TY - JOUR A1 - Heßmann, Jennifer A1 - Bachmann, Marcel A1 - Hilgenberg, Kai T1 - Numerical and experimental investigation of controlled weld pool displacement by electromagnetic forces for joining dissimilar materials N2 - In order to reduce CO2 emissions, an increasing interest in lightweight construction exists in the automotive industry, especially the multi-material-design approach. The main construction materials here are steels and aluminium alloys. Due to their different physical material properties and limited mutual solubility, these two materials cannot be joined thermally without difficulty. This paper presents a new joining approach for dissimilar materials. It uses electromagnetic displacement of a laser-generated melt pool to produce overlap joints between 1 mm steel (1.0330) and 2 mm aluminium alloy (EN AW 5754). Contactless induced Lorentz forces are generated by an alternating current (AC) magnet system. The controlled displacement of the aluminium alloy melt into the hole of the overlying steel sheet is investigated through numerical and experimental studies. The numerical results are compared with cross sections and thermocouple measurements. For the first time, it is possible to achieve a reproducible controlled melt pool displacement on thin sheets to produce overlap joints between dissimilar materials. KW - Displacement KW - Laser beam welding KW - Dissimilar materials KW - Joining technology KW - Electromagnetic field KW - Lorentz force KW - Numerical investigation PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-516640 DO - https://doi.org/10.3390/met10111447 VL - 10 IS - 11 SP - 1447 EP - 1462 PB - MDPI CY - Basel, Schweiz AN - OPUS4-51664 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmier, Michael T1 - Influence of the spatial laser energy absorption on the molten pool dynamics in high-power laser beam welding N2 - The spatial laser energy absorption inside the keyhole is decisive for the dynamic molten pool behaviors and the resultant weld properties in high-power laser beam welding (LBW). In this paper, a numerical simulation of the LBW process, considering the 3D transient heat transfer, fluid flow, and keyhole dynamics, is implemented, in which the free surface is tracked by the volume-of-fluid algorithm. The underlying laser-material interactions, i.e., the multiple reflections and Fresnel absorption, are considered by an advanced ray-tracing method based on a localized level-set strategy and a temperature-dependent absorption coefficient. The laser energy absorption is analyzed from a time-averaged point of view for a better statistical representation. It is found for the first time that a significant drop in the time-averaged laser energy absorption occurs at the focus position of the laser beam and that the rest of the keyhole region has relatively homogeneous absorbed energy. This unique absorption pattern may lead to a certain keyhole instability and have a strong correlation with the detrimental bulging and narrowing phenomena in the molten pool. The influence of different focus positions of the laser beam on the keyhole dynamics and molten pool profile is also analyzed. The obtained numerical results are compared with experimental measurements to ensure the validity of the proposed model. KW - Laser beam welding KW - Laser energy absorption KW - Molten pool KW - Keyhole dynamics KW - Numerical modeling PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-587531 DO - https://doi.org/10.2351/7.0001078 SN - 1042-346X VL - 35 IS - 4 SP - 1 EP - 8 PB - AIP Publishing AN - OPUS4-58753 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yang, Chunliang A1 - Yan, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Phase-field simulation of the dendrite growth in aluminum alloy AA5754 during alternating current electromagnetic stirring laser beam welding N2 - Electromagnetic stirring is known to promote material flow, reduce porosity, uniform elements distribution, and refine grain in laser beam welding (LBW), which enhances the applicability of LBW in various industries. In this study, a phase-field model of dendrite growth in AA5754 Al alloy electromagnetic stirring laser beam welding was established. The model considered the thermal electromagnetic Lorentz force resulting from the interaction between the electric field generated by the Seebeck effect and the magnetic field, as well as the temperature gradient and solidification rate of the solidification interface obtained from the computational fluid dynamics electromagnetic stirring LBW model. The variation rules of dendrite growth with different magnetic parameters and effects are analyzed. Comprehensively, the magnetic field promotes the solidification rate, thus promoting interfacial instability and a large magnetic flux density leads to a faster interface instability. The solidification rate as well as the temperature gradient affect the growth rate, and the accelerated growth caused by the so lidification rate with a high frequency and a large magnetic flux density effectively inhibits the slow growth caused by the temperature gradient. The thermal electromagnetic Lorentz force is the main factor for the branch increment at low frequencies, while both thermal electromagnetic Lorentz force and temperature gradient in crease the number of branches at high frequencies. The calculated average branch numbers considering various factors in the stable stage under different magnetic parameters were consistent with the results of the scanning electron microscope tests. KW - Laser beam welding KW - Electromagnetic KW - Aluminum alloys KW - Phase field method KW - Dendrite growth PY - 2024 DO - https://doi.org/10.1016/j.ijheatmasstransfer.2023.124754 SN - 0017-9310 VL - 218 SP - 1 EP - 16 PB - Elsevier Ltd. AN - OPUS4-58489 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Heßmann, Jennifer A1 - Hilgenberg, Kai T1 - New approach for multi-material design: Combination of laser beam and electromagnetic melt pool displacement by induced Lorentz forces N2 - Multimaterial structures are a promising solution to reduce vehicle weight and save fuel or electric energy in automotive design. However, thermal joining of steel and aluminum alloys is a challenge to overcome due to different material properties and the formation of brittle intermetallic phases. In this study, a new joining approach for producing overlap line-shaped joints is presented. The lower joining partner (EN AW 5754) is melted by a laser beam, and this melt is displaced into a line-shaped cavity of the upper joining partner (1.0330) by induced Lorentz forces. The melt solidifies in the cavity to a material and form-fitting joint. This approach needs no auxiliary joining elements or filler materials. Previous investigation to produce spot-shaped joints by using this approach showed that quality and reproducibility were limited by known melt pool dynamics of aluminum alloys (keyhole collapses). For line-shaped joints, the melt displacement can take place behind the keyhole. This allows the displacement process to be spatially uncoupled from the influence of keyhole collapses. The study shows that this improved the process stability and the quality of the joint. The created line-shaped joints were microstructurally characterized by transversal sections. Intermetallic phases were identified by electron backscatter diffraction and EDX analysis. The detected intermetallic phases consist of a 5–6 μm compact phase seam of Al5.6Fe2 and a needle-shaped phase of Al13Fe4. Tensile shear tests were carried out to quantify the load capacity. It was possible to create a joint with a load capacity of about 2 kN. KW - Electromagnetic forces KW - Joining dissimilar materials KW - Laser beam welding KW - Steel and aluminium KW - Lorentz forces PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-564840 DO - https://doi.org/10.2351/7.0000763 SN - 1042-346X VL - 35 IS - 1 SP - 1 EP - 8 PB - Laser Institute of America CY - Orlando, Fla. AN - OPUS4-56484 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Numerical studies of process porosity suppression by magnetohydrodynamic technology during the laser beam welding of aluminum alloy N2 - Magnetohydrodynamic (MHD) technology is acknowledged as a promising method for mitigating the porosity defects in laser-welded joints of aluminum alloys. A transient 3D multi-physical numerical model of laser beam welding (LBW), coupled with the MHD and oscillating metal vapor plume model, is developed to study the suppression mechanisms of process porosity by an external magnetic field. The experimental results demonstrate that the porosity ratio is reduced by 93.5 % as the oscillating magnetic field is applied. This significant reduction confirms the effectiveness of the MHD technology in suppressing porosity defects. A downward time-averaged Lorentz force is induced in the weld pool, which affects the fluid flow pattern and the weld pool profile. The change of the flowing pattern in the weld pool by the magnetic field does not always have a positive effect on the porosity suppression. In addition, an analytical model shows that the bubble escape window is expanded by 62 % under the effect of the oscillating magnetic field. The additional upward velocity provided by the electromagnetic expulsive force on the bubbles and the change of weld pool profile are considered favorable factors in eliminating the porosity defects. The numerical and analytical model developed for analyzing the bubble escape window have been validated by experimental results. KW - Laser beam welding KW - Aluminum alloy KW - Process porosity defects KW - Magnetohydrodynamic technology KW - Bubble escape KW - Numerical simulation PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-637642 DO - https://doi.org/10.1016/j.ijheatmasstransfer.2025.127525 SN - 0017-9310 VL - 253 SP - 1 EP - 13 PB - Elsevier Ltd. AN - OPUS4-63764 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Artinov, Antoni A1 - Karkhin, V. A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Mathematical modeling of the geometrical differences between the weld end crater and the steady-state weld pool N2 - The geometrical characteristics of the weld end crater are commonly used as a means of validating numerical results in welding simulations. In this paper, an analytical model is developed for calculating the cooling stage of the welding process after the moving energy source is turned off. Solutions for various combinations of heat sources and heated bodies are found. It is shown that after turning off the Energy source, additional melting of the base material in the longitudinal direction may occur due to the overheated liquid metal. The developed technique is applied to complete-penetration keyhole laser beam welding of 2 mm thick austenitic stainless-steel plate 316L at a Welding speed of 20 mm/s and a laser power of 2.3 kW. The results show a theoretical increase in the weld end crater length of up to 19% compared to the length of the steady-state weld pool. It is found that at the moment of switch off, the weld end crater center, where solidification of the liquid metal ends, is shifted from the heat source axis toward the weld pool tail. The solidification rate and the direction of crystallization of the molten material during the welding process and those in the weld end crater differ significantly. A good agreement between the computational results and the welding experiments is achieved. KW - Weld end crater KW - Steady-state weld pool KW - Mathematical modeling KW - Solidification KW - Laser beam welding PY - 2020 DO - https://doi.org/10.2351/7.0000068 VL - 32 IS - 2 SP - 022024-1 EP - 022024-6 PB - AIP Publishing AN - OPUS4-50767 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Artinov, Antoni A1 - Meng, Xiangmeng A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Study on the transition behavior of the bulging effect during deep penetration laser beam welding N2 - The present work is devoted to the study of the transition behavior of the recently confirmed widening of the weld pool, known as the bulging effect, during high-power deep penetration laser beam welding of thick unalloyed steel sheets. A three-dimensional transient multi-physics numerical model is developed, allowing for the prediction of the bulge formation and the study of its temporal behavior. The model is generalized to account automatically for the transition from partial to complete penetration. Several experimental measurements and observations, such as drilling period, weld pool length, temperature, efficiency, and metallographic cross-sections are used to verify the model and assure the plausibility of the numerical results. The analysis of the calculated temperature and velocity distributions, as well as the evolution of the keyhole geometry, shows that the formation of a bulging region strongly depends on the penetration depth of the weld. Based on the numerical results, the bulge is found to occur transiently, having its transition from a slight bulge to a fully developed bulging between penetration depths of 6 mm and 9 mm, respectively. KW - Laser beam welding KW - Deep penetration KW - Bulge formation KW - Numerical modeling PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-545067 DO - https://doi.org/10.1016/j.ijheatmasstransfer.2021.122171 VL - 184 SP - 122171 PB - Elsevier Ltd. AN - OPUS4-54506 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Straße, Anne A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Study on Duplex Stainless Steel Powder Compositions for the Coating of thick Plates of Laser Beam Welding N2 - Duplex stainless steels combine the positive properties of its two phases, austenite and ferrite. Due to its good corrosion resistance, high tensile strength, and good ductility, it has multiple applications. But laser beam welding of duplex steels changes the balanced phase distribution in favor of ferrite. This results in a higher vulnerability to corrosion and a lower ductility. Herein, different powder combinations consisting of duplex and nickel for coating layers by laser metal deposition (LMD) are investigated. Afterward, laser tracks are welded, and the temperature cycles are measured. The ferrite content of the tracks is analyzed by feritscope, metallographic analysis, and electron backscatter diffraction. The goal is the development of a powder mixture allowing for a duplex microstructure in a two-step process, where first the edges of the weld partners are coated with the powder mixture by LMD and second those edges are laser beam welded. The powder mixture identified by the pretests is tested in the two-step process and analyzed by metallographic analysis, energy-dispersive X-ray spectroscopy, and Vickers hardness tests. The resulting weld seams show a balanced duplex microstructure with a homogenous nickel distribution and a hardness of the weld seam similar to the base material. KW - Duplex AISI 2205 KW - Laser metal deposition KW - Laser beam welding KW - Nickel KW - Stainless steels PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-547024 DO - https://doi.org/10.1002/adem.202101327 SN - 1438-1656 SP - 1 EP - 11 PB - Wiley-VCH CY - Weinheim AN - OPUS4-54702 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bachmann, Marcel A1 - Meng, Xiangmeng A1 - Artinov, Antoni A1 - Rethmeier, Michael T1 - Evaluation of narrowed weld pool shapes and their effect on resulting potential defects during deep penetration laser beam welding N2 - This study presents mechanisms of the evolution of a narrowed region in the weld pool center during deep penetration laser beam welding. In numerous numerical studies presented in this study, it was also found that the local reduction of the weld pool size can cause detrimental effects on the melt flow behavior and the resulting properties of the welds. A particularly large influence of this effect was identified in three aspects. First, the local variation of the solidification sequence of the weld pool causes an increase in the hot-cracking susceptibility due to a locally delayed solidification. Second, it was proven that a change in the local length and width of the weld pool is associated with an adverse impact on the potential flow routes of the molten material that induces stronger local variations of its solidification. Thus, the element mixing, e.g., during the welding with filler materials, is blocked. This leads to a non-homogeneous chemical composition of the final weld and can cause undesired effects on the final material properties. Finally, another observed effect is related to the reduced ability of process pores to reach the top surface. As this type of porosity is usually produced around the keyhole tip, the change of the fluid flow regime above this area plays a significant role in determining the final path of the pores until the premature solidification in the middle of the weld pool captures them. This study summarizes mainly numerical results that were supported by selected experimental validation results. KW - Weld pool shape KW - Laser beam welding KW - Solidification KW - Porosity KW - Numerical process simulation PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-557759 DO - https://doi.org/10.2351/7.0000733 SN - 1042-346X VL - 34 IS - 4 SP - 1 EP - 7 PB - Laser Institute of America CY - Orlando, Fla. AN - OPUS4-55775 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Churiaque Bermejo, C. A1 - Sánchez-Amaya, J. M. A1 - Porrúa-Lara, M. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - The Effects of HLAW Parameters for One Side T-Joints in 15 mm Thickness Naval Steel N2 - The present contribution is the first research reporting full penetration HLAW joints in 15 mm thick EH36 steel butt T-welds with square grooves on 2F welding position by single-sided welding. The effects of welding parameters were investigated to increase the quality of the joints. Conditions leading to defect-free full penetration welds fulfilling naval regulations includes a laser power of 12.5 kW, a welding speed of 1.6 m/min and the vertical laser offset distance from the flange of 1 mm. Advanced characterization of selected welds included a microstructural identification by optical microscopy, SEM, and XRD, revealing the presence of acicular, polygonal and Widmanstätten ferrite, lath martensite, and some retained austenite at FZ. Hardness and microhardness mapping tests showed values of 155 HV at base metal and 200 to 380 HV at the fusion zone connecting the web to the flange. KW - Ship building KW - Laser beam welding KW - Hybrid laser arc welding PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-523931 DO - https://doi.org/10.3390/met11040600 VL - 11 IS - 4 SP - 600 PB - MDPI CY - Basel, Switzerland AN - OPUS4-52393 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -