TY - CONF A1 - Fischer, Franziska A1 - Kulla, Hannes A1 - Emmerling, Franziska A1 - Rademann, K. T1 - In situ investigation of the mechanochemical formation of cocrystals unsing combined PXRD and Raman spectroscopy N2 - We present an in situ investigation of the mechanochemical formation of cocrystals using synchrotron XRD and Raman spectroscopy. This combination allows to study milling processes on the level of the molecular and crystalline structure thus obtaining reliable data for mechanistic studies. Thereby, mechanochemical syntheses can be optimized to isolate new crystal structures. T2 - Joint BER II and BESSY II User Meeting 2016 CY - Berlin, Germany DA - 07.12.2016 KW - Intermediate KW - Mechanochemistry KW - Cocrystal KW - In situ KW - Milling PY - 2016 AN - OPUS4-38722 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Akhmetova, Irina A1 - Wilke, Manuel A1 - Emmerling, Franziska A1 - Rademann, K. T1 - In situ investigation of mechanochemical syntheses of metal phosphonates N2 - We report on the in situ investigation of mechanochemical syntheses of metal phosphonates. The metal phosphonates are formed in milling reactions starting from a metal acetate and a phosphonic acid. The conversions are observed by synchrotron PXRD and Raman spectroscopy to shed light on the reaction mechanisms including possible intermediates. T2 - 8th HZB User Meeting CY - Berlin, Germany DA - 07.12.2016 KW - Mechanochemistry KW - In situ KW - Metal phosphonates KW - XRD KW - Raman spectroscopy PY - 2016 AN - OPUS4-38780 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Naghib-zadeh, Hamid A1 - Güther, Wolfgang A1 - Rabe, Torsten T1 - High-strength and gas-tight ceramic-ceramic joints by RAB composite tapes N2 - Ceramic components with complex shape cannot be produced frequently by usual ceramic forming and sintering processes. Therefore, numerous joining methods were developed and introduced in industrial scale. Nowadays, multi-stage Mo-Mn-process and active brazing are preferentially used, if temperature-stable and gastight joints are required. Unfortunately, both processes involve cost-intensive thermal processes: hydrogenous atmosphere is essential for metallization in Mo-Mn-process and active brazing takes place under vacuum. Thermal processes can be drastically simplified by using Reactive Air Brazing (RAB). Joining under air atmosphere is an interesting alternative, especially to join oxide ceramic components among themselves. So far, main disadvantage of RAB is low strength of join connections. Aim of this investigation was the development of high-strength, thermal shock resistant and gastight ceramic-ceramic joints by RAB. Therefore, - commercial, silver and copper oxide containing RAB soldering composition was modified by addition of ceramic particles with low thermal expansion coefficients (TEC). Hence, thermal misfit between TEC of solder and ceramic components was significantly reduced. - RAB soldering paste was replaced with newly developed RAB composite tapes, produced by ceramic “doctor blade” technology. Thereby, improved potential exist to tailor the brazing layer relating to composition, thickness and thickness uniformity. Gastight alumina-alumina, alumina-zirconia and zirconia-zirconia joints with strongly improved strength were produced by novel composite tapes. No strength degradation of joints was observed after thermal cycling up to 700°C. T2 - Jahrestagung der Deutschen Keramischen Gesellschaft (DKG) 2016 CY - Freiberg, Germany DA - 07.03.2016 KW - Brazing KW - Compsite tapes KW - Ceramic-ceramc joints PY - 2016 AN - OPUS4-36114 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bonse, Jörn A1 - Derra, U. A1 - Mescheder, H. A1 - Winands, K. A1 - Emonts, C. A1 - Comanns, P. A1 - Krüger, Jörg A1 - Kirner, Sabrina A1 - Skoulas, E. A1 - Tsibidis, G.D. A1 - Stratakis, E. T1 - Mimicking lizard-like surface structures upon ultrashort laser pulse irradiation of inorganic materials N2 - The wetting behavior of material surfaces can be controlled by surface structures. We functionalized inorganic material surfaces, such as steel, titanium alloy and silicon, to modify the wetting behavior using ultrashort laser pulses (fs- to ps-range). The laser processing was performed by scanning the laser beam across the surface of initially polished flat sample material. A combined experimental and theoretical study of the laser processing parameters (peak fluence, scan velocity, line overlap) allowed the identification of different regimes associated with characteristic surface morphologies (laser-induced periodic surface structures, grooves, micro cones, dimples, etc.). Analyses of the surface using optical as well as scanning electron microscopy allowed the identification of morphologies providing the optimum similarity to the natural skin of lizards. For mimicking skin structures of moisture-harvesting lizards towards an optimization of the surface wetting behavior, additionally, a two-step laser processing strategy was established for realizing hierarchical micro- and nanostructures. In this approach, a laser-generated regular array of small dimples was superimposed (step 2) to the micron-scaled capillaries processed before (step 1). Optical focus variation imaging measurements finally revealed the three dimensional topography of the laser processed surfaces derived from lizard skin structures. The functionality of these surfaces was analyzed in view of wetting properties. T2 - E-MRS 2016 Spring Meeting, Symposium C: "Laser-material interactions for tailoring future applications" CY - Lille, France DA - 02.05.2016 KW - Laser-induced periodic surface structures (LIPSS) KW - Femtosecond laser ablation KW - Steel KW - Lizard KW - Wetting PY - 2016 AN - OPUS4-36047 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bonse, Jörn A1 - Koter, Robert A1 - Hartelt, Manfred A1 - Spaltmann, Dirk A1 - Kirner, Sabrina A1 - Pentzien, Simone A1 - Höhm, S. A1 - Rosenfeld, A. A1 - Krüger, Jörg T1 - Tribological properties of femtosecond laserinduced periodic surface structures on metals N2 - Laser-induced periodic surface structures (LIPSS, ripples) were generated on steel and titanium surfaces upon irradiation with multiple linear polarized femtosecond laser pulses (pulse duration 30 fs, central wavelength 790 nm). The experimental conditions (laser fluence, spatial spot overlap) were optimized in a sample-scanning geometry for the processing of large surface areas covered homogeneously by the nanostructures. The irradiated surface regions were subjected to optical microscopy (OM), white light interference microscopy (WLIM) and scanning electron microscopy (SEM) revealing sub-wavelength spatial periods. The nanostructured surfaces were tribologically tested under reciprocal sliding conditions against a sphere of hardened 100Cr6 steel at 1 Hz using paraffin oil and engine oil as lubricants. After 1000 sliding cycles at a load of 1.0 N, the corresponding wear tracks were characterized by OM and SEM. For specific conditions the laser-generated nanostructures endured the tribological treatment. Simultaneously, a significant reduction of the friction coefficient was observed in the laser-irradiated (LIPSS-covered) areas when compared to the non-irradiated surface, indicating the potential benefit of laser surface structuring for tribological applications. T2 - SPIE Photonics West Conference, Symposium "Laser Applications in Microelectronic and Optoelectronic Manufacturing" (LAMOM) XXI CY - San Francisco, CA, USA DA - 13.02.2016 KW - Femtosecond laser ablation KW - Laser-induced periodic surface structures (LIPSS) KW - Tribology KW - Friction KW - Wear PY - 2016 AN - OPUS4-36041 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kirner, Sabrina A1 - Bonse, Jörn A1 - Koter, Robert A1 - Spaltmann, Dirk A1 - Pentzien, Simone A1 - Krüger, Jörg T1 - Femtosecond laser-induced periodic surface structures on titanium nitride coatings for tribological applications N2 - Laser-induced periodic surface structures (LIPSS) were generated on titanium nitride (TiN) hardcoating surfaces (deposited on metallic substrates) upon irradiation with multiple linearly polarized femtosecond laser pulses in air (30 fs duration, 790 nm wavelength, 1 kHz pulse repetition rate). The conditions were optimized in a sample-scanning geometry for the processing of large surface areas (5 mm x 5 mm) covered homogeneously by nanostructures with sub-wavelength periods ranging between ~200 nm and 700 nm. For these nanostructures the coefficient of friction was characterized under reciprocating sliding condition against a ball of hardened steel at 1 Hz using different lubricants (regime of mixed friction). After 1000 cycles, the corresponding wear tracks were characterized by optical and scanning electron microscopy. High-resolution energy dispersive X-ray analyzes (EDX) allowed the visualization of chemical alterations within the wear tracks. For specific conditions, the nanostructures endured the tribological treatment. Our experiments provide a qualification of the tribological performance of the fs-LIPSS on TiN surfaces. T2 - E-MRS 2016 Spring Meeting, Symposium C: "Laser-material interactions for tailoring future applications" CY - Lille, France DA - 02.05.2016 KW - Femtosecond laser ablation KW - Laser-induced periodic surface structures (LIPSS) KW - Tribology KW - Friction KW - Wear KW - Titanium nitride PY - 2016 AN - OPUS4-36042 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Epperlein, Nadja A1 - Menzel, Friederike A1 - Schwibbert, Karin A1 - Koter, Robert A1 - Bonse, Jörn A1 - Sameith, Janin A1 - Krüger, Jörg A1 - Toepel, Jörg T1 - Influence of femtosecond laser produced nanostructures on biofilm growth on steel N2 - Large area periodic surface structures were generated on steel surfaces using 30-fs laser pulses at 790 nm wavelength. Two types of steel exhibiting a different corrosion resistance were used, i.e. a plain structural steel (corrodible) and a stainless steel (resistant to corrosion). Homogeneous fields of laser-induced periodic surface structures (LIPSS) were realized utilizing laser fluences close to the ablation threshold while scanning the sample under the focused laser beam in a multi-pulse regime. The nanostructures were characterized with optical and scanning electron microscopy. For each type of steel, more than ten dentical samples were laser-processed. These samples were subjected to microbial adhesion tests, investigating bacterial adhesion behavior on the laser structures in comparison to polished reference surfaces. Short term experiments (<24h) were carried out to determine initial biofilm development. E. coli as a typical bacterium representing pathogenic bacteria and Shewanella putrefaciens as metal corrosive bacterium were used for biofilm development analyses. Bacterial cell adhesion was determined microscopically after DAPI cell staining (DNA staining). Comparison of the coverage areas between nanostructured and polished surfaces revealed differences in cell adhesion behavior and biofilm structure. T2 - E-MRS 2016 Spring Meeting, Symposium C: "Laser-material interactions for tailoring future applications" CY - Lille, France DA - 02.05.2016 KW - Laser-induced periodic surface structures (LIPSS) KW - Femtosecond laser ablation KW - Biofilms KW - Steel PY - 2016 AN - OPUS4-36045 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Walter, Astrid A1 - von Oertzen, Alexander T1 - EU-Projekt HOMER, home made explosives (HMEs) and recipes characterisation N2 - Das EU-Projekt HOMER befasst sich mit den sogenannten Home Made Explosives (HMEs) und frei verfügbaren Rezepten für deren Herstellung. Diese Selbstlaborate spielen in der heutigen Zeit vor allem im Zusammenhang mit terroristischen Aktivitäten eine bedeutende Rolle. Informationen zu HMEs und ihrer Herstellung werden einfacher denn je über das Internet verbreitet. Hier knüpft das im 7. EU‑Forschungsrahmenprogramm finanzierte Projekt an und bezweckt, die im Internet verfügbaren Quellen auszuwerten und so die Informationslage für Sicherheitskräfte und Ermittlungsbehörden zu verbessern. Im Rahmen des Projektes wird eine automatisierte Suche von Rezepten im Internet entwickelt. Die gefundenen sowie die im Projekt generierten Informationen über HMEs sollen im Endergebnis in Form einer Software (Knowledge Management Platform) informationstechnisch nutzbar gemacht werden. Diese Datenbank soll auch für mobile Geräte zur Verfügung stehen. Der Schwerpunkt der Projektbeteiligung des Fachbereichs 2.3 Explosivstoffe der BAM liegt in der Bewertung der Rezepturen und der auf ihrer Grundlage hergestellten Laborate. Es wurden HMEs entsprechend der vorgefundenen Rezepte und unter Beachtung aller notwendigen Sicherheitsvorkehrungen hergestellt und anschließend sicherheitstechnisch geprüft und bewertet. Dabei wurden sowohl Handhabungsparameter wie die Empfindlichkeiten gegen Schlag, Reibung und thermische Einflüsse ermittelt, als auch die Leistungsparameter wie Detonationsgeschwindigkeit und Luftstoßdruckwirkung gemessen. Die gewonnen Erkenntnisse fließen in die genannte Datenbank ein und sollen beispielsweise Einsatzkräften vor Ort helfen, angemessene Schutzabstände zu ermitteln. Auch das Personal in Laboren der Kriminalämter profitiert von der zusammengetragenen Information über HMEs bei der Analyse von unbekannten Explosivstoffspuren. T2 - 14. BAM-PTB-Kolloquium zur chemischen und physikalischen Sicherheitstechnik CY - Berlin, Germany DA - 14.06.2016 KW - Homemade explosives KW - Explosivstoffe KW - TATP KW - Ammoniumnitrat PY - 2016 AN - OPUS4-36594 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Welter, T. A1 - Deubener, J. A1 - Reinsch, Stefan A1 - Marzok, Ulrich A1 - Müller, Ralf T1 - Glasstrukturen mit geringer Helium- und Wasserstoffpermeation N2 - Wasserstoffbarrieren aus Glas erfahren zunehmend Bedeutung als Werkstoff in der Energietechnik. Trotz wachsender Anwendungen liegen überwiegend empirisch gewonnene Beziehungen zwischen Glaszusammensetzung und Wasserstoffpermeation vor, die im wesentlichen aus dem Verhalten von Kieselglas abgeleitet werden. In dieser Studie werden daher topologische Parameter der Glasstruktur identifiziert und mit thermodynamischen Parametern korreliert. Auf der Seite der Glastopologie steht das freie Volumen und der Vernetzungsgrad des Netzwerkes während auf der thermodynamischen Seite die Konfigurationsentropie bzw. die Konfigurationswärmekapazität Aufschluss über die Verteilung des freien Volumens geben kann. Dabei wird angenommen, dass für Temperaturen weit unterhalb der Glasübergangstemperatur die chemische Löslichkeit von H2 zu vernachlässigen ist. Um die eingeschränkte Datenlage für die Wasserstoffpermeation kompositionell zu erweitern, wurden zusätzlich Heliumpermeationsmessungen ausgewertet. Die Ergebnisse zeigen, dass für Silicatgläser ein charkteristisches Verhältnis von freiem Volumen zu Netzwerkaufspaltung herrschen muss, um permeationsstabile Gläser zu erhalten. T2 - 90. Glastechnische Tagung CY - Goslar, Germany DA - 06.06.2016 KW - Glasstruktur KW - Helium- und Wasserstoffpermeation KW - Alkalialumosilicatsysteme KW - Thermodynamik KW - Energietechnik PY - 2016 AN - OPUS4-36583 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kulla, Hannes A1 - Rademann, K. A1 - Emmerling, Franziska T1 - In situ investigation of mechanochemical reactions with PXRD and Raman spectroscopy - cocrystals of pyrazinamide with dicarboxylic acids N2 - - Cocrystal formation of pyrazinamide with dicarboxylic acids proceeds either directly or via a crystalline intermediate. - Two new crystal structures were discovered by in situ investigations. T2 - ICS 2016 CY - Granada, Spain DA - 30.05.2016 KW - In situ KW - Mechanochemie KW - XRD KW - Cocrystal PY - 2016 AN - OPUS4-36620 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Münster, Christoph A1 - Mente, Tobias A1 - Steger, Jörg A1 - Böllinghaus, Thomas T1 - Influence of experimental conditions and calculation method on hydrogen diffusion coefficient evaluation at elevated temperatures N2 - Hydrogen-assisted cracking (HAC) represents a significant failure risk for (high strength) creep resistant low-alloyed steel components in fossil-fired power plant applications at temperatures of up to and above 200 °C. This particularly applies to respective start-up and shut-down processes associated with alternating service-conditions in terms of load flexible power plants. For quantitative determination of localized crack critical hydrogen concentrations, the temperature dependent hydrogen diffusion coefficients have to be determined as exactly as possible. However, available literature provides a wide range of hydrogen diffusion coefficients for low alloyed steels with similar microstructures. Additionally, the available diffusion data seem not to be very reliable and their scatter increases with decreasing temperature. One reason is that the experimental boundary conditions can have a major impact on the determination of respective effective diffusion coefficients. Hence, the scope of this study is to evaluate the influence of the experimental boundary conditions on the derived diffusion coefficients. In addition, different methods for calculating diffusion coefficients are discussed. To elucidate such influences and to draw a line to practical application, the diffusion and trapping behavior in the creep resistant steel 7CrMoVTiB10 10 has been studied. For such purpose, hydrogen charged specimens were isothermally degassed at different temperatures using carrier gas hot extraction (CGHE). Based on experimental data, a numerical model has been developed by which the hydrogen transport behavior and the respective hydrogen distribution during CGHE can be assessed. It is demonstrated that the specimen heating rate has a large influence on the calculated diffusion coefficients under assumption of isothermal degassing which elsewhere has been underestimated in the assessment of diffusion data in creep-resistant steels. The numerical results suggest that calculation methods for diffusion coefficients are limited if compared to experimental results. It also turned out that the sample preparation time before CGHE can enormously influence determined diffusion coefficients. Consequently, non-homogeneous hydrogen concentration profiles have to be anticipated in the simulations to arrive at characteristic effusion curves consistent to respective CGHE experiments. In turn, validated diffusion coefficients are now available for the low-alloyed Cr-Mo-V steel which might be helpful to calculate appropriate hydrogen removal heat treatment procedures, for instance. T2 - International Hydrogen Conference - Material Performance in Hydrogen Environments CY - Jackson Lake Lodge, Moran, Wyoming, USA DA - 11.09.2016 KW - Hydrogen diffusion KW - Elevated temperatures KW - Welding KW - Creep-resistant steel KW - Numerical modeling KW - Calculation PY - 2016 AN - OPUS4-37403 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Mente, Tobias A1 - Böllinghaus, Thomas T1 - Modeling of hydrogen-assisted cracking (HAC) in duplex stainless steels (DSS) N2 - Modeling of Hydrogen-Assisted Cracking (HAC) in Duplex Stainless Steels (DSS): - Hydrogen causes significant degradation in DSS and consequently HAC - Mechanisms of HAC have not been fully understood in two-phase microstructures - Mesoscale numerical modeling for HAC in DSS was created, coupled to the macroscale, enabling simulation of HAC in both phases independent from predefined crack paths T2 - International Hydrogen Conference - Material Performance in Hydrogen Environments CY - Jackson Lake Lodge, Moran, Wyoming, USA DA - 11.09.2016 KW - Hydrogen KW - Numerical modeling KW - Duplex stainless steel KW - Hydrogen assisted cracking PY - 2016 AN - OPUS4-37404 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Münster, Christoph A1 - Mente, Tobias A1 - Steger, Jörg A1 - Böllinghaus, Thomas T1 - Influence of Experimental Conditions and Calculation Method on Hydrogen Diffusion Coefficient Evaluation at Elevated Temperatures N2 - Hydrogen-assisted cracking (HAC) represents a significant failure risk for (high strength) creep resistant low-alloyed steel components in fossil-fired power plant applications at temperatures of up to and above 200 °C. This particularly applies to respective start-up and shut-down processes associated with alternating service-conditions in terms of load flexible power plants. For quantitative determination of localized crack critical hydrogen concentrations, the temperature dependent hydrogen diffusion coefficients have to be determined as exactly as possible. However, available literature provides a wide range of hydrogen diffusion coefficients for low alloyed steels with similar microstructures. Additionally, the available diffusion data seem not to be very reliable and their scatter increases with decreasing temperature. One reason is that the experimental boundary conditions can have a major impact on the determination of respective effective diffusion coefficients. Hence, the scope of this study is to evaluate the influence of the experimental boundary conditions on the derived diffusion coefficients. In addition, different methods for calculating diffusion coefficients are discussed. To elucidate such influences and to draw a line to practical application, the diffusion and trapping behavior in the creep resistant steel 7CrMoVTiB10 10 has been studied. For such purpose, hydrogen charged specimens were isothermally degassed at different temperatures using carrier gas hot extraction (CGHE). Based on experimental data, a numerical model has been developed by which the hydrogen transport behavior and the respective hydrogen distribution during CGHE can be assessed. It is demonstrated that the specimen heating rate has a large influence on the calculated diffusion coefficients under assumption of isothermal degassing which elsewhere has been underestimated in the assessment of diffusion data in creep-resistant steels. The numerical results suggest that calculation methods for diffusion coefficients are limited if compared to experimental results. It also turned out that the sample preparation time before CGHE can enormously influence determined diffusion coefficients. Consequently, non-homogeneous hydrogen concentration profiles have to be anticipated in the simulations to arrive at characteristic effusion curves consistent to respective CGHE experiments. In turn, validated diffusion coefficients are now available for the low-alloyed Cr-Mo-V steel, which can be helpful to calculate appropriate hydrogen removal heat treatment procedures. T2 - Project Meeting CAStLE CY - Colorado Springs, CO, USA DA - 07.09.2016 KW - Hydrogen KW - Diffusion Coefficient KW - Elevated Temperatures KW - Numerical Modeling KW - Carrier Gas Hot Extraction PY - 2016 AN - OPUS4-37408 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weltschev, Margit A1 - Schwarzer, Stefanie A1 - Eiben, Mario T1 - Comparison of the environmental stress cracking behaviour of polyethylene and polyethylene terephthalate as materials for dangerous goods packagings N2 - The chemical industry has expressed great interest in using polyethylene terephthalate (PET) as material for packagings for the transport of dangerous goods. Due to the high strength and stiffness of PET, the wall thickness and weight of packagings can be reduced. This is a relevant cost factor. PET is a semi-crystalline thermoplast which is produced by polycondensation of terephthalic acid and ethylene glycol. According to the European dangerous goods regulations RID and ADR, samples of PET design types of packagings for dangerous goods must be pre-stored with the original filling good for six months at 23°C, before the design type tests can be carried out. For packagings made of polyethylene (PE) tests to prove the stress cracking resistance by using laboratory methods are possible to reduce time and costs. Therefore, standard liquids, simulating the different types of damaging effects on PE are defined in RID and ADR. However, there is no information and research available about the damaging mechanisms on PET in comparison to PE, especially regarding to stress cracking resistance and test methods. The aim of this work is to compare the stress cracking resistance of PE and PET with the Full Notch Creep Test (FNCT), which was developed by chemical industry and is described in the standards EN ISO 16101 and EN 15507. It was investigated whether testing specimens made of PE and PET with a full coplanar notch around the middle of the specimens show weakening after the impact of a tensile force in a wetting solution (Lutensol® FSA 10) at 50°C in a test device on the basis of the FNCT. The test results confirmed the suitability of the method for eight PE grades. Unfortunately, this method couldn’t be used for PET because the specimens broke during notching. In addition the molding of the sheets and the following temper process for twelve hours are very time-consuming, and the specimens broke during notching due to the high brittleness of PET. Another possibility to provide evidence of stress cracking resistance of PE packagings is laid down in BAM’s Dangerous Goods Rule BAM-GGR 015. This test was carried out with PE and PET bottles to compare both materials. Therefore 1l test bottles were filled with a 5% wetting solution and mounted with a clamping tool for 28 days at 40°C. Tensile test specimens were cut out afterwards from the middle of the bottles in the deformed areas. Tensile strength and breaking elongation of PE specimens were determined in comparison to the PET specimens. The tensile properties of the PET specimens couldn’t be determined due to the strength and the stiffness of the material. In conclusion the only way to provide information about the stress cracking resistance of PET was to perform stacking tests. 1l bottles made of PE and PET were filled with a 5% wetting solution and stored with a stacking load for 28 days at 40°C according to EN ISO 16495. Design types of PE and PET both passed the stacking tests. T2 - EUROCORR 2016 CY - Montpellier, France DA - 11.09.2016 KW - polyethylene terephthalate KW - stress cracking resistance KW - test methods KW - dangerous goods packagings PY - 2016 AN - OPUS4-37448 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Holzweber, Markus A1 - Sobol, Oded A1 - Wirth, Thomas A1 - Böllinghaus, Thomas A1 - Unger, Wolfgang T1 - Deuterium permeation and cracking in duplex steels as viewed by ToF-SIMS and HR-SEM with data fusion N2 - Better understanding of hydrogen assisted degradation and trapping mecha-nisms requires sufficient imaging techniques for respective hydrogen-microstructure interaction studies, in particular with multi-phase metallic micro-structures [1]. The present work is focusing on the elucidation of deuterium be-havior in two austenitic-ferritic duplex stainless steels (DSS) under the assumption that deuterium behaves in many ways similarly to hydrogen [2]. For case studies standard 2205 and lean 2101 DSSs were chosen due to the extensive use of these steels in industry [3]. The analyses were conducted by using a novel in-situ permeation and Time-of-Flight secondary ion mass spectrometry (ToF-SIMS) imaging technique or by ex-situ ToF-SIMS imaging following electrochemical charging experiments. Another pioneering procedure was data fusion (including chemometry) of results of powerful laterally resolved chemical analysis and high resolution structural characterization techniques . Results for the ex-situ observations showed a different influence of deuterium loading on the two steel grades as well as different damage mechanisms in each phase. Formation of sub-surface blisters between the ferrite and austenite were obtained in both the standard and the lean DSS. In both steels, an increased deuterium concentration was observed around deformed regions such as cracks, confirming that they originate from the presence of deuterium [4]. The formation of parallel cracks was obtained only in the austenite within the standard duplex whereas in the lean duplex the highest intensity of deuterium was obtained in the austenite along the ferrite-austenite interphase. In comparison, application of the novel in-situ permeation technique enabled to register and record the deuterium permeation through the material and the respective saturation sequence of the two phases as well as the interfaces. Faster diffusion of the deuterium was observed in the ferrite and a direct proof for deuterium enrichment at the austenite-ferrite interface has been given [1]. The integration of the specified techniques gives a better insight into the processes leading to hydrogen induced failure. These two experimental techniques provide very valuable tools for elucidation of respective metallurgical failure mechanisms that can be used for the validation of respective numerical models for hydrogen assisted cracking (HAC). T2 - 19. Arbeitstagung Angewandte Oberflächenanalytik CY - Soest, Germany DA - 05.09.2016 KW - ToF-SIMS KW - Hydrogen assisted cracking KW - Data fusion KW - SEM PY - 2016 AN - OPUS4-37484 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Scheuerlein, A1 - Lackner, F. A1 - Savary, F. A1 - Rehmer, Birgit A1 - Finn, Monika A1 - Uhlemann, P. T1 - Mechanical properties of the HL-LHC 11 Tesla Nb3Sn magnet constituent materials N2 - A test campaign was launched to determine the mechanical properties of the HL-LHC 11 T Nb3Sn magnet components in order to accurately model the mechanical properties in Finite Element simulations that predict the stress and strain distribution in These magnets. Static and dynamic test methods have been applied for determining elastic materials behavior, and highly accurate Young’s moduli are obtained with the dynamic methods resonance and impulse excitation. These non-destructive methods also enable temperature dependent modulus measurements during in situ heat cycles. T2 - Applied Superconductivity Conference CY - Denver, Colorado, USA DA - 04.09.2016 KW - Young's modulus KW - Tensile test KW - Resonanz KW - Impact excitation PY - 2016 AN - OPUS4-37414 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Babutzka, Martin A1 - Burkert, Andreas A1 - Heyn, A. T1 - Corrosion investigations by using gel-type electrolytes N2 - In the presentation different zinc coatings are presented and investigated. Their naturally formed protective layers are electrochemically characterized and corrosion relevant values are determined by using a gel pad based on polysaccharide. The corrosion relevant values allow the differentiation of various zinc coating systems and can describe the current protective effect provided by the coating. It is shown that gel-type electrolytes influence protective layers and coatings considerably less than corresponding bulk electrolytes. From the results it is evident that gel-type electrolytes represent a viable and promising field in corrosion research.zeige mehr T2 - EUROCORR European Corrosion Congress 2016 CY - Montpellier, France DA - 11.09.216 KW - Corrosion investigations KW - Gel-type electrolytes KW - Zinc coatings PY - 2016 AN - OPUS4-37496 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Lüth, Peter A1 - Brandes, E. A1 - Frost, K. A1 - Kurth, Lutz A1 - Schmidt, Martin A1 - Michael-Schulz, Heike A1 - Uhlig, S. T1 - CEQAT-DGHS Ringversuchsprogramm der BAM in Kooperation mit QuoData und PTB N2 - Bei der Bewertung der Verlässlichkeit der im Labor gewonnenen Prüfergebnisse spielen Ringversuche eine entscheidende Rolle. Die Bundesanstalt für Materialforschung und -prüfung (BAM) unterstützt deshalb den weiteren Ausbau des Ringversuchsprogramms des im Jahr 2007 gegründeten Kompetenzzentrums zur Qualitätssicherung für Prüfungen von Gefahrgütern und Gefahrstoffen auf physikalische Gefahren (Centre for quality assurance for testing of dangerous goods and hazardous substances, CEQAT-DGHS). Bei allen bisher untersuchten Prüfmethoden besteht ein Verbesserungsbedarf. Die RV müssen daher zunächst auf die Methodenentwicklung, -verbesserung und -validierung abzielen und nicht auf Leistungstests. T2 - 14. Kolloquium zur chemischen und physikalischen Sicherheitstechnik (BAM-PTB-Kolloquium) CY - Berlin, Germany DA - 14.06.2016 KW - Gefahrgut KW - Gefahrstoff KW - Ringversuch KW - Prüfmethode KW - Validierung KW - Qualitätssicherung PY - 2016 AN - OPUS4-38465 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jürgens, Maria A1 - Olbricht, Jürgen A1 - Skrotzki, Birgit A1 - Fedelich, Bernard T1 - Ermüdungsverhalten, Lebensdauer und Schädigungsprozesse von P92 unter zyklischen Betriebsbedingungen N2 - Schnelle Lastwechsel mit hohen Temperaturgradienten führen zu thermischen und mechanischen Beanspruchungen v.a. in dickwandigen Bauteilen. Daraus ergibt sich ein komplexes Lastkollektiv, bei dem der Werkstoff sowohl durch Kriechermüdung als auch durch thermomechanische Ermüdung (TMF) geschädigt wird. Welche Auswirkungen hat eine gleichzeitige Änderung von Temperatur, mechanischer Beanspruchung und Arbeitsmedium auf die Schädigungsprozesse? T2 - KWT Dresden CY - Dresden, Germany DA - 18.10.2016 KW - LCF KW - P92 KW - TMF PY - 2016 AN - OPUS4-38587 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hemmleb, M. A1 - Bettge, Dirk A1 - Berger, D. A1 - Driehorst, I. T1 - 3D surface reconstruction with segmented BSE detector: New improvements and application for fracture analysis in SEM N2 - Application of 4Q-BSE detector and dedicated software enables 3D surface measurements of fracture samples in SEM. 3D surface measurement is independent from magnification and material invariant. Quantitative height measurements require careful detector adjustment and system calibration. Live 3D view allows a fast assessment of topographical features. In addition to SE and BSE imaging, 3D surface data help to analyse and interpret fracture samples. T2 - European Microscopy Congress 2016 CY - Lyon, France DA - 28.08.2016 KW - Topography KW - SEM KW - 3D analysis KW - Fractography PY - 2016 AN - OPUS4-38456 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -