TY - JOUR A1 - Schröder, Jakob A1 - Evans, Alexander A1 - Polatidis, E. A1 - Čapek, J. A1 - Mohr, Gunther A1 - Serrano-Munoz, Itziar A1 - Bruno, Giovanni T1 - Understanding the impact of texture on the micromechanical anisotropy of laser powder bed fused Inconel 718 N2 - The manufacturability of metallic alloys using laser-based additive manufacturing methods such as laser powder bed fusion has substantially improved within the last decade. However, local melting and solidification cause hierarchically structured and crystallographically textured microstructures possessing large residual stress. Such microstructures are not only the origin of mechanical anisotropy but also pose metrological challenges for the diffraction-based residual stress determination. Here we demonstrate the influence of the build orientation and the texture on the microstructure and consequently the mechanical anisotropy of as-built Inconel 718. For this purpose, we manufactured specimens with [001]/[011]-, [001]- and [011]/[111]-type textures along their loading direction. In addition to changes in the Young’s moduli, the differences in the crystallographic textures result in variations of the yield and ultimate tensile strengths. With this in mind, we studied the anisotropy on the micromechanical scale by subjecting the specimens to tensile loads along the different texture directions during in situ neutron diffraction experiments. In this context, the response of multiple lattice planes up to a tensile strain of 10% displayed differences in the load partitioning and the residual strain accumulation for the specimen with [011]/[111]-type texture. However, the relative behavior of the specimens possessing an [001]/[011]- and [001]-type texture remained qualitatively similar. The consequences on the metrology of residual stress determination methods are discussed. KW - Laser powder bed fusion KW - Additive manufacturing KW - Electron backscatter diffraction KW - Tensile testing KW - Diffraction PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-555840 DO - https://doi.org/10.1007/s10853-022-07499-9 SN - 1573-4803 VL - 2022 IS - 57 SP - 15036 EP - 15058 PB - Springer Science + Business Media B.V. CY - Dordrecht AN - OPUS4-55584 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Jakob A1 - Fritsch, Tobias A1 - Ferrari, Bruno A1 - Altmann, Mika León A1 - Bruno, Giovanni A1 - Toenjes, Anastasiya T1 - Laser powder bed fusion: Defect type influences critical porosity re-growth during reheating after hot isostatic pressing N2 - Despite the remarkable product design flexibility offered by additive manufacturing (AM) techniques, such as laser powder bed fusion, AM processes are susceptible to the formation of defects. In this context, the control of process parameters and the application of post-processing treatments, such as hot isostatic pressing (HIP), are of paramount importance to achieve the desired mechanical properties. The present study investigates the effectiveness of HIP as a function of process parameters in laser powder bed fused Ti-6V-4Al (PBF-LB/Ti64) using X-ray computed tomography. The process parameters are modified to obtain reference samples with low porosity, lack of fusion defects, or keyhole porosity. In all instances, subsurface keyhole porosity was observed in the as-built parts. Moreover, it was found that the efficacy of pore closure is dependent on the specific defect type. In the case of low porosity and keyhole pores, HIP resulted in effective closure. Conversely, larger lack of fusion defects were not closed due to their interconnectivity and the entrapment of argon gas. Subsequent heat treatments above the β-transus temperature allowed the investigation of the impact of defect type on porosity re-growth. For the first time, we reveal that lack of fusion defects are affected by considerable pore re-growth during post-HIP heat treatments of PBF-LB/Ti64. Such phenomenon is driven by the increasing internal pore pressure and local creep deformation at high temperatures. In contrast, re-growth is limited in samples with low porosity or keyhole pores. KW - Additive Manufacturing KW - Hot Isostatic Pressing KW - Titanium KW - Laser Powder Bed Fusion KW - X-ray Computed Tomography KW - Heat Treatment KW - Porosity PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-629289 DO - https://doi.org/10.1016/j.jmatprotec.2025.118839 VL - 340 SP - 1 EP - 9 PB - Elsevier B.V. AN - OPUS4-62928 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Jakob A1 - Fritsch, Tobias A1 - Luzin, Vladimir A1 - Ferrari, Bruno A1 - Simón-Muzás, Juan A1 - Evans, Alexander A1 - Bruno, Giovanni T1 - Impact of scan strategy on principal stresses in laser powder bed fusion N2 - Additive manufacturing techniques, such as laser powder bed fusion (PBF-LB), are well known for their exceptional freedom in part design. However, these techniques are also characterized by the development of large thermal gradients during production and thus residual stress (RS) formation in produced parts. In this context, neutron diffraction enables the non-destructive characterization of the bulk RS distribution. By control of the thermal gradients in the powder-bed plane by scan strategy variation we study the impact of in-process scan strategy variations on the microstructure and the three-dimensional distribution of RS. Microstructural analysis by means of electron backscatter diffraction reveals sharp microstructure transitions at the interfaces ranging from 100-200 µm. The components of the RS tensor are determined by means of neutron diffraction and the principal stress directions and magnitudes are determined by eigenvalue decomposition. We find that the distribution of RS in the powder-bed plane corresponds to the underlying scan strategy. When the alternating scan vectors align with the x- and y sample coordinate axes, the principal stress directions co-align. In the present geometry, nearly transverse isotropic stress states develop when the scan vectors are either aligned 45° between x and y or continuously rotated by 67° between each layer. KW - Additive Manufacturing KW - Laser Powder Bed Fusion KW - Electron Backscatter Diffraction KW - Neutron Diffraction KW - Residual Stress KW - Principal Stress PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-607910 DO - https://doi.org/10.1016/j.matdes.2024.113171 SN - 0264-1275 VL - 244 SP - 1 EP - 10 PB - Elsevier Ltd. AN - OPUS4-60791 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Jakob A1 - Heldmann, A. A1 - Hofmann, M. A1 - Evans, Alexander A1 - Petry, W. A1 - Bruno, Giovanni T1 - Determination of diffraction and single-crystal elastic constants of laser powder bed fused Inconel 718 N2 - High energy X-ray synchrotron diffraction is used to investigate the elastic anisotropy of the nickel-based superalloy IN718 produced by laser powder bed fusion (PBF-LB). This material is characterized by a columnar grain morphology with some crystallographic texture. The material is subjected to elastic loading to determine the diffraction elastic constants (DECs). Furthermore, the single-crystal elastic constants (SCEC) are refined from these experiments using different micromechanical models. The results show that each micromechanical model predicts a specific set of SCEC that well describes the elastic anisotropy of PBF-LB/IN718. KW - Mechanical Engineering KW - Mechanics of Materials KW - Condensed Matter Physics KW - General Materials Science PY - 2023 DO - https://doi.org/10.1016/j.matlet.2023.135305 SN - 0167-577X VL - 353 SP - 1 EP - 5 PB - Elsevier B.V. AN - OPUS4-58477 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Jakob A1 - Mishurova, Tatiana A1 - Fritsch, Tobias A1 - Serrano-Munoz, Itziar A1 - Evans, Alexander A1 - Sprengel, Maximilian A1 - Klaus, M. A1 - Genzel, C. A1 - Schneider, J. A1 - Bruno, Giovanni T1 - On the influence of heat treatment on microstructure and mechanical behavior of laser powder bed fused Inconel 718 N2 - A range of heat treatments have been developed for wrought Inconel 718 to obtain desired properties. For additively manufactured Inconel 718, the recently developed standard ASTM F3301 provides guidance for heat treatment of powder bed fusion specimens. Although this standard is based on standards developed for wrought Inconel 718, it does not include direct aging. Since direct aging reduces the number of processing steps, it can result in a post processing cost reduction if the desired properties are obtained. In this study, we characterized the microstructure and tensile behavior of Inconel 718 specimens produced by a laser powder bed fusion process. The specimens were heat treated according to two different routines after stress relieving: a full heat Treatment versus a one-step direct aging process. Differences in the resulting texture and grain morphology were observed. The ex-situ stress-strain behavior was broadly similar. However, a slight increase in yield strength was observed for the direct aged specimen. In order to understand this behavior, investigations with in-situ synchrotron Energy dispersive X-ray diffraction tensile testing revealed differences in the load partitioning among different Crystal directions. Importantly, the elastic anisotropy expressed by the magnitude of the diffraction elastic constants showed a dependency on the microstructures. KW - Electron microscopy KW - X-ray analysis KW - Inconel 718 KW - Additive Manufacturing KW - Mechanical behavior KW - Diffraction elastic constants PY - 2021 DO - https://doi.org/10.1016/j.msea.2020.140555 VL - 805 SP - 40555 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-52142 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Schumacher, David A1 - Waske, Anja T1 - XCT data of metallic feedstock powder with pore size analysis N2 - X-Ray computed tomography (XCT) scan of 11 individual metallic powder particles, made of (Mn,Fe)2(P,Si) alloy. The data set consists of 4 single XCT scans which have been stitched together [3] after reconstruction. The powder material is an (Mn,Fe)2(P,Si) alloy with an average density of 6.4 g/cm³. The particle size range is about 100 - 150 µm with equivalent pore diameters up to 75 µm. The powder and the metallic alloy are described in detail in [1, 2]. KW - Additive Manufacturing KW - Feedstock powder KW - Powder Characterization KW - X-Ray Computed Tomography PY - 2022 DO - https://doi.org/10.5281/zenodo.5796487 PB - Zenodo CY - Geneva AN - OPUS4-55556 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Serrano-Munoz, Itziar T1 - Influence of microstructure and residual stress state on the fatigue behaviour of a PBF-LB/M AlSi10Mg alloy N2 - The high cooling rates (~106 K/s) occurring during Laser Powder Bed Fusion (PBF-LB/M) of AlSi10Mg induce to the formation of a fine nanometric silicon network in the as-built condition. Such unprecedented microstructure enhances the mechanical strength when compared to equivalent as-cast materials. Nevertheless, PBF-LB/M also leads to high magnitude residual stress (RS) due to the extreme localized temperature gradients. The presence of RS can be detrimental to the fatigue life of engineering components, and great efforts are focused on understanding their generation and evolution after post-process heat treatments. Typically, T6 heat treatments are used to mitigate RS and improve mechanical performances by Mg2Si precipitation during ageing at 160-180°C. Nevertheless, the solutionizing at 500-540°C vanishes the fine silicon network, leading to the formation of micrometric (average of ~2-5 µm) polygonal Si particles, similar to those observed in T6 heat-treated Al-Si cast materials. Therefore, the aim of this work is to evaluate the ability of two so-called low temperature heat treatments (i.e., at 265°C and 300°C) to mitigate RS while retaining the fine as-built microstructure inherent to PBF-LB/M AlSi10Mg. The fatigue behavior of the as-built material is subsequently compared to the two low temperature conditions. T2 - LightMat 2023 CY - Trondheim, Norway DA - 21.06.2023 KW - AlSi10Mg KW - Fatigue crack propagation KW - Residual stress KW - Post processing heat treatment PY - 2023 AN - OPUS4-57807 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Serrano-Munoz, Itziar T1 - 3D imaging and residual stress analysis for AM Materials N2 - Metal Additive Manufacturing (AM) technologies such as Laser Powder Bed Fusion (LPBF) are characterized by layer wise construction, which enable advancements of component design, leading to potential efficiency and performance improvements. However, the rapid cooling rates associated with the process consequently leads to the generation of high magnitude residual stresses (RS). Therefore, a deep understanding of the formation of RS, the influence of process parameters on their magnitude and the impact on mechanical performance is crucial for widespread application. The experimental characterization of these RS is essential for safety related engineering application and supporting the development of reliable numerical models. Diffraction-based methods for RS analysis using high energy synchrotron X-rays and neutrons enable non-destructive spatially resolved characterization of both surface and bulk residual stresses in complex components. This presentation will provide an overview of recent research conducted by the BAM at large scale facilities for the characterization of residual stresses in LPBF metallic alloys. Special focus will be given to the challenges posed by textured LPBF materials for the reliable choice of the diffraction elastic constants (DECs), which is crucial to the accurate calculation of the level of RS. T2 - Seminar at LTDS, Ecole Centrale de Lyon CY - Lyon, France DA - 15.06.2023 KW - Residual stress KW - Additive manufacturing KW - Diffraction methods PY - 2023 AN - OPUS4-57808 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Serrano-Munoz, Itziar T1 - Synchrotron x ray refraction detects microstructure and porosity evolution during in situ heat treatments in an LPBF ALSI10MG alloy N2 - The complexity of any microstructural characterization significantly increases when there is a need to evaluate the icrostructural evolution as a function of temperature. To date, this characterization is primarily performed by undertaking elaborative ex-situ experiments where the material’s heating procedure is interrupted at different temperatures or times. Moreover, these studies are often limited to a region smaller than the representative elementary volume, which can lead to partial or even biased interpretations of the collected data. This limitation can be greatly overcome by using in-situ synchrotron X-ray refraction (SXRR). T2 - ICTMS 2022 CY - Grenoble, France DA - 27.06.2022 KW - Synchrotron refraction KW - In situ heating KW - AlSi10Mg alloy KW - Additive manufacturing KW - Microstructural evolution PY - 2022 AN - OPUS4-55199 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Serrano-Munoz, Itziar T1 - Influence of the scanning strategy on the residual stress state in IN718 additive manufactured parts N2 - Laser Powder Bed Fusion (L-PBF) is an additive manufacturing technique enabling the design of complex geometries that are unrivalled by conventional production technologies. Nevertheless, L-PBF process is known to induce a high amount of residual stresses (RS) due to the high temperature gradients present during powder melting by laser. High tensile residual stresses are to be found the edges whereas the bulk material shows balancing compressive RS. Literature shows that the RS is highly sensitive to the process parameters. In particular, this study presents the characterization of the RS state in two L-PBF parts produced with a rastering scan vector that undergoes 90° or 67° rotation between subsequent layers. T2 - MLZ User Meeting 2020 CY - Online meeting DA - 08.12.2020 KW - Laser Powder Bed Fusion KW - IN718 KW - EBSD analysis KW - Residual stress state PY - 2020 AN - OPUS4-51821 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -