TY - CONF A1 - Brunner-Schwer, Chr. A1 - Biegler, M. A1 - Rethmeier, Michael T1 - Investigation on laser cladding of rail steel without preheating N2 - The contact between train wheels and rail tracks is known to induce material degradation in the form of wear, and rolling contact fatigue in the railhead. Rails with a pearlitic microstructure have proven to provide the best wear resistance under severe wheel-rail interaction in heavy haul applications. High speed laser cladding, a state-of-the-art surface engineering technique, is a promising solution to repair damaged railheads. However, without appropriate preheating or processing strategies, the utilized steel grades lead to martensite formation and cracking during deposition welding. In this study, laser cladding of low-alloy steel at very high speeds was investigated, without preheating the railheads. Process speeds of up to 27 m/min and laser power of 2 kW are used. The clad, heat affected zone and base material are examined for cracks and martensite formation by hardness tests and metallographic inspections. A methodology for process optimization is presented and the specimens are characterized for suitability. Within the resulting narrow HAZ, the hardness could be significantly reduced. T2 - Lasers in Manufacturing Conference 2021 CY - Erlangen, Germany DA - 21.06.2021 KW - High speed laser cladding KW - Preheatin KW - Rail tracks KW - Pearlitic microstructure PY - 2021 AN - OPUS4-53974 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Biegler, M. A1 - El-Sari, B. A1 - Rethmeier, Michael A1 - Finus, F. T1 - Schweißen unter Zug – LME-Eingangsprüfung für die Autoindustrie N2 - Der Trend zum Leichtbau und die Transformation zur E-Mobilität in der Automobilindustrie befeuern die Entwicklung neuer hochfester Stähle für den Karosseriebau. Derartige Werkstoffe sind beim Widerstandspunktschweißen besonders rissanfällig (LME). Das Schweißen unter Zug stellt eine effektive Methode um die LME-Anfälligkeit unterschiedlicher Werkstoffe qualitativ zu bestimmen. KW - Automobilindustrie KW - Widerstandspunktschweißen KW - Liquid Metal Embrittlement KW - Zinkbeschichtung KW - Hochfester Stahl PY - 2021 IS - 6 SP - 54 EP - 55 AN - OPUS4-54057 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Meyerdierks, M. A1 - Schreiber, V. A1 - Böhne, Ch. A1 - Jüttner, S. A1 - Meschut, G. A1 - Rethmeier, Michael T1 - Validierung von Methoden zur Vermeidung von Liquid Metal Embrittlement an realitätsnahen Prinzipbauteilen (IGF 21483 BG / P 1488) N2 - Ziel des Forschungsprojekts ist es, eine Korrelation zwischen Gleeble-Heißzug-Prüfverfahren und Widerstandspunktschweiß-basierten Prüfverfahren herzustellen. Es soll die Effektivität von Methoden zu Vermeidung von Liquid Metal Embrittlement an realitätsnahen Prinzipbauteilen bewertet werden. Weiterhin soll Kenntnis über Auswirkungen von LME Rissen auf das Tragverhalten von realitätsnahen Prinzipbauteilen gewonnen werden. T2 - 30. Schweißtechnische Fachtagung CY - Barleben, Germany DA - 07.10.2021 KW - Liquid Metal Embrittlement KW - Gleeble KW - Heißzug KW - Widerstandpunktschweißen KW - Flüssigmetallversprödung PY - 2021 AN - OPUS4-54061 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, V. A1 - Marko, A. A1 - Kruse, T. A1 - Biegler, M. A1 - Rethmeier, Michael T1 - Analysis and recycling of bronze grinding waste to produce maritime components using directed energy deposition N2 - Additive manufacturing promises a high potential for the maritime sector. Directed Energy Deposition (DED) in particular offers the opportunity to produce large-volume maritime components like propeller hubs or blades without the need of a costly casting process. The post processing of such components usually generates a large amount of aluminum bronze grinding waste. The aim of the presented project is to develop a sustainable circular AM process chain for maritime components by recycling aluminum bronze grinding waste to be used as raw material to manufacture ship Propellers with a laser-powder DED process. In the present paper, grinding waste is investigated using a dynamic image Analysis system and compared to commercial DED powder. To be able to compare the material quality and to verify DED process parameters, semi-academic sample geometries are manufactured. T2 - LiM 2021 CY - Munich, Germany DA - 21.06.2021 KW - Additive Manufacturing KW - Maritime Components KW - Powder Analysis KW - Recycling KW - Directed Energy Deposition PY - 2021 SP - 1 EP - 9 AN - OPUS4-54067 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rethmeier, Michael A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey T1 - Investigation of the gap bridgeability at high-power laser hybrid welding of plasma-cut thick mild steels with AC magnetic support N2 - One of the challenges of the high-power hybrid laser welding of thick steels is the sensitivity of the process of the process to manufacturing tolerances. This usually leads to a time-consuming preparation of the welding edges, such as milling. The study deals with the influence of the edge quality of milled and plasma-cut steel made of S355J2 with a wall thickness of 20 mm on the laser hybrid welded seam quality. Furthermore, the gap bridgeability and the tolerances towards edge misalignment was investigated. An AC magnet was used as backing support to prevent sagging and positioned under the workpiece, to generate an upwards directed electromagnetic pressure. The profiles of the edges and the gap on the top and root side were measured using a digital camera. Single-pass laser hybrid welds of plasma-cut edges could be welded using a laser beam power of just 13.7 kW. A gap bridgeability up to 2 mm and misalignment of edges up to 2 mm could be achieved successful. Additionally, the independence of the cutting side and the welding side was shown, so that samples were welded to the opposite side to their cutting. For evaluation of internal defects or irregularities, X-ray images were carried out. Charpy impact strength tests were performed to determine the toughness of the welds. T2 - X International Conference «Beam Technologies & Laser Application CY - Online meeting DA - 20.09.2021 KW - Plasma-cutting KW - Hybrid laser-arc welding KW - Thick-walled steel KW - Edge quality KW - Gap bridgeability KW - Misalignment of the edges PY - 2021 AN - OPUS4-53920 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Investigation of the gap bridgeability at high-power laser hybrid welding of plasma-cut thick mild steels with AC magnetic support N2 - One of the challenges of the high-power hybrid laser welding of thick steels is the sensitivity of the process of the process to manufacturing tolerances. This usually leads to a time-consuming preparation of the welding edges, such as milling. The study deals with the influence of the edge quality of milled and plasma-cut steel made of S355J2 with a wall thickness of 20 mm on the laser hybrid welded seam quality. Furthermore, the gap bridgeability and the tolerances towards edge misalignment was investigated. An AC magnet was used as backing support to prevent sagging and positioned under the workpiece, to generate an upwards directed electromagnetic pressure. The profiles of the edges and the gap on the top and root side were measured using a digital camera. Single-pass laser hybrid welds of plasma-cut edges could be welded using a laser beam power of just 13.7 kW. A gap bridgeability up to 2 mm and misalignment of edges up to 2 mm could be achieved successful. Additionally, the independence of the cutting side and the welding side was shown, so that samples were welded to the opposite side to their cutting. For evaluation of internal defects or irregularities, X-ray images were carried out. Charpy impact strength tests were performed to determine the toughness of the welds. T2 - X International Conference «Beam Technologies & Laser Application» KW - Laser hybrid welding KW - Magnetic bath support KW - Plasma-cut samples KW - Thick plate welding PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-539248 DO - https://doi.org/10.1088/1742-6596/2077/1/012007 VL - 2077 IS - 012007 SP - 1 EP - 8 PB - IOP Publishing AN - OPUS4-53924 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Winterkorn, R. A1 - Pittner, Andreas A1 - Rethmeier, Michael T1 - Vorteile und Herausforderungen dynamischer Parameterstudien beim Wire Arc Additive Manufacturing von Al-Mg-Si-Legierungen N2 - Der Einsatz von Aluminiumlegierungen als Konstruktionswerkstoff hat in den letzten Jahren stetig zugenommen. Insbesondere höherfeste Aluminiumlegierungen, wie die Vertreter der 6000’er Aluminiumgruppe, rücken Aufgrund ihres hervorragenden Festigkeits- / Gewichtsverhältnisses immer mehr in den Fokus. Vertreter dieser Aluminiumklasse, die als Hauptlegierungselemente Magnesium und Silizium beinhalten, weisen neben der bei allen Aluminiumlegierungen präsenten Affinität zur Porenbildung zusätzlich eine ausgeprägte Heißrissanfälligkeit auf. Die additive Verarbeitung von Al-Mg-Si-Legierungen mittels MSG Verfahren gestaltet sich daher herausfordernd. Neben der Schweißeignung ist die geometrische Gestalt der Schweißraupe für die additive Fertigung von entscheidender Bedeutung. Spurbreite und Spurhöhe sind maßgebliche Größen, die bei der Pfadgenerierung im Hinblick auf Endkonturnähe und der Vermeidung von Ungänzen, Poren und Bildefehlern zu beachten sind. Dieser Beitrag zeigt am Beispiel des Wire Arc Additive Manufacturing von Al-Mg-Si-Legierungen einen Ansatz, mit dem es möglich ist, zeit- und kostenintensive vollfaktorielle Parameterstudien zum Erhalt von Spurgeometrie und Schweißqualität durch dynamische Parameterstudien zu ersetzen. T2 - 41. Assistentenseminar Fügetechnik CY - Magdeburg, Germany DA - 02.09.2020 KW - WAAM PY - 2021 SN - 978-3-96144-141-9 VL - 370 SP - 1 EP - 10 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-52902 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bakir, Nasim A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Observation of the weld pool shape in partial penetration welding and its influence on solidification crack formation for high-power laser beam welding N2 - In this study, steel-glass experiments were conducted to observe the melt pool geometry using a high-speed camera. The high-speed recordings and optical flow analysis show that two main flows take place in form of vortices. The lower vortex drives the melt backwards from the front keyhole wall and thus causes an extension of the melt pool, which is called bulging. This bulging promotes solidification cracking by forming a closed area filled with melt and the accumulation of impurities in the final solidification phase, resulting in low-melting phases which are under tensile stress at the end of solidification. T2 - Lasers in Manufacturing Conference 2021 CY - Online meeting DA - 21.06.2021 KW - Laser beam welding KW - Weld pool shape KW - Solidification craking KW - Partial penetration PY - 2021 SP - 1 EP - 5 AN - OPUS4-53587 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jokisch, T. A1 - Gook, S. A1 - Marko, A. A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Laserstrahlschweißen additiv gefertigter Bauteile: Einsetzbarkeit bestehender Bewertungsvorschriften N2 - Bei der additiven Fertigung im Pulverbett ist die Bauteilgröße durch den Bauraum begrenzt. Das Verbindungsschweißen additiv gefertigter Teile bietet eine Möglichkeit diese Größenbegrenzung aufzuheben. Aufgrund des spezifischen Spannungs- und Gefügezustands im additiv aufgebauten Teil ist jedoch unklar, inwiefern bestehende Bewertungsvorschriften des Verbindungsschweißens auch für Schweißnähte an additiv gefertigten Bauteilen geeignet sind. Dies wird anhand des Laserstrahlschweißens additiv gefertigter Rohrverbindungen untersucht. Die Schweißnähte werden mittels visueller Prüfung, metallografischer Untersuchungen sowie Computertomografie ausgewertet. Die festgestellten Fehlerarten sind vergleichbar zu konventionellen Bauteilen. Dies ist ein Indikator dafür, dass bestehende Bewertungsvorschriften die möglichen auftretenden Defekte auch für Schweißnähte an additiven Bauteilen abbilden. KW - Schweißunregelmäßigkeiten KW - Additive Fertigung KW - Laserstrahlschweißen KW - Schweißeignung PY - 2021 VL - 73 IS - 3 SP - 132 EP - 137 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-53575 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bachmann, Marcel A1 - Artinov, Antoni A1 - Meng, Xiangmeng A1 - Rethmeier, Michael T1 - Numerical study of the bulging effect in deep penetration laser beam welding N2 - This article is devoted to the study of the bulging effect in deep penetration laser beam welding. The numerical results of the investigations are based upon experimental results from previous studies to reveal the relationship between the bulging effect and the hot cracking formation, as well as the mixing of alloying elements in the weld pool. The widening of the molten pool in its center area can be observed in full penetration as well as in partial penetration welds on 8 mm and 12 mm thick structural steel plates, respectively. The weld pool shape is extracted from the simulations to evaluate the extent of the necking of the solidification line as well as the bulging phenomena and its influence on the hot cracking phenomena. Relying on an earlier numerical study utilizing a fixed keyhole, simulation models considering a dynamic keyhole are developed thereto. Additionally, the mixing behavior of alloying elements during partial penetration is investigated. The link between the bulge and the studied phenomena is found to be significant. T2 - Lasers in Manufacturing Conference 2021 CY - Online meeting DA - 21.06.2021 KW - Deep penetration laser beam welding KW - Welding simulation KW - Solidification cracking KW - Bulging effect PY - 2021 SP - 1 EP - 8 AN - OPUS4-52848 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittner, Andreas A1 - Rethmeier, Michael T1 - Ökologische Bilanzierung von Schmelzschweißverfahren unter Berücksichtigung vor- und nachgelagerter Prozessschritte N2 - Ein wesentliches Ziel der deutschen Industriepolitik besteht darin, Rahmenbedingungen zu schaffen, welche die Positionierung nachhaltiger Produkte und Prozesse innerhalb globaler Wertschöpfungsketten ermöglichen und ökoeffiziente Fertigungsprozesse langfristig sichern. In diesem Beitrag werden aktuelle Forschungsarbeiten zur Bewertung der Umweltwirkungen der schweißtechnischen Fertigungskette anhand ausgewählter Schmelzschweißverfahren unter Berücksichtigung vor- sowie nachgelagerter Fertigungsschritte dargestellt. Eine weit verbreitete und standardisierte Methode zur Abschätzung der Umweltwirkungen eines Produkts oder Prozesses ist die Ökobilanzierung. Hierbei stellen die Sachbilanzierung, das heißt die Ermittlung sämtlicher relevanter Energie- und Ressourcenverbräuche während der schweißtechnischen Fertigung, aufgrund des hohen Dokumentationsaufwands, sowie die Ableitung assoziierter Wirkkategorien das größte Hindernis für eine Etablierung und Akzeptanz der Ökobilanzierung in der Praxis dar. Gleichwohl wird seitens Unternehmen, welche als Zulieferer von OEM’s (engl.: original equipment manufacturer) agieren, die Dokumentation des fertigungsspezifischen CO2-Verbrauches gefordert. Ein weiterer Aspekt der Arbeiten beinhaltet Methoden zur automatisierten Erfassung von schweißtechnischen Produktionsdaten sowie deren Nachverfolgbarkeit. Anhand unterschiedlicher Schweißverfahren werden die aus den Produktionsdaten abgeleiteten Energie- und Ressourcenverbräuche automatisiert in die relevanten Umweltwirkungen überführt. Die analysierten Schweißprozesse umfassen dabei ein breites für kleine und mittlere Unternehmen (KMU) relevantes Spektrum. Durch die softwareseitige Bereitstellung der aufgestellten Umweltprofile ist der Anwender in der Lage, Schweißprozesse unter ökologischen Aspekten zu bewerten und die effizienteste Variante zu identifizieren. T2 - Webinar „Zukunft des Bauens – Nachhaltigkeit bei Errichtung, Abbruch und Rückbau“ CY - Online meeting DA - 15.11.2021 KW - Ökobilanzierung KW - Verfahrensvergleich KW - Umweltwirkungen PY - 2021 AN - OPUS4-56649 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittner, Andreas A1 - Rethmeier, Michael T1 - SmartWeld - Innovatives Design und Fertigungskonzept zur Steigerung der Leichtbaupotenziale im Stahlbau N2 - Die Anwendung von Leichtbauprinzipien im Stahlbau, wie z.B. die Verwendung von aufgelösten Tragstrukturen, sog. Jackets-Fundamenten, bietet ein großes Potential zur Reduzierung des Ressourcenverbrauchs, insbesondere im Hinblick auf die benötigte Stahlmenge. In diesem Vortrag zeigen wir die Potenziale einer vollständigen Digitalisierung der schweißtechnischen Fertigungs- und Prüfkette auf, um eine vollautomatische Fertigung sowie Qualitätsprüfung von Rohrknoten als Schlüsselelement von Jackets-Fundamenten zu ermöglichen. Darüber hinaus wird der Zusammenhang zwischen der Geometrie der Nahtform und der resultierenden Ermüdungsfestigkeit durch numerische Methoden unter Einbeziehung bionischer Prinzipien bewertet. Es wird gezeigt, dass Hohlprofilknoten vollautomatisch unter Berücksichtigung von Geometrietoleranzen geschweißt werden können. Darüber hinaus konnte die Nahtform gemäß den numerischen Modellen hergestellt werden, was ein großes Potenzial für eine verlängerte Lebensdauer bietet. Anschließend werden die Verbesserungen bei der Ressourceneffizienz und die Reduzierung der Kohlendioxidemissionen durch eine Lebenszyklusanalyse bewertet. T2 - Bundesverband der Windparkbetreiber Offshore: Tagung der Arbeitsgruppe Engineering CY - Online meeting DA - 26.11.2021 KW - Offshore Windenergieanlagen KW - Gründungsstrukturen KW - Automatisierte Fertigung KW - Aufgelöste Tragstrukturen PY - 2021 AN - OPUS4-56652 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Uhlmann, E. A1 - Düchting, J. A1 - Petrat, T. A1 - Krohmer, E. A1 - Graf, B. A1 - Rethmeier, Michael T1 - Effects on the distortion of Inconel 718 components along a hybrid laser‑based additive manufacturing process chain using laser powder bed fusion and laser metal deposition N2 - The combination of laser powder bed fusion (LPBF), known for its geometrical freedom and accuracy, and the nozzle-based laser metal deposition process (LMD), known for its high build-up rates, has great potential to reduce the additive manufacturing times for large metallic parts. For the industrial application of the LPBF-LMD hybrid process chain, it is necessary to investigate the infuence of the LMD process on the LPBF substrate. In addition, the build plate material also has a signifcant impact on the occurrence of distortion along the additive manufacturing process chain. In the literature, steel build plates are often used in laser-based additive manufacturing processes of Inconel 718, since a good metallurgical Bonding can be assured whilst reducing costs in the production and restoration of the build plates. This paper examines the distortion caused by LMD material deposition and the infuence of the build plate material along the hybrid additive manufacturing process chain. Twin cantilevers are manufactured by LPBF and an additional layer is subsequently deposited with LMD. The distortion is measured in the as-built condition as well as after heat treatment. The efect of diferent LMD hatch strategies on the distortion is determined. The experiments are conducted using the nickel-base alloy Inconel 718. The results show a signifcant infuence of LMD path strategies on distortion, with shorter tool paths leading to less distortion. The remaining distortion after heat treatment is considerably dependent on the material of the build plate. KW - Laser powder bed fusion KW - Directed energy deposition KW - Laser metal deposition KW - Distortion KW - Heat treatment PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-521439 DO - https://doi.org/10.1007/s40964-021-00171-9 SP - 1 EP - 10 PB - Springer-Verlag GmbH CY - Heidelberg AN - OPUS4-52143 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gook, S. A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Verfahren zum fehlerfreien Laserstrahl-MSG-Hybridschweißen geschlossener Rundnähte N2 - In diesem Beitrag werden Ergebnisse der Untersuchungen eines Verfahrens zum fehlerfreien Laserstrahl-MSG-Hybridschweißen von geschlossenen Rundnähten vorgestellt. Das Verfahren zielt auf die Vermeidung von Schweißnahtunregelmäßigkeiten im Überlappbereich einer hybridgeschweißten Rundnaht. Eine Strategie der Prozessführung beim Schließen der Rundnaht wurde entwickelt, mit der ein fehlerfreier Überlappbereich durch die Kontrolle der Erstarrungsbedingungen am Schweißnahtende erreicht wird. Die kontrollierte Wärmeführung wird durch eine Anpassung der Parameter von beiden beteiligten Schweißprozessen, dem Laserstrahl sowie dem Metallschutzgas (MSG)-Schweißprozess, realisiert. Experimentelle Untersuchungen wurden an 12 bis 15 mm dicken Rohrabschnitten durchgeführt. Der Einfluss von Prozessparametern wie der Veränderung des Abbildungsmaßstabs und der Defokussierung des Laserstrahls auf die Erstarrungsbedingungen am Ende der Rundnaht wurde untersucht, um eine optimale Strategie zum Herausführen der Prozessenergie zu finden. Im Rahmen der experimentellen Untersuchungen konnte gezeigt werden, dass eine Defokussierung des Laserstrahls im Bereich zwischen 60 mm und 100 mm über einen kurzen Auslaufbereich der Naht von etwa 15 mm zu einer deutlich besseren Nahtausbildung im Überlappbereich führt. Es konnte eine günstige kelchförmige Schweißnaht ohne eine Tendenz zur Rissbildung erzielt werden. Die Laseroptik mit motorisch angesteuertem Linsensystem ermöglichte dabei eine Vergrößerung des Laserstrahldurchmessers ohne eine Veränderung der Position des MSG-Lichtbogens relativ zur Bauteiloberfläche. KW - Hybrid welding KW - Laser beam welding KW - Pipe manufacturing KW - As-shielded arc welding KW - Weld defects PY - 2021 VL - 73 IS - 3 SP - 116 EP - 121 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-52365 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Straße, Anne A1 - Gumenyuk, Andrey A1 - Scheuschner, Nils A1 - Altenburg, Simon A1 - Pignatelli, Giuseppe A1 - Gornushkin, Igor B. A1 - Baensch, Franziska A1 - Rethmeier, Michael T1 - In-situ Prozessüberwachung beim Laser-Pulver-Auftragschweißen (LPA) mittels Thermografie, optischer Emissionsspektroskopie (OES) und Schallemissionsanalyse (SEA) N2 - Vor allem in den letzten Jahren ist das Interesse der Industrie an der additiven Fertigung deutlich gestiegen. Die Vorteile dieser Verfahren sind zahlreich und ermöglichen eine ressourcenschonende, kundenorientierte Fertigung von Bauteilen, welche zur stetigen Entwicklung neue Anwendungsbereiche und Werkstoffe führen. Aufgrund der steigenden Anwendungsfälle, nimmt auch der Wunsch nach Betriebssicherheit unabhängig von anschließenden kostenintensiven zerstörenden und zerstörungsfreien Prüfverfahren zu. Zu diesem Zweck werden im Rahmen des von der BAM durchgeführten Themenfeldprojektes „Prozessmonitoring in Additive Manufacturing“ verschiedenste Verfahren auf ihre Tauglichkeit für den in-situ Einsatz bei der Prozessüberwachung in der additiven Fertigung untersucht. Hier werden drei dieser in-situ Verfahren, die Thermografie, die optische Emissionsspektroskopie und die Schallmissionsanalyse für den Einsatz beim Laser-Pulver-Auftragschweißen betrachtet. T2 - 41. Assistentenseminar der Füge- und Schweißtechnik CY - Magdeburg, Germany DA - 02.09.2020 KW - Laser-Pulver-Auftragschweißen (LPA) KW - Thermographie KW - Optische Emissionsspektroskopie (OES) KW - Schallemissionsanalyse (SEA) PY - 2021 SN - 978-3-96144-141-9 VL - 370 SP - 132 EP - 140 PB - DVS MEdia CY - Düsseldorf AN - OPUS4-53967 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Raute, J. A1 - Marquardt, R. A1 - Biegler, M. A1 - Rethmeier, Michael T1 - Untersuchung zum Elektronenstrahlschweißen additiv gefertigter Ni-Basis-Bauteile N2 - Die vorliegende Untersuchung befasst sich mit dem Einfluss des Additive Manufacturing auf die Schweißeignung von Bauteilen aus Inconel 718. Hierfür wurden Proben mittels DED und L-PBF hergestellt und ihr Verhalten in Blindschweißversuchen anhand eines Vergleichs mit konventionellen Gussblechen untersucht. Im zweiten Schritt wurden die verschiedenen additiv hergestellten Proben mit dem Gussmaterial im I-Stoß sowie untereinander verschweißt. Als Schweißverfahren wurde für alle Proben das Elektronenstrahlschweißen angewandt. Zur Auswertung wurde anhand von Schliffen das Nahtprofil vermessen und die Proben auf Poren und Risse untersucht. Zusätzlich wurde die Dichte vermessen und eine Prüfung auf Oberflächenrisse durchgeführt. Das AM-Material zeigte dabei Unterschiede in Nahtform und Defektneigung im Vergleich zum Gusswerkstoff. Insbesondere die DED-proben neigten unter bestimmten Parameterkonstellationen verstärkt zu Porenbildung. Risse konnten nicht beobachtet werden. Trotz auftretender Nahtunregelmäßigkeiten wurde in den kombinierten AM-Schweißproben die Bewertungsgruppe C erreicht. Eine Prüfung der bestehenden Regelwerke zur Schweißnahtbewertung anhand der gewonnenen Erkenntnisse zu additiv gefertigten Proben im Elektronenstrahlschweißprozess zeigte keinen Ergänzungsbedarf. T2 - #additivefertigung: Metall in bestForm CY - Essen, Germany DA - 26.10.2022 KW - Elektronenstrahlschweißen KW - Additive Fertigung KW - Schweißnahtbewertung PY - 2022 SN - 978-3-96144-202-7 VL - 383 SP - 81 EP - 92 PB - DVS-Media GmbH AN - OPUS4-56173 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Marko, A. A1 - Bähring, S. A1 - Raute, J. A1 - Biegler, M. A1 - Rethmeier, Michael T1 - Prognose von Qualitätsmerkmalen durch Anwendung von KI-Methoden beim Directed 10 Energy Deposition N2 - Dieser Beitrag enthält die Ergebnisse eines im Rahmen der DVS Forschung entwickelten Ansatzes zur Qualitätssicherung im Directed Energy Deposition. Es basiert auf der Verarbeitung verschiedener während des Prozesses gesammelter Sensordaten unter Anwendung Künstlicher Neuronale Netze (KNN). So ließen sich die Qualitätsmerkmale Härte und Dichte auf der Datenbasis von 50 additiv gefertigten Probenwürfel mit einer Abweichung < 2 % vorhersagen. Des Weiteren wurde die Übertragbarkeit des KNN auf eine Schaufelgeometrie untersucht. Auch hier ließen sich Härte und Dichte hervorragend prognostizieren (Abweichung < 1,5 %), sodass der Ansatz als validiert betrachtet werden kann. KW - Kl KW - Directed Energy Depositio KW - Qualitätssicherung PY - 2022 SN - 0036-7184 VL - 74 IS - 10 SP - 672 EP - 679 PB - DVS Media CY - Düsseldorf AN - OPUS4-56284 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Raute, J. A1 - Biegler, M. A1 - Rethmeier, Michael T1 - Untersuchung zur Herstellung von Cu-Strukturen mittels Wire Electron Beam Additive Manufacturing N2 - Das Additive Manufacturing gewinnt zunehmend an Bedeutung für die Fertigung metallischer Bauteile im industriellen Umfeld. Hierbei wird zunehmend auch auf drahtförmige Ausgangswerkstoffe gesetzt, da diese Vorteile im Handling bieten, bereits in der Industrie etabliert sind und sich in der Regel durch geringere Beschaffungskosten auszeichnen. In den letzten Jahren entwickelte sich neben den bereits im großen Umfeld untersuchten Wire-DED-Verfahren auch eine Prozessvariante unter Nutzung des Elektronenstrahls zur industriellen Marktreife. Dabei zeigt die als Wire Electron Beam Additive Manufacturing bezeichnete Technologie besondere Vorteile gegenüber anderen, zumeist Laser- oder Lichtbogen-basierten DED-Prozessen. Das Verfahren bietet vor allem Potenzial für die Verarbeitung von hochleitfähigen, reflektierenden oder oxidationsgefährdeten Werkstoffen. Insbesondere für die Herstellung von Bauteilen aus Kupferlegierungen zeigt sich der Elektronenstrahl als besonders geeignet. Um das Verfahren einem breiten Anwenderkreis in der Industrie zugänglich zu machen, fehlen jedoch übergreifende Daten zu Leistungsfähigkeit, Prozessgrenzen und Anwendungsmöglichkeiten. Die vorliegende Untersuchung beschäftigt sich mit dieser Problemstellung am Beispiel zweier Cu-Werkstoffe. Dabei werden ein korrosionsbeständiger Werkstoff aus dem maritimen Bereich sowie eine Bronze mit guten Verschleißeigenschaften aus dem Anlagenbau getestet. Über mehrstufige Testschweißungen wurden die physikalisch möglichen Prozessgrenzen ermittelt und Rückschlüsse über die Eignung der Parameter zum additiven Aufbau gezogen. Hierfür wurden zunächst optimale Bereiche für den Energieeintrag anhand von Volumenenergie sowie mögliche Schweißgeschwindigkeiten untersucht. Anschließend wurde die Skalierbarkeit des Prozesses anhand von Strahlstrom und Drahtvorschub getestet. Als wesentliche Zielgrößen wurden dabei Spurgeometrie, Aufmischung und Härte herangezogen. Die Eignung der ermittelten Parameter wurde im letzten Schritt exemplarisch anhand einer additiven Testgeometrie in Form eines Zylinders nachgewiesen. T2 - DVS Congress 2022 Große Schweißtechnische Tagung DVS CAMPUS CY - Koblenz, Germany DA - 19.09.2022 KW - WEBAM KW - Electron beam KW - EBAM KW - Wire electron beam additive manufacturing PY - 2022 SN - 978-3-96144-189-1 VL - 382 SP - 446 EP - 454 PB - DVS Media AN - OPUS4-56058 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rethmeier, Michael A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey T1 - Welding of thick metal plates with laser - Where are the limits? N2 - -With modern high-power lasers (and vacuum) penetration around 100 mm is possible -Important for industrial applications: single-pass full penetration welds with tolerances -Contactless EM-backing helps to overcome many main restrictions: -Single-pass HLAW of up to 30 mm can be realized with 20 kW laser power -Increase of the gap bridgeability and misalignement of edges -Lower sensitivity to manufacturing tolerances and edge quality; samples can be prepared by a plasma-cut instead of time-consuming milling process -Gives the possibility to increase the welding parameter window and cooling rate so that the required mechanical properties can be reached -Improved filler wire mixing behaviour T2 - AKL22 - International Laser Technology Congress CY - Aachen, Germany DA - 04.05.2022 KW - Laser hybrid welding KW - Thick-walled steel KW - High-power laser KW - Electromagnetic backing PY - 2022 AN - OPUS4-56367 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Pittner, Andreas A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Einlagiges MSG-Hochleistungsschweißen von dickwandigen Baustählen mit kontaktloser elektromagnetischer Schmelzbadsicherung N2 - Diese Arbeit zeigt erstmals die Anwendung einer elektromagnetischen Schmelzbadsicherung beim einlagigen MSG-Schweißen von dickwandigen Stählen. Die innovativen Entwicklungen im Bereich des Lichtbogenschweißverfahrens ermöglichen eine Erhöhung der Abschmelzleistung, um die Einschweißtiefe zu steigern. Somit kann die Lagenanzahl reduziert und die Produktivität gesteigert werden. Allerdings besteht insbesondere beim einlagigen Schweißen von dickwandigen Bauteilen in PA-Position ein erhöhtes Risiko für das gravitationsbedingte Austropfen der Schmelze an der Wurzel. Zur Verhinderung werden Badsicherungen eingesetzt, die mechanisch angebracht und nach dem Schweißen entfernt werden müssen, was zeit- und kostenintensiv ist. Die im Rahmen dieser Studie eingesetzte elektromagnetische Schmelzbadsicherung wirkt dem gravitationsbedingten Austropfen der Schmelze entgegen und kompensiert den hydrostatischen Druck. Sie wirkt kontaktlos, was im Gegensatz zu herkömmlichen Badsicherungen vorteilhaft ist, so dass auf eine zeit- und kostenintensive Nachbearbeitung der Schweißnahtwurzel verzichtet werden kann. Das auf extern angelegten oszillierenden Magnetfeldern beruhende Verfahren wird dabei unterhalb des zu schweißenden Bauteils positioniert. Die Magnetfeldlinien sind quer zur Schweißrichtung ausgerichtet, sodass längs zur Schweißrichtung Wirbelströme im Werkstück und eine stets nach oben gerichtete Lorentzkraft generiert werden. Mit Hilfe der elektromagnetischen Badsicherung konnten beim einlagigen MSG-Schweißen von bis zu 10 mm dicken Blechen die Tropfenbildung vermieden werden. Die innovative Technologie ermöglicht es, dickwandige Bauteile einlagig zu schweißen und reduziert die Nachbearbeitungszeiten und -kosten deutlich. T2 - DVS Congress 2022 - Große Schweißtechnische Tagung CY - Koblenz, Germany DA - 19.09.2022 KW - Elektromagnetische Schmelzbadsicherung KW - Hochleistungsschweißen KW - MSG-Schweißen PY - 2022 SN - 978-3-96144-189-1 VL - 382 SP - 640 EP - 645 PB - DVS Media GmbH AN - OPUS4-56371 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Brunner-Schwer, C. A1 - Knöfel, F. A1 - Gook, S. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Laserstrahlhybridschweissen von Türmen für Windkraftanlagen Ökonomische und ökologische Vorteile N2 - Das Laserstrahlhybridschweißen ist beim Schweißen von Türmen für Windkraftanlagen eine Alternative zum Unterpulverschweißen von Dickblechen in Mehrlagentechnik und bietet hier ökonomische und ökologische Vorteile. Der industrielle Einsatz des Verfahrens ist jedoch durch prozessspezifische Herausforderungen eingeschränkt. Die im Beitrag beschriebene kontaktlose elektromagnetische Badstütze dient zur Erweiterung des Verfahrenspotenzials im Dickblechbereich >15 mm. KW - Elektromagnetische Badstütze KW - Laserhybridschweißen KW - Windkraftanlagen KW - Ökonomische und ökologische Vorteile PY - 2022 VL - 7 SP - 340 EP - 347 PB - DVS Media GmbH AN - OPUS4-56372 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Improvement of Charpy impact toughness by using an AC magnet backing system for laser hybrid welding of thick S690QL steels N2 - The study deals with the influence of the heat input and the resulting cooling times on the microstructure and Charpy impact toughness of single-pass laser hybrid welded 20-mm thick high-strength steel S690QL. The main focus is on the change of the mechanical properties over the entire seam thickness. The cooling times were measured in-situ using a pyrometer and an optical fibre in three different depths of the seam where Charpy impact test specimens were also later taken. Thereby, three different heat inputs from 1.3 kJ/mm to 2 kJ/mm were investigated. Despite the observed decreased values of both t8/5-cooling time and the Charpy impact toughness in the root part of the seam, the required impact toughness of 38 J/cm2 could be reached in dependance on applied heat input, especially at the heat input of 1.6 kJ/mm. T2 - 12th CIRP conference on photonic technologies [lane 2022] CY - Fürth, Germany DA - 04.09.2022 KW - Thick-plate welding KW - Laser hybrid welding KW - Electromagnetic backing KW - Charpy impact toughness KW - Thermal cycles PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-563731 DO - https://doi.org/10.1016/j.procir.2022.08.067 VL - 111 SP - 462 EP - 465 PB - Elsevier B.V. AN - OPUS4-56373 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jokisch, T. A1 - Gook, S. A1 - Marko, A. A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Laser beam welding of additive manufactured components: Applicability of existing valuation regulations N2 - With additive manufacturing in the powder bed, the component size is limited by the installation space. Joint welding of additively manufactured parts offers a possibility to remove this size limitation. However, due to the specific stress and microstructure state in the additively built material, it is unclear to what extent existing evaluation rules of joint welding are also suitable for welds on additive components. This is investigated using laser beam welding of additively manufactured pipe joints. The welds are evaluated by means of visual inspection, metallographic examinations as well as computed tomography. The types of defects found are comparable to conventional components. This is an indicator that existing evaluation regulations also map the possible defects occurring for weld seams on additive components. KW - Weld imperfections KW - Additive manufacturing KW - Weldability KW - Laser welding PY - 2022 VL - 2 SP - 109 EP - 113 PB - DVS Media GmbH AN - OPUS4-56374 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Elektromagnetische Schmelzbadbeeinflussung beim Laserhybridschweißen von Dickblechen N2 - Die technischen Entwicklungen in der Lasertechnologie in den letzten Jahrzehnten haben eine neue Generation von Hochleistungslasersystemen im Leistungsbereich bis zu 100 kW auf den Markt gebracht. Dennoch ist die industrielle Anwendung des Hochleistungslaserstrahlschweißens auf bis zu 15 mm dicke Bleche beschränkt. Mögliche Ursachen der Einschränkungen des Verfahrens sind z.B. die Sensibilität des Verfahrens auf Fertigungstoleranzen wie Spalt und Kantenversatz, die erhöhte Tropfenbildung bei höheren Blechdicken und eine inhomogene Verteilung des Zusatzwerkstoffes beim Laserhybridschweißen. In dieser Studie wird ein auf extern angelegte Magnetfelder basierte elektromagnetische Schmelzbadstütze eingesetzt, um die Grenzen des Verfahrens zu erweitern und die Herausforderungen zu minimieren. Der wesentliche Vorteil der elektromagnetischen Schmelzbadstütze ist, dass sie berührungslos arbeitet. Mit Hilfe der elektromagnetischen Schmelzbadstütze konnten bei 20 mm dicken Proben aus S355J2 die Tropfenbildung an der Wurzel vermieden werden. Zudem wurde der Einfluss der Kantenqualität auf die Schweißnahtqualität untersucht, wobei verschiedene Schneidverfahren zur Kantenvorbereitung eingesetzt wurden, wie z.B. Plasma-, Brenn- oder Laserschneiden. Es konnte gezeigt werden, dass auch bei schlechteren Kantenvorbereitung im Gegensatz zu gefrästen Bauteilen die Werkstoffe einlagig mittels Laserhybridschweißen bei einer hohen Schweißnahtqualität gefügt werden konnten. Bei plasmageschnittenen Proben wurden zudem eine Spaltüberbrückbarkeit bzw. Kantenversatz von bis zu 2 mm sicher überbrückt. Des Weiteren war es mit Hilfe der externen Magnetfelder möglich, die Durchmischung des Zusatzwerkstoffes über die gesamte Schweißnahttiefe deutlich zu homogenisieren. T2 - 42. Assistentenseminar der Wissenschaftlichen Gesellschaft Fügetechnik e.V. CY - Blankenau, Germany DA - 06.10.2021 KW - Elektromagnetische Schmelzbadstütze KW - Laserhybridschweißen KW - Dickblech PY - 2022 VL - 385 SP - 1 EP - 7 PB - DVS Media GmbH AN - OPUS4-56375 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bakir, Nasim A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Influence of the weld pool geometry on solidification cracking in partial penetration high power laser beam welding N2 - Solidification cracking is still a serious problem in laser beam welding, especially in the welding of thick-walled plates. The influence of weld pool geometry on solidification cracking in partial penetration welding of thick plates is investigated within scope of this study. Therefore, a specific experimental setup of steel and quartz glass in butt configuration and on the side with high-speed camera were used to record the weld pool shape. In addition, the influence of laser inclination angle on the weld pool geometry and on solidification crack formation was investigated. The results show a bulge in the weld pool root, which is separated from an upper region by a necking region. This leads to a case where there are three different longitudinal region lengths with different solidification zones. This temporal sequence of solidification strongly promotes the formation of solidification cracks in the weld root. T2 - 12th CIRP Conference on photonic technologies (LANE 2022) CY - Fürth, Germany DA - 04.09.2022 KW - Laser beam welding KW - Partial penetration KW - Weld pool shape PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-563940 DO - https://doi.org/10.1016/j.procir.2022.08.174 VL - 111 SP - 397 EP - 400 PB - Elsevier B.V. AN - OPUS4-56394 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bachmann, Marcel A1 - Meng, Xiangmeng A1 - Artinov, Antoni A1 - Rethmeier, Michael T1 - Evaluation of narrowed weld pool shapes and their effect on resulting potential defects during deep penetration laser beam welding N2 - This study presents mechanisms of the evolution of a narrowed region in the weld pool center during deep penetration laser beam welding. In numerous numerical studies presented in this study, it was also found that the local reduction of the weld pool size can cause detrimental effects on the melt flow behavior and the resulting properties of the welds. A particularly large influence of this effect was identified in three aspects. Firstly, the local variation of the solidification sequence of the weld pool causes an increase in the hot-cracking susceptibility due to a locally delayed solidification. Secondly, it was proven that a change in the local length and width of the weld pool is associated with an adverse impact on the potential flow routes of the molten material that induces stronger local variations of its solidification. Thus, the element mixing, e.g. during the welding with filler materials, is blocked. This leads to a non-homogeneous chemical composition of the final weld and can cause undesired effects on the final material properties. Finally, another observed effect is related to the reduced ability of process pores to reach the top surface. As this type of porosity is usually produced around the keyhole tip, the change of the fluid flow regime above this area plays a significant role in determining the final path of the pores until the premature solidification in the middle of the weld pool captures them. This study summarizes mainly numerical results which were supported by selected experimental validation results. T2 - International Congress of Applications of Lasers & Electro-Optics 2022 CY - Orlando, FL, USA DA - 17.10.2022 KW - Weld pool shape KW - Laser beam welding KW - Solidification KW - Porosity KW - Numerical process simulation PY - 2022 SP - 1 AN - OPUS4-56532 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Artinov, Antoni A1 - Rethmeier, Michael T1 - The influence of the free surface reconstruction on the spatial laser energy distribution in high power laser beam welding modeling N2 - An accurate and efficient description of the spatial distribution of laser energy is a crucial factor for the modeling of laser material processing, e.g., laser welding, laser cutting, or laser-based additive manufacturing. In this study, a 3D heat transfer and fluid flow model coupled with the volume-of-fluid algorithm for free surface tracking is developed for the simulation of molten pool dynamics in high-power laser beam welding. The underlying laser-material interactions, i.e., the multiple reflections and Fresnel absorption, are considered by a ray-tracing method. Two strategies of free surface reconstruction used in the ray-tracing method are investigated: a typical piecewise linear interface calculation (PLIC)-based method and a novel localized Level-Set method. The PLIC-based method is discrete, resulting in non-continuous free surface reconstruction. In the localized Level-Set method, a continuous free surface is reconstructed, and thus the exact reflection points can be determined. The calculated spatial laser energy distribution and the corresponding molten pool dynamics from the two methods are analyzed and compared. The obtained numerical results are evaluated with experimental measurements to assure the validity of the proposed model. It is found that distinct patterns of the beam multiple reflections are obtained with the different free surface reconstructions, which shows significant influence not only on the molten pool behaviors but also on the localized keyhole dynamics. T2 - International Congress of Applications of Lasers & Electro-Optics 2022 CY - Orlando, FL, USA DA - 17.10.2022 KW - Laser beam welding KW - laser energy distribution KW - Weld pool dynamics KW - Ray-tracing PY - 2022 SP - 1 EP - 9 AN - OPUS4-56533 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Winterkorn, René A1 - Pittner, Andreas A1 - Rethmeier, Michael T1 - Lichtbogenbasierte additive Fertigung dickwandiger Strukturen aus einer höherfesten Al-Mg-Si-Aluminiumlegierungen N2 - Die lichtbogenbasierte, additive Fertigung ist dank hoher erreichbarer Aufbauraten und nahezu uneingeschränktem Bauraum zur Fertigung großvolumiger Bauteile prädestiniert. Die Kombination etablierter Maschinenkomponenten aus Robotertechnik, Schweißtechnik und Sensorik ermöglicht den präzisen schichtweisen Materialauftrag. Die Wirkmechanismen zwischen Prozessparametern und den daraus resultierenden mechanisch-technologischen Eigenschaften der additiv gefertigten Bauteile stellen eine Herausforderung dar. Dies gilt insbesondere auch für dickwandige Bauteile. Bei der Fertigung von Bauteilen aus höherfesten Al-Mg-Si-Aluminiumlegierungen ist aufgrund der hohen Anfälligkeit für Erstarrungsrisse und der Neigung zu wasserstoffinduzierter Porosität im besonderen Maße auf das Temperaturregime und die gewählte Aufbaustrategie zu achten. Der Einfluss der Prozessparameter auf die Bauteilqualität wurde durch die Analyse der Größe und Verteilung von Poren sowie der resultierenden Festigkeit untersucht. Darüber hinaus wurde der Einfluss einer Wärmenachbehandlungsstrategien auf das Festigkeitsverhalten analysiert. Es konnte gezeigt werden, dass dickwandige Strukturen aus höherfesten Al-Mg-Si-Aluminiumlegierungen mit mechanischen Kennwerten im Bereich des Referenzmaterials mittels MSGLichtbogenverfahren additiv gefertigt werden können. T2 - Additive Fertigung – Werkstoffe – Prozesse – Wärmebehandlung 2022 CY - Bremen, Germany DA - 29.06.2022 KW - WAAM KW - Al-Mg-Si-Legierungen KW - Porosität KW - Wärmenachbehandlung KW - Mechanisch technologische Kennwerte PY - 2022 SP - 169 EP - 181 PB - Arbeitsgemeinschaft Wärmebehandlung und Werkstofftechnik e. V. CY - Bremen AN - OPUS4-56673 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gook, S. A1 - El-Sari, B. A1 - Biegler, M. A1 - Rethmeier, Michael A1 - Lichtenthäler, F. A1 - Stark, M. T1 - Multiple-wire submerged arc welding of high-strength fine-grained steels N2 - Ensuring the required mechanical-technological properties of welds is a critical issue in the application of multi-wire submerged arc welding processes for welding high-strength fine-grained steels. Excessive heat input is one of the main causes for microstructural zones with deteriorated mechanical properties of the welded joint, such as a reduced notched impact strength and a lower structural robustness. A process variant is proposed which reduces the weld volume as well as the heat input by adjusting the welding wire configuration as well as the energetic parameters of the arcs, while retaining the advantages of multiwire submerged arc welding such as high process stability and production speed. KW - Submerged arc welding KW - High-strength fine-grained steels KW - Mechanical properties of the joints KW - Energy parameters of the arc PY - 2022 DO - https://doi.org/10.37434/tpwj2022.01.02 SN - 0957-798X IS - 1 SP - 9 EP - 13 PB - Paton Publishing House CY - Kiev AN - OPUS4-54701 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rethmeier, Michael A1 - Gumenyuk, Andrey A1 - Artinov, Antoni A1 - Meng, Xiangmeng A1 - Bakir, Nasim A1 - Üstündag, Ömer A1 - Bachmann, Marcel T1 - The bulging effect and its relevance in high power laser beam welding N2 - The present work deals with the recently confirmed widening of the weld pool interface, known as a bulging effect, and its relevance in high power laser beam welding. A combined experimental and numerical approach is utilized to study the influence of the bulge on the hot cracking formation and the transport of alloying elements in the molten pool. A technique using a quartz glass, a direct-diode laser illumination, a high speed camera, and two thermal imaging cameras is applied to visualize the weld pool geometry in the longitudinal section. The study examines the relevance of the bulging effect on both, partial and complete penetration, as well as for different sheet thicknesses ranging from 8 mm to 25 mm. The numerical analysis shows that the formation of a bulge region is highly dependent on the penetration depth and occurs above 10 mm penetration depth. The location of the bulge correlates strongly with the cracking location. The obtained experimental and numerical results reveal that the bulging effect increases the hot cracking susceptibility and limits the transfer of alloying elements from the top of the weld pool to the weld root T2 - The 18th Nordic Laser Materials Processing Conference CY - Lulea, Sweden DA - 18.01.2022 KW - Laser beam welding KW - Melt pool dinamics PY - 2022 AN - OPUS4-54333 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Böhne, C. A1 - Meschut, G. A1 - Biegler, M. A1 - Rethmeier, Michael T1 - The Influence of Electrode Indentation Rate on LME Formation during RSW N2 - During resistance spot welding of zinc-coated advanced high-strength steels (AHSSs) for automotive production, liquid metal embrittlement (LME) cracking may occur in the event of a combination of various unfavorable influences. In this study, the interactions of different welding current levels and weld times on the tendency for LME cracking in third-generation AHSSs were investigated. LME manifested itself as high penetration cracks around the circumference of the spot welds for welding currents closely below the expulsion limit. At the same time, the observed tendency for LME cracking showed no direct correlation with the overall heat input of the investigated welding processes. To identify a reliable indicator of the tendency for LME cracking, the local strain rate at the origin of the observed cracks was analyzed over the course of the welding process via finite element simulation. While the local strain rate showed a good correlation with the process-specific LME cracking tendency, it was difficult to interpret due to its discontinuous course. Therefore, based on the experimental measurement of electrode displacement during welding, electrode indentation velocity was proposed as a descriptive indicator for quantifying cracking tendency. KW - Liquid Metal Embrittlement (LME) KW - Crack KW - Resistance Spot Welding (RSW) KW - Advanced High-Strength Steel (AHSS) KW - Welding Current KW - Heat Input KW - Simulation PY - 2022 DO - https://doi.org/10.29391/2022.101.015 SN - 0043-2296 VL - 101 IS - 7 SP - 197-s EP - 207-s PB - American Welding Society CY - New York, NY [u.a.] AN - OPUS4-55600 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Marquardt, R. A1 - Biegler, M. A1 - Rethmeier, Michael T1 - Funktional gradierte Materialien auf Basis von Stellite und Stahl im Laserpulver-Auftragschweißen N2 - Das Hinzufügen von Stellite auf Stahl ist eine typische Vorgehensweise um Bauteile gegen Verschleiß und Korrosion zu schützen. Der Sprung in den Materialeigenschaften kann jedoch zu Rissen und somit zum Versagen der Beschichtung führen. Um die Lebensdauer von Beschichtungen zu erhöhen wird daher ein gradierter Übergang mit verschiedenen Materialpaarungen untersucht. T2 - 13. Fachtagung Verschleiss- und Korrosionsschutz von Bauteilen durch Auftragschweißen CY - Haale (Saale), Germany DA - 22.06.2022 KW - FGM KW - DED KW - AM KW - Functionally Graded Materials KW - Additive Manufacturing KW - Directed Energy Deposition PY - 2022 SP - 66 EP - 73 AN - OPUS4-55504 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Marko, A. A1 - Bähring, S. A1 - Raute, J. A1 - Biegler, M. A1 - Rethmeier, Michael T1 - Quality Prediction in Directed Energy Deposition Using Artificial Neural Networks Based on Process Signals N2 - The Directed Energy Deposition process is used in a wide range of applications including the repair, coating or modification of existing structures and the additive manufacturing of individual parts. As the process is frequently applied in the aerospace industry, the requirements for quality assurance are extremely high. Therefore, more and more sensor systems are being implemented for process monitoring. To evaluate the generated data, suitable methods must be developed. A solution, in this context, was the application of artificial neural networks (ANNs). This article demonstrates how measurement data can be used as input data for ANNs. The measurement data were generated using a pyrometer, an emission spectrometer, a camera (Charge-Coupled Device) and a laser scanner. First, a concept for the extraction of relevant features from dynamic measurement data series was presented. The developed method was then applied to generate a data set for the quality prediction of various geometries, including weld beads, coatings and cubes. The results were compared to ANNs trained with process parameters such as laser power, scan speed and powder mass flow. It was shown that the use of measurement data provides additional value. Neural networks trained with measurement data achieve significantly higher prediction accuracy, especially for more complex geometries. KW - DED KW - Artificial neural network KW - Data preparation KW - Quality assurance KW - Process monitoring PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-555063 DO - https://doi.org/10.3390/app12083955 SN - 2076-3417 VL - 12 IS - 8 SP - 1 EP - 13 PB - MDPI CY - Basel AN - OPUS4-55506 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Straße, Anne A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael ED - Schmidt, M. ED - Vollertsen, F. ED - Schmidt, B. M. T1 - Preliminary study to investigate the applicability of optical strain measurement technique for the detection of hot cracks in laser metal deposited layers N2 - Laser metal deposition (LMD) as an additive manufacturing technique became increasingly important in recent years and thus the demand for component safety. This is the reason, for the need for reliable in-situ defect detection techniques. For laser beam weld seams an optical measurement technique based on an optical flow algorithm was successfully used to define the critical straining conditions that lead to hot cracking. This algorithm was adapted for bead-on-plate weld seams on LMD deposited layers of IN718 alloy while performing external strain on the specimen in an externally loaded hot cacking test facility. The resulting transversal hot cracks along the weld seam were localized via X-Ray inspection and the type of cracking confirmed by Scanning Electron Microscopy (SEM). The strain distribution was measured in the vicinity of the solidification front and correlated to the detected hot cracks. Based on the results this technique could be adopted for LMD experiments. T2 - 12th CIRP Conference on Photonic Technologies [LANE 2022] CY - Fürth, Germany DA - 04.09.2022 KW - Laser Metal Deposition (LMD) KW - Strain measurement KW - Optical flow KW - Critical strain PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-556445 DO - https://doi.org/10.1016/j.procir.2022.08.034 VL - 111 SP - 335 EP - 339 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-55644 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Straße, Anne A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Study on Duplex Stainless Steel Powder Compositions forthe Coating of Thick Plates for Laser Beam Welding N2 - Duplex stainless steels combine the positive properties of its two phases, austenite and ferrite. Due to its good corrosion resistance, high tensile strength and good ductility it has multiple applications. But laser beam welding of duplex steels changes the balanced phase distribution in favor of ferrite. This results in a higher vulnerability to corrosion and a lower ductility. In this study different powder combinations consisting of duplex and nickel for coating layers by laser metal deposition are investigated. Afterwards laser tracks are welded, and the temperature cycles measured. The ferrite content of the tracks are analyzed by feritscope, metallographic analysis and Electron Backscatter Diffraction. The goal is the development of a powder mixture allowing for a duplex microstructure in a two-step process, where firstly the edges of the weld partners are coated with the powder mixture by LMD and secondly those edges are laser beam welded. The powder mixture identified by the pretests is tested in the two-step process and analyzed by metallographic analysis, energy dispersive X-ray spectroscopy and Vickers hardness tests. The resulting weld seams show a balanced duplex microstructure with a homogenous nickel distribution and a hardness of the weld seam similar to the base material. KW - Duplex AISI 2205 KW - Stainless Steel KW - Laser Beam Welding KW - Nickel KW - Laser Metal Deposition PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-554663 DO - https://doi.org/10.1002/adem.202101327 SN - 1438-1656 VL - 24 IS - 6 SP - 1 EP - 11 PB - Wiley-VCH CY - Weinheim AN - OPUS4-55466 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittner, Andreas A1 - Rethmeier, Michael T1 - Ökobilanzierung schweißtechnischer Fertigungsverfahren - Methodik, Einflussgrößen und Implementierung N2 - Ein wesentliches Ziel der deutschen Industriepolitik besteht darin, Rahmenbedingungen zu schaffen, welche die Positionierung nachhaltiger Produkte und Prozesse innerhalb globaler Wertschöpfungsketten ermöglichen und ökoeffiziente Fertigungsprozesse langfristig sichern. In diesem Beitrag werden aktuelle Forschungsarbeiten zur Bewertung der Umweltwirkungen der schweißtechnischen Fertigungskette anhand ausgewählter Schmelzschweißverfahren unter Berücksichtigung vor- sowie nachgelagerter Fertigungsschritte dargestellt. Eine weit verbreitete und standardisierte Methode zur Abschätzung der Umweltwirkungen eines Produkts oder Prozesses ist die Ökobilanzierung. Hierbei stellen die Sachbilanzierung, das heißt die Ermittlung sämtlicher relevanter Energie- und Ressourcenverbräuche während der schweißtechnischen Fertigung, aufgrund des hohen Dokumentationsaufwands, sowie die Ableitung assoziierter Wirkkategorien das größte Hindernis für eine Etablierung und Akzeptanz der Ökobilanzierung in der Praxis dar. Gleichwohl wird seitens Unternehmen, welche als Zulieferer von OEM’s (engl.: original equipment manufacturer) agieren, die Dokumentation des fertigungsspezifischen CO2-Verbrauches gefordert. Ein weiterer Aspekt der Arbeiten beinhaltet Methoden zur automatisierten Erfassung von schweißtechnischen Produktionsdaten sowie deren Nachverfolgbarkeit. Anhand unterschiedlicher Schweißverfahren werden die aus den Produktionsdaten abgeleiteten Energie- und Ressourcenverbräuche automatisiert in die relevanten Umweltwirkungen überführt. Die analysierten Schweißprozesse umfassen dabei ein breites für kleine und mittlere Unternehmen (KMU) relevantes Spektrum. Durch die softwareseitige Bereitstellung der aufgestellten Umweltprofile ist der Anwender in der Lage, Schweißprozesse unter ökologischen Aspekten zu bewerten und die effizienteste Variante zu identifizieren. T2 - Woche der Fügetechnik 2022, HWK Münster CY - Online meeting DA - 30.11.2022 KW - Ökobilanzierung KW - Verfahrensvergleich KW - Schweißprozesse KW - Umweltwirkungen KW - Implementierung PY - 2022 AN - OPUS4-56650 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - El-Sari, B. A1 - Biegler, M. A1 - Rethmeier, Michael T1 - Einfluss von Oberflächenbeschichtungen auf die flüssigmetallinduzierte Rissbildung beim Widerstandspunktschweißen von hochfesten Stahlfeinblechen BT - Schlussbericht vom 15.09.2022 zu IGF-Vorhaben Nr. 20812 N : Berichtszeit: 01.10.2019 bis 31.03.2022 N2 - Die Beschichtung hochfester Stahlfeinbleche beeinflusst das Auftreten von flüssigmetallinduzierter Rissbildung (LME). Daher wurden in dieser Arbeit industrieübliche Beschichtungen bei gleichem Grundwerkstoff hinsichtlich ihres Aufbaus und chemischer Zusammensetzung charakterisiert und bezüglich ihrer LME Anfälligkeit untersucht. Aus dieser vergleichenden Untersuchung heraus wurden Potentiale für die Widerstandsfähigkeit gegen LME identifiziert. Diese Potentiale werden experimentell durch den Einsatz einer von der Forschungsstelle entwickelten Methode überprüft. Gegenstand der Untersuchungen waren neben unbeschichteten Proben industrieübliche Zinküberzüge wie Elektrolytisch verzinkt, Feuerverzinkt, Galvannealed und Zink-Magnesium Beschichtungen. Die LME Anfälligkeit dieser unterschiedlichen Überzüge wird mit einem Schweißen unter Zugbelastung Versuchsaufbau untersucht. Dabei ergibt sich die resultierende Anfälligkeit aus den auftretenden Risslängen und der Auftrittswahrscheinlichkeit von LME bei den einzelnen Versuchen. Es konnte eine LME Anfälligkeits-Rangfolge für die Zinküberzüge festgestellt werden. Zink-Magnesium Beschichtungen galten als besonders LME Anfällig, gefolgt von Feuerverzinkt und Galvannealed. Die größte LME Resistenz wurde bei elektrolytisch verzinkten Proben festgestellt. Aus den Ergebnissen werden Handlungsempfehlungen zur Erhöhung der Verarbeitungssicherheit bzw. Schweißpunktqualität abgeleitet. KW - Widerstandspunktschweißen KW - Hochfester Stahl KW - Liquid Metal Embrittlement KW - Flüssigmetallinduzierte Rissbildung KW - Zink PY - 2022 SN - 978-3-96780-030-2 SP - 1 EP - 39 PB - Forschungsvereinigung Stahlanwendung e. V. CY - Düsseldorf AN - OPUS4-58060 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bachmann, Marcel A1 - Meng, Xiangmeng A1 - Artinov, Antoni A1 - Rethmeier, Michael T1 - Investigating defects caused by narrow pool shapes in deep penetration welding N2 - Laser beam welding is a widely used joining technique in many industrial applications. This is mainly due to its many unique advantages, especially compared to conventional arc welding processes. These advantages include, among others, highly concentrated energy deposition, low total heat input and a capacity to penetrate deep into the material while causing only small welding distortions. However, at the same time, the small dimension of the laser spot, high solidification rates, and small dimensions of the weld pool itself can provoke issues regarding the assembly tolerances of the workpiece, the hot-cracking phenomena, as well as keyhole-induced bubbles escaping from the melt. Weld pool shapes in laser beam welding are elongated at the external, free surfaces under the action of the main driving forces in the melt – such as recoil pressure and surface tension forces – while being shorter in the internal areas of the weld pool. This leads to a regular solidification sequence from the internal zones toward the free surfaces, e.g. from the bottom to the top in partial penetration welding. However, in recent studies reported in the literature and seen in the experimental and numerical investigations of BAM Bundesanstalt für Materialforschung und -prüfung in Berlin, it was found that an internal narrowing phenomenon can occur that is often accompanied by a distinct bulging of the weld bead in deeper zones. As the internal behaviour of the melt during the process is hardly optically accessible, several numerical models and experimental techniques were established to visualise the mechanisms of the formation of the bulging and the narrowing phenomenon and to reveal the consequences on the solidification sequence, pore formation, and filler metal dilution. KW - Weld pool shape KW - Laser beam welding KW - Solidification PY - 2022 SN - 1759-0752 IS - 57 SP - 28 EP - 29 PB - Europa Science CY - Cambridge, UK AN - OPUS4-56995 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Raute, J. A1 - Biegler, M. A1 - Rethmeier, Michael T1 - Untersuchung zum Elektronenstrahlschweißen von additiv gefertigtem Inconel 939 N2 - Hochfeste Nickelbasislegierungen wie Inconel 939 spielen eine wesentliche Rolle im modernen Turbinenbau. Additive Fertigungstechnologien eröffnen hierbei neue Möglichkeiten für die Verarbeitung, jedoch fehlen verlässliche Fügeprozesse für die Absicherung der additiven Prozesskette im Bereich Neuteilfertigung und Instandsetzung. Insbesondere Heißrisse stellen eine große Herausforderung an die Fügetechnik. Die vorliegende Untersuchung befasst sich daher mit dem Verhalten von additiv gefertigten Blechen aus Inconel 939 beim Elektronenstrahlschweißen. Es werden grundlegende Zusammenhänge zwischen Prozessparametern, Härte und Rissneigung betrachtet und Ansätze für eine Optimierung auf Basis statistischer Versuchsplanung aufgezeigt. Hierbei erfolgt eine Einteilung der Risse nach bestimmten Nahtbereichen. Risse am Nahtkopf können durch die Faktoren Vorschub und Streckenenergie sowie die Härte des Schweißgutes beeinflusst werden. Risse im Bereich der parallelen Nahtflanken stehen hingegen im Zusammenhang mit der Härte der Wärmeinflusszone. Ein abschließender Vergleich der angepassten Parameter mit der Ausgangssituation zeigt, dass durch Anwendung der statistischen Optimierung eine deutliche Reduzierung der Rissneigung erreicht werden kann. T2 - 42. Assistentenseminar Fügetechnik CY - Beverungen, Germany DA - 06.10.2021 KW - Elektronenstrahlschweißen KW - Additive Fertigung KW - Schweißnahtbewertung PY - 2022 SN - 978-3-96144-210-2 VL - 385 SP - 1 EP - 8 PB - DVS Media GmbH AN - OPUS4-57320 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Simón Muzás, Juan A1 - Brunner-Schwer, C. A1 - Rethmeier, Michael A1 - Hilgenberg, Kai T1 - Mitigation of liquation cracking in laser welding of pairs of L-PBF processed and wrought plates of Inconel 718 N2 - Laser welding is an appropriate technique for joining Laser Powder Bed Fusion (L-PBF) parts together and to conventional wrought ones. The potential consists of profiting from synergies between additive and conventional manufacturing methods and overcoming the existing limitations of both. On the one hand, L-PBF is a widely spread metal-based additive manufacturing technique suitable for generating complex parts which can present intrinsic designed cavities, conformal cooling channels, and filigree structures contributing to sustainable manufacturing and efficiency-oriented designs. On the other hand, chamber sizes for producing L-PBF parts are limited, and the process is time-consuming. Thus, its employment is not for every geometry justified. Additionally, they are in most cases individual elements of a larger assembly and need to be joined together to conventionally fabricated parts. The present research suggests laser welding parameters to adequately bond pairs of wrought and L-PBF processed plates and two L-PBF plates of Inconel 718 in butt position. L-PBF samples are printed in three different build-up orientations. Additionally, the influence of as-built L-PBF roughness qualities and usual pre-weld preparations such as edge milling are examined. The effect of normed pre-weld heat treatments is also contemplated. Identified cracks are analyzed by means of EDS in order to confirm the present phases on the areas of interest. EBSD is also employed to obtain a clear depiction of the crystallographic texture and distribution of the hot cracks. The quality of the weldment was examined according to existing standards. Substantial differences in seam geometry and microstructure across different edge’s surface qualities and build directions of stress relieved L-PBF parts have not been detected. Nevertheless, even if no other irregularities are present in the seam, variability in liquation cracking susceptibility has been confirmed. This defect is prone to happen when parts made of this nickel-based superalloy are welded together when not enough precautions are taken. It has been determined that grain size and ductility of the material before welding play a crucial role and mitigating or intensifying these imperfections. Moreover, recommendations are presented to avoid this potential welding defect. T2 - IIW 2022 International Conference on Welding and Joining CY - Tokyo, Japan DA - 17.07.2022 KW - Hybrid Part KW - Liquation Cracking KW - Build-up Orientation KW - Pre-weld Preparation KW - Heat treatment KW - Inconel 718 KW - Laser Welding KW - Laser Powder Bed Fusion KW - Selective Laser Melting KW - SLM KW - L-PBF KW - PBF-LB/M KW - LW PY - 2022 UR - www.iiw2022.com SP - 372 EP - 375 PB - The International Institute of Welding (IIW) CY - Tokyo, Japan AN - OPUS4-56066 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Brunner-Schwer, C. A1 - Simón Muzás, Juan A1 - Biegler, M. A1 - Hilgenberg, Kai A1 - Rethmeier, Michael T1 - Laser Welding of L-PBF AM components out of Inconel 718 N2 - With regard to efficient production, it is desirable to combine the respective advantages of additively and conventionally manufactured components. Particularly in the case of large-volume components that also include filigree or complex structures, it makes sense to divide the overall part into individual elements, which afterwards have to be joined by welding. The following research represents a first step in fundamentally investigating and characterizing the joint welding of Laser Powder Bed Fusion (L-PBF) components made of Inconel 718. For this purpose, bead-on-plate welds were performed on plates manufactured using the L-PBF process and compared with the conventionally manufactured material. Conventional laser beam welding was used as welding process. The weld geometry was investigated as a function of the L-PBF build-up orientation. It was found that the welding depth and weld geometry differ depending on this orientation and in comparison to the conventional material. T2 - 12th CIRP Conference on Photonic Technologies [LANE 2022] CY - Fürth, Germany DA - 04.09.2022 KW - Laser Welding KW - L-PBF KW - PBF-LB/M KW - Seam geometry KW - Bead-on-plate welds PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-560012 DO - https://doi.org/10.1016/j.procir.2022.08.072 SN - 2212-8271 VL - 111 SP - 92 EP - 96 PB - Elsevier B.V. AN - OPUS4-56001 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittner, Andreas A1 - Winterkorn, René A1 - Fabry, Çağtay A1 - Rethmeier, Michael A1 - Ratkovac, Mirjana A1 - Thiele, Marc A1 - Baeßler, Matthias T1 - Innovative Design- und Fertigungsstrategien zur Steigerung der Leichtbaupotenziale im Stahlbau N2 - Offshore wind energy plays an important role for the desired transition towards a carbon dioxide free industry within the next decades. However, the grounding of the offshore wind plants governs the overall installation process besides bureaucratic bottlenecks. The application of lightweight principles in steel construction, e.g. the usage dissolved load-bearing structures, so called Jackets foundations, offer great potential in reducing the resource consumption, especially with respect to the needed amount of steel. In this context this presentation focuses on a fully digitalization of the welding manufacturing and as well as testing chain to enable a fully automated manufacturing as well as quality assessment of tubular nodes as key element of Jackets foundation structures. Furthermore, the relationship between the seam shape geometry and resulting fatigue strength is evaluated by numerical methods incorporating bionic principles. It is shown that tubular nodes can be welded fully automatically taking geometry tolerances into account. Moreover, the seam shape could be manufactured as requested by the numerical models which offers great potential for an extended lifetime. Subsequently, the improvements in resource efficiency and reduction of carbon dioxide emissions are evaluated by a life-cycle-assessment. T2 - Leichtbau in der Hauptstadtregion - Rohstoffe - Recycling - Rohstoffe: Kreislaufwirtschaft im Leichtbau CY - Berlin, Germany DA - 28.11.2022 KW - Offshore Windenergie KW - Gründungsstrukturen KW - Leichtbau KW - Automatisierte schweißtechnische Fertigung PY - 2022 AN - OPUS4-56657 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittner, Andreas A1 - Winterkorn, René A1 - Fabry, Çağtay A1 - Rethmeier, Michael A1 - Ratkovac, Mirjana A1 - Thiele, Marc A1 - Baeßler, Matthias T1 - Innovative Design- und Fertigungsstrategien zur Steigerung der Leichtbaupotenziale im Stahlbau N2 - Ziel des Verbundvorhabens „SmartWeld“ ist es, für die schweißtechnische Fertigung von Stahlbaustrukturen exemplarisch am Beispiel von Hohlprofilknoten, welche als designrelevante Elemente von Gründungsstrukturen für Offshore-Windenergieanlagen (OWEA) einsetzbar sind, die Möglichkeiten des Leichtbaus unter konsequenter Digitalisierung der Fertigungskette aufzuzeigen, um einerseits die Ressourceneffizienz zu forcieren und gleichzeitig wettbewerbsfähige Fertigungsstrategien aufzuzeigen. Innerhalb von „SmartWeld“ werden daher die Möglichkeiten einer wirtschaftlichen Fertigung von Leichtbau-Gründungsstrukturen am Beispiel aufgelöster Tragstrukturen (Jackets) aufgezeigt. Eine lastgerechte Auslegung der Schweißverbindungen nach bionischen Prinzipien ermöglicht, weitere Einsparpotenziale an Ressourcen bei gleichzeitiger Erhöhung der Lebensdauer zu erschließen. Die Ausnutzung konstruktiver Prinzipien des Leichtbaus zur Erzeugung innovativer und ressourcenschonender Produkte erfordert den Einsatz digitaler Werkzeuge in der Designphase, der virtuellen Absicherung, der Fertigung und Qualitätsüberwachung sowie nachgelagerten Bauteilprüfung zur Abbildung der Nutzungsphase. Im Rahmen der Arbeiten wird daher der gesamte Produktentstehungs- und Prüfprozess betrachtet. Dies beinhaltet das Design im Kontext des konstruktiven Leichtbaus, den schweißtechnischen Fertigungsprozess, die Bauteilprüfung sowie den Transfer der Ergebnisse in die Industrie durch serientaugliche Demonstratoren. Der Fokus der Arbeiten ist, die Fertigung auch im Umfeld eines für großskalige Stahlstrukturen üblichen hohen Individualisierungsgrades schweißtechnisch zu automatisieren und das Leichtbaupotenzial gezielt umzusetzen. Die Vorgaben aus der Designphase hinsichtlich einer lastgerechten Gestaltung bzw. Implementierung bionischer Ansätze können so gezielt durch einen adaptiven, automatisierten Schweißprozess eingestellt werden. Dies führt zu einer Erhöhung der Ermüdungs¬festigkeit und damit Produktlebensdauer, wodurch die Strukturen dünnwandiger ausgeführt und Ressourcen sowie CO2 eingespart werden können. T2 - Sitzung des DVS Fachausschuss FA03 - Lichtbogenschweißen CY - Rostock, Germany DA - 11.10.2022 KW - Offshore Windenergieanlagen KW - Gründungsstrukturen KW - Leichtbau KW - Automatisierte schweißtechnische Fertigung PY - 2022 AN - OPUS4-56656 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittner, Andreas A1 - Winterkorn, René A1 - Fabry, Çağtay A1 - Rethmeier, Michael A1 - Ratkovac, Mirjana A1 - Thiele, Marc A1 - Baeßler, Matthias T1 - Innovative Design- und Fertigungsstrategien zur Steigerung der Leichtbaupotenziale im Stahlbau N2 - Ziel des Verbundvorhabens „SmartWeld“ ist es, für die schweißtechnische Fertigung von Stahlbaustrukturen exemplarisch am Beispiel von Hohlprofilknoten, welche als designrelevante Elemente von Gründungsstrukturen für Offshore-Windenergieanlagen (OWEA) einsetzbar sind, die Möglichkeiten des Leichtbaus unter konsequenter Digitalisierung der Fertigungskette aufzuzeigen, um einerseits die Ressourceneffizienz zu forcieren und gleichzeitig wettbewerbsfähige Fertigungsstrategien aufzuzeigen. Innerhalb von „SmartWeld“ werden daher die Möglichkeiten einer wirtschaftlichen Fertigung von Leichtbau-Gründungsstrukturen am Beispiel aufgelöster Tragstrukturen (Jackets) aufgezeigt. Eine lastgerechte Auslegung der Schweißverbindungen nach bionischen Prinzipien ermöglicht, weitere Einsparpotenziale an Ressourcen bei gleichzeitiger Erhöhung der Lebensdauer zu erschließen. Die Ausnutzung konstruktiver Prinzipien des Leichtbaus zur Erzeugung innovativer und ressourcenschonender Produkte erfordert den Einsatz digitaler Werkzeuge in der Designphase, der virtuellen Absicherung, der Fertigung und Qualitätsüberwachung sowie nachgelagerten Bauteilprüfung zur Abbildung der Nutzungsphase. Im Rahmen der Arbeiten wird daher der gesamte Produktentstehungs- und Prüfprozess betrachtet. Dies beinhaltet das Design im Kontext des konstruktiven Leichtbaus, den schweißtechnischen Fertigungsprozess, die Bauteilprüfung sowie den Transfer der Ergebnisse in die Industrie durch serientaugliche Demonstratoren. Der Fokus der Arbeiten ist, die Fertigung auch im Umfeld eines für großskalige Stahlstrukturen üblichen hohen Individualisierungsgrades schweißtechnisch zu automatisieren und das Leichtbaupotenzial gezielt umzusetzen. Die Vorgaben aus der Designphase hinsichtlich einer lastgerechten Gestaltung bzw. Implementierung bionischer Ansätze können so gezielt durch einen adaptiven, automatisierten Schweißprozess eingestellt werden. Dies führt zu einer Erhöhung der Ermüdungs¬festigkeit und damit Produktlebensdauer, wodurch die Strukturen dünnwandiger ausgeführt und Ressourcen sowie CO2 eingespart werden können. T2 - 9. Forum Leichtbau - Fortschrittliche Fertigungstechnologien und Werkstoffe für den Klimaschutz CY - Berlin, Germany DA - 29.09.2022 KW - Offshore Windenergieanlagen KW - Gründungsstrukturen KW - Leichtbau KW - Bionik KW - Automatisierte schweißtechniche Fertigung PY - 2022 AN - OPUS4-56655 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittner, Andreas A1 - Winterkorn, René A1 - Fabry, Çağtay A1 - Rethmeier, Michael A1 - Thiele, Marc A1 - Baeßler, Matthias A1 - Brauser, S. T1 - SmartWeld - Leichtbautechnik für Tragstrukturen von Offshore Windenergieanlagen N2 - Die Anwendung von Leichtbauprinzipien im Stahlbau, wie z.B. die Verwendung von aufgelösten Tragstrukturen, sog. Jackets-Fundamenten, bietet ein großes Potential zur Reduzierung des Ressourcenverbrauchs, insbesondere im Hinblick auf die benötigte Stahlmenge. In diesem Vortrag zeigen wir die Potenziale einer vollständigen Digitalisierung der schweißtechnischen Fertigungs- und Prüfkette auf, um eine vollautomatische Fertigung sowie Qualitätsprüfung von Rohrknoten als Schlüsselelement von Jackets-Fundamenten zu ermöglichen. Darüber hinaus wird der Zusammenhang zwischen der Geometrie der Nahtform und der resultierenden Ermüdungsfestigkeit durch numerische Methoden unter Einbeziehung bionischer Prinzipien bewertet. Es wird gezeigt, dass Hohlprofilknoten vollautomatisch unter Berücksichtigung von Geometrietoleranzen geschweißt werden können. Darüber hinaus konnte die Nahtform gemäß den numerischen Modellen hergestellt werden, was ein großes Potenzial für eine verlängerte Lebensdauer bietet. Anschließend werden die Verbesserungen bei der Ressourceneffizienz und die Reduzierung der Kohlendioxidemissionen durch eine Lebenszyklusanalyse bewertet. T2 - 11. Zukunftskonferenz Wind & Maritim CY - Rostock, Germany DA - 01.09.2022 KW - Offshore Windenergieanlagen KW - Gründungsstrukturen KW - Leichtbauprinzipien KW - Automatisierte Fertigung PY - 2022 AN - OPUS4-56654 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittner, Andreas A1 - Rethmeier, Michael A1 - Winterkorn, René A1 - Fabry, Çağtay T1 - Automated arc welding of support structures for offshore wind turbines N2 - Offshore wind energy plays an important role for the desired transition towards a carbon dioxide free industry within the next decades. However, the grounding of the offshore wind plants governs the overall installation process besides bureaucratic bottlenecks. The application of lightweight principles in steel construction, e.g. the usage dissolved load-bearing structures, so called Jackets foundations, offer great potential in reducing the resource consumption, especially with respect to the needed amount of steel. In this context this paper focuses on a fully digitalization of the welding manufacturing and as well as testing chain to enable a fully automated manufacturing as well as quality assessment of tubular nodes as key element of Jackets foundation structures. Furthermore, the relationship between the seam shape geometry and resulting fatigue strength is evaluated by numerical methods incorporating bionic principles. It is shown that tubular nodes can be welded fully automatically taking geometry tolerances into account. Moreover, the seam shape could be manufactured as requested by the numerical models which offers great potential for an extended lifetime. Subsequently, the improvements in resource efficiency and reduction of carbon dioxide emissions are evaluated by a life-cycle-assessment. T2 - IIW Annual Assembly 2022 Tokyo, Japan CY - Tokyo, Japan DA - 21.07.2022 KW - Offshore wind turbines KW - Support structures KW - Automated welding KW - Lightweight principles PY - 2022 AN - OPUS4-56653 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Karkhin, Victor A1 - Artinov, Antoni A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Simulation of solidification during laser welding of thin plates T1 - Моделирование процесса кристаллизации при лазерной сварке пластин малой толщины N2 - It is proposed to model the experimentally observed weld pool boundary with superellipses (Lamé curves) and to find the unknown parameters of the curves using optimization methods. It has been shown experimentally that during laser welding of austenitic stainless steel with a thickness of 2 mm at a speed of 20 mm/s, the rear weld pool part has a shape close to triangular which can be accurately approximated by a superellipse. Analytical dependences of the trajectory and growth rate of the crystal and its cross-sectional area on the geometry of the rear weld pool part are obtained. KW - Laser beam welding KW - Plane crystalization KW - Mathematical modeling KW - Superellipse KW - Thin steel plates PY - 2023 DO - https://doi.org/10.34641/SP.2023.1061.4.033 VL - 4 SP - 28 EP - 33 AN - OPUS4-59649 LA - rus AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Strobl, Dominic A1 - Unger, Jörg F. A1 - Chady, G. A1 - Klawoon, Alexander A1 - Pittner, Andreas A1 - Rethmeier, Michael A1 - Robens-Radermacher, Annika T1 - Efficient bead-on-plate weld model for parameter estimation towards effective wire arc additive manufacturing simulation N2 - Despite the advances in hardware and software techniques, standard numerical methods fail in providing real-time simulations, especially for complex processes such as additive manufacturing applications. A real-time simulation enables process control through the combination of process monitoring and automated feedback, which increases the flexibil- ity and quality of a process. Typically, before producing a whole additive manufacturing structure, a simplified experiment in form of a bead-on- plate experiment is performed to get a first insight into the process and to set parameters suitably. In this work, a reduced order model for the transient thermal problem of the bead-on-plate weld simulation is devel- oped, allowing an efficient model calibration and control of the process. The proposed approach applies the proper generalized decomposition (PGD) method, a popular model order reduction technique, to decrease the computational effort of each model evaluation required multiple times in parameter estimation, control and optimization. The welding torch is modeled by a moving heat source, which leads to difficulties separating space and time, a key ingredient in PGD simulations. A novel approach for separating space and time is applied and extended to 3D problems allowing the derivation of an efficient separated representation of the tem- perature. The results are verified against a standard finite element model showing excellent agreement. The reduced order model is also leveraged in a Bayesian model parameter estimation setup, speeding up calibrations and ultimately leading to an optimized real-time simulation approach for welding experiment using synthetic as well as real measurement data. KW - Ermüdung PY - 2023 DO - https://doi.org/10.5281/zenodo.7456813 PB - Zenodo CY - Geneva AN - OPUS4-59651 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Artinov, Antoni A1 - Meng, Xiangmeng A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Numerical study on the formation of a bulging region in partial penetration laser beam welding N2 - A transient three-dimensional thermo-fluid dynamics numerical model was developed to study the formation of a bulging region in partial penetration laser beam welding. The model accounts for the coupling between the fluid flow, the heat transfer, and the keyhole dynamics by considering the effects of multiple reflections and Fresnel absorption of the laser beam in the keyhole, the phase transitions during melting and evaporating, the thermo-capillary convection, the natural convection, and the phase-specific and temperature-dependent material properties up to the evaporation temperature. The validity of the model was backed up by experimentally obtained data, including the drilling time, the weld pool length, the local temperature history outside the weld pool, the process efficiency, and a range of metallographic crosssections. The model was applied for the cases of partial penetration laser beam welding of 8 mm and 12 mm thick unalloyed steel sheets. The obtained experimental and numerical results reveal that the bulging region forms transiently depending on the penetration depth of the weld, showing a tendency to transition from a slight bulging to a fully developed bulging region between penetration depths of 6 mm and 9 mm, respectively. T2 - 13th International Seminar "Numerical Analysis of Weldability" CY - Seggau, Austria DA - 04.09.2022 KW - Laser beam welding KW - Deep penetration KW - Bulge formation KW - Numerical modeling PY - 2023 SN - 978-3-85125-968-1 SN - 978-3-85125-969-8 SN - 2410-0544 VL - 13 SP - 101 EP - 126 PB - Verlag der Technischen Universität Graz AN - OPUS4-58802 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Artinov, Antoni A1 - Kising, Pascal A1 - Bachmann, Marcel A1 - Meng, Xiangmeng A1 - Rethmeier, Michael T1 - Numerical analysis of the dependency of the weld pool shape on turbulence and thermodynamic activity of solutes in laser beam welding of unalloyed steels N2 - A three-dimensional numerical model was developed to accurately predict the steady-state weld pool shape in full penetration laser beam welding. The model accounts for the coupling between the heat transfer and the fluid dynamics by considering the effects of solid/liquid phase transition, thermo-capillary convection, natural convection, and phase-specific and temperature-dependent material properties up to the evaporation temperature. A fixed right circular cone was utilized as a keyhole geometry to consider the heat absorbed from the laser beam. The model was used to analyze the influence of the thermodynamic activity of solutes and turbulence on the weld pool shape. A mesh sensitivity analysis was performed on a hybrid mesh combining hexahedral and tetrahedral elements. For the case of full penetration laser beam welding of 8 mm thick unalloyed steel sheets, the dependence of the weld pool shape on the surface-active element sulfur was found to be negligible. The analysis of the results showed that a laminar formulation is sufficient for accurately predicting the weld pool shape since the turbulence has a minor impact on the flow dynamics in the weld pool. The validity of the numerical results was backed up by experimental measurements and observations, including weld pool length, local temperature history, and a range of metallographic crosssections. T2 - 13th International Seminar Numerical Analysis of Weldability CY - Seggau, Austria DA - 04.09.2022 KW - Weld pool shape KW - Numerical modeling KW - Laser beam welding KW - Thermo-capillary convection KW - Turbulence PY - 2023 SN - 978-3-85125-968-1 SN - 978-3-85125-969-8 SN - 2410-0544 VL - 13 SP - 161 EP - 188 PB - Verlag der Technischen Universität Graz AN - OPUS4-58803 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -