TY - CONF A1 - Ávila Calderón, Luis T1 - Creep Behavior of Stainless Steel 316L Manufactured by Laser Powder Bed Fusion N2 - This contribution presents the results of an experimental study on the creep behavior of an austenitic 316L stainless steel produced by laser powder bed fusion (PBF-LB/M/316L) with an emphasis on understanding the effects of microstructure on the creep mechanisms. Hot tensile tests and constant force creep tests at 600 °C and 650 °C, X-ray computed tomography, as well as optical and electron microscopy were performed. The produced PBF-LB/M/316L exhibits a low void population (< 0.01 %) resulting from the manufacturing parameters used and which allowed us to understand the effects of other microstructural aspects on creep behavior, e.g., grain morphology and dislocation substructure. A hot‑rolled variant of 316L was also tested as a reference. T2 - International Materials Science and Engineering Congress - MSE 2024 CY - Darmstadt, Germany DA - 24.09.2024 KW - AGIL KW - Additive Fertigung KW - Mikrostruktur KW - Mikrostrukturentwicklung KW - Kriechen KW - Kriechschädigung PY - 2024 AN - OPUS4-61169 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Ávila Calderón, Luis T1 - Kriech- und Bruchverhalten von additiv hergestelltem austenitischem Stahl 316L. Vergleich zum konventionellen Werkstoff. N2 - Eine kritische Aufgabe im Rahmen der Etablierung von Prozess-Struktur-Eigenschafts-Performance-Beziehungen bei der additiven Fertigung (AM) von Metallen ist die Ermittlung von zuverlässigen und gut dokumentierten Kennwerten zum Materialverhalten sowie das Schaffen von Wissen über die Struktur-Eigenschafts-Korrelation. Schließlich ist dies die Grundlage für die Entwicklung gezielterer Prozessoptimierungen und zuverlässigerer Lebensdauer-Vorhersagen. In diesem Zusammenhang zielt dieser Beitrag darauf ab, Daten und Erkenntnisse über das Kriechverhalten des austenitischen Edelstahls 316L zu liefern, der mittels Laser-Powder-Bed-Fusion (L-PBF) hergestellt wird. Um dieses Ziel zu erreichen, wurden Proben aus konventionellem warmgewalztem sowie AM-Material gemäß den bestehenden Normen für konventionelles Material geprüft und vor und nach dem Versagen mikrostrukturell charakterisiert. Die Probekörper wurden aus einzelnen Blöcken des AM-Materials gefertigt. Die Blöcke wurden mit einer Standard-Scan- und Aufbaustrategie hergestellt und anschließend wärmebehandelt. Das Kriechverhalten wird anhand der Kriechlebensdauer und ausgewählter Kriechkurven und Kennwerte beschrieben und vergleichend bewertet. Der Einfluss von Defekten und Mikrostruktur auf das Materialverhalten wird anhand von zerstörenden und zerstörungsfreien Auswertungen an ausgewählten Proben analysiert. Der AM-Werkstoff zeigt kürzere Kriechlebensdauern, erreicht das sekundäre Kriechstadium deutlich schneller und bei geringerer Dehnung und weist eine geringere Kriechduktilität im Vergleich zu seinem konventionellen Gegenstück auf. Das Kriechschädigungsverhalten des AM-Werkstoffs ist eher mikrostruktur- als defektgesteuert und ist durch die Bildung intergranularer Kriechrisse gekennzeichnet. Als kritische Merkmale werden die Versetzungsdichte sowie die Versprödung der Korngrenzen identifiziert. Die Mikro-Computertomographie (µCT) erweist sich als Alternative zur Metallographie, um die Kriechschädigung zu analysieren. T2 - Sitzung des DGM-Arbeitskreises Mechanisches Werkstoffverhalten bei hoher Temperatur CY - Online meeting DA - 07.10.2020 KW - 316L KW - Kriechen KW - Additive Fertigung KW - Mikrostruktur KW - Mikro-Computertomographie PY - 2020 AN - OPUS4-51824 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Ávila Calderón, Luis T1 - Cyclic Deformation Behavior of Laser Powder Bed Fused Stainless Steel 316L Role of the Manufacturing Induced Cell Structure N2 - The cyclic deformation behavior of an austenitic 316L stainless steel produced by laser powder bed fusion in two heat treated conditions and featuring a low defect population is presented. Strain controlled push/pull tests were performed between room temperature and 600 °C. The PBF‑LB/M/316L exhibits an initial cyclic hardening, followed by a cyclic softening. The grade of softening decreases (i) with increasing test temperature and (ii) after a partial dissolution of its dislocation substructure through heat treatment. The deformation behavior and its dependency on test temperature and heat-treated/microstructural condition are attributed to the slip character and related changes. With either a partially dissolved dislocation substructure or increasing test temperature the material exhibits typical wavy slip characteristics. In the opposite case, the deformation mechanism seems to be rather planar dislocation slip as the formation of slip planes spanning through entire grains was observed, seemingly acting as pathways of easy dislocation movement. T2 - TMS 2025 CY - Las Vegas, Nevada, US DA - 23.03.2025 KW - AGIL KW - Additive Fertigung KW - Low-Cycle-Fatigue KW - Mikrostruktur KW - 316L PY - 2025 AN - OPUS4-64855 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Werner, Tiago T1 - Experimentelle und numerische Untersuchung des Druckanschwingens von bruchmechanischen Proben aus konventionell und additiv gefertigtem 316L Stahl N2 - Die Erzeugung rissschließfreier Anrisse in gekerbten bruchmechanischen Proben für anschließende Ermüdungsversuche kann durch eine zyklische Druckbelastung an der Kerbe erfolgen: Bei der Erstbelastung wird eine plastische Verformung an der Kerbspitze erzeugt, welche Zugeigenspannungen und damit eine risstreibende Kraft bei der folgenden zyklischen Druckbelastung hervorruft. Durch das Risswachstum kommt es zu einer Entspannung, bis der Riss schließlich arretiert, weil die effektive risstreibende Kraft auf den Schwellenwert abgesunken ist. Um Kurzrisswachstum in additiv, mittels pulverbettbasiertem Laserstrahlschmelzen (Laser Powder Bed Fusion - LPBF) gefertigtem AISI 316L Stahl und seinem konventionell erzeugten, warmgewalzten Pendant zu untersuchen, wurde dieses Verfahren im Rahmen der vorliegenden Arbeit genutzt. Im Falle des additiv gefertigten Materials kam es zu unerwartet langem Ermüdungsrisswachstum, bevor der Riss arretierte. Zur Ermittlung der Ursache erfolgte eine Messung der Eigenspannungsverteilungen mittels Neutronendiffraktion in der Kerbebene der additiv gefertigten Proben. Anschließend wurde ein Finite-Elemente-Modell zur Simulation des Ermüdungsrisswachstums in konventionellem und additiv gefertigtem Material implementiert. Im Rahmen dieses Vortrages wird insbesondere auf das Vorgehen bei der Simulation und auf die getroffenen Annahmen und Vereinfachungen eingegangen. Die Resultate werden mit den experimentellen Ergebnissen verglichen und das für die Simulation von Risswachstum genutzte Knoten-Freigabe-Verfahren (Node-Release), das Einbringen von Eigenspannungen als initiale Spannungen in der Simulation, und die Rechengrößen zur Quantifizierung der risstreibenden Kraft kritisch diskutiert. T2 - 56. DVM Tagung "Bruchmechanik und Bauteilsicherheit" CY - Kassel, Germany DA - 20.02.2024 KW - PBF/LB KW - Additive Fertigung KW - Ermüdungsrisswachstum KW - Druckanschwingen KW - FEM KW - Node-release KW - Eigenspannungsmessung KW - Neutronendiffraktion PY - 2024 AN - OPUS4-59559 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Werner, Tiago T1 - Ermüdung von additiv gefertigtem Stahl AISI 316L: Zyklische plastische Verformung N2 - Das zyklische plastische Verformungsverhalten von additiv gefertigtem Edelstahl AISI 316L wurde in dehnungsgeregelten Kurzzeitfestigkeitsversuchen (LCF-Versuchen) untersucht. Dabei wurden zwei Wärmebehandlungszustände betrachtet: Beim ersten Zustand war die fertigungsbedingte zelluläre Struktur vorhanden, während sie durch die zweite Wärmebehandlung aufgelöst wurde. Untersuchungen im Transmissions-Elektronen-Mikroskop (TEM) zeigten, dass die zyklische Verformung die Zellstruktur lokal zerstörte und Gleitbänder entstanden, was die Entfestigung in diesem Fall erklärt. Für Material ohne Zellstrukturen resultierten nach zyklischer Verformung ähnliche Versetzungsstrukturen wie in konventionell gefertigtem (warmgewalzten) Material. T2 - OVGU-Kolloquium (BMDK des IWF) CY - Magdeburg, Germany DA - 23.06.2022 KW - Additive Fertigung KW - Kurzzeitfestigkeit KW - Mikrostrukturentwicklung KW - Versetzungsstrukturen KW - TEM PY - 2022 AN - OPUS4-56789 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Waske, Anja T1 - A unique Authenticator for additively manufactured parts N2 - Components produced using additive manufacturing can be marked for unique identification and secure authentication [1,2]. Serial numbers and machine-readable codes can be used to identify the component, and link digital product-related data (i.e., a digital product passport) to the actual components. The most prevailing solution consists of local process manipulation, such as printing a quick response (QR) code [3] or a set of blind holes on the surface of the internal cavity of hollow components. However, local manipulation of components may alter the properties, and external tagging features can be altered or even removed by post-processing treatments. This work therefore aims to provide a new methodology for identification, authentication, and traceability of additively manufactured (AM) components using microstructural features that are unique to each part. X-ray computed tomography (XCT) was employed to image the microstructural features of AlSi10Mg parts. Based on size and geometry, the most prominent features were selected to create a unique digital authenticator. We implemented a framework in Python using open-access modules that can successfully create a digital object authenticator using the segmented microstructure information from XCT. The authenticator is stored as a QR code, along with the 3D information of the selected features. T2 - DGM Additive Berlin 2024 CY - Berlin, Germany DA - 12.06.2024 KW - Additive Fertigung KW - Authentifizierung KW - Mikrostruktur PY - 2024 AN - OPUS4-60957 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten A1 - Schröpfer, Dirk A1 - Kannengießer, Thomas A1 - Scharf-Wildenhain, Ronny A1 - Hälsig, Andre A1 - Kromm, Arne A1 - Hensel, J. T1 - Fertigungsbedingte Beanspruchungen und Kaltrisssicherheit in generativ gefertigten Bauteilen aus hochfesten Feinkornbaustählen N2 - Additive Fertigungsverfahren wie das Direct Energy Deposition-Arc (DED-Arc) oder Wire Arc Additive Manufacturing (WAAM) ermöglichen die effiziente Herstellung gewichtsoptimierter, endkonturnaher Bauteile im modernen Stahlbau. Steigerungen der Effizienz können durch den Einsatz hochfester Stähle erreicht werden, insbesondere durch Verringerung von Wandstärken und Bauteilgewicht sowie signifikante Einsparung von Kosten, Zeit und Ressourcen. DED-Arc Schweißzusatzwerkstoffe sind bereits auf dem Markt verfügbar, allerdings fehlen Richtlinien und quantitative Kenntnisse über die schweißbedingte Beanspruchung während der Fertigung und im Betrieb, welche den industriellen Einsatz stark limitieren. In einem gemeinsamen Projekt der BAM und der Technischen Universität Chemnitz wurden die wesentlichen Einflüsse und komplexen Wechselwirkungen von Werkstoff, Fertigungsverfahren, Konstruktion und Bearbeitungsschritten auf die Eigenspannungen untersucht. Ziel war es, den stahlverarbeitenden Anwendern, insbesondere KMU, eine risssichere und beanspruchungsgerechte Herstellung und Modifizierung von Bauteilen und Halbzeugen aus hochfesten Feinkornbaustahl unter Verwendung MSG-basierter generativer Verfahren zu ermöglichen. T2 - DVS Innovationstage 2024 CY - Düsseldorf, Germany DA - 10.04.2024 KW - Feinkornbaustähle KW - Additive Fertigung KW - Kaltrisssicherheit KW - Direct Energy Deposition-Arc (DED-Arc), Wire Arc Additive Manufacturing (WAAM) PY - 2024 AN - OPUS4-61934 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Einfluss der Prozessführung auf den Eigenspannungszustand beim WAAM-Schweißen hochfester Stahlbauteile N2 - Hochfeste Feinkornbaustähle verfügen über großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. Hochfeste Zusatzwerkstoffe für additives MSG-Schweißen (engl.: Wire Arc Additive Manufacturing, WAAM) sind bereits von den Schweißzusatzherstellern lieferbar. Eine breite industrielle Anwendung insbesondere für KMU ist aufgrund fehlender quantitativer Erkenntnisse und Richtlinien bezüglich schweißbedingter Beanspruchungen und Bauteilsicherheit während der Herstellung und des Betriebs derzeit stark limitiert. In einem gemeinsamen Forschungsprojekt (FOSTA-P1380/IGF21162BG) der BAM und der TU Chemnitz werden daher die mit Eigenspannungsausbildung und der Gefahr einer Kaltrissbildung verbundenen prozess- und werkstoffbedingten sowie konstruktiven Einflüsse beim WAAM hochfester Stähle untersucht. Der vorliegende Beitrag fokussiert die Analyse der Auswirkungen von Schweißwärmeführung und Design der WAAM-Bauteile auf die Abkühlbedingungen, Gefüge, mechanisch-technologischen Eigenschaften und Eigenspannungen. Hierfür werden geometrisch definierte Probenkörper (Hohlquader) vollautomatisiert mit einem speziellen, hochfesten WAAM-Massivdraht (Streckgrenze >790 MPa) geschweißt. Die Wärmeführung und Probenabmessungen werden innerhalb eines statistischen Versuchsplans variiert. Die Schweißwärmeführung wird dabei so eingestellt, dass die t8/5-Abkühlzeiten im empfohlenen Verarbeitungsbereich (ca. 5 s bis 20 s) sichergestellt sind. Hierzu ließen sich über zusätzliche thermo-physikalische Umformsimulationen mittels Dilatometer die komplexen Wärmezyklen abbilden und die resultierende Zugfestigkeit des Schweißgutes bestimmen. Das WAAM-Schweißen komplexer Geometrien mit variierenden Schweißwärmeführungen und geometrischen Verhältnissen bzw. Wanddicken bedingt neben den Auswirkungen auf die Abkühlbedingungen, Abkühlzeiten und Gefüge deutliche Einflüsse auf die konstruktiven Steifigkeitsverhältnisse beim Schweißen. Es zeigen sich anhand der Schweißexperimente signifikante Auswirkungen durch Probenskalierung und Wärmeeinbringung auf die resultierenden lokalen Eigenspannungen. Die Folge können ungünstige Bauteileigenschaften und risskritische Zugeigenspannungen sein. Im Rahmen der Normungssitzung werden praktikable Verarbeitungsempfehlungen basierend auf den Erkenntnissen des Vh. mit Vertretern aus Industrie und Forschung diskutiert. T2 - NA 092-00-05 GA: Gemeinschaftsarbeitsausschuss NAS/NMP: Zerstörende Prüfung von Schweißverbindungen (DVS AG Q 4/Q 4.1) CY - Online meeting DA - 10.03.2022 KW - MAG-Schweißen KW - Additive Fertigung KW - Eigenspannungen KW - Hochfester Stahl KW - Kaltrisssicherheit KW - Wärmeführung KW - Windenergie PY - 2022 AN - OPUS4-56722 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Einfluss der Wärmeführung auf den Beanspruchungszustand in additiv gefertigten Bauteilen aus hochfestem Stahl N2 - Hochfeste Feinkornbaustähle verfügen über großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. Hochfeste Zusatzwerkstoffe für additives MSG-Schweißen (engl.: Wire Arc Additive Manufacturing, WAAM) sind bereits von den Schweißzusatzherstellern lieferbar. Eine breite industrielle Anwendung insbesondere für KMU ist aufgrund fehlender quantitativer Erkenntnisse und Richtlinien bezüglich schweißbedingter Beanspruchungen und Bauteilsicherheit während der Herstellung und des Betriebs derzeit stark limitiert. In einem gemeinsamen Forschungsprojekt (FOSTA-P1380/IGF21162BG) der BAM und der TU Chemnitz werden daher die mit Eigenspannungsausbildung und der Gefahr einer Kaltrissbildung verbundenen prozess- und werkstoffbedingten sowie konstruktiven Einflüsse beim WAAM hochfester Stähle untersucht. Der vorliegende Beitrag fokussiert die Analyse der Auswirkungen von Schweißwärmeführung und Design der WAAM-Bauteile auf die Abkühlbedingungen, Gefüge, mechanisch-technologischen Eigenschaften und Eigenspannungen. Hierfür werden geometrisch definierte Probenkörper (Hohlquader) vollautomatisiert mit einem speziellen, hochfesten WAAM-Massivdraht (Streckgrenze >790 MPa) geschweißt. Die Wärmeführung und Probenabmessungen werden innerhalb eines statistischen Versuchsplans variiert. Die Schweißwärmeführung wird dabei so eingestellt, dass die t8/5-Abkühlzeiten im empfohlenen Verarbeitungsbereich (ca. 5 s bis 20 s) sichergestellt sind. Hierzu ließen sich über zusätzliche thermo-physikalische Umformsimulationen mittels Dilatometer die komplexen Wärmezyklen abbilden und die resultierende Zugfestigkeit des Schweißgutes bestimmen. Das WAAM-Schweißen komplexer Geometrien mit variierenden Schweißwärmeführungen und geometrischen Verhältnissen bzw. Wanddicken bedingt neben den Auswirkungen auf die Abkühlbedingungen, Abkühlzeiten und Gefüge deutliche Einflüsse auf die konstruktiven Steifigkeitsverhältnisse beim Schweißen. Es zeigen sich anhand der Schweißexperimente signifikante Auswirkungen durch Probenskalierung und Wärmeeinbringung auf die resultierenden lokalen Eigenspannungen. Die Folge können ungünstige Bauteileigenschaften und risskritische Zugeigenspannungen sein. T2 - OVGU-Kolloquium (BMDK des IWF) CY - Magdeburg, Germany DA - 23.06.2022 KW - MAG-Schweißen KW - Additive Fertigung KW - Eigenspannungen KW - Hochfester Stahl KW - Kaltrisssicherheit KW - Wärmeführung KW - Windenergie PY - 2022 AN - OPUS4-56726 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Residual Stress Evolution During Slot Milling for Repair Welding and WAAM of High-Strength Steel Components N2 - High-strength steels have great potential for weight optimization due to reduced wall thicknesses in many modern steel constructions. Further advances in efficiency can be achieved through the application of additive manufacturing processes, such as Wire Arc Additive Manufacturing (WAAM). These technologies enable the sustainable and resource-efficient manufacturing of high-strength steels into near-net-shape, efficient structures. During the production of steel structures, unacceptable defects may occur in the weld area or in the WAAM component, e.g., due to unstable process conditions. The economical solution for most of the cases is local gouging or machining of the affected areas and repair welding. With respect to the limited ductility of high-strength steels, it is necessary to clarify the effects of machining steps on the multiaxial stress state and the high design-induced shrinkage restraint. In this context, the component-related investigations in two research projects are concerned with the residual stress evolution during welding and slot milling of welds and WAAM structures made of high-strength steels with yield strengths ≥790 MPa. In-situ digital image correlation (DIC) and ex-situ X-ray diffraction (XRD) were used to analyse the stresses and strains induced on specimens during and after milling. The systematic analyses revealed a significant interaction of the stiffness and relaxation of the specimens with the initial residual stresses induced by welding. T2 - ICRS 11 - The 11th International Conference on Residual Stresse CY - Nancy, France DA - 27.03.2022 KW - MAG-Schweißen KW - Eigenspannungen KW - Additive Fertigung KW - Hochfester Stahl KW - Reparaturschweißen KW - Gefügedegradation KW - Windenergie PY - 2022 AN - OPUS4-56708 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Generative Fertigung und Kaltrisssicherheit N2 - Hochfeste Feinkornbaustähle verfügen über ein großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. In dieser Präsentation werden erste Ergebnisse der Eigenspannungsanalysen von additiv gefertigten Bauteilen aus hochfestem Stahl vorgestellt. T2 - Bachelor-, Master-, Doktoranden-Kolloquium CY - Online meeting DA - 10.06.2021 KW - Additive Fertigung KW - Wärmeführung KW - Hochfester Stahl KW - Eigenspannungen KW - Härteprüfung nach Vickers PY - 2021 AN - OPUS4-53326 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Einfluss trennender Fertigungsschritte auf die Eigenspannungen in additiv gefertigten Bauteilen aus hochfestem Stahl N2 - Additive Fertigungsverfahren wie das Wire Arc Additive Manufacturing (WAAM) ermöglichen die effiziente Fertigung von gewichtsoptimierten endkonturnahen Strukturen in modernen Stahlkonstruktionen. Ihre Effizienz kann weiter durch die Verwendung von hochfesten Stählen gesteigert werden. Dies erlaubt eine signifikante Einsparung von Kosten, Zeit und Ressourcen. Entsprechende Schweißzusatzwerkstoffe für Lichtbogenschweißverfahren sind kommerziell verfügbar. Fehlende Richtlinien und fehlende quantitative Kenntnisse über die schweißtechnische Beanspruchung während der Fertigung und im Betrieb limitieren den industriellen Einsatz stark. Daher werden in einem aktuellen Vorhaben (IGF-Nr. 21162 BG) der BAM und TU Chemnitz die wesentlichen Einflüsse und komplexen Interaktionen durch Werkstoff, Fertigungsprozess, Konstruktion und trennende Fertigungsschritte auf den Beanspruchungszustand untersucht. Der vorliegende Beitrag fokussiert hierfür die Auswirkungen trennender Fertigungsschritte auf Verzug und Eigenspannungen definierter WAAM-Prüfkörper. Die Eigenspannungsanalyse erfolgt mittels Röntgenbeugung. Die große Anzahl an Ergebnissen von zuvor untersuchten Referenzproben, die mit einem speziellen WAAM-Massivdraht (Streckgrenze >820 MPa) bei unterschiedlicher Wärmeführung und Geometrie vollautomatisiert geschweißt wurden, lässt eine Korrelation der Messdaten zu. Hierzu erfolgt die Analyse des Ausgangszustandes und abschließend des Zustandes nach trennender Bearbeitung, welche begleitend mittels digitaler Bildkorrelation hinsichtlich des Verzuges untersucht wurden. So ist zu beobachten, dass die Geometrie deutlichen Einfluss auf Relaxation und Umlagerung der Eigenspannungen hat und damit die Risssicherheit positiv beeinflussen kann. T2 - Werkstofftechnisches Kolloquium 2023 Chemnitz CY - Chemnitz, Germany DA - 29.03.2023 KW - Additive Fertigung KW - Hochfester Stahl KW - Eigenspannungen PY - 2023 AN - OPUS4-57690 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Erste Untersuchungen auf dem Weg zum WAAM-Kaltrisstest für hochfeste Stähle N2 - Hochfeste Feinkornbaustähle verfügen über ein großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. In dieser Präsentation werden erste Analysen des Einflusses der Fertigungsstrategie auf die Härte in additiv gefertigten Bauteilen aus hochfestem Stahl vorgestellt. T2 - NA 092-00-05 GA (DVS AG Q 4/Q 4.1) CY - Online meeting DA - 10.03.2021 KW - Additive Fertigung KW - Hochfester Stahl KW - Härteprüfung nach Vickers PY - 2021 AN - OPUS4-53327 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Einfluss trennender Fertigungsschritte auf die Eigenspannungen in Bauteilen aus hochfestem Stahl N2 - Der Vortrag gibt einen Überblick über den Einfluss Trennender Fertigungsschritte auf die Eigenspannungen in einer Schweißverbindung und an additiv gefertigten Bauteilen aus hochfestem Stahl. Es wird dargestellt, wie die Spanende Bearbeitung in Wechselwirkung mit der lokalen Mikrostruktur die Eigenspannungen beeinflusst. T2 - Bachelor-, Master-, Doktoranden-Kolloquium OvGU Magdeburg CY - Magdeburg, Germany DA - 17.01.2024 KW - Hochfester Stahl KW - Additive Fertigung KW - Reparaturschweißen KW - Eigenspannungen PY - 2024 AN - OPUS4-59413 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Neutronen- und Röntgendiffraktion Zur Einflussanalyse des Bauteil-Designs auf die Eigenspannungen bei der additiven Fertigung mit hochfestem Stahl N2 - Der Vortrag gibt einen Überblick über die mittels XRD und Neutronenbeugung ermittelten Eigenspannungen in additiv gefertigten Bauteilen. Zusätzliche wird der Einfluss von Geometrieparameters auf de Eigenspannungen betrachtet T2 - Sitzung DIN NA 092-00-05 GA CY - Berlin, Germany DA - 15.03.2023 KW - Additive Fertigung KW - Hochfester Stahl KW - Eigenspannungen PY - 2023 AN - OPUS4-59236 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Einfluss trennender Fertigungsschritte auf die Eigenspannungen in additiv gefertigten Bauteilen aus hochfestem Stahl N2 - Additive Fertigungsverfahren wie das Wire Arc Additive Manufacturing (WAAM) ermöglichen die effiziente Fertigung von gewichtsoptimierten endkonturnahen Strukturen in modernen Stahlkonstruktionen. Ihre Effizienz kann weiter durch die Verwendung von hochfesten Stählen gesteigert werden. Dies erlaubt eine signifikante Einsparung von Kosten, Zeit und Ressourcen. Entsprechende Schweißzusatzwerkstoffe für Lichtbogenschweißverfahren sind kommerziell verfügbar. Fehlende Richtlinien und fehlende quantitative Kenntnisse über die schweißtechnische Beanspruchung während der Fertigung und im Betrieb limitieren den industriellen Einsatz stark. Daher werden in einem aktuellen Vorhaben (IGF-Nr. 21162 BG) der BAM und TU Chemnitz die wesentlichen Einflüsse und komplexen Interaktionen durch Werkstoff, Fertigungsprozess, Konstruktion und trennende Fertigungsschritte auf den Beanspruchungszustand untersucht. Der vorliegende Beitrag fokussiert hierfür die Auswirkungen trennender Fertigungsschritte auf Verzug und Eigenspannungen definierter WAAM-Prüfkörper. Die Eigenspannungsanalyse erfolgt mittels Röntgenbeugung. Die große Anzahl an Ergebnissen von zuvor untersuchten Referenzproben, die mit einem speziellen WAAM-Massivdraht (Streckgrenze >820 MPa) bei unterschiedlicher Wärmeführung und Geometrie vollautomatisiert geschweißt wurden, lässt eine Korrelation der Messdaten zu. Hierzu erfolgt die Analyse des Ausgangszustandes und abschließend des Zustandes nach trennender Bearbeitung, welche begleitend mittels digitaler Bildkorrelation hinsichtlich des Verzuges untersucht wurden. So ist zu beobachten, dass die Geometrie deutlichen Einfluss auf Relaxation und Umlagerung der Eigenspannungen hat und damit die Risssicherheit positiv beeinflussen kann. T2 - Bachelor-, Master-, Doktoranden-Kolloquium OvGU Magdeburg CY - Magdeburg, Germany DA - 31.05.2023 KW - Additive Fertigung KW - Hochfester Stahl KW - Eigenspannungen PY - 2023 AN - OPUS4-57689 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Neutronen- und Röntgendiffraktion zur Einflussanalyse des Bauteil-Designs auf die Eigenspannungen bei der additiven Fertigung mit hochfestem Stahl N2 - Vorstellung und Gegenüberstellung von Eigenspannungsanalysen mittels Röntgen- und Neutronenbeugung an einer additiven Prüfgeometrie aus hochfestem Stahl. Einflussanalyse des Designs (Länge, Höhe, Wandstärke) von additiv gefertigten Bauteilen aus hochfestem Stahl auf die Eigenspannungen. T2 - Bachelor-, Master-, Doktoranden-Kolloquium OvGU Magdeburg CY - Magdeburg, Germany DA - 25.01.2023 KW - Additive Fertigung KW - Hochfester Stahl KW - Eigenspannungen PY - 2023 AN - OPUS4-57688 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Residual stress formation in DED-arc manufactured high strength steel components N2 - Additive manufacturing (AM) processes enable the efficient production of advanced constructions. New developments in topology optimization are leading to weight-optimized designs of increasing complexity. Direct energy deposition processes (DED) such as wire and arc-based additive manufacturing are an important method of additive manufacturing. The wire filler metals enable a wide range of materials, while the arc process provides a high deposition rate compared to laser and powder-based processes. Combined with the use of high-strength steels, the thickness of walls or components can be significantly reduced in the context of lightweight construction, which results in significant savings in energy, costs, time and resources. Suitable high-strength steel filler metals are commercially available for DED-arc AM processes. However, guidelines and quantitative knowledge about welding stresses and cold cracking issues during component production and service are lacking. This limits the industrial application considerably. In a joint project of BAM and Chemnitz University of Technology, the main influences and complex interactions of material, production process, design and processing steps on the residual stress level are investigated. The aim is to develop processing recommendations and a cold cracking test for economical processing and stress-related design of high-strength steels with DED-arc. This study focuses on residual stress analysis by neutron diffraction (ND) and X-ray diffraction (XRD) on defined test specimens. The ND analysis were performed at the Paul Scherrer Institute- Villigen, Switzerland (PSI) and the XRD analysis at BAM. The study shows a quantitative and qualitative comparison of the residual stress magnitudes and distribution between the component bulk (ND) and surface (XRD) analyses. The ND analysis reveals that in DED-arc AM walls the residual stresses dominate in the direction of welding and are negligibly small in each case transverse to the direction of welding. The topology of the analyzed residual stresses shows almost identical residual stress maps compared to XRD. In addition, the residual stresses are significantly influenced by the solid phase transformation of the material due to low cooling times and less post heat treatment cycles of following AM layers in the area of the top layer. T2 - 76th IIW Annual Assembly and International Conference on Welding and Joining CY - Singapore DA - 16.07.2023 KW - Additive Fertigung KW - Hochfester Stahl KW - Eigenspannungen PY - 2023 AN - OPUS4-59233 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wandtke, Karsten T1 - Einfluss trennender Fertigungsschritte auf die Eigenspannungen in additiv gefertigten Bauteilen aus hochfestem Stahl N2 - Additive Fertigungsverfahren wie das Wire Arc Additive Manufacturing (WAAM) ermöglichen die effiziente Fertigung von gewichtsoptimierten endkonturnahen Strukturen in modernen Stahlkonstruktionen. Ihre Effizienz kann weiter durch die Verwendung von hochfesten Stählen gesteigert werden. Dies erlaubt eine signifikante Einsparung von Kosten, Zeit und Ressourcen. Entsprechende Schweißzusatzwerkstoffe für Lichtbogenschweißverfahren sind kommerziell verfügbar. Fehlende Richtlinien und fehlende quantitative Kenntnisse über die schweißtechnische Beanspruchung während der Fertigung und im Betrieb limitieren den industriellen Einsatz stark. Daher werden in einem aktuellen Vorhaben (IGF-Nr. 21162 BG) der BAM und TU Chemnitz die wesentlichen Einflüsse und komplexen Interaktionen durch Werkstoff, Fertigungsprozess, Konstruktion und trennende Fertigungsschritte auf den Beanspruchungszustand untersucht. Der vorliegende Beitrag fokussiert hierfür die Auswirkungen trennender Fertigungsschritte auf Verzug und Eigenspannungen definierter WAAM-Prüfkörper. Die Eigenspannungsanalyse erfolgt mittels Röntgenbeugung. Die große Anzahl an Ergebnissen von zuvor untersuchten Referenzproben, die mit einem speziellen WAAM-Massivdraht (Streckgrenze >820 MPa) bei unterschiedlicher Wärmeführung und Geometrie vollautomatisiert geschweißt wurden, lässt eine Korrelation der Messdaten zu. Hierzu erfolgt die Analyse des Ausgangszustandes und abschließend des Zustandes nach trennender Bearbeitung, welche begleitend mittels digitaler Bildkorrelation hinsichtlich des Verzuges untersucht wurden. So ist zu beobachten, dass die Geometrie deutlichen Einfluss auf Relaxation und Umlagerung der Eigenspannungen hat und damit die Risssicherheit positiv beeinflussen kann. T2 - 23. Werkstofftechnisches Kolloquium CY - Chemnitz, Germany DA - 29.03.2023 KW - Additive Fertigung KW - Hochfester Stahl KW - Eigenspannungen KW - Residual stress PY - 2023 AN - OPUS4-59231 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröpfer, Dirk T1 - Correlation of process, design and welding residual stresses in WAAM of high-strength steel components N2 - High-strength fine-grained structural steels have great potential for modern weight optimized steel construc-tions. Efficient manufacturing and further weight savings are achievable due to Wire Arc Additive Manu-facturing (WAAM). First commercial high-strength welding consumables for WAAM are already available. However, the application is still severely limited due to a lack of knowledge and guidelines for the industry regarding welding residual stresses and component safety in manufacturing and operation. Residual stresses may be critical regarding the special microstructure of high-strength steels in context with the risk of cold cracking and component performance in service. Therefore, process- and material-related influences, as well as the design effects on residual stress formation and cold cracking, are being investi-gated in a research project (IGF 21162 BG) focusing a high-strength WAAM welding consumable with yield strength of over 800 MPa. Objectives are the establish-ment of special WAAM cold cracking tests and pro-cessing recommendations allowing economical, suita-ble, and crack-safe WAAM of high-strength steels. First studies on process-related influences showed transfor-mation residual stresses arising during cooling, which significantly influence stress evolution of the compo-nent during layer-wise build-up. This has not yet been investigated for WAAM of high-strength steels. Focus of this study is on the systematic investigation of interactions of the WAAM welding process and design with cooling time, hardness, and residual stresses. Defined open hollow cuboids were welded and investi-gated under systematic variation (design of experi-ments, DoE) of the scale/dimensions (cf. Fig. 1a) and heat control (interlayer temperature Ti: 100–300 °C), heat input E: 200–650 kJ/m. The welding parameters were kept constant as possible to avoid any influence by the arc and the material transfer mode. The heat input adjusted primarily via the welding speed. The resulting different weald bead widths were considered by different build-up strategies (weld beads per layer) to ensure defined wall thicknesses. The hardness was determined on cross-sections taken from the manufac-tured hollow cuboids (Fig. 1c) and the analysis of the residual stress state was carried out by means of X-ray diffraction (XRD) at defined positions on the lateral wall (Fig. 1b). The hardness is higher at the top compared to the lower weld beads, as shown in Fig. 1c exemplarily for central test parameters of the DoE = 425 kJ/mm, Ti = 200 °C). This may be attributed to the specific heat control of the top weld beads, i.e., quenching effects, which are not tempered by weld beads above as is the case for lower weld beads implying a higher hardness. It was observed that the hardness level decreases with increasing energy per unit length, while the in-terpass temperature has a rather low influence on the hardness Residual stress analysis was performed on the lat-eral wall in the welding direction, cf. Fig. 1b, to deter-mine the influence of heat control and design. In the top area of the wall, maximum longitudinal residual stress-es of up to over 500 MPa exhibit, which corresponds to approx. 65% of the nominal yield strength of the mate-rial. The statistic evaluation of stress levels in welding direction of all test specimens show that adaption of heat input may reduce welding stresses up to 50%. In-terpass temperature has less pronounced effect on cool-ing times, microstructure, and on the residual level within parameter matrix. Overall, the results show a significant influence of heat input and component di-mensions on the residual stresses and minor effect of the interpass temperature. Hence, the properties of the specimens may be effectively adjusted via heat input. The working temperatures should be considered for global shrinkage behavior or restraints. Such investiga-tions of residual stress are necessary to further deter-mine local and global welding stresses regarding the consequences on the component safety during manu-facturing and service. T2 - 6th International Symposium on Visualization in Joining & Welding Science through Advanced Measurements and Simulation CY - Osaka, Japan DA - 25.10.2022 KW - MAG-Schweißen KW - Additive Fertigung KW - Eigenspannungen KW - Hochfester Stahl KW - Kaltrisssicherheit KW - Wärmeführung KW - Windenergie PY - 2022 AN - OPUS4-56725 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröpfer, Dirk T1 - Begrüßung und Vorstellung der BAMund des Fachbereichs 9.2 - Zentrale Forschungswerkstatt N2 - Die Zentralwerkstatt der BAM übernimmt die Fertigung und Konstruktion komplexer Prüf- und Versuchseinrichtungen und adressiert zugleich zentrale Forschungsthemen zur Werkstoff- und Komponentensicherheit. Dazu gehören die Entwicklung innovativer Fertigungstechnologien, ressourceneffiziente Verarbeitungskonzepte für hochfeste und additive Komponenten sowie die Untersuchung von Fertigungseinflüssen auf Oberflächenintegrität und Werkstoffdegradation. Ein besonderer Fokus liegt auf der H₂-Sicherheit, insbesondere der Fertigung und Prüfung von Hohlzugproben für Wasserstoff-Pipelines. Ergänzend werden Automatisierungslösungen, digitale Methoden und moderne Spanntechnik zur Effizienzsteigerung eingesetzt. Die Arbeiten sind eng mit den BAM-Kompetenzzentren AM@BAM, H2Safety@BAM und WIND@BAM verzahnt und leisten einen Beitrag zur Energiewende sowie zur Normung und zum Technologietransfer. T2 - 37. Stammtisch Metall des "Der Mittelstand BVMW e.V. " CY - Berlin, Germany DA - 17.09.2025 KW - Werkstoffsicherheit KW - H₂-Sicherheit KW - Additive Fertigung KW - Ressourceneffizienz KW - Automatisierung in der Fertigung KW - Prüftechnikentwicklung KW - Normung und Technologietransfer KW - Oberflächenintegrität PY - 2025 AN - OPUS4-65245 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scheuschner, Nils T1 - In-situ Prozessüberwachung in der additiven Fertigung von Metallen (PBF-LB /M) mittels TT und ET N2 - Durch die additive Fertigung ergeben sich durch die nun mögliche wirtschaftliche Fertigung hochgradig individueller und komplexer metallischer Bauteile in kleinen Stückzahlen bis hinunter zum Einzelstück für viele Industriebereiche ganz neue Möglichkeiten. Gleichzeitig entstehen jedoch neue Herausforderungen im Bereich der Qualitätssicherung, da sich auf statistischen Methoden beruhende Ansätze nicht anwenden lassen, ohne wiederum die Vorteile der Fertigung massiv einzuschränken. Eine mögliche Lösung für dieses Problem liegt in der Anwendung verschiedener In-situ-Überwachungstechniken während des Bauprozesses. Jedoch sind nur wenige dieser Techniken kommerziell verfügbar und noch nicht so weit erforscht, dass die Einhaltung strenger Qualitäts- und Sicherheitsstandards gewährleistet werden kann. In diesem Beitrag stellen wir die Ergebnisse einer Studie über mittels L-PBF gefertigte Probekörper aus der Nickelbasis-Superlegierung Haynes 282 vor, bei denen die Bildung von Defekten durch lokale Variationen der Prozessparameter wie der Laserleistung provoziert wurde. Die Proben wurden in-situ mittels Thermographie, optischer Tomographie, Schmelzbadüberwachung und Wirbelstromprüfung sowie ex-situ mittels Computertomographie (CT) überwacht, mit dem Ziel, die Machbarkeit und die Aussichten der einzelnen Methoden für die zuverlässige Erkennung der Bildung relevanter Defekte zu bewerten. T2 - DGZfP Jahrestagung 2022 CY - Kassel, Germany DA - 23.05.2022 KW - Additive Manufacturing KW - Thermografie KW - Additive Fertigung KW - Thermography PY - 2022 AN - OPUS4-55851 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scheuschner, Nils T1 - In-situ Monitoring of PBF-LB/M by thermography, optical tomography, melt-pool-monitoring and eddy current N2 - The formation of defects such as keyhole pores is a major challenge for the production of metal parts by Laser Powder Bed Fusion (LPBF). The LPBF process is characterized by a large number of influencing factors which can be hard to quantify. Machine Learning (ML) is a prominent tool to predict the outcome of complex processes on the basis of different sensor data. In this study, a ML model for defect prediction is created using thermographic image features as input data. As a reference, the porosity information calculated from an x-ray Micro Computed Tomography (µCT) scan of the produced specimen is used. Physical knowledge about the keyhole pore formation is incorporated into the model to increase the prediction accuracy. From the prediction result, the quality of the input data is evaluated and future demands on in-situ monitoring of LPBF processes are formulated. T2 - AM Bench 2022 CY - Bethesda, Washingthon DC, USA DA - 15.08.2022 KW - Additive Manufacturing KW - Thermography KW - Additive Fertigung KW - Thermografie PY - 2022 AN - OPUS4-55854 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scheuschner, Nils T1 - In-situ Monitoring der Additiven Fertigung von Metallen im LPA Prozess mittels Optischer Emissionsspektrometrie (OES) und Thermografie (TT) N2 - Einer der aussichtsreichsten Ansätze, die Qualität und Sicherheit der gefertigten Teile in der metallbasierten additiven Fertigung (AM) zu erhöhen und die Notwendigkeit aufwändiger und zeitintensiver, zerstörender oder zerstörungsfreier Prüfungen (ZfP) nach der Fertigung zu verringern, liegt in dem Einsatz von in-situ Prozessüberwachungstechniken. Viele wichtige Prozessgrößen bei der additiven Fertigung sind thermischer Natur, wie z.B. die Temperatur des Schmelzbades. Aufgrund der Zugänglichkeit zum Werkstück während des Bauprozesses bieten sich optische Verfahren zur Temperaturbestimmung an. Für die Thermografie und Optische Emissionsspektrometrie im IR-Bereich, welche für die in-situ Anwendung prinzipiell als geeignet angesehen werden können, gibt es allerdings noch wenig konkrete praktische Umsetzungen, da die Möglichkeiten und individuellen Grenzen dieser Methoden, angewendet auf AM, noch nicht ausreichend erforscht sind. Aus diesem Grund verfolgt die BAM mit dem Projekt „Process Monitoring of AM“ (ProMoAM) im Themenfeld Material das Ziel, Verfahren des Prozessmonitorings zur in-situ Bewertung der Qualität additiv gefertigter Metallbauteile weiterzuentwickeln. Im Beitrag wird der Fokus auf eine Versuchsserie gelegt, bei der Aufbau von Probekörpern aus dem austenitischen Edelstahl 316L mittels Laser-Pulver-Auftragschweißen (LPA) durch od. mit Hilfe von IR-Spektrometrie und Thermografie in-situ überwacht wurde. Hierbei stellen u.a. die hohe Bandbreite der zu messenden Temperaturen, die Bestimmung der Emissivität und ihre Änderung bei Phasenübergängen des Metalls große experimentelle Herausforderungen dar, wobei jede Methode individuelle Vor- und Nachteile aufweist, welche verglichen werden. T2 - DGZfP-Jahrestagung 2021 CY - Online meeting DA - 10.05.2021 KW - Additive Manufacturing KW - Thermography KW - Direct Energy Deposition KW - Additive Fertigung KW - Thermografie KW - Laserauftragschweißen PY - 2021 AN - OPUS4-52744 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scharf-Wildenhain, R. T1 - Heat control and design-related effects on the properties and welding stresses in WAAM components of high-strength structural steels N2 - Commercial high-strength filler metals for wire arc additive manufacturing (WAAM) are already available. However, widespread industrial use is currently limited due to a lack of quantitative knowledge and guidelines regarding welding stresses and component safety during manufacture and operation for WAAM structures. In a joint research project (FOSTA-P1380/IGF21162BG), the process- and material-related as well as design influences associated with residual stress formation and the risk of cold cracking are being investigated. For this purpose, reference specimens are welded fully automated with defined dimensions and systematic variation of heat control using a special, high-strength WAAM filler metal (yield strength >790 MPa). Heat control is varied by means of heat input (200–650 kJ/m) and interlayer temperature (100–300 °C). The ∆t8/5 cooling times correspond with the recommendations of steel producers (approx. 5–20 s). Welding parameters and AM geometry are correlated with the resulting microstructure, hardness and residual stress state. High heat input leads to a lower tensile stress in the component and may cause unfavorable microstructure and mechanical properties. However, a sufficiently low interlayer temperature is likely to be suitable for obtaining adequate properties at a reduced tensile stress level when welding with high heat input. The component design affects heat dissipation conditions and the intensity of restraint during welding and has a significant influence on the residual stress. These complex interactions are analyzed within this investigation. The aim is to provide easily applicable processing recommendations and standard specifications for an economical, appropriate and crack-safe WAAM of high-strength steels. T2 - Third edition of the International Congress on Welding, Additive Manufacturing and associated non destructive testing CY - Online meeting DA - 08.06.2022 KW - MAG-Schweißen KW - Eigenspannungen KW - Additive Fertigung KW - Hochfester Stahl KW - Kaltrisssicherheit PY - 2022 AN - OPUS4-56710 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scharf-Wildenhain, R. T1 - Fertigungsbedingte Beanspruchungen und Kaltrisssicherheit in generativ gefertigten Bauteilen aus hochfesten Feinkornbaustählen N2 - Der Vortrag gibt einen Überblick über den Einfluss der Prozessparameter auf die Eigenspannungen sowie die Härte in additiv gefertigten Bauteilen aus hochfestem stahl. Des Weiteren wird dargestellt, wie sich das Bauteildesign und trennende Fertigungsschritte auf die Eigenspannungen der Bauteile auswirken. T2 - DVS Arbeitsgruppe (AG) V 12 CY - Online meeting DA - 15.11.2023 KW - Additive Fertigung KW - Hochfester Stahl KW - Eigenspannungen PY - 2023 AN - OPUS4-59235 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scharf-Wildenhain, R. T1 - Einfluss der Wärmeführung auf die Eigenschaften und fertigungsbedingten Beanspruchungen additiv geschweißter hochfester Feinkornbaustähle N2 - Hochfeste Feinkornbaustähle verfügen über ein großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. Kommerzielle hochfeste Zusatzwerkstoffe für additives MSG-Schweißen (engl.: Wire Arc Additive Manufacturing, WAAM) sind bereits von den Schweißzusatzherstellern lieferbar. Derzeit ist jedoch eine breite industrielle Anwendung insbesondere für KMU aufgrund fehlender quantitativer Erkenntnisse und Richtlinien bezüglich schweißbedingter Beanspruchungen und Bauteilsicherheit während der Herstellung und des Betriebs stark limitiert. In einem gemeinsamen Forschungsprojekt (FOSTA-P1380/IGF21162BG) der BAM und der TU Chemnitz werden die mit Eigenspannungsausbildung und der Gefahr einer Kaltrissbildung verbundenen prozess- und werkstoffbedingten sowie konstruktiven Einflüsse untersucht. Im Fokus dieser Analysen steht die Bestimmung der Wechselwirkungen zwischen WAAM-Prozessparametern bzw. der Wärmeführung auf das Gefüge und die Eigenspannungen. Hierfür werden Referenzproben als offene Hohlquader mit definierten Abmessungen vollautomatisiert mit einem speziellen, hochfesten WAAM-Massivdraht (Streckgrenze >790 MPa) geschweißt. Die gezielte Einstellung der geometrischen Eigenschaften erfolgt durch Schweißparameter und Nahtaufbau bei ca. 4 kg/h mittlerer Abschmelzleistung. Die Wärmeführung wird innerhalb eines statistischen Versuchsplanes mittels Streckenenergie (200 kJ/m bis 650 kJ/m) und Zwischenlagentemperatur (100 °C bis 300 °C) so variiert, dass die t8/5-Abkühlzeiten dem empfohlenen Verarbeitungsbereich entsprechen (ca. 5 s bis 20 s). Ziel ist es bei konstanten geometrisch-konstruktiven Randbedingungen, den Einfluss der Wärmeführung auf Gefüge und resultierende Eigenspannungen zu analysieren. Darüber hinaus erfolgt die Bestimmung des Einflusses der t8/5-Abkühlzeit auf die mechanisch-technologischen Eigenschaften des speziellen, hochfesten WAAM-Massivdrahts mithilfe von Dilatometeranalysen. Für die Streckenenergie können neben den Gefügeeinflüssen aufgrund der resultierenden Abkühlzeit deutliche Effekte insbesondere auf die lokalen Eigenspannungen im Bauteil belegt werden. Das Schweißen mit zu hoher Wärmeeinbringung bzw. Abschmelzleistung kann zu ungünstigen Gefüge- und Bauteileigenschaften führen, gleichzeitig jedoch niedrigere Zugeigenspannungsniveaus bewirken. Die Dilatometeranalysen zeigen für den untersuchten WAAM-Schweißzusatzwerkstoff eine großes t8/5-Zeitfenster mit einer vergleichsweise geringen Abnahme der Zugfestigkeit mit zunehmender t8/5-Abkühlzeit. Solche komplexen Wechselwirkungen gilt es letztlich mit diesen Untersuchungen zu klären, um leicht anwendbare Verarbeitungsempfehlungen und Normvorgaben für ein wirtschaftliches, anforderungsgerechtes und risssicheres WAAM von hochfesten Stählen den Anwendern zur Verfügung zu stellen. T2 - 42. Assistentenseminar Fügetechnik CY - Braunschweig, Germany DA - 06.10.2021 KW - MAG-Schweißen KW - Eigenspannungen KW - Additive Fertigung KW - Hochfester Stahl KW - Kaltrisssicherheit PY - 2021 AN - OPUS4-56691 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scharf-Wildenhain, R. T1 - Einfluss der Wärmeführung auf die Eigenschaften und fertigungsbedingten Beanspruchungen additiv geschweißter hochfester Feinkornbaustähle N2 - Hochfeste Feinkornbaustähle verfügen über ein großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. Kommerzielle hochfeste Zusatzwerkstoffe für additives MSG-Schweißen (engl.: Wire Arc Additive Manufacturing, WAAM) sind bereits von den Schweißzusatzherstellern lieferbar. Derzeit ist jedoch eine breite industrielle Anwendung insbesondere für KMU aufgrund fehlender quantitativer Erkenntnisse und Richtlinien bezüglich schweißbedingter Beanspruchungen und Bauteilsicherheit während der Herstellung und des Betriebs stark limitiert. In einem gemeinsamen Forschungsprojekt (FOSTA-P1380/IGF21162BG) der BAM und der TU Chemnitz werden die mit Eigenspannungsausbildung und der Gefahr einer Kaltrissbildung verbundenen prozess- und werkstoffbedingten sowie konstruktiven Einflüsse untersucht. Im Fokus dieser Analysen steht die Bestimmung der Wechselwirkungen zwischen WAAM-Prozessparametern bzw. der Wärmeführung auf das Gefüge und die Eigenspannungen. Hierfür werden Referenzproben als offene Hohlquader mit definierten Abmessungen vollautomatisiert mit einem speziellen, hochfesten WAAM-Massivdraht (Streckgrenze >790 MPa) geschweißt. Die gezielte Einstellung der geometrischen Eigenschaften erfolgt durch Schweißparameter und Nahtaufbau bei ca. 4 kg/h mittlerer Abschmelzleistung. Die Wärmeführung wird innerhalb eines statistischen Versuchsplanes mittels Streckenenergie (200 kJ/m bis 650 kJ/m) und Zwischenlagentemperatur (100 °C bis 300 °C) so variiert, dass die t8/5-Abkühlzeiten dem empfohlenen Verarbeitungsbereich entsprechen (ca. 5 s bis 20 s). Ziel ist es bei konstanten geometrisch-konstruktiven Randbedingungen, den Einfluss der Wärmeführung auf Gefüge und resultierende Eigenspannungen zu analysieren. Für die Streckenenergie können neben den Gefügeeinflüssen aufgrund der resultierenden Abkühlzeit deutliche Effekte insbesondere auf die lokalen Eigenspannungen im Bauteil belegt werden. Das Schweißen mit zu hoher Wärmeeinbringung bzw. Abschmelzleistung kann zu ungünstigen Gefüge- und Bauteileigenschaften führen, gleichzeitig jedoch niedrigere Zugeigenspannungsniveaus bewirken. Solche komplexen Wechselwirkungen gilt es letztlich mit diesen Untersuchungen zu klären, um leicht anwendbare Verarbeitungsempfehlungen und Normvorgaben für ein wirtschaftliches, anforderungsgerechtes und risssicheres WAAM von hochfesten Stählen den Anwendern zur Verfügung zu stellen. T2 - DVS Congress 2021 CY - Online meeting DA - 14.09.2021 KW - MAG-Schweißen KW - Additive Fertigung KW - Eigenspannungen KW - Kaltrisssicherheit KW - Hochfester Stahl PY - 2021 AN - OPUS4-56668 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scharf-Wildenhain, R. T1 - Herstellung und Charakterisierung von WAAM-Bauteilen aus hochfesten Zusatzwerkstoffe N2 - Hochfeste Feinkornbaustähle verfügen über großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. Hochfeste Zusatzwerkstoffe für additives MSG-Schweißen (engl.: Wire Arc Additive Manufacturing, WAAM) sind bereits von den Schweißzusatzherstellern lieferbar. Eine breite industrielle Anwendung insbesondere für KMU ist aufgrund fehlender quantitativer Erkenntnisse und Richtlinien bezüglich schweißbedingter Beanspruchungen und Bauteilsicherheit während der Herstellung und des Betriebs derzeit stark limitiert. In einem gemeinsamen Forschungsprojekt (FOSTA-P1380/IGF21162BG) der BAM und der TU Chemnitz werden daher die mit Eigenspannungsausbildung und der Gefahr einer Kaltrissbildung verbundenen prozess- und werkstoffbedingten sowie konstruktiven Einflüsse beim WAAM hochfester Stähle untersucht. Der vorliegende Beitrag fokussiert die Analyse der Auswirkungen von Schweißwärmeführung und Design der WAAM-Bauteile auf die Abkühlbedingungen, Gefüge, mechanisch-technologischen Eigenschaften und Eigenspannungen. Hierfür werden geometrisch definierte Probenkörper (Hohlquader) vollautomatisiert mit einem speziellen, hochfesten WAAM-Massivdraht (Streckgrenze >790 MPa) geschweißt. Die Wärmeführung und Probenabmessungen werden innerhalb eines statistischen Versuchsplans variiert. Die Schweißwärmeführung wird dabei so eingestellt, dass die t8/5-Abkühlzeiten im empfohlenen Verarbeitungsbereich (ca. 5 s bis 20 s) sichergestellt sind. Hierzu ließen sich über zusätzliche thermo-physikalische Umformsimulationen mittels Dilatometer die komplexen Wärmezyklen abbilden und die resultierende Zugfestigkeit des Schweißgutes bestimmen. Das WAAM-Schweißen komplexer Geometrien mit variierenden Schweißwärmeführungen und geometrischen Verhältnissen bzw. Wanddicken bedingt neben den Auswirkungen auf die Abkühlbedingungen, Abkühlzeiten und Gefüge deutliche Einflüsse auf die konstruktiven Steifigkeitsverhältnisse beim Schweißen. Es zeigen sich anhand der Schweißexperimente signifikante Auswirkungen durch Probenskalierung und Wärmeeinbringung auf die resultierenden lokalen Eigenspannungen. Die Folge können ungünstige Bauteileigenschaften und risskritische Zugeigenspannungen sein. Im vorliegenden Beitrag werden einige Verarbeitungsempfehlung auf Basis der Ergebnisse für den Arbeitskreis des DVS AG V 12 (Additive Fertigung) abgeleitet. T2 - Sitzung der DVS Arbeitsgruppe (AG) V 12 Additive Fertigung CY - Online meeting DA - 23.11.2022 KW - MAG-Schweißen KW - Additive Fertigung KW - Eigenspannungen KW - Hochfester Stahl KW - Kaltrisssicherheit KW - Wärmeführung KW - Windenergie PY - 2022 AN - OPUS4-56721 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scharf-Wildenhain, R. T1 - Einfluss von Wärmeführung und Bauteildesign auf die Beanspruchungen additiv geschweißter hochfester Feinkornbaustähle N2 - Hochfeste Feinkornbaustähle verfügen über großes Potenzial für gewichtsoptimierte, effiziente Strukturen in vielen modernen Stahlkonstruktion. Weitere Effizienzsteigerungen können durch additives Fertigen sowie bionische Bauweisen erreicht werden. Hochfeste Zusatzwerkstoffe für additives MSG-Schweißen (engl.: Wire Arc Additive Manufacturing, WAAM) sind bereits von den Schweißzusatzherstellern lieferbar. Eine breite industrielle Anwendung insbesondere für KMU ist aufgrund fehlender quantitativer Erkenntnisse und Richtlinien bezüglich schweißbedingter Beanspruchungen und Bauteilsicherheit während der Herstellung und des Betriebs derzeit stark limitiert. In einem gemeinsamen Forschungsprojekt (FOSTA-P1380/IGF21162BG) der BAM und der TU Chemnitz werden daher die mit Eigenspannungsausbildung und der Gefahr einer Kaltrissbildung verbundenen prozess- und werkstoffbedingten sowie konstruktiven Einflüsse beim WAAM hochfester Stähle untersucht. Der vorliegende Beitrag fokussiert die Analyse der Auswirkungen von Schweißwärmeführung und Design der WAAM-Bauteile auf die Abkühlbedingungen, Gefüge, mechanisch-technologischen Eigenschaften und Eigenspannungen. Hierfür werden geometrisch definierte Probenkörper (Hohlquader) vollautomatisiert mit einem speziellen, hochfesten WAAM-Massivdraht (Streckgrenze >790 MPa) geschweißt. Die Wärmeführung und Probenabmessungen werden innerhalb eines statistischen Versuchsplans variiert. Die Schweißwärmeführung wird dabei so eingestellt, dass die t8/5-Abkühlzeiten im empfohlenen Verarbeitungsbereich (ca. 5 s bis 20 s) sichergestellt sind. Hierzu ließen sich über zusätzliche thermo-physikalische Umformsimulationen mittels Dilatometer die komplexen Wärmezyklen abbilden und die resultierende Zugfestigkeit des Schweißgutes bestimmen. Das WAAM-Schweißen komplexer Geometrien mit variierenden Schweißwärmeführungen und geometrischen Verhältnissen bzw. Wanddicken bedingt neben den Auswirkungen auf die Abkühlbedingungen, Abkühlzeiten und Gefüge deutliche Einflüsse auf die konstruktiven Steifigkeitsverhältnisse beim Schweißen. Es zeigen sich anhand der Schweißexperimente signifikante Auswirkungen durch Probenskalierung und Wärmeeinbringung auf die resultierenden lokalen Eigenspannungen. Die Folge können ungünstige Bauteileigenschaften und risskritische Zugeigenspannungen sein. T2 - DVS Congress 2022 CY - Koblenz, Germany DA - 19.09.2022 KW - WAAM KW - Eigenspannungen KW - Additive Fertigung KW - Hochfester Stahl KW - Kaltrisssicherheit KW - Windenergie KW - Wärmeführung PY - 2022 AN - OPUS4-56718 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Räpke, Toni T1 - Geometrie- und Prozesseinflüsse auf lokale Bauteileigenschaften in der metallischen additiven Fertigung mittels Laserstrahlschmelzen N2 - Die mechanischen Eigenschaften und die Standardparametersätze werden im additiven Fertigungsverfahren Laser Powder Bed Fusion (L-PBF) zumeist an Körpern ermittelt, die unter festen Randbedingungen gefertigt werden. In der Literatur wird allerdings von verschiedenen Autoren auf einen Einfluss von Geometrie und Prozess auf die resultierenden Eigenschaften hingewiesen [1, 2, 3]. Aufgrund des häufig großen Komplexitätsgrads von L-PBF Bauteilen und Prozessen, ist eine Abweichung angenommener Eigenschaften daher nicht auszuschließen. Das kann besonders für tragende und sicherheitsrelevante Komponenten kritisch sein und ist eine Herausforderung für die Qualitätssicherung. Aufwendige Trial-and-Error Versuche sind zumeist die Folge. Ein einheitliches und umfassendes Verständnis der Einflussfaktoren auf die resultierenden Eigenschaften im L-PBF Prozess ist zum aktuellen Stand nicht vorhanden. In diesem Vortrag werden erste Ergebnisse einer Studie vorgestellt, in der systematisch die Bandbreite möglicher Defekt- und Mikrostrukturvariationen in L-PBF Bauteilen am Beispiel der Nickelbasislegierung Haynes 282 untersucht wird. Aufbauend auf einer modellbasierten Beschreibung des lokalen Wärmehaushalts wurden Versuchspläne entwickelt, die eine Vielzahl möglicher Prozess- und Geometriekonfigurationen realer Anwendungen abbilden können. Zur Untersuchung des Geometrieeinflusses wurden typische Geometrieelemente komplexer Strukturen und deren Ausprägungen identifiziert. Prozessseitig wurden die Position im Bauraum, Schwankungen der Laserleistung, die Zwischenlagenzeit und die Belichtungsstrategie innerhalb der Schicht als typische Faktoren berücksichtigt. Die Zwischenlagenzeit bildet dabei Variationen im Bauraumfüllgrad ab. Die Belichtungsstrategie untersucht Effekte wie die Zwischenvektorzeit (engl. inter vector time, IVT) oder die lokale Vektorlänge. Die verschiedenen Konfigurationen wurden metallografisch bewertet. Die bisherigen Ergebnisse können einen Einfluss der Geometrie und des Prozesses auf die Defektbildung und die Mikrostruktur in L-PBF Bauteilen aufzeigen. Durch prozessbegleitende thermografische in situ Messungen konnte außerdem eine Abhängigkeit von lokalen und globalen Temperaturfeldern identifiziert werden. Die Erkenntnisse zeigen zudem, dass der geometrische Einfluss auf den lokalen Wärmehaushalt von Anordnung, Gestalt und Dimensionen der zweidimensionalen Belichtungsbereiche über die Aufbauhöhe abhängt. Das gewonnene Verständnis soll in die Entwicklung von Konstruktionsrichtlinien und Prüfkörpern einfließen, um Variationen lokaler Bauteileigenschaften in der zukünftigen Bauteil- und Prozessauslegung berücksichtigen zu können. T2 - 3. Fachtagung Werkstoffe und Additive Fertigung 2022 CY - Dresden, Germany DA - 11.05.2022 KW - Additive Fertigung KW - L-PBF PY - 2022 AN - OPUS4-55516 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Fügetechnik in Wasserstofftechnologien: Prozesse und Perspektiven N2 - Der Vortrag gibt einen tiefen Überblick über die Bedeutung der Füge- und Schweißtechnik in Wasserstofftechnologien. Dazu gliedert sich der Vortrag in die Komplexe H2-Erzeugung, Speicherung, Transport, Anwendung auf und gibt jeweils repräsentative Industriebeispiele für den heutigen Anwendungsstand. Insbesondere werden hier Fertigungstechnologien für Brennstoffzellen vorgestellt, sowie Herausforderungen beim Reparaturschweißen von Wasserstoffpipelines. Zeitgleich wird in einem eigenen Kapitel die Bedeutung der additiven Fertigung ebenso erläutert, wie die aktuellen und umfassenden Tätigkeiten auf dem Gebiet der Normung zu H2-Technologien. T2 - Vortragsreihe der VDI-Ortsgruppe Magdeburg CY - Magdeburg, Germany DA - 23.10.2023 KW - Wasserstofftechnologien KW - Fügetechnik KW - Pipelines KW - Additive Fertigung KW - Normung PY - 2023 AN - OPUS4-58671 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Portella, Pedro Dolabella A1 - Ulbricht, Alexander A1 - Evans, Alexander A1 - Altenburg, Simon A1 - Ehlers, Henrik A1 - Hilgenberg, Kai A1 - Mohr, Gunther T1 - Monitoring additive manufacturing processes by using NDT methods N2 - In this presentation we discuss the online monitoring of metallic AM parts produced by the Laser Powder Bed Fusion (LPBF) process by using optical, thermographic and electromagnetic methods. In a first approach we present the detection of defects generated during the process and discuss how to improve these methods for the optimization of design and production of metallic AM parts. T2 - ABENDI - Workshop CY - Online meeting DA - 19.11.2020 KW - Additive Fertigung PY - 2020 AN - OPUS4-52042 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Portella, Pedro Dolabella T1 - Monitoring additive manufacturing N2 - Additive manufacturing (AM) processes allow a high level of freedom in designing and producing components for complex structures. They offer the possibility of a significant reduction of the process chain. However, the large number of process parameters influence the structure and the behavior of AM parts. A thorough understanding of the interdependent mechanisms is necessary for the reliable design and production of safe AM parts. In this presentation we discuss the online monitoring of metallic AM parts produced by the Laser Powder Bed Fusion (LPBF) process by using optical, thermographic and electromagnetic methods. In a first approach we present the detection of defects generated during the process and discuss how to improve these methods for the optimization of design and production of metallic AM parts. T2 - Conaendi&IEV 2021 CY - Online meeting DA - 10.03.2021 KW - Additive Fertigung PY - 2021 AN - OPUS4-52241 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Mohr, Gunther T1 - Einfluss der Zwischenlagenzeit und der Bauteilhöhe auf die resultierenden Eigenschaften laserstrahlgeschmolzener austenitischer Stahlbauteile N2 - Das pulverbettbasierte selektive Laserstrahlschmelzen (engl. laser powder bed fusion, L-PBF) ist die am weitesten verbreitete additive Fertigungstechnologie für die Herstellung metallischer Komponenten. Unter der Vielzahl an Einflussfaktoren auf die Qualität und die mechanischen Eigenschaften von L PBF-Bauteilen hat die Zwischenlagenzeit (engl. inter layer time, ILT) bisher kaum Beachtung in der wissenschaftlichen Literatur gefunden, obwohl sie je nach Bauraumausnutzungsgrad stark variieren kann. In diesem Vortrag werden Ergebnisse einer Studie präsentiert, die den Einfluss der ILT in Kombination mit der Bauteilhöhe und unter Berücksichtigung verschiedener Volumenenergiedichten am Beispiel der austenitischen Stahllegierung AISI 316L untersucht. Die Fertigungsprozesse wurden in situ mittels Thermographiekamera überwacht, sodass Informationen über das Abkühlverhalten der Bauteile während des Prozesses gewonnen werden konnten. Es wurden signifikante Effekte der ILT und der Bauteilhöhe auf Wärmeakkumulation, Mikrostruktur, Schmelzbadgeometrie und Härte festgestellt. Ferner konnte ein Anstieg von Defektdichten bei einem gegenseitigen Wechselspiel aus Bauteilhöhe und ILT aufgezeigt werden. Die Zwischenlagenzeit wurde somit als kritischer Faktor für die L-PBF-Fertigung von Realbauteilen identifiziert. T2 - DGM Fachtagung "Werkstoffe und Additive Fertigung" CY - Online meeting DA - 13.05.2020 KW - Laser Powder Bed Fusion KW - Additive Fertigung KW - Zwischenlagenzeit KW - In-situ Monitoring PY - 2020 AN - OPUS4-50788 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Madia, Mauro T1 - Thermografie-gestützte Untersuchung des Potentials des Kaltgasspritzens für die Reparatur zyklisch belasteter Bauteile N2 - Die Reparatur mittels Kaltgasspritzen ist eine vielversprechende Alternative zum teuren Austausch fehlerbehafteter Bauteile in der Luft- und Raumfahrt. Durch die Beschleunigung von Metallpartikeln auf Überschallgeschwindigkeiten und die resultierende plastische Verformung der Partikel beim Aufschlag auf das Substrat ohne Aufschmelzen ermöglicht Kaltgasspritzen den schichtweisen Materialauftrag. Die Gewährleistung der Strukturintegrität reparierter Bauteile, insbesondere an der Schnittstelle zwischen dem Substrat und dem aufgetragenen Material, bleibt jedoch eine große Herausforderung. Um dieses Problem zu lösen, wurden verschiedene Prozesse und Behandlungen untersucht, um die Festigkeit und Tragfähigkeit der Reparatur unter zyklischer Belastung zu optimieren. Röntgen-Computertomographie (XCT) ermöglicht die Analyse der Defekte in dem aufgetragenen Material und in der Grenzfläche. Die XCT kann jedoch nur mit hohem Aufwand in-situ während der mechanischen Prüfung eingesetzt werden. Im Gegensatz dazu kann die digitale Bildkorrelation (DIC) in-situ verwendet werden, da es sich um eine berührungslose Vollfeldtechnik handelt, die jedoch in erster Linie die durch das Prüfverfahren bedingten Verschiebungen an der Oberfläche erfasst. Um die Entwicklung der Schädigung an der Grenzfläche zu überwachen, wurde die Infrarot-Thermografie (IRT) parallel zur DIC bei der Zug- und Ermüdungsprüfung von reparierten Al6061 Proben eingesetzt. Es wurde eine gekühlte IRT-Kamera mit hoher Bildrate verwendet, die Nachverarbeitung erfolgte mittels Lock-in IRT. Mit Hilfe von IRT war es möglich, die frühe Schadensentstehung an der Grenzfläche des Substrats zu erkennen und das Risswachstum zu verfolgen. Die Bruchflächen bestätigten, dass die identifizierten Merkmale an der Grenzfläche lagen. Es werden Ergebnisse eines Vergleichs von DIC und IRT aus Ermüdungs- und Zugversuchen vorgestellt. T2 - Werkstoffprüfung 2025 CY - Dresden, Germany DA - 27.11.2025 KW - Additive Fertigung KW - Kaltgasspritzen KW - Thermografie KW - Digitale Bildkorrelation KW - Ermüdungsfestigkeit PY - 2025 AN - OPUS4-64998 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Koch, Claudia A1 - Hilgenberg, Kai T1 - Eine moderne Qualitätsinfrastruktur: digital und vernetzt N2 - Der Vortrag stellt die Arbeiten der BAM in der Initiative QI-Digital vor, in deren Rahmen Lösungen für eine moderne und digitale Qualitätsinfrastruktur entwickelt werden. Schwerpunkt liegt auf dem zentralen Werkzeug Quality-X sowie dem Pilotprojekt "Moderne Qualitätssicherung in der Additiven Fertigung". T2 - BAM Kuratoriumssitzung CY - Berlin, Germany DA - 22.06.2023 KW - Qualitätsinfrastruktur KW - Digitalisierung KW - Quality-X KW - Additive Fertigung PY - 2023 AN - OPUS4-58121 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kempf, A. T1 - Einfluss der Porosität auf die Duktilitätseigenschaften von additiv gefertigtem AlSi10Mg N2 - Die Werkstoffeigenschaften im selektiven Laserstrahlschmelz-Verfahren hergestellter Bauteile werden von einer Vielzahl technologischer Parameter beeinflusst, sodass sich die Fertigungsgüte verschiedener Anlagen voneinander unterscheiden kann. Vor diesem Hintergrund wurde in der vorliegenden Arbeit untersucht, inwiefern sich durch verschiedene nachgelagerte Wärmebehandlungen die Mikrostruktur und die quasistatischen Festigkeitseigenschaften von Proben aus der Aluminiumlegierung AlSi10Mg, die mit verschiedenen Anlagen, Pulvern, Belichtungsstrategien und Prozessparametern gefertigt wurden, harmonisieren lassen. Die Versuche zeigten u.a., dass die erheblichen Festigkeitsunterschiede im Ausgangszustand unabhängig von der angewendeten Wärmebehandlungsroute aufgehoben wurden. Dennoch wurden signifikante Unterschiede in der Duktilität ermittelt. Anhand umfangreicher Bruchflächenanalysen konnte nachgewiesen werden, dass die in der Bruchfläche ermittelte Porosität eine lineare Korrelation zu der Bruchdehnung aufwies. T2 - 5. Tagung des DVM-Arbeitskreises Additiv gefertigte Bauteile und Strukturen CY - Online meeting DA - 04.11.2020 KW - Duktilität KW - Additive Fertigung KW - Laser powder bed fusion KW - AlSi10Mg KW - Festigkeit PY - 2020 AN - OPUS4-51656 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hilgenberg, Kai A1 - Madia, Mauro T1 - Additive Fertigung von Bauteilen und Strukturen – Grenzen, Risiken, Chancen N2 - Dieser Eröffnungsvortrag des DVM-Tages beleuchtet Herausforderungen in der additiven Fertigung und plädiert für eine enge Zusammenarbeit von Fertigungstechnik und Bruchmechanik für die Vorhersage der Lebensdauer AM-gefertigter Komponenten. T2 - DVM-Tag CY - Berlin, Germany DA - 08.04.2025 KW - Additive Fertigung KW - Digitale Qualitätssicherung KW - Ermüdungsfestigkeit PY - 2025 AN - OPUS4-62971 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hilgenberg, Kai T1 - Additive Fertigungsverfahren und Defekte N2 - Überblick über die derzeitig wichtigsten additiven Fertigungsverfahren für metallische Werkstoffe in der Industrie (PBF, DED, BJT) und Berücksichtigung der wesentlichen Prozessmerkmale und Nachbearbeitungsschritte. Vorstellung der wichtigsten Defektphänomene und Nennung von Ursachen und Abhilfemaßnahmen. T2 - BAM Akademie: Qualitätssicherung in der additiven Fertigung CY - Online meeting DA - 14.09.023 KW - Additive Fertigung KW - Defekte KW - Überblick PY - 2023 AN - OPUS4-58302 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hilgenberg, Kai T1 - Eine digitale QI für die moderne Produktion: Digital Quality Assurance in der Additiven Fertigung N2 - Der Vortragt stellt den Use Case Additive Fertigung und das zugehörige Reallabor in QI Digital in Kürze vor und zeigt, mit welchen digitalen Tools das Reallabor mit der übergeordneten Plattform QualityX Daten austauscht. T2 - QI Forum 2023 CY - Berlin, Germany DA - 10.10.2023 KW - Additive Fertigung KW - Digitale Qualitätssicherung KW - QI Digital PY - 2023 AN - OPUS4-58830 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hilgenberg, Kai T1 - Additive Fertigungsverfahren und Defekte N2 - Überblick über die derzeitig wichtigsten additiven Fertigungsverfahren für metallische Werkstoffe in der Industrie (PBF, DED, BJT) und Berücksichtigung der wesentlichen Prozessmerkmale und Nachbearbeitungsschritte. Vorstellung der wichtigsten Defektphänomene und Nennung von Ursachen und Abhilfemaßnahmen. T2 - BAM Akademie: Qualitätssicherung in der additiven Fertigung CY - Online meeting DA - 17.09.2024 KW - Additive Fertigung KW - Defekte KW - Überblick PY - 2024 AN - OPUS4-61172 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hilgenberg, Kai T1 - Herausforderungen in der additiven Fertigung sicherheitsrelevanter Komponenten N2 - Der Vortrag stellt nach einer kurzen allgemeinen Einleitung zur additiven Fertigung und des Laser Powder Bed Fusion Verfahrens einige Herausforderungen vor, die derzeitig den Einsatz von AM-Komponenten in sicherheitsrelevanten Anwendungen erschweren. Abschließend werden zwei Beispiele von Arbeiten der BAM gezeigt, die zur Überwindung dieser Herausforderungen beitragen können. T2 - Anwendertreffen des Laserverbundes Berlin-Brandenburg CY - Berlin, Germany DA - 25.11.2022 KW - Additive Fertigung KW - Laser Powder Bed Fusion PY - 2022 AN - OPUS4-56435 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hilgenberg, Kai T1 - Digitale Qualitätssicherung in der Additiven Fertigung N2 - Der Vortrag stellt das Pilotprojekt Additive Fertigung innerhalb von QI Digital vor und zeigt bisher Erreichtes. Dies umfasst eine digital durchgängige Baujobvorbereitung, automatisierte Datenerhebung und -registrierung sowie die Einbindung des Prozessmonitorings. Seitens der PTB wird ein digitaler Prüfbericht vorgestellt. T2 - QI Forum 2024 CY - Berlin, Germany DA - 09.10.2024 KW - Additive Fertigung KW - Digitale Qualitätssicherung KW - QI Digital PY - 2024 AN - OPUS4-61361 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hilgenberg, Kai T1 - Redesign, Repair, Recycle: R-Strategien bei der additiven Fertigung N2 - Der Vortrag stellt ausgewählte Beispiele aus Projekten des Kompetenzzentrums AM@BAM vor, die das Potenzial der additiven Fertigung bei der Umsetzung von R-Strategien im Kontext der Kreislaufwirtschaft aufzeigen. PBF-LB/M kann genutzt werden für ein Redesign von Komponenten mit dem Ziel der Gewicht- und Materialeinsparung. Das gleiche Verfahren wie auch DED-ARC und das Kaltgasspritzen können für die Reparatur anspruchsvoller Legierungen oder Geometrien genutzt werden. Das Thema Recycling wird am Beispiel der Wiedernutzung von Pulver aus dem PBF-LB/M-Prozess adressiert. T2 - DVM-Tagung: Strukturfestigkeit und Produktlebenszyklus – Vom Design bis zur Kreislaufwirtschaft CY - Berlin, Germany DA - 07.10.2025 KW - Additive Fertigung KW - R-Strategien KW - Repair KW - Reparatur PY - 2025 AN - OPUS4-64324 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Evans, Alexander T1 - Entwicklung der Mikrostruktur der mechanischen Eigenschaften und der Eigenspannungen in L-PBF 316L N2 - Die additive Fertigung (AM) metallischer Werkstoffe mittels Laser Powder Bed Fusion (L-PBF) ermöglicht einzigartige hierarchische Mikrostrukturen, die zu Verbesserungen bestimmter mechanischer Eigenschaften gegenüber konventionell hergestellten Varianten derselben Legierung führen können. Allerdings ist das L-PBF-Verfahren häufig durch das Vorhandensein hoher Eigenspannungen gekennzeichnet, die es zu verstehen und zu mindern gilt. Daher ist das Verständnis der Mikrostrukturen, der Eigenspannungen und der daraus resultierenden mechanischen Eigenschaften entscheidend für eine breite Akzeptanz bei sicherheitskritischen Anwendungen. Die BAM hat ein multidisziplinäres Forschungsprogramm gestartet, um diese Aspekte bei LPBF 316L zu untersuchen. Der vorliegende Beitrag stellt einige der wichtigsten Ergebnisse vor: der Einfluss von Prozessparametern auf die Mikrostruktur, der Einfluss von Mikrostruktur und Textur auf die Festigkeit, Kriechverhalten und Schädigung und die Stabilität von Eigenspannungen und Mikrostruktur unter Wärmebehandlungsbedingungen. T2 - DGM 3. Fachtagung Werkstoffe und Additive Fertigung CY - Dresden, Germany DA - 11.05.2022 KW - Mechanische Eigenschaften KW - Additive Fertigung KW - L-PBF 316L KW - Entwicklung KW - Mikrostruktur KW - Eigenspannung PY - 2022 AN - OPUS4-55786 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Epperlein, Martin T1 - Eine digital gestützte Qualitätssicherung für die additive Fertigung N2 - Die additive Fertigung (ugs. „3D-Druck“) ist bei der Herstellung von hochkomplexen metallischen Bauteilen, bionisch inspiriertem Leichtbau oder Prototypen nicht mehr wegzudenken. Für die konventionelle Fertigung hat sich das bestehende System der Qualitätsinfrastruktur (QI) bewährt. Die additive Fertigung vergrößert den gestalterischen Spielraum von möglichen Bauteilgeometrien und Prozessfehlern jedoch erheblich. Hier gerät die QI an ihre Grenzen, sodass die Fertigung und Zulassung sicherheitsrelevanter Bauteile sehr zeit- und kostenintensive Versuche erfordern. Eine moderne digitale QI erlaubt eine effizientere Qualitätssicherung für additiv gefertigte Bauteile. Dies erfordert eine durchgängig digitale Abbildung des physischen Materialflusses. T2 - Werner-von-Siemens Centre for Industry and Science - AM Querschnittstreffen CY - Online meeting DA - 21.06.2022 KW - Additive Fertigung KW - Qualitätssicherung KW - Digitalisierung PY - 2022 AN - OPUS4-55127 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Epperlein, Martin T1 - Digitalisierung in der Additiven Fertigung N2 - Die Entwicklung einer digitalen QI ermöglicht die objektive Qualitätssicherung in der Additiven Fertigung und macht die Technologie gerade auch für kleine und mittelständische Unternehmen besser nutzbar. Sie wird vollwertig im Rahmen des Qualitätsanspruchs „Made in Germany“ einsetzbar – gerade auch beim Umbruch in Industriezweigen. Der Vortrag gibt Einblicke in aktuelle Arbeiten und die Ziele des Use Case Additive Fertigung. T2 - LEF-Themenwoche, Bayerisches Laserzentrum CY - Online meeting DA - 21.03.2023 KW - Digitalisierung KW - Qualitätsinfrastruktur KW - Additive Fertigung KW - Qualitätssicherung PY - 2023 AN - OPUS4-57186 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Epperlein, Martin T1 - Digitale Qualitätssicherung in der Additiven Fertigung und Voraussetzungen in der Qualitätsinfrastruktur N2 - Der Vortrag gibt einen Überblick über die Aktivitäten im QI-Digital Use Case Additive Fertigung, den aktuellen Stand und nächste Schritte. Es wurde eine digitale Prozesskette für den PBF-LB/M Prozess aufgebaut. Hier werden Daten entlang der gesamten Fertigungsstrecke gesammelt, ausgewertet und zur Qualitätssicherung weiterverarbeitet. Die grundlegende Datenstruktur wurde in die Normung überführt. T2 - TÜV SÜD Fachtagung: Additive Fertigung von Druckgeräten CY - Munich, Germany DA - 17.09.2024 KW - Digitalisierung KW - Qualitätsinfrastruktur KW - Additive Fertigung PY - 2024 AN - OPUS4-61089 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Epperlein, Martin T1 - Eine digital gestützte Qualitätssicherung für die additive Fertigung N2 - Die Digitalisierung der Qualitätsinfrastruktur (QI) am Beispiel der Additiven Fertigung. Der Vortrag erörtert, wie die Elemente einer digitalen QI zur Qualitätssicherung und Zertifizierung in der Additiven Fertigung beitragen können. T2 - Treffen der Arbeitsgemeinschaft Additive Fertigung des VDMA CY - Coburg, Germany DA - 27.10.2022 KW - Qualitätsinfrastruktur KW - Additive Fertigung KW - Digitalisierung PY - 2022 AN - OPUS4-56165 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -