TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Influence of an external applied AC magnetic field on the melt pool dynamics at high-power laser beam welding N2 - The study deals with the determination of the influence of an externally applied oscillating magnetic field on the melt pool dynamics in high power laser beam and hybrid laser arc welding processes. An AC magnet was positioned under the workpiece which is generating an upward directed electromagnetic force to counteract the formation of the droplets. To visualise the melt flow characteristics, several experiments were carried out using a special technique with mild steel from S355J2 with a plate thickness of up to 20 mm and a quartz glass in butt configuration. The profile of the keyhole and the melt flow were recorded with a highspeed camera from the glass side. Additionally, the influence of the magnetic field orientation to the welding direction on the filler material dilution on laser hybrid welding was studied with variating oscillation frequency. The element distribution over the whole seam thickness was measured with X-ray fluorescence (XRF). The oscillation frequency demonstrated a great influence on the melt pool dynamics and the mixing of the elements of the filler wire. The highspeed recordings showed, under the influence of the magnetic field, that the melt is affected under strong vortex at the weld root, which also avoids the formation of droplets. T2 - 18th Nordic Laser Materials Processing Conference (18th NOLAMP) KW - Laser beam welding KW - AC magnetic field KW - Melt pool dynamics KW - Filler wire mixing PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-539231 DO - https://doi.org/10.1088/1757-899X/1135/1/012017 VL - 1135 IS - 012017 SP - 1 EP - 10 PB - IOP Publishing AN - OPUS4-53923 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Influence of oscillating magnetic field on the keyhole stability in deep penetration laser beam welding N2 - The stability of the keyhole decreases for deep penetrated high-power laser beam welding. The keyhole tends to collapse with increasing laser power and e.g. keyhole induced porosity can occur. This study deals with the observation of the keyhole during high-power laser beam welding in partial penetration mode by means of a high-speed camera. A butt configuration of 25 mm thick structural steel and transparent quartz glass was used for the experiments. An oscillating magnetic field was applied perpendicular to the welding direction on the root side of the steel plate. The keyhole was highlighted with a coaxial diode laser. It was ascertained that the stability of the keyhole and the weld penetration depth were increased by applying an oscillating magnetic field with an oscillating frequency of 1.2 kHz and a magnetic flux density of 50 mT. KW - Magnetic field KW - Laser beam welding KW - Keyhole stability PY - 2021 DO - https://doi.org/10.1016/j.optlastec.2020.106715 SN - 0030-3992 VL - 135 SP - 106715 PB - Elsevier Ltd. AN - OPUS4-52007 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Numerical studies of process porosity suppression by magnetohydrodynamic technology during the laser beam welding of aluminum alloy N2 - Magnetohydrodynamic (MHD) technology is acknowledged as a promising method for mitigating the porosity defects in laser-welded joints of aluminum alloys. A transient 3D multi-physical numerical model of laser beam welding (LBW), coupled with the MHD and oscillating metal vapor plume model, is developed to study the suppression mechanisms of process porosity by an external magnetic field. The experimental results demonstrate that the porosity ratio is reduced by 93.5 % as the oscillating magnetic field is applied. This significant reduction confirms the effectiveness of the MHD technology in suppressing porosity defects. A downward time-averaged Lorentz force is induced in the weld pool, which affects the fluid flow pattern and the weld pool profile. The change of the flowing pattern in the weld pool by the magnetic field does not always have a positive effect on the porosity suppression. In addition, an analytical model shows that the bubble escape window is expanded by 62 % under the effect of the oscillating magnetic field. The additional upward velocity provided by the electromagnetic expulsive force on the bubbles and the change of weld pool profile are considered favorable factors in eliminating the porosity defects. The numerical and analytical model developed for analyzing the bubble escape window have been validated by experimental results. KW - Laser beam welding KW - Aluminum alloy KW - Process porosity defects KW - Magnetohydrodynamic technology KW - Bubble escape KW - Numerical simulation PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-637642 DO - https://doi.org/10.1016/j.ijheatmasstransfer.2025.127525 SN - 0017-9310 VL - 253 SP - 1 EP - 13 PB - Elsevier Ltd. AN - OPUS4-63764 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Experimental and numerical investigations of suppression mechanisms by an oscillating magnetic field on process porosity during laser beam welding N2 - The magnetohydrodynamic (MHD) technology is recognized as a promising approach for improving the quality of deep penetration laser beam welding. This study employs experimental and numerical methods to investigate the effects of an auxiliary oscillating magnetic field on reducing porosity in the laser beam welding of 5754 aluminum alloy. The experimental results clearly demonstrate a significant reduction of 97% in the porosity ratio of the welded joints applied with an oscillating magnetic field compared to those without magnetic field, thereby validating the efficiency of applying MHD technology in mitigating porosity during the laser beam welding process. In addition, a transient 3D multi-physical model has been developed, integrating the MHD model and metal vapor plume, to gain a more comprehensive understanding of the porosity suppression mechanism. The weld pool shape is significantly widened and enlarged because of the Lorentz force, which facilitates the escape of gas bubbles. Meanwhile, the introduction of an oscillating magnetic field generates a time-averaged downward Lorentz force. This averaged downward Lorentz force, in turn, enhances and stables the downward fluid flow, which hinders the bubble backward movement. Meanwhile, this averaged downward Lorentz force induces an upward electromagnetic expulsive force on the bubble, which effectively increases the upward escape velocity of bubbles in the weld pool. The simulation results agree well with the experimental results. T2 - 44. Assistentenseminar Füge- und Schweißtechnik CY - Päwesin, Germany DA - 20.09.2023 KW - Laser beam welding KW - Numerical simulation KW - Magnetohydrodynamic technology KW - Porosity defect KW - Keyhole PY - 2024 UR - https://www.dvs-media.eu/de/neuerscheinungen/4671/44.-assistentenseminar-fuegetechnik SN - 978-3-96144-267-6 VL - 394 SP - 77 EP - 86 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-60784 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Numerical studies of magnetohydrodynamic technology in suppressing process porosity during laser beam welding N2 - The magnetohydrodynamic (MHD) technology is employed to mitigate the porosity problem during partial penetration laser beam welding (LBW) of 10 mm thick aluminum alloy. The effectiveness and universal applicability of the MHD technology in reducing porosity during the LBW process are confirmed by a reduction in the porosity ratio of more than 89%. A transient 3D multi-physical model coupled with the MHD effect has been developed to investigate the suppression mechanism of process porosity. Due to the influence of Lorentz force, there is an obvious change in the weld pool length. This change widens the escaping channel of bubbles escaping from the weld pool. The application of an oscillating magnetic field changes the fluid flow pattern noticeably, whose influence on the formation of porosity defects is highly complicated and nonlinear. T2 - CIRP Conference on Photonic Technologies [LANE 2024] CY - Fürth, Germany DA - 15.09.2024 KW - Laser beam welding KW - Aluminum alloy KW - Process Porosity KW - Porosity suppression KW - Magnetohydrodynamic technology PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-616053 DO - https://doi.org/10.1016/j.procir.2024.08.175 VL - 124 SP - 565 EP - 569 PB - Elsevier B.V. AN - OPUS4-61605 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Numerical studies of magnetohydrodynamic technology in suppressing process porosity during laser beam welding N2 - The magnetohydrodynamic (MHD) technology is employed to mitigate the porosity problem during partial penetration laser beam welding (LBW) of 10 mm thick aluminum alloy. The effectiveness and universal applicability of the MHD technology in reducing porosity during the LBW process are confirmed by a reduction in the porosity ratio of more than 89%. A transient 3D multi-physical model coupled with the MHD effect has been developed to investigate the suppression mechanism of process porosity. Due to the influence of Lorentz force, there is an obvious change in the weld pool length. This change widens the escaping channel of bubbles escaping from the weld pool. The application of an oscillating magnetic field changes the fluid flow pattern noticeably, whose influence on the formation of porosity defects is highly complicated and nonlinear. T2 - 13th CIRP Conference on Photonic Technologies CY - Nuremberg, Germany DA - 15.09.2024 KW - Laser beam welding KW - Aluminum alloy KW - Process Porosity KW - Porosity suppression KW - Magnetohydrodynamic technology PY - 2024 AN - OPUS4-61604 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yang, Chunliang A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Experimental and numerical study on grain refinement in electromagnetic assisted laser beam welding of 5754 Al alloy N2 - Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase in the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are analyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain size after welding verify the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains, that have been solidified and formed previously, from further growth and generates some small cellular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement. KW - Laser beam welding KW - Magnetic field KW - Crystal branch development KW - Grain refinement KW - Periodic solidification pattern PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-584905 DO - https://doi.org/10.2351/7.0001085 SN - 1042-346X VL - 35 IS - 4 SP - 1 EP - 10 PB - AIP Publishing AN - OPUS4-58490 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yang, Chunliang A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Multi-refining effects of an AC electromagnetic field on the microstructure in AA5754 laser beam welding N2 - Fine-grain structure is beneficial to the mechanical properties of the joint. Different kinds of grain and sub-grain structures refined by magnetic field during laser beam welding of AA5754 aluminum alloy are analyzed in this manuscript, and the influences of different magnetic field parameters (magnetic flux density and frequency) in these refining effects are also studied. Using the scanning electron microscope (SEM), the sub-grain structure near the fusion line was obtained, and it was found that the branching promotion and branches refinement can be achieved by the magnetic field. The branches become finer with the magnetic flux density or frequency increases, and this effect is stronger in the dendritic region than in the equiaxed region. The results of electron backscatter diffraction (EBSD) in the equiaxed region show that a high-frequency magnetic field can greatly reduce the average grain size, while a low-frequency one has little effect. A phenomenological nucleation model based on dendrite fragmentation theory was established, and it was introduced into the phase field model to analyze the equiaxed grains evolution process. In addition, another refinement mechanism was also observed. The periodic solidification pattern caused by the unstable solidification in the molten pool can refine the grains, and the magnetic field promotes this kind of grain refinement by promoting the solidification period. KW - Laser beam welding KW - Magnetic field KW - Aluminum alloy KW - Crystal branch development KW - Periodic solidification pattern KW - Grain refinement PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-637222 DO - https://doi.org/10.1016/j.ijheatmasstransfer.2025.127509 SN - 0017-9310 VL - 252 SP - 1 EP - 16 PB - Elsevier Ltd. AN - OPUS4-63722 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Yang, Chunliang A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Experimental and numerical study on grain refinement in electromagnetic assisted laser beam welding of 5754 al alloy N2 - Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase of the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are analyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain size after welding verifies the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains that have been solidified and formed previously from further growth and generates some small cellular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement. T2 - International Congress of Applications of Lasers & Electro-Optics 2023 CY - Chicago, USA DA - 16.10.2023 KW - Laser beam welding KW - Magnetic field KW - Crystal branch development KW - Grain refinement KW - Periodic solidification pattern PY - 2023 SP - 1 EP - 10 AN - OPUS4-58809 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Yang, Chunliang A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Bachmann, Marcel A1 - Putra, Stephen Nugraha A1 - Rethmeier, Michael T1 - Experimental and numerical study on grain refinement in electromagnetic assisted laser beam welding of 5754 al alloy N2 - Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase in the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are ana lyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain size after welding verify the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains, that have been solidified and formed previously, from further growth and generates some small cel lular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement. T2 - ICALEO 2023 CY - Chicago, IL, USA DA - 16.10.2023 KW - Laser beam welding KW - Magnetic field KW - Crystal branch development KW - Grain refinement KW - Periodic solidification pattern PY - 2023 AN - OPUS4-58493 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -