TY - CONF A1 - Petrat, T. A1 - Graf, B. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Build-up Strategies for Laser Metal Deposition in Additive Manufacturing N2 - Laser Metal Deposition (LMD) as a technology for additive manufacturing allows the production of large components outside of closed working chambers. Industrial applications require a stable process as well as a constant deposition of the filler material in order to ensure uniform volume growth and reproducible mechanical properties. This paper deals with the influence of travel path strategies on temperature profile and material deposition. Meandering and spiral hatching strategies are used in the center as well as in the edge of a specimen. The temperature is measured with thermocouples attatched to the backside of the specimen. The tests are carried out on the materials S235JR and 316L. The results show a strong dependence of the maximum temperatures on the travel path strategy and the welding position on the component. T2 - Fraunhofer Direct Digital Manufacturing Conference (DDMC) CY - Berlin, Germany DA - 14.03.2018 KW - Additive Manufacturing KW - Temperature behavior KW - Laser Metal Deposition KW - Stainless Steel KW - 316L KW - Edge effects PY - 2018 SN - 978-3-8396-1320-7 VL - 1 SP - 1 EP - 6 PB - Fraunhofer-Gesellschaft CY - München AN - OPUS4-44719 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pavlov, V.A. A1 - Zavialov, S.V. A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Development of a measuring technology of strain field in welds N2 - In the article considered the problem of hot cracks occurrence during laser welding process. The main reason of their appearance is strain. The optical method for measuring full field strain locally near the solidification front during laser welding process is proposed. The proposed method of optical measurement allows to determine the real values of the critical strain for various materials characterizing the occurrence of hot cracks in laser welding process. T2 - 20th international conference "Digital signal processing and applications DSPA-2018" CY - Moskau, Russia DA - 28.03.2018 KW - Solidification cracking KW - Critical strain KW - Strain rate KW - Optical measurement KW - Laser welding KW - In situ strain PY - 2018 SN - 978-5-905278-33-4 SP - 749 EP - 754 AN - OPUS4-44910 LA - rus AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Rethmeier, Michael A1 - Gumenyuk, Andrey A1 - Bakir, Nasim T1 - Entwicklung eines Verfahrens zur Untersuchung der Heißrissresistenz lasergeschweißter Verbindungen N2 - In den letzten Jahrzehnten hat sich die Strahlschweißtechnik signifikant weiterentwickelt und als effizientes und wirtschaftliches Werkzeug in der Industrie etabliert. Für die Untersuchung der Heißrissresistenz verschiedener Werkstoffe existieren zahlreiche eigen- und fremdbeanspruchende Tests. Diese wurden aber speziell für andere Schweißverfahren, insbesondere das Lichtbogenschweißen, konzipiert. Daher besteht die Notwendigkeit eines geeigneten Heißrisstests, bei dem Werkstoffe realen Strahlschweißbedingungen ausgesetzt werden können. Die Entwicklung sowie die Standardisierung einer aussagekräftigen experimentellen Methode stellen einen wichtigen Schritt auf dem Weg zur Vermeidung von Heißrissen und damit für die Gewährleistung der Sicherheit von gefügten Bauteilen dar. Ziel der Forschungsarbeiten ist es, einen geeigneten Test zur effektiven Untersuchung der Heißrissanfälligkeit von lasergeschweißten Verbindungen zu konzipieren und zu entwickeln. KW - Heißrissresistenz PY - 2016 SN - 978-3-942541-94-7 SP - 1 EP - 110 PB - Verlag und Vertriebsgesellschaft mbH CY - Düsseldorf AN - OPUS4-41846 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pavlov, V. A1 - Gumenyuk, Andrey A1 - Volvenko, S. A1 - Rethmeier, Michael A1 - Bakir, Nasim T1 - Investigation of solidification cracking susceptibility of type 316L stainless steel during laser beam welding using an in-situ observation technique N2 - Laser welding is a widely established manufacturing process in many industry sectors. Solidification cracking as well as the weldability of materials is still since many years a highly contentious issue, particularly regarding the causes of the hot crack formation. Many of studies have been conducted to determine the critical conditions of occurrence of the solidification cracking. In this study a 2D in-situ observation technique in conjunction with laser diodes as the illuminating source has been employed to measure the arising strain field during the laser beam welding process. For the first time the employed technique enabled the in-situ measurement of the transient strain field at the surface of the workpiece directed to the laser beam in the critical range, where the solidification cracking normally occurs. Thus the critical threshold strain values at high temperatures characterizing transition from crack free to crack concomitant welding process could be deduced. T2 - Lasers in Manufacturing Conference 2017 CY - Munich, Germany DA - 26.06.2017 KW - Laser beam Welding KW - Optical measurement technique KW - Critical strain KW - Solidification cracking PY - 2017 SP - 1 EP - 7 AN - OPUS4-41175 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - Hybrid laser arc welding of thick-walled ferromagnetic steels with electromagnetic weld pool support N2 - Electromagnetic weld pool support system is illustrated successfully for hybrid laser arc welding of 20 mm ferromagnetic steels. Welding of thick-walled steels in flat position and reduced welding velocities is possible. Skin depth must be smaller than the plate thickness for protect the electric arc against external oscillating magnetic field. Residual magnetic field has a low influence, the deflection of the arc can be neglected. At high AC frequency more AC power is needed for ideal compensation (Hysteresis losses). T2 - The 70th IIW Annual Assembly and International Conference CY - Shanghai, People's Republic of China DA - 25.06.2017 KW - Electromagnetic weld pool support KW - Hybrid laser arc welding PY - 2017 AN - OPUS4-41259 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - Use of optical measurement technique to investigate the hot cracking sensitivity of 316L during laser beam welding N2 - This technique is the first to provide a measurement of the full strain field locally in the immediate vicinity of the solidification front. Dependency between the external strain rate and the critical local strain has been observed. The local critical strain in vicinity of the solidification front has observed between 3.6 and 4.2%. T2 - The 70th IIW Annual Assembly and International Conference CY - Shanghai, People's Republic of China DA - 25.06.2017 KW - Optical measurment technique KW - Hot crack PY - 2017 AN - OPUS4-41258 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Untersuchungen der Heißrissanfälligkeit laserstrahlgeschweißter Verbindungen austenitischer Stähle N2 - Die lokalen Dehnungen bzw. Dehngeschwindigkeiten im heißrisskritischen Temperaturintervall sind Funktionen des Temperaturfeldes im Nahbereich des Schmelzbades (Schweißverfahren, Werkstoff), der thermo-mechanischen Kennwerte des Versuchswerkstoffes sowie von außen aufgebrachten Verfor-mungen. Da die lokal vorherrschenden Dehnungen im Nahbereich des Schmelzbades nicht bzw. nur mit sehr aufwendigen Methoden ermittelt werden können, dienen bespielweise die im CTW-Test (Controlled Tensile Weldability) von außen aufgebrachten Dehnungen oder Dehnraten als Kriterium für die Heißriss-empfindlichkeit. In dieser Studie wurde CTW-Test zur Untersuchung der Heißrissresistenz verschiedenen austenitischen Stählen eingesetzt. T2 - 36. Assistentenseminar Füge- und Schweißtechnik CY - Brunswick, Germany DA - 05.10.2015 KW - Heißriss KW - Heißrissresistenz KW - Austenitische Stähle KW - CTW-Test PY - 2017 SN - 978-3-945023-57-0 SP - 106 EP - 111 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-41246 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Investigation of solidification cracking susceptibility during laser beam welding using an in-situ observation technique N2 - Using the novel optical measurement technique together with the optical flow algorithm, a twodimensional deformation analysis during welding has been conducted. This technique provides for the first time a measurement of the strain field locally in the immediate vicinity of the assumed solidification front. The described procedure of the opticalmeasurement allows to determine the real martial-dependent values of critical strain and strain rate characterising transition to the hot cracking during laser welding processes. The local critical strain that obtained in the assumed solidification showed that the local critical strain decreases as the strain rate increases. Moreover, this phenomenon has also been shown with results from the CTW-test, since the global strain decreases with an increase in the external strain rate. KW - Novel optical measurement KW - Local critical strain KW - Solidification cracking KW - Laser beam Welding PY - 2017 DO - https://doi.org/10.1080/13621718.2017.1367550 SN - 1362-1718 SP - 1 EP - 7 PB - Taylor & Francis AN - OPUS4-42918 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - Anwendung der Magnettechnik zum Laserstrahlschweißen von dickwandigen Konstruktionen N2 - Elektromagnetische Schmelzbadkontrolle wurde erfolgreich für Laser-MSG-Hybridprozess an einem (ferromagnetischen) 20 mm Baustahl und einem Pipelinestahl eingesetzt. Einlagiges Laserstrahlschweißen von dickwandigen(>20 mm) in PA-Position bei geringeren Schweißgeschwindigkeiten prinzipiell möglich. Reduzierung der Schweißgeschwindigkeit beim Laserstrahlschweißen hat eine Verringerung der notwendigen Laserleistung und eine Verbesserung der mechanisch-technologischen Eigenschaften von Schweißverbindungen zur Folge. T2 - Anwendertreffen Laserverbund Berlin-Brandenburg e.V. CY - Berlin, Germany DA - 17.10.2018 KW - Magnettechnik PY - 2018 AN - OPUS4-43943 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Petrat, T. A1 - Graf, B. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael ED - Witt, G. ED - Eichmann, M. ED - Kniffka, W. T1 - Strategien zur Erreichung eines konstanten Volumenaufbaus bei der additiven Fertigung mittels Laser-Pulver-Auftragschweißen T1 - Strategies to achieve constant build-up with laser metal deposition N2 - Der Einsatz von Hochleistungswerkstoffen verlangt nach einer hohen Endformnähe der zu fertigenden Bauteile, um den Aufwand und somit die Kosten für Materialeinsatz und Nachbearbeitung möglichst gering zu halten. Der additive Einsatz in Form des Laser-Pulver-Auftragschweißens bietet hierfür durch den gezielten Materialauftrag ein hohes Potential. Herausforderungen bestehen in Bereichen der Vorhersagbarkeit und der Reproduzierbarkeit des Materialauftrages, sowie der Fertigungszeit. Unterschiedliche Einflüsse bei der Schichterzeugung führen dabei zu Abweichungen von der Soll-Geometrie. Die vorliegenden Untersuchungen behandeln den Einfluss von Spurgeometrie, Spurüberlappung, Verfahrweg und Aufbaureihenfolge auf die entstehende Bauteilform. Die Teilung einer Lage in Rand- und Kernbereich ermöglicht einen konturangepassten Verfahrweg und eine Erhöhung der Endformnähe innerhalb einer Ebene. Die Verwendung unterschiedlicher Spurgrößen bei der Bauteilerzeugung verdeutlicht die Möglichkeiten einer hohen Auftragsrate bei gleichzeitig hoher Formgenauigkeit. Bereits kleine Unterschiede beim Materialauftrag zwischen Kern- und Randbereichen, Start- und Endpunkten sowie in Bereichen des Richtungswechsels führen aufgrund von Fehlerfortpflanzung nachmehreren Lagen zu Abweichungen in der Aufbaurichtung. Kompensierungen mittels angepasster Baustrategien werden aufgezeigt und diskutiert. Die Nickelbasislegierung Inconel 718, die Titanlegierung Ti-6Al-4V sowie der austenitische Stahl 316L sind Bestandteil der vorliegenden Untersuchungen. Die gewonnenen Erkenntnisse verdeutlichen das Potenzial einer angepassten Aufbaustrategie zur reproduzierbaren Erzeugung von Bauteilen am Beispiel unterschiedlicher Körpergeometrien. T2 - Rapid.Tech International Trade Show & Conference for Additive Manufacturing CY - Erfurt, Germany DA - 14.06.2016 KW - Laser-Pulver-Auftragschweißen KW - Additive Fertigung KW - Aufbaustrategie KW - 3DDruck KW - Ti-6Al-4V KW - Inconel 718 KW - 316L PY - 2016 SN - 978-3-446-45017-2 SP - 49 EP - 60 PB - Carl Hanser Verlag CY - München, Germany AN - OPUS4-36571 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - Novel metrology to determine the critical strain conditions required for solidification cracking during laser welding of thin sheets N2 - The weldability of materials is still for many years a highly contentious issue, particularly regarding the causes of the hot crack formation. Because of the process-related temperature and emissions, direct measurement for the arising strain in the close vicinity of the welding process is challenged. therefore, the externally loaded hot cracking testes remain for decades the only way to determine the critical straining conditions for solidification cracking. In this study, a novel optical two-dimensional in situ observation technique has been developed to analyse the strain evaluation during the welding process in the moment of crack formation. Additionally, the Controlled Tensile Weldability test (CTW test) was used to generate the hot crack under different global straining conditions. To record the welding process and the moment of the solidification crack initiation a CMOS camera was used which inserted coaxially into the optical path of the welding laser. As illumination source a diode laser with wave length 808 nm was employed to illuminate the welding region. An interference filter was placed on the camera lens, allowing only the illumination wavelength to pass through and reflecting all other wavelengths, so that the melt pool and the re-solidifying metal could be visualized in a single image. in order to obtain good temporal resolution, the frame rate of the camera was set to 1100 frame per second in. The contrast in images obtained using this unique setup allows to apply the optical flow technique based on Lucas-Kanade (LK) algorithm to follow the pixels in each image sequence and then to calculate the displacement field. The strain was calculated based on the estimated displacement. Using this technique, the local strains and strain rates under different global straining condition has been determined and analysed. The results shown Dependency between the external strain rate and the critical local strain and strain rate has been observed. That is to say, the critical local strain and strain rate are increased with an increase of the strain rate. Moreover, the described procedure of the optical measurement allows to determine the real martial dependent values of critical strain and strain rate characterizing transition to the hot cracking during laser welding processes.The experiments as well as the measurement has been performed on the stainless steel 316L (1.4404) T2 - 9-th international Conference Beam Technology and Laser Application CY - St. Petersburg, Russia DA - 17.09.2018 KW - Laser welding KW - Novel optical metrology KW - Solidification cracking KW - Stainless steel PY - 2018 AN - OPUS4-46287 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bakir, Nasim A1 - Artinov, Antoni A1 - Bachmann, Marcel A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - About the origin of solidification cracking in laser welded thick-walled structures N2 - In this study, a three-dimensional CFD-simulation model was developed to simulate the fluid flow in the weld pool. The CFD-model showed a bulging region in the middle of the depth, which is separated from the top surface and bottom surface by two narrowing regions. It can be concluded that the interaction of the movement of the laser source with the Marangoni vortex leads to a teardrop shape at the upper and bottom surface of the workpiece. Additionally, it shows that the bulging in the weld is a result of the backflows on the upper and lower sides due to the thermo-capillary-driven flows. The weld pool shape was used as a heat source in a two-dimensional thermomechanical model, which allows a highly accurate transformation of the weld pool dimensions obtained from the CFD model. This developed technique allows the consideration of physical aspects, which cannot be considered when using traditional heat sources. The mechanical model has shown that the chronological order of the solidification of the weld has a significant influence on the nature and distribution of the stresses in the weld. High tensile stress has been observed in the bulging region, i.e. in the susceptible region for solidification cracking, when compared to the other narrowing regions, which show compressive stress. T2 - 4th International Conference on Welding and Failure Analysis of Engineering Materials CY - Aswan, Egypt DA - 19.11.2018 KW - Laser beam welding KW - Solidification cracking KW - Numerical simulation KW - Weld pool geometry KW - CFD-model KW - FE-model PY - 2018 SP - W-6, 1 EP - 10 CY - Aswan, Egypt AN - OPUS4-46735 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Siayah, A. A1 - El-Batahgy, A. A1 - Khafagi, S. A1 - Gumenyuk, Andrey A1 - Gook, S. A1 - Rethmeier, Michael T1 - A study on shielded metal arc welding of 9%Ni steel using non-conventional ferritic welding electrode for LNG facilities N2 - The present research work aims at clarification of the effect of the welding electrode type on the mechanical properties of SMA welded joints of 9%Ni steel plates. Properties of produced SMA welded joints were evaluated using different non-destructive and destructive investigation methods. In comparison with the conventionally used Ni-based welding electrode ENiCrMo-3 (AWS A5.11), an experimentally produced non-conventional ferritic welding electrode with 11%Ni (ENi11-Company specification) has resulted in a better combination of the mechanical properties of SMA welded joints of this steel type for critical cryogenic applications. Besides, a positive economic impact for the experimentally produced non-conventional ferritic welding electrode, due to its lower cost, could be another attractive aspect. T2 - 4th International Conference on Welding and Failure Analysis of Engineering Materials CY - Aswan, Egypt DA - 19.11.2018 KW - 9%Ni steel, KW - SMAW KW - Conventional Ni-based austenitic welding electrode KW - Mechanical properties KW - Ferritic welding electrode PY - 2018 SP - W-21, 1 EP - 3 AN - OPUS4-46736 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Avilov, Vjaceslav A1 - Fritzsche, André A1 - Bachmann, Marcel A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Full penetration laser beam welding of thick duplex steel plates with electromagnetic weld pool support N2 - Full penetration high power bead-on-plate laser beam welding tests of up to 20 mm thick 2205 duplex steel plates were performed in PA position. A contactless inductive electromagnetic (EM) weld pool support system was used to prevent gravity drop-out of the melt. Welding experiments with 15 mm thick plates were carried out using IPG fiber laser YLR 20000 and Yb:YAG thin disk laser TruDisk 16002. The laser power needed to achieve a full penetration was found to be 10.9 and 8.56kW for welding velocity of 1.0 and 0.5 m min(-1), respectively. Reference welds without weld pool support demonstrate excessive root sag. The optimal value of the alternating current (AC) power needed to completely compensate the sagging on the root side was found to be approximate to 1.6 kW for both values of the welding velocity. The same EM weld pool support system was used in welding tests with 20 mm thick plates. The laser beam power (TRUMPF Yb:YAG thin disk laser TruDisk 16002) needed to reach a full penetration for 0.5 m min(-1) was found to be 13.9 kW. Full penetration welding without EM weld pool support is not possible-the surface tension cannot stop the gravity drop-out of the melt. The AC power needed to completely compensate the gravity was found to be 2 kW. (C) 2016 Laser Institute of America T2 - ICALEO 2015 - 34th International congress on applications of lasers & electro-optics CY - Atlanta, GA, USA DA - 2015-10-18 KW - Electromagnetic weld pool support KW - Laser beam welding KW - Duplex stainless steel PY - 2015 SN - 978-1-940168-05-0 SP - 571 EP - 579 PB - Amer inst physics CY - Melville, NY, USA AN - OPUS4-35035 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey A1 - Üstündag, Ö. A1 - Fritzsche, André A1 - Avilov, V. A1 - Rethmeier, Michael T1 - High power laser beam welding of thick materials using EM melt pool control N2 - Electromagnetic weld pool support system is illustrated successfully for hybrid laser arc welding of 20 -30 mm ferromagnetic Steels Welding of thick-walled steels in flat position and reduced welding velocities is possible Gap and misalignment between welded plates can be tolerated by use of this Technology Opportunity to reduce the laser beam power because of reduced welding velocity respectively increase of weldable material thickness with a 20 kW- fibre laser Mechanical properties of welds are in correspondence with requirements of Standards. T2 - SLT 2018 10. Stuttgarter Lasertage CY - Suttgart, Germany DA - 05.06.2018 KW - Hydrostatic and arc pressure exceed the Laplace pressure PY - 2018 AN - OPUS4-45229 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gook, S. A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Verfahren zum fehlerfreien Laserstrahl-MSG-Hybridschweißen geschlossener Rundnähte N2 - In diesem Beitrag werden Ergebnisse der Untersuchungen eines Verfahrens zum fehlerfreien Laserstrahl-MSG-Hybridschweißen von geschlossenen Rundnähten vorgestellt. Das Verfahren zielt auf die Vermeidung von Schweißnahtunregelmäßigkeiten im Überlappbereich einer hybridgeschweißten Rundnaht. Eine Strategie der Prozessführung beim Schließen der Rundnaht wurde entwickelt, mit der ein fehlerfreier Überlappbereich durch die Kontrolle der Erstarrungsbedingungen am Schweißnahtende erreicht wird. Die kontrollierte Wärmeführung wird durch eine Anpassung der Parameter von beiden beteiligten Schweißprozessen, dem Laserstrahl sowie dem Metallschutzgas (MSG)-Schweißprozess, realisiert. Experimentelle Untersuchungen wurden an 12 bis 15 mm dicken Rohrabschnitten durchgeführt. Der Einfluss von Prozessparametern wie der Veränderung des Abbildungsmaßstabs und der Defokussierung des Laserstrahls auf die Erstarrungsbedingungen am Ende der Rundnaht wurde untersucht, um eine optimale Strategie zum Herausführen der Prozessenergie zu finden. Im Rahmen der experimentellen Untersuchungen konnte gezeigt werden, dass eine Defokussierung des Laserstrahls im Bereich zwischen 60 mm und 100 mm über einen kurzen Auslaufbereich der Naht von etwa 15 mm zu einer deutlich besseren Nahtausbildung im Überlappbereich führt. Es konnte eine günstige kelchförmige Schweißnaht ohne eine Tendenz zur Rissbildung erzielt werden. Die Laseroptik mit motorisch angesteuertem Linsensystem ermöglichte dabei eine Vergrößerung des Laserstrahldurchmessers ohne eine Veränderung der Position des MSG-Lichtbogens relativ zur Bauteiloberfläche. KW - Hybrid welding KW - Laser beam welding KW - Pipe manufacturing KW - As-shielded arc welding KW - Weld defects PY - 2021 VL - 73 IS - 3 SP - 116 EP - 121 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-52365 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - Influence of an external applied AC magnetic field on the melt pool dynamics at high-power laser beam welding N2 - The study deals with the determination of the influence of an externally applied oscillating magnetic field on the melt pool dynamics in high power laser beam and hybrid laser arc welding processes. An AC magnet was positioned under the workpiece which is generating an upward directed electromagnetic force to counteract the formation of the droplets. To visualise the melt flow characteristics, several experiments were carried out using a special technique with mild steel from S355J2 with a wall thickness of up to 20 mm and a quartz glass in butt configuration. The profile of the keyhole and the melt flow were recorded with a high-speed camera from the glass side. Additionally, the influence of the magnetic field orientation to the welding direction on the filler material dilution on laser hybrid welding was studied with variating oscillation frequency. The element distribution over the whole seam thickness was measured with X-ray fluorescence (XRF). The oscillation frequency demonstrated a greater influence on the melt pool dynamics and the mixing of the elements of the filler wire. The high-speed recordings showed, under the influence of the magnetic field, that the melt is affected under strong vortex at the weld root, which also avoids the formation of droplets T2 - The 18th Nordic Laser Materials Processing Conference CY - Lulea, Sweden DA - 18.01.2022 KW - Laser beam welding KW - Melt pool dinamics PY - 2022 AN - OPUS4-54331 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jokisch, T. A1 - Gook, S. A1 - Marko, A. A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Laserstrahlschweißen additiv gefertigter Bauteile: Einsetzbarkeit bestehender Bewertungsvorschriften N2 - Bei der additiven Fertigung im Pulverbett ist die Bauteilgröße durch den Bauraum begrenzt. Das Verbindungsschweißen additiv gefertigter Teile bietet eine Möglichkeit diese Größenbegrenzung aufzuheben. Aufgrund des spezifischen Spannungs- und Gefügezustands im additiv aufgebauten Teil ist jedoch unklar, inwiefern bestehende Bewertungsvorschriften des Verbindungsschweißens auch für Schweißnähte an additiv gefertigten Bauteilen geeignet sind. Dies wird anhand des Laserstrahlschweißens additiv gefertigter Rohrverbindungen untersucht. Die Schweißnähte werden mittels visueller Prüfung, metallografischer Untersuchungen sowie Computertomografie ausgewertet. Die festgestellten Fehlerarten sind vergleichbar zu konventionellen Bauteilen. Dies ist ein Indikator dafür, dass bestehende Bewertungsvorschriften die möglichen auftretenden Defekte auch für Schweißnähte an additiven Bauteilen abbilden. KW - Schweißunregelmäßigkeiten KW - Additive Fertigung KW - Laserstrahlschweißen KW - Schweißeignung PY - 2021 VL - 73 IS - 3 SP - 132 EP - 137 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-53575 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Thermal Cycles and Charpy Impact Toughness of Single-Pass Hybrid Laser-Arc Welded Thick-Walled Structures N2 - The study deals with the influence of the heat input on the thermal cycles and Charpy impact toughness for hybrid laser-arc welding of 25 mm thick structural steel S355J2 using a 20-kW high-power laser in combination with an electromagnetic weld pool support. The main focus is on the change of the mechanical properties over the entire seam thickness. The cooling times were measured using a pyrometer in combination with an optical fibre in three different locations near to fusion lines corresponding to different heights of the seam. Also, Charpy impact specimens were taken from different parts of the weld joint corresponding to the different heights. The influence of the heat input was investigated for 1.8 kJ mm-1 and 3.2 kJ mm-1. Despite the observed decreased values of both t8/5-cooling time and the Charpy impact toughness in the root part of the seam, the required values could be reached in dependance on applied heat input. T2 - Lasers in Manufacturing Conference 2021 CY - Online meeting DA - 21.06.2021 KW - laser hybrid welding KW - Charpy impact toughness KW - thick plate welding KW - thermal cycles PY - 2021 SP - 1 EP - 8 AN - OPUS4-53926 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Straße, Anne A1 - Gumenyuk, Andrey A1 - Scheuschner, Nils A1 - Altenburg, Simon A1 - Pignatelli, Giuseppe A1 - Gornushkin, Igor B. A1 - Baensch, Franziska A1 - Rethmeier, Michael T1 - In-situ Prozessüberwachung beim Laser-Pulver-Auftragschweißen (LPA) mittels Thermografie, optischer Emissionsspektroskopie (OES) und Schallemissionsanalyse (SEA) N2 - Vor allem in den letzten Jahren ist das Interesse der Industrie an der additiven Fertigung deutlich gestiegen. Die Vorteile dieser Verfahren sind zahlreich und ermöglichen eine ressourcenschonende, kundenorientierte Fertigung von Bauteilen, welche zur stetigen Entwicklung neue Anwendungsbereiche und Werkstoffe führen. Aufgrund der steigenden Anwendungsfälle, nimmt auch der Wunsch nach Betriebssicherheit unabhängig von anschließenden kostenintensiven zerstörenden und zerstörungsfreien Prüfverfahren zu. Zu diesem Zweck werden im Rahmen des von der BAM durchgeführten Themenfeldprojektes „Prozessmonitoring in Additive Manufacturing“ verschiedenste Verfahren auf ihre Tauglichkeit für den in-situ Einsatz bei der Prozessüberwachung in der additiven Fertigung untersucht. Hier werden drei dieser in-situ Verfahren, die Thermografie, die optische Emissionsspektroskopie und die Schallmissionsanalyse für den Einsatz beim Laser-Pulver-Auftragschweißen betrachtet. T2 - 41. Assistentenseminar der Füge- und Schweißtechnik CY - Magdeburg, Germany DA - 02.09.2020 KW - Laser-Pulver-Auftragschweißen (LPA) KW - Thermographie KW - Optische Emissionsspektroskopie (OES) KW - Schallemissionsanalyse (SEA) PY - 2021 SN - 978-3-96144-141-9 VL - 370 SP - 132 EP - 140 PB - DVS MEdia CY - Düsseldorf AN - OPUS4-53967 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Altenburg, Simon A1 - Maierhofer, Christiane A1 - Straße, Anne A1 - Gumenyuk, Andrey T1 - Comparison of MWIR thermography and high-speed NIR thermography in a laser metal deposition (LMD) process N2 - Additive manufacturing (AM) offers a range of novel applications. However, the manufacturing process is complex and the production of defect-free parts with high reliability and durability is still a challenge. Thermography is a valuable tool for process surveillance, especially in metal AM processes. The high process temperatures allow one to use cameras usually operating in the visible spectral range. Here, we compare the results of measurements during the manufacturing process of a commercial laser metal deposition setup using a mid-wavelength-IR camera with those from a visual spectrum high-speed camera with band pass filter in the near-IR range. T2 - Conference QIRT 2018 CY - Berlin, Germany DA - 25.06.2018 KW - Additive manufacturing KW - Laser metal deposition KW - ProMoAM KW - Thermography PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-454993 UR - http://www.qirt.org/archives/qirt2018/papers/p35.pdf DO - https://doi.org/10.21611/qirt.2018.p35 SP - 1 EP - 5 PB - QIRT Council CY - Quebec, Canada AN - OPUS4-45499 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - Investigation of the gap bridgeability at high-power laser hybrid welding of plasma-cut thick mild steels with AC magnetic support N2 - One of the challenges of the high-power hybrid laser welding of thick steels is the sensitivity of the process of the process to manufacturing tolerances. This usually leads to a time-consuming preparation of the welding edges, such as milling. The study deals with the influence of the edge quality of milled and plasma-cut steel made of S355J2 with a wall thickness of 20 mm on the laser hybrid welded seam quality. Furthermore, the gap bridgeability and the tolerances towards edge misalignment was investigated. An AC magnet was used as backing support to prevent sagging and positioned under the workpiece, to generate an upwards directed electromagnetic pressure. The profiles of the edges and the gap on the top and root side were measured using a digital camera. Single-pass laser hybrid welds of plasma-cut edges could be welded using a laser beam power of just 13.7 kW. A gap bridgeability up to 2 mm and misalignment of edges up to 2 mm could be achieved successful. Additionally, the independence of the cutting side and the welding side was shown, so that samples were welded to the opposite side to their cutting. For evaluation of internal defects or irregularities, X-ray images were carried out. Charpy impact strength tests were performed to determine the toughness of the welds. T2 - X International Conference «Beam Technologies in Welding and Materials Processing» CY - Odessa, Ukraine DA - 7.09.2021 KW - Laser beam welding KW - Hybrid laser arc welding KW - Material transport PY - 2021 AN - OPUS4-53569 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - Improvement of the mechanical properties and corrosion resistance of laser welds on thick duplex plates by laser cladded buttering N2 - Because of its excellent corrosion resistance, high tensile strength and high ductility, duplex stainless steel 2205 offers many areas of application. Though laser beam welding accompanied by high cooling rates, duplex steels tend to perform higher ferrite contents in weld metal as the base metal, which leads to a reduction of ductility and corrosion resistance of the weld joint. To overcome this problem, a solution, based on buttering the plate edges by laser metal deposition (LMD) with material containing higher Ni concentrations prior to laser welding was suggested. In this context different process parameters for LMD and different mixtures of duplex and nickel powder, were investigated. In a second step the possibility of welding those edges defect free while achieving balanced austenite-ferrite ratio was verified with metallographic analysis, Electron Backscatter Diffraction (EBSD) and impact testing according to Charpy. The improved corrosion resistance was observed with ASTM G48 standard test method. T2 - X International Conference «Beam Technologies in Welding and Materials Processing» CY - Odessa, Ukraine DA - 7.09.2021 KW - Laser beam welding KW - Laser metal deposition KW - Duplex steels PY - 2021 AN - OPUS4-53568 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Meng, Xiangmeng A1 - Artinov, Antoni A1 - Bachmann, Marcel A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - A numerical study on the suppression of a detrimental weld pool profile in wire feed laser beam welding by magnetohydrodynamic technique N2 - The weld quality and the possible defect formation are directly determined by the weld pool shape and the thermo-fluid dynamics therein. In this paper, an untypical weld pool profile, i.e., elongated at its top and bottom but narrowed at the middle, is found experimentally and numerically in the wire feed laser beam welding. The detrimental influence of the weld pool narrowing on the element transport is analyzed and discussed. A magnetohydrodynamic technique is utilized to suppress the narrowing, aiming at a more homogenous element distribution. It is found that a low-temperature region is formed in the middle of the weld pool due to the interaction of the two dominant circulations from the top and bottom regions. The weld pool is significantly narrowed due to the untypical growth of the mushy zone in the low-temperature region, which results in a direct blocking effect on the downward flow and the premature solidification in the middle region. The Lorentz force produced by a transverse oscillating magnetic field shows the potential to change the flow pattern into a single-circulation type and the low-temperature-gradient region is mitigated. Therefore, the downward transfer channel is widened, and its premature solidification is prevented. The numerical results are well validated by experimental measurements of metal/glass observation and X-ray fluorescence element mapping. T2 - 13th International Seminar Numerical Analysis of Weldability CY - Seggau, Austria DA - 04.09.2022 KW - Thermo-fluid flow KW - Element transport KW - Laser beam welding KW - Magnetohydrodynamics KW - Multi - physical modeling PY - 2023 SN - 2410-0544 VL - 13 SP - 143 EP - 160 PB - Verlag der Technischen Universität Graz AN - OPUS4-58806 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Brunner-Schwer, C. A1 - Knöfel, F. A1 - Gook, S. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Laserstrahlhybridschweissen von Türmen für Windkraftanlagen Ökonomische und ökologische Vorteile N2 - Das Laserstrahlhybridschweißen ist beim Schweißen von Türmen für Windkraftanlagen eine Alternative zum Unterpulverschweißen von Dickblechen in Mehrlagentechnik und bietet hier ökonomische und ökologische Vorteile. Der industrielle Einsatz des Verfahrens ist jedoch durch prozessspezifische Herausforderungen eingeschränkt. Die im Beitrag beschriebene kontaktlose elektromagnetische Badstütze dient zur Erweiterung des Verfahrenspotenzials im Dickblechbereich >15 mm. KW - Elektromagnetische Badstütze KW - Laserhybridschweißen KW - Windkraftanlagen KW - Ökonomische und ökologische Vorteile PY - 2022 VL - 7 SP - 340 EP - 347 PB - DVS Media GmbH AN - OPUS4-56372 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - Determination of critical local straining conditions for solidification cracking at laser beam welding by experimental and numerical methods N2 - The phenomenon of solidification cracking has been the subject of numerous research projects over the years. Great efforts have been made to understand the fundamentals of hot cracking. It is generally agreed that solidification cracks form in the solidification range between the liquidus and solidus temperatures under the combination of thermal, metallurgical and mechanical factors. There is still a need to determine the time-resolved strain distribution in the cracksensitive region in order to analyse the local critical conditions for solidification cracking phenomena. This was a strong motivation for the development of a measurement system used in this study to estimate the local strains and strain rates in the zone where the solidification crack is expected to occur. The laser beam welding experiments were conducted using the Controlled-Tensile-Weldability test (CTW test) to apply an external strain condition during welding to generate solidification cracks. The CTW test is a test method for investigating the suscep�tibility of laser-welded joints to solidification cracking, in which the sample can be subjected to a defined strain at a defined strain rate during welding. In combination with experimental investigations, numerical simulations provide spatially detailed and time-dependent information about the strain development during the welding process, especially regarding the critical conditions for solidification cracking. Therefore, this tool was also used in the present study to evaluate the accuracy of measurement methods and to estimate experimentally derived values and their concrete influence on the formation of solidification cracks. By integrating experimental methods and numerical simulations, this study investigates the spatially resolved and temporally changing development of strain during welding, with a particular focus on the critical conditions that lead to the formation of solidification cracks. T2 - GAMM 94th Annual Meeting CY - Magdeburg, Germany DA - 18.03.2024 KW - Laser beam welding KW - Solidification cracking KW - FEM simulation PY - 2024 AN - OPUS4-62417 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rethmeier, Michael A1 - Gook, Sergej A1 - Biegler, Max A1 - Gumenyuk, Andrey T1 - Anwendung einer Kombination aus Laserhybrid- und Unterpulverschweißen zum Fügen dicker Bleche aus Schiffbaustahl EH36 N2 - In diesem Beitrag wird ein Schweißverfahren vorgestellt, mit dem 30 mm dicke Bleche aus Schiffbaustahl EH36 effizient und werkstoffgerecht gefügt werden können. Die wirtschaftlichen Vorteile des Verfahrens ergeben sich aus dem Wegfall der aufwendigen Kantenvorbereitung und der Reduzierung des Schweißzusatzbedarfs. Die Stumpfschweißnähte werden in einer Lagen-/Gegenlage-Technik durch Laserhybridschweißen und Unterpulverschweißen ausgeführt. Dabei erfolgt die Laserhybridschweißung als Einschweißung mit einer Tiefe von etwa 25 mm, während die Unterpulvernaht als zweiter Durchgang auf der gegenüberliegenden Seite des Bauteils mit einer Einschweißtiefe von 8 mm aufgebracht wird. Die Überlappung der beiden Lagen gewährleistet einen geschlossenen Nahtquerschnitt. Dank der partiellen Durchschweißung der Laserhybridnaht entfällt die Notwendigkeit zur Wurzelformierung. Darüber hinaus bietet die Prozesskombination eine höhere Toleranz gegenüber Ungenauigkeiten in der Kantenvorbereitung, was die Prozesskomplexität reduziert. Der Einsatz dieses robusteren Verfahrens, das weniger von einer präzisen Kantenvorbereitung abhängig ist, erleichtert die Produktionsvorbereitung, minimiert die Fehleranfälligkeit und senkt die Nachbearbeitungskosten. Dies macht das Laserhybridschweißen besonders attraktiv für Anwendungen im Schiffbau. T2 - 22. Tagung Schweißen in der maritimen Technik und im Ingenieurbau CY - Hamburg, Germany DA - 13.05.2025 KW - Laserhybridschweißen KW - Unterpulverschweißen KW - Kerbschlagbiegeversuch PY - 2025 SP - 87 EP - 98 PB - DVS – Deutsche Verband für Schweißen und verwandte Verfahren e. V AN - OPUS4-63342 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bakir, Nasim A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Observation of the weld pool shape in partial penetration welding and its influence on solidification crack formation for high-power laser beam welding N2 - In this study, steel-glass experiments were conducted to observe the melt pool geometry using a high-speed camera. The high-speed recordings and optical flow analysis show that two main flows take place in form of vortices. The lower vortex drives the melt backwards from the front keyhole wall and thus causes an extension of the melt pool, which is called bulging. This bulging promotes solidification cracking by forming a closed area filled with melt and the accumulation of impurities in the final solidification phase, resulting in low-melting phases which are under tensile stress at the end of solidification. T2 - Lasers in Manufacturing Conference 2021 CY - Online meeting DA - 21.06.2021 KW - Laser beam welding KW - Weld pool shape KW - Solidification craking KW - Partial penetration PY - 2021 SP - 1 EP - 5 AN - OPUS4-53587 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - The effect of an AC magnetic field on flow dynamics and filler wire mixing in high power laser hybrid welding N2 - The use of the oscillating magnetic field as a backing support for the welding of thick components is already known. The influence of the magnetic field and the induced Lorentz forces in the melt on the melt pool geometry and the fluid flows is not yet fully investigated. The study deals with the determination of the influence of an externally applied oscillating magnetic field on the melt pool dynamics in high power laser hybrid welding process. An AC magnet was positioned under the specimen to create an electromagnetic force directed upwards to oppose dropping. To visualise the flow characteristics of the melt, several experiments were carried out using a technique specifically designed for this purpose with mild steel made of S355J2 with a wall thickness of 20 mm and a quartz glass in a butt configuration. A high-speed camera was used to monitor the geometry of the melt pool through the glass. The influence of the magnetic field orientation to the welding direction and the oscillation frequency on the molten pool was investigated for the case of the metal-glass configuration and for laser hybrid welding. The high-speed recordings were analysed with the Optical Flow Algorithm to characterise the flow within the melt pool. The element distribution over the whole seam thickness was evaluated by X-ray fluorescence (XRF). The high-speed analysis showed that in the melt pool two vortices are formed, one in the upper part and the other in the lower part. In the region where the two vortices come together, a narrow region (necking region) forms in the melt pool. The evaluation of the high-speed recordings shows that the depth of the region where the two vortices meet is strongly influenced by the oscillation frequency. Additionally, the oscillation frequency demonstrated a greater influence on the melt pool dynamics and the mixing of the elements of the filler wire. T2 - X International Conference «Beam Technologies & Laser Application» CY - Pushkin (St. Petersburg), Russia DA - 20.09.2021 KW - Hybrid laser arc welding KW - Laser beam welding KW - Material transport PY - 2021 AN - OPUS4-53573 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - Two-colour thermography for measurement of temperature distribution in laser beam welding N2 - Solidification cracking is a frequently observed phenomenon in laser beam welding of austenitic stainless steels and other metallic alloys. Characterisation of cracking susceptibility requires knowledge of the precise and spatially resolved temperature distribution near the solidification front in the welding process. Thermography is a standard tool that provides a qualitative estimate of the 2D temperature field. The general disadvantage of this method is its dependence on the emission characteristics of the measured object. For welding applications, these can vary significantly in the temperature range above and below the melting temperature. For this purpose, we have developed a thermography-based measurement technique using a SWIR camera system in combination with two narrow bandpass filters that use the principle of two-wavelength pyrometry to estimate absolute temperature values. This technique was used to determine the temperature distributions and gradients near the solidification front of laser-welded austenitic steel. The results were validated by other measurements. T2 - 13th CIRP Conference on Photonic Technologies [LANE 2024] CY - Fürth, Germany DA - 16.09.2024 KW - Laser beam welding KW - Solidification cracking KW - FEM simulation PY - 2024 AN - OPUS4-62415 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - Strain distribution vs strain evolution during solidification cracking CTW test for laser beam welding of 1 mm austenitic stainless steels N2 - Laser welding is a widely established manufacturing process across many industrial sectors. However, solidification cracking and the weldability of materials have remained contentious issues for many years, particularly concerning the causes of hot crack formation. The local distribution of total strain was measured in close proximity to the solidification zone during laser welding of AISI 304 and AISI 310S stainless steels, using the Controlled Tensile Weldability (CTW) test. In this setup, 1 mm thick weld coupons were subjected to a defined external tensile load during welding. Mechanical loading parameters were varied by adjusting the strain rate and ultimate strain level to identify the critical conditions that lead to solidification crack formation along the weld seam centerline. Using Digital Image Correlation (DIC) and the optical flow method [1], we estimated the local strain distribution at the surface near the molten pool and tracked its evolution across several characteristic zones—before, during, and after the application of mechanical loading. The results revealed that solidification crack formation coincides with regions of high plastic deformation within a critical temperature range. Furthermore, we identified a clear relationship between strain rate and both crack initiation probability and maximum local strain. Importantly, neither strain rate nor maximum strain alone is sufficient to predict cracking; instead, their combined effect must be considered to accurately assess hot cracking susceptibility. T2 - AJP 2025 CY - Coimbra, Portugal DA - 16.10.2025 KW - Laser beam welding KW - Solidification cracking KW - Optical measurement PY - 2025 AN - OPUS4-64431 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey T1 - Reducing Noise Impact on Strain Accuracy Measurement by Optical Flow and DIC for Laser Welding Applications N2 - In recent years, non-contact methods for in situ local strain measurement during welding processes have gained increasing importance. This trend is driven by advancements in both measurement technology—such as improved camera systems, illumination sources, and X-ray techniques—and in image processing algorithms for strain evaluation. Laser beam welding poses specific challenges for optical strain measurement due to various types of process-related emissions that impair measurement accuracy. In this study, two different algorithms were applied to analyze the local strain field in the solidification zone during laser welding of AISI 310S stainless steel: the inverse compositional Gauss-Newton algorithm for Digital Image Correlation (DIC) and the Lucas-Kanade method for optical flow analysis [1]. Video sequences were recorded under Controlled Tensile Weldability Test (CTW) conditions, in which the specimens were subjected to a defined external tensile load during welding. This setup consistently induced solidification cracking at the material surface, which could be observed in the video recordings. To enhance the robustness and accuracy of the strain evaluation, various noise reduction techniques were implemented. These included identification and mitigation of erroneous frames caused by process emissions and dynamic disturbances. The resulting strain distributions showed high repeatability across multiple experiments and were in good qualitative agreement with predictions from high-fidelity finite element simulations. [2]. T2 - AJP 2025 CY - Coimbra, Portugal DA - 16.10.2025 KW - Laser beam welding KW - Solidification cracking KW - Optical measurement PY - 2025 AN - OPUS4-64428 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Artinov, Antoni A1 - Bakir, Nasim A1 - Bachmann, Marcel A1 - Gumenyuk, Andrey A1 - Na, S.-J. A1 - Rethmeier, Michael T1 - On the search for the origin of the bulge effect in high power laser beam welding N2 - The shape of the weld pool in laser beam welding plays a major role to understand the dynamics of the melt and its solidification behavior. The aim of the present work was its experimental and numerical investigation. To visualize the geometry of the melt pool in the longitudinal section a butt joint configuration of 15 mm thick structural steel and transparent quartz glass was used. The weld pool shape was recorded by means of a high-speed video camera and two thermal imaging MWIR and VIS cameras. The observations show that the dimensions of the weld pool vary depending on the depth. The regions close to the surface form a teardrop shaped weld pool. A bulge-region and its temporal evolution were observed approximately in the middle of the depth of the weld pool. Additionally, a transient numerical simulation was performed until reaching a steady state to obtain the weld pool shape and to understand the formation mechanism of the observed bulging phenomena. A fixed keyhole with an experimentally obtained shape was used to represent the full-penetration laser beam welding process. The model considers the local temperature field, the effects of phase transition, thermo-capillary convection, natural convection and temperature-dependent material properties up to evaporation temperature. It was found that the Marangoni convection and the movement of the laser heat source are the dominant factors for the formation of the bulging-region. Good correlation between the numerically calculated and the experimentally observed weld bead shapes and the time-temperature curves on the upper and bottom surface were found. T2 - International Congress on Applications of Lasers & Electro-Optics (ICALEO®) CY - Orlando, USA DA - 14.10.2018 KW - Bulging effect KW - High power laser beam welding KW - Numerical modelling KW - Solidification cracking PY - 2019 SP - 1 EP - 8 AN - OPUS4-47139 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Artinov, Antoni A1 - Karkhin, V. A1 - Bakir, Nasim A1 - Meng, Xiangmeng A1 - Bachmann, Marcel A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Lamé curves approximation for the assessment of the 3-D temperature distribution in keyhole mode welding processes N2 - A novel approach for the reconstruction of an equivalent volumetric heat source from a known weld pool shape is proposed. It is based on previously obtained weld pool geometries from a steady-state thermo-fluid dynamics simulation. Hereby the weld pool dimensions are obtained under consideration of the most crucial physical phenomena, such as phase transformations, thermo-capillary convection, natural convection and temperature-dependent material properties. The algorithm provides a time and calibration efficient way for the reproduction of the weld pool shape by local Lamé curves. By adjusting their parameters, the identification of the finite elements located within the weld pool is enabled. The heat input due to the equivalent heat source is assured by replacing the detected nodes’ temperature by the melting temperature. The model offers variable parameters making it flexible and adaptable for a wide range of workpiece thicknesses and materials and allows for the investigation of transient thermal effects, e.g. the cooling stage of the workpiece. The calculation times remain acceptably short especially when compared to a fully coupled process simulation. The computational results are in good agreement with performed complete-penetration laser beam welding experiments. T2 - ICALEO 2019 - 38th International congress on applications of lasers & electro-optics CY - Orlando, FL, USA DA - 07.10.2019 KW - Weld pool shape approximation KW - Keyhole mode laser beam welding KW - Numerical simulation KW - Superelliptic Lamé curves PY - 2019 UR - http://icaleo.conferencespot.org/2019-proceedings?qr=1 SN - 978-1-940168-1-42 SP - Paper # Macro 1002 AN - OPUS4-49310 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gook, Sergej A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Vermeidung von Schweißimperfektionen im Überlappbereich bei laserstrahlhybridgeschweißten Rundnähten N2 - Die Laserstrahl-Hybrid-Schweißtechnologie erweist sich in der schweißtechnischen Fertigung immer mehr als innovative Alternative gegenüber anderen Schweißverfahren. Obwohl das Laserstrahl-Hybridschweißverfahren viele wirtschaftliche Vorteile gegenüber herkömmlichen Schweißverfahren aufweist, wie z.B. große Einschweißtiefe und dadurch eine reduzierte Anzahl von Schweißlagen, geringe thermische Belastung des Grundwerkstoffes aufgrund reduziertem Wärmeeintrag, konnte das Schweißverfahren überwiegend für das Schweißen von Längsnähten demonstriert werden. Eine Vielzahl von Schweißaufgaben, z.B. beim Schweißen von Segmenten von Windkraftanlagen oder dem Orbitalschweißen beim Verlegen von Großrohrleitungen sieht vor, dass die zu schweißenden Bauteile mit einer Rundnaht zusammengefügt werden. Die schweißtechnische Herausforderung ist hier, dass beim Schließen einer Rundnaht mit der Entstehung eines fehlerbehafteten Überlappbereiches zu rechnen ist. Ein zentrales Problem im Überlappbereich einer laserstrahl- sowie laserhybridgeschweißten Rundnaht ist die Bildung von Imperfektionen wie Poren, Rissen sowie die Bildung eines Endkraters, welcher als geometrische Kerbe wirkt. Bisher liegen keine universellen Lösungen zur fehlerfreien Ausführung von geschlossenen Rundnähten beim Laserstrahl-Hybridschweißen vor. Diese Studie befasst sich mit der Entwicklung eines Verfahrens, mit dem die Entstehung von o.g. Schweißimperfektionen vermieden wird. Die Strategie der Prozessführung beim Schließen der Rundnaht sieht hervor, dass ein fehlerfreier Überlappbereich durch die Kontrolle der Erstarrungsbedingungen am Schweißnahtende erreicht werden kann. Die kontrollierte Wärmeführung wird durch eine Anpassung der Parameter von beiden beteiligten Schweißprozessen, dem Laserstrahl- sowie MSG-Schweißprozess realisiert. Im Rahmen dieser Arbeit wurde eine Serie von Schweißversuchen an 9,5 mm dicken Rohabschnitten aus hochfestem Pipelinestahl X100Q mit Variation der Prozessparameter wie der Laserleistung, der Defokussierung des Laserstrahls sowie der Endkraterfüllzeit im Überlappbereich der Rundnaht durchgeführt. Nachfolgend werden die erzielten Ergebnisse dargestellt und diskutiert. T2 - DVS-Studentenkongress 2019 CY - Dusseldorf, Germany DA - 16.09.2019 KW - Laserstrahlschweißen KW - Laserhybridschweißen KW - Rundnaht KW - Endkrater KW - Überlappbereich KW - Defokussierung PY - 2019 SP - 370 EP - 378 AN - OPUS4-49242 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schnieder, V. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Additive Fertigung von Nickel-Titan-Formgedächtnislegierungen aus den Elementpulvern mittels Laserpulverauftragschweißen N2 - Additive Fertigungsverfahren gewinnen aufgrund der schnellen, flexiblen und kosten-günstigen Fertigung von Bauteilen zunehmend an Bedeutung. Das Laserpulverauf-tragschweißen (LPA) wurde anfangs hauptsächlich als Beschichtungsverfahren ein-gesetzt. Diese Technologie bewerkstelligt aber auch das Reparieren von verschlisse-nen Bauteilen, sodass diese zeitsparend und ressourcenschonend erneuert werden können. Die hohe Aufbaurate, die flexible Pulverzusammensetzung sowie die hohe Endkonturnähe ermöglichen heutzutage die Entwicklung und additive Fertigung von neuen Materialien, wie zum Beispiel Nickel-Titan-Formgedächtnislegierungen. T2 - 39. Assistentenseminar CY - Eupen, Germany DA - 12.09.2018 KW - Laserpulverauftragschweißen PY - 2019 SN - 978-3-96144-070-2 SP - 27 EP - 33 PB - DVS Media GmbH AN - OPUS4-51316 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gumenyuk, Andrey A1 - Üstündag, Ö. A1 - Gook, S. A1 - Rethmeier, Michael T1 - Laserhybridschweißen von dickwandigen Stählen mit elektromagnetischer Schmelzbadunterstützung N2 - Die steigenden Anforderungen in Hinsicht auf Sicherheitsfaktoren von gefügten Bauteilen führen zu einer Zunahme der zu schweißenden Bauteildicken. Das Laserstrahl-Lichtbogen-Hybridschweißverfahren – verbreitet im industriellen Einsatz vor allem im Schiffs- und Windkraftanlagenbau – ermöglicht das einlagige Fügen von dickwandigen Strukturen. Eine Herausforderung stellt das Schweißen von dickwandigen Bauteilen mit reduzierter Geschwindigkeit in Wannenlage (PA-Position) da. Sie ist aufgrund des erhöhten hydrostatischen Druckes und die daraus resultierenden Tropfenbildung an der Wurzelseite bedingt realisierbar. Die im Rahmen dieser Studie eingesetzte elektromagnetische Schmelzbadunterstützung wirkt dem gravitationsbedingten Austropfen der Schmelze entgegen und kompensiert den hydrostatischen Druck. Dabei werden unterhalb der Schweißzone mit Hilfe eines extern angelegten oszillierenden Magnetfeldes Wirbelströme im Werkstück induziert, die eine nach oben gerichtete Lorentzkraft erzeugt. Die Lorentzkraft wirkt dem hydrostatischen Druck entgegen und stellt einen sicheren Schweißprozess ohne Tropfenbildung dar. Mit dem Hybridschweißverfahren mithilfe der elektromagnetischen Schmelzbadunterstützung gelingt es mit einem 20-kW Faserlaser bis zu 30 mm dicke Bleche in einer Lage zu schweißen. Bei 25 mm dicken einlagig geschweißten Platten aus S355 konnte ein Spalt bis 1 mm und ein Kantenversatz bis zu 2 mm sicher überbrückt werden. Die Reduzierung der Schweißgeschwindigkeit hat eine Verringerung der notwendigen Laserleistung zur Folge und begünstigt außerdem die mechanisch-technologischen Eigenschaften, infolge der reduzierten Abkühlgeschwindigkeit. Durch die geringe Martensitbildung führt dies zu einer Verbesserung der Kerbschlagzähigkeit. T2 - 19. Tagung in Hamburg - DVS CY - Hamburg, Germany DA - 24.04.2019 KW - Laser-Hybridschweißen KW - Elektromagnetische Schmelzbadunterstützung KW - Schweißen von kaltzähen Stählen PY - 2019 SP - 34 EP - 46 PB - DVS AN - OPUS4-47918 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Stankevich, S. A1 - Gumenyuk, Andrey A1 - Straße, Anne A1 - Rethmeier, Michael ED - Reisgen, U. ED - Schmidt, M. ED - Zaeh, M. ED - Rethmeier, Michael T1 - Measurement of thermal cycle at multi-pass layer build-up with different travel path strategies during DLMD process N2 - The shape of the parts, created by the technology of direct laser metal deposition (DLMD), is influenced by various parameters, for example, the power and diameter of the laser source spot. The contribution of energy from the laser affects the temperature distribution in the formed layers. The changing temperature in the working area entails a Change in the geometry of the layers and affects the stability of the process. In this paper, experiments on the measurement of temperature cycles in the DLMD process with different directions of the filling track are carried out. An infrared camera was used to measure thermal cycles. The calibration of the acquired data (i.e. correspondence table between the intensity of thermal radiation of the material and the absolute temperature) was done with help of two-color pyrometer ex situ and in situ measurements. The experiments are carried out on two materials 316L and Inconel 718. The effect of the maximum temperature on the layer height is shown, and thermal cycles in the formation of layers for different filling strategies are presented. T2 - Laser in Manufacturing Conference 2019 CY - Munich, Germany DA - 24.06.2019 KW - Thermography KW - Direct Laser Metal Deposition PY - 2019 SP - 1 EP - 9 AN - OPUS4-48716 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bakir, Nasim A1 - Biltgen, J. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Influence of Partial Penetration Laser Hybrid Welding Parameters on the Solidification Cracking for Thick-Walled Structures N2 - In this study, the influence of the welding speed and the arc power on the solidification crack formation for partial penetration laser hybrid welded Thick-Walled plates were investigated. Experimentally, a linear correlation between the welding velocity and the crack number was observed. That is by reducing the welding velocity the crack number was reduced. The reduced welding velocity showed a strong impact on stress, as the model demonstrated a very lower stress amount in comparison to the reference case. The reduction of the welding speed could be a helpful technique to reduce the hot cracking. The wire feed speed showed a very slight influence on the crack formation. That can be returned to the large distance between the critical region for cracking and the arc region. T2 - Lasers in Manufacturing Conference 2019 CY - Munich, Germany DA - 24.06.2019 KW - Hybrid laser-arc welding KW - Solidification cracking KW - Thick-walled steel KW - Numerical simulation PY - 2019 SP - 1 EP - 7 PB - WLT Wissenschaftliche Gesellschaft Lasertechnik e.V AN - OPUS4-48733 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ö. A1 - Gook, S. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Mechanical Properties of Single-pass Hybrid Laser Arc Welded 25 mm Thick-walled Structures Made of Fine-grained Structural Steel N2 - The presented study deals with the performing and mechanical testing of single pass hybrid laser-arc welds (HLAW) on 25 mm thick plates made of steel grade S355J2. One of the challenges have to be solved at full penetration HLAW of thick plates is the drop formation occurring due to the disbalances of the forces acting in the keyhole and on the melt pool surface. Such irregularities mostly limit the use of high-power laser beam welding or HLAW of thick-walled constructions. To overcome this problem, an innovative concept of melt pool support based on generating Lorentz forces in the weld pool is used in this work. This method allows to perform high quality welds without sagging even for welding of 25 mm thick plates in flat position at a welding speed of 0.9 m min-1. For the obtain of full penetrated welds a laser beam power of 19 kW was needed. A high V-impact energy of up to 160 J could be achieved at the test temperature of 0 °C. Even at the most critical part in the weld root an impact energy of 60 J in average could be reached. The tensile strength of the weld reaches that of the base material. An introduce of the HLAW process with electromagnetic support of the melt pool in the industrial practice is an efficient alternative to the time- and cost-intensive arc-based multi-layer welding techniques which are established nowadays for joining of thick-walled constructions. KW - Mechanical Properties KW - Hybrid Laser Arc Welding KW - Thick-walled Structures KW - Fine-grained Steel PY - 2019 DO - https://doi.org/10.1016/j.promfg.2019.08.016 SN - 2351-9789 VL - 36 SP - 112 EP - 120 PB - Elsevier B.V. AN - OPUS4-48969 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Üstündag, Ö. A1 - Gook, S. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Investigation of the mechanical properties of single-pass hybrid laser-arc welded thick X120 pipeline steel plates N2 - With global increases in clean energy demand, the natural gas is gaining in importance. Pipelines are the safest and most cost-effective way of transporting natural gas. Due to high transport volume and resulting high operation pressure, the demand for ultra-high strength steel grades such as X120 is very strong. As a result of the fact that these steels are produced by thermo-mechanical controlled processing, the welding process must be selected accordingly. Based on investigations, a high heat input such as by submerged arc welding process leads to softening in the weld metal and loss of strength whereas pure laser beam welding results in high cooling rates and deteriorate toughness of the weld metal. The objective of this research is to investigate the influence of heat input to mechanical properties of hybrid laser-arc welded pipeline steels of grade X120. Test specimens with a thickness of 20 mm could be welded without preheating in a single-pass with different welding velocities to observe the largest possible parameter window of the heat input. The achieved V-notch impact energy for hybrid laser-arc welded samples was 144±37 J at a testing temperature of -40 °C. With a tensile strength of 930±4 MPa the requirements of API 5L was achieved. To prevent gravity drop-outs at the slow welding speeds, an electromagnetic weld pool support system was used, which works contactless and is based on generating Lorentz forces. It was therefore possible to control the cooling rate in order to meet the requirements of the mechanical properties. By adapting the electromagnetic weld pool support to the laser and laser hybrid welding process, the application potential of these technologies for industrial implementation can be drastically increased. T2 - 14th Pipeline Technology Conference CY - Berlin, Germany DA - 18.03.2019 KW - Mechanical properties KW - Hybrid laser arc welding KW - Pipeline steel X120 PY - 2019 UR - https://www.pipeline-conference.com/conferences/14th-pipeline-technology-conference-2019 SN - 2510-6716 SP - 1 EP - 10 AN - OPUS4-48970 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gook, S. A1 - El-Batahgy, A. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Hybrid laser arc welding of thick plates X8Ni9 for LNG tank construction N2 - Results of experimental investigations of the relationship between laser-hybrid welding process parameters, type of the filler metal and the mechanical properties of the welds made from 9% nickel cryogenic steel X8Ni9 are discussed. The results contribute to the development and conversion in the industrial practice a new laser beam-based welding technology for the automated manufacturing of LNG tanks. The remarkable heterogeneity in the chemical composition of the weld metal as well as an insufficient impact toughness could be indicated by using austenitic filler wire. The most promising results were achieved by applying 11%Ni filler wire, which is similar to the base material. A correlation between impact toughness and wire feeding speed could be shown. The highest impact toughness was 134 J at -196°C. The laser-hybrid welds passed the tensile test. The failure stress of 720 MPa with a fracture location in the base metal was achieved for all samples tested. T2 - Lasers in Manufacturing Conference 2019 CY - Munich, Germany DA - 24.06.2019 KW - X8Ni9 KW - Hybrid Laser Arc Welding KW - Cryogenic Steel KW - Low Temperature Toughness PY - 2019 SP - 1 EP - 11 PB - WLT Wissenschaftliche Gesellschaft Lasertechnik e.V. AN - OPUS4-48972 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Üstündag, Ö. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Single-pass Hybrid Laser Arc Welding of Thick Materials Using Electromagnetic Weld Pool Support N2 - Hybrid laser-arc welding process allows single-pass welding of thick materials, provides good quality formation of joints with minimal thermal deformations and a high productivity in comparison with arc-based welding processes. Nevertheless, thick-walled steels with a thickness of 20 mm or more are still multi-pass welded using arc welding processes, due to increased process instability by increasing laser power. One limitation factor is the inadmissible formation of gravity drop-outs at the root. To prevent this, an innovative concept of electromagnetic weld pool support is used in this study. With help of such system a stable welding process can be established for 25 mm thick steel plates and beyond. Sound welds could be obtained which are tolerant to gaps and misalignment of the welded parts. The adaptation of this system to laser and hybrid laser-arc welding process can dramatically increase the potential field of application of these technologies for real industrial implementation. T2 - Lasers in Manufacturing Conference 2019 CY - Munich, Germany DA - 24.06.2019 KW - Full Penetration KW - Hybrid Laser Arc Welding KW - Electromagnetic Weld Pool Support KW - Thick Materials PY - 2019 SP - 1 EP - 8 PB - WLT Wissenschaftliche Gesellschaft Lasertechnik e.V. AN - OPUS4-48971 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Huo, Wenjie A1 - Schmies, Lennart A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael A1 - Wolter, Katinka T1 - An illumination based backdoor attack against crack detection systems in laser beam welding N2 - Deep neural networks (DNNs) have been wildly used in engineering and have achieved state-of-the-art performance in prediction and measurement tasks. A solidification crack is a serious fault during laser beam welding and it has been proven to be successfully detected using DNNs. Recently, research on the security of DNNs is receiving increasing attention because it is necessary to explore the reliability of DNNs to avoid potential security risks. The backdoor attack is a serious threat, where attackers aim to inject an inconspicuous pattern referred to as trigger into a small portion of training data, resulting in incorrect predictions in the reference phase whenever the input contains the trigger. In this work, we first generate experimental data containing actual cracks in the welding laboratory for training a crack detection model. Then, targeting this scenario, we design a new type of backdoor attack to induce the model to predict the crack as a normal state. Considering the stealthiness of the attack, a common phenomenon during the welding process, illumination, is used as the backdoor trigger. Experimental results demonstrate that the proposed method can successfully attack the crack detection system and achieve over 90% attack success rate on the test set. T2 - 8th ML4CPS 2025 – Machine Learning for Cyber-Physical Systems CY - Berlin, Germany DA - 06.03,2025 KW - System security KW - Welding crack detection KW - Backdoor attack KW - Deep neural networks PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-651357 DO - https://doi.org/10.24405/20021 VL - 2025 SP - 12 EP - 21 PB - Universitätsbibliothek der HSU/UniBw H CY - Hamburg AN - OPUS4-65135 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bevilacqua, Tommaso A1 - Gumenyuk, Andrey A1 - Habibi, Niloufar A1 - Hartwig, Philipp A1 - Klawonn, Axel A1 - Lanser, Martin A1 - Rethmeier, Michael A1 - Scheunemann, Lisa A1 - Schröeder, Jöerg T1 - Large-scale thermo-mechanical simulation of laser beam welding using high-performance computing: A qualitative reproduction of experimental results N2 - Laser beam welding (LBW) is a non-contact joining technique that has gained significant importance in modern industrial manufacturing. One potential problem, however, is the formation of solidification cracks, which particularly affects alloys with a pronounced melting range. The aim of the present work is the development of computational methods and software tools to numerically simulate LBW. In order to obtain a sufficiently accurate solution, a large number of finite elements has to be used. Therefore, a highly parallel scalable solver framework, based on the software library PETSc, was used to solve this computationally challenging problem on a high-performance computing architecture. Finally, the experimental results and the numerical simulations are compared. They are found to be in good qualitative agreement, which confirms the validity of the numerical simulations and allows for a better interpretation of the experimentally observed strain distribution. KW - Laser beam welding KW - Termo-mechanical processes KW - Solidification cracking KW - High-performance computing KW - Domain decomposition methods PY - 2025 DO - https://doi.org/10.1016/j.rineng.2025.108827 SN - 2590-1230 SP - 1 EP - 33 PB - Elsevier B.V. AN - OPUS4-65290 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ö. A1 - Avilov, V. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Full penetration hybrid laser arc welding of up to 28 mm thick S355 plates using electromagnetic weld pool support N2 - The laser hybrid welding process offers many advantages regarding deep penetration, increased welding velocity and with the help of the supplied filler wire an improved bridgeability to gap and misalignment tolerances. High power laser systems with a power of approx. 30 kW are already available on the market. Nevertheless, multi-layer technology with an arc process is still used for welding of plates from a thickness from 20 mm. A potential cause is the process instability with increasing laser power. It is inevitable that gravity drop-out due to the high hydrostatic pressure at increasing wall thickness especially at welding in flat position and with a low welding speed. The surface tension decreases with increasing root width resulting from low welding velocities. To prevent such inadmissible defects of the seam a use of weld pool support is required. Usual weld pool support systems such as ceramic or powder supports require a mechanical detachment which is time-consuming. The electromagnetic weld pool support system described in this work shows an alternative weld pool support which works contactless. It is based on generating Lorentz forces in the weld pool due to oscillating magnetic field and induced eddy currents. This innovative technology offers single pass welds up to 28 mm in flat position and reduced welding velocity with a laser power of just 19 kW. It also leads to improved mechanical-technological properties of the seams because of the slow cooling rate. With usage of an electromagnetic weld pool support the limitation of the hybrid laser arc welding process in the thick sheet metal will be extend. KW - Electromagnetic weld pool support KW - Hybrid laser arc welding KW - Thick-walled steel KW - Single pass welding PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-468276 DO - https://doi.org/10.1088/1742-6596/1109/1/012015 SN - 1742-6596 VL - 1109 SP - 1 EP - 7 PB - IOP Publ. AN - OPUS4-46827 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -