TY - JOUR A1 - Grengg, C. A1 - Koraimann, G. A1 - Ukrainczyk, N. A1 - Rudic, O. A1 - Luschnig, S. A1 - Gluth, Gregor A1 - Radtke, Martin A1 - Dietzel, M. A1 - Mittermayr, F. T1 - Cu- and Zn-doped alkali activated mortar – Properties and durability in (bio)chemically aggressive wastewater environments N2 - Metakaolin-based alkali activated mortars (AAM) - with and without CuSO4·5H2O and ZnO addition (mass ratio Mn+/solid binder 0.08% to 1.7%) - were casted and exposed within an extensive long-term field campaign over the period of 20 months to a sewer basin, strongly affected by biogenic acid corrosion. (Un-)exposed AAM were tested regarding their physicochemical and microstructural properties, bioreceptivity and overall durability. Metal addition led to a retarding effect during alkali-activation reaction, as well as to an increase in open porosity of up to 3.0% and corresponding lower compressive strength of up to 10.9%. Reduced microbial colonization and diversity were observed on AAM with Cu, while Zn addition led to increased biodiversity. We propose that the observed higher durability of Cu-doped AAM is due to antibacterial effects and associated reduction of biogenic acid production, superseding overall negative effects of metal-dosage on physical material properties. Observed lower durability of Zn-doped AAM was related to combined negative physicochemical and microbial effects. KW - Microbially induced corrosion KW - Alkali-activated materials KW - Biogenic acid corrosion KW - Biogene Schwefelsäurekorrosion KW - MIC PY - 2021 U6 - https://doi.org/10.1016/j.cemconres.2021.106541 SN - 0008-8846 VL - 149 SP - 1 EP - 15 PB - Elsevier CY - Oxford AN - OPUS4-53070 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -