TY - CONF A1 - Nikoonasab, Ali A1 - Licht, M. A1 - Weiler, L. A1 - Achenbach, R. A1 - Raupach, M. A1 - Gluth, Gregor T1 - Pore Solution composition of GGBFS-containing cement pastes N2 - Ground Granulated Blast-Furnace Slag (GGBFS), a by-product of the iron-making process, has gained significant attention as a supplementary cementitious material and has become increasingly popular in recent years due to its remarkable properties. GGBFS can significantly reduce the environmental impact of cement production when it comes to building concrete structures. GGBFS can either be blended with ordinary Portland cement (OPC) (up to a 90% replacement), or it can be used in the production of alkali-activated materials (AAMs). However, a comprehensive understanding of the pore solution composition is necessary for understanding various aspects of cementitious materials and their durability, including corrosion behavior, passivation of steel, and resistance to deteriorative processes. In the present work, the pore solutions of seven different GGBFS-containing cements (alkali-activated slag, alkali-activated slag/fly ash blends, a hybrid alkaline cement, CEM III/C, and CEM III/B) were extracted and analysed by inductively coupled plasma-optical emission spectroscopy, ion chromatography, pH, redox potential, and conductivity measurements. For comparison, a Portland cement pore solution was analysed similarly. The Concentrations of reduced sulfur were noteworthy in all GGBFS-containing cements, particularly in alkali-activated cements, where concentrations were notably higher compared to standard cements. The redox potentials of the pore solutions were primarily dictated by the concentrations of reduced sulfur, although other factors may contribute. Additionally, sulfur species in the pore solutions had an impact on pH, electrical conductivity, and other properties pertinent to the corrosion of reinforcements. T2 - RILEM Spring Convention 2024 & Conference on Advanced Construction Materials and Processes for a Carbon Neutral Society CY - Milan, Italy DA - 10.04.2024 KW - GGBFS KW - AAM KW - Sulfide KW - Pore solution composition KW - Redox potential PY - 2024 AN - OPUS4-59960 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Nikoonasab, Ali A1 - Licht, M. A1 - Müller, Thoralf A1 - Achenbach, R. A1 - Raupach, M. A1 - Gluth, Gregor T1 - Electrochemical study of steel reinforcement in the synthetic pore solution of alkali-activated binders: Pore solution composition N2 - It is well known that cement manufacture, including CaCO3 calcination and clinker formation, is associated with substantial energy consumption and significant greenhouse gas emissions. Alkali-activated binders (AAB) and concretes made from them can significantly contribute to reducing CO2 emissions caused by the construction industry. However, to what extent and for how long concretes made from AAB can protect the steel in reinforced concrete components from corrosion is still unclear. Unlike PC-based binders, AABs are made by reacting alkaline solutions with solid precursors such as fly ash and ground granulated blast furnace slag (GGBFS). Therefore, steel reinforcement corrosion mechanisms in AAMs differ from PC-based binders. The present study aims to evaluate the corrosion behavior of steel rebar in alkali-activated materials (AAMs) synthetic pore solution with different chemical concentrations representing different GGBFS and Flay Ash based binders by performing electrochemical tests to measure the corrosion rate and corrosion potential of steel rebar. This information can be used to improve the design of AAMs in order to ensure a longer service life for these materials. T2 - Eurocorr2023 CY - Brussels, Belgium DA - 27.08.2023 KW - GGBFS KW - AAM KW - Sulfide KW - Pore solution composition KW - Redox potential KW - Corrosion PY - 2023 AN - OPUS4-59090 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -