TY - JOUR A1 - Akyel, Fatma A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Brunner-Schwer, Christian A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Influence of heat input on cooling rates and mechanical properties of laser hybrid welded thick structural steels N2 - Laser hybrid welding presents several challenges when used to weld thick steels. A typical weld is divided into the arcdominated and laser-dominated zone. These zones lead to variations in the mechanical properties of the weld. The laserdominated zone is of particular importance regarding mechanical properties, notably Charpy impact toughness, due to the high cooling rates and the absence of filler wire. The low heat input of the laser can lead to martensitic microstructure causing hardening and deterioration of impact toughness. The high heat input of the arc can lead to grain coarsening and even loss of impact toughness. This study examines the influence of heat input on the cooling rates, microstructure and mechanical properties of single-pass laser hybrid welded steels of S355J2 and EH36 with thicknesses up to 30 mm. The experiments were performed with a 20-kW fibre laser and a contactless electromagnetic weld backing in the butt-joint configuration in 1G welding position. The cooling time was measured in three different locations near the fusion lines corresponding to different heights of the seam using a special configuration with pyrometers, collimators and optical fibres. The test specimens for the Charpy impact testing and tensile testing were extracted in three different depths. The experiments indicated that a heat input of 1.6 kJ/mm–2 kJ/mm, 2 kJ/mm–2.4 kJ/mm and 3.7 kJ/mm were recommended when single-pass laser hybrid welding of 20-, 25-, and 30-mm-thick structural steels regarding the minimum requirements of the mechanical properties, respectively. KW - Laser hybrid welding KW - Heat input KW - Mechanical properties KW - Charpy impact toughness KW - Cooling rate PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-625282 DO - https://doi.org/10.1007/s40194-025-01924-8 SN - 1878-6669 SP - 1 EP - 15 PB - Springer CY - United Kingdom AN - OPUS4-62528 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - El-Batahgy, A. A1 - Saiyah, A. A1 - Khafagi, S. A1 - Gumenyuk, Andrey A1 - Gook, S. A1 - Rethmeier, Michael T1 - Shielded metal arc welding of 9%Ni steel using matching ferritic filler metal N2 - Motivated by the tensile strength loss of 9%Ni steel arc welded joints made using Ni-based austenitic filler metals, the feasibility of maintaining the tensile strength using matching ferritic filler metal has been demonstrated. In comparison with shielded metal arc welded joint made using Ni-based austenitic electrode ENiCrMo-6, higher tensile strength comparable to that of the base metal was obtained using matching ferritic electrode. Besides, sufficient impact toughness energies with much lower mismatch were obtained for weld metal and heat-affected zone. Welded joint with a lower mechanical mismatching is of considerable importance for achieving acceptable combination of tensile strength and impact toughness.Abetter combination of These mechanical properties is ensured by applying a post weld heat treatment. KW - Mechanical mismatching KW - Mechanical properties KW - Microstructure KW - Austenitic welding electrode KW - Matching ferritic welding electrode PY - 2020 DO - https://doi.org/10.1080/13621718.2020.1846936 SN - 1362-1718 SP - 1 EP - 7 PB - Taylor & Francis AN - OPUS4-51835 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - El-Batahgy, A. A1 - Saiyah, A. A1 - Khafagi, S. A1 - Gumenyuk, Andrey A1 - Gook, Sergej A1 - Rethmeier, Michael T1 - Shielded metal arc welding of 9%Ni steel using matching ferritic filler metal N2 - Motivated by the tensile strength loss of 9%Ni steel arc welded joints made using Ni-based austenitic filler metals, the feasibility of maintaining the tensile strength using matching ferritic filler metal has been demonstrated. In comparison with shielded metal arc welded joint made using Ni-based austenitic electrode ENiCrMo-6, higher tensile strength comparable to that of the base metal was obtained using matching ferritic electrode. Besides, sufficient impact toughness energies with much lower mismatch were obtained for weld metal and heat-affected zone. Welded joint with a lower mechanical mismatching is of considerable importance for achieving acceptable combination of tensile strength and impact toughness. A better combination of These mechanical properties is ensured by applying a post weld heat treatment. KW - 9%Ni steel KW - Ni-based austenitic welding electrode KW - Matching ferritic welding electrode KW - Mechanical properties KW - Mechanical mismatching KW - Microstructure KW - SMAW PY - 2020 DO - https://doi.org/10.1080/13621718.2020.1846936 VL - 26 IS - 2 SP - 116 EP - 122 PB - Taylor & Francis AN - OPUS4-52025 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -