TY - CONF A1 - Bäßler, Ralph T1 - Suitability of high alloyed materials in molten salts at 600 °C N2 - Within the last years the use of feasible alternative energy sources has risen and is going to replace fossil resources more and more. Nevertheless, service conditions in solar facilities are due to the chemical composition of heat transmission media and temperatures, in many cases, extreme in terms of corrosion. Since the construction of power plants shall be economical with maximum life service, materials selection based on preliminary material qualification is essential to guarantee a secure and reliable operation of those facilities. The materials selection depends on the operation temperature of a power plant on the chemical composition of the transmission fluid used. In high corrosive environments Ni-based alloys are often used as an all-round solution for the construction of corrosion resistant parts, because of their good corrosion properties. However, there might be limits for their use regarding their corrosion behavior, with which this contribution deals. By means of electrochemical measurements and exposure tests the suitability of two high alloyed materials X8NiCrSi38-18 and NiCr25FeAlYB in molten nitrate salt (60 % NaNO3/40 % KNO3) was characterized at 600 °C. T2 - NACE International Annual Corrosion Conference 2016 CY - Vancouver, BC, Canada DA - 6.3.2016 KW - Localized corrosion KW - Nickel based alloys KW - Solar energy KW - Renewables KW - Electrochemical characterization KW - X8NiCrSi38-18 KW - NiCr25FeAlYB PY - 2016 AN - OPUS4-36989 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph T1 - Study of Polyaniline/Silicon Dioxide based Coating on Carbon Steel in Artificial Geothermal Brine N2 - By using the available resources in Indonesia, such as silicon dioxide and marine coating base, the PANI/SiO2 modified alkyd coating was able to protect carbon steel in a deaerated artificial geothermal water. The screening of coatings shows that the modification by adding individual pigment was not sufficient to protect carbon steel even during a short-term exposure, indicated by the discoloration after only seven days of exposure. Electrochemical tests indicated that there was no significant change in the Ecorr between the coated and uncoated carbon steel at room temperature. At 150 °C, the coated carbon steel has a lower potential than that of carbon steel, indicating that the coating is protecting carbon steel cathodically or slowing down the corrosion reaction. Finally, a long-term exposure test confirmed that the PANI/SiO2 modified coating successfully protects the carbon steel in the Sibayak artificial geothermal water up to 150 °C for 6 months. T2 - World Geothermal Congress CY - Online meeting DA - 15.06.2021 KW - Coatings KW - Corrosion KW - Polyaniline KW - Sibayak KW - SiO2 KW - Geothermal PY - 2021 AN - OPUS4-52831 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph T1 - Preliminary Study on Al2O3 Sol-Gel Coating for Corrosion Protection of Martensitic Stainless Steel in Artificial Geothermal Water N2 - Al2O3 coatings are often used as protective layers on steels against electrochemical and high-temperature corrosion because they are chemically inert and stable at elevated temperatures. This study presents preliminary work on the possibilities of using Al2O3 sol-gel coatings for corrosion protection of martensitic stainless steels in geothermal environments. Al2O3 sol-gel coatings were applied on UNS S42000, which is known to be susceptible to uniform and localized corrosion. The coated steel specimens were then tested in two types of artificial geothermal water, which simulate the geothermal fluids found in Sibayak (SBY), Indonesia, and North German Basin (NGB), Germany, respectively. SBY has pH 4 and 1.5 g/L of chloride ions, whereas NGB has a pH of 6 and 166 g/L of chloride ions. All experiments were carried out in autoclaves at 150 °C and 1 MPa under the deaerated condition. Evaluations were performed by investigating the surface profiles of both uncoated and coated steels before and after the corrosion test using a Laser Scanning Microscope (LSM) and Scanning Electron Microscope (SEM). Finally, Electrochemical Impedance Spectroscopy (EIS) was performed to compare the corrosion resistance of Al2O3 coated steels in SBY and NGB solutions. It was observed from the corrosion test that Al2O3 coatings are more suitable for use in the geothermal water with a higher pH. T2 - AMPP Annual International Corrosion Conference 2021 CY - Online Meeting DA - 19.04.2021 KW - Protective coating KW - Sol-gel coating KW - Geothermal KW - Martensitic steel KW - Corrosion PY - 2021 AN - OPUS4-52500 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph T1 - Corrosion Aspects for Materials to be Used in CC(U)S Applications N2 - This contribution provides current findings regarding materials susceptibility for carbon capture, utilization and storage (CCUS) applications. Basing on results gathered in 2 German long-term projects (COORAL and CLUSTER) suitable materials are introduced as well as dominating impurities of the CO2-stream and corrosion mechanisms. Investigations cover the whole CCUS process chain and provide material recommendations for certain parts. T2 - 1st International Conference on Corrosion Protection and Application CY - Chongqing, China DA - 09.09.2019 KW - Carbon KW - Capture KW - Storage KW - Utilization KW - CCS KW - CCU KW - CO2 KW - Corrosion PY - 2019 AN - OPUS4-49302 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph T1 - Determination of Corrosivity: Approach according to UN Regulations N2 - “Corrosive to Metals” (H290) describes the general potential danger of a substance to metallic materials. Uniform and localized attack is considered. It has nothing to do with containment material. Corrosion resistance of materials is determined similarly, but with much lower threshold values. Manual shall provide a simple test to easily determine the aggressivity potential to cause corrosion on metallic materials. Even a simple test requires experienced personnel. There seems to be a need of awareness and understanding training for both officials and applicants. T2 - ECHA GHS Training CY - Online meeting DA - 16.03.2021 KW - Corrosivity KW - Dangerous good KW - Corrosion PY - 2021 AN - OPUS4-52295 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph T1 - Components in CO2-stream, corrosive to Materials to be Used in CC(U)S Applications N2 - CO2 quality specifications are not only a matter of CO2 purity (i.e. CO2 content). The “rest” also matters, in particular contents of reactive impurities affecting material corrosion (and rock alteration). Also chemical reactions in CO2 stream needs to be considered, in particular when combining CO2 streams of different compositions. T2 - WCO Forum at AMPP Annual International Corrosion Conference 2021 CY - Online Meeting DA - 26.04.2021 KW - Carbon capture storage KW - Corrosion PY - 2021 AN - OPUS4-52502 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph T1 - Influence of Precipitating Brine Components on Materials Selection for Geothermal Applications N2 - By exposure and electrochemical tests in the laboratory the Cu- and Pb-effect on corrosion behavior and performance of carbon steel and a corrosion resistant alloy could be assessed. Critical material specific properties were determined by static exposure and electrochemical tests in artificial geothermal water with high salinity and low pH, containing Cu/Pb. It could be shown that significant Cu- resp. Pb-deposition and precipitation only occurred in combination with carbon steel. Corrosion resistant alloys (e. g. Cr- and Ni-dominated stainless steels) prevent the disturbing Cu-agglomeration resp. Pb-deposition. Therefore, they are suitable to be chosen for future design of geothermal piping system, either in massive or in cladded form. Regarding corrosion, formation of crevices with non-metallic materials shall be avoided. So, in addition to its already known limited corrosion resistance, carbon steel shall not be used when copper or lead species are content of the geothermal brine. Otherwise precipitation and/or deposition of metallic copper resp. lead must be expected, increasing the susceptibility of clogging the piping system. From the interactions and pitting corrosion point of view, corrosion resistant alloys (preferably Ni-rich) seem to be most favorable when selecting materials for applications in such geothermal brines. T2 - World Geothermal Congress CY - Online meeting DA - 15.06.2021 KW - Copper KW - Lead KW - Corrosion KW - Steel KW - Geothermal energy PY - 2021 AN - OPUS4-52829 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph T1 - A Coating System for Corrosion Protection of Carbon Steel as an Alternative for High Alloyed Materials N2 - The screening of coatings shows that the modification by adding individual pigment was not sufficient to protect carbon steel even during a short-term exposure, indicated by the discoloration after only seven days of exposure. Electrochemical tests indicated that the coating cathodically protects carbon steel or slows down the corrosion reaction. A long-term exposure test confirmed that the PANI/SiO2 modified coating successfully protects the carbon steel in the Sibayak artificial geothermal water at 150 °C for 6 months. T2 - European Geothermal Congress CY - Berlin, Germany DA - 17.10.22 KW - Corrosion KW - Geothermal KW - Coatings KW - Polyaniniline KW - Silicate PY - 2022 AN - OPUS4-56084 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph T1 - Evaluation of Corrosion Resistance of Metallic Materials in Geothermal Applications N2 - Evaluation of corrosion resistance of metallic materials is essential to assure safe and reliable operation of geothermal sites. One need to be aware that corrosion is not a material's but a system property, determined by medium, material and construction aspects. Various corrosion types have to be evaluated. Conditions in laboratory shall reflect on-site reality. Depending on brine composition and temperature suitability of metallic materials can be ranked. Most important outcome of the research is that highly saline geothermal brines require high alloyed materials, for safe long-term operation. T2 - Geothermal Essentials - Moving Geothermal Forward in Canada: Scaling and Corrosion (Surface Facilities) CY - Online Webinar DA - 16.03.2022 KW - Corrosion KW - Geothermal KW - Steel PY - 2022 AN - OPUS4-54482 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bäßler, Ralph T1 - Corrosion Effects on Materials Considered for CC(U)S Applications N2 - Commercially available carbon steels are suitable for compression and pipelines as long as moisture content and impurities are limited. (water 50 to 100 ppmv, SO2 and NO2 ca. 100 ppmv) Corrosion rates increase with increasing water content. (0.2 – 20 mm/a) Condensation of acids and therefore droplet formation is always possible, even at low water contents. A low SO2 content within the CO2-stream might be more important than a low water content. Cr13-steels showed a general susceptibility to shallow pitting and pitting. So, they seem to be not suitable for CCUS applications. Low alloyed steels showed better corrosion behavior (predictable uniform corrosion). For direct contact with saline aquifer fluids only high alloyed steels shall be used. T2 - EFC Webinar CY - Online Meeting (Chongqing, China) DA - 18.05.2022 KW - Corrosion KW - CO2 quality KW - CO2 KW - CCS KW - CCU KW - Pipeline PY - 2022 AN - OPUS4-54854 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -