TY - CONF A1 - Frenzel, Florian T1 - Spectroscopic study of plasmon enhanced UPCON luminescence of silica-metal core-shell nanocomposites - status report N2 - The presentation focuses on the current state of the optical spectroscopic studies on plasmon enhanced upconversion luminescent processes of silica-metal core-shell nanocomposites. A general introduction of the upconversion process, the theoretical basis of plasmonic enhancement, the theoretical requirements in regard to NP architecture for plasmon enhanced UC will be outlined. The first proof-of-concept measurements show the difficulty in realization the theoretical measurement parameters in laboratory conditions and underline the need for shifting the experiments to single particle level.“ T2 - Gruppenseminar der Nanooptik an der HU Berlin, Prof. Benson, Institut für Physik, Raum 1‘404 CY - Berlin, Germany DA - 09.05.2017 KW - Upconversion KW - Pplasmon enhancement KW - Core-shell nanoparticles KW - Silca-metal nanoparticles PY - 2017 AN - OPUS4-50698 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bonse, Jörn A1 - Höhm, S. A1 - Kirner, Sabrina V. A1 - Rosenfeld, A. A1 - Krüger, Jörg T1 - Laser-induced periodic surface structures — a scientific evergreen N2 - Laser-induced periodic surface structures (LIPSS, ripples) are a universal phenomenon and can be generated on almost any material upon irradiation with linearly polarized radiation. With the availability of ultrashort laser pulses, LIPSS have gained an increasing attraction during the past decade, since these structures can be generated in a simple single-step process, which allows a surface nanostructuring for tailoring optical, mechanical, and chemical surface properties. In this study, the current state in the field of LIPSS is reviewed. Their formation mechanisms are analyzed in ultrafast time-resolved scattering, diffraction, and polarization constrained double-pulse experiments. These experiments allow us to address the question whether the LIPSS are seeded via ultrafast energy deposition mechanisms acting during the absorption of optical radiation or via self-organization after the irradiation process. Relevant control parameters of LIPSS are identified, and technological applications featuring surface functionalization in the fields of optics, fluidics, medicine, and tribology are discussed. KW - Laser ablation KW - Nanostructures KW - Surface functionalization KW - Surface texture KW - Laser-induced periodic surface structures (LIPSS) PY - 2017 DO - https://doi.org/10.1109/JSTQE.2016.2614183 SN - 1077-260X SN - 1558-4542 VL - 23 IS - 3 SP - 9000615 PB - IEEE AN - OPUS4-38633 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dabah, Eitan A1 - Pfretzschner, Beate A1 - Schaupp, Thomas A1 - Kardjilov, N. A1 - Manke, I. A1 - Boin, M. A1 - Woracek, R. A1 - Griesche, Axel T1 - Time-resolved Bragg-edge neutron radiography for observing martensitic phase transformation from austenitized super martensitic steel N2 - Neutron Bragg-edge imaging was applied for the visualization of a γ-Austenite to α'-martensite phase transformation. In the present study, a super martensitic stainless steel sample was heated until complete austenitization and was subsequently cooled down to room temperature. The martensitic phase Transformation started at Ms = 190 °C. Using a monochromatic neutron beam with λ = 0.390 nm, the transmitted intensity was significantly reduced during cooling below Ms, since the emerging martensitic phase has a higher attenuation coefficient than the austenitic phase at this wavelength. The phase Transformation process was visualized by filming the transmission images from a scintillator screen with a CCD camera with a temporal resolution of 30 s and a spatial resolution of 100 µm. KW - Neutron imaging KW - Bragg-edge imaging KW - Phase transformation PY - 2017 DO - https://doi.org/10.1007/s10853-016-0642-9 SN - 0022-2461 SN - 1573-4803 VL - 52 IS - 6 SP - 3490 EP - 3496 AN - OPUS4-38574 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Cappella, Brunero T1 - Force-distance curves on lubricant films: An approach to the characterization of the shape of the AFM tip N2 - Force-distance curves have been acquired with an atomic force microscope on perfluorpolyether films. It is shown that curves acquired on films of different thickness, at different rates and with different dwell times can be overlapped by rescaling the time or distance axis.When the time or distance axis is rescaled,the force depends only on the surface tension of perfluorpolyether and on geometrical properties of thetip (aperture and perimeter of the tip at a given distance from the apex). Hence, curves acquired with thesame tip overlap. By comparing curves acquired at different rates the dynamics of tip-wetting can be investigated. Fur-thermore, rescaled force-distance curves have been matched with the perimeter of cross sections ofthe tip, i.e. with the perimeter of the three-phase contact line. Such measurements pave the way for anon-destructive investigation of the tip shape. KW - Lubricant films KW - Surface tension KW - Atomic force microscopy KW - Force-distance curves KW - AFM tip shape PY - 2017 DO - https://doi.org/10.1016/j.micron.2016.11.006 SN - 0968-4328 VL - 93 SP - 20 EP - 28 AN - OPUS4-38391 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zerbst, Uwe A1 - Madia, Mauro A1 - Beier, H. Th. T1 - Fatigue strength and life determination of weldments based on fracture mechanics N2 - The paper provides an overview on the results of a German cluster project on the use of fracture mechanics to the determination of the fatigue strength of weldments with fatigue cracks originating at the weld toes. The approach includes (a) a concept for short crack propagation for which the common ΔK concept is not applicable and the crack closure effects are still being gradually build-up, (b) a method for determining fatigue life relevant initial crack sizes as they are needed in any fracture mechanics analysis and (c) multiple cracking and crack coalescence at load levels higher than the endurance limit. The analyses are stochastically performed. Both, the endurance limit and the finite life branch of the S-N curve are determined. Besides a brief introduction into the approach, validation examples are presented. These comprise different weldment types (butt welds, cross joints and longitudinal stiffened plates), two steels (S355NL and S960QL) of quite different strengths, different weld geometries due to different welding techniques (WIG, MAG), as-welded and stress relieved welds and different stress ratios varying from R = -1 to R = 0.5. T2 - FDMD 2017 CY - Lecco, Italy DA - 19.09.2017 KW - Weldments KW - Fatigue strength KW - Fracture mechanics KW - Initial crack size KW - Short crack propagation KW - Multiple crack propagation PY - 2017 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-438500 DO - https://doi.org/10.1016/j.prostr.2017.11.106 SN - 2452-3216 VL - 7 SP - 407 EP - 414 PB - ScienceDirect CY - Lecco, Italy AN - OPUS4-43850 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zerbst, Uwe A1 - Hilgenberg, Kai T1 - Damage development and damage tolerance of structures manufactured by selective laser melting - a review N2 - The additive manufacturing technology of Selective Laser Melting (SLM) experiences a rapid development within an increasing marked of quite different application fields. The properties of SLM materials and structures are influenced by a number of tech-nological parameters such as the metal powder (particle size, homogeneity, cleanliness), the laser tool (power, beam diameter, pulse lengths), the scanning operation (speed, sequence and orientation of melting paths), parameters of the over-all equipment (design and preheating of the base plate, currents and turbulence in the protective gas atmosphere) and, last not least, the hatching strategy including the build-up direction of the structure with respect to the loading direction of the component. For the perspective use of SLM structures as load carrying, safety-relevant components the knowledge of their mechanical properties is necessary. It is essential to understand these in the context of the manufacturing-related features and at the back-ground of the basic characteristics of metallic materials: crystal lattice, microstructure and material defects. The paper provides an overview on factors which affect the mechanical parameters stiffness, strength, ductility, toughness, fatigue crack propagation and fatigue strength in the context of selective laser melting. T2 - FDMD 2017 CY - Lecco, Italy DA - 19.09.2017 KW - Fatigue strength KW - Fracture mechanics KW - Initial crack size KW - Short crack propagation KW - Multiple crack propagation PY - 2017 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-438511 DO - https://doi.org/10.1016/j.prostr.2017.11.071 SN - 2452-3216 VL - 7 SP - 141 EP - 148 PB - ScienceDirect CY - Lecco, Italy AN - OPUS4-43851 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Zerbst, Uwe T1 - Damage development and damage tolerance of structures manufactured by selective laser melting N2 - The additive manufacturing technology of Selective Laser Melting (SLM) experiences a rapid development within an increasing marked of quite different application fields. The properties of SLM materials and structures are influenced by a number of tech-nological parameters such as the metal powder (particle size, homogeneity, cleanliness), the laser tool (power, beam diameter, pulse lengths), the scanning operation (speed, sequence and orientation of melting paths), parameters of the over-all equipment (design and preheating of the base plate, currents and turbulence in the protective gas atmosphere) and, last not least, the hatching strategy including the build-up direction of the structure with respect to the loading direction of the component. For the perspective use of SLM structures as load carrying, safety-relevant components the knowledge of their mechanical properties is necessary. It is essential to understand these in the context of the manufacturing-related features and at the back-ground of the basic characteristics of metallic materials: crystal lattice, microstructure and material defects. The paper provides an overview on factors which affect the mechanical parameters stiffness, strength, ductility, toughness, fatigue crack propagation and fatigue strength in the context of selective laser melting. T2 - 3rd International Symposium on Fatigue Design an Material Defects, FDMD 2017 CY - Lecco, Italy DA - 19.09.2017 KW - Fatigue strength KW - Fracture mechanics KW - Initial crack size KW - Short crack propagation KW - Multiple crack propagation PY - 2017 AN - OPUS4-43853 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gollwitzer, Christian T1 - Synchrotron based absorption edge tomography for §D characterization of the microstructure of MG-Y-Zn alloys N2 - Absorption edge tomography is a method which exploits the sudden change of the attenuation coefficient, when the photon energy crosses the absorption edge of an element. The beamline BAMline at BESSY II, which is operated by the Federal Institute for Materials Research and Testing, can provide a monochromatized beam in a photon energy range from 5 keV up to 80 keV with a bandwidth of 2%. Together with the microtomography setup, this enables differential tomography sensitive to any element with N >= 24 (Cr) by using an appropriate K- or L-edge in this range. Here, absorption edge tomography at the Yttrium edge is employed to perform a non-destructive 3D characterization of the microstructure of a high strength Mg-Y-Zn alloy. The long period stacking ordered (LPSO) phase which forms fibres in this material was extracted based on the Yttrium content and the fibre length distribution was analysed. T2 - Ninth Joint BER II and BESSY II User Meeting CY - Berlin, Germany DA - 13.12.2017 KW - Synchrotron KW - Computed Tomography KW - Absorption edge KW - BAMline PY - 2017 AN - OPUS4-43854 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wachtendorf, Volker A1 - Barthel, Anne-Kathrin A1 - Geburtig, Anja A1 - Trubiroha, P. ED - Reichert, T. T1 - Low-Temperature Irradiation Experiments for PE, PA, and PC Matrices N2 - In this paper, we demonstrate the effects of radiation exposures of polymeric materials with UV-A 340 nm lamps (ISO 4892-3, Type 1A) at -10 °C in comparison to an irradiation at +50 °C using a Global UV Test 200 fluorescent lamp device from Weiss Umwelttechnik GmbH, which incorporates an active cooling appliance. While the effects at -10 °C actually are lower than at + 50°C their extent was clearly beyond expectations. T2 - 8th European Weathering Symposium CY - Vienna, Austria DA - 20.09.2017 KW - Artificial weathering KW - Irradiation KW - Low-temperature KW - Photo-oxidation KW - Polyamide KW - Polycarbonate KW - Polyethylene PY - 2017 SN - 978-3-9818507-1-0 VL - 18 SP - Paper 22, 319 EP - 329 PB - Thomas Würtz Grafik Design CY - Karlsruhe AN - OPUS4-42130 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Martynenko, Irina A1 - Litvin, A.P. A1 - Purcell-Milton, F. A1 - Baranov, A. V. A1 - Fedorov, A.V. A1 - Gun´ko, Y.K. T1 - Application of semiconductor quantum dots in bioimaging and biosensing N2 - In this review we present new concepts and recent progress in the application of semiconductur quantum dots (QD) as labels in two important areas of biology, bioimaging and biosensing. We analyze the biologically relevant properties of QDs focusing on the following topics: QD surface treatment and stability labeling of cellular structures and receptors with QDs, incorporation of QDs in living cells, cytotoxicity of QDs and influence of the biolocical environment on the biological and optical properties of QDs. Initially, we consider utilization of QDs as agants in high-resolution bioimaging techniques that can provide information at the molecular levels. The deverse range of modern live-cell QD-based imaging techniques with resolution far beyond the diffraction limit of light is examined. In each technique, we discuss the pros and cons of QD use and deliberate how QDs can be further engineered to facilitate their application in the respective imaging techniques and to produce significant improvements in resolution. Then we review QD-based point-of-care bioassays, bioprobes, and biosensors designed in different formats ranging from analytic biochemistry assays and ELISA, to novel point-of-care smartphone integrated QD-based biotests. Here, a wide range of QD-based fluorescence bioassays with optical transduction, electrochemiluminescence and photoelectrochemical assays are discussedc. Finally, this review provides an analysis of the prospects of application of QDs in selected important Areas of biology. KW - Fluorescence KW - Semiconductor quantum dot KW - Imaging KW - Quantification KW - Nanoparticle KW - NIR KW - IR KW - Quantum yield KW - Method KW - Microscopy KW - Assay KW - Bioconjugate PY - 2017 DO - https://doi.org/10.1039/c7tb01425b VL - 5 IS - 33 SP - 6701 EP - 6727 PB - Royal Society of Chemistry AN - OPUS4-43027 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -