TY - JOUR A1 - Kömmling, Anja A1 - Chatzigiannakis, E. A1 - Beckmann, Jörg A1 - Wachtendorf, Volker A1 - von der Ehe, Kerstin A1 - Braun, Ulrike A1 - Jaunich, Matthias A1 - Schade, U. A1 - Wolff, Dietmar T1 - Discoloration Effects of High-Dose gamma-Irradiation and Long-Term Thermal Aging of (U) HMW-PE N2 - Two polyethylene types with ultra-high (UHMWPE) and high molecular weight (HMW-PE) used as neutron radiation shielding materials in casks for radioactive waste were irradiated with doses up to 600 kGy using a 60Co gammasource. Subsequently, thermal aging at 125∘C was applied for up to one year. Degradation effects in the materials were characterized using colorimetry, UV-Visspectroscopy, IR spectroscopy, and DSC. Both materials exhibited a yellowing upon irradiation.The discoloration of UHMW-PE disappeared again after thermal aging.Therefore, the yellowing is assumed to originate fromannealable color centers in the formof free radicals that are trapped in the crystalline regions of the polymer and recombine at elevated temperatures. For the antioxidantcontaining HMWPE, yellowing was observed after both irradiation and thermal aging. The color change was correlated mainly to decomposition products of the antioxidant in addition to trapped radicals as in UHMW-PE. Additionally, black spots appeared after thermal aging of HMW-PE. KW - Irradiation KW - UHMWPE KW - Colour center KW - Yellowness index PY - 2017 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:kobv:b43-423992 SN - 1687-9422 VL - 2017 IS - Article ID 1362491 SP - 1 EP - 10 PB - Hindawi AN - OPUS4-42399 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wachtendorf, Volker A1 - Barthel, Anne-Kathrin A1 - Geburtig, Anja A1 - Trubiroha, P. ED - Reichert, T. T1 - Low-Temperature Irradiation Experiments for PE, PA, and PC Matrices N2 - In this paper, we demonstrate the effects of radiation exposures of polymeric materials with UV-A 340 nm lamps (ISO 4892-3, Type 1A) at -10 °C in comparison to an irradiation at +50 °C using a Global UV Test 200 fluorescent lamp device from Weiss Umwelttechnik GmbH, which incorporates an active cooling appliance. While the effects at -10 °C actually are lower than at + 50°C their extent was clearly beyond expectations. T2 - 8th European Weathering Symposium CY - Vienna, Austria DA - 20.09.2017 KW - Artificial weathering KW - Irradiation KW - Low-temperature KW - Photo-oxidation KW - Polyamide KW - Polycarbonate KW - Polyethylene PY - 2017 SN - 978-3-9818507-1-0 VL - 18 SP - Paper 22, 319 EP - 329 PB - Thomas Würtz Grafik Design CY - Karlsruhe AN - OPUS4-42130 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -