TY - CONF A1 - Sankaran, Shivasarathy A1 - Ebell, Gino T1 - Analyzing the performance of discrete galvanic anode systems using electrochemical investigations N2 - Corrosion of reinforcement is one of the major reasons in questioning the service life of building structures. The application of cathodic protection techniques plays a big role in controlling the corrosion process to ensure a longer service life of building structures. This systematic study compares the efficiency and durability of various discrete galvanic zinc anode systems available in the current market using different criteria for measuring efficiency such as potential measurements, electrolyte resistance measurements and several polarization methods to determine the polarizability of the anodes. The results to validate the performance of long-time exposure of discrete zinc anodes in concrete medium are discussed. T2 - EUROCORR 2021 CY - Online meeting DA - 20.09.2021 KW - Corrosion KW - Cathodic Protection KW - Zinc anodes KW - Electrochemical PY - 2021 AN - OPUS4-53507 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kauss, Norman A1 - Heyn, A. A1 - Michael, O. A1 - Schymura, M. A1 - Rosemann, P. T1 - Application limits and sensitisation behaviour of the manganese- and nitrogen-alloyed austenitic stainless steel P2000 (X13CrMnMoN18-14-3) N2 - Nickel‐free high‐nitrogen‐alloyed stainless steels like the P2000 (X13CrMnMoN18‐14‐3) were developed to enhance the strength and corrosion resistance of austenitic stainless steels like 304 and 316 while keeping the typical high ductility. The mechanical and corrosive properties of P2000 were investigated and compared with 304 and 316 to highlight the application opportunities of this new alloy. The microstructure of the solution‐annealed condition was characterised by electron backscatter diffraction and the mechanical properties were studied by uniaxial tensile tests, Charpy impact tests and hardness measurements. The passivation behaviour was analysed using the electrochemical potentiodynamic reactivation, whereas the pitting corrosion resistance was compared by pitting potentials and pitting temperatures. However, secondary thermal influences or suboptimal heat treatment can impair the corrosion resistance due to the precipitation of secondary phases and the resulting sensitisation. Thermodynamic calculations and artificial ageing treatment in the range of 500–900°C for up to 100 h were used to determine critical time–temperature parameters for sensitisation. The microstructure of the various aged states was evaluated by scanning electron microscopy and compared with the degrading corrosion resistance characterised by the KorroPad method. KW - Austenitic stainless steel KW - Electrochemical methods KW - High‐nitrogen steel KW - Mechanical properties KW - Corrosion resistance PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-527925 DO - https://doi.org/10.1002/maco.202112450 VL - 71 IS - 10 SP - 1656 EP - 1667 PB - Wiley-VCH GmbH AN - OPUS4-52792 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Babutzka, Martin T1 - New findings on the formation of corrosion product layers on zinc in the atmosphere N2 - The presentation shows systematic investigations to describe the corrosion and corrosion product formation processes of pure zinc under the climatic conditions currently prevailing in the Federal Republic of Germany. The investigations in their entirety aim at questioning current and establishing new ways of looking at the formation of corrosion products of pure zinc under atmospheric corrosion conditions. Thus, they make a significant contribution in understanding corrosion protection by zinc and zinc coatings. In particular, the focus is placed on the initial stage of the corrosion product formation. A systematic investigation of this time range, which is characterized by very reactive corrosion products, is only made possible by using gel-type electrolytes. The short periods of time at the beginning of weathering is now measurable and their influence on the formation of corrosion products and the kinetics of layer formation describable. By combining the new electrochemical approach with gravimetric, microscopic and analytical methods, new insights could be gained both on a methodic and scientific level. T2 - 2nd Task Group Meeting TC124 WG4-TC 250 SC5 Task Group Corrosion CY - Online Meeting DA - 06.05.2021 KW - Zinc KW - Corrosion products KW - Gel-type electrolytes KW - Corrosion KW - Atmospheric corrosion PY - 2021 AN - OPUS4-52604 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Valet, Svenja A1 - Burkert, Andreas A1 - Ebell, Gino A1 - Babutzka, Martin T1 - Determination of the corrosion product layer resistance on zinc and electrolytically galvanized steel samples by using gel electrolytes N2 - Although zinc and zinc coatings have been widely used for corrosion protection for decades new zinc coatings are constantly being developed. Characterizing the corrosion protectiveness of these new coatings, however, should not be underestimated. While exposure tests are time intensive, cyclic tests can only be used for a very limited field of application. Thus, electrochemical measurements provide both an efficient and an effective alternative. Conventional aqueous bulk electrolytes influence the surface layers of a tested zinc coating and are therefore not reliable. Gel electrolytes, however, have evolved over the last few years, are minimally invasive and provide reliable results. This work describes experiments with gel electrolytes made of agar. Unlike previous work, it proposes a composition of gel electrolyte for minimally invasive description of the protective power of naturally formed oxide layers on zinc and zinc coatings. Therefore, as a first part, the gel electrolyte made of agar is verified as a method for zinc and zinc-coated samples. Afterwards, this paper introduces the corrosion product layer resistance RL as a promising parameter to evaluate the protective power of zinc coatings. Results are verified with EIS and FTIR measurements. An example on a representative zinc coating demonstrates the practical application. KW - Gel electrolytes KW - Agar KW - Zinc coatings KW - Atmospheric exposure KW - Corrosion PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-526053 DO - https://doi.org/10.1016/j.electacta.2021.138191 SN - 0013-4686 VL - 385 SP - 138191 PB - Elsevier Ltd. AN - OPUS4-52605 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Babutzka, Martin T1 - New findings on the formation of corrosion product layers on zinc in the atmosphere N2 - The presentation shows systematic investigations to describe the corrosion and corrosion product formation processes of pure zinc under the climatic conditions currently prevailing in the Federal Republic of Germany. The investigations in their entirety aim at questioning current and establishing new ways of looking at the formation of corrosion products of pure zinc under atmospheric corrosion conditions. Thus, they make a significant contribution in understanding corrosion protection by zinc and zinc coatings. In particular, the focus is placed on the initial stage of the corrosion product formation. A systematic investigation of this time range, which is characterized by very reactive corrosion products, is only made possible by using gel-type electrolytes. The short periods of time at the beginning of weathering is now measurable and their influence on the formation of corrosion products and the kinetics of layer formation describable. By combining the new electrochemical approach with gravimetric, microscopic and analytical methods, new insights could be gained both on a methodic and scientific level. T2 - EUROCORR 2021 CY - Online meeting DA - 20.09.2021 KW - Atmospheric Corrosion KW - Corrosion KW - Corrosion products KW - Gel-type electrolytes KW - Zinc PY - 2021 AN - OPUS4-53332 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Babutzka, Martin A1 - Lehmann, Jens A1 - Burkert, Andreas T1 - Process- and material-related causes for corrosion defects on stainless steels N2 - The presentation provides information on process- and material-related causes for corrosion on stainless steels. The influence of surface grinding is discussed. Methods for enhancing the corrosion resistance of stainless steels are shown. T2 - 3M Webinar “Technologies, Tools & Tips to avoid corrosion on Stainless Steel” CY - Online meeting DA - 25.02.2021 KW - Stainless steel KW - Corrosion KW - Grinding processes PY - 2021 AN - OPUS4-52358 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Aristia, Gabriela A1 - Le, Quynh Hoa A1 - Nofz, Marianne A1 - Sojref, Regine A1 - Bäßler, Ralph T1 - Study of Al2O3 Sol-Gel Coatings on X20Cr13 in Artificial North German Basin Geothermal Water at 150 °C N2 - Al2O3 has been widely used as a coating in industrial applications due to its excellent chemical and thermal resistance. Considering high temperatures and aggressive mediums exist in geothermal systems, Al2O3 can be a potential coating candidate to protect steels in geothermal applications. In this study, γ-Al2O3 was used as a coating on martensitic steels by applying AlOOH sol followed by a heat treatment at 600 °C. To evaluate the coating application process, one-, two-, and three-layer coatings were tested in the artificial North German Basin (NGB), containing 166 g/L Cl−, at 150 °C and 1 MPa for 168 h. To reveal the stability of the Al2O3 coating in NGB solution, three-layer coatings were used in exposure tests for 24, 168, 672, and 1296 h, followed by surface and cross-section characterization. SEM images show that the Al2O3 coating was stable up to 1296 h of exposure, where the outer layer mostly transformed into boehmite AlOOH with needle-like crystals dominating the surface. Closer analysis of cross-sections showed that the interface between each layer was affected in long-term exposure tests, which caused local delamination after 168 h of exposure. In separate experiments, electrochemical impedance spectroscopy (EIS) was performed at 150 °C to evaluate the changes of coatings within the first 24 h. Results showed that the most significant decrease in the impedance is within 6 h, which can be associated with the electrolyte penetration through the coating, followed by the formation of AlOOH. Here, results of both short-term EIS measurements (up to 24 h) and long-term exposure tests (up to 1296 h) are discussed. KW - Al2O3 KW - Geothermal KW - Martensitic steels KW - Behmite KW - Corrosion PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-525551 DO - https://doi.org/10.3390/coatings11050526 SN - 2079-6412 VL - 11 IS - 5 SP - 526 PB - MDPI CY - Basel AN - OPUS4-52555 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Le, Quynh Hoa A1 - Bäßler, Ralph A1 - Bettge, Dirk A1 - Buggisch, E. A1 - Schiller, Bernadette Nicole A1 - Beck, M. T1 - Corrosion Study on Wellbore Materials for the CO2 Injection Process N2 - For reliability and safety issues of injection wells, corrosion resistance of materials used needs to be determined. Herein, representative low-cost materials, including carbon steel X70/1.8977 and low alloyed steel 1.7225, were embedded in mortar to mimic the realistic casing-mortar interface. Two types of cement were investigated: (1) Dyckerhoff Variodur commercial Portland cement, representing a highly acidic resistant cement and (2) Wollastonite, which can react with CO2 and become stable under a CO2 stream due to the carbonation process. Exposure tests were performed under 10 MPa and at 333 K in artificial aquifer fluid for up to 20 weeks, revealing crevice corrosion and uniform corrosion instead of expected pitting corrosion. To clarify the role of cement, simulated pore water was made by dispersing cement powder in aquifer fluid and used as a solution to expose steels. Surface analysis, accompanied by element mapping on exposed specimens and their crosssections, was carried out to trace the chloride intrusion and corrosion process that followed. KW - Carbon capture storage KW - CCS KW - Carbon dioxide KW - Corrosion KW - Carbon steel KW - Aquifer fluid KW - Cement KW - Casing KW - Pitting PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-519774 DO - https://doi.org/10.3390/pr9010115 SN - 2227-9717 VL - 9 IS - 1 SP - 115 PB - MDPI CY - Basel AN - OPUS4-51977 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rütters, H. A1 - Fischer, S. A1 - Le, Quynh A1 - Bettge, Dirk A1 - Bäßler, Ralph A1 - Maßmann, J. A1 - Ostertag-Henning, C. A1 - Wolf, J. Lennard A1 - Pumpa, M. A1 - Lubenau, U. A1 - Knauer, S. A1 - Jaeger, P. A1 - Neumann, A. A1 - Svensson, K. A1 - Lempp, C. A1 - Menezes, F. A1 - Hagemann, B. T1 - Towards defining reasonable minimum composition thresholds – impacts of variable CO2 stream compositions on transport, injection and storage N2 - The collaborative project “Impacts of impurities in CO2 streams captured from different emitters in a regional cluster on transport, injection and storage (CLUSTER)” aimed to set up recommendations on how to define “reasonable minimum composition thresholds” that CO2 streams should meet when accessing CO2 transport pipeline networks. Within CLUSTER, we investigated potential impacts of CO2 streams with different and temporally variable compositions and mass flow rates along the whole CCS chain. Investigations included, amongst others, impacts on: Corrosion of pipeline steel, pipeline network design and related transport costs, alteration of well bore cements, pressure development and rock integrity, geochemical reactions, and petrophysical and geomechanical rock properties. All investigations are based on a generic CCS chain scenario. In this scenario, CO2 streams are captured from a spatial cluster of eleven emitters and collected in a regional pipeline network. Emitters comprise seven fossil fuel-fired power plants equipped with different capture technologies, two cement plants, one refinery and one integrated iron and steel plant. In total, 19.78 Mio t CO2 (including impurities) are captured in the emitter cluster annually. The combined CO2 stream is transported in a trunk line with a length of 400 km (100 km of these offshore) and is injected into five generic storage structures. The storage reservoirs are saline aquifers of the Buntsandstein. The investigations revealed beneficial and deteriorating impacts of different impurities and combinations thereof. Overall, no fundamental technical obstacles for transporting, injecting and storing CO2 streams of the modelled variable compositions and mass flow rates were observed. Based on the results, the CLUSTER project team recommends not to define “minimum composition thresholds” for CO2 streams as strict threshold values for each individual impurity in the stream. Instead, CO2 stream compositions and variabilities for specific CCS projects should be constrained with regard to a set of parameters including i) the overall CO2 content, ii) maximum contents of relevant impurities or elements, iii) acceptable variability of CO2 stream composition, and iv) impurity combinations to be avoided. T2 - 15th International Conference on Greenhouse Gas Control Technologies, GHGT-15 CY - Online meeting DA - 15.03.2021 KW - Corrosion KW - Impurities KW - CO2 quality KW - Pipeline network KW - Whole-chain CCS scenario KW - Recommendations PY - 2021 DO - https://doi.org/10.2139/ssrn.3816427 SP - 1 EP - 18 AN - OPUS4-52418 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Aristia, Gabriela A1 - Bäßler, Ralph A1 - Nofz, Marianne A1 - Sojref, Regine A1 - Kohl, Anka T1 - Short-term exposure tests of ɣ-Al2O3 Sol-gel coating on X20Cr13 in artificial geothermal waters with different pH N2 - The suitability of an Al2O3 coating for corrosion protection on X20Cr13 was evaluated in various artificial geothermal brines, focusing on the influence of different pH (4, 6 and 8) and their chemical compositions on the coating properties. All experiments were performed in the laboratory using autoclaves at 150 ◦C and 1 MPa in deaerated condition for 1 and 7 days. Results showed that the pH of geothermal waters is the most detrimental factor in the transformation of ɣ-Al2O3 and its protective abilities. Delaminations were found in the Coating exposed to geothermal brines with pH 4. FTIR spectra indicated a transformation of ɣ-Al2O3 to boehmite AlOOH after exposure to pH 4 and 6, and bayerite Al(OH)3 was formed after exposure to pH 8. Different Crystal structures of the hydrated Al2O3 also contribute to the stability of the coatings, observed by the SEM- EDX of the surface and cross-section of coatings. This study indicated that ɣ-Al2O3 sol-gel coating presents a promising aspect of corrosion protection in geothermal environment with a neutral pH. KW - Al2O3 KW - Corrosion KW - Coating KW - Martensitic steel PY - 2021 DO - https://doi.org/10.1016/j.geothermics.2021.102193 SN - 0375-6505 VL - 96 SP - 102193 PB - Elsevier Ltd. CY - Amsterdam AN - OPUS4-52931 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -