TY - GEN A1 - Chaurasia, Prashant Kumar A1 - Fabry, Çağtay A1 - Pittner, Andreas A1 - Rethmeier, Michael T1 - Tandem-GMAW: advanced pulsed and short cicuiting process mode experimental data N2 - This dataset consists of raw recordings for 5 Tandem gas metal arc welding experiments (Tandem-GMAW / T-GMAW). KW - T-GMAW KW - High power welding KW - Deposition efficiency KW - Life Cycle Assessment PY - 2025 DO - https://doi.org/10.5281/zenodo.17951724 PB - Zenodo CY - Geneva AN - OPUS4-65206 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Chaurasia, Prashant Kumar A1 - Cagtay, Fabry A1 - Andreas, Pittner A1 - Rethmeier, Michael T1 - Automated in situ monitoring and analysis of process signatures and build profiles during wire arc directed energy deposition N2 - Wire arc directed energy deposition (DED-Arc) is an emerging metal additive manufacturing process to build near-net shaped metallic parts in a layer-by-layer with minimal material wastage. Automated in situ monitoring and fast-responsive analyses of process signatures and deposit profiles during DED-Arc are in ever demand to print dimensionally consistent parts and reduce post-deposition machining. A comprehensive experimental investigation is presented here involving real-time synchronous measurement of arc current, voltage, and the deposit profile using a novel multi-sensor monitoring framework integrated with the DED-Arc set-up. The recorded current–voltage transients are used to estimate the time-averaged arc power, and energy input in real time for an insight of the influence of wire feed rate and printing travel speed on the deposit characteristics. A unique attempt is made to represent the geometric profiles of the single-track deposits in a generalized mathematical form corresponding to a segmented ellipse, which has exhibited the minimum root-mean-square error of 0.03 mm. The dimensional inconsistency of multi-track deposits is evaluated quantitatively in terms of waviness using build profile monitoring and automated estimation, which is found to increase with an increase in step-over ratio and energy input. For the multi-track mild steel deposits, the suitable range of step-over ratio for the minimum surface waviness is observed to lie between 0.6 and 0.65. Collectively, the proposed framework of synchronized process monitoring and real-time analysis provides a pathway to achieve dimensionally consistent and defect-free parts, and highlights the potential for closed-loop control systems for a wider industrial application of DED-Arc. T2 - IIW Annual Assembly 2025 CY - Genova, Italy DA - 23.06.2025 KW - Additive Manufacturing KW - Arc welding KW - Real-time monitoring and control KW - Dimensional inconsistency KW - DED-arc PY - 2025 AN - OPUS4-65231 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bevilacqua, Tommaso A1 - Gumenyuk, Andrey A1 - Habibi, Niloufar A1 - Hartwig, Philipp A1 - Klawonn, Axel A1 - Lanser, Martin A1 - Rethmeier, Michael A1 - Scheunemann, Lisa A1 - Schröeder, Jöerg T1 - Large-scale thermo-mechanical simulation of laser beam welding using high-performance computing: A qualitative reproduction of experimental results N2 - Laser beam welding (LBW) is a non-contact joining technique that has gained significant importance in modern industrial manufacturing. One potential problem, however, is the formation of solidification cracks, which particularly affects alloys with a pronounced melting range. The aim of the present work is the development of computational methods and software tools to numerically simulate LBW. In order to obtain a sufficiently accurate solution, a large number of finite elements has to be used. Therefore, a highly parallel scalable solver framework, based on the software library PETSc, was used to solve this computationally challenging problem on a high-performance computing architecture. Finally, the experimental results and the numerical simulations are compared. They are found to be in good qualitative agreement, which confirms the validity of the numerical simulations and allows for a better interpretation of the experimentally observed strain distribution. KW - Laser beam welding KW - Termo-mechanical processes KW - Solidification cracking KW - High-performance computing KW - Domain decomposition methods PY - 2025 DO - https://doi.org/10.1016/j.rineng.2025.108827 SN - 2590-1230 SP - 1 EP - 33 PB - Elsevier B.V. AN - OPUS4-65290 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yang, Chunliang A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Phase-field simulation of the dendrite fragmentation by electromagnetic stirring in AA5754 aluminum alloy laser beam welding N2 - A phase-field model including magnetic field induced dendrite fragmentation was established and applied to the cases with different initial crystal nuclear positions for AA5754 aluminum alloy electromagnetic laser beam welding. Compare the calculated results that include dendrite fragmentation caused by the thermal electromagnetic Lorentz force with the results that consider only the thermal electromagnetic Lorentz force, without fragmentation, at the characteristic time instants. Both in the early and late stages, the small fragmentation at the dendrite tip promotes the number of higher-order branches and their growth, especially in the direction perpendicular to the solidification. The later stage fragmentation has the possibility of breaking one grain into several, which verifies the possibility of grain refinement caused by dendrite fragmentation. The fracture surface caused by fragmentation also makes more solid-liquid interfaces and their growth. In addition, the cases with different initial nuclear positions were compared. The grain growth in the low-temperature zone can be inhibited by the equiaxed grains' fragmentation at the high-temperature area (179.8 μm² and 14.7 % start at the center, 115.4 μm² and 9.4 % start at the high-temperature corner, 134.3 μm² and 10.9 % start at the low-temperature corner), which is another kind of grain refinement by the dendrite fragmentation. This kind of inhibition effect on grain growth in the low-temperature region will be enhanced with the increasing time interval between the two crystal nuclei’ appearance (179.8 μm² and 14.7 % when virtual grains appear at t = 4.3803 s and t = 4.3803 s, 134.3 μm² and 10.9 % at t = 4.0977 s and t = 3.9564 s, and 115.4 μm² and 9.4 % at t = 3.8151 s and t = 3.5325 s). KW - Laser beam welding KW - Electromagnetic KW - Aluminum alloys KW - Phase field method KW - Equiaxed grain KW - Dendrite fragmentation PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-656610 DO - https://doi.org/10.1016/j.cwe.2025.100014 SN - 3117-4159 VL - 35 IS - 1 SP - 1 EP - 12 PB - Elsevier B.V. AN - OPUS4-65661 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -