TY - JOUR A1 - Goedecke, Caroline A1 - Dittmann, Daniel A1 - Eisentraut, Paul A1 - Wiesner, Yosri A1 - Schartel, Bernhard A1 - Klack, Patrick A1 - Braun, Ulrike T1 - Evaluation of thermoanalytical methods equipped with evolved gas analysis for the detection of microplastic in environmental samples N2 - Microplastic particles are currently detected in almost all environmental compartments. The results of detection vary widely, as a multitude of very different methods are used with very different requirements for analytical validity. In this work four thermoanalytical methods are compared and their advantages and limitations are discussed. One of them is thermal extraction-desorption gas chromatography mass spectrometry (TED-GC/MS), an analysis method for microplastic detection that has become established in recent years. In addition, thermogravimetric analysis coupled with Fourier-transform infrared spectroscopy (TGA-FTIR) and mass spectrometry (TGA-MS) were applied, two methods that are less common in this field but are still used in other research areas. Finally, microscale combustion calorimeter (MCC) was applied, a method not yet used for microplastic detection. The presented results are taken from a recently published interlaboratory comparison test by Becker et al. (2020). Here a reference material consisting of suspended matter and specified added polymer masses was examined, and only the results of the recoveries were presented. In the present paper, however, the results for the individual polymers are discussed in detail and individual perspectives for all instruments are shown. It was found that TED-GC/MS is the most suitable method for samples with unknown matrix and unknown, variable kinds and contents of microplastic. TGA-FTIR is a robust method for samples with known matrix and with defined kinds of microplastic. TGA-MS may offer a solution for the detection of PVC particles in the future. MCC can be used as a very fast and simple screening method for the identification of a potential microplastic load of standard polymers in unknown samples. KW - Microplastic KW - TED-GC/MS KW - TGA-MS KW - TGA-FTIR KW - MCC KW - Thermal analysis PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-516687 DO - https://doi.org/10.1016/j.jaap.2020.104961 VL - 152 SP - 104961 PB - Elsevier B.V. AN - OPUS4-51668 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Scholz, Philipp A1 - Falkenhagen, Jana A1 - Wachtendorf, Volker A1 - Brüll, Robert A1 - Simon, Franz-Georg T1 - Investigation on the Durability of a Polypropylene Geotextile under Artificial Aging Scenarios N2 - Geosynthetics are widely used in various civil engineering applications, such as geotextiles in coastal protection, and display a sustainable alternative to natural mineral materials. However, the full benefits of using geosynthetics can only be gained with a long service lifetime of the products. With the use of added stabilizers to the polymers, service lifetimes can be achieved in the range of 100 years. Therefore, accelerated aging methods are needed for the assessment of the long-term performance of geotextiles. In the present study, the behavior of geosynthetic materials made of polypropylene was investigated under artificial aging conditions involving elevated temperatures ranging from 30 to 80 °C, increased oxygen pressures ranging from 10 to 50 bar in water-filled autoclaves, and UV irradiation under atmospheric conditions. ATR-IR spectroscopy was employed to detect the increase in the carbonyl index over various aging durations, indicating the oxidative degradation of the geotextile. The most pronounced increase was observed in the case of aging through UV irradiation, followed by thermal aging. Elevated pressure, on the other hand, had a lower impact on oxidation. High-temperature size exclusion chromatography was utilized to follow the reduction in molar mass under different degradation conditions, and the results were consistent with those obtained from ATR-IR spectroscopy. In polyolefins such as polypropylene, Hindered Amine Stabilizers (HAS) are used to suppress oxidation caused by UV radiation. The quantitative analysis of HAS was carried out using a UV/Vis method and HPLC. The degradation of UV stabilizers during the aging of geotextiles is responsible for the oxidation and the reduction in the molar mass of polypropylene. From the results, it can be concluded that applications of PP geotextile without soil or sand cover might cause the risk of the formation of microplastic particles. Material selection, design, and maintenance of the construction must follow best practices, including the system’s removal or replacement at end-of-life. Otherwise, a sustainable use of geotextiles in civil engineering is not possible. KW - Geotextiles KW - Microplastic KW - Size exclusion chromatography KW - Accelerated aging PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-599739 DO - https://doi.org/10.3390/su16093559 SN - 2071-1050 VL - 16 IS - 9 SP - 1 EP - 15 PB - MDPI AG CY - Basel AN - OPUS4-59973 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Axel A1 - Altmann, Korinna A1 - Kocher, B. A1 - Braun, U. T1 - Determination of tire wear markers in soil samples and their distribution in a roadside soil N2 - Tire wear (TW) constitutes a significant source of microplastic in terrestrial ecosystems. It is known that particles emitted by roads can have an effect up to 100 m into adjacent areas. Here, we apply for the first-time thermal extraction desorption gas chromatography-mass spectrometry (TED-GC/MS) to determine TW in soil samples by detection of thermal decomposition products of styrene-butadiene rubber (SBR), without additional enrichment. Additionally, zinc contents were determined as an elemental marker for TW. Mixed soil samples were taken along three transects along a German motorway in 0.3, 2.0, and 5.0 m distance from the road. Sampling depths were 0–2, 2–5, 5–10, and 10–20 cm. Four fine fractions, 1 000–500, 500–100, 100–50, and <50 μm, were analyzed. TW contents based on SBR ranged from 155 to 15 898 mg kg−1. TW contents based on zinc were between 413 and 44 812 mg kg−1. Comparison of individual values of SBR and zinc reveals SBR as a more specific marker. Results confirm that most TW ends up in the topsoil within a 2 m distance. The sampling strategy resulted in representative data for a larger area. Standard deviations of quadruple TED-GC/MS determination of SBR were <10% for all grain size fractions. TED-GC/MS is a suitable analytical tool for determining TW in soil samples without the use of toxic chemicals, enrichment, or special sample preparation. KW - Microplastic KW - TED-GC/MS KW - Tire wear PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-543344 DO - https://doi.org/10.1016/j.chemosphere.2022.133653 VL - 294 SP - 1 EP - 8 PB - Elsevier Ltd. AN - OPUS4-54334 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Braun, U. T1 - Detection of plastics in soil N2 - Soil acts as a final sink for pollutants. Microplastics from different sources such as plastic mulching, littering, compost, sewage sludge, sedimentary deposition, and tyre abrasion are expected to be found in soil. However, representative and comprehensive information is missing on the sources, transport, and fate. Therefore, a reliable analysis method for microplastics in soils needs to be developed. The presented work describes the development of a procedure for microplastics analysis in soils. A representative sampling based on the on-site conditions and a sample preparation method was established and comprised of a drying step, the separation of microplastic particles > 1 mm, and a density separation for particles < 1 mm. The detection of the large microplastic particles (> 1 mm) was conducted with Attenuated Total Reflection - Fourier Transform infrared Spectroscopy (ATR-FTIR) , while Thermal Extraction Desorption - Gas Chromatography / Mass Spectrometry (TED-GC/MS) was applied for particles < 1 mm, gaining information on the type of polymer and mass fraction. Based on the established method, 14 environmental soil samples ? with different exposure of microplastics from agriculture, industrial sites, roads, and floods were investigated. Due to the arbitrary microplastic particle distribution among the samples for large microplastics, it was reasoned that the found particles were unrepresentative. In contrast, microplastic particles < 1 mm were discovered in a high mass in soil samples exposed to plastic mulching or fertilization with sewage sludge or compost (0 – 115 mg/kg). On average, microplastic contents detected in soil samples taken from a construction site and an inner-city lake were higher (13 – 238 mg/kg). As expected, microplastic content in soil sampled in proximity to roads was more pronounced in the upper soil layers. In contrast, very remote sampling sites, expectably uncontaminated, did not lead to the detection of microplastic regarding to thermoanalytical detection method. In a proof of concept experiment several in vivo and in vitro ecotoxicological tests were applied to evaluate the effect of microplastics (tyre abrasion, polystyrene containing hexabromocyclododecane) in natural soils. In summary, while no effects of the examined probes could be detected on higher levels of biological organization after exposures to earthworm E. andrei, significant changes in several oxidative stress related biomarkers were observed. T2 - SETAC Europe 2022 CY - Kopenhagen, Denmark DA - 15.05.2022 KW - Microplastic KW - TED-GC/MS KW - Soil PY - 2022 AN - OPUS4-55872 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Waniek, Tassilo T1 - The practical implementation of MP reference material production according to ISO standards N2 - Micro- and nanoplastic particles became a topic of public concern all over the world e.g. in water, soil, sludge and air. For a profound risk assessment, it is necessary to identify the origins, hotspots, or transport between different media. Therefore, a representative repeatable analysis is required and reference materials (RM) to proof and compare methods. The basis of MNP investigations is a harmonized analysis which includes sampling, sample preparation and detection. In recent years, spectroscopic methods like µRaman and µFTIR for the determination of particle numbers or thermoanalytical methods like Pyrolysis gas chromatography/mass spectrometry (py-GC/MS) and Thermo extraction/ desorption gas chromatography / mass spectrometry (TED-GC/MS) for mass determination have proven to be particularly suitable. The technical committees (TC) of ISO TC 61 “plastics” and TC 147 “water quality" are working on harmonisation processes on international level. For all standardization approaches, it is necessary that the detection methods and analysis processes can be validated. Therefore, BAM develops reference material for microplastic (MP) analysis for several years with focus on the most common polymers PE, PP, PS, PET and PA. MP particles with a close to reality fragment shape are obtained by cryomilling and sieving. For sample preparation purposes with mass detection methods MP particles are pressed into pills with a water-soluble matrix. Thereby losses due to sample preparation e.g. filtration are included in the verification of an analysis. To ensure a constant quality throughout all MP RM batches the homogeneity and stability is controlled according to ISO Guide 35. Next to TED-GC/MS measurements particle size distribution, infrared spectroscopy and differential scanning calorimetry spectra are taken as accompanying parameters. This presentation aims to introduce into the MP RM production process with ensured quality and special focus on pointing out customized setups for particle comminution, separation, and characterization for standardization. T2 - ASTM Syposioum on Microplastic Analytical and Reference Standards - Opportunities to Advance Microplastic Science CY - Seattle, WA, USA DA - 30.06.2022 KW - Microplastic KW - Reference material KW - Cryo milling KW - Polymer PY - 2022 AN - OPUS4-55891 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Altmann, Korinna T1 - Materials N2 - The talk is a summary of materials and challenges recognized in the CUSP Cluster. T2 - CUSP Annual Meeting at JRC (ISPRA) CY - Ispra, Italy DA - 08.06.2022 KW - Microplastic KW - CUSP KW - H2020 PY - 2022 AN - OPUS4-55099 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Waniek, Tassilo T1 - MNP test and reference material production N2 - Reference materials are essential to analyze the impact of micro- and nanoplastics. The particle size D50 has been chosen as property of interest. They can be produced top-down by milling. For size separation down to a particle size D50 of 50 µm sieving is suitable while smaller particle sizes can be obtained by filtration. After production it is important to control the stability because microplastic in the size range below 10 µm tend to agglomerate. T2 - CUSP early-stage researchers meeting CY - Online meeting DA - 08.11.2022 KW - Particale size KW - Microplastic KW - Reference material KW - Cryo milling KW - Polymer PY - 2022 AN - OPUS4-56214 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Altmann, Korinna T1 - Stakeholder Workshop – Plastictrace WP1 N2 - The talk is about WP1 in the PlasticTrace project funded by Euromat. The projects harmonizes microplastic analysis by developing SOPs and reference materials. WP1 is responsible for material selection and preparation. All particles are homogeneity and stability checked according to ISO guide 35. T2 - Stakeholder workshop of PlasticTrace project CY - Online meeting DA - 14.12.2022 KW - Microplastic KW - Microplastics standardisation KW - Reference materials PY - 2022 AN - OPUS4-56772 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Meurer, Maren T1 - Is olypropylene relevant for microplastic analytics? N2 - Nowadays, in every terrestrial and aquatic ecosystem, even in the remotest areas, small residues of plastics, the so called microplastic (MP) can be found. MPs are particles with a size of 1-1000 µm (ISO/TR 21960:2020), mainly containing synthetic polymers like polyethylene (PE), polypropylene (PP), polystyrene (PS) or polyethylene terephthalate (PET). Even styrene-butadiene rubber (SBR) as an indication for tire wear is included due to similar particle formation. To understand the MPs consequences to the environment, it is of high priority to capture its extent of contamination. It is surprising that in the analysis of polymer masses in environmental samples, PE, PS and SBR are often detected, but only small amounts of PP, although this is the second most commonly produced standard plastic and many MP particles originate from carelessly disposed packaging materials. This presentation provides hypotheses about the reasons of rare PP identification and mass quantification in environmental samples. Different investigations of pristine PP and representative environmental samples, including the pre-treatment by Accelerated Solvent Extraction (ASE) or with density separation followed by the thermal extraction / desorption gas chromatography-mass spectrometry (TED-GC/MS) are presented. The results are discussed according to the material properties and a possible degradation mechanism under different weathering conditions which indicate less stability under relevant storage conditions. T2 - Society of Environmental Toxicology and Chemistry CY - Dublin, Ireland DA - 30.04.2023 KW - Sample preparation KW - Polypropylene KW - Microplastic KW - Degradation PY - 2023 AN - OPUS4-57474 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weber, Simone T1 - Influence of the pH Value to the Degradation of Ester-Based Thermoplastic Polyurethanes N2 - Microplastics are solid polymeric particles with a size of 1-1000 μm (ISO/TR21960:2020), which can be emitted from mismanaged waste into the environment, where microplastic is now ubiquitous. What happens to the microplastics after ending up in the environment, which risks entail and what effects it has are not sufficiently clarified up to now. The most certain issue is that the plastic particles in the environment are exposed to natural ageing, are fragmenting and degrading, such that the potential risk to ecosystems and humans is increasing due to the formation of smaller and smaller particles, potentially even including nanoplastics, if these are ingested before their further degradation. Therefore, and in view of a possible registration of polymers under REACH in the future, it is necessary to investigate the degradation of thermoplastic polyurethanes (TPU) regarding hydrolysis stability to evaluate possible risks and effects to the environment. In the present studies, one thermoplastic polyurethane – with and without hydrolysis stabilizer – is exposed to different pH buffers at 50°C for 14 days to investigate hydrolysis depending to different pH values (acid, alkali and neutral) based on OECD guideline TG111. The hydrolysis behavior of the TPUs is characterized by surface sensitive techniques and on bulk properties. First degradation effects can be detected by SEC. Hydrolysis, especially under acidic and basic conditions, leads to chain scissions to lower molecular masses. Furthermore, the degradation products which indicate the structure of the bulk material were detected by thermo-analytical methods like TGA-FTIR for the small degradation products and the thermo extraction/desorption-gaschromatography/mass spectrometry (TED-GC/MS) for bigger degradation products. Acidic and basic hydrolysis shows the same degradation behavior which is caused by a preferred scission of the ester and urethane functionalities. Surface-sensitive techniques such as XPS demonstrate less carboxylic acid formation at acidic than at alkaline pH value in the TPU without stabilator, where as the TPU with stabilator ages to the same extent in both pH ranges. Altogether, the hydrolysis of TPUs – independently of added stabilizer or not – in acid and alkali environment is accelerated compared to the neutral hydrolysis. T2 - SETAC CY - Dubin, Ireland DA - 30.04.2023 KW - Degradation KW - Thermoplastic Polyurethane KW - Microplastic KW - Polymer Hydrolysis KW - Polymer 3R KW - REACH PY - 2023 AN - OPUS4-58906 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -