TY - CONF A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Assessment of keyhole stability in laser beam welding with external magnetic field using numerical simulation N2 - The challenge of understanding the physical mechanisms behind porosity reduction by a magnetic field during laser beam welding (LBW) is partly due to the difficulty in quantitatively evaluating keyhole stability. The commonly used index, such as keyhole depth, is typically one-dimensional, which is insufficient to capture the dynamic and three-dimensional fluctuations of the keyhole. In this paper, by utilizing a 3D multiphysical model of LBW with magnetic field, a novel keyhole geometry reconstruction algorithm has been developed to describe the keyhole profile and its fluctuation in a statistical manner to evaluate keyhole stability quantitatively. An equivalent diameter is proposed in this algorithm to reduce the irregularity of the keyhole geometry. The calculation results indicate that the time-averaged keyhole shape over 300 ms in the LBW of steel is conical, regardless of the application of an external magnetic field, which provides a more representative shape. Meanwhile, it is observed from the statistical aspect that the keyhole diameter becomes smaller, except the top part, under the influence of the magnetic field. The standard deviation of the equivalent diameter can be used as a physical variable to assess the keyhole stability quantitatively. The application of an external magnetic field can produce a noticeable reduction of the standard deviation of the equivalent diameter, namely, stabilizing the keyhole during LBW of steel. However, the different contribution from the keyhole stability affected by a magnetic field in suppressing porosity is different with materials. T2 - International Congress of Applications of Lasers & Electro-Optics 2024 CY - Hollywood, Los Angeles, USA DA - 04.11.2024 KW - Deep penetration laser beam welding KW - Numerical simulation KW - Keyhole shape KW - Keyhole stability KW - Magnetic field PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-616024 DO - https://doi.org/10.2351/7.0001528 VL - 36 IS - 4 SP - 1 EP - 7 PB - AIP Publishing AN - OPUS4-61602 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yang, Chunliang A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Experimental and numerical study on grain refinement in electromagnetic assisted laser beam welding of 5754 Al alloy N2 - Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase in the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are analyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain size after welding verify the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains, that have been solidified and formed previously, from further growth and generates some small cellular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement. KW - Laser beam welding KW - Magnetic field KW - Crystal branch development KW - Grain refinement KW - Periodic solidification pattern PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-584905 DO - https://doi.org/10.2351/7.0001085 SN - 1042-346X VL - 35 IS - 4 SP - 1 EP - 10 PB - AIP Publishing AN - OPUS4-58490 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Assessment of keyhole stability in laser beam welding with external magnetic field using numerical simulation N2 - The challenge of understanding the physical mechanisms behind porosity reduction by a magnetic field during laser beam welding (LBW) is partly due to the difficulty in quantitatively evaluating keyhole stability. The commonly used index, such as keyhole depth, is typically one-dimensional, which is insufficient to capture the dynamic and three-dimensional fluctuations of the keyhole. In this paper, by utilizing a 3D multiphysical model of LBW with magnetic field, a novel keyhole geometry reconstruction algorithm has been developed to describe the keyhole profile and its fluctuation in a statistical manner to evaluate keyhole stability quantitatively. An equivalent diameter is proposed in this algorithm to reduce the irregularity of the keyhole geometry. The calculation results indicate that the time-averaged keyhole shape over 300 ms in the LBWof steel is conical, regardless of the application of an external magnetic field, which provides a more representative shape. Meanwhile, it is observed from the statistical aspect that the keyhole diameter becomes smaller, except the top part, under the influence of the magnetic field. The standard deviation of the equivalent diameter can be used as a physical variable to assess the keyhole stability quantitatively. The application of an external magnetic field can produce a noticeable reduction of the standard deviation of the equivalent diameter, namely, stabilizing the keyhole during LBW of steel. However, the different contribution from the keyhole stability affected by a magnetic field in suppressing porosity is different with materials. T2 - International Congress of Applications of Lasers & Electro-Optics 2024 CY - Los Angeles, CA, USA DA - 04.11.2024 KW - Deep penetration laser beam welding KW - Numerical simulation KW - Keyhole shape KW - Keyhole stability KW - Magnetic field PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-614984 DO - https://doi.org/10.2351/7.0001528 VL - 36 IS - 4 SP - 1 EP - 7 PB - AIP Publishing CY - Melville, NY AN - OPUS4-61498 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yang, Chunliang A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Multi-refining effects of an AC electromagnetic field on the microstructure in AA5754 laser beam welding N2 - Fine-grain structure is beneficial to the mechanical properties of the joint. Different kinds of grain and sub-grain structures refined by magnetic field during laser beam welding of AA5754 aluminum alloy are analyzed in this manuscript, and the influences of different magnetic field parameters (magnetic flux density and frequency) in these refining effects are also studied. Using the scanning electron microscope (SEM), the sub-grain structure near the fusion line was obtained, and it was found that the branching promotion and branches refinement can be achieved by the magnetic field. The branches become finer with the magnetic flux density or frequency increases, and this effect is stronger in the dendritic region than in the equiaxed region. The results of electron backscatter diffraction (EBSD) in the equiaxed region show that a high-frequency magnetic field can greatly reduce the average grain size, while a low-frequency one has little effect. A phenomenological nucleation model based on dendrite fragmentation theory was established, and it was introduced into the phase field model to analyze the equiaxed grains evolution process. In addition, another refinement mechanism was also observed. The periodic solidification pattern caused by the unstable solidification in the molten pool can refine the grains, and the magnetic field promotes this kind of grain refinement by promoting the solidification period. KW - Laser beam welding KW - Magnetic field KW - Aluminum alloy KW - Crystal branch development KW - Periodic solidification pattern KW - Grain refinement PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-637222 DO - https://doi.org/10.1016/j.ijheatmasstransfer.2025.127509 SN - 0017-9310 VL - 252 SP - 1 EP - 16 PB - Elsevier Ltd. AN - OPUS4-63722 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Yang, Chunliang A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Bachmann, Marcel A1 - Putra, Stephen Nugraha A1 - Rethmeier, Michael T1 - Experimental and numerical study on grain refinement in electromagnetic assisted laser beam welding of 5754 al alloy N2 - Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase in the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are ana lyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain size after welding verify the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains, that have been solidified and formed previously, from further growth and generates some small cel lular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement. T2 - ICALEO 2023 CY - Chicago, IL, USA DA - 16.10.2023 KW - Laser beam welding KW - Magnetic field KW - Crystal branch development KW - Grain refinement KW - Periodic solidification pattern PY - 2023 AN - OPUS4-58493 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Influence of oscillating magnetic field on the keyhole stability in deep penetration laser beam welding N2 - The stability of the keyhole decreases for deep penetrated high-power laser beam welding. The keyhole tends to collapse with increasing laser power and e.g. keyhole induced porosity can occur. This study deals with the observation of the keyhole during high-power laser beam welding in partial penetration mode by means of a high-speed camera. A butt configuration of 25 mm thick structural steel and transparent quartz glass was used for the experiments. An oscillating magnetic field was applied perpendicular to the welding direction on the root side of the steel plate. The keyhole was highlighted with a coaxial diode laser. It was ascertained that the stability of the keyhole and the weld penetration depth were increased by applying an oscillating magnetic field with an oscillating frequency of 1.2 kHz and a magnetic flux density of 50 mT. KW - Magnetic field KW - Laser beam welding KW - Keyhole stability PY - 2021 DO - https://doi.org/10.1016/j.optlastec.2020.106715 SN - 0030-3992 VL - 135 SP - 106715 PB - Elsevier Ltd. AN - OPUS4-52007 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Meng, Xiangmeng A1 - Bachmann, Marcel A1 - Artinov, Antoni A1 - Rethmeier, Michael T1 - The influence of magnetic field orientation on metal mixing in electromagnetic stirring enhanced wire feed laser beam welding N2 - The application of the electromagnetic stirring from an oscillating magnetic field can improve the metal mixing in wire feed laser beam welding. However, the extra parameters introduced in this technique make the selection of an optimal combination of process parameters more difficult. In the current study, besides the commonly concerned magnetic flux density and frequency, the influence of the magnetic field orientation (magnetic field angle) on the transport of filler metal is studied numerically and experimentally. Ex-situ X-ray fluorescence spectrometer measurements are used to map the metal mixing in the final weld. A three-dimensional transient multi-physical model is developed to reveal the deeper physical essence, considering the coupling between heat transfer, fluid flow, keyhole dynamics, element transport and magnetohydrodynamics. The spatial distribution of the laser energy on the keyhole wall is calculated by a ray tracing algorithm. The results show that the magnetic field with smaller angle with respect to the transverse direction provides better penetration capacity, and its stirring effect can reach the lower part of the molten pool. Therefore, the smaller magnetic field angle produces better metal mixing. A constant downward flow is formed at the lower part of the molten pool when magnetic field of 10° angle is applied, which brings the filler metal to the root region. As the magnetic field angle increases to 40°, the beneficial downward flow changes into a constant upward flow, resulting in a concentration of the filler metal in the upper region. This study provides further insight of the underlying physics in the electromagnetically enhanced laser beam welding, which may guide the optimization of parameters to achieve property homogeneity or to avoid potential defects. KW - Laser welding KW - Metal mixing KW - Magnetic field KW - Magnetohydrodynamics KW - Multi-physical modelling PY - 2021 DO - https://doi.org/10.1016/j.jmatprotec.2021.117135 VL - 294 SP - 117135 PB - Elsevier B.V. AN - OPUS4-52469 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Meng, Xiangmeng T1 - An investigation of keyhole dynamics and porosity mitigation in laser beam welding with external magnetic field N2 - The macro and micro benefits from a magnetic field have been well recognized in the laser beam welding, but the influence mechanism, especially on the local keyhole dynamics, is yet not fully understood. A combination of experimental approach and numerical modeling was conducted to study the highly transient keyhole dynamics under the magnetic field. It was found that the magnetic field gave a direct impact on the laser energy absorption at the keyhole front wall. The keyhole-induced porosity was suppressed under the influence of the magnetic field, which was confirmed by the micro-X-ray computed tomography. The porosity mitigation comes from multiple physical aspects, including keyhole stabilization, widening of the bubble floating channel, and the electromagnetic expulsive force. The predicted penetration depth and weld pool profiles with/without magnetic field show a good agreement with the experimental measurements, including optical micrographs and in-situ metal/glass observation. T2 - The 75th IIW Annual Assembly and International Conference CY - Tokyo, Japan DA - 17.07.2022 KW - Laser beam welding (LBW) KW - Keyhole dynamics KW - Porosity KW - Magnetic field KW - Multi-physical modeling PY - 2022 AN - OPUS4-55781 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Yang, Chunliang A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Experimental and numerical study on grain refinement in electromagnetic assisted laser beam welding of 5754 al alloy N2 - Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase of the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are analyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain size after welding verifies the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains that have been solidified and formed previously from further growth and generates some small cellular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement. T2 - International Congress of Applications of Lasers & Electro-Optics 2023 CY - Chicago, USA DA - 16.10.2023 KW - Laser beam welding KW - Magnetic field KW - Crystal branch development KW - Grain refinement KW - Periodic solidification pattern PY - 2023 SP - 1 EP - 10 AN - OPUS4-58809 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Yang, Fan T1 - Numerical Investigations of Porosity Mitigation in High-Power Laser Beam Welding with an External Magnetic Field N2 - The application of an external magnetic field has been found to significantly mitigate the porosity ratio in laser beam welded joints of AlMg3 aluminum alloy. To investigate the suppression mechanism, a 3D transient multi-physics coupled numerical model of laser beam welding (LBW), including laser propagation, laser-material interaction, and magnetohydrodynamic effects, has been developed to calculate the keyhole dynamics and weld pool behaviors during the welding process. The induced time-averaged Lorenz force is directed downward. Under the effects of the external magnetic field, the fluid flow pattern and the weld pool profile are both affected. The keyhole geometry reconstruction algorithm is proposed to calculate the keyhole diameter and its fluctuation, which is used to evaluate the keyhole stability. The results indicate that the oscillating magnetic field does not affect keyhole stability obviously in the LBW of aluminum alloy. Moreover, an electromagnetic expulsive force is induced on the bubble because of the time-averaged downward Lorentz force. This electromagnetic expulsive force can accelerate the bubble escape speed considerably. An analytical model is developed for investigating the bubble escape window, which shows that the bubble escape window is expanded by 45% under the effect of the external magnetic field. The calculated results based on the developed model agree well with the experimental results. T2 - 77th IIW Annual Assembly and International Conference CY - Rhodes, Greece DA - 07.07.2024 KW - Numerical simulation KW - Deep penetration laser beam welding; Keyhole stability KW - Porosity defects KW - Magnetic field PY - 2024 AN - OPUS4-60667 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Yang, Fan T1 - Assessment of keyhole stability in laser beam welding with external magnetic field using numerical simulation N2 - The challenge of understanding the physical mechanisms behind porosity reduction by a magnetic field during laser beam welding (LBW) is partly due to the difficulty in quantitatively evaluating keyhole stability. The commonly used index, such as keyhole depth, is typically one-dimensional, which is insufficient to capture the dynamic and three-dimensional fluctuations of the keyhole. In this paper, by utilizing a 3D multiphysical model of LBW with magnetic field, a novel keyhole geometry reconstruction algorithm has been developed to describe the keyhole profile and its fluctuation in a statistical manner to evaluate keyhole stability quantitatively. An equivalent diameter is proposed in this algorithm to reduce the irregularity of the keyhole geometry. The calculation results indicate that the time-averaged keyhole shape over 300 ms in the LBW of steel is conical, regardless of the application of an external magnetic field, which provides a more representative shape. Meanwhile, it is observed from the statistical aspect that the keyhole diameter becomes smaller, except the top part, under the influence of the magnetic field. The standard deviation of the equivalent diameter can be used as a physical variable to assess the keyhole stability quantitatively. The application of an external magnetic field can produce a noticeable reduction of the standard deviation of the equivalent diameter, namely, stabilizing the keyhole during LBW of steel. However, the different contribution from the keyhole stability affected by a magnetic field in suppressing porosity is different with materials. T2 - International Congress of Applications of Lasers & Electro-Optics 2024 CY - Los Angeles, CA, USA DA - 04.11.2024 KW - Deep penetration laser beam welding KW - Numerical simulation KW - Keyhole shape KW - Keyhole stability KW - Magnetic field PY - 2024 AN - OPUS4-61600 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -