allows consistent assessments of hydrogen compatibility across different countries, offering a structured framework to help overcome the challenges inherent to the assessments of the components for the injection of hydrogen across Europe. Further, the SHIMMER database provides a valuable information source for future research on the European gas networks. T2 - ICHS 2025 CY - Seoul, South Korea DA - 22.09.2025 KW - Database KW - Hydrogen KW - Gas Grid KW - Low-carbon KW - Pipeline Steel PY - 2025 AN - OPUS4-64288 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Maiwald, Michael T1 - Competence Centre H2Safety@BAM – Safeguarding the Quality Infrastructure in the Hydrogen Economy N2 - Hydrogen is a central component of the energy transition and the European Green Deal for a climate-neutral Europe. To achieve the goals defined for 2050, the EU and the German government have developed a framework for action and are making long-term investments in research, development, and the rapid implementation of innovative hydrogen technologies. With the Competence Centre "H2Safety@BAM", BAM is creating the safety-related prerequisites for the successful implementation of hydrogen technologies at national as well as European level. To this end, BAM conducts research, testing and consulting in a holistic and inter-disciplinary manner under one roof – in the Competence Centre H2Safety@BAM. The activities of the competence centre focus on ensuring the safety of infra-structures, plants, and processes as well as innovative hydrogen transport and storage systems based on digital quality testing and the experimental testing of components and systems. It thus creates the prerequisites for the implementation and adaptation of legal framework conditions as well as for standardization. Closely related to this are investigations into the properties and compatibility of metallic materials and polymers as well as friction systems for the safe operation of components, plants, processes, and systems. This interdisciplinary and holistic approach is complemented by the development of gas analytics and suitable sensors, online measurements of gas properties in process control, test scenarios under real conditions as well as impact assessments of accidents and risk assessments and risk management systems derived from them. With its portfolio of tasks and competences, BAM builds trust in the safety and reliability of technical system solutions for hydrogen. T2 - 772. WE-Heraeus-Seminar - Metrology and Process Safety for Hydrogen Technologies & Applications CY - Bad Honnef, Germany DA - 10.10.2022 KW - H2Safety@BAM KW - Hydrogen KW - Competence Center KW - Hydrogen Strategy KW - Green Deal KW - Safety KW - Risk Assessment KW - Quality Infrastructure PY - 2022 UR - https://www.we-heraeus-stiftung.de/veranstaltungen/metrology-and-process-safety-for-hydrogen-technologies-and-applications/ AN - OPUS4-55986 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Additive manufacturing for components in hydrogen technologies N2 - With the introduction of a hydrogen-based energy and national economy, safety-relevant components for hydrogen technologies are becoming increasingly important. Characteristic of hydrogen technologies are, for example, harsh environmental conditions such as cryogenic or high-pressure storage, corrosion issues in fuel cells and electrolyzers, turbines, and many more. Additive manufacturing of components is becoming increasingly important and irreplaceable for the production of complex technical systems. Using the case studies of burners for gas turbines and electrodes and membranes for polymer (PEMFC) and solid oxide (SOFC) fuel cells, this article shows the potential of additive manufacturing of components. At the same time, however, the challenge of considering divergent mechanical properties depending on the direction of assembly in a "hydrogen-compatible" manner is also highlighted. Finally, the challenges posed by additive manufacturing and hydrogen for materials testing are highlighted under scenarios that are as realistic as possible. T2 - MPA-Workshop Hydrogen CY - Online meeting DA - 10.11.2022 KW - Additive manufacturing KW - Hydrogen KW - Technologies KW - Overview KW - Component PY - 2022 AN - OPUS4-56233 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hickel, Tilmann T1 - Data driven research on hydrogen in metals N2 - The talk gives an overview on data-driven research on hydrogen in metals performed at BAM. The focus is on a ab-initio based high-throughput study on the hydrogen solubility in metals and metallic alloys. Furthermore, the redistribution of hydrogen in transforming microstructures is addressed. The talk ends with an explanation of participant projects in NFDI-MatWerk, motivating the formation of a new project connected to hydrogen technology. T2 - DGM Fachausschuss “Wasserstoffeffekte in Werkstoffen" CY - Saarbrücken, Germany DA - 05.05.2024 KW - Hydrogen KW - Solubility KW - High-throughput study KW - Ab initio simulation KW - NFDI-MatWerk PY - 2024 AN - OPUS4-62721 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hickel, Tilmann T1 - Hydrogen redistribution during electrochemical charging and mechanical testing: insights from a combined ab initio and finite element method N2 - In advanced high strength steels the mechanisms of hydrogen embrittlement are expected to be strongly connected to the amount of retained austenite (RA) contained in the microstructure and its transformation upon deformation. We have developed a multi-scale model for the hydrogen redistribution during hydrogen charging and tensile loading within martensitic/austenitic microstructure. Ab initio simulations have been used to resolve the complex energy profile of hydrogen in the martensite/austenite interface. Representative microstructures with different amounts of RA have been converted form experimental SEM-EBSD measurements. Simulations with the finite element method (FEM) have been used to analyse H concentration profiles within the microstructure. The simulations confirm an accumulation of H within the austenitic phase during charging, which undergoes a phase transformation under applied mechanical load during tensile testing and releases accumulated H into the martensite matrix. As a result, there is a pronounced H segregation to the microstructure regions subjected to high hydrostatic tensile stresses and plastic strains, which has a strong impact on the embrittlement behaviour. T2 - DPG Frühjahrstagung Sektion SKM CY - Berlin, Germany DA - 17.03.2024 KW - Hydrogen KW - Steel KW - Structural transformation KW - Ab initio simulation KW - Multiscale simulation PY - 2024 AN - OPUS4-62726 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hickel, Tilmann T1 - Effect of Hydrogen on the Phase Stability of Steels N2 - In this work, we studied the role of extreme hydrogen concentrations on the relative stability of the fcc/bcc/hcp phases using the ab initio thermodynamics. The results indicate that at low hydrogen chemical potentials the stability of the fcc phase, which can be representative of retained austenite (RA) in steels, is slightly enhanced by the presence of H atoms. In contrast, at high hydrogen chemical potentials the bcc phase is stabilized by H. Moreover, since the excess volume of the hydrogen-rich bcc phase is significantly larger than that of the fcc phase, the presence of a stress field can change the relative stability of these phases in the coexistence regions of the phase diagram. This feature is particularly important for cyclic loading conditions: during loading cycles forward and reverse phase transformations occur and the H released by these transformations can damage the material. T2 - TMS Annual Meeting 2024 CY - Orlando, FL, USA DA - 03.03.2024 KW - Hydrogen KW - Ab initio thermodynamics KW - Multiscale simulation KW - Hydride formation KW - Workflow PY - 2024 AN - OPUS4-62730 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hickel, Tilmann T1 - Fundamental insights into the mechanism of hydrogen embrittlement N2 - The talks starts with a study on H trapping and embrittlement in high-strength Al alloys. Then the phase stability and transformation between different Fe-H phases is discussed, together with implications on crack nucleation. In the last part MD-MC simulation of hydride formation at crack tips in Al alloys are shown. T2 - Integrated Computational Materials, Process and Product Engineering Conference, IC-MPPE CY - Leoben, Austria DA - 06.06.2024 KW - Hydrogen KW - Ab initio thermodynamics KW - Multiscale simulation KW - Hydride formation KW - Cracks PY - 2024 AN - OPUS4-62727 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sreekala, L. A1 - Dey, P. A1 - Hickel, Tilmann A1 - Neugebauer, J. T1 - Unveiling nonmonotonic chemical trends in the solubility of H in complex Fe-Cr-Mn carbides by means of ab initio based approaches N2 - The microstructure of advanced high-strength steels often shows a sensitive dependence on alloying. For example, adding Cr to improve the corrosion resistance of medium-Mn steels also enhances the precipitation of carbides. The current study focuses on the behavior of H in such complex multicomponent carbides by employing different methodological strategies. We systematically analyze the impact of Cr, Mn, and Fe using density functional theory (DFT) for two prototype precipitate phases, M3C and M23C6, where M represents the metal sublattice. Our results show that the addition of these alloying elements yields strong nonmonotonic chemical trends for the H solubility. We identify magnetovolume effects as the origin for this behavior, which depend on the considered system, the sites occupied by H, and short- vs long-range interactions between H and the alloying elements. We further show that the H solubility is directly correlated with the occupation of its nearest-neighbor shells by Cr and Mn. Based on these insights, DFT data from H containing binary-metal carbides are used to design a ridge regression based model that predicts the solubility of H in the ternary-metal carbides (Fe-Cr-Mn-C). KW - Hydrogen KW - High-strength steel KW - Carbide KW - Ab initio KW - Complexity PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-542271 DO - https://doi.org/10.1103/PhysRevMaterials.6.014403 SN - 2475-9953 VL - 6 IS - 1 SP - 1 EP - 14 PB - American Physical Society (APS) CY - College Park, MD AN - OPUS4-54227 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Processing and application properties of multiple principal element alloys (MPEA) N2 - The presentation gives an overview of BAM's activities on processing influences and application properties of MPEAs in the form of joined and machined high and medium entropy alloys (CoCrFeMnNi and CoCrNi). In the case of welding, the focus is on defect-free welded joints with sufficient mechanical properties. In the case of machining, the focus is on the possible influence on the surface quality of the materials through adequate milling parameters. In addition, the hydrogen absorption and diffusion properties as well as the electrochemical corrosion behavior are fundamentally examined. T2 - FAU-Department Werkstoffwissenschaften, Seminar: Aktuelle Probleme der Werkstoffwissenschaften CY - Erlangen, Germany DA - 25.04.2024 KW - Welding KW - Application properties KW - Machining KW - High-entropy alloy KW - Hydrogen PY - 2024 AN - OPUS4-59975 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bayat, Mehmet E. A1 - Huber, C. A1 - Kipphardt, Heinrich A1 - Tiebe, Carlo A1 - Engelhard, Carsten T1 - Towards a sensor-based methodology to determine online calorific values of H2-enriched natural gases in the grid N2 - The German National Hydrogen Strategy (NWS) envisions a transition towards a hydrogen-based energy grid. However, due to the material incompatibility of existing pipeline infrastructure for amounts of hydrogen higher than 10 cmol/mol, many system components of the existing grid must be replaced with significant costs and considerable time investments. Given these constraints, the admixture of hydrogen into natural gas (NG) to create a hydrogen-enriched NG blend has been designated as a transitional technology. The NWS supports this approach on a regional and time-limited basis, but clearly states that it is not intended as a permanent solution. Nevertheless, the conversion to a fully hydrogen-based grid is expected to take several decades. During this transitional phase, precise process analytical monitoring of hydrogen amounts in the NG blend is essential to ensure both energy efficiency via calorific value control and operational safety. These procedures require cost-effective, robust, and reliable sensor technologies capable of real-time, in situ/on-site quantification of hydrogen amounts in NG. In response to this need, we have advanced a physical sensing approach utilizing an oscillating cantilever in collaboration with Truedyne Sensor AG. This sensor system enables quantification of hydrogen amounts, direct calorific value determination as well as display of beneficial gas properties, like density, viscosity, and thermal conductivity. Moreover, the enhanced cantilever system enables direct physical sensing and can also be operated in a quasi-binary mode. We performed comparative evaluations against two benchmark sensor systems to validate the developed technology. One utilizes chemical sensing, and the other operates on thermal conductivity measurements for hydrogen quantification. Through standardized testing, we demonstrated that the cantilever-based sensor offers both high effectiveness and competitive performance compared to current state-of-the-art technologies for accurate hydrogen detection in natural gas and precise determination of its calorific value. T2 - Gas Analysis 2026 CY - Paris, France DA - 27.01.2026 KW - Hydrogen KW - Natural Gas KW - Sensor KW - Calorific Value KW - Grid PY - 2026 AN - OPUS4-65505 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Hydrogen diffusion in creep-resistant 9%-Cr P91 steel weld metal N2 - 9 %-Cr steel P91 is widely used in power plants due to the excellent creep-resistance. Components of this steel are typically welded and demand for careful welding fabrication, whereas a so-called post weld heat treatment (PWHT), must be conducted to increase the toughness and decrease the hardness of the martensitic as-welded (AW) microstructure. Before the PWHT, a hydrogen removal (or dehydrogenation) heat treatment is necessary as hardened AW martensitic microstructure is generally prone to delayed hydrogen assisted cracking (HAC). The microstructure and temperature dependent hydrogen diffusion is an important issue as it determines how long a potential crack-critical hydrogen concentration could remain in the microstructure. In this context, reliable hydrogen diffusion coefficients of P91 weld metal are rare. Hence, the diffusion behavior of P91 multi-layer weld metal was investigated in two different microstructure conditions: AW and further PWHT (760 °C for 4 h). Two different experimental techniques were used to cover a wide range of hydrogen diffusion temperatures: the electrochemical permeation technique (PT) at room temperature and the carrier gas hot extraction (CGHE) for a temperature range from 100 to 400 °C. From both techniques typical hydrogen diffusion coefficients were calculated and the corresponding hydrogen concentration was measured. It was ascertained that both heat treatment conditions show significant differences in hydrogen diffusivity. The biggest deviations were identified for room temperature. In this case, the AW condition shows significant hydrogen trapping and up to seven times lower diffusion coefficients. Additionally, PT investigations showed a preferred diffusion direction of hydrogen in the weld metal expressed by the diffusion coefficients and the permeability for both heat treatment conditions. The CGHE generally revealed lower diffusion coefficients for the AW microstructure up to 200 °C. In addition, the AW condition showed hydrogen concentrations up to 50 ml/100 g (considering electrochemical charging). Nonetheless, this hydrogen was not permanently (reversibly) trapped. Nonetheless, this temperature is approximately 100 °C below recommended dehydrogenation heat treatment (DHT). This has two main consequences: (I) in case of welding is interrupted or no DHT is conducted, a HAC susceptibility of hardened martensitic P91 weld metal cannot be excluded and (II) DHT can be conducted at temperatures around 200 °C below the recommended temperatures. T2 - IIW Annual Assembly, Meeting of Commission IX-C "Creep and heat resistant welds" CY - Bratislava, Slovakia DA - 07.07.2019 KW - Hydrogen KW - Diffusion KW - Weld metal KW - Microstructure KW - Post weld heat treatment PY - 2019 AN - OPUS4-48449 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias T1 - Comparison of ageing behaviour of O-ring seals under hydrogen and air N2 - Elastomeric seals are essential components in the infrastructure which prevent leakage of gas and proper function of technical devices and are therefore highly safety relevant. For proper function a remaining resilience and tolerance to pressure changes is required. The ageing of elastomers is an undesirable but inevitable process leading to a limited lifetime of rubber products such as seals. Independent of the application, as e.g. automotive, piping or container applications, a long lifetime or at least a timely exchange of a seal before occurrence of critical failure is desired. Hydrogen is a key element for the energy turnaround and therefore the compatibility of seals with hydrogen is essential. In addition to the effect of hydrogen uptake and release, which might also cause destructive effects such as rapid gas decompression, ageing at high temperature under hydrogen atmosphere is of interest too. Most of the existing work is addressing the performance of new materials and comprises only very limited investigations concerning long-term use and the behaviour of aged materials in contact with hydrogen. As ageing can lead to substantial changes of material properties, it must be evaluated whether these changes are beneficial or deteriorating for the component function. In this work we present and compare results of the characterisation of three sealing materials (EPDM, HNBR, FKM) after ageing at high temperature under hydrogen and air. Despite the common assumption that ageing under hydrogen atmosphere should be less severe for the material in comparison to air ageing, this is not the case for every material. T2 - RubberCon 2023 CY - Edinburgh, Scotland DA - 09.05.2023 KW - Hydrogen KW - Ageing KW - Seal PY - 2023 AN - OPUS4-58178 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zaghdoudi, M. A1 - Kömmling, Anja A1 - Böhning, Martin A1 - Jaunich, Matthias T1 - Ageing of elastomers in air and in hydrogen environment - A comparative study N2 - EPDM, HNBR and FKM materials were exposed at 150 ◦C to air under atmospheric pressure and to hydrogen at 50 bar for different ageing times. All measurements after hydrogen exposure were conducted on samples in degassed condition to assess irreversible effects resulting from that exposure and to compare them to those after ageing in air. Density, hardness, tensile properties, compression set, and hydrogen permeability of all samples were analysed. In both ageing environments, HNBR exhibited the most significant changes of material properties. However, for both EPDM and HNBR, considerably less severe ageing effects were observed under hydrogen in comparison to ageing in air. On the other hand, FKM showed about the same low level of deterioration in both ageing environments but exhibited poor resistance against damage due to rapid gas decompression in hydrogen environment that can lead to seal failure. The obtained results may serve as a guidance toward a better understanding for design and utilisation of elastomeric materials in future hydrogen infrastructure components. KW - Rapid gas decompression KW - Condensed matter physics KW - Hydrogen KW - Sustainability and the environment KW - Rubber sealing KW - Renewable energy PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-597417 DO - https://doi.org/10.1016/j.ijhydene.2024.03.053 SN - 0360-3199 SN - 1879-3487 VL - 63 SP - 207 EP - 216 PB - Elsevier CY - Oxford AN - OPUS4-59741 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Géraldine T1 - Tribological behavior of polymeric materials in hydrogen N2 - In this talk, an overview of BAM research activities related to Hydrogen is given with a brief presentation of the Competence Center H2Safety@bam. The second part focuses on current projects dealing with the tribological behavior of polymeric materials in Hydrogen. In particular, results regarding the performances of PTFE -free and sustainable materials are given and promising candidates are suggested along with friction mechanisms. T2 - International Hydrogen Energy Development Forum & HYDROGENIUS SYMPOSIUM 2025 CY - Kyushu, Japan DA - 17.12.2025 KW - Hydrogen KW - Friction KW - Wear KW - PTFE-free KW - Sustainable material PY - 2025 AN - OPUS4-65364 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias T1 - Ageing under Hydrogen: effects on O-ring seals N2 - In this work we present results for three typical sealing materials (EPDM, HNBR, FKM) after up to 100 days ageing at high temperature under hydrogen. To allow for a better evaluation of the occurring changes the results are compared with effects of ageing in air on the material properties. Despite the common assumption that ageing under hydrogen atmosphere is expected to be less severe for the material in com-parison to air ageing, this is not seen for every material. T2 - Technomer 2023 CY - Chemnitz, Germany DA - 09.11.2023 KW - Hydrogen KW - Ageing KW - Seal KW - Compression set PY - 2023 AN - OPUS4-58818 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bayat, Mehmet Emin A1 - Kipphardt, Heinrich A1 - Tiebe, Carlo A1 - Tuma, Dirk A1 - Engelhard, Carsten T1 - Trace-Level Ammonia–Water Interactions in Hydrogen: Challenges in Gas Purity Analysis Using Optical-Feedback Cavity-Enhanced Absorption Spectroscopy (OF-CEAS) N2 - Ammonia is a critical impurity in hydrogen fuel due to its irreversible poisoning effect on proton exchange membrane fuel cells. Therefore, international standards (e.g., ISO 14687) set a stringent threshold of 100 nmol/mol. Furthermore, with the growing potential use of ammonia as a hydrogen carrier, its accurate quantification is becoming increasingly important. However, the presence of trace humidity poses analytical challenges, as ammonia may interact with water or interfaces, thereby affecting its detectability. Therefore, the goal of this work is to enable accurate trace ammonia quantification for hydrogen purity measurements through fundamental studies of the methodological challenges. Here, low-pressure sampling (ultra)long-path Optical-Feedback Cavity-Enhanced Absorption Spectroscopy (OF-CEAS) was applied with an effective optical path length of approximately 6.17 km. We studied three average amounts of ammonia: (38.2 ± 0.8) nmol/mol, (74.8 ± 0.7) nmol/mol, and (112.1 ± 1.2) nmol/mol. Furthermore, these amounts were investigated at trace-humidity levels ranging from 0.8 to 8.5 ppmV. We observed a systematic, nonlinear, and humidity-dependent positive measurement bias of up to + (1.0 ± 0.2) nmol/mol at the maximum investigated trace-humidity volume fraction of 8.5 ppmV. This bias was not caused by spectral interference but rather by water-induced accumulation of ammonia within the optical cavity. Moreover, time-resolved measurements in the presence of trace ammonia showed that water desorption follows first-order kinetics, whereas water adsorption followed mixed-order kinetics with an apparent reaction order of 1.57 ± 0.03. Distinct hydration states of surface-bound ammonia were identified, whereas under dry conditions and with increasing amounts of ammonia, enhanced surface adhesion through intermolecular clustering was observed. In addition, the presence of ammonium species within the sorption layer was indirectly confirmed by our experiments. In conclusion, we provide a deeper insight into trace-level ammonia–water interactions and establish a framework for optimizing methodologies, particularly for (ultra)long-path optical gas measurement systems. KW - Ammonia KW - Hydrogen KW - OF-CEAS KW - Humidity KW - Surface Interactions KW - Adsorption PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-643627 DO - https://doi.org/10.1021/acsmeasuresciau.5c00105 SN - 2694-250X SP - 1 EP - 15 PB - American Chemical Society (ACS) AN - OPUS4-64362 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Mair, Georg W. A1 - Bock, Robert A1 - Günzel, Stephan A1 - Gesell, Stephan T1 - Monte-Carlo-Analysis of Minimum Burst Requirements for Composite Cylinders for Hydrogen Service N2 - For achieving Net Zero-aims hydrogen is an indispensable component, probably the main component. For the usage of hydrogen, a wide acceptance is necessary, which requires trust in hydrogen based on absence of major incidents resulting from a high safety level. Burst tests stand for a type of testing that is used in every test standard and regulation as one of the key issues for ensuring safety in use. The central role of burst and proof test is grown to historical reasons for steam engines and steel vessels but - with respect for composite pressure vessels (CPVs) - not due an extraordinary depth of outcomes. Its importance results from the relatively simple test process with relatively low costs and gets its importance by running of the different test variations in parallel. In relevant test und production standards (as e. g. ECE R134) the burst test is used in at least 4 different meanings. There is the burst test on a) new CPVs and some others b) for determining the residual strength subsequent to various simulations of ageing effects. Both are performed during the approval process on a pre-series. Then there is c) the batch testing during the CPVs production and finally d) the 100% proof testing, which means to stop the burst test at a certain pressure level. These different aspects of burst tests are analysed and compared with respect to its importance for the resulting safety of the populations of CPVs in service based on experienced test results and Monte-Carlo simulations. As main criterial for this the expected failure rate in a probabilistic meaning is used. This finally ends up with recommendations for relevant RC&S especially with respect to GTR 13. T2 - 9th International Conference on Hydrogen Safety CY - Online meeting DA - 21.09.2021 KW - Hydrogen KW - Burst test KW - Composite pressure vessels KW - Net zero KW - Monte-Carlo-Analysis PY - 2021 SP - 133 EP - 146 PB - IGEM AN - OPUS4-55668 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bayat, Mehmet A1 - Kipphardt, Heinrich A1 - Tiebe, Carlo A1 - Engelhard, Carsten T1 - Effect of Trace Humidity on Trace Ammonia Quantification N2 - Hydrogen is receiving growing attention as a promising medium for energy storage and transportation. Proton exchange membrane (PEM) fuel cells are a key technology for energy conversion from hydrogen. However, high purity hydrogen is required for this technology, as described in standards such as ISO 14687:2019. A critical impurity that impairs PEM efficiency is ammonia, for which a limit value of 100 nmol/mol applies. In addition, the maximum amount of humidity is specified with 5 µmol/mol. The presence of humidity in hydrogen at levels up to 50 times higher than ammonia raises the critical question of whether ammonia can still be quantified accurately in the lower nmol/mol range without interference from water. In addition, the general question arises as to whether the critical analyte, ammonia, can still be detected at all, given the expected surface effects at such amounts of trace humidity. In this work, we describe the influence of trace humidity on the surface behavior of adsorbed ammonia on stainless steel. Samples with ammonia at approximately 100 nmol/mol in hydrogen, with trace humidity levels ranging from 3 µmol/mol to 10 µmol/mol, were carefully prepared using dynamic mixing. Humidification was conducted using an advanced saturation method. These samples were investigated under atmospheric conditions using low pressure sampling Optical Feedback Cavity Enhanced Absorption Spectroscopy (OFCEAS). From the observed time-dependent signals, kinetics were determined and analyzed, yielding insights on the strength of the adsorption behavior of the analytes. T2 - ANAKON 2025 CY - Leipzig, Germany DA - 10.03.2025 KW - OF-CEAS KW - Hydrogen KW - Ammonia KW - Water KW - Humidity KW - Kinetics KW - Adsorption PY - 2025 UR - https://veranstaltungen.gdch.de/microsite/index.cfm?l=11713&sp_id=2&selSiteID=vplanner AN - OPUS4-64046 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Solberg, S. A1 - Zimmermann, P. A1 - Wilhelmsen, Ø. A1 - Lamb, J. A1 - Bock, Robert A1 - Burheim, O. T1 - Heat to Hydrogen by Reverse Electrodialysis—Using a Non-Equilibrium Thermodynamics Model to Evaluate Hydrogen Production Concepts Utilising Waste Heat N2 - The reverse electrodialysis heat engine (REDHE) is a promising salinity gradient energy technology, capable of producing hydrogen with an input of waste heat at temperatures below 100 °C. A salinity gradient drives water electrolysis in the reverse electrodialysis (RED) cell, and spent solutions are regenerated using waste heat in a precipitation or evaporation unit. This work presents a non-equilibrium thermodynamics model for the RED cell, and the hydrogen production is investigated for KCl/water solutions. The results show that the evaporation concept requires 40 times less waste heat and produces three times more hydrogen than the precipitation concept. With commercial evaporation technology, a system efficiency of 2% is obtained, with a hydrogen production rate of 0.38 gH2 m−2h−1 and a waste heat requirement of 1.7 kWh g−1H2. The water transference coefficient and the salt diffusion coefficient are identified as membrane properties with a large negative impact on hydrogen production and system efficiency. Each unit of the water transference coefficient in the range tw=[0–10] causes a −7 mV decrease in unit cell electric potential, and a −0.3% decrease in system efficiency. Increasing the membrane salt diffusion coefficient from 10−12 to 10−11 leads to the system efficiency decreasing from 2% to 0.6% KW - Non-equilibrium thermodynamics KW - Hydrogen KW - Waste heat KW - RED PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-556677 DO - https://doi.org/10.3390/en15166011 VL - 15 IS - 16 SP - 6011 PB - MDPI AN - OPUS4-55667 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Mair, Georg W. A1 - Günzel, Stephan T1 - The maximum acceptable consequence limit as a control instrument N2 - The presentation starts with the first agreement of making a national attempt for the introduction of a pV-limit for hydrogen transport. It explains aspects of the technical development, provides an impression of catastrophic incidents, and explains the difference between risk control and consequence limitation. Then the process of determining consequences and the result from the discussion at the UN-WG are explained. The next part summarises the approach for counting the number of impacted persons as a function of the model of pressure wave, the pressure peak, the limits of injured persons and the population density. Finally, the latest state of the discussion and the subsequent recommendations for a pV-value and the adequate phrases for explanation are introduced. T2 - 29th BAM-DIN-IGV-DVFG-Meeting CY - Online meeting DA - 23.02.2022 KW - Hydrogen KW - Pressure recepacles KW - Consequence limit KW - Risk control KW - Population density KW - Pressure wave PY - 2022 AN - OPUS4-54608 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Holtappels, Kai T1 - Safety Aspects for Hydrogen Technologies - H2Safety@BAM N2 - Hydrogen is a central component of the energy transition and the European Green Deal for a climate-neutral Europe. To be able to achieve the targets defined by 2045, the EU and the German government have drafted a framework for action and are making long-term investments in research, development and the rapid implementation of innovative hydrogen technologies. The conditions for a successful energy transition and the economic use of green hydrogen as a clean energy carrier are Hydrogen readiness and a rapid market ramp-up, as well as the establishment of the necessary value chains in the national and European framework. Reliable quality and safety standards are the prerequisite for ensuring safety of supply and environmental compatibility and for creating trust in these technologies. BAM has bundled its expertise in the field of hydrogen technologies into a competence center H2Safety@BAM to create confidence in the technology and to support the hydrogen strategies of the German government and the EU. The topic of hydrogen has been current at BAM for more than one hundred years and is also currently the focus of numerous research and cooperation activities. The competence centre H2Safety@BAM and its vision of “We build trust in hydrogen technologies” will be presented with its many safety-related topics, which can be found throughout the entire hydrogen value chain. Two deep dives will present the results on projects dealing with the design-to-cost issue of classical pressurized gas storage containments and the consequences of the release of liquid hydrogen, which will be roughly compared to the release of ammonia. T2 - 25. Kalorimetrietage CY - Braunschweig, Germany DA - 31.05.2023 KW - H2Safety@BAM KW - Safety KW - Hydrogen KW - Gas cylinders KW - DELFIN KW - LH2 KW - Hydrogen release KW - Rapid phase transition KW - Consequences KW - Cyro storage tanks PY - 2023 AN - OPUS4-57629 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - Fretting wear of elastomer materials in hydrogen N2 - This paper presents an experimental study on the fretting wear behavior of two types of cross-linked hydrogenated acrylonitrile butadiene rubbers against 316L steel ball in hydrogen environment. Furthermore, aging experiments were conducted for 7 days under static conditions in 100 MPa hydrogen. The influences of hydrogen pressure as well as the aging exposure on the fretting behavior are discussed by means of surface analyses and well as material properties. T2 - WHEC-2022, 23rd World Hydrogen Energy Conference CY - Istanbul, Turkey DA - 26.06.2022 KW - Rubbers KW - Hydrogen KW - Fretting PY - 2022 AN - OPUS4-62086 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - Polymer tribology in cryogenic hydrogen N2 - In this presentation, an overview of polymer tribology in cryogenic hydrogen is given along comparison with other environments. T2 - Hydrogenius Symposium 2024 CY - Kyushu University Ito Campus, Japan DA - 12.09.2024 KW - Hydrogen KW - Friction KW - Wear KW - Polymer materials KW - Cryogenic PY - 2024 AN - OPUS4-61426 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Drexler, A.-K. A1 - Konert, Florian A1 - Nietzke, Jonathan A1 - Hodžić, E. A1 - Pastore, S. A1 - Domitner, J. A1 - Rhode, Michael A1 - Sommitsch, C. A1 - Böllinghaus, Thomas T1 - Effect of Tensile Loading and Temperature on the Hydrogen Solubility of Steels at High Gas Pressure N2 - The hydrogen solubility in ferritic and martensitic steels is affected by hydrostatic stress, pressure, and temperature. In general, compressive stresses decrease but tensile stresses increase the hydrogen solubility. This important aspect must be considered when qualifying materials for high‐pressure hydrogen applications (e.g., for pipelines or tanks) by using autoclave systems. In this work, a pressure equivalent for compensating the effect of compressive stresses on the hydrogen solubility inside of closed autoclaves is proposed to achieve solubilities that are equivalent to those in pipelines and tanks subjected to tensile stresses. Moreover, it is shown that the temperature effect becomes critical at low temperatures (e.g., under cryogenic conditions for storing liquid hydrogen). Trapping of hydrogen in the microstructure can increase the hydrogen solubility with decreasing temperature, having a solubility minimum at about room temperature. To demonstrate this effect, the generalized law of the hydrogen solubility is parameterized for different steels using measured contents of gaseous hydrogen. The constant parameter sets are verified and critically discussed with respect to the high‐pressure hydrogen experiments. KW - Hydrogen KW - Solubility KW - Temperature KW - Tensile loading KW - Analytical calculation PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-586701 DO - https://doi.org/10.1002/srin.202300493 SN - 1611-3683 SP - 1 EP - 9 PB - Wiley AN - OPUS4-58670 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Drexler, A A1 - Konert, Florian A1 - Sobol, Oded A1 - Rhode, Michael A1 - Domitner, J A1 - Sommitsch, C A1 - Böllinghaus, Thomas T1 - Enhanced gaseous hydrogen solubility in ferritic and martensitic steels at low temperatures N2 - Metals that are exposed to high pressure hydrogen gas may undergo detrimental failure by embrittlement. Understanding the mechanisms and driving forces of hydrogen absorption on the surface of metals is crucial for avoiding hydrogen embrittlement. In this study, the effect of stress-enhanced gaseous hydrogen uptake in bulk metals is investigated in detail. For that purpose, a generalized form of Sievert's law is derived from thermodynamic potentials considering the effect of microstructural trapping sites and multiaxial stresses. This new equation is parametrized and verified using experimental data for carbon steels, which were charged under gaseous hydrogen atmosphere at pressures up to 1000 bar. The role of microstructural trapping sites on the parameter identification is critically discussed. KW - Hydrogen KW - Thermodynamic modelling KW - Pressure-dependent solubility KW - Steel KW - Trapping PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-559307 DO - https://doi.org/10.1016/j.ijhydene.2022.09.109 SN - 0360-3199 VL - 47 IS - 93 SP - 39639 EP - 39653 PB - Elsevier Ltd. AN - OPUS4-55930 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Konert, Florian A1 - Nietzke, Jonathan A1 - Grimault de Freitas, Tomás A1 - Rhode, Michael A1 - Sobol, Oded A1 - Böllinghaus, Thomas T1 - Investigation of resistance to gaseous hydrogen of a longitudinal weld seam in a X65 pipeline using the hollow specimen technique N2 - The constantly increasing demand for renewable energy sources leads to the necessity of transporting large amounts of hydrogen. Since pipelines enable a cost-effective way for the distribution of gaseous hydrogen, the interaction of hydrogen and the pipeline materials must be carefully investigated as hydrogen can cause a degradation of the mechanical properties under certain conditions. Especially welds, which are assumed to be more susceptible to the degradation enhanced by hydrogen, are of great interest. The aim of this study is to investigate the effect of gaseous hydrogen on the mechanical properties of an X65 pipeline, and the longitudinal submerged arc welding (SAW) welded joint. The tests are conducted using the hollow specimen technique on two types of specimens: one extracted from the base material (BM) and the other extracted as a cross-weld (CW) specimen consisting of BM and weld seam. The specimens are charged in situ under a pressure of 60 bar and tested using slow strain rate (SSR) tensile tests with a nominal strain rate of 10−5 s−1. The properties obtained of specimens tested in hydrogen atmosphere are compared to the properties of comparable specimen in inert argon atmosphere as a reference. The performed tests showed a decrease of the reduction of area (RA) from 72% in inert atmosphere to 52% in hydrogen atmosphere for the CW specimen and a decrease from 73% in inert atmosphere to 51% for the BM. Metallographic analyses showed the crack initiation between fine-grained heat-affected zone (FGHAZ) and BM for the specimens tested in hydrogen atmosphere as well as for the reference specimens. This leads to the conclusion that the location of the crack initiation does not change due to the presence of gaseous hydrogen. KW - Hydrogen KW - Hollow specimen technique KW - Pipeline KW - SSRT KW - Hydrogen embrittlement KW - Cross-weld specimen PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-624658 DO - https://doi.org/10.1007/s40194-025-01953-3 SN - 0043-2288 SN - 1878-6669 VL - 69 IS - 3 SP - 861 EP - 870 PB - Springer CY - Berlin AN - OPUS4-62465 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Hydrogen in Welded Microstructures of T24 Steel: Effect on Mechanical Properties and Corresponding Hydrogen Diffusion N2 - Low-alloyed CrMoV steels, such as T24, are widely used for welded components in fossil power stations due to their excellent creep-strength. Spectacular failure cases in the recent years exhibited severe cracking in T24 welds. The results showed that hydrogen-assisted cracking (HAC) occurring up to 200 degree Celsius cannot be excluded. Hence, a basic understanding is necessary on how hydrogen affects the material properties of welded microstructures. In this regard, each weld microstructure (HAZ and weld metal) has influence on the HAC susceptibility and respective hydrogen diffusion. Thus, the present contribution summarizes different results obtained from experiments with grades T24 (CrMoV alloy) and T22 (CrMo) and thermally simulated HAZ. Tensile tests were conducted with hydrogen charged specimens and compared to hydrogen-assisted stress corrosion cracking results obtained from slow strain rate tests (SSRT) up to 200 degree Celsius. Electrochemical permeation and degassing experiments were performed to identify a particular weld microstructure influence on hydrogen diffusion and trapping (especially in the HAZ). The results showed that T24 base material has improved resistance to hydrogen-assisted degradation/cracking. In contrast, the as-welded HAZ had remarkably increased susceptibility (tesnile tests at hydrogen concentration of 1 to 2 ppm). SSRT experiments confirmed this at elevated temperatures for both the T24 and the T22. Hence, the evaluation of a particular degradation of the mechanical properties should be performed independently for each weld microstructure. In addition, the HAZ showed decreased diffusion coefficients (at room temperature) of approximately one magnitude compared to the base materials. Trapped hydrogen was determined in the T24 at temperatures up to 120 degree Celsius compared to 75 degree Celsius in the T22. This has to be considered in case of changing operational temperatures, e.g. in the case of start-up and shutdown processes of boiler components. T2 - 10th Conference on Trends in Welding Research CY - Tokyo, Japan DA - 11.10.2016 KW - Degradation of Mechanical Properties KW - Hydrogen KW - Creep-resistant Steel KW - Weld Joint KW - Diffusion PY - 2016 AN - OPUS4-37827 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Grimault de Freitas, Tomás T1 - Hollow Specimen Method for Tests in High-Pressure Hydrogen Gas: The TransHyDE - H2HohlZug Project N2 - As the world moves towards a decarbonised economy, the demand for sustainable and low-carbon alternatives is growing rapidly. Hydrogen has an important role to play in this transition, but in order to make the most of hydrogen as an energy carrier, a comprehensive understanding of its impact on the integrity of structural materials is necessary. Metallic materials, mainly steels, are the most commonly used structural materials in various components throughout the hydrogen supply chain. Ensuring their sustainable and safe use in hydrogen technologies is a crucial factor in the development of the hydrogen economy. This is particularly important since hydrogen can promote crack formation and ultimately lead to premature failure in these materials when combined with mechanical load. This process is commonly known as Hydrogen Embrittlement and can occur in almost all the steels used for the hydrogen technologies. Extensive materials qualification is required for the rapid implementation of hydrogen technologies, however, most accepted, and standardised test methods for determining the effect of gaseous hydrogen on metallic materials describe complex and costly procedures that are only available to a very limited extent worldwide. The hollow specimen technique is a simple and economical method that has the potential to overcome the limitations of the current methods and complement them for qualifying metallic materials under high-pressure hydrogen gas. Unlike the conventional autoclave technique, this method requires significantly lower amounts of hydrogen, resulting in fewer safety measures and no need for complex equipment or a specialised laboratory. The technique's low investment and testing costs, simple operation, and shorter testing time make it an optimal for widespread use around the world, thereby increasing the output of results. Initial studies have demonstrated the feasibility of assessing hydrogen effects in metallic materials using the hollow specimen technique. This led to the establishment of an ISO committee to standardise the method. However, there are open questions that currently prevent the technique from being standardised for hydrogen testing. These open questions relate to specimen geometry, inner hole surface and gas quality and are being addressed in the H2HohlZug project, of which the overall aim is to systematically close the gaps towards a standard. This contribution presents the structure and milestones of the project, followed by initial results. T2 - TransHyDE Vollversammlung 2025 CY - Leipzig, Germany DA - 26.11.2025 KW - Hydrogen KW - Hydrogen Embrittlement KW - Hollow Specimen Technique KW - High-Pressure Gaseous Hydrogen KW - TransHyDE KW - H2HohlZug KW - Standardisation PY - 2025 AN - OPUS4-64938 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - El Harrab, Hayat A1 - Askar, Enis A1 - Franken, T. A1 - Mauss, F. T1 - Experimental and Kinetic Study of Lubrication Oil Composition on Hydrogen Auto-Ignition N2 - Hydrogen internal combustion engines (H₂ ICEs) present a promising alternative to conventional fuels, but they face challenges such as pre-ignition, where lubricating oils play a critical role. This study investigates the auto-ignition behavior of two base oils — Group II (mineral) and Group V (Ester) — and three formulated oils (Oils A, B, and C) at 20 bar using a heated constant-volume autoclave. Oil A and Oil B share a Group II (mineral) base, with Oil A containing lower levels of calcium-based detergents and higher levels of phosphorus-based antioxidants compared to Oil B. In contrast, Oil C is formulated with a Group V (ester) base oil, incorporating magnesium-calcium detergents. The auto-ignition temperature was measured in both air and stoichiometric hydrogen-air mixtures to assess the influence of oil composition, additives, and hydrogen addition on ignition characteristics. Results show that hydrogen’s AIT at 20 bar is 460°C but drops to 270°C with the addition of 0.2 ml of base oil. Base oils exhibited similar AITs in air (260°C) and hydrogen-air mixtures (270°C), with reactivity differences linked to molecular composition — ester (Group V) displayed lower reactivity compared to mineral oil (Group II). Formulated oils demonstrated slightly higher AITs (up to 290°C), where phosphorus-based additives reduced reactivity, while lower calcium content further slowed ignition. Among the tested oils, the ester-based oil with a mixture of calcium and magnesium detergents exhibited the lowest reactivity, making it a promising candidate for hydrogen engines. Additionally, reduced oxygen availability increased AIT by 10°C and prolonged ignition delay. A chemical analysis was also performed to evaluate the ignition properties of Group II (mineral) and Group V (ester) oils under varying temperatures. These findings highlight the impact of lubricant composition on pre-ignition behavior in H₂ ICEs, offering valuable insights for optimizing lubricant formulations. T2 - 12th European Combustion Meeting CY - Edinburgh, United Kingdom DA - 07.04.2025 KW - Hydrogen KW - Pre-Ignition KW - Group V Ester Oil KW - Auto-Ignition Temperature KW - Additive Effects KW - Ignition Delay Time KW - Group II Mineral Oil KW - Lubricating Oil PY - 2025 AN - OPUS4-64761 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Konert, Florian T1 - Evaluation of hydrogen effect on hardened and annealed 100Cr6 steel N2 - The use of hydrogen demands high safety requirements, since hydrogen can be absorbed by metallic materials and may cause hydrogen embrittlement (HE) under certain conditions. Slow strain rate (SSR) tensile testing is a widespread method to quantify the hydrogen-induced ductility loss of alloys. Here, the hollow specimen technique was used to evaluate the effect of 150 bar hydrogen on the tensile properties of solution annealed and hardened 100Cr6 steel, which is a common material for bearing systems. This technique reduces the required amount of hydrogen and minimizes the duration and costs of the tests performed compared to in-situ tensile tests in autoclaves. T2 - EPRI Workshop on Hydrogen Embrittlement 2024 CY - Oxford, UK DA - 23.06.2024 KW - Hydrogen KW - Hydrogen Embrittlement KW - Hollow Specimen Technique KW - 100Cr6 PY - 2024 AN - OPUS4-60476 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Nietzke, Jonathan T1 - Influence of strain rate on the effect of hydrogen in pre-charged 316L stainless steel: A comparison of conventional and hollow specimen testing N2 - The growing demand for hydrogen requires an expansion of testing capabilities to assess the performance of metallic materials under hydrogen exposure. Considering only gaseous atmospheres, there is a variety of in-situ and ex-situ methods used to investigate the material behavior while or after exposed to hydrogen, respectively. Among these methods, a more conservative one is the in-situ testing at slow strain rates (SSRT) using conventional tensile specimens. While results obtained by a conservative procedure may be more applicable in many cases than those of ex-situ experiments, the tests are quite demanding, leading to limited testing capacities and high costs, especially for very slow strain rates. A possible solution that can enable in-situ testing at relatively low cost is the hollow specimen technique which gained increasing interest in the last decade. The main reasons are the minimal volume of hydrogen required and the elimination of a high-pressure hydrogen autoclave leading to significantly lower costs and enabling more laboratories worldwide to perform these tests. However, interpreting results from hollow specimens, especially when compared to conventional ones, remains a significant challenge. To address this, an experimental study was conducted using conventional and hollow specimens, both uncharged and pre-charged. Pre-charging was achieved using pure hydrogen (5.0, i.e. 99.999 %) at 100 bar and 300 °C for around 21 days. In order to obtain suitable reference specimens, other specimens were stored in argon at 100 bar and 300 °C for the same period of time. The tests were performed at various strain rates, down to 1E-6 1/s. While these ex-situ experiments are not directly comparable to in-situ tests with both types of specimens, they do provide some insights into the differences between the results of hollow and conventional specimens. Therefore, the elongation at fracture and reduction of area (RA) were compared, among other aspects. In addition, fractographical analyses were carried out using SEM images. Elongation at fracture was not significantly affected by hydrogen in conventional specimens, but it was slightly reduced in hollow specimens. RA, on the other hand, was lower for tests with hydrogen in both types of specimens across all strain rates. Moreover, the strain rate did not appear to influence hydrogen embrittlement in conventional specimens whereas in hollow specimens, tests conducted at higher strain rates (1E-4 1/s) showed a greater impact of hydrogen on elongation at fracture than those at lower strain rates (1E-6 1/s), which is contrary to the typical expectation. These findings suggest that the influence of hydrogen differs between conventional and hollow specimens, possibly due to factors such as surface roughness and differing stress states. However, further experiments are needed to fully understand these differences, including in-situ experiments to understand potential differences in hydrogen absorption between the two specimen types. T2 - EPRI Workshop on Hydrogen Embrittlement CY - Oxford, England, United Kingdom DA - 23.06.2024 KW - Stainless steel KW - Hollow specimen KW - Pre-charging KW - Hydrogen PY - 2024 AN - OPUS4-60494 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Röhsler, Andreas A1 - Sobol, Oded A1 - Hänninen, H. A1 - Böllinghaus, Thomas T1 - In-situ ToF-SIMS analyses of deuterium re-distribution in austenitic steel AISI 304L under mechanical load N2 - Hydrocarbons fuel our economy. Furthermore, intermediate goods and consumer products are often hydrocarbon-based. Beside all the progress they made possible, hydrogen-containing substances can have severe detrimental effects on materials exposed to them. Hydrogen-assisted failure of iron alloys has been recognised more than a century ago. The present study aims to providing further insight into the degradation of the austenitic stainless steel AISI 304L (EN 1.4307) exposed to hydrogen. To this end, samples were electrochemically charged with the hydrogen isotope deuterium (2H, D) and analysed by scanning electron microscopy (SEM), electron back-scatter diffraction (EBSD) and time-of-flight secondary ion mass spectrometry (ToF-SIMS). It was found that deuterium caused a phase transformation from the original γ austenite into ε- and α’-martensite. Despite their low solubility for hydrogen, viz. deuterium, the newly formed phases showed high deuterium concentration which was attributed to the increased density of traps. Information about the behaviour of deuterium in the material subjected to external mechanical load was gathered. A four-point-bending device was developed for this purpose. This allowed to analyse in-situ pre-charged samples in the ToF-SIMS during the application of external mechanical load. The results indicate a movement of deuterium towards the regions of highest stress. KW - ToF-SIMS KW - Hydrogen KW - Deuterium KW - AISI 304L KW - EBSD PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-505142 DO - https://doi.org/10.1038/s41598-020-60370-2 VL - 10 IS - 1 SP - 3611 PB - Nature AN - OPUS4-50514 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Nietzke, Jonathan T1 - Evolution of tensile testing methodologies for hydrogen embrittlement in austenitic steels: a comparative study N2 - The energy transition towards hydrogen utilisation has increased the demand for reliable testing methods to evaluate the susceptibility of metallic materials to hydrogen degradation. However, traditional electrochemical pre-charging techniques have limitations in represent-ing realistic gaseous hydrogen exposure conditions. This study presents three comparative analyses of tensile testing methodologies, focusing on the differences between electrochem-ical pre-charging, gaseous pre-charging, and in-situ testing using hollow specimens for aus-tenitic steels AISI 304L and 316L type austenitic steels. Based on the results obtained, the first comparison reveals that electrochemically pre-charged and gaseously pre-charged specimens exhibit different behaviours regarding the impact on the mechanical properties. This effect can be retraced to the varying distribution of hydrogen throughout the specimens. Although comparable embrittlement was observed for similar hydrogen concentrations, the relationship appears to be non-systematic. The second comparison evaluates the performance of pre-charged hollow specimens (300°C, 100 bar, 21 days) in comparison to hollow specimens tested in-situ under 200 bar hydrogen during slow strain rate tensile tests (SSRT). While pre-charged specimens show a slight de-crease in elongation at fracture and a noticeable decrease in reduction of area (RA), in-situ tested specimens exhibit significantly more pronounced embrittlement. This is in accord-ance with the results of Michler et. al. In the third comparison, geometry effects between pre-charged conventional and pre-charged hollow specimens are explored. In this case, the hydrogen effect appears to be of the same order of magnitude for both specimen types, although some differences are ob-served. The study's findings underscore the importance of considering differences between test methods when assessing materials’ compatibility with hydrogen. It specifically emphasises the need for in-situ testing with gaseous hydrogen to better represent real conditions in ap-plications within the hydrogen sector. Furthermore, the study provides an initial compari-son between conventional and hollow specimens, demonstrating their capability to reveal hydrogen effects. However, additional research is essential to enhance the comparability of results yielded by these testing methods. T2 - European Conference on Fracture 2024 CY - Zagreb, Croatia DA - 26.08.2024 KW - Hollow Specimen Technique KW - Hydrogen KW - Austenitic Stainless Steel KW - Hydrogen Testing KW - AISI 316L PY - 2024 AN - OPUS4-60929 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Grimault de Freitas, Tomás T1 - Hollow Specimen Technique for Tests in High-Pressure Hydrogen Gas: The Path Towards Standardisation and the Case Study of a Pipeline Steel and its Weld N2 - The hollow specimen technique is a simple method that has the potential to make material qualification with gaseous pressurized hydrogen widely applicable for the hydrogen industry at low cost. The feasibility of this method has been demonstrated in several studies, leading to the establishment of an ISO committee for its standardization. Questions have emerged during this process, that currently prevent the method from being standardized for hydrogen testing. These questions relate to specimen geometry, specimen manufacturing and gas quality and are being systematically addressed in the TransHyDE-H2HohlZug project. The aim is to close the identified gaps towards the standardization of this method for hydrogen testing. This contribution presents the structure and milestones of the project, followed by the results regarding the influence of specimen production and its response to hydrogen effects. Depending on the production method, different roughness and residual stresses can be expected on the inner hole surface of the specimens. This is of importance since an increase in stress concentration sites have been found to be associated to a higher severity of hydrogen effects. This influence has been investigated after applying the following machining processes: a) drilled only; b) drilled and reamed; c) drilled and honed; d) electro-discharge machining (EDM) and honed; e) EDM and reamed. Roughness measurements using a profilometer, electron back-scatter diffraction (EBSD) analysis and microhardness tests have been performed previous to mechanical testing to infer on the effect of the different production methods on the surface of the inner hole. Next, the specimens were mechanically tested via slow strain rate tensile tests in a argon and in hydrogen, both at 150 bar and room temperature. Here, a strain-rate sensibility analysis was also performed to identify an optimal strain-rate for the mechanical tests. Based on the results an optimal production method is identified and proposed. T2 - ASTM Conference on Hydrogen Materials CY - La Rochelle, France DA - 03.06.2025 KW - Hydrogen KW - Hydrogen Embrittlement KW - Hollow Specimen Technique KW - High-Pressure Gaseous Hydrogen KW - Austenitic Stainless Steel KW - H2HohlZug KW - TransHyDE KW - Tensile Test KW - Pipeline Steel PY - 2025 AN - OPUS4-63329 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Mair, Georg W. A1 - Becker, Ben A1 - Duffner, Eric A1 - John, Sebastian T1 - Storage systems for CGH2- systematic improvement of RC&s composite storage systems for compressed hydrogen - systematic improvement of regulations for more attractive storage units N2 - Hydrogen is an attractive energy carrier that requires high effort for safe storage. For ensuring safety they have to undergo a challenging approval process. Relevant standards and regulations for composite cylinders used for the transport of for on-board storage of hydrogen are currently based on deterministic (e.g. ISO 11119-3) or semi-probabilistic (UN GTR No. 13) criteria. This paper analysis the properties of such methods in regards to the evaluation of load cycle strength. Their characteristics are compared with the probabilistic approach of the BAM. Based on Monte-Carlo simulations, the available design range (mean value and scatter of strength criteria) of current concepts were exemplarily estimated. The aspect of small sample sizes is analysed and discussed with respect to the evaluation procedures. T2 - 10th International Conference on Sustainable Energy and Environmental Protection CY - Bled, Slovenia DA - 27.06.2017 KW - Probabilistic KW - Hydrogen KW - Composite KW - Cylinder KW - Regulations KW - Load cycles KW - GTR 13 KW - ISO 11119 PY - 2017 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-416820 SN - 978-961-286-054-7 DO - https://doi.org/10.18690/978-961-286-054-7 SP - 1 EP - 10 PB - University of Maribor Press CY - Maribor, Slovenia AN - OPUS4-41682 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kehr, Torsten T1 - Project QI-Digital - Quo vadis Use Case H2 Refueling Station? N2 - As a part of the QI-Digital cooperation project, BAM is setting up a hydrogen refuelling station research platform at the Test site for Technical Safety in Horstwalde. Based on this platform, BAM intends to develop, to test and to optimize new measurement techniques as well as data acquisition and processing methods for hydrogen refuelling stations and their periphery in close cooperation with partners from the quality infrastructure and industry. The presentation will introduce the hydrogen refuelling station use case and provide insights into the issues and research goals of the associated subprojects. T2 - H2-Colloquium of the Competence Centre „H2SAFETY@BAM” CY - Online meeting DA - 16.02.2022 KW - Hydrogen KW - Safety KW - QI-Digital PY - 2022 AN - OPUS4-54361 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Tiebe, Carlo T1 - Error prevention, damage prevention, and safety management in hydrogen technologies N2 - This tutorial presents requirements and properties of sensor systems and shows application examples of these technologies for safety and process control for hydrogen technologies. Sensor systems are widely used in hydrogen technologies. The focus is on gas sensors as well as sensors for pressure, temperature, and gas flow. These systems are applied, among other things, for monitoring and control of operating conditions, indication of hazardous conditions and triggering of alarms. To integrate the error avoidance and loss prevention strategy into hydrogen technologies. This includes the implementation of preventive measures as elements of safety management to identify and eliminate potential sources of error. In addition, training should be specifically focused on avoiding errors and the safe use of hydrogen technologies. A well-thought-out strategy for error prevention makes a significant contribution to preventing accidents and increasing overall safety when using hydrogen. T2 - Sensor and Measurement Science International (SMSI) CY - Nuremberg, Germany DA - 06.05.2025 KW - Hydrogen KW - Safety Management KW - Gas Sensors KW - Performance Testing PY - 2025 AN - OPUS4-63280 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Holtappels, Kai T1 - Competence Centre H2Safety@BAM N2 - Deutschland hat mit verschiedenen Ländern Energiepartnerschaften geschlossen, darunter auch mit Japan. Im Rahmen des 3. Treffens der Wasserstoff-Arbeitsgruppe wurde das strategische Vorgehen beider Länder zu Entwicklungen von Wasserstoffrichtlinien, Zertifizierung und Sicherheit vorgestellt und diskutiert. Die BAM hat in einem Vortrag wichtige Themen aus dem Bereich der Sicherheitsforschung sowie zu sicherheitstechnischen Fragestellungen über die Wertschöpfungskette vorgestellt. Außerdem wurde das Arbeitsprogramm und ausgewählte Projekte des Kompetenzzentrums H2Safety@BAM vorgestellt. N2 - Germany has concluded energy partnerships with various countries, including Japan. During the 3rd meeting of the Hydrogen Working Group, the strategic approach of both countries on developments of hydrogen guidelines, certification and safety was presented and discussed. BAM gave a presentation on important topics in the field of safety research and on safety-related issues along the value chain. Furthermore, the work program and selected projects of the competence center H2Safety@BAM were presented. T2 - 3rd Meeting of the Hydrogen Working Group - Japanese-German Energy Partnership CY - Berlin, Germany DA - 27.02.2023 KW - Hydrogen KW - Japanese-German energy partnership KW - Safety KW - H2Safety@BAM PY - 2023 AN - OPUS4-57126 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Holtappels, Kai T1 - Hydrogen - Safety of Energy Carriers N2 - Eine sichere Versorgung mit Energie stellt für moderne Industriegesellschaften eine elementare Grundvoraussetzung dar. Inwieweit in Deutschland die Energiewende im Sinne von zum Beispiel Energiepolitik, Förderung aber auch gesellschaftlicher Entwicklung gestaltet wird, wurde im Rahmen der 12. Wildauer Wissenschaftswoche diskutiert. Die BAM hat einen Beitrag zum Thema Sicherheit von Energieträgern beigetragen und das Kompetenzzentrum H2Safety@BAM vorgestellt. N2 - A safe supply of energy is a fundamental prerequisite for modern industrial societies. The extent to which the energy turnaround is being shaped in Germany in terms of, for example, energy policy, promotion, but also social development was discussed during the 12th Wildau Science Week. BAM contributed to the topic of safety of energy sources and presented the competence center H2Safety@BAM. T2 - 12. Wildauer Wissenschaftswoche CY - Wildau, Germany DA - 27.02.2023 KW - Hydrogen KW - Safety KW - H2Safety@BAM PY - 2023 AN - OPUS4-57125 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kröll, Mirco T1 - Harmonising Tribotests of Polymers in Hydrogen N2 - This talk harmonised methods to investigate friction and wear of commercial and experimental polymer compounds in hydrogen using several tribometers. T2 - Surface Ventures - Symposium on Hydrogen Tribology CY - Online meeting DA - 31.07.2025 KW - Hydrogen KW - Polymers KW - Tribometer KW - Wear KW - Coefficient of Friction KW - Interlaboratory comparison KW - Comparability KW - Harmonisation KW - Standardisation KW - Tribology KW - Oil-coupled compounds KW - FAIR data KW - Database KW - i-TRIBOMAT PY - 2025 AN - OPUS4-63838 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Nattuveettil, Keerthana A1 - Brunner, Nanine A1 - Tiebe, Carlo A1 - Melzer, Michael A1 - Johann, Sergej A1 - Neumann, Patrick P. A1 - Bartholmai, Matthias T1 - Einsatz von Sensortechnologien an einer Wasserstofftankstelle als Beitrag zur digitalen Qualitätsinfrastruktur T1 - Use of sensor technologies at hydrogen test platform as a part of QI Digital N2 - Die Optimierung und Validierung des digitalen Wasserstofftankstellenmanagements mit Sensortechnologien ist das übergeordnete Ziel des Teilprojekts Digitale Qualitätsinfrastruktur mit Sensortechnologien (QIST) am Use Case H2, im Rahmen der digitalen Qualitätsinfrastruktur (QI digital[1]). Hierfür sollen u.a. Sensornetzwerke mit digital-gestützten Auswertungsstrategien intelligent gestaltet werden (Stichwort KI bzw. digitaler Zwilling). Verschiedene, sich ergänzende Sensoren, Systemkomponenten und KI-Methoden stehen als Bausteine intelligenter Sensorsysteme zur Verfügung, mit dem Zweck, die physikalischen und chemischen Parameter an und in Anlagen umfassend und effizient zu überwachen sowie Fehlfunktionen zuverlässig zu detektieren und zu interpretieren, Abbildung 1. Konkrete Arbeitsschritte sind, nach dem Aufbau der Versuchsplattform „Wasserstofftankstelle“, die Instrumentierung von Sensorik und deren digitale Integration in das Tankstellenmanagementsystem sowie die Validierung im Realbetrieb. Die somit erzielten Messergebisse sowie die Messunsicherheiten, Historien und Verfahren werden in digitaler Form aufbereitet, gespeichert und fortlaufend in die KI-basierte Datenauswertung einbezogen, inkl. der Anbindung an die metrologische Rückführungskette. Ziele sind: • Einführung eines neuen messtechnischen Ansatzes und eines digitalen Zwillings für den Anwendungsfall "Wasserstofftankstelle" auf Basis der H2-Sensorik sowie der Zustandsgrößen Druck und Temperatur • Qualitätssicherung durch Applikationen zuverlässiger Gassensorik, Manometer und Thermometer sowie KI-Methoden zur Prozesskontrolle und Detektion von Fehlfunktionen • Nutzung von digitalen Kalibrierscheinen (DCCs) insbesondere für die Messgröße Temperatur zur Realisierung der metrologischen Rückführung in einer digitalen Qualitätsinfrastruktur T2 - Sensorik für die Digitalisierung chemischer Produktionsanlagen CY - Frankfurt a. M., Germany DA - 13.06.2022 KW - QI Digital KW - H2Safety@BAM KW - Wasserstoff KW - Hydrogen KW - Sensorik KW - Digitalisierung KW - Digitalisation PY - 2022 AN - OPUS4-55399 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - Effect of temperature on the friction behaviour of rubber materials in hydrogen N2 - Safety and reliability are the major challenges to face for the development and acceptance of hydrogen technology. It is therefore crucial to study deeply material compatibility, in particular for tribological components that are directly in contact with hydrogen. Some of the most critical parts are sealing components that face high risk of damage due variation of pressure, temperature and mechanical stress. In this study, the friction and wear behaviour of several rubber materials was evaluated in hydrogen environment at ambient and low temperature. Tests were performed against 316L disks in a reciprocation motion. Results reveal that the hydrogen affects the friction and wear behaviour of most materials. The friction mechanism is dominated by deformation for most rubber materials at ambient temperature while sliding occurs at low temperature due to the increased hardness of the rubbers. T2 - Polytrib 2024 CY - Portorož, Slovenia DA - 03.10.2024 KW - Reciprocating sliding KW - Rubber materials KW - Hydrogen KW - Low temperature PY - 2024 AN - OPUS4-62019 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - Effect of high-pressure hydrogen environment on the physical and mechanical properties of elastomers N2 - This presentation deals with the exposure of HNBR rubbers to high pressure hydrogen (100 MPa) at 120 °C for 7 and 21 days under static conditions followed by characterization of their physical and mechanical properties.The core areas include swelling, rapid gas decompression, dynamic mechanical analysis (DMA), tensile strength and compression set properties. This study will assist in expanding the knowledge base of elastomer compatibility with hydrogen and therefore contribute significantly to the selection and development of polymer materials deploying hydrogen as a future energy carrier. T2 - EHEC European Hydrogen Energy Conferecne 2022 CY - Madrid, Spain DA - 18.05.2022 KW - Rubbers KW - Hydrogen KW - Characterization PY - 2022 AN - OPUS4-62084 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Tiebe, Carlo T1 - Sensors for safety and process control in hydrogen technologies N2 - This tutorial provides an overview of the utilization of sensor systems in hydrogen technologies. It discusses the necessary criteria and characteristics of sensor systems, and also demonstrates practical applications of these technologies in terms of safety and process control. Emphasis is placed on various types of sensors such as gas sensors, pressure sensors, temperature sensors, and gas flow sensors. These systems find application in monitoring and regulating operational parameters, detecting potentially dangerous situations, and activating alarm systems. T2 - Sensor and Measurement Science International - SMSI 2023 CY - Nuremberg, Germany DA - 08.05.2023 KW - H2Safety@BAM KW - SensRef KW - Hydrogen KW - Gas sensor KW - Functional safety KW - Uncertainty KW - QI-Digital PY - 2023 AN - OPUS4-57532 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kröll, Mirco T1 - Harmonised tribological testing of polymers in hydrogen N2 - The focus of this work is to study the tribological performance of polymers in hydrogen atmosphere. Additionally, tests were carried out with up to three different tribometers at two institutions. The challenge to compare and harmonise equipment, procedures, and methods is an important part of the study. T2 - PolyTrib 2024 CY - Portoroz, Slovenia DA - 03.10.2024 KW - Hydrogen KW - Tribometer KW - Comparability KW - Harmonisation KW - Oil-coupled compounds PY - 2024 AN - OPUS4-61224 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kröll, Mirco T1 - Tribological performance of polymer compounds in gaseous hydrogen N2 - In this study, friction and wear of conventional and alternative high performance polymer compounds, typically used for components of compressors, were investigated in gaseous hydrogen and nitrogen up to 80 bar of gas pressure. The compounds used were a commercial PEEK matrix with 10 wt.% each of PTFE, graphite, and short carbon fibres, a PPS matrix with 10 wt.% each of PTFE and graphite, and an experimental PA12 matrix with PTFE chemically coupled with an oleyl alcohol. Due to the cylindrical shape of the polymer samples, the contact area and pressure change if wear occurs. Therefore, experimental results of pre-screening tests have been used as input for FEM and an analytical model to determine the decreasing contact pressure over time. Afterwards, the outcome of the models was used to determine the duration of the experiments to reach typical contact pressures of seals in hydrogen compressors. T2 - ASMET TriboCorrosion International Conference 2025 CY - Vienna, Austria DA - 23.10.2025 KW - Hydrogen KW - Polymer KW - Tribometer KW - Comparability KW - Harmonisation KW - Oil-coupled compounds KW - Coefficient of Friction KW - Wear KW - FAIR data KW - Standardisation KW - Tribology KW - Database KW - i-TRIBOMAT PY - 2025 AN - OPUS4-64473 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Theiler, Geraldine A1 - Gradt, Thomas T1 - Comparison of the sliding behavior of several polymers in gaseous and liquid hydrogen N2 - The development of hydrogen technologies entails high safety requirements in distribution and dispensing infrastructure. Therefore, it is necessary to pursue research on material compatibility in hydrogen, especially for critical parts with tribological issues. The focus of this study is to evaluate the influence of hydrogen on a wider range of commercially available polymer materials. Thereby, the friction and wear behavior of different grades of TPE, POM, PA66, PA12, PPA, PEEK, PPS, PTFE, PAI, PI and PBI were investigated against a rotating steel disk (AISI 304). Filled and unfilled polymers from different suppliers were evaluated at room temperature in air, vacuum and hydrogen gas (H2) as well as in liquid hydrogen at - 253°C (LH2). The sliding behavior of the polymer materials is discussed by means of surface analyses, whereby special attention is paid to the formation of a transfer film. According to the results at ambient temperature, the effect of hydrogen environment on the tribological behavior of neat polymers may be related to lack of moisture, but also to saturated hydrocarbons in gaseous hydrogen. In liquid hydrogen, the best tribological performances were achieved with neat PA polymers as well as PPS and PI composites. KW - Polymers KW - Composites KW - Sliding wear KW - Hydrogen KW - Cryogenic temperature PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-597123 DO - https://doi.org/10.2474/trol.18.217 SN - 1881-2198 VL - 18 IS - 5 SP - 217 EP - 231 PB - Japanese Society of Tribologists AN - OPUS4-59712 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine A1 - Gradt, Thomas T1 - Comparison of the sliding behaviour of several polymers in hydrogen N2 - The work presented here deals with the friction and wear behaviour of polymer materials in hydrogen. Commercially available grades of PEEK, PA, PPA, PAI, PI and PBI were investigated at room temperature in air and hydrogen gas (H2) as well as in liquid hydrogen at -253°C (LH2). T2 - 7th World Tribology Congress, WTC 2022 CY - Lyon, France DA - 10.07.2022 KW - Friction KW - Wear KW - Polymers KW - Hydrogen KW - Cryogenic PY - 2021 SP - 1 AN - OPUS4-62089 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -