TY - JOUR A1 - Gook, Sergej A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Method for defect-free hybrid laser-arc welding of closed circumferential welds JF - Welding and Cutting N2 - This paper presents investigation results of a process for defect-free hybrid laser arc welding (HLAW) of closed circumferential welds. The process aims to avoid weld imperfections in the overlap area of a HLAW circumferential weld. A process control strategy for closing the circumferential weld was developed to achieve a defect-free overlap region by controlling the solidification conditions at the end of the weld. The controlled heat flow is achieved by adjusting the parameters of both welding processes involved, the laser beam as well as gas metal arc welding (GMAW) process. Experimental investigations were carried out on 12 mm to 15 mm thick tube sections. The influence of process parameters such as the laser ramp time, the change in magnification scale and the defocusing of the laser beam on the solidifi-cation conditions at the end of the circumferential weld was investigated to find an optimum strategy for ramping out the process energy. Within the framework of the experimental studies, it was demonstrated that defocusing the laser beam in the range between 60 mm and 100 mm over a short run-out area of the weld of approximately 15 mm led to a significantly better weld formation in the overlap area. A favourable cup-shaped weld shape could be achieved without a tendency to crack. The laser optics with a motor-driven lens system made it possible to increase the laser beam diameter without changing the position of the GMAW arc relative to the component surface. KW - Weld defects KW - Hybrid welding KW - Laser beam welding KW - Pipe manufacturing KW - Gas shielded arc welding PY - 2021 VL - 20 IS - 4 SP - 334 EP - 339 PB - DVS Media AN - OPUS4-54665 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Artinov, Antoni A1 - Bachmann, Marcel A1 - Rethmeier, Michael A1 - Karkhin, V. A1 - Khomich, P. T1 - Modeling of hydrodynamic and thermal processes at laser welding with through penetration JF - Welding International N2 - A mathematical model for physical processes in fusion welding has been developed. It is based on the equivalent heat source concept and consists of two parts: thermo-hydrodynamics of the weld pool and heat conduction in the weldment outside the pool. In thermo-hydrodynamic problem, temperature – dependent material properties, keyhole shape, thermo-capillary and natural convection, phase transformations and other physical phenomena are taken into consideration. Solution of the thermo-hydrodynamic problem by the finite element method is demonstrated with keyhole laser beam welding of a 15 mm thick steel plate. Thermo-capillary convection is primarily responsible for the intricate convex-concave melt pool shape and pool enlargement near the plate surfaces. The calculated and experimental molten pool dimensions are in close agreement. KW - Laser welding KW - Weld pool modeling KW - Heat conduction KW - Greens function method PY - 2021 DO - https://doi.org/10.1080/09507116.2021.1989209 SP - 1 EP - 12 PB - Taylor & Francis Group AN - OPUS4-54022 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Thermal Cycles and Charpy Impact Toughness of Single-Pass Hybrid Laser-Arc Welded Thick-Walled Structures T2 - Lasers in Manufacturing Conference 2021 N2 - The study deals with the influence of the heat input on the thermal cycles and Charpy impact toughness for hybrid laser-arc welding of 25 mm thick structural steel S355J2 using a 20-kW high-power laser in combination with an electromagnetic weld pool support. The main focus is on the change of the mechanical properties over the entire seam thickness. The cooling times were measured using a pyrometer in combination with an optical fibre in three different locations near to fusion lines corresponding to different heights of the seam. Also, Charpy impact specimens were taken from different parts of the weld joint corresponding to the different heights. The influence of the heat input was investigated for 1.8 kJ mm-1 and 3.2 kJ mm-1. Despite the observed decreased values of both t8/5-cooling time and the Charpy impact toughness in the root part of the seam, the required values could be reached in dependance on applied heat input. T2 - Lasers in Manufacturing Conference 2021 CY - Online meeting DA - 21.06.2021 KW - laser hybrid welding KW - Charpy impact toughness KW - thick plate welding KW - thermal cycles PY - 2021 SP - 1 EP - 8 AN - OPUS4-53926 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rethmeier, Michael A1 - Gumenyuk, Andrey A1 - Bachmann, Marcel T1 - High-power laser beam welding for thick section steels – new perspectives using electromagnetic systems JF - Science and Technology of Welding and Joining N2 - In recent years, it was shown that the introduction of additional oscillating and permanent magnetic fields to laser beam and laser-arc hybrid welding can bring several beneficial effects. Examples are a contactless weld pool support for metals of high thickness suffering from severe drop-out when being welded conventionally or an enhanced stirring to improve the mixing of added filler material in the depth of the weld pool to guarantee homogeneous resulting mechanical properties of the weld. The latest research results show the applicability to various metal types over a wide range of thicknesses and welding conditions. The observations made were demonstrated in numerous experimental studies and a deep understanding of the interaction of the underlying physical mechanisms was extracted from numerical calculations. KW - Laser beam welding KW - Numerical simulations KW - Electromagnetic support PY - 2021 DO - https://doi.org/10.1080/13621718.2021.1999763 VL - 27 IS - 1 SP - 43 EP - 51 PB - Taylor & Francis Group AN - OPUS4-53970 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Brunner-Schwer, Chr. A1 - Biegler, M. A1 - Rethmeier, Michael T1 - Investigation on laser cladding of rail steel without preheating N2 - The contact between train wheels and rail tracks is known to induce material degradation in the form of wear, and rolling contact fatigue in the railhead. Rails with a pearlitic microstructure have proven to provide the best wear resistance under severe wheel-rail interaction in heavy haul applications. High speed laser cladding, a state-of-the-art surface engineering technique, is a promising solution to repair damaged railheads. However, without appropriate preheating or processing strategies, the utilized steel grades lead to martensite formation and cracking during deposition welding. In this study, laser cladding of low-alloy steel at very high speeds was investigated, without preheating the railheads. Process speeds of up to 27 m/min and laser power of 2 kW are used. The clad, heat affected zone and base material are examined for cracks and martensite formation by hardness tests and metallographic inspections. A methodology for process optimization is presented and the specimens are characterized for suitability. Within the resulting narrow HAZ, the hardness could be significantly reduced. T2 - Lasers in Manufacturing Conference 2021 CY - Erlangen, Germany DA - 21.06.2021 KW - High speed laser cladding KW - Preheatin KW - Rail tracks KW - Pearlitic microstructure PY - 2021 AN - OPUS4-53974 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Müller, V. A1 - Marko, A. A1 - Kruse, T. A1 - Biegler, M. A1 - Rethmeier, Michael T1 - Analysis and recycling of bronze grinding waste to produce maritime components using directed energy deposition N2 - Additive manufacturing promises a high potential for the maritime sector. Directed Energy Deposition (DED) in particular offers the opportunity to produce large-volume maritime components like propeller hubs or blades without the need of a costly casting process. The post processing of such components usually generates a large amount of aluminum bronze grinding waste. The aim of the presented project is to develop a sustainable circular AM process chain for maritime components by recycling aluminum bronze grinding waste to be used as raw material to manufacture ship Propellers with a laser-powder DED process. In the present paper, grinding waste is investigated using a dynamic image Analysis system and compared to commercial DED powder. To be able to compare the material quality and to verify DED process parameters, semi-academic sample geometries are manufactured. T2 - LiM 2021 CY - Munich, Germany DA - 21.06.2021 KW - Additive Manufacturing KW - Maritime Components KW - Powder Analysis KW - Recycling KW - Directed Energy Deposition PY - 2021 SP - 1 EP - 9 AN - OPUS4-54067 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Artinov, Antoni A1 - Meng, Xiangmeng A1 - Bakir, Nasim A1 - Üstündag, Ömer A1 - Bachmann, Marcel A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - The bulging effect and its relevance in high power laser beam welding JF - IOP Conference Series: Materials Science and Engineering N2 - The present work deals with the recently confirmed widening of the weld pool interface, known as a bulging effect, and its relevance in high power laser beam welding. A combined experimental and numerical approach is utilized to study the influence of the bulge on the hot cracking formation and the transport of alloying elements in the molten pool. A technique using a quartz glass, a direct-diode laser illumination, a high-speed camera, and an infrared camera is applied to visualize the weld pool geometry in the longitudinal section. The study examines the relevance of the bulging effect on both, partial and complete penetration, as well as for different sheet thicknesses ranging from 8 mm to 25 mm. The numerical analysis shows that the formation of a bulge region is highly dependent on the penetration depth and occurs more frequently during partial penetration above 6 mm and complete penetration above 8 mm penetration depth, respectively. The location of the bulge correlates strongly with the cracking location. The obtained experimental and numerical results reveal that the bulging effect increases the hot cracking susceptibility and limits the transfer of alloying elements from the top of the weld pool to the weld root. T2 - 18th Nordic Laser Materials Processing Conference (18th NOLAMP) KW - High-power laser beam welding KW - Bulge effect KW - Solidification cracking KW - Multi-physical modelling KW - Metal mixing PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-539149 DO - https://doi.org/10.1088/1757-899X/1135/1/012003 VL - 1135 IS - 012003 SP - 1 EP - 11 PB - IOP Publishing AN - OPUS4-53914 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rethmeier, Michael A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey T1 - Investigation of the gap bridgeability at high-power laser hybrid welding of plasma-cut thick mild steels with AC magnetic support N2 - One of the challenges of the high-power hybrid laser welding of thick steels is the sensitivity of the process of the process to manufacturing tolerances. This usually leads to a time-consuming preparation of the welding edges, such as milling. The study deals with the influence of the edge quality of milled and plasma-cut steel made of S355J2 with a wall thickness of 20 mm on the laser hybrid welded seam quality. Furthermore, the gap bridgeability and the tolerances towards edge misalignment was investigated. An AC magnet was used as backing support to prevent sagging and positioned under the workpiece, to generate an upwards directed electromagnetic pressure. The profiles of the edges and the gap on the top and root side were measured using a digital camera. Single-pass laser hybrid welds of plasma-cut edges could be welded using a laser beam power of just 13.7 kW. A gap bridgeability up to 2 mm and misalignment of edges up to 2 mm could be achieved successful. Additionally, the independence of the cutting side and the welding side was shown, so that samples were welded to the opposite side to their cutting. For evaluation of internal defects or irregularities, X-ray images were carried out. Charpy impact strength tests were performed to determine the toughness of the welds. T2 - X International Conference «Beam Technologies & Laser Application CY - Online meeting DA - 20.09.2021 KW - Plasma-cutting KW - Hybrid laser-arc welding KW - Thick-walled steel KW - Edge quality KW - Gap bridgeability KW - Misalignment of the edges PY - 2021 AN - OPUS4-53920 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Influence of an external applied AC magnetic field on the melt pool dynamics at high-power laser beam welding JF - IOP Conference Series: Materials Science and Engineering N2 - The study deals with the determination of the influence of an externally applied oscillating magnetic field on the melt pool dynamics in high power laser beam and hybrid laser arc welding processes. An AC magnet was positioned under the workpiece which is generating an upward directed electromagnetic force to counteract the formation of the droplets. To visualise the melt flow characteristics, several experiments were carried out using a special technique with mild steel from S355J2 with a plate thickness of up to 20 mm and a quartz glass in butt configuration. The profile of the keyhole and the melt flow were recorded with a highspeed camera from the glass side. Additionally, the influence of the magnetic field orientation to the welding direction on the filler material dilution on laser hybrid welding was studied with variating oscillation frequency. The element distribution over the whole seam thickness was measured with X-ray fluorescence (XRF). The oscillation frequency demonstrated a great influence on the melt pool dynamics and the mixing of the elements of the filler wire. The highspeed recordings showed, under the influence of the magnetic field, that the melt is affected under strong vortex at the weld root, which also avoids the formation of droplets. T2 - 18th Nordic Laser Materials Processing Conference (18th NOLAMP) KW - Laser beam welding KW - AC magnetic field KW - Melt pool dynamics KW - Filler wire mixing PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-539231 DO - https://doi.org/10.1088/1757-899X/1135/1/012017 VL - 1135 IS - 012017 SP - 1 EP - 10 PB - IOP Publishing AN - OPUS4-53923 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Investigation of the gap bridgeability at high-power laser hybrid welding of plasma-cut thick mild steels with AC magnetic support JF - IOP Journal of Physics: Conference Series N2 - One of the challenges of the high-power hybrid laser welding of thick steels is the sensitivity of the process of the process to manufacturing tolerances. This usually leads to a time-consuming preparation of the welding edges, such as milling. The study deals with the influence of the edge quality of milled and plasma-cut steel made of S355J2 with a wall thickness of 20 mm on the laser hybrid welded seam quality. Furthermore, the gap bridgeability and the tolerances towards edge misalignment was investigated. An AC magnet was used as backing support to prevent sagging and positioned under the workpiece, to generate an upwards directed electromagnetic pressure. The profiles of the edges and the gap on the top and root side were measured using a digital camera. Single-pass laser hybrid welds of plasma-cut edges could be welded using a laser beam power of just 13.7 kW. A gap bridgeability up to 2 mm and misalignment of edges up to 2 mm could be achieved successful. Additionally, the independence of the cutting side and the welding side was shown, so that samples were welded to the opposite side to their cutting. For evaluation of internal defects or irregularities, X-ray images were carried out. Charpy impact strength tests were performed to determine the toughness of the welds. T2 - X International Conference «Beam Technologies & Laser Application» KW - Laser hybrid welding KW - Magnetic bath support KW - Plasma-cut samples KW - Thick plate welding PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-539248 DO - https://doi.org/10.1088/1742-6596/2077/1/012007 VL - 2077 IS - 012007 SP - 1 EP - 8 PB - IOP Publishing AN - OPUS4-53924 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -