TY - JOUR A1 - Mundra, Shishir A1 - Provis, J. L. T1 - Mechanisms of passivation and chloride-induced corrosion of mild steel in sulfide-containing alkaline solutions N2 - The pore fluid within many concretes is highly alkaline and rich in reduced sulfur species, but the influence of such alkaline-sulfide solutions on the surface film formed on steel reinforcement is poorly understood. This study investigates the critical role of HS− in defining mild steel passivation chemistry. The surface film formed on the steel in alkaline-sulfide solutions contains Fe(OH)2 and Fe–S complexes, and the critical chloride concentration to induce corrosion increases at high sulfide concentration. However, this behavior is dependent on the duration of exposure of the steel to the electrolyte, and the nature of the sulfidic surface layer. KW - Alkali-activated materials KW - Steel corrosion KW - Sulfide KW - Chloride PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-528861 DO - https://doi.org/10.1007/s10853-021-06237-x VL - 56 IS - 26 SP - 14783 EP - 14802 PB - Springer Nature AN - OPUS4-52886 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Durlo Tambara, Luís Urbano A1 - Nikoonasab, Ali A1 - Radtke, Martin A1 - de Oliveira Guilherme Buzanich, Ana A1 - Gluth, Gregor T1 - Determination of the oxidation depths of ground granulated blast furnace slag-containing cement pastes using Mn K-edge X-ray absorption near-edge structure spectroscopy N2 - The redox potential of the pore solution of hardened cements containing ground granulated blast furnace slag (GGBFS) affects reinforcement corrosion and immobilization of radioactive waste. Here, Mn K-edge X-ray absorption near-edge structure (XANES) spectroscopy was applied to determine the depth profile of the oxidation state of manganese in hardened GGBFS-containing cement pastes. Manganese was oxidized in the outer regions of some of the pastes, but the depth to which this occurred was not identical with the ‘blue-green/white color change front’, usually interpreted as indicating oxidation of sulfur species. For CEM III/B, the color change of the material was gradual and thus unsuitable for a precise determination of the oxidation depth, while for the alkali-activated slag, a distinct color change front was found, but full oxidation of manganese and sulfur had not occurred in the brighter region. Mn K-edge XANES spectroscopy is thus a more reliable method than the determination of the visual color change front to follow the ingress of the oxidation front. KW - Manganese KW - Oxidation KW - Sulfide KW - Alkali-activated materials KW - Redox conditions PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-651469 DO - https://doi.org/10.1111/jace.70445 SN - 0002-7820 SN - 1551-2916 VL - 109 IS - 1 SP - 1 EP - 11 PB - Wiley CY - Oxford AN - OPUS4-65146 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -