TY - JOUR A1 - Schaumann, P. A1 - Schürmann, K. A1 - Pittner, Andreas A1 - Rethmeier, Michael T1 - Automatically Welded Tubular X-Joints for Jacket Substructures N2 - To increase the competitiveness of jacket substructures compared to monopiles a changeover from an individual towards a serial jacket production based on automated manufactured tubular joints combined with standardized pipes has to be achieved. Therefore, this paper addresses fatigue tests of automatically welded tubular X-joints focusing on the location of the technical fatigue crack. The detected location of the technical crack is compared to numerical investigations predicting the most fatigue prone notch considering the structural stress approach as well as the notch stress approach. Besides, the welding process of the automated manufactured tubular X-joints is presented. KW - Tubular X-joints KW - Fatigue tests KW - Technical crack detection KW - Local fatigue spproaches PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-513228 DO - https://doi.org/10.1002/cepa.1140 VL - 3 IS - 3-4 SP - 823 EP - 828 PB - Ernst & Sohn Verlag für Architektur und technische Wissenschaften GmbH & Co. KG CY - Berlin AN - OPUS4-51322 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gook, S. A1 - Krieger, S. A1 - Gumenyuk, Andrey A1 - El-Batahgy, A. M. A1 - Rethmeier, Michael T1 - Notch impact toughness of laser beam welded thick sheets of cryogenic nickel alloyed steel X8Ni9 N2 - The paper deals with the investigations of the impact toughness of laser beam welded 14.5 mm thick sheets made of cryogenic steel X8Ni9 as a function of preheating. This 9% nickel alloyed steel is widely used in the liquefied natural gas (LNG) industry. An application of highly efficient welding processes such as high-power laser beam welding (LBW) in LNG sector requires an understanding of the interactions between the LBW process parameters and weld properties, in particular the impact toughness. The results show that the original fine-grained martensitic microstructure of the base metal (BM) is significantly changed by melting and crystallization during the LBW, what can lead to a decrease in the impact toughness of the weld metal (WM) below the required level. An optimal preheating temperature range leads to the favorable thermal welding cycle and is of remarkable importance for maintaining the notch impact toughness of laser beam welded joints of these thick steel sheets. A parameter window was identified in which V-notch impact toughness comparable to that of the BM at -196 °C was achieved. KW - Cryogenic steel KW - Laser beam welding KW - Preheating KW - Welding thermal cycle KW - Microstructure KW - Hardness KW - V-notch impact toughness PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-513250 DO - https://doi.org/10.1016/j.procir.2020.09.095 VL - 94 SP - 627 EP - 631 PB - Elsevier B.V. AN - OPUS4-51325 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Gook, S. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Hybrid laser-arc welding of thick-walled pipe segments with optimization of the end crater N2 - The study deals with the application of the high-power hybrid-laser arc welding process on up to 15 mm thick pipe segments with the intention to avoid end crater imperfections during closing of the circumferential welds, where the pipes were turned during welding in 1G- and 2Gpositions. Different techniques such as laser power ramp-down, abrupt switch-off of the laser power and change of the magnification of the laser spot diameter and defocusing of the laser beam relative to the workpiece were tested to remove the laser energy from the process. It could be shown that a high defocusing of the optic system above 40 mm with a resulting beam diameter > 2.9 mm in a short overlap length of approx. 20 mm leads to the formation of a cup-shaped weld seam, which is preferred for avoidance of cracks and pores in the end crater. A laser optics with motor-driven lens system was used for the welding experiments to defocuse the laser beam without changing the position of the arc. KW - Hybrid laser-arc welding KW - Circumferential weld KW - Thick-walled steel KW - Single-pass welding KW - End crater PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-513260 DO - https://doi.org/10.1016/j.procir.2020.09.106 VL - 94 SP - 676 EP - 679 PB - Elsevier B.V. AN - OPUS4-51326 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Meng, Xiangmeng A1 - Artinov, Antoni A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Numerical study of additional element transport in wire feed laser beam welding N2 - The transport phenomena in the wire feed laser beam welding are investigated numerically. A three-dimensional transient heat transfer and fluid flow model coupled with free surface tracing and element transport is developed. A ray-tracing method with local grid refinement algorithm is used to calculate the multiple reflections and Fresnel absorption on the keyhole wall. The filler material flows backward along the lateral side of the weld pool, and subsequently flows forward along the longitudinal plane. The occurrence of the bulging phenomenon may further prevent the downward transfer of the additional elements to the root of the weld pool. KW - Laser beam welding KW - Element transport KW - Filler wire KW - Numerical modelling PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-513271 DO - https://doi.org/10.1016/j.procir.2020.09.129 VL - 94 SP - 722 EP - 725 PB - Elsevier B.V. AN - OPUS4-51327 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Biegler, M. A1 - Graf, B. A1 - Rethmeier, Michael T1 - Assessing the predictive capability of numerical additive manufacturing simulations via in-situ distortion measurements on a LMD component during build-up N2 - Due to rapid, localized heating and cooling, distortions accumulate in additive manufactured laser metal deposition (LMD) components, leading to a loss of dimensional accuracy or even cracking. Numerical welding simulations allow the prediction of these deviations and their optimization before conducting experiments. To assess the viability of the simulation tool for the use in a predictive manner, comprehensive systems as well as to choose the optimal product matches, product analysis methods are needed. Indeed, most of the known methods aim to analyze a product or one product family on the physical level. Different product families, however, may differ largely in terms of the number and nature of components. This fact impedes an efficient comparison and choice of appropriate product family combinations for the production system. A new methodology is proposed to analyze existing products in view of their functional and physical architecture. The aim is to Cluster these products in new assembly oriented product families for the optimization. KW - Laser metal deposition KW - Directed Energy Deposition KW - DED KW - Welding Simulation KW - Digital Image Correlation KW - Cimensional Accuracy PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-502567 DO - https://doi.org/10.1016/j.procir.2018.08.069 VL - 74 SP - 158 EP - 162 PB - Elsevier AN - OPUS4-50256 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Improvement of Charpy impact toughness by using an AC magnet backing system for laser hybrid welding of thick S690QL steels N2 - The study deals with the influence of the heat input and the resulting cooling times on the microstructure and Charpy impact toughness of single-pass laser hybrid welded 20-mm thick high-strength steel S690QL. The main focus is on the change of the mechanical properties over the entire seam thickness. The cooling times were measured in-situ using a pyrometer and an optical fibre in three different depths of the seam where Charpy impact test specimens were also later taken. Thereby, three different heat inputs from 1.3 kJ/mm to 2 kJ/mm were investigated. Despite the observed decreased values of both t8/5-cooling time and the Charpy impact toughness in the root part of the seam, the required impact toughness of 38 J/cm2 could be reached in dependance on applied heat input, especially at the heat input of 1.6 kJ/mm. T2 - 12th CIRP conference on photonic technologies [lane 2022] CY - Fürth, Germany DA - 04.09.2022 KW - Thick-plate welding KW - Laser hybrid welding KW - Electromagnetic backing KW - Charpy impact toughness KW - Thermal cycles PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-563731 DO - https://doi.org/10.1016/j.procir.2022.08.067 VL - 111 SP - 462 EP - 465 PB - Elsevier B.V. AN - OPUS4-56373 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bakir, Nasim A1 - Üstündag, Ömer A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Influence of the weld pool geometry on solidification cracking in partial penetration high power laser beam welding N2 - Solidification cracking is still a serious problem in laser beam welding, especially in the welding of thick-walled plates. The influence of weld pool geometry on solidification cracking in partial penetration welding of thick plates is investigated within scope of this study. Therefore, a specific experimental setup of steel and quartz glass in butt configuration and on the side with high-speed camera were used to record the weld pool shape. In addition, the influence of laser inclination angle on the weld pool geometry and on solidification crack formation was investigated. The results show a bulge in the weld pool root, which is separated from an upper region by a necking region. This leads to a case where there are three different longitudinal region lengths with different solidification zones. This temporal sequence of solidification strongly promotes the formation of solidification cracks in the weld root. T2 - 12th CIRP Conference on photonic technologies (LANE 2022) CY - Fürth, Germany DA - 04.09.2022 KW - Laser beam welding KW - Partial penetration KW - Weld pool shape PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-563940 DO - https://doi.org/10.1016/j.procir.2022.08.174 VL - 111 SP - 397 EP - 400 PB - Elsevier B.V. AN - OPUS4-56394 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Investigation of the gap bridgeability at high-power laser hybrid welding of plasma-cut thick mild steels with AC magnetic support N2 - One of the challenges of the high-power hybrid laser welding of thick steels is the sensitivity of the process of the process to manufacturing tolerances. This usually leads to a time-consuming preparation of the welding edges, such as milling. The study deals with the influence of the edge quality of milled and plasma-cut steel made of S355J2 with a wall thickness of 20 mm on the laser hybrid welded seam quality. Furthermore, the gap bridgeability and the tolerances towards edge misalignment was investigated. An AC magnet was used as backing support to prevent sagging and positioned under the workpiece, to generate an upwards directed electromagnetic pressure. The profiles of the edges and the gap on the top and root side were measured using a digital camera. Single-pass laser hybrid welds of plasma-cut edges could be welded using a laser beam power of just 13.7 kW. A gap bridgeability up to 2 mm and misalignment of edges up to 2 mm could be achieved successful. Additionally, the independence of the cutting side and the welding side was shown, so that samples were welded to the opposite side to their cutting. For evaluation of internal defects or irregularities, X-ray images were carried out. Charpy impact strength tests were performed to determine the toughness of the welds. T2 - X International Conference «Beam Technologies & Laser Application» KW - Laser hybrid welding KW - Magnetic bath support KW - Plasma-cut samples KW - Thick plate welding PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-539248 DO - https://doi.org/10.1088/1742-6596/2077/1/012007 VL - 2077 IS - 012007 SP - 1 EP - 8 PB - IOP Publishing AN - OPUS4-53924 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Uhlmann, E. A1 - Düchting, J. A1 - Petrat, T. A1 - Krohmer, E. A1 - Graf, B. A1 - Rethmeier, Michael T1 - Effects on the distortion of Inconel 718 components along a hybrid laser‑based additive manufacturing process chain using laser powder bed fusion and laser metal deposition N2 - The combination of laser powder bed fusion (LPBF), known for its geometrical freedom and accuracy, and the nozzle-based laser metal deposition process (LMD), known for its high build-up rates, has great potential to reduce the additive manufacturing times for large metallic parts. For the industrial application of the LPBF-LMD hybrid process chain, it is necessary to investigate the infuence of the LMD process on the LPBF substrate. In addition, the build plate material also has a signifcant impact on the occurrence of distortion along the additive manufacturing process chain. In the literature, steel build plates are often used in laser-based additive manufacturing processes of Inconel 718, since a good metallurgical Bonding can be assured whilst reducing costs in the production and restoration of the build plates. This paper examines the distortion caused by LMD material deposition and the infuence of the build plate material along the hybrid additive manufacturing process chain. Twin cantilevers are manufactured by LPBF and an additional layer is subsequently deposited with LMD. The distortion is measured in the as-built condition as well as after heat treatment. The efect of diferent LMD hatch strategies on the distortion is determined. The experiments are conducted using the nickel-base alloy Inconel 718. The results show a signifcant infuence of LMD path strategies on distortion, with shorter tool paths leading to less distortion. The remaining distortion after heat treatment is considerably dependent on the material of the build plate. KW - Laser powder bed fusion KW - Directed energy deposition KW - Laser metal deposition KW - Distortion KW - Heat treatment PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-521439 DO - https://doi.org/10.1007/s40964-021-00171-9 SP - 1 EP - 10 PB - Springer-Verlag GmbH CY - Heidelberg AN - OPUS4-52143 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ö. A1 - Fritzsche, André A1 - Avilov, V. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Study of gap and misalignment tolerances at hybrid laser arc welding of thick-walled steel with electromagnetic weld pool support system N2 - The hybrid laser arc welding (HLAW) process provides many advantages such as improved gap bridgeability, deep penetration and misalignment of edges, that is why the process is used increasingly in industrial applications e.g. shipbuilding, power plant industry and line-pipe manufacturing. The obvious encountered problem for single pass welding in flat position is the gravity drop-out at low welding velocities. With the usage of an electromagnetic weld pool support system, which is based on generating Lorentz forces within the weld pool, wide seams followed by reduced welding velocities could be achieved in this study leading to the realization of a gap bridgeability up to 1 mm, misalignment of edges up to 2 mm and a single pass weld up to 28 mm thickness with a 20-kW fibre laser. These developments expand the boundaries of the HLAW process for different industrial applications. As a result, less accurate preparation of the edges would be sufficient, which saves time for manufacturing. KW - Hybrid laser-arc welding KW - Electromagnetic weld pool support system KW - Thick-walled steel KW - Gap bridgeability KW - Single pass welding KW - Misalignment of edges PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-468263 DO - https://doi.org/10.1016/j.procir.2018.08.016 SN - 2212-8271 VL - 74 SP - 757 EP - 760 PB - Elsevier AN - OPUS4-46826 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Üstündag, Ö. A1 - Avilov, V. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Full penetration hybrid laser arc welding of up to 28 mm thick S355 plates using electromagnetic weld pool support N2 - The laser hybrid welding process offers many advantages regarding deep penetration, increased welding velocity and with the help of the supplied filler wire an improved bridgeability to gap and misalignment tolerances. High power laser systems with a power of approx. 30 kW are already available on the market. Nevertheless, multi-layer technology with an arc process is still used for welding of plates from a thickness from 20 mm. A potential cause is the process instability with increasing laser power. It is inevitable that gravity drop-out due to the high hydrostatic pressure at increasing wall thickness especially at welding in flat position and with a low welding speed. The surface tension decreases with increasing root width resulting from low welding velocities. To prevent such inadmissible defects of the seam a use of weld pool support is required. Usual weld pool support systems such as ceramic or powder supports require a mechanical detachment which is time-consuming. The electromagnetic weld pool support system described in this work shows an alternative weld pool support which works contactless. It is based on generating Lorentz forces in the weld pool due to oscillating magnetic field and induced eddy currents. This innovative technology offers single pass welds up to 28 mm in flat position and reduced welding velocity with a laser power of just 19 kW. It also leads to improved mechanical-technological properties of the seams because of the slow cooling rate. With usage of an electromagnetic weld pool support the limitation of the hybrid laser arc welding process in the thick sheet metal will be extend. KW - Electromagnetic weld pool support KW - Hybrid laser arc welding KW - Thick-walled steel KW - Single pass welding PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-468276 DO - https://doi.org/10.1088/1742-6596/1109/1/012015 SN - 1742-6596 VL - 1109 SP - 1 EP - 7 PB - IOP Publ. AN - OPUS4-46827 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Petrat, T. A1 - Kersting, R. A1 - Graf, B. A1 - Rethmeier, Michael T1 - Embedding electronics into additive manufactured components using laser metal deposition and selective laser melting N2 - The paper deals with the integration of a light emitting diode (LED) into an additive manufactured metal component. Selective laser melting (SLM) and laser metal deposition (LMD) are used. The material used is the chrome-nickel steel 316L. The basic component is manufactured by means of SLM and consists of a solid body and an area with grid structure. The solid body includes a duct in the shape of a groove with a recess for the positioning of the power cable. The LED is embedded in the grid structure via an inlet from the solid body. In further processing, the groove is filled with LMD. Two strategies with different parameter combinations were investigated. It shows that a high energy input near the power cable leads to its destruction. By using multiple parameter combinations during the manufacturing process, this destruction can be prevented. There was a comparison of both strategies with regard to the necessary number of tracks and duration of welding time. KW - Additive manufacturing KW - Condition monitoring KW - Process chain KW - Laser-metal-deposition KW - Selektive-laser-melting KW - Embedded electronics PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-479469 DO - https://doi.org/10.1016/j.procir.2018.08.071 SP - 168 EP - 171 PB - Elsevier Ltd. AN - OPUS4-47946 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bakir, Nasim A1 - Pavlov, V. A1 - Zavjalov, S. A1 - Volvenko, S. A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Novel metrology to determine the critical strain conditions required for solidification cracking during laser welding of thin sheets N2 - This paper represents the results for proposed optical flow method based on the Lucas-Kanade (LK) algorithm applied to two different problems. The following observations can be made: - The estimated strain and displacement for conducted tensile test are generally very close to those measured with conventional DIC-technique. - The LK technique allows measurement of strain or displacement without special selection of a region of interest. Using a novel optical measurement technique together with the optical flow algorithm, a twodimensional deformation analysis during welding was conducted. This technique is the first to provide a measurement of the full strain field locally in the immediate vicinity of the solidification front. Additionally, the described procedure of the optical measurement allows the real material-dependent values of critical strain characterizing the transition to hot cracking during laser welding processes to be determined. T2 - Beam Technologies and Laser Application CY - Sankt Petersburg, Russia KW - Hot cracking test KW - Local critical strain KW - Solidification cracking KW - Laser beam welding KW - Novel metrology PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-467226 DO - https://doi.org/10.1088/1742-6596/1109/1/012047 SN - 1742-6596 VL - 1109 IS - 012047 SP - 1 EP - 9 PB - IOP Publ. CY - Bristol AN - OPUS4-46722 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Straße, Anne A1 - Bakir, Nasim A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael ED - Schmidt, M. ED - Vollertsen, F. ED - Schmidt, B. M. T1 - Preliminary study to investigate the applicability of optical strain measurement technique for the detection of hot cracks in laser metal deposited layers N2 - Laser metal deposition (LMD) as an additive manufacturing technique became increasingly important in recent years and thus the demand for component safety. This is the reason, for the need for reliable in-situ defect detection techniques. For laser beam weld seams an optical measurement technique based on an optical flow algorithm was successfully used to define the critical straining conditions that lead to hot cracking. This algorithm was adapted for bead-on-plate weld seams on LMD deposited layers of IN718 alloy while performing external strain on the specimen in an externally loaded hot cacking test facility. The resulting transversal hot cracks along the weld seam were localized via X-Ray inspection and the type of cracking confirmed by Scanning Electron Microscopy (SEM). The strain distribution was measured in the vicinity of the solidification front and correlated to the detected hot cracks. Based on the results this technique could be adopted for LMD experiments. T2 - 12th CIRP Conference on Photonic Technologies [LANE 2022] CY - Fürth, Germany DA - 04.09.2022 KW - Laser Metal Deposition (LMD) KW - Strain measurement KW - Optical flow KW - Critical strain PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-556445 DO - https://doi.org/10.1016/j.procir.2022.08.034 VL - 111 SP - 335 EP - 339 PB - Elsevier B.V. CY - Amsterdam AN - OPUS4-55644 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -