TY - JOUR A1 - Blaeß, Carsten A1 - Müller, Ralf T1 - Viscous healing of Vickers indentation–induced cracks in glass N2 - AbstractViscous healing of cracks induced by the Vickers indentation in a soda lime magnesium silicate, a soda borosilicate, and a soda aluminosilicate glass (NAS) was studied by laser scanning microscopy. Plots of the crack length, width, and depth normalized to the initial crack length versus time over viscosity merge into single master curves of each of these quantities for each glass. Despite glass properties do not differ strikingly from each other, however, these master curves strongly differ among the glasses. This finding was attributed to a different interplay of various crack healing phenomena. Lateral cracks were found to be responsible for the bulging of the sample surface around the Vickers imprint, which in turn promotes radial crack widening as the main cause of healing delay. The most rapid healing of lateral cracks was observed in NAS in which bulging and crack widening were least pronounced. KW - Crack healing KW - Glass KW - Vickers indentation PY - 2023 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-587295 SN - 0002-7820 VL - 106 IS - 10 SP - 5795 EP - 5805 PB - Wiley AN - OPUS4-58729 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Blaeß, Carsten A1 - Müller, Ralf A1 - Thompson, Cyrus T1 - Crack healing in glasses N2 - Fundamental understanding of crack healing in glassy crystalline materials is very important for many applications, especially for solid oxide fuel cells (SOFC) sealants since cracks caused by mechanical stress or thermal cycling still remain a substantial bottleneck in developing durable SOFC. Previous studies on soda lime silicate glass published by Singh showed that crack healing is driven by viscous flow. There he postulated that the healing progress is proportional to time, t, and the inverse viscosity. This finding would allow to present for a given glass data of crack healing measured at different temperatures in a master curve, if the healing progress is plotted versus t/η. Such master curves would be a helpful tool in understanding crack healing kinetics. To verify the applicability of such master curves, crack healing in non-crystallizing soda-lime-silicate (NCS) and sodium-borosilicate glasses (NBS) was studied. Cracks were generated by Vickers indention and healed isothermally at different temperatures. Crack healing progress was monitored by optical and electron microscopy. The results show that the above mentioned proportionalities applies to the two glasses. In both cases the afore developed master curve could be obtained. T2 - 91. Jahrestagung HVG-DGG CY - Weimar, Germany DA - 29.05.2017 KW - Glass KW - Crack healing PY - 2017 AN - OPUS4-41347 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Blaeß, Carsten A1 - Müller, Ralf A1 - Thompson, Cyrus T1 - Crack healing in glass matrix composites N2 - Partially crystalline glasses are predominantly used as solid oxide fuel cell (SOFC) sealants due to their superior long term durability. However, cracks caused by thermal cycling still remain a substantial bottleneck in developing durable SOFC sealants inasmuch as, in contrast to crystal free glasses, large crystal volume fractions can retard healing. Hence, the basic understanding of crack healing in glassy crystalline materials and the effects of micro structure are important for finding optimum micro structures for both, durability and crack healing. For studying these effects, several model glass matrix composites (GMC), for which simultaneous crystal growth and crack healing can be excluded, have been synthesized. Sodium calcium silicate glass – zirconia GMC turned out to provide sufficiently homogeneous, dense and durable model GMC for our studies. The microstructure of this GMC shows large crystal free glassy regions embedded in network of finely dispersed ZrO2 nanoscale crystals. Whereas the glassy regions allow easy local crack healing, the network of dispersed crystals increases the effective viscosity on a global scale. This effect substantially retards crack broadening during later healing stages, which often ends up in large pores. Therefore, this type of microstructure seems to be an interesting candidate for crack healing optimized sealants. T2 - 91. Jahrestagung HVG-DGG CY - Weimar, Germany DA - 29.05.2017 KW - Glass KW - Crack healing KW - Glass ceramic KW - Composite PY - 2017 AN - OPUS4-41348 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -