TY - CONF A1 - Hensel, J. T1 - Influence of build-up height and heat input on distortion and residual stresses in additive repair and modification of multi-material composites using DED-Arc N2 - In hybrid additive manufacturing, components or semi-finished products manufactured by conventional primary forming are enhanced or modified by additive manufactured structures. The integration of additive manufacturing steps into existing production routes opens up significant economic and technical potential. However, systematic investigations focusing on the critical transition area between the specific properties of the substrate (like high-strength) and the additively manufactured component, made of specific filler material, are still lacking. Residual stresses heighten the risk of cold cracking, excessive distortion and a reduction in yield stress. This is particularly evident in sensitive transition areas, resulting from a complex interaction among the material used, process conditions, and component design. This risk can be minimized by an optimized layer structure in combination with suitable process parameters. The focus of the present study was to determine the influence of deposition strategy on t T2 - International Materials Science and Engineering Congress - MSE 2024 CY - Darmstadt, Germany DA - 02.04.2024 KW - DED-Arc KW - Residual stress KW - Heat control PY - 2024 AN - OPUS4-61929 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wandtke, Karsten ED - Becker, Amadeus ED - Schröpfer, Dirk ED - Kromm, Arne ED - Kannengießer, Thomas ED - Scharf-Wildenhain, R. ED - Hälsig, A. ED - Hensel, J. T1 - Residual Stress Evolution during Slot Milling for Repair Welding and Wire Arc Additive Manufacturing of High-Strength Steel Components N2 - High-strength steels offer potential for weight optimization due to reduced wall thicknesses in modern constructions. Additive manufacturing processes such as Wire Arc Additive Manufacturing (WAAM) enable the resource-efficient production of structures. In the case of defects occurring in weld seams orWAAM components due to unstable process conditions, the economical solution is local gouging or machining and repair welding. It is important to understand the effects of machining steps on the multiaxial stress state in conjunction with the design-related shrinkage restraints. Research into how welding and slot milling of welds andWAAM structures affects residual stresses is still lacking. For this reason, component-related investigations with high-strength steels with yield strengths ≥790 MPa are carried out in our research. In-situ digital image correlation (DIC) and ex-situ X-ray diffraction (XRD) were used to analyze the stresses and strains induced on specimens during and after milling. The systematic analyses revealed a significant interaction of the stiffness and microstructure of the specimens with the initial residual stresses induced by welding. Subsequent repair welds can result in significantly higher residual stresses. KW - High strength steels KW - Additive manufacturing KW - Residual stress KW - Repair welding KW - Ditigtal image correlation PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-593515 DO - https://doi.org/10.3390/met14010082 VL - 14 IS - 1 SP - 1 EP - 11 PB - MDPI CY - Basel AN - OPUS4-59351 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scharf-Wildenhain, R. T1 - Effect of deposition strategies on mechanical properties and residual stresses at the transition zone of component and substrate in hybrid DED-arc manufacturing N2 - In hybrid additive manufacturing, components or semi-finished products manufactured by conventional primary forming are enhanced or modified by additive manufactured structures. The integration of additive manufacturing steps into existing production routes opens up significant economic and technical potential. However, systematic investigations focusing on the critical transition area between the specific properties of the substrate (like high-strength) and the additively manufactured component, made of specific filler material, are still lacking. Residual stresses heighten the risk of cold cracking, excessive distortion and a reduction in yield stress. This is particularly evident in sensitive transition areas, resulting from a complex interaction among the material used, process conditions, and component design. This risk can be minimized by an optimized layer structure in combination with suitable process parameters. The focus of the present study was to determine the influence of deposition strategy on the Δt8/5 cooling time, the mechanical properties and the residual stresses in order to establish a correlation between heat control, cooling conditions and residual stresses in the transition area of hybrid-additive components. This contributed to the knowledge regarding the safe avoidance of cold cracking, excessive distortion and a reduction in yield stress and the implementation of hybrid DED-arc manufacturing. The heat control was varied by means of the build-up strategy, heat input and working temperature such that the Δt8/5 cooling times corresponded to the recommended processing range. For the deposition strategy, significant effects were exhibited, in particular on the local residual stresses in the transition area. The working temperature showed a higher influence on cooling time, displacement and residual stresses than the heat input. A low working temperature of 100 °C produces almost twice as much deformation of the substrate plate in the tests compared to manufacturing at a high working temperature of 300 °C. Furthermore, compressive longitudinal residual stresses in the sensitive transition area are reduced from 500 MPa to approx. 100 MPa by adjusting the working temperature from 100 °C to 300 °C. Such complex interactions must be clarified comprehensively to provide users with easily applicable processing recommendations and standard specifications for an economical hybrid additive manufacturing of components, for example made of high-strength steels in the transition area. T2 - 77th IIW Annual Assembly and International Conference on Welding and Joining CY - Rhodes, Greece DA - 06.07.2024 KW - DED-Arc KW - Residual stress KW - Heat control PY - 2024 AN - OPUS4-61925 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Evans, Alexander T1 - RS analysis in laser powder bed fused austenitic stainless steel N2 - The determination of residual stress in additively manufactured materials is a challenge, even after decades from the establishment of the basics of residual stress analysis. This is due to the peculiar microstructure of such materials. In fact, researchers have discovered that conventional methods for the determination of RS in materials do not properly work for AM materials. In this tutorial, the basics of RS analysis will be explained, together with the basics of AM manufacturing techniques. The microstructure of the peculiar materials (AM) dealt with here will be elucidated. Successively, the necessary modifications to the conventional approaches to RS analysis will be explained and case studies will be displayed, for the attendant to touch with hands the peculiarities of the approaches. Finally, a few experimental and theoretical tips will be given on dos and don’ts for a correct determination of RS in AM materials. T2 - 11th edition of the European Conference on Residual Stress (ECRS11) CY - Prague, Czech Republic DA - 03.06.2024 KW - Residual stress KW - Additive manufacturing KW - Diffraction KW - Laser Powder Bed Fusion KW - AGIL KW - 316L PY - 2024 AN - OPUS4-60445 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Evans, Alexander T1 - Diffraction based residual stress analysis for laser powder bed fusion alloys N2 - Laser Powder Bed Fusion (PBF-LB/M) is a layer wise metal additive manufacturing (AM) technology, which enables significant advancements of component design, leading to potential efficiency and performance improvements. However, the thermal cycles inherent to the process comprising large localized thermal gradients and repeated melting and solidification cycles leads to the generation of high magnitude residual stresses. These residual stresses can be detrimental both during manufacturing of components and in subsequent application. Therefore, a deep understanding of the influence of process parameters on the residual stresses are crucial for efficient manufacturing and safe application. The experimental characterization of these residual stresses is therefore crucial and can provide a reliable baseline for simulations of both the process and applications. Diffraction-based methods for residual stress analysis using penetrating neutrons and high energy X-rays enable non-destructive spatially resolved characterization of both surface and bulk residual stresses. However, the unique microstructural features inherent to the process can challenge some of our assumptions when using these methods. These challenges include the determination of a stress-free reference, the use of correct elastic constants (both SCEC and DEC) and the influence of surface roughness, texture, and porosity on residual stresses. This presentation will detail recent insights and recommendations for the characterization of residual stresses in a range of PBF-LB/M metallic alloys (Fe, Ni, Al and Ti) T2 - 11th edition of the European Conference on Residual Stress (ECRS11) CY - Prague, Czech Republic DA - 03.06.2024 KW - Residual stress KW - Additive manufacturing KW - Laser Powder Bed Fusion KW - Diffraction PY - 2024 AN - OPUS4-60443 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -