TY - CONF A1 - Pavlov, V.A. A1 - Zavialov, S.V. A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Development of a measuring technology of strain field in welds N2 - In the article considered the problem of hot cracks occurrence during laser welding process. The main reason of their appearance is strain. The optical method for measuring full field strain locally near the solidification front during laser welding process is proposed. The proposed method of optical measurement allows to determine the real values of the critical strain for various materials characterizing the occurrence of hot cracks in laser welding process. T2 - 20th international conference "Digital signal processing and applications DSPA-2018" CY - Moskau, Russia DA - 28.03.2018 KW - Solidification cracking KW - Critical strain KW - Strain rate KW - Optical measurement KW - Laser welding KW - In situ strain PY - 2018 SN - 978-5-905278-33-4 SP - 749 EP - 754 AN - OPUS4-44910 LA - rus AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Brunner-Schwer, C. A1 - Graf, B. A1 - Rethmeier, Michael A1 - Schreiber, F. T1 - Hybrides Auftragschweißen: Potentiale des laserunterstützten Plasma-Pulver-Auftragschweißens (PTA) N2 - In diesem Beitrag wurden Untersuchungen zu einem neuartigen hybriden Laser-Plasma-Beschichtungsverfahren vorgestellt. Mit dem Ziel, die Produktivität und Wirtschaftlichkeit von Korrosions- und Verschleißschutzschichten zu steigern, wurde das kostengünstige PTA-Verfahren durch einen Laser als zweite Energiequelle ergänzt. Die vorlaufende Laserstrahlung stabilisiert den Plasmalichtbogen und ermöglicht erst eine Auftragsschweißung bei hohen Geschwindigkeiten. Die hohen Auftragraten von 4,2-5,7 kg/h bei gleichzeitig Streckenenergien von 630-720 J/cm zeigen das mögliche Potential des vorgestellten hybriden Ansatzes. In weiteren Untersuchungen muss der Prozess z.B. in Bezug auf die Oberflächenwelligkeit der Beschichtungen über eine Parameteroptimierung weiter verbessert werden. Nach den bisherigen gesammelten Erfahrungen mit dem Hybridprozess ist davon auszugehen, dass durch eine Anpassung der Energiedichteverteilung das Lasers, die Prozessgeschwindigkeiten noch einmal gesteigert werden können. T2 - 12. Fachtagung Verschleissschutz von Bauteilen durch Auftragschweissen CY - Halle, Germany DA - 13.06.2018 KW - Laser- und Lichtbogenenergie PY - 2018 SP - 104 EP - 108 AN - OPUS4-45230 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rethmeier, Michael T1 - Full penetration hybrid laser arc welding of up to 28 mm thick S355 plates using electromagnetic weld pool support N2 - The laser hybrid welding process offers many advantages regarding deep penetration, increased welding velocity and with the help of the supplied filler wire an improved bridgeability to gap and misalignment tolerances. High power laser systems with a power of approx. 30 kW are already available on the market. Nevertheless, multi-layer technology with an arc process is still used for welding of plates from a thickness from 20 mm. A potential cause is the process instability with increasing laser power. It is inevitable that gravity drop-out due to the high hydrostatic pressure at increasing wall thickness especially at welding in flat position and with a low welding speed. The surface tension decreases with increasing root width resulting from low welding velocities. To prevent such inadmissible defects of the seam a use of weld pool support is required. Usual weld pool support systems such as ceramic or powder supports require a mechanical detachment which is time-consuming. The electromagnetic weld pool support system described in this work shows an alternative weld pool support which works contactless. It is based on generating Lorentz forces in the weld pool due to oscillating magnetic field and induced eddy currents. This innovative technology offers single pass welds up to 28 mm in flat position and reduced welding velocity with a laser power of just 19 kW. It also leads to improved mechanical-technological properties of the seams because of the slow cooling rate. With usage of an electromagnetic weld pool support the limitation of the hybrid laser arc welding process in the thick sheet metal will be extend. T2 - 9-th international Conference Beam Technology and Laser Application CY - St. Petersburg, Russia DA - 17.09.2018 KW - Hybrid laser arc welding KW - Electromagnetic support PY - 2018 AN - OPUS4-46290 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bakir, Nasim A1 - Artinov, Antoni A1 - Bachmann, Marcel A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - About the origin of solidification cracking in laser welded thick-walled structures N2 - In this study, a three-dimensional CFD-simulation model was developed to simulate the fluid flow in the weld pool. The CFD-model showed a bulging region in the middle of the depth, which is separated from the top surface and bottom surface by two narrowing regions. It can be concluded that the interaction of the movement of the laser source with the Marangoni vortex leads to a teardrop shape at the upper and bottom surface of the workpiece. Additionally, it shows that the bulging in the weld is a result of the backflows on the upper and lower sides due to the thermo-capillary-driven flows. The weld pool shape was used as a heat source in a two-dimensional thermomechanical model, which allows a highly accurate transformation of the weld pool dimensions obtained from the CFD model. This developed technique allows the consideration of physical aspects, which cannot be considered when using traditional heat sources. The mechanical model has shown that the chronological order of the solidification of the weld has a significant influence on the nature and distribution of the stresses in the weld. High tensile stress has been observed in the bulging region, i.e. in the susceptible region for solidification cracking, when compared to the other narrowing regions, which show compressive stress. T2 - 4th International Conference on Welding and Failure Analysis of Engineering Materials CY - Aswan, Egypt DA - 19.11.2018 KW - Laser beam welding KW - Solidification cracking KW - Numerical simulation KW - Weld pool geometry KW - CFD-model KW - FE-model PY - 2018 SP - W-6, 1 EP - 10 CY - Aswan, Egypt AN - OPUS4-46735 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Siayah, A. A1 - El-Batahgy, A. A1 - Khafagi, S. A1 - Gumenyuk, Andrey A1 - Gook, S. A1 - Rethmeier, Michael T1 - A study on shielded metal arc welding of 9%Ni steel using non-conventional ferritic welding electrode for LNG facilities N2 - The present research work aims at clarification of the effect of the welding electrode type on the mechanical properties of SMA welded joints of 9%Ni steel plates. Properties of produced SMA welded joints were evaluated using different non-destructive and destructive investigation methods. In comparison with the conventionally used Ni-based welding electrode ENiCrMo-3 (AWS A5.11), an experimentally produced non-conventional ferritic welding electrode with 11%Ni (ENi11-Company specification) has resulted in a better combination of the mechanical properties of SMA welded joints of this steel type for critical cryogenic applications. Besides, a positive economic impact for the experimentally produced non-conventional ferritic welding electrode, due to its lower cost, could be another attractive aspect. T2 - 4th International Conference on Welding and Failure Analysis of Engineering Materials CY - Aswan, Egypt DA - 19.11.2018 KW - 9%Ni steel, KW - SMAW KW - Conventional Ni-based austenitic welding electrode KW - Mechanical properties KW - Ferritic welding electrode PY - 2018 SP - W-21, 1 EP - 3 AN - OPUS4-46736 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittner, Andreas A1 - Rethmeier, Michael T1 - Ökologische Bilanzierung von Schmelzschweißverfahren unter Berücksichtigung vor- und nachgelagerter Prozessschritte N2 - In diesem Vortrag werden die aktuellen Forschungsergebnisse im Bereich der ökologischen Bilanzierung von Schweißprozessen dargestellt. Der Fokus liegt hierbei in der Ermittlung relevanter Wirkkategorien zur Charakterisierung der Umweltwirkungen von Schweißprozessen. Exemplarisch für verschiedene Verfahrenskombinationen werden die ökologischen Umweltwirkungen auf Basis eines Life Cycle Assessments ermittelt und verfahrensspezifische Einflussgrößen analysiert. T2 - DVS Fachausschuss 3 "Lichtbogenschweißen" CY - Salzgitter Mannesmann Forschung, Duisburg, Germany DA - 13.03.2018 KW - Life Cycle Assessment (LCA) Schweißprozesse KW - Life Cycle Assessment (LCA) Umweltwirkungen KW - Life Cycle Assessment (LCA) Fusion welding KW - Life Cycle Assessment (LCA) Impact categories PY - 2018 AN - OPUS4-46641 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey A1 - Üstündag, Ö. A1 - Fritzsche, André A1 - Avilov, V. A1 - Rethmeier, Michael T1 - High power laser beam welding of thick materials using EM melt pool control N2 - Electromagnetic weld pool support system is illustrated successfully for hybrid laser arc welding of 20 -30 mm ferromagnetic Steels Welding of thick-walled steels in flat position and reduced welding velocities is possible Gap and misalignment between welded plates can be tolerated by use of this Technology Opportunity to reduce the laser beam power because of reduced welding velocity respectively increase of weldable material thickness with a 20 kW- fibre laser Mechanical properties of welds are in correspondence with requirements of Standards. T2 - SLT 2018 10. Stuttgarter Lasertage CY - Suttgart, Germany DA - 05.06.2018 KW - Hydrostatic and arc pressure exceed the Laplace pressure PY - 2018 AN - OPUS4-45229 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ö. A1 - Avilov, V. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Full penetration hybrid laser arc welding of up to 28 mm thick S355 plates using electromagnetic weld pool support N2 - The laser hybrid welding process offers many advantages regarding deep penetration, increased welding velocity and with the help of the supplied filler wire an improved bridgeability to gap and misalignment tolerances. High power laser systems with a power of approx. 30 kW are already available on the market. Nevertheless, multi-layer technology with an arc process is still used for welding of plates from a thickness from 20 mm. A potential cause is the process instability with increasing laser power. It is inevitable that gravity drop-out due to the high hydrostatic pressure at increasing wall thickness especially at welding in flat position and with a low welding speed. The surface tension decreases with increasing root width resulting from low welding velocities. To prevent such inadmissible defects of the seam a use of weld pool support is required. Usual weld pool support systems such as ceramic or powder supports require a mechanical detachment which is time-consuming. The electromagnetic weld pool support system described in this work shows an alternative weld pool support which works contactless. It is based on generating Lorentz forces in the weld pool due to oscillating magnetic field and induced eddy currents. This innovative technology offers single pass welds up to 28 mm in flat position and reduced welding velocity with a laser power of just 19 kW. It also leads to improved mechanical-technological properties of the seams because of the slow cooling rate. With usage of an electromagnetic weld pool support the limitation of the hybrid laser arc welding process in the thick sheet metal will be extend. KW - Electromagnetic weld pool support KW - Hybrid laser arc welding KW - Thick-walled steel KW - Single pass welding PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-468276 DO - https://doi.org/10.1088/1742-6596/1109/1/012015 SN - 1742-6596 VL - 1109 SP - 1 EP - 7 PB - IOP Publ. AN - OPUS4-46827 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Artinov, Antoni A1 - Bakir, Nasim A1 - Bachmann, Marcel A1 - Gumenyuk, Andrey A1 - Na, S.-J. A1 - Rethmeier, Michael T1 - On the search for the origin of the bulge effect in high power laser beam welding N2 - The shape of the weld pool in laser beam welding plays a major role to understand the dynamics of the melt and its solidification behavior. The aim of the present work was its experimental and numerical investigation. To visualize the geometry of the melt pool in the longitudinal section a butt joint configuration of 15 mm thick structural steel and transparent quartz glass was used. The weld pool shape was recorded by means of a high-speed video camera and two thermal imaging MWIR and VIS cameras. The observations show that the dimensions of the weld pool vary depending on the depth. The regions close to the surface form a teardrop shaped weld pool. A bulge-region and its temporal evolution were observed approximately in the middle of the depth of the weld pool. Additionally, a transient numerical simulation was performed until reaching a steady state to obtain the weld pool shape and to understand the formation mechanism of the observed bulging phenomena. A fixed keyhole with an experimentally obtained shape was used to represent the full-penetration laser beam welding process. The model considers the local temperature field, the effects of phase transition, thermo-capillary convection, natural convection and temperature-dependent material properties up to evaporation temperature. It was found that the Marangoni convection and the movement of the laser heat source are the dominant factors for the formation of the bulging-region. Good correlation between the numerically calculated and the experimentally observed weld bead shapes and the time-temperature curves on the upper and bottom surface were found. T2 - International Congress on Applications of Lasers & Electro-Optics (ICALEO®) CY - Orlando, USA DA - 14.10.2018 KW - Bulging effect KW - High power laser beam welding KW - Numerical modelling KW - Solidification cracking PY - 2019 SP - 1 EP - 8 AN - OPUS4-47139 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Meng, Xiangmeng A1 - Artinov, Antoni A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - A theoretical study of influence of electromagnetic stirring on transport phenomena in wire feed laser beam welding N2 - The additional element from the filler wire in the laser beam welding is usually distributed inhomogeneously in the final weld due to the high solidification rate of weld pool. It has been found that the electromagnetic stirring produced by an external oscillating magnetic field can enhance the material mixing in the weld pool to achieve a more uniform element distribution. However, the magnetic field has a highly non-linear and multi-coupled interaction with the weld pool behavior, which makes the quantitative explanation of the physical mechanism difficult. In this study, the effect of electromagnetic stirring on the transport phenomena in the wire feed laser beam welding is investigated by a numerical modelling. A 3D transient multi-physical model considering the magnetohydrodynamics, heat transfer, fluid flow, keyhole dynamics and element transport is developed. The multiple reflections and the Fresnel absorption of the laser on the keyhole wall are calculated using the ray tracing method. The numerical results show that a Lorentz force produced by the oscillating magnetic field and its induced eddy current gives significant influence on the transport phenomena in the molten pool. The forward and downward flow is enhanced by the electromagnetic stirring, which homogenizes the distribution of the additional elements from a nickel-based filler wire in a steel weld pool. The numerical results show a good agreement with the high-speed images of the molten pool, the fusion line from the optical micrograph and the element distribution from the energy dispersive X-ray spectroscopy. This work provides a physical base for the electromagnetic-controlled laser beam welding and some guidance for the selection of electromagnetic parameters. T2 - ICALEO 2019 CY - Orlando, US DA - 07.10.2019 KW - Magnetohydrodynamics KW - Molten pool dynamics KW - Element transport KW - Laser beam welding PY - 2019 AN - OPUS4-49300 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Artinov, Antoni A1 - Karkhin, V. A1 - Bakir, Nasim A1 - Meng, Xiangmeng A1 - Bachmann, Marcel A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Lamé curves approximation for the assessment of the 3-D temperature distribution in keyhole mode welding processes N2 - A novel approach for the reconstruction of an equivalent volumetric heat source from a known weld pool shape is proposed. It is based on previously obtained weld pool geometries from a steady-state thermo-fluid dynamics simulation. Hereby the weld pool dimensions are obtained under consideration of the most crucial physical phenomena, such as phase transformations, thermo-capillary convection, natural convection and temperature-dependent material properties. The algorithm provides a time and calibration efficient way for the reproduction of the weld pool shape by local Lamé curves. By adjusting their parameters, the identification of the finite elements located within the weld pool is enabled. The heat input due to the equivalent heat source is assured by replacing the detected nodes’ temperature by the melting temperature. The model offers variable parameters making it flexible and adaptable for a wide range of workpiece thicknesses and materials and allows for the investigation of transient thermal effects, e.g. the cooling stage of the workpiece. The calculation times remain acceptably short especially when compared to a fully coupled process simulation. The computational results are in good agreement with performed complete-penetration laser beam welding experiments. T2 - ICALEO 2019 - 38th International congress on applications of lasers & electro-optics CY - Orlando, FL, USA DA - 07.10.2019 KW - Weld pool shape approximation KW - Keyhole mode laser beam welding KW - Numerical simulation KW - Superelliptic Lamé curves PY - 2019 UR - http://icaleo.conferencespot.org/2019-proceedings?qr=1 SN - 978-1-940168-1-42 SP - Paper # Macro 1002 AN - OPUS4-49310 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Artinov, Antoni A1 - Karkhin, V. A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Mathematical modeling of the geometrical differences between the weld end crater and the steady-state weld pool N2 - The geometrical characteristics of the weld end crater are commonly used for the validation of numerical results in welding simulation. A semi-analytical model calculating the cooling stage of the welding process after the moving energy source is turned off has been developed. A solution for various combinations of heat sources and workpieces has been found. The theoretical limits for the heat transfer of the absorbed energy during cooling in a thin plate and a semi-infinite body were studied. It is shown that after turning off the energy source, an additional melting of the base material in longitudinal direction may occur. The developed technique is applied to complete-penetration keyhole laser beam welding of a 2 mm thick austenitic chromium-nickel 316L steel plate at a welding speed of 20 mm/s and a laser power of 2.3 kW. The results show a theoretical increase of the weld end crater length in comparison to the length of the steady-state weld pool of up to 19 %. A shift of the centre of the end crater, in which the solidification of the liquid metal ends, towards the tail of the end crater relative to the axis of the heat source at the time of its termination, was computed. The speed and the direction of crystallization of the molten material in the weld pool and the end crater were found to be different. A good agreement between the computational results and the welding experiments was achieved. T2 - ICALEO 2019 - The International Congress on Applications of Lasers & Electro-Optics (Proceedings) CY - Orlando, FL USA DA - 07.10.2019 KW - Keyhole mode welding KW - Weld pool shape KW - End-crater KW - Heat conduction PY - 2019 UR - http://icaleo.conferencespot.org/2019-proceedings?qr=1 SN - 978-1-940168-1-42 SP - 1 EP - 8 AN - OPUS4-49344 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Artinov, Antoni A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Äquivalente Wärmequellenmodellierung beim Hochleistungslaserstrahlschweißen dicker Bleche N2 - Der vorgestellte Modellierungsprozess dient zur Abschätzung einer geeigneten äquivalenten Wärmequelle und Berechnung des thermischen Verhaltens beim Laserstrahlschweißen. Die Methode Kombiniert die Vorteile von gägngigen Simulationsverfahren und reduziert die berücksichtigte Anzahl an physikalischen Aspekten und Kalibrierungsparameter. Durch die modellierten physikalischen Phänomene konnten die Informationen über die Strömung im Schmelzbad und dessen Einfluss auf die resultierende lokale Temperaturverteilung und folglich auf das transiente Temperaturfeld gewonnen werden. Dadurch wurde die Simulatioszeit(inkl. Kalibrierungsaufwand) auf weniger als einen Tag Rechenzeit verringert. T2 - 38. Assistentenseminar Füge- und Schweißtechnik CY - Rabenau, Germany DA - 06.10.2017 KW - Äquivalente Wärmequelle KW - Bewegtes Gitter KW - Hochleistungslaserstrahlschweißen KW - Prozesssimulation KW - Knotenweise Zwangsbedingungen PY - 2019 SN - 978-3-96144-028-3 VL - 342 SP - 66 EP - 76 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-47699 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Spranger, Felix A1 - Hilgenberg, Kai A1 - Rethmeier, Michael T1 - Anwendung der Laserimplantation zur Strukturierung verschleißgefährdeter Werkzeuge N2 - In einer Vielzahl technischer Anwendungen spielt die Aufrechterhaltung eines definierten Reibungs- und Verschleißverhaltens zwischen bewegten Oberflächen für die Sicherheit und Funktionalität eine ent-scheidende Rolle. Die Oberflächentechnik versucht durch geeignete Verfahren die Randschichten zu ertüchtigen, um Reibung und Verschleiß zu kontrollieren. Eine Verbesserung der Materialeigenschaften kann durch flächige Beschichtungen erreicht werden. Zusätzlich ermöglichen Oberflächenstrukturierun-gen breite Möglichkeiten zur Beeinflussung des Schmierungszustandes bzw. der Kontaktbedingungen. Neben Negativstrukturen bieten ebenfalls erhabene Mikrostrukturen großes Potenzial zur Beeinflussung des tribologischen Verhaltens. Ihr Einsatz ist aber aufgrund der besonderen Verschleißproblematik er-habener Strukturen momentan limitiert, so dass in der Regel zusätzliche verschleißreduzierende Be-schichtungen notwendig werden. In diesem Beitrag wurde das Verfahren der Laserimplantation angewandt, mit dem erhabene und sepa-rierte Oberflächenstrukturen hoher Verschleißfestigkeit in einem Fertigungsschritt erzeugbar sind. Das Verfahren basiert auf einem lokalisierten Dispergieren von Hartstoffpartikeln. Hierfür wurde erstmalig ein gepulster Faserlaser mit hoher Strahlqualität zur Erzeugung punkt- und linienförmiger Mikrostrukturen angewandt. Versuche wurden auf dem Kaltarbeitsstahl X153CrMoV12 unter Anwendung von Titandibo-rid als Hartstoff durchgeführt. Anhand von Härtemessungen konnte gezeigt werden, dass sowohl punkt- als auch linienförmige Strukturen mit Härten über 1000 HV1 und einer feinkörnigen Mikrostruktur mit feinverteilten Hartstoffpartikeln herstellbar sind. Des Weiteren war es möglich, die Implantgeometrien, welche an Querschliffen und durch Weißlichtinterferometeraufnahmen erfasst wurden, durch die Puls-leistung und Pulsdauer zu steuern. T2 - 38. Assistentenseminar Füge- und Schweißtechnik CY - Rabenau, Germany DA - 06.10.2017 KW - Laserimplantation PY - 2019 UR - https://www.dvs-media.eu/de/neuerscheinungen/3646/38.-assistentenseminar-fuegetechnik SN - 978-3-96144-028-3 VL - 342 SP - 24 EP - 34 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-47637 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Fritzsche, André A1 - Hilgenberg, Kai A1 - Rethmeier, Michael T1 - Elektromagnetische Porenreduktion beim Laserstrahlschweißen von Aluminium-Druckgusslegierungen N2 - Innerhalb der vorliegenden Untersuchung wurde ein elektromagnetisches Schmelzbadbeeinflussungssys-tem zur Reduktion des Porenanteils beim Laserstrahlschweißen von Aluminium-Druckguss verwendet. Hierbei wird der Unterschied der elektrischen Leitfähigkeiten zwischen Gas- bzw. Lufteinschlüssen und geschmolzenem Aluminium gezielt genutzt, um die im Schmelzbad eingeschlossenen Poren während des Laserstrahlprozesses zur Oberfläche zu verdrängen. Die dafür erforderlichen Lorentzkräfte werden durch ein oszillierendes Magnetfeld erzeugt. Bei den Laserstrahlschweißversuchen handelt es sich um Ein-schweißungen in Wannenlage (PA-Position) von 6 mm dickem Aluminium-Druckguss AC-AlSi9MnMg. Über einen zuvor optimierten Laserschweißprozess wurde durch zusätzlichen Einsatz eines elektromag-netischen Feldes dessen Wirkung hinsichtlich des Porengehaltes und der Oberflächenrauheit untersucht. Die Auswertung der Schweißnähte erfolgte anhand von Querschliffaufnahmen, Röntgenbildern sowie Computer-Tomographie (CT) Aufnahmen. In Abhängigkeit von der verwendeten magnetischen Fluss-dichte konnte eine Reduktion des Porenanteils von bis zu 75 % erzielt werden, wobei vor allem großvolu-mige Poren erfolgreich aus dem Schmelzbad entfernt werden konnten. Zudem konnte eine Reduktion der Oberflächenrauigkeit von ebenfalls bis zu 75 % erreicht werden. T2 - Assistentenseminar 2017 der Wissenschaftlichen Gesellschaft Fügetechnik e.V. im DVS CY - Rabenau bei Dresden, Sachsen, Germany DA - 06.09.2017 KW - Laserstrahlschweißen KW - Aluminium-Druckguss KW - Auftriebskräfte KW - Elektromagnetische Porenreduktion PY - 2019 SN - 978-3-96144-028-3 VL - 342 SP - 103 EP - 110 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-47622 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gook, Sergej A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Vermeidung von Schweißimperfektionen im Überlappbereich bei laserstrahlhybridgeschweißten Rundnähten N2 - Die Laserstrahl-Hybrid-Schweißtechnologie erweist sich in der schweißtechnischen Fertigung immer mehr als innovative Alternative gegenüber anderen Schweißverfahren. Obwohl das Laserstrahl-Hybridschweißverfahren viele wirtschaftliche Vorteile gegenüber herkömmlichen Schweißverfahren aufweist, wie z.B. große Einschweißtiefe und dadurch eine reduzierte Anzahl von Schweißlagen, geringe thermische Belastung des Grundwerkstoffes aufgrund reduziertem Wärmeeintrag, konnte das Schweißverfahren überwiegend für das Schweißen von Längsnähten demonstriert werden. Eine Vielzahl von Schweißaufgaben, z.B. beim Schweißen von Segmenten von Windkraftanlagen oder dem Orbitalschweißen beim Verlegen von Großrohrleitungen sieht vor, dass die zu schweißenden Bauteile mit einer Rundnaht zusammengefügt werden. Die schweißtechnische Herausforderung ist hier, dass beim Schließen einer Rundnaht mit der Entstehung eines fehlerbehafteten Überlappbereiches zu rechnen ist. Ein zentrales Problem im Überlappbereich einer laserstrahl- sowie laserhybridgeschweißten Rundnaht ist die Bildung von Imperfektionen wie Poren, Rissen sowie die Bildung eines Endkraters, welcher als geometrische Kerbe wirkt. Bisher liegen keine universellen Lösungen zur fehlerfreien Ausführung von geschlossenen Rundnähten beim Laserstrahl-Hybridschweißen vor. Diese Studie befasst sich mit der Entwicklung eines Verfahrens, mit dem die Entstehung von o.g. Schweißimperfektionen vermieden wird. Die Strategie der Prozessführung beim Schließen der Rundnaht sieht hervor, dass ein fehlerfreier Überlappbereich durch die Kontrolle der Erstarrungsbedingungen am Schweißnahtende erreicht werden kann. Die kontrollierte Wärmeführung wird durch eine Anpassung der Parameter von beiden beteiligten Schweißprozessen, dem Laserstrahl- sowie MSG-Schweißprozess realisiert. Im Rahmen dieser Arbeit wurde eine Serie von Schweißversuchen an 9,5 mm dicken Rohabschnitten aus hochfestem Pipelinestahl X100Q mit Variation der Prozessparameter wie der Laserleistung, der Defokussierung des Laserstrahls sowie der Endkraterfüllzeit im Überlappbereich der Rundnaht durchgeführt. Nachfolgend werden die erzielten Ergebnisse dargestellt und diskutiert. T2 - DVS-Studentenkongress 2019 CY - Dusseldorf, Germany DA - 16.09.2019 KW - Laserstrahlschweißen KW - Laserhybridschweißen KW - Rundnaht KW - Endkrater KW - Überlappbereich KW - Defokussierung PY - 2019 SP - 370 EP - 378 AN - OPUS4-49242 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Biegler, M. A1 - Khazan, P. A1 - Gazen, M. A1 - Rethmeier, Michael T1 - Improvement of numerical simulation model setup and calculation time in additive manufacturing-laser-metal-deposition components with an advanced modelling strategy N2 - Rapid localized heating and cooling during additive manufacturing using laser deposition method (LMD) lead to loss of dimensional accuracy as well as cracking of built parts. Finite-Element welding simulations allow prediction of geometrical deviations and accumulated residual stresses as well as their optimization before conducting experiments. Due to the great length of stacked welds, calculation times for fully transient thermomechanical simulations are currently long, the calculation stability suffers from the high number of contact bodies in the model and the modelling effort is high, as the geometries need to be sliced and positioned layer-wise. In this contribution, an integrated modelling approach is demonstrated for a thin-walled LMD component made from 30 layers of 1.4404 (316L) stainless steel: Instead of the layer-by-layer modelling strategy commonly found in the literature, the whole component mesh is kept in one piece and the fully transient, layer-by-layer material deposition is implemented via element sets. In contrast to prior simulations, nonlinear contact between the layers does not have to be considered, significantly decreasing calculation times. The calculated distortions are compared to recently published, in-situ digital image correlation (DIC) measurements as well as numerical simulations conducted with the established layer-wise modelling strategy to judge result quality. Finally, the improvement in calculation time and ease-of-use is compared between both modelling approaches and conclusions regarding future usage for industrial-scale components are drawn. T2 - 12th International Seminar ‘Numerical Analysis of Weldability' CY - Graz, Austria DA - 23.09.2018 KW - Additive Manufacturing KW - Laser Metal Deposition KW - Distortion simulation KW - Calculation time KW - Directed energy deposition KW - Efficient modelling PY - 2019 SN - 978-3-85125-615-4 SN - 978-3-85125-616-1 DO - https://doi.org/10.3217/978-3-85125-615-4-52 SN - 2410-0544 VL - 2019 SP - 979 EP - 1003 PB - Verlag der Technischen Universität Graz CY - Graz AN - OPUS4-49274 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Biegler, M. A1 - Wang, J. A1 - Graf, B. A1 - Rethmeier, Michael T1 - Automated tool-path generation for rapid manufacturing and numerical simulation of additive manufacturing LMD geometries N2 - In additive manufacturing (AM) Laser Metal Deposition (LMD), parts are built by welding layers of powder feedstock onto a substrate. Applications for steel powders include forging tools and structural components for various industries. For large parts, the choice of tool-paths influences the build-rate, the part performance and the distortions in a highly geometry-dependent manner. With weld-path lengths in the range of hundreds of meters, a reliable, automated tool path generation is essential for the usability of LMD processes. In this contribution, automated tool-path generation approaches are shown and their results are discussed for arbitrary geometries. The investigated path strategies are the classical approaches: “Zig-zag-” and “contour-parallel-strategies”. After generation, the tool-paths are automatically formatted into g-code for experimental build-up and ASCII for a numerical simulation model. Finally, the tool paths are discussed in regards to volume-fill, microstructure and porosity for the experimental samples. This work presents a part of the IGF project 18737N “Welding distortion simulation” (FOSTA P1140) T2 - 4th European Steel Technology and Application Days CY - Dusseldorf, Germany DA - 24.06.2019 KW - Additive manufacturing KW - Directed Energy Deposition KW - Path planning KW - DED KW - Mechanical properties KW - Porosity PY - 2019 SP - 1 AN - OPUS4-50045 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - El-Sari, B. A1 - Biegler, M. A1 - Graf, B. A1 - Rethmeier, Michael T1 - Numerische Simulation einer AM-Prozesskette im DED Auftragschweißen N2 - Das DED Auftragschweißen ist ein additives Fertigungsverfahren für Metalle, bei dem das Material schichtweise auf ein Substrat aufgetragen wird. Die schnellen Temperaturzyklen rufen Spannungsgradienten im Bauteil hervor. Der schichtweise Aufbau der Bauteile verursacht eine anisotrope Mikrostruktur. Mittels nachgelagerter Wärmebehandlung können diese Effekte verringert werden. Im anschließenden Schritt der Prozesskette wird das additiv hergestellte Bauteil mittels Drahterodieren von dem Substrat abgetrennt. In diesem Beitrag wird eine thermo-mechanische Simulation der gesamten Prozesskette vorgestellt, welche den additiven Aufbau, Wärmebehandlung und das Abtrennen vom Substrat beinhaltet. Anstelle der in der Literatur üblichen schichtweisen Modellierungsstrategie für die DED Simulation wird das gesamte Bauteil in einem Stück vernetzt und der vollständig transiente, schichtweise Materialauftrag über Elementgruppen realisiert. Im Gegensatz zu früheren Simulationen muss der nichtlineare Kontakt zwischen den Schichten nicht berücksichtigt werden, was die Rechenzeiten deutlich verkürzt. Das Modell wurde validiert mittels Abgleiches des Verzugs aus Simulation und Experiment. Die Proben, bestehend aus DIN 1.4404 (AISI 316L), wurden nach jedem Prozessschritt 3D gescannt um den Verzug zu quantifizieren. Zusätzlich wurden Querschnitte und Härtetests nach Vickers von unterschiedlich behandelten Proben durchgeführt, um den Effekt der Wärmebehandlung auf die Mikrostruktur und die Härte des Bauteils zu untersuchen. T2 - 20. Roundtable Simulating Manufacturing CY - Marburg, Germany DA - 22.05.2019 KW - Numerische ISmulation KW - DED KW - AM KW - Laser-Pulver-Auftragschweißen PY - 2019 SP - 1 EP - 14 AN - OPUS4-50046 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Häberle, Nicolas A1 - Pittner, Andreas A1 - Rethmeier, Michael T1 - Abschlusspräsentation SimCoLas Verbundprojekt -- Arbeitspakete BAM N2 - Die Präsentation gibt einen Überblick bezüglich der von der BAM im Rahmen des SimCoLas Verbundprojekts durchgeführten Arbeiten zum Thema "Photonische Prozessketten". Die numerisch abgebildete Prozesskette Tiefziehen/Laserstrahlschweißen wird darsgestellt und diskutiert. Fokus der Diskussion ist die entwickelte Methodik zur konsistenten Abbildung numerischer Prozessketten mit der Applikation Heissrisskritikalität beim Laserstrahlschweißen. T2 - Verbundprojekt SimCoLas Abschlusstreffen CY - Robert Bosch GmbH Corporate Research Centre, Renningen bei Stuttgart, Germany DA - 13.06.2019 KW - Laserstrahlschweißen KW - Heissrisse KW - Prozesskette PY - 2019 AN - OPUS4-50033 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -