TY - JOUR A1 - Theiler, Geraldine A1 - Cano Murillo, Natalia A1 - Hausberger, Andreas T1 - Effect of hydrogen pressure on the fretting behavior of rubber materials N2 - Safety and reliability are the major challenges to face for the development and acceptance of hydrogen technology. It is therefore crucial to deeply study material compatibility, in particular for tribological components that are directly in contact with hydrogen. Some of the most critical parts are sealing materials that need increased safety requirements. In this study, the fretting behavior of several elastomer materials were evaluated against 316L stainless steel in an air and hydrogen environment up to 10 MPa. Several grades of cross-linked hydrogenated acrylonitrile butadiene (HNBR), acrylonitrile butadiene (NBR) and ethylene propylene diene monomer rubbers (EPDM) were investigated. Furthermore, aging experiments were conducted for 7 days under static contions in 100 MPa of hydrogen followed by rapid gas decompression. Fretting tests revealed that the wear of these compounds is significantly affected by the hydrogen environment compared to air, especially with NBR grades. After the aging experiment, the friction response of the HBNR grades is characterized by increased adhesion due to elastic deformation, leading to partial slip. KW - Fretting wear KW - Rubbers KW - Hydrogen KW - High-pressure PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-608462 DO - https://doi.org/10.3390/lubricants12070233 VL - 12 IS - 7 SP - 1 EP - 17 PB - MDPI AN - OPUS4-60846 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jentzsch, Stefan A1 - Stock, Daniel A1 - Häcker, Ralf A1 - Skrotzki, Birgit A1 - Darvishi Kamachali, Reza A1 - Klingbeil, Dietmar A1 - Kindrachuk, Vitaliy T1 - Shear Band Formation with Split Hopkinson Bar Experiments N2 - The essence of dynamic failure is closely linked to dramatic shear deformations which often lead to the formation of adiabatic shear bands (ASB). Under high loading velocities and the subsequent rapid temperature increase, the localization of shear strain is crucial in view of safety issues of systems in mechanical and aircraft engineering, especially with respect to fast rotating components and diverse crash scenarios. In this research, we perform high speed impact tests at the split Hopkinson pressure bar (SHPB) setup and use particular hat-shaped specimen geometries that resemble the stresses and failure conditions at the component level. In the first step, we specify a notched specimen geometry using finite element (FE) simulations to ensure pure shear. Further, quasi-static compressive tests and a series of impact tests at high strain rates of 10^3-10^4 s^-1 are conducted on specimens manufactured from a fine-grain structural steel with the properties of S355. Optical microscopy and electron backscatter diffraction (EBSD) of the sheared zones unveil significant localization to maximal shear strains of about 0.9 accompanied by grain refinement by factors 5 to 14. The displacements across the surface of the specimens are captured with subset-based local digital image correlation (DIC) during the impact time, and serve as an objective to validate a viscoplastic constitutive relationship. More precisely, the deformation distribution is accurately reproduced by the widely recognized Johnson-Cook (JC) model, which features an enhanced description of damage evolution. Thus, combining experimental and characterization techniques, continuum mechanics and reasonable optimization strategies for the identification of model parameters provides an efficient approach for comprehensive insights into the strain localization behaviour and its impact on the mechanical performance of S355 under extreme strain rates and deformations. KW - Adiabatic shear bands KW - Finite element analysis KW - Viscoplastic material modelling KW - Split Hopkinson pressure bar KW - Hat-shaped specimen KW - Johnson–Cook parameter identification PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-613339 DO - https://doi.org/10.1016/j.ijmecsci.2024.109749 VL - 284 SP - 1 EP - 14 PB - Elsevier BV AN - OPUS4-61333 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bhadeliya, Ashok A1 - Rehmer, Birgit A1 - Fedelich, Bernard A1 - Jokisch, T. A1 - Skrotzki, Birgit A1 - Olbricht, Jürgen T1 - Fatigue and fracture in dual-material specimens of nickel-based alloys fabricated by hybrid additive manufacturing N2 - The integration of additive manufacturing with traditional processes, termed hybrid additive manufacturing, has expanded its application domain, particularly in the repair of gas turbine blade tips. However, process-related defects in additively manufactured materials, interface formation, and material property mismatches in dual-material structures can significantly impact the fatigue performance of components. This investigation examines the low cycle fatigue and fatigue crack growth behaviors in dual-material specimens of nickel-based alloys, specifically the additively manufactured STAL15 and the cast alloy 247DS, at elevated temperatures. Low cycle fatigue experiments were conducted at temperatures of 950 °C and 1000 °C under a range of strain levels (0.3%–0.8%) and fatigue crack growth tests were conducted at 950 °C with stress ratios of 0.1 and −1. Fractographic and microscopic analyses were performed to comprehend fatigue crack initiation and crack growth mechanisms in the dual-material structure. The results consistently indicated crack initiation and fatigue fracture in the additively manufactured STAL15 material. Notably, fatigue crack growth retardation was observed near the interface when the crack extended from the additively manufactured STAL15 material to the perpendicularly positioned interface. This study highlights the importance of considering yield strength mismatch, as well as the potential effects of residual stresses and grain structure differences, in the interpretation of fatigue crack growth behavior at the interface. KW - Hybrid additive manufacturing KW - Dual-material nickel-based alloys KW - High-temperature fatigue crack growth KW - Low cycle fatigue PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-609340 DO - https://doi.org/10.1016/j.jmrt.2024.08.211 SN - 2238-7854 VL - 32 SP - 3737 EP - 3749 PB - Elsevier B.V. AN - OPUS4-60934 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sonntag, Nadja A1 - Piesker, Benjamin A1 - Ávila Calderón, Luis A1 - Mohr, Gunther A1 - Rehmer, Birgit A1 - Agudo Jácome, Leonardo A1 - Hilgenberg, Kai A1 - Evans, Alexander A1 - Skrotzki, Birgit T1 - Tensile and Low‐Cycle Fatigue Behavior of Laser Powder Bed Fused Inconel 718 at Room and High Temperature N2 - This study investigates the room‐ and high‐temperature (650 °C) tensile and low‐cycle‐fatigue behavior of Inconel 718 produced by laser powder bed fusion (PBF‐LB/M) with a four‐step heat treatment and compares the results to the conventional wrought material. The microstructure after heat treatment is characterized on different length scales. Compared to the wrought variant, the elastic and yield properties are comparable at both test temperatures while tensile strength, ductility, and strain hardening capacity are lower. The fatigue life of the PBF‐LB/M variant at room temperature is slightly lower than that of the wrought material, while at 650 °C, it is vice versa. The cyclic stress response for both material variants is characterized by cyclic softening, which is more pronounced at the higher test temperature. High strain amplitudes (≥0.7%) at room temperature and especially a high testing temperature result in the formation of multiple secondary cracks at the transitions of regions comprising predominantly elongated grain morphology and columns of stacked grains with ripple patterns in the PBF‐LB/M material. This observation and pronounced crack branching and deflection indicate that the cracks are controlled by sharp micromechanical gradients and local crystallite clusters. KW - Additive manufacturing KW - Fatigue damage KW - Heat treatment KW - Inconel 718 KW - Laser powder bed fusion KW - Low-cycle fatigue KW - Tensile strength PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-599316 DO - https://doi.org/10.1002/adem.202302122 SN - 1527-2648 SP - 1 EP - 17 PB - Wiley AN - OPUS4-59931 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Campari, Alessandro A1 - Konert, Florian A1 - Sobol, Oded A1 - Alvaro, Antonio T1 - A comparison of vintage and modern X65 pipeline steel using hollow specimen technique for in-situ hydrogen testing N2 - The transition toward a hydrogen-based economy requires a widespread transport and distribution network, and repurposed natural gas pipelines are a viable option. An assessment of the hydrogen-induced degradation of pipeline steels is needed to inject H2 gas into the existing infrastructure safely. The conservative and standardized method consists of in-situ tensile tests in an autoclave filled with high-pressure hydrogen gas. A proposed alternative method involves using a hollow specimen as containment volume and applying the gas pressure in the inner cavity. This technique has lower costs and shorter test preparation time but is not standardized yet. This study aims to evaluate and compare the tensile properties of API 5L X65 pipeline steel in two states: vintage and modern. The influence of the surface roughness is investigated through parallel tests with drilled and reamed specimens. Hydrogen tests are compared with reference tests in an inert environment. A significant hydrogen-induced decrease in tensile properties is observed, and no significant difference between vintage and modern X65 can be drawn. The reduction in tensile properties is more significant in specimens with higher inner surface roughness. The evaluation of surface conditions appears crucial when assessing the HE susceptibility of hydrogen transport and storage equipment. KW - Hydrogen embrittlement KW - Hollow specimen technique KW - Pipeline steel KW - SSRT PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-603013 DO - https://doi.org/10.1016/j.engfailanal.2024.108530 VL - 163 SP - 1 EP - 15 PB - Elsevier Ltd. AN - OPUS4-60301 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Grimault de Freitas, Tomás A1 - Konert, Florian A1 - Nietzke, Jonathan A1 - Krzysch, Zephanja A1 - Böllinghaus, Thomas A1 - Michler, Thorsten A1 - Wackermann, Ken A1 - Oesterlin, Heiner A1 - Tlili, Mohamed A1 - Ruchti, Peter A1 - Beitelschmidt, Denise A1 - Elsen-Humberg, Stephan A1 - Koenigs, Timo A1 - Systermans, Thomas A1 - Sobol, Oded T1 - Tensile testing in high-pressure gaseous hydrogen using the hollow specimen method N2 - Metallic materials, predominantly steels, are the most common structural materials in the various components along the hydrogen supply chain. Ensuring their sustainable and safe use in hydrogen technologies is a key factor in the ramp-up of the hydrogen economy. This requires extensive materials qualification, however, most of the accepted; and standardized test methods for determining the influence of gaseous hydrogen on metallic materials describe complex and costly procedures that are only available to a very limited extent worldwide. The hollow specimen technique is a simple, rapid, and economical method designed to overcome the limitations of the current methods for the qualification of metallic materials under high-pressure hydrogen gas. However, this technique is not yet standardized. The TransHyDE-H2Hohlzug project is presented in this article, along with the main steps required to optimize the hollow specimen technique. This includes closing knowledge gaps related to the specimen geometry, surface quality, and gas purity in dedicated working packages, thus contributing to a comprehensive standardization of the technique for tests in high-pressure hydrogen gas. KW - High-pressure Gaseous Hydrogen KW - Hydrogen Embrittlement KW - Tensile Testing KW - Hollow Specimen Technique PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-610557 DO - https://doi.org/10.1557/s43577-024-00776-9 VL - 49 SP - 1 EP - 9 PB - Springer Nature AN - OPUS4-61055 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Konert, Florian A1 - Campari, Alessandro A1 - Nietzke, Jonathan A1 - Sobol, Oded A1 - Paltrinieri, Nicola A1 - Alvaro, Antonio T1 - Evaluation of the tensile properties of X65 pipeline steel in compressed gaseous hydrogen using hollow specimens N2 - Hydrogen has great potential on the path towards decarbonization of the energy and transport sectors and can mitigate the urgent issue of global warming. It can be sustainably produced through water electrolysis with potentially zero emissions, and efficiently used (e.g., in fuel cell systems). Despite its environmental advantages, hydrogen-metal interactions could result in the degradation of the mechanical properties of several structural materials. In order to determine the magnitude of the material degradation in relation to hydrogen exposure, extensive material testing is required. The standardized procedure for in-situ testing for the quantification of the impact of compressed gaseous hydrogen (CGH2) relies on the utilization of an autoclave around the tested specimen. Such test set-up is complex, expensive, time-consuming and requires special equipment, trained personnel, and strict safety procedures. A relatively recent method to circumvent these issues and provide affordable results consists of using hollow specimens, thus applying the hydrogen pressure inside rather than outside the specimen. It allows to reduce the volume of hydrogen by several orders of magnitude and to perform the tests more efficiently and in a safer manner. This study focuses on evaluating the tensile properties of X65 vintage pipeline steel tested in a high-pressure hydrogen environment using hollow specimens. Tests are performed in 6 MPa H2 and Ar at the nominal strain rate of 10−6 s−1 to evaluate the reduced area at fracture and the elongation loss. The effect of surface finishing on crack initiation and propagation is investigated by comparing two different manufacturing techniques. In this way, this study provides insights into the applicability of a novel, reliable, and safe testing method which can be used to assess the hydrogen-assisted ductility loss in metallic materials. KW - Mechanical Engineering KW - Hydrogen Embrittlement KW - SSRT KW - Hollow specimen KW - Pipeline steel KW - In-situ tensile test PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-595887 DO - https://doi.org/10.1016/j.prostr.2024.01.074 SN - 2452-3216 VL - 54 SP - 1 EP - 8 PB - Elsevier B.V. AN - OPUS4-59588 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Konert, Florian A1 - Wieder, Frank A1 - Nietzke, Jonathan A1 - Meinel, Dietmar A1 - Böllinghaus, Thomas A1 - Sobol, Oded T1 - Evaluation of the impact of gaseous hydrogen on pipeline steels utilizing hollow specimen technique and μCT N2 - The high potential of hydrogen as a key factor on the pathway towards a climate neutral economy, leads to rising demand in technical applications, where gaseous hydrogen is used. For several metals, hydrogen-metal interactions could cause a degradation of the material properties. This is especially valid for low carbon and highstrength structural steels, as they are commonly used in natural gas pipelines and analyzed in this work. This work provides an insight to the impact of hydrogen on the mechanical properties of an API 5L X65 pipeline steel tested in 60 bar gaseous hydrogen atmosphere. The analyses were performed using the hollow specimen technique with slow strain rate testing (SSRT). The nature of the crack was visualized thereafter utilizing μCT imaging of the sample pressurized with gaseous hydrogen in comparison to one tested in an inert atmosphere. The combination of the results from non-conventional mechanical testing procedures and nondestructive imaging techniques has shown unambiguously how the exposure to hydrogen under realistic service pressure influences the mechanical properties of the material and the appearance of failure. KW - Energy Engineering and Power Technology KW - Condensed Matter Physics KW - Fuel Technology KW - Renewable Energy, Sustainability and the Environment KW - µCT KW - Hollow Specimen Technique KW - Hydrogen Embrittlement PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-595077 DO - https://doi.org/10.1016/j.ijhydene.2024.02.005 SN - 0360-3199 VL - 59 SP - 874 EP - 879 PB - Elsevier B.V. AN - OPUS4-59507 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Böllinghaus, Thomas A1 - Cross, Carl T1 - Obituary: Prof. Dr.-Ing. Hans Hoffmeister N2 - On November 3, 2023, our dear colleague, Prof. Dr.-Ing. Hans Hoffmeister, born in 1932 in Kassel, Germany, passed away in Ahrensburg, near Hamburg, Germany. KW - Metals and Alloys KW - Mechanical Engineering KW - Mechanics of Materials PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-594160 DO - https://doi.org/10.1007/s40194-023-01675-4 SP - 1 EP - 2 PB - Springer Science and Business Media LLC AN - OPUS4-59416 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Strauß, Lea A1 - Duarte, Larissa A1 - Kruse, Julius A1 - Madia, Mauro A1 - Löwisch, Günther T1 - An equivalent stress approach for predicting fatigue behavior of additively manufactured AlSi10Mg N2 - Laser-based powder bed fusion (PBF-LB) is an advanced additive manufacturing technique renowned for its precision and capability to fabricate complex metal components. However, the high thermal gradients and rapid cooling rates intrinsic to this process introduce significant process-induced effects, such as inhomogeneities, surface roughness, anisotropy, and residual stress, all of which critically influence the fatigue behavior of the produced parts. This study investigates the fatigue performance of AlSi10Mg samples produced by PBF-LB, examining the impact of varying surface conditions, geometries, and residual stress levels. Fatigue-life prediction models are formulated based on nominal stress amplitude, residual stress, form factor, crack-initiating inhomogeneity, and surface roughness, with smooth samples serving as a baseline reference. The study presents two empirical models for predicting fatigue life and fatigue strength using S–N curves and the Kitagawa–Takahashi diagram with the El Haddad approach, derived from comprehensive experimental data, including finite element modeling, fatigue-life measurements, surface roughness evaluations, and residual stress analysis. KW - AlSi10Mg KW - Kitagawa–Takahashi diagram KW - El Haddad KW - Equivalent stress KW - Fatigue-life prediction KW - PBF-LB/M PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-625176 DO - https://doi.org/10.1007/s40964-025-00974-0 SP - 1 EP - 16 PB - Springer Science and Business Media LLC AN - OPUS4-62517 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Poka, Konstantin A1 - Ali, Sozol A1 - Saeed, Waleed A1 - Merz, Benjamin A1 - Epperlein, Martin A1 - Hilgenberg, Kai T1 - Quality assurance via a cyber physical system of a PBF-LB/M machine N2 - Powder Bed Fusion with Laser Beam of Metals (PBF-LB/M) faces challenges in reproducibility and quality assurance, even for widely applied alloys like AlSi10Mg. This work introduces a digital provenance framework for PBF-LB/M, showcased through the EOS M 300–4 multi-laser machine. An Extract, Transform, Load (ETL) pipeline autonomously captures machine data, including scan vectors as well as process signals, and organizes them into a Digital Shadow (DS). The DS is further extended by external data sources, such as Melt Pool Monitoring (MPM), to enable comprehensive analysis and root cause identification. This approach ensures continuous data representation and facilitates the development of new quality metrics. Moreover, the framework enhances quality assurance and traceability, supports compliance with industry standards, and improves productivity. It also enables more precise cost calculations and predictive maintenance. By addressing these challenges, the framework is essential for advancing PBF-LB/M in industrial applications, achieving greater consistency and scalability in production. KW - PBF-LB/M KW - Data driven quality assurance KW - Data engineering KW - Digital shadow PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-625187 DO - https://doi.org/10.1007/s40964-025-00978-w SN - 2363-9520 VL - 10 IS - 3 SP - 1771 EP - 1783 PB - Springer Science and Business Media LLC AN - OPUS4-62518 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zhu, Jiangchao A1 - Madia, Mauro A1 - Schurig, Michael A1 - Kruse, Julius A1 - Conrad, Fabian A1 - Schlums, Hartmut A1 - Kontermann, Christian A1 - Zerbst, Uwe T1 - On the use of representative specimens for the structural integrity assessment of safety-relevant rotating components N2 - Safety-relevant components, for which a failure in service could have catastrophic consequences, are usually designed for extremely low probability of failure and they are subjected to stringent part qualification procedures according to guidelines set by regulatory agencies. Manufacturers are often forced to perform tests on full scale or scaled components to ensure the structural integrity under defined loading conditions, which usually implies a huge experimental and financial effort. Therefore, companies try to develop new strategies such as digital twins, which allow to massively reduce costs, without compromising safety. This work presents a new quasi-static testing and assessment concept, the main idea of which is to replace, or at least reduce, the experimental testing on components by testing specimens representative of the component. Fracture mechanics specimens have been designed iteratively by numerical simulations to match the stress state at the crack-tip of the maximum permissible defect defined by regulatory agencies for the component. Potentially, the major benefit of the proposed approach is that the tests can be performed on conventional laboratory testing machines. The effectiveness of the methodology is demonstrated in case of the structural integrity assessment of a Ni-base superalloy aero-engine turbine disk at overspeed conditions. KW - Structural integrity KW - Turbine disk KW - Burst KW - Fracture mechanics KW - Representative specimens KW - Quasi-static testing PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-624208 DO - https://doi.org/10.1016/j.engfracmech.2024.110710 SN - 0013-7944 VL - 314 SP - 1 EP - 23 PB - Elsevier Ltd. AN - OPUS4-62420 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Erxleben, Kjell A1 - Kaiser, Sebastian A1 - Rhode, Michael A1 - Kannengiesser, Thomas A1 - Kromm, Arne T1 - In-service and repair welding of pressurized hydrogen pipelines–a review on current challenges and strategies N2 - Hydrogen is the energy carrier for a sustainable future without fossil fuels. As this requires a reliable transportation infrastructure, the conversion of existing natural gas (NG) grids is an essential part of the worldwide individual national hydrogen strategies, in addition to newly erected pipelines. In view of the known effect of hydrogen embrittlement, the compatibility of the materials already in use (typically low-alloy steels in a wide range of strengths and thicknesses) must be investigated. Initial comprehensive studies on the hydrogen compatibility of pipeline materials indicate that these materials can be used to a certain extent. Nevertheless, the material compatibility for hydrogen service is currently of great importance. However, pipelines require frequent maintenance and repair work. In some cases, it is necessary to carry out welding work on pipelines while they are under pressure, e.g., the well-known tapping of NG grids. This in-service welding brings additional challenges for hydrogen operations in terms of additional hydrogen absorption during welding and material compatibility. The challenge can be roughly divided into two parts: (1) the possible austenitization of the inner piping material exposed to hydrogen, which can lead to additional hydrogen absorption, and (2) the welding itself causes an increased temperature range. Both lead to a significantly increased hydrogen solubility in the respective materials compared to room temperature. In that connection, the knowledge on hot tapping on hydrogen pipelines is rare so far due to the missing service experiences. Fundamental experimental investigations are required to investigate the possible transferability of the state-of-the-art concepts from NG to hydrogen pipeline grids. This is necessary to ensure that no critical material degradation occurs due to the potentially increased hydrogen uptake. For this reason, the paper introduces the state of the art in pipeline hot tapping, encompassing current research projects and their individual solution strategies for the problems that may arise for future hydrogen service. Methods of material testing, their limitations, and possible solutions will be presented and discussed. KW - In-service KW - Welding KW - Hydrogen pipeline KW - Review PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-638847 DO - https://doi.org/10.1007/s40194-025-02127-x SN - 0043-2288 SP - 1 EP - 24 PB - Springer Science and Business Media LLC AN - OPUS4-63884 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Liepold, Philipp A1 - Kromm, Arne A1 - Kannengießer, Thomas T1 - A Force Based Determination of Hot Cracking Susceptibility N2 - Two high-strength, low-alloy Gas Metal Arc Welding (GMAW) wires were evaluated for their susceptibility to Solidification Cracking (SC) using a modified version of the Transverse Motion Weldability (TMW) test. In theoriginal TMW test, the Transverse Displacement Speed (TDS) is varied iteratively, and crack lengths are measured in each iteration. The modified version eliminates the need for multiple runs by continuously reducing the TDS over a single run. Rather than emphasizing crack lengths, this method assesses the reaction force to the TDS, thereby determining a Critical TDS (CTDS). This critical point directly correlates with the cessation of SC growth. CTDS values were measured under a range of welding parameters, thereby demonstrating the influence of Welding speed and arc energy (U × I/welding speed) on SC susceptibility for the tested filler metals. The CTDS data obtained from this testing method have the potential to provide valuable insights for practical applications in the field. KW - Force based KW - Neural Network KW - TRS PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-640140 DO - https://doi.org/10.5781/JWJ.2025.43.4.10 SN - 2466-2100 VL - 43 IS - 4 SP - 447 EP - 457 AN - OPUS4-64014 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Numerical studies of process porosity suppression by magnetohydrodynamic technology during the laser beam welding of aluminum alloy N2 - Magnetohydrodynamic (MHD) technology is acknowledged as a promising method for mitigating the porosity defects in laser-welded joints of aluminum alloys. A transient 3D multi-physical numerical model of laser beam welding (LBW), coupled with the MHD and oscillating metal vapor plume model, is developed to study the suppression mechanisms of process porosity by an external magnetic field. The experimental results demonstrate that the porosity ratio is reduced by 93.5 % as the oscillating magnetic field is applied. This significant reduction confirms the effectiveness of the MHD technology in suppressing porosity defects. A downward time-averaged Lorentz force is induced in the weld pool, which affects the fluid flow pattern and the weld pool profile. The change of the flowing pattern in the weld pool by the magnetic field does not always have a positive effect on the porosity suppression. In addition, an analytical model shows that the bubble escape window is expanded by 62 % under the effect of the oscillating magnetic field. The additional upward velocity provided by the electromagnetic expulsive force on the bubbles and the change of weld pool profile are considered favorable factors in eliminating the porosity defects. The numerical and analytical model developed for analyzing the bubble escape window have been validated by experimental results. KW - Laser beam welding KW - Aluminum alloy KW - Process porosity defects KW - Magnetohydrodynamic technology KW - Bubble escape KW - Numerical simulation PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-637642 DO - https://doi.org/10.1016/j.ijheatmasstransfer.2025.127525 SN - 0017-9310 VL - 253 SP - 1 EP - 13 PB - Elsevier Ltd. AN - OPUS4-63764 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yang, Keke A1 - Wang, Zhuoqun A1 - Haak, Viktor A1 - Olfert, Viktoria A1 - El-Sari, Bassel A1 - Hein, David A1 - Biegler, Max A1 - Rethmeier, Michael A1 - Meschut, Gerson T1 - A novel welding schedule for expanding the expulsion-free process window in resistance spot welding of dissimilar joints with ultra-high strength steel N2 - This study introduces a novel approach to expanding the maximum expulsion-free process window in resistance spot welding (RSW) of dissimilar joints between ultra-high strength steel (UHSS) and mild steel. Quantitative analysis revealed that expulsion is driven by the interaction between nugget growth rate and plastic shell thickness. Based on this finding, the welding schedule was optimized by applying a preheating current to form an initial plastic shell, followed by a ramp-up current profile during the main welding phase. Welding simulations indicated that the ramp-up current slowed nugget growth, improved plastic shell formation, and prevented nugget breakthrough, thereby reducing the risk of expulsion. Experimental validation showed a 19 % increase in maximum expulsion-free heat input, with the nugget diameter increasing by 7.6 % to 8.94 mm compared to the reference welding schedule. Furthermore, even when expulsion occurred beyond the process window, this optimization delayed its occurrence, minimizing its impact on spot weld quality. Finally, the optimized welding schedule also exhibited significant robustness. Despite a 2 mm initial gap disturbance, the maximum expulsionfree heat input increased by 57 %, while the nugget diameter grew by 30 % to 8.92 mm. These results confirm that the proposed approach effectively extends the process window by preventing expulsion and enhances process stability. KW - Expulsion KW - Resistance spot welding KW - Finite element modelling KW - Preheating KW - Ultra-high-strength steel PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-626877 DO - https://doi.org/10.1016/j.jmapro.2025.02.009 SN - 2212-4616 VL - 137 SP - 306 EP - 309 PB - Elsevier BV AN - OPUS4-62687 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yalçınyüz, Aybike A1 - Raute, Julius A1 - Gonzalez-Gutierrez, Joamin A1 - Pei, Eujin A1 - Biegler, Max A1 - Rethmeier, Michael T1 - Electron Beam Bonding: A novel method for joining additively manufactured carbon fiber thermoplastic composites with aluminum to produce multi-material joints for lightweight applications N2 - In recent years, new solutions have been explored to reduce the weight of components for the automotive, railway, and aerospace industries. For this reason, Carbon Fiber Composites (CFCs) have increasingly replaced metals in products that need to be lightweight. However, due to their poor thermal conductivity, CFCs have limited use in applications requiring efficient heat dissipation. In such applications, conventionally manufactured metal alloys are typically utilized. To address these limitations, a novel approach using a combination of additively manufactured aluminum and CFCs is proposed to exploit the distinct advantages of both materials. These innovative hybrid structures aim to combine good structural and thermal management properties with reduced weight compared to conventionally produced metal products. In this study, additively manufactured aluminum alloy (AlSi10Mg) and short carbon fiber Polyamide 6 composite (sCF-PA6) are utilized to produce metal–polymer pairs using electron beam energy to bond the two materials. Direct irradiation of short CFCs with electron beam leads to polymer degradation. Thus, a novel method “Electron Beam Bonding” for joining CFCs with aluminum alloy in various joint configurations using electron beam technology is demonstrated. This innovative approach presents a promising solution for creating metal–polymer multi-materials for lightweight applications. KW - Electron beam bonding KW - Multi-material KW - Lightweight KW - Additive manufactured materials KW - Short carbon fiber composites KW - AlSi10Mg KW - Joining PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-641705 DO - https://doi.org/10.1007/s40964-025-01206-1 SN - 2363-9512 SP - 1 EP - 7 PB - Springer International Publishing CY - Cham AN - OPUS4-64170 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Meng, Xiangmeng A1 - Bachmann, Marcel A1 - Yang, Fan A1 - Rethmeier, Michael T1 - Toward prediction and insight of porosity formation in laser welding: A physics-informed deep learning framework N2 - The laser welding process is an important manufacturing technology for metallic materials. However, its application is often hindered by the occurrence of porosity defects. By far, an accurate prediction of the porosity defects and an insight into its formation mechanism are still challenging due to the highly nonlinear physics involved. In this paper, we propose a physics-informed deep learning (PIDL) framework by utilizing mechanistic modeling and experimental data to predict the porosity level during laser beam welding of aluminum alloys. With a proper selection of the physical variables (features) concerning the solidification, liquid metal flow, keyhole stability, and weld pool geometry, the PIDL model shows great superiority in predicting the porosity ratio, with a reduction of mean square error by 41 %, in comparison with the conventional DL model trained with welding parameters. Furthermore, the selected variables are fused into dimensionless features with explicit physical meanings to improve the interpretability and extendibility of the PIDL model. Based on a well-trained PIDL model, the hierarchical importance of the physical variables/procedures on the porosity formation is for the first time revealed with the help of the Shapley Additive Explanations analysis. The keyhole ratio is identified as the most influential factor in the porosity formation, followed by the downward flow-driven drag force, which offers a valuable guideline for process optimization and porosity minimization. KW - Laser beam welding KW - Physics-informed deep learning KW - Porosity prediction KW - Feature fusion KW - Hierarchical importance PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-624708 DO - https://doi.org/10.1016/j.actamat.2025.120740 VL - 286 SP - 1 EP - 13 PB - Elsevier B.V. AN - OPUS4-62470 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Akyel, Fatma A1 - Üstündag, Ömer A1 - Bakir, Nasim A1 - Brunner-Schwer, Christian A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Influence of heat input on cooling rates and mechanical properties of laser hybrid welded thick structural steels N2 - Laser hybrid welding presents several challenges when used to weld thick steels. A typical weld is divided into the arcdominated and laser-dominated zone. These zones lead to variations in the mechanical properties of the weld. The laserdominated zone is of particular importance regarding mechanical properties, notably Charpy impact toughness, due to the high cooling rates and the absence of filler wire. The low heat input of the laser can lead to martensitic microstructure causing hardening and deterioration of impact toughness. The high heat input of the arc can lead to grain coarsening and even loss of impact toughness. This study examines the influence of heat input on the cooling rates, microstructure and mechanical properties of single-pass laser hybrid welded steels of S355J2 and EH36 with thicknesses up to 30 mm. The experiments were performed with a 20-kW fibre laser and a contactless electromagnetic weld backing in the butt-joint configuration in 1G welding position. The cooling time was measured in three different locations near the fusion lines corresponding to different heights of the seam using a special configuration with pyrometers, collimators and optical fibres. The test specimens for the Charpy impact testing and tensile testing were extracted in three different depths. The experiments indicated that a heat input of 1.6 kJ/mm–2 kJ/mm, 2 kJ/mm–2.4 kJ/mm and 3.7 kJ/mm were recommended when single-pass laser hybrid welding of 20-, 25-, and 30-mm-thick structural steels regarding the minimum requirements of the mechanical properties, respectively. KW - Laser hybrid welding KW - Heat input KW - Mechanical properties KW - Charpy impact toughness KW - Cooling rate PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-625282 DO - https://doi.org/10.1007/s40194-025-01924-8 SN - 1878-6669 SP - 1 EP - 15 PB - Springer CY - United Kingdom AN - OPUS4-62528 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Willeke, Maraike A1 - Giese, Marcel A1 - Lorenz, Swenja A1 - Treutler, Kai A1 - Schröpfer, Dirk A1 - Wesling, Volker A1 - Kannengießer, Thomas T1 - Effect of alloy modification on the wear protection coatings made of Ni- and Co-based materials and surface machinability via ultrasonic milling process N2 - AbstractWear-resistant coatings are required for highly efficient and economical steel components in equipment, process, and power plant engineering to withstand high corrosive, tribological, thermal, and mechanical stresses. Co-alloys are used as wear-resistant coatings for steel components, tailored to the specific application. The substitutability of Co alloys with Ni-based wear protection systems, in addition to price and supply uncertainties, is facilitated by the combination of innovative welding and machining processes such as ultrasonic-assisted milling. The aim of the study is to improve the machinability of two different hard-facing alloys while maintaining the same wear protection potential. Therefore, the wear-resistant alloys NiMoCrSi (Colmonoy C56) and CoMnCrSi (Tribaloy T400) were modified by the alloying additions Nb, Hf, and Ti and then applied to a carbon-manganese steel S355 using the plasma transfer arc (PTA) welding process. The influence of the alloying additions on the microstructure as KW - Wear resistance KW - Co-based alloy KW - Ni-based alloy KW - PTA welding process KW - Ultrasonic assisted milling process PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-623931 DO - https://doi.org/10.1007/s00170-024-14955-0 SN - 0268-3768 SP - 1 EP - 17 PB - Springer Science and Business Media LLC AN - OPUS4-62393 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Liepold, Philipp A1 - Kromm, Arne A1 - Kannengießer, Thomas T1 - Transvarestraint testing of high-strength steel filler metal N2 - High-strength steel welds are typically not known to be susceptible to Solidification Cracking (SC). However, modern light-weight constructions may force welding in highly restrained conditions, which are known to increase the probability of Solidification Crack (SC) emergence. In this article, the Modified Varestraint-Transvarestraint (MVT) test was used to evaluate the hot cracking susceptibility of welds made from high-strength, low-alloyed filler material. The materials tested include solid wires and a metal-cored wire. All wires are typically used in the Gas Metal Arc Welding (GMAW) process. Susceptibility to SC was measured over a wide range of welding parameters and bending speeds. Results show little affinity of the tested materials to SC. However, crack length increases in most cases with arc energy ( U ∙ I∕welding speed ) and welding speed. The length of the longest crack in one test specimen follows a similar trend until high welding speeds, where stagnation of crack length with changing arc energy was observed. KW - MVT KW - Varestraint KW - Transvarestraint KW - Solidification cracking KW - High-strength steel PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-630084 DO - https://doi.org/10.1007/s40194-025-02042-1 SN - 1878-6669 VL - 2025 SP - 1 EP - 12 PB - Springer CY - Berlin ; Heidelberg AN - OPUS4-63008 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Reichel, Levin A1 - Kromm, Arne A1 - Michael, Thomas A1 - Schroepfer, Dirk A1 - Kannengiesser, Thomas T1 - Modern welding processes for optimizing repair welding on high-strength offshore steels N2 - The successful energy transition in Germany will require offshore wind turbines with outputs >10 MW in the future, for which high-strength steels with a yield strength of up to 500 MPa and wall thicknesses up to 150 mm are increasingly being used. The repair of weld seams when detecting defects during NDT requires localized gouging and rewelding. This involves high demands on welding manufacturing, especially for highstrength steels. Due to a lack of investigations, there are no repair concepts and information in standards and guidelines, particularly for high-strength thick plate joints made of high-strength offshore steels. However, these are urgently needed to enable processors, especially SMEs, to carry out safe and economical repairs. Therefore, BAM startedthe FOSTA project P1629 (IGF 01IF22746N) to investigate the stress-optimized repair(local gouging and welding) of high-strength thick plate joints made of offshore grades in the yield strength range off 355 to 460 MPa and similar weld metal with controlled high-performance GMAW processes and optimized narrower gouging grooves. The experimental analyses consider the complex interaction of material, process, and designrelated influences on the formation of weld-related stresses and the special microstructure of high-strength fine-grain structural steels. Welding-related material Degradation and crack-critical residual tensile stresses need to be avoided to ensure high component safety and performance. With component-related welding experiments on special testing equipment, adapted process and heat control concepts along with variable groove configurations will be developed and recommendations for guidelines elaborated. This is the prerequisite for fully utilizing the strength potential of high-strength steels and making a valuable contribution to the energy transition in Germany, especially for steelprocessing SMEs. T2 - 6. Symposium Materialtechnik CY - Clausthal-Zellerfeld, Germany DA - 20.02.2025 KW - Narrow groove KW - Optimized repair welding KW - Modern welding processes KW - High-strength steel PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-636520 DO - https://doi.org/10.21268/20250507-5 SP - 3 EP - 15 AN - OPUS4-63652 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yang, Chunliang A1 - Yang, Fan A1 - Meng, Xiangmeng A1 - Putra, Stephen Nugraha A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Multi-refining effects of an AC electromagnetic field on the microstructure in AA5754 laser beam welding N2 - Fine-grain structure is beneficial to the mechanical properties of the joint. Different kinds of grain and sub-grain structures refined by magnetic field during laser beam welding of AA5754 aluminum alloy are analyzed in this manuscript, and the influences of different magnetic field parameters (magnetic flux density and frequency) in these refining effects are also studied. Using the scanning electron microscope (SEM), the sub-grain structure near the fusion line was obtained, and it was found that the branching promotion and branches refinement can be achieved by the magnetic field. The branches become finer with the magnetic flux density or frequency increases, and this effect is stronger in the dendritic region than in the equiaxed region. The results of electron backscatter diffraction (EBSD) in the equiaxed region show that a high-frequency magnetic field can greatly reduce the average grain size, while a low-frequency one has little effect. A phenomenological nucleation model based on dendrite fragmentation theory was established, and it was introduced into the phase field model to analyze the equiaxed grains evolution process. In addition, another refinement mechanism was also observed. The periodic solidification pattern caused by the unstable solidification in the molten pool can refine the grains, and the magnetic field promotes this kind of grain refinement by promoting the solidification period. KW - Laser beam welding KW - Magnetic field KW - Aluminum alloy KW - Crystal branch development KW - Periodic solidification pattern KW - Grain refinement PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-637222 DO - https://doi.org/10.1016/j.ijheatmasstransfer.2025.127509 SN - 0017-9310 VL - 252 SP - 1 EP - 16 PB - Elsevier Ltd. AN - OPUS4-63722 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Biegler, Max A1 - Yang, Keke A1 - Meschut, Gerson A1 - Rethmeier, Michael T1 - Occurrence and avoidance of liquid metal embrittlement in resistance spot welding of springback-afflicted deep-drawn components N2 - This study investigates the occurrence and mitigation of liquid metal embrittlement occurring during resistance spot welding in deep-drawn automotive components, specifically focusing on an S-Rail made from advanced high-strength steel. A simulation-based liquid metal embrittlement risk criterion based on local major component stresses was established and used to quantify and compare liquid metal embrittlement risks between different tests. Experimental and numerical analyses were conducted, revealing that springback significantly impacts liquid metal embrittlement formation. Adjustments in electrode geometry and hold time post-welding were found to mitigate liquid metal embrittlement risks. The effects of stack-up configuration and related parameter settings on liquid metal embrittlement occurrence were identified and liquid metal embrittlement was effectively prevented across both stack-up configurations. These findings advance the understanding of liquid metal embrittlement mechanisms and provide practical approaches to enhance the spot weld quality in AHSS-based body-in-whites. KW - Liquid metal embrittlement KW - Crack KW - Advanced high-strength steels KW - Resistance spot welding KW - Weld current KW - Heat input KW - Simulation KW - Springback KW - Deep drawing KW - S-Rail PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-636577 DO - https://doi.org/10.1177/13621718251340452 SN - 1362-1718 SP - 1 EP - 9 PB - SAGE Publications AN - OPUS4-63657 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Vinzenz A1 - Fasselt, Janek Maria A1 - Klötzer-Freese, Christian A1 - Kruse, Tobias A1 - Kleba-Ehrhardt, Rafael A1 - Biegler, Max A1 - Rethmeier, Michael T1 - Recycling nickel aluminium bronze grinding chips to feedstock for directed energy deposition via impact whirl milling: Investigation on processability, microstructure and mechanical properties N2 - During the production of ship propellers, considerable quantities of grinding chips from nickel aluminium bronze are produced. This paper examines the mechanical comminution of such chips via impact whirl milling and the utilization of two chip-powder batches as feedstock for a laser-based directed energy deposition process. The materials are characterized via digital image analysis, standardized flowability tests, scanning electron microscopy and energy dispersive X-ray spectroscopy and are compared to conventional, gas atomized powder. The specimens deposited via directed energy deposition are analyzed for density, hardness and microstructure and tensile properties for vertical and horizontal build up directions are compared. At elevated mill rotation speeds, the comminution with impact whirl milling produced rounded particles, favorable flow properties and particle size distribution, making them suitable to deposit additive specimens. The microstructure exhibited characteristic martensitic phases due to the high cooling rates of the additive manufacturing process. The presence of ceramic inclusions was observed in both the powder and on the tensile fracture surfaces, partly impairing the mechanical properties. However, specimens in the vertical build-up direction (Z) showed competitive tensile results, with 775 MPa in tensile strength, 455 MPa in yield strength and 12.6 % elongation at break. The findings of this study indicate that recycling of machining chips to additive manufacturing feedstock can be a viable option for reducing material costs and environmental impact. KW - Nickel aluminium bronze KW - Grinding chips KW - Recycling KW - Directed energy deposition KW - Material characterization PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-633442 DO - https://doi.org/10.1016/j.addma.2025.104804 SN - 2214-8604 VL - 105 SP - 1 EP - 9 PB - Elsevier BV AN - OPUS4-63344 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Marquardt, Raphael A1 - Biegler, Max A1 - Rethmeier, Michael T1 - Influence of laser power on the melt pool shape of handheld laser beam welding of 1.5 mm thick micro alloyed steel N2 - Manual welding of structures requires highly skilled welders due to the large heat-affected zone of arc-based processes, that can negatively impact microstructure and cause distortion. Handheld laser beam welding is a promising alternative with high welding velocity and a concentrated heat input. However, its current use in industry is limited to parts with aesthetic requirements, often made of high-alloyed steel. To extend the use of handheld laser beam welding to low-cost steels with good mechanical properties, this study investigates the influence of laser power on the melt pool shape for micro-alloyed steel with a thickness of 1.5 mm. Tested joint geometries are T-joints welded with filler wire as well as butt joints and overlap joints without filler wire, which are typically found in assemblies under mechanical load. Weld quality is assessed by weld porosity analysis. The results show that the handheld laser beam welding with filler wire produces T-joints with a very good external appearance, but with porosity between level C and D in the cross sections according to DIN EN ISO 13919-1. By increasing the laser power, a deep penetration of the T-joint zone can be achieved without increasing the actual throat thickness. For handheld laser beam welding of butt joints a full penetration weld of the highest quality class can be reached. Overlap joints can be welded with full or partial penetration depending on the laser power selected, with quality classes between B and C in terms of porosity. T2 - 20th Nordic Laser Materials Processing Conference CY - Kongens Lyngby, Denmark DA - 26.08.2025 KW - Hand held laser welding KW - Laser beam welding KW - Low alloyed steel KW - Process parameter PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-641671 DO - https://doi.org/10.1088/1757-899X/1332/1/012015 SN - 1757-899X VL - 1332 SP - 1 EP - 6 PB - Institute of Physics CY - London [u.a.] AN - OPUS4-64167 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Savitsky, Viktor A1 - Schmies, Lennart A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Comparative performance of DIC and optical flow algorithms for displacement and strain analysis in laser beam welding N2 - The measurement of strain and displacement in the context of the welding process represents a significant challenge. Optical methods, such as digital image correlation (DIC) or optical flow algorithms, have demonstrated their efficacy in robust and reliable data acquisition in harsh environments, including those encountered in welding processes. Concurrently, a trade-off between the accuracy of the measurement and the computational resources required for the associated calculations must be evaluated on a case-by-case basis. The application of filters to initial images represents a technique that serves to enhance the quality and accuracy of the strain and displacement prediction. In the present study, the estimated error of two algorithms, namely the Lucas-Kanade (LK) and the inverse compositional Gauss-Newton (IC-GN), is compared on the basis of both synthetic and real welding images. The displacement field is evaluated for different zones in the laser weld seam with varying contrast performance. Based on the aforementioned results, a strain calculation was conducted for both methods, which yielded comparable results for the LK and IC-GN algorithms. KW - Laser speckle KW - DIC KW - Optical flow KW - Error estimation KW - Strain measurement KW - Laser beam welding PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-625919 DO - https://doi.org/10.1016/j.optlaseng.2025.108870 SN - 1873-0302 VL - 187 SP - 1 EP - 15 PB - Elsevier Ltd. AN - OPUS4-62591 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Tobias, Charlie A1 - Gehrenkemper, Lennart A1 - Bernstein, Thomas A1 - Schlau, Sven A1 - Simon, Fabian A1 - Röllig, Mathias A1 - Meermann, Björn A1 - von der Au, Marcus T1 - Development of a fully automated slurry sampling introduction system for GF-AAS and its application for the determination of cadmium in different matrices N2 - element analysis, offering high sensitivity and precision. However, its effectiveness is limited by sample preparation challenges for solid samples like soils and microplastics. Traditional methods include sample preparation, such as digestion, which is time-consuming and involves reagents, like acids, contributing to measurement uncertainty and higher carbon footprints. Slurry sampling allows direct analysis of suspensions, offering a more efficient alternative. However, maintaining suspension stability is challenging, requiring robust autosampler systems to streamline the process and enhance analytical performance. Results: We present a novel autosampler extension for slurry sample introduction into GF-AAS. This system ensures suspension stability with a stirring device and closed vessels to prevent evaporation and contamination, incorporating a cooling unit to reduce solvent and analyte losses. It installs and removes in minutes without additional connections. Validation with cadmium analysis in BAM-U110 (Soil) and BAM-H010 (ABS) showed high reliability. For BAM-U110 (Soil), we achieved recovery rates of 94 % ± 13 % in water suspension. The recovery rate for BAM-H010 (ABS) was 104 % ±11 % in acetonitrile suspension. These results demonstrate the system’s robustness, versatility, and accuracy for different matrices. Significance: The autosampler extension helps solve key problems in trace element analysis of solid samples, making the process faster and more accurate. It works well with complex materials, making it useful for areas like microplastic or nanoparticle analysis. This improvement also helps meet regulations for monitoring environ mental and polymer samples, offering a reliable and flexible tool for high-throughput analysis with fewer errors. KW - Slurry AAS KW - Soil KW - Cd PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-618531 DO - https://doi.org/10.1016/j.aca.2024.343460 SN - 0003-2670 VL - 1335 SP - 1 EP - 7 PB - Elsevier BV AN - OPUS4-61853 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Erxleben, Kjell A1 - Kaiser, Sebastian A1 - Rhode, Michael A1 - Kannengiesser, Thomas A1 - Kromm, Arne T1 - In-service and repair welding of pressurized hydrogen pipelines–a review on current challenges and strategies N2 - Hydrogen is the energy carrier for a sustainable future without fossil fuels. As this requires a reliable transportation infrastructure, the conversion of existing natural gas (NG) grids is an essential part of the worldwide individual national hydrogen strategies, in addition to newly erected pipelines. In view of the known effect of hydrogen embrittlement, the compatibility of the materials already in use (typically low-alloy steels in a wide range of strengths and thicknesses) must be investigated. Initial comprehensive studies on the hydrogen compatibility of pipeline materials indicate that these materials can be used to a certain extent. Nevertheless, the material compatibility for hydrogen service is currently of great importance. However, pipelines require frequent maintenance and repair work. In some cases, it is necessary to carry out welding work on pipelines while they are under pressure, e.g., the well-known tapping of NG grids. This in-service welding brings additional challenges for hydrogen operations in terms of additional hydrogen absorption during welding and material compatibility. The challenge can be roughly divided into two parts: (1) the possible austenitization of the inner piping material exposed to hydrogen, which can lead to additional hydrogen absorption, and (2) the welding itself causes an increased temperature range. Both lead to a significantly increased hydrogen solubility in the respective materials compared to room temperature. In that connection, the knowledge on hot tapping on hydrogen pipelines is rare so far due to the missing service experiences. Fundamental experimental investigations are required to investigate the possible transferability of the state-of-the-art concepts from NG to hydrogen pipeline grids. This is necessary to ensure that no critical material degradation occurs due to the potentially increased hydrogen uptake. For this reason, the paper introduces the state of the art in pipeline hot tapping, encompassing current research projects and their individual solution strategies for the problems that may arise for future hydrogen service. Methods of material testing, their limitations, and possible solutions will be presented and discussed. KW - In-service KW - Hydrogen KW - Repair welding KW - Pipeline PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-638944 DO - https://doi.org/10.1007/s40194-025-02127-x SN - 0043-2288 SP - 1 EP - 24 PB - Springer Science and Business Media LLC AN - OPUS4-63894 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schmidt, Jonathan A1 - Merz, Benjamin A1 - Poka, Konstantin A1 - Mohr, Gunther A1 - Hilgenberg, Kai T1 - Surface structure analysis using visual high-resolution in situ process monitoring in laser powder bed fusion N2 - Parameter studies are a common step in selecting process parameters for laser powder bed fusion of metals (PBF-LB/M). Density cubes are commonly used for this purpose. Density cubes manufactured with varied process parameters can exhibit distinguishable surface structures visible to the human eye. The layer-wise process enables such surface structures to be detected during manufacturing. However, industrial visual in situ monitoring systems for PBF-LB/M currently have limited resolution and are incapable of reliably capturing small differences in the surface structures. In this work, a 65 MPixel high-resolution monochrome camera was integrated into an industrial PBF-LB/M machine together with a high-intensity LED (light-emitting diode) bar. Post-exposure images were taken to analyse differences in light reflection of fused areas. It is revealed that the grey-level co-occurrence matrix can be used to quantify the visual surface structure of nickel-based superalloy Inconel®939 density cubes per layer. The properties of the grey-level co-occurrence matrix correlate to the energy input and the resulting porosity of density cubes. Low-energy samples containing lack of fusion flaws show an increased contrast in the grey-level co-occurrence matrix compared to specimens with optimal energy input. The potential of high-resolution images for quality assurance via in situ process monitoring in PBF-LB/M is further discussed. KW - Additive manufacturing KW - Powder bed fusion KW - In situ monitoring KW - Image processing KW - High resolution camera PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-626685 DO - https://doi.org/10.1007/s40194-025-01955-1 SN - 1878-6669 SP - 1 EP - 15 PB - Springer Science and Business Media LLC AN - OPUS4-62668 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Czeskleba, Denis A1 - Fleißner-Rieger, H. A1 - Nietzke, Jonathan A1 - Kannengießer, Thomas T1 - Combined heating rate and restraint condition effect on stress relief cracking during PWHT of thick-walled Cr–Mo-V steel SAW joints N2 - Creep-resistant steels such as 13CrMoV9-10 are utilized in the manufacture of thick-walled pressure vessels and are typically joined by submerged arc welding (SAW). However, these materials are susceptible to stress relief cracking (SRC) if the required post weld heat treatment (PWHT) is not applied correctly. Existing PWHT guidelines, encompassing heating rate and dwell (or holding) time at a given temperature, are derived from a synthesis of empirical knowledge and typically free-shrinkage weld experiments to assess the susceptibility to SRC. Therefore, this study discusses the combined effect of the PWHT heating rate under free-shrinkage compared to restrained shrinkage. Welding experiments were conducted (using plates with a thickness of 25 mm) for both shrinkage conditions for a variety of heating rates and maximum temperatures. In-situ acoustic emission analysis was used to locate propagating SRCs during PWHT. Hardness measurements, mechanical property characterization (Charpy impact strength), and microstructure correlation were used to evaluate the SRC susceptibility. The results suggested that the influence of heating rate could not be directly related to SRC formation and that the initial weld microstructure prior to PWHT was more relevant in terms of very high hardness in the coarse grain heat affected zone, especially that of the last beads in the top layer of the welding sequence. This was seen in the form of random, unexpected SRC occurrence in only one specimen at a heating rate commonly used in welding practice (approximately 100 K/h). In this context, the additional effect of an external shrinkage restraint on SRC must be considered in the form of increasing mechanical loads during welding, which are typically not within the scope of welding practice. To mitigate the probability of SRC during PWHT, it is imperative to reduce the welding heat input and to restrict the structural shrinkage restraint of the weld joint. KW - Component test KW - Stress relief cracking KW - PWHT KW - Creep-resistant steel PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-631439 DO - https://doi.org/10.1007/s40194-025-02062-x SN - 1878-6669 SP - 1 EP - 17 PB - Springer Nature AN - OPUS4-63143 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Liepold, Philipp A1 - Kromm, Arne A1 - Kannengießer, Thomas T1 - Investigation of restraint intensity influence on solidification cracking of high-strength filler materials in fillet welds via CTS testing N2 - In addition to chemical composition, metallurgy, and welding parameters, the intensity of restraint is one of the key variables influencing solidification cracking (SC). Due to their high strength-to-density ratio, many modern lightweight steel constructions increasingly rely on high-strength steel. Given the theoretical framework of solidification cracking theory, tests tend to focus on the effects of strain rate. Externally restrained tests have provided valuable insights into solidification crack susceptibility. In practice, most welded structures are self-restrained; therefore, self-restraint tests more accurately reflect real-world applications. By varying the plate thickness in controlled thermal severity (CTS) tests conducted on S1100 QL, it was possible to adjust the intensity of restraint on fillet welds at a high level. Testing was performed using four different filler wires for gas metal arc welding (GMAW), including three solid wires and one metal-cored wire. Additionally, two sets of welding parameters were evaluated. High arc energy (U × I/welding speed) and increased welding speed were found to be more prone to solidification cracking compared to the parameter set with lower arc energy and welding speed. The results indicate a correlation between increasing restraint severity and a higher incidence of solidification cracking. KW - CTS KW - Controlled thermal severity KW - High-strength steel KW - GMAW KW - Restraint PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-631315 UR - 1878-6669 DO - https://doi.org/10.1007/s40194-025-02046-x SP - 1 EP - 13 PB - Springer AN - OPUS4-63131 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hübner, Martin A1 - Dittmann, Florian A1 - Kromm, Arne A1 - Varfolomeev, Igor A1 - Kannengießer, Thomas T1 - Residual stress reduction using a low transformation temperature welding consumable with focus on the weld geometry N2 - Low transformation temperature (LTT) welding consumables represent an innovative approach to realize compressive residual stress in the weld seam and HAZ. LTT welding consumables use the volume-expanding martensitic phase transformation near room temperature to generate compressive residual stress during cooling. This article focuses on the weld geometry and its influence on residual stress reduction using an LTT welding consumable. For this purpose, layers with an LTT welding consumable were additionally applied to the front sides of conventionally welded longitudinal stiffeners. Different weld geometries of the second weld seam could be realized by varying the welding parameters. These samples were analyzed for geometric parameters, chemical composition, and residual stress. While the chemical composition and martensite start temperature (MS) were only slightly influenced by parameter changes, a clear influence with regard to residual stress and weld geometry was observed. Depending on the shape of the second LTT weld seam, residual stress reductions of 200 to 500 MPa were achieved using the same LTT welding consumable. T2 - IIW Annual Assembly and International Conference CY - Rhodes Island, Dodecanisa, Greece DA - 07.07.2024 KW - Low transformation temperature (LTT) KW - Martensite start temperature KW - Dilution KW - Weld geometry KW - Residual stress PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-633707 DO - https://doi.org/10.1007/s40194-025-02094-3 SN - 1878-6669 SP - 1 EP - 11 PB - Springer Nature CY - Berlin ; Heidelberg AN - OPUS4-63370 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Engelking, Lorenz A1 - Scharf-Wildenhain, R. A1 - Schröpfer, Dirk A1 - Hälsig, A. A1 - Kannengießer, Thomas A1 - Hensel, J. T1 - Influence of heat input on properties and residual stresses in hybrid addi-tive manufacturing of high strength steels using MSG processes N2 - The application of steels with a higher yield strength allows reductions in wall thickness, component weight and production costs. Hybrid additive manufacturing based on Gas Metal Arc Welding (GMAW) processes (DED-Arc) can be used to realise highly effi-cient component modifications and repairs on semi-finished products and additively manufactured structures. There are still a number of key issues preventing widespread implementation, particularly for SMEs. In addition to the manufacturing design, detailed information about assembly strategy and geometric adaptation of the component for modifications or repairs are missing. These include the welding-related stresses associ-ated with the microstructural influences caused by the additive manufacturing steps, particularly in the transition area of the substrate and filler material interface. The pre-sent research focuses the effect of welding heat control during DED-Arc process on the residual stresses, especially in the transition area. Defined specimens were welded fully automatically with a high-strength solid wire (yield strength > 790 MPa) especially adapted for DED-Arc on S690QL substrate. The working temperature and heat input were systematically varied for a statistical effect analysis on the residual stress state of the hybrid manufactured components. Regarding heat control, t8/5 cooling times within the recommended processing range (approx. 5 s to 20 s) were complied. The investiga-tion revealed a significant influence of the working temperature Ti on the compressive residual stresses in the transition area and the tensile residual stresses at the base of the substrate. High working temperatures result in lower compressive residual stresses, heat input E does not significantly affect the tensile stresses. T2 - 6. Symposium Materialtechnik CY - Clausthal-Zellerfeld, Germany DA - 20.02.2025 KW - DED-Arc KW - Residual stress KW - Heat control PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-632188 DO - https://doi.org/10.21268/20250506-3 SP - 110 EP - 122 AN - OPUS4-63218 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kaiser, Sebastian A1 - Erxleben, Kjell A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Schweißen im Betrieb an Wasserstoff-Ferngasleitungen N2 - Wasserstoff gilt als Energieträger für die Erreichung der Klimaziele und einer nachhaltigen zukünftigen Energieversorgung. Für den notwendigen Transport des Wasserstoffs in großem Maßstab und über weite Entfernungen ist eine zuverlässige Pipeline-Infrastruktur erforderlich. Umfassende weltweite Forschungsprojekte deuten auf die allgemeine Kompatibilität der verwendeten überwiegend ferritischen Stähle für die vorgesehenen Betriebsbedingungen von bis zu 60 °C bei 100 bar Wasserstoff hin. Dies ist jedoch nicht direkt übertragbar auf schweißtechnische Reparatur- und Wartungsarbeiten an im Betrieb befindlichen Pipelines. Ein im Erdgasnetz etabliertes Verfahren stellt das „Hot-Tapping“ dar, bei dem eine unter Druck stehende Pipeline im Betrieb angebohrt wird. Hierfür kommt ein an die Rohrleitung geschweißtes Formstück zum Einsatz, das die Montage der Bohr-/Lochschneidemaschine ermöglicht. In den Richtlinien EIGA 121/14 bzw. AIGA 033/14 wird darauf hingewiesen, dass das Anbohren von Wasserstoffleitungen kein Routineverfahren darstellt: “[…] a hydrogen hot-tap shall not be considered a routine procedure […]“. Dieser Aussage liegt unter anderem zugrunde, dass das Anschweißen des Formstücks an das Rohr und alle zu erwartenden Wärmebehandlungen vor und nach dem Schweißen eine lokale Temperaturerhöhung verursachen. Insbesondere auch an der Rohrinnenfläche, die dem Wasserstoff ausgesetzt ist. Diese erhöhten Temperaturen begünstigen die Absorption und Diffusion von Wasserstoff in das Material. Besonders zu beachten ist außerdem die lokal auftretende kurzzeitige Austenitisierung des Materials, die eine lokal stark erhöhte Wasserstoffkonzentration verursachen kann. Aus den genannten Gründen gibt diese Studie einen kurzen Überblick über die derzeit weltweit verfügbaren Forschungsprojekte zum Schweißen von Wasserstoff-Pipelines im Betrieb. Vorgestellt werden unter anderem erste Ergebnisse des Kooperationsforschungsprojektes H2SuD, das derzeit an der BAM bearbeitet wird. T2 - 6. Symposium Materialtechnik CY - Clausthal-Zellerfeld, Germany DA - 20.02.2025 KW - Materialdegradation KW - Pipeline KW - Schweißen KW - Wasserstoff PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-632731 SN - 978-3-8440-9961-4 SN - 978-3-8191-0041-3 DO - https://doi.org/10.21268/20250506-12 SN - 2364-0804 SN - 3052-3524 N1 - Serientitel: Fortschrittsberichte der Materialforschung und Werkstofftechnik – Series title: Bulletin of Materials Research and Engineering VL - 15 SP - 381 EP - 390 PB - Shaker Verlag CY - Düren AN - OPUS4-63273 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröder, Nina A1 - Kromm, Arne A1 - Schröpfer, Dirk A1 - Kannengießer, Thomas T1 - Innovatives Instandsetzungsschweißen von Altstahl: Materialverhalten und Herausforderungen N2 - Aus Gründen der Nachhaltigkeit und Wirtschaftlichkeit gibt es in der stahlverarbeiten-den Industrie einen Trend zum Bauen im Bestand, um kostenintensive Sperrungen oder Rückbau zu vermeiden. Schweißen wird dabei als wirtschaftliches Fügeverfahren im Zusammenhang mit Altstählen kaum genutzt, obwohl Nieten- und Schraubenverbindungen oft unwirtschaftlich sind. Für die Instandsetzung ist häufig beschädigtes Bestands-material durch neue Stähle zu ersetzen bzw. Alt-Neu-Stahl-Mischverbindungen herzu-stellen. Aufgrund der verschiedenen Herstellungsprozesse von Altstählen ist nicht jeder Stahl aus dem 20. Jahrhundert schweißgeeignet. Daher ist zunächst eine Schweißeignungsprüfung erforderlich. In den vorliegenden Untersuchungen wurden verschiedene Altstähle hinsichtlich ihres Schweißverhaltens mittels Dilatometrie analysiert. Ziel war es, eine Datenbasis aus Schweiß-Zustands-Zeit-Diagrammen und Simulationen der Wärmeeinflusszone zu erstellen, um praxisrelevante Schweißuntersuchungen ableiten zu können. Diese geben wesentlichen Aufschluss hinsichtlich ihres schweißmetallurgischen Verhaltens und ihrer Schweißeignung. Solche Grundlagen sind zur Entwicklung innovativer schweißtechnischer Konzepte zur beanspruchungsgerechten Instandsetzung bestehender Altstahl-Infrastruktur in Deutschland notwendig. T2 - 6. Symposium Materialtechnik, 20. bis 21. Februar 2025 CY - Clausthal-Zellerfeld, Germany DA - 20.02.2025 KW - Altstahl KW - Schweiß-ZTU Diagramme KW - Instandsetzungsschweißen KW - Schweißeignungsprüfung KW - Dilatometrie PY - 2025 SN - 978-3-8440-9961-4 DO - https://doi.org/10.21268/20250505-1 VL - 15 SP - 370 EP - 380 PB - Shaker Verlag GmbH CY - Düren AN - OPUS4-63377 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Rhode, Michael A1 - Mente, Tobias A1 - Kannengießer, Thomas A1 - Czeskleba, Denis T1 - Simulation of hydrogen distribution in submerged arc welded heavy plates as tool for evaluating cold cracking sensitivity for offshore structures N2 - Foundation structures for offshore wind turbines are typically made of heavy plate struc-tural steels, such as S420ML, welded by submerged arc welding. Due to the welding process conditions, higher amounts of hydrogen can be introduced. In this context, large plate thicknesses result in long diffusion paths and a prolonged diffusion time for hydrogen at ambient temperature and possible delayed hydrogen-assisted cold cracking. As a result, hydrogen can accumulate in areas of high mechanical stress and strain. Due to the delayed diffusion, a minimum waiting time of up to 48 h must be observed before non-destructive testing can be performed. In addition, the assessment of possible cold crack locations is very complex. For this reason, a numerical model of a component-like weld test was developed to simulate the temperature field during welding and subsequent cooling. A hydrogen diffusion model based on the temporal-local temperature distribution was established. It was applied to simulate the change of hydrogen distribution as a function of temperature cycle during multi-layer welding and further for the entire waiting time interval ≤ 48 h. As a result, crack critical areas could be evaluated in terms of accu-mulated hydrogen. An advantage of the diffusion model is the simulation of a normalized concentration, i.e. between "0" (no hydrogen) and "1" (max. concentration), which can be scaled to experimentally determined hydrogen concentrations. Finally, selected results for increased real hydrogen ingress are presented, which confirm the relatively high crack resistance of the S420 submerged arc welded joint. KW - Hydrogen assisted cracking KW - Diffusion KW - Numerical simulation KW - Offshore steel PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-632416 DO - https://doi.org/10.21268/20250507-6 SP - 1 EP - 12 PB - Technische Universität Clausthal CY - Clausthal-Zellerfeld, Deutschland AN - OPUS4-63241 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gupta, Kanhaiya A1 - Poka, Konstantin A1 - Ulbricht, Alexander A1 - Waske, Anja T1 - Identification and authentication of additively manufactured components using their microstructural fingerprint N2 - In the field of additive manufacturing, the ability to uniquely identify and authenticate parts is crucial for certification, logistics, and anti-counterfeiting efforts. This study introduces a novel methodology that leverages the intrinsic microstructural features of additively manufactured components for their identification, authentication, and traceability. Unlike traditional tagging methods, such as embedding QR codes on the surface or within the volume of parts, this approach requires no alteration to the printing process, as it utilizes naturally occurring microstructural characteristics. The proposed workflow involves the analysis of 3D micro-computed tomography data to identify specific voids that meet predefined identification criteria. This method is demonstrated on a batch of 24 parts manufactured with identical process parameters, proving capable of achieving unambiguous identification and authentication. By establishing a tamper-proof link between the physical part and its digital counterpart, this methodology effectively bridges the physical and digital realms. This not only enhances the traceability of additively manufactured parts but also provides a robust tool for integrating digital materials, parts databases, and product passports with their physical counterparts. KW - Authentication KW - Additive manufacturing KW - X-ray Computed Tomography KW - Digital fingerprint KW - Unique identification PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-630356 DO - https://doi.org/10.1016/j.matdes.2025.113986 SN - 1873-4197 VL - 254 SP - 1 EP - 12 PB - Elsevier Ltd. CY - Amsterdam AN - OPUS4-63035 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Huo, Wenjie A1 - Schmies, Lennart A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael A1 - Wolter, Katinka T1 - Prediction of mean strain from laser beam welding images and detection of defects via strain curves based on machine learning N2 - With the advancement of machine learning, many predictions and measurements in visual tasks can be achieved by convolutional neural networks (CNNs). Solidification hot cracking is a significant defect in laser beam welding, commonly encountered in practical applications. Existing theories indicate that the formation of cracks is closely related to strain accumulation near the solidification front. In this paper, we first leverage supervised Regression networks to design CNNs that achieve real-time average strain estimation for each frame in the collected welding videos. Two different architectures are proposed and compared: the first model stacks two frames at a set interval and feeds them into the network, while the second model extracts image features individually and predicts the results by calculating the correlation between them. Each network has its own advantages in Terms of computational efficiency and accuracy. Finally, we further train a multilayer perceptron (MLP) classification model that can detect the occurrence of cracks based on the predicted strain behaviors. KW - Laser beam welding KW - Mean strain prediction KW - Solidification cracking detection Convolutional neural networks KW - Convolutional neural networks PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-644495 DO - https://doi.org/10.1016/j.optlastec.2025.113975 SN - 0030-3992 VL - 192, Part F SP - 1 EP - 8 PB - Elsevier Ltd. AN - OPUS4-64449 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Scharf-Wildenhain, R. A1 - Engelking, Lorenz A1 - Hälsig, A. A1 - Schröpfer, Dirk A1 - Kannengießer, Thomas A1 - Hensel, J. T1 - Effect of heat control on mechanical properties and residual stresses at the transition zone of component and substrate in hybrid DED‑arc manufacturing N2 - In hybrid additive manufacturing, components or semi-finished products manufactured by conventional primary forming are enhanced or modified by additive manufactured structures. However, systematic investigations focusing on the critical transition area between the specific properties of the substrate (like high-strength) and the additively manufactured component, made of specific filler material, are still lacking. The focus of the present study was to determine the influence of heat control on the Δt8/5 cooling time, the distortion, the mechanical properties, and the residual stresses in the transition area of hybrid-additive components. This contributed to the knowledge regarding the safe avoidance of cold cracking, excessive distortion, a reduction in yield stress, and the implementation of hybrid DED-arc manufacturing. The heat control was varied by means of heat input and working temperature such that the Δt8/5 cooling times corresponded to the recommended processing range. The heat input has a greater influence on the cooling time in the transition area than the working temperature. Working temperature and the total energy applied per layer have a significant effect on component distortion. The lowest working temperature of 100 °C in combination with the highest total energy per layer leads to significantly greater distortion compared to manufacturing with a high working temperature of 300 °C and low total energy per layer. In addition, the longitudinal residual compressive stresses in the sensitive transition area are reduced from − 500 MPa to approx. − 200 MPa by adjusting the working temperature from 100 to 300 °C. Such complex interactions must be clarified comprehensively to provide users with easily applicable processing recommendations and standard specifications for an economical hybrid additive manufacturing of components made, for example, of high-strength steels in the transition area. T2 - IIW Annual Assembly and International Conference CY - Rhodes Island, Greece DA - 07.07.2024 KW - Hybrid additive manufacturing KW - DED-arc KW - Heat control KW - High-strength metals KW - Residual stress PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-630415 DO - https://doi.org/10.1007/s40194-025-02036-z SN - 1878-6669 SP - 1 EP - 15 PB - Springer AN - OPUS4-63041 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Chaurasia, Prashant Kumar A1 - Fabry, Çağtay A1 - Pittner, Andreas A1 - De, Amitava A1 - Rethmeier, Michael T1 - Automated in situ monitoring and analysis of process signatures and build profiles during wire arc directed energy deposition N2 - Wire arc directed energy deposition (DED-Arc) is an emerging metal additive manufacturing process to build near-net shaped metallic parts in a layer-by-layer with minimal material wastage. Automated in situ monitoring and fast-responsive analyses of process signatures and deposit profiles during DED-Arc are in ever demand to print dimensionally consistent parts and reduce post-deposition machining. A comprehensive experimental investigation is presented here involving real-time synchronous measurement of arc current, voltage, and the deposit profile using a novel multi-sensor monitoring framework integrated with the DED-Arc set-up. The recorded current–voltage transients are used to estimate the time-averaged arc power, and energy input in real time for an insight of the influence of wire feed rate and printing travel speed on the deposit characteristics. A unique attempt is made to represent the geometric profiles of the single-track deposits in a generalized mathematical form corresponding to a segmented ellipse, which has exhibited the minimum root-mean-square error of 0.03 mm. The dimensional inconsistency of multi-track deposits is evaluated quantitatively in terms of waviness using build profile monitoring and automated estimation, which is found to increase with an increase in step-over ratio and energy input. For the multi-track mild steel deposits, the suitable range of step-over ratio for the minimum surface waviness is observed to lie between 0.6 and 0.65. Collectively, the proposed framework of synchronized process monitoring and real-time analysis provides a pathway to achieve dimensionally consistent and defect-free parts, and highlights the potential for closed-loop control systems for a wider industrial application of DED-Arc. KW - Additive Manufacturing KW - Arc welding KW - DED-arc KW - Real-time monitoring and control KW - Dimensional inconsistency PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-642029 DO - https://doi.org/10.1007/s40964-025-01333-9 SN - 2363-9512 SP - 1 EP - 20 PB - Springer Science and Business Media LLC CY - Cham AN - OPUS4-64202 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas A1 - Kromm, Arne A1 - Kadoke, Daniel A1 - Kruse, Julius T1 - Effect of Ti microalloying on the local strain behavior of cross-weld tensile samples determined by digital image correlation N2 - High-strength low-alloyed (HSLA) steels with yield strength / proof stress ≥ 600 MPa are the basis of modern light-weight steel constructions. Indeed, the economic and ecological benefits strongly depend on their processability in terms of welding. In this context, the use of highly productive welding processes and suitable welding consumables is of vital interest and requires a fundamental understanding of the microstructural changes in the HSLA steel and especially the heat-affected zone (HAZ) of the welded joint. Microalloying elements, such as Ti or Nb, are essential to achieve the desired mechanical properties. To analyse the weldability, three-layer welds were performed using gas metal arc welding (GMAW) and critical microstructures, such as areas of the HAZ that exhibit significant softening or hardening, were identified. The effect of the softened HAZ region on failure was evaluated using cross-weld tensile specimens. Digital image correlation (DIC) was used for in-situ monitoring of the development and accumulation of the local strains in different HAZ regions during tensile testing. Using a specially designed mirror system, the local strains of the microstructure zones on the top and bottom of the weld were recorded simultaneously. In addition, the analysis of the local deformation helps to understand the effects of the softened HAZ on the global strain, the reduction in area, the fracture position, and the overall fracture behavior. KW - High-strength structural steel KW - Microalloying influences KW - HAZ-softening KW - Digital Image Correlation KW - Constraint effect KW - Thermodynamic simulation PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-643558 DO - https://doi.org/10.1007/s40194-025-02185-1 SP - 1 EP - 17 PB - Springer Nature AN - OPUS4-64355 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Poka, Konstantin A1 - Ali, Sozol A1 - Ulbricht, Alexander A1 - Schröder, Jakob A1 - Khambayat, Jiganesh A1 - Scholz, Maik A1 - Saeed, Waleed A1 - Merz, Benjamin A1 - Epperlein, Martin A1 - Hilgenberg, Kai T1 - Reduction of extraneous variance in powder bed fusion with laser beam of metals by means of advanced digital preprocessing N2 - Data-driven quality assurance and reproducibility are critical for advancing the industrial maturity of Powder Bed Fusion with Laser Beam of Metals (PBF-LB/M). This study addresses the extraneous variance in scan vectors that arises even for identical cross sections of nominally identical components but located at different positions on the build platform. This inherent variance, common across most PBF-LB/M machines, is caused by scan vector computation relative to the machine coordinate origin and subsequent projection of the resulting pattern onto individual component cross sections. In this work, scan vectors are computed still following conventional slicing, but relative to the workpiece origin of each component, using an EOS M 300-4. This digital preprocessing approach homogenizes fabrication conditions, ensuring that anomalies, such as scan vector overlaps, occur consistently across identical components. The impact during fabrication is assessed through powder bed imaging, melt pool monitoring, and operational data from the multilaser PBF-LB/M machine. Components are manufactured from AlSi10Mg for each scan vector computation origin and subsequently qualified using x-ray computed tomography, optical coordinate measurement, and optical surface measurement. A comprehensive evaluation is conducted, comparing the results in terms of component density, geometric accuracy, and surface roughness to those obtained using conventional preprocessing. Based on these findings, practical recommendations are provided, focusing on achieved quality criteria to identify potential drawbacks, while also considering the life cycle analysis of fabrication. Finally, the study emphasizes the significance of consistent scan vector provisioning for identical components placed at different build platform positions, assuming no roll or pitch during nesting. T2 - ICALEO CY - Orlando, FL, USA DA - 13.10.2025 KW - Quality assurance KW - Data management KW - 3D printing KW - Laser fabrication KW - Life cycle analysis PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-642104 DO - https://doi.org/10.2351/7.0001890 SN - 1042-346X VL - 37 IS - 4 SP - 1 EP - 14 PB - American Institute of Physics Publishing CY - New York AN - OPUS4-64210 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Fabry, Çağtay A1 - Pittner, Andreas A1 - Rethmeier, Michael T1 - Arc-sidewall-attaching-driven control of swing arc motion in narrow gap GMAW N2 - A novel, event-driven approach to controlling the weaving motion in swing arc narrow gap GMAW is presented in this study. The control method is based on independently detecting the arc attachment event at each sidewall of the narrow groove to adjust the weaving motion in real time. Previous arc sensing approaches for swing arc principles are based on evaluating and comparing arc sensor readings collected during the dwell periods at each sidewall. Not only does this require the torch to be positioned at the groove centre and the arc motion to be symmetric, but previous methods have also been shown to rely on complex parametrization of control parameters. The newly presented approach is based on the real-time monitoring of the welding current progression during the approach of the arc towards the sidewall of the groove independently on each side. As soon as the arc attachment at the sidewall is detected based on a characteristic rise in the current signal, the weaving motion is stopped. For reference experiments in a 21-mm wide groove, the weaving angle amplitude is controlled and limited to 50° on both sides individually, resulting in stable process conditions and uniform sidewall fusion. It is further shown that the newly developed control method can successfully be applied to groove widths of 18 mm and 24 mm without reconfiguration of the control parameters, highlighting the flexibility of the approach. KW - Gas metal arc welding KW - Narrow gap KW - Arc sensor KW - Control PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-647640 DO - https://doi.org/10.1007/s40194-025-02238-5 SN - 0043-2288 SP - 1 EP - 11 PB - Springer Science and Business Media LLC AN - OPUS4-64764 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Iskhakov, Tagir A1 - Breese, Philipp A1 - Altenburg, Simon A1 - Hilgenberg, Kai T1 - Numerical and experimental analysis of temperature compensation for eddy current testing during laser powder bed fusion N2 - The quality of parts produced via laser powder bed fusion (PBF-LB/M) can be affected by microstructural defects inherent to the process. In-situ monitoring technologies are crucial for ensuring consistent component quality. Eddy current testing (ECT) offers a viable method for real time monitoring during the PBF-LB/M build cycle. However, complex temperature fields arising during manufacturing significantly impact electrical conductivity, posing a challenge for ECT accuracy. Thus, precise temperature distribution prediction is essential for reliable flaw detection. This study develops a Finite Element (FE) model to predict the temperature field in multi-part build cycles. Scan vectors are grouped into clusters based on their timestamps, enabling the homogenization of thermal loads from multiple scan vectors. This approach allows for optimizing the trade-off between modeling accuracy and computational efficiency in a multi-part build. The study assesses the prediction accuracy required for ECT and investigates the appropriate level of homogenization needed to achieve it. Model predictions are validated through comparisons with thermography images and thermocouple measurements conducted during the manufacturing of 316L steel components. KW - PBF-LB/M KW - FEM KW - Heat accumulation KW - Eddy current testing KW - 316L PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-650165 DO - https://doi.org/10.1007/s40964-025-01429-2 SP - 1 EP - 20 PB - Springer Nature AN - OPUS4-65016 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Vinzenz A1 - Klement, Oliver A1 - Sander, Steffen A1 - Biegler, Max A1 - Rethmeier, Michael T1 - Recycling of Stainless Steel Milling Chips for Additive Manufacturing: A Three-Stage Comminution Approach Using a Fine Impact Mill N2 - The production of conventional metal powders for additive manufacturing process is energy intensive and costly. This study introduces a sustainable alternative by recycling stainless steel milling chips as feedstock for laser-powder directed energy deposition. The recycling process employs a three-stage mechanical comminution method utilizing a fine impact mill UPZ100 from Hosokawa Alpine AG. Characterization of the resulting powders is conducted through particle morphology analysis, flowability tests, and mechanical property assessments. The chip-derived powders exhibit comparable aspect ratios and sphericity to conventional water atomized powders, though with reduced flowability due to a pronounced fine fraction content. Elevated levels of oxides are observed, leading to the formation of an oxide layer on specimen blocks, without impairing the mechanical properties. Analyses of porosity, microstructure, and hardness indicate no significant differences when compared to conventional powders from water or gas atomization. This recycling approach not only mitigates waste but also enhances the potential for a circular and sustainable manufacturing process in the additive manufacturing industry and beyond. KW - Directed Energy Deposition KW - Recycling KW - Stainless steel KW - Comminution KW - Powder characteristics PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-652037 DO - https://doi.org/10.1088/1757-899X/1332/1/012014 SN - 1757-8981 VL - 1332 IS - 1 SP - 1 EP - 7 PB - IOP Publishing AN - OPUS4-65203 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Chand, Keerthana A1 - Fritsch, Tobias A1 - Oster, Simon A1 - Ulbricht, Alexander A1 - Poka, Konstantin A1 - Bruno, Giovanni T1 - A Comparative Study of Rigid Three-Dimensional Image Registration Methods for Powder Bed Fusion with Laser Beam of Metals Using a Gold Standard Approach N2 - In Additive Manufacturing (AM), precise rigid three-dimensional (3D) image registration between X-ray Computed Tomography (XCT) scans and Computer-Aided Design (CAD) models is an important step for the quantification of distortions in produced parts. Given the absence of standardized benchmarks for image registration in AM, we introduce a gold standard for 3D image registration, using a reference base plate beneath the build structure. This gold standard is used to quantify the accuracy of rigid registration, with a proof of concept demonstrated in PBF-LB/M. In this study, we conduct a comparative analysis of various rigid 3D registration methods useful for quality assurance of PBF-LB/M parts including feature-based, intensity-based, and point cloud-based approaches. The performance of each registration method is evaluated using measures of alignment accuracy based on the gold standard and computational efficiency. Our results indicate significant differences in the efficacy of these methods, with point cloud based Coherent Point Drift (CPD) showing superior performance in both alignment and computational efficiency. The rigidly registered 3D volumes are used to estimate the deformation field of the printed parts relative to the nominal CAD design using Digital Volume Correlation (DVC). The quality of the estimated deformation field is assessed using the Dice score metric. This study provides insights into methods for enhancing the precision and reliability of AM process. KW - Digital volume correlation KW - 3D image registration KW - 3D image processing KW - X-ray computed tomography KW - Computer-aided design KW - Displacement field estimation PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-627043 DO - https://doi.org/10.1007/s10921-025-01174-0 SN - 1573-4862 VL - 44 IS - 30 SP - 1 EP - 20 PB - Springer AN - OPUS4-62704 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Jakob A1 - Han, Ying A1 - Fritsch, Tobias A1 - Hejazi, Bardia A1 - Ulbricht, Alexander A1 - Skrotzki, Birgit A1 - Bruno, Giovanni T1 - X-ray computed tomography quantifies primary phases and reveals crack morphology in high-cycle fatigue of aluminum alloy EN AW-2618A N2 - Since the introduction of high-strength aluminum alloys understanding their fatigue behavior is of high interest for the structural integrity of engineering components, in this context, the alloy EN AW-2618A gains its high strength from both nanometer size precipitates and micrometer size primary phases. The latter phases are often identified as crack initiation sites. In this study, it uses a combination of synchrotron and laboratory-based X-ray computed tomography to image and quantify such primary phases and the fatigue cracks appearing in interrupted tests. Based on the gray-level differences in the synchrotron X-ray computed tomography scans, this study is able to distinguish low- and high-absorbing particles. The dominant (volume fraction >99%) high absorbing primary phase can be quantified in good agreement with results of Thermo-Calc calculations. To image the fatigue crack, laboratory X-ray computed tomography scans are performed at different tensile loads to open the crack. The results show that with an appropriate crack opening tensile load, the fatigue crack morphology can be reliably revealed. Based on these results, the influence of the primary phases on the fatigue crack initiation and propagation are discussed. KW - X-ray computed tomography KW - Fatigue KW - Aluminum KW - Primary phases PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-632724 DO - https://doi.org/10.1002/adem.202500235 SN - 1527-2648 SP - 1 EP - 9 PB - Wiley-VCH CY - Weinheim AN - OPUS4-63272 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Suárez Ocaño, Patricia A1 - Ávila Calderón, Luis A1 - Agudo Jácome, Leonardo A1 - Rehmer, Birgit A1 - Mohr, Gunther A1 - Evans, Alexander A1 - Skrotzki, Birgit T1 - Effect of 700–900 °C heat treatments and room and high temperature tensile deformation on the microstructure of laser powder bed fused 316L stainless steel N2 - The effect of post-processing heat treatments on the hierarchical microstructure evolution and mechanical strength of the austenitic stainless steel 316L produced by laser powder bed fusion has been investigated. Heat treatments between 700 and 900 ◦C and 0.5 to 3 h, were applied to samples treated at 450 ◦C for 4 h. The results showed a stable microstructure at all studied temperatures and times in terms of grain size, morphology, aspect ratio, density of low-angle grain boundaries, and texture. However, temperature and time promoted the diffusion of segregated elements together with a reduction in dislocation density and disappearance of the cellular structure. This was associated with a reduction in hardness and tensile proof strength at both room and high temperature. In addition, microstructural characterization coupled with thermodynamic CALPHAD-based equilibrium calculations showed that the formation of carbides and intermetallic phases was already visible after annealing at 800 ◦C for 3 hours, although these intermetallics did not affect the tensile properties at this level. Analysis of the microstructure evolution after tensile deformation showed differences in the deformation mechanisms at room and high temperature, with twinning and martensitic transformation occurring at room temperature, the latter not widely reported for additively manufactured 316L. Finally, comparisons with similar materials produced under comparable conditions showed differences in the tensile properties, attributed to differences in chemical composition and the associated presence of stacking faults in the undeformed state. KW - Additive manufacturing KW - 316L stainless steel KW - Heat treatments KW - Tensile properties KW - Microstructure PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-632471 DO - https://doi.org/10.1016/j.msea.2025.148469 SN - 0921-5093 VL - 939 SP - 1 EP - 24 PB - Elsevier CY - Amsterdam AN - OPUS4-63247 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Müller, Vinzenz A1 - Fasselt, Janek Maria A1 - Klötzer-Freese, Christian A1 - Kruse, Tobias A1 - Kleba-Ehrhardt, Rafael A1 - Biegler, Max A1 - Rethmeier, Michael T1 - Recycling nickel aluminium bronze grinding chips to feedstock for directed energy deposition via impact whirl milling: Investigation on processability, microstructure and mechanical properties N2 - During the production of ship propellers, considerable quantities of grinding chips from nickel aluminium bronze areproduced. This paper examines the mechanical comminution of such chips via impact whirl milling and the utilization of twochip-powder batches as feedstock for a laser-based directed energy deposition process. The materials are characterized viadigital image analysis, standardized flowability tests, scanning electron microscopy and energy dispersive X-ray spectroscopyand are compared to conventional, gas atomized powder. The specimens deposited via directed energy deposition areanalyzed for density, hardness and microstructure and tensile properties for vertical and horizontal build up directions arecompared. At elevated mill rotation speeds, the comminution with impact whirl milling produced rounded particles, favorableflow properties and particle size distribution, making them suitable to deposit additive specimens. The microstructureexhibited characteristic martensitic phases due to the high cooling rates of the additive manufacturing process. The presenceof ceramic inclusions was observed in both the powder and on the tensile fracture surfaces, partly impairing the mechanicalproperties. However, specimens in the vertical build-up direction (Z) showed competitive tensile results, with 775 MPa intensile strength, 455 MPa in yield strength and 12.6 % elongation at break. The findings of this study indicate that recyclingof machining chips to additive manufacturing feedstock can be a viable option for reducing material costs and environmentalimpact. KW - Nickel aluminium bronze KW - Grinding chips KW - Recycling KW - Directed energy deposition KW - Material characterization PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-651214 DO - https://doi.org/10.1016/j.addma.2025.104804 SN - 2214-8604 VL - 105 SP - 1 EP - 9 PB - Elsevier B.V. AN - OPUS4-65121 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Huo, Wenjie A1 - Schmies, Lennart A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael A1 - Wolter, Katinka T1 - An illumination based backdoor attack against crack detection systems in laser beam welding N2 - Deep neural networks (DNNs) have been wildly used in engineering and have achieved state-of-the-art performance in prediction and measurement tasks. A solidification crack is a serious fault during laser beam welding and it has been proven to be successfully detected using DNNs. Recently, research on the security of DNNs is receiving increasing attention because it is necessary to explore the reliability of DNNs to avoid potential security risks. The backdoor attack is a serious threat, where attackers aim to inject an inconspicuous pattern referred to as trigger into a small portion of training data, resulting in incorrect predictions in the reference phase whenever the input contains the trigger. In this work, we first generate experimental data containing actual cracks in the welding laboratory for training a crack detection model. Then, targeting this scenario, we design a new type of backdoor attack to induce the model to predict the crack as a normal state. Considering the stealthiness of the attack, a common phenomenon during the welding process, illumination, is used as the backdoor trigger. Experimental results demonstrate that the proposed method can successfully attack the crack detection system and achieve over 90% attack success rate on the test set. T2 - 8th ML4CPS 2025 – Machine Learning for Cyber-Physical Systems CY - Berlin, Germany DA - 06.03,2025 KW - System security KW - Welding crack detection KW - Backdoor attack KW - Deep neural networks PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-651357 DO - https://doi.org/10.24405/20021 VL - 2025 SP - 12 EP - 21 PB - Universitätsbibliothek der HSU/UniBw H CY - Hamburg AN - OPUS4-65135 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Nietzke, Jonathan A1 - Konert, Florian A1 - Poka, Konstantin A1 - Merz, Benjamin A1 - Sobol, Oded A1 - Böllinghaus, Thomas T1 - Comparison of hydrogen effects on additively manufactured and conventional austenitic steels N2 - Hydrogen and its derivatives are promising energy carriers for future renewable energy supplies. Austenitic stainless steels, such as AISI 316L, are commonly used in hydrogen transportation systems. While often thought to be resistant to hydrogen embrittlement, studies have shown that 316L is susceptible under certain conditions. As demand for hydrogen applications grows, additive manufacturing (AM) technologies offer design flexibility and customisation benefits. However, data on AM parts behaviour in hydrogen environments is lacking. This study investigates the influence of hydrogen on mechanical properties using slow strain rate testing (SSRT) on conventional AISI 304L, 316L and AM 316L specimens. The results indicate a greater effect of hydrogen on 304L compared to 316L, with AM 316L showing increased susceptibility. However, the ductility of AM 316L remains comparable to conventional 316L due to its initial ductility. The study provides insights into the performance of conventional and AM austenitic stainless steels in gaseous hydrogen environments. KW - Slow strain rate testing KW - Hollow specimen KW - Hydrogen embrittlement KW - Additive manufacturing KW - Austenitic steel PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-615919 DO - https://doi.org/10.1016/j.engfailanal.2024.109042 SN - 1350-6307 VL - 167 SP - 1 PB - Elsevier B.V. AN - OPUS4-61591 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Konert, Florian A1 - Nietzke, Jonathan A1 - Grimault de Freitas, Tomás A1 - Rhode, Michael A1 - Sobol, Oded A1 - Böllinghaus, Thomas T1 - Investigation of resistance to gaseous hydrogen of a longitudinal weld seam in a X65 pipeline using the hollow specimen technique N2 - The constantly increasing demand for renewable energy sources leads to the necessity of transporting large amounts of hydrogen. Since pipelines enable a cost-effective way for the distribution of gaseous hydrogen, the interaction of hydrogen and the pipeline materials must be carefully investigated as hydrogen can cause a degradation of the mechanical properties under certain conditions. Especially welds, which are assumed to be more susceptible to the degradation enhanced by hydrogen, are of great interest. The aim of this study is to investigate the effect of gaseous hydrogen on the mechanical properties of an X65 pipeline, and the longitudinal submerged arc welding (SAW) welded joint. The tests are conducted using the hollow specimen technique on two types of specimens: one extracted from the base material (BM) and the other extracted as a cross-weld (CW) specimen consisting of BM and weld seam. The specimens are charged in situ under a pressure of 60 bar and tested using slow strain rate (SSR) tensile tests with a nominal strain rate of 10−5 s−1. The properties obtained of specimens tested in hydrogen atmosphere are compared to the properties of comparable specimen in inert argon atmosphere as a reference. The performed tests showed a decrease of the reduction of area (RA) from 72% in inert atmosphere to 52% in hydrogen atmosphere for the CW specimen and a decrease from 73% in inert atmosphere to 51% for the BM. Metallographic analyses showed the crack initiation between fine-grained heat-affected zone (FGHAZ) and BM for the specimens tested in hydrogen atmosphere as well as for the reference specimens. This leads to the conclusion that the location of the crack initiation does not change due to the presence of gaseous hydrogen. KW - Hydrogen KW - Hollow specimen technique KW - Pipeline KW - SSRT KW - Hydrogen embrittlement KW - Cross-weld specimen PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-624658 DO - https://doi.org/10.1007/s40194-025-01953-3 SN - 0043-2288 SN - 1878-6669 VL - 69 IS - 3 SP - 861 EP - 870 PB - Springer CY - Berlin AN - OPUS4-62465 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Shikomba, Nikanor A1 - Böllinghaus, Thomas A1 - Konert, Florian A1 - Sobol, Oded A1 - Blasón Gonzalez, Sergio A1 - Ohijeagbon, Idehai Olayemi A1 - Krafft, Eike A1 - Staudt, Thorsten T1 - Resistance of welded low-alloyed pressure vessel and pipeline steels in gaseous hydrogen N2 - Green hydrogen has become an essential energy carrier to achieve a climate-neutral economy. The production, storage, transport and usage of green hydrogen require safe and sustainable facilities and systems. The present contribution provides a procedure guideline to investigate the compatibility of steel welds for pressurised gaseous hydrogen applications under quasi-static mechanical loads, utilising the slow strain rate test and hollow specimen technique. Exemplarily, a weld of the low-alloyed steel P355NL1 was investigated and compared to an X65 weld. The results indicate that the base metal exhibits a higher ductility than the weld metal for both steels. Generally, hydrogen-exposed specimens exhibited a reduced strain, as compared to reference specimens. The hydrogen degradation, evaluated by the hydrogen embrittlement index, was more pronounced in the weld metal compared to the base P355NL1 material, whereas the X65 exhibited a larger hydrogen degradation of the base material than in the weld metal. Fractographic analysis of the test specimens revealed that hydrogen causes a transition from ductile to brittle features. Generally, the results of this study indicate a mild but significant degradation of the mechanical properties in terms of the ductility of the welds in the respective pressurised hydrogen atmosphere. KW - Hydrogen-assisted cracking KW - Welded joint KW - Slow strain rate test KW - Hollow Specimen KW - Structural steel PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-634138 DO - https://doi.org/10.1007/s40194-025-02074-7 SN - 0043-2288 SP - 1 EP - 15 PB - Springer CY - Berlin AN - OPUS4-63413 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Graebner, Maraike A1 - Giese, Marcel A1 - Lorenz, Svenja A1 - Treutler, Kai A1 - Schröpfer, Dirk A1 - Wesling, Volker A1 - Kannengießer, Thomas T1 - Wear resistance of modified NiMoCrSi claddings in relation to the resulting surface machinability via ultrasonic-assisted milling N2 - In the field of plastics processing, extruder screws are subjected to significant wear stresses. The extruder screw is the main wear component in those production machines and is usually coated with intermetallic wear protection alloys composed of Ni-based alloys, specifically Colmonoy C56 PTA (NiMoCrSi). There is a growing demand for providing an economic machinability of these alloys to achieve defined contours with a sufficient surface integrity. Recent investigations exhibit promising results applying ultrasonic milling for such hard-to-cut materials. The Colmonoy C56 is modified by various alloying additions Ti, Nb, Mo, Hf, and Al, and then cladded on a steel S355 via Plasma Transferred Arc process. The effect of alloying additions on the microstructure is analyzed regarding their resistance to abrasive and adhesive wear. With Miller test ASTM G75 the influence of alloying elements on resistance to abrasive wear for two abrasive materials is investigated (high-grade corundum F220 and quartz powder). The wear loss is not increased for additions of Nb and Ti compared to the base material C56. Modifications with Hf or Al reduces the resistance to abrasive wear and significantly increases material loss. The extruder screw is also subject to adhesive wear, which can be quantified by means of the pin-roll test. It is demonstrated that the addition of Hf, for example, contributes to a reduction in wear loss. Aim of the investigations is to find suitable modifications for the wear claddings of C56 for a sufficient machineability, without compemising the wear resistant. The machinability is considerably affected by the alloy additions, and is determined using ultrasonic-assisted milling. The addition of hafnium reduces machinability, i.e. significantly increases cutting forces. The incorporation of Nb exhibits a significant reduction of cutting forces, and results in reduced tool wear and an enhanced of surface integrity (roughness, density of defects, residual stresses). KW - Colmonoy C56 KW - PTA welding KW - Adhesive wear KW - Abrasive wear KW - Ultrasonic-assisted milling process KW - Surface integrity KW - Service life and efficiency KW - Substitution of critical raw materials PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-651530 DO - https://doi.org/10.1016/j.wear.2025.205830 SN - 0043-1648 VL - 571 SP - 1 EP - 10 PB - Elsevier B.V. AN - OPUS4-65153 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Denora, Isabella A1 - Clute, Clara A1 - Murillo, Natalia Cano A1 - Theiler, Geraldine A1 - Balasooriya, Winoj A1 - Kaiser, Andreas A1 - Fasching, Michael A1 - Schwarz, Thomas A1 - Marano, Claudia T1 - A study on the mechanical behaviour of carbon black and Struktosil-filled NBR compounds for hydrogen applications N2 - This study investigates the effect of the addition of a 2D filler (Struktosil) to a carbon black-filled acrylonitrile butadiene rubber, developed for seals in hydrogen applications. Several characterization methods have been adopted. The addition of Struktosil increases the stiffness of the material up to a strain of about 100%, to a lesser extent in presence of a plasticizer. The dissipative response of the material is increased by Struktosil addition and decreased in presence of the plasticizer. Concerning fracture behaviour, the crack initiation and Rapid Gas Decompression (RGD) resistance were not affected by the addition of Struktosil but decreased in presence of plasticizer. Furthermore, the addition of Struktosil had a positive effect on crack propagation resistance. The effects of pressurized hydrogen exposure on physical-mechanical properties were also evaluated and correlated with the results. A correlation between fracture toughness and RGD resistance has been also attempted. KW - Acrylonitrile Butadiene rubber KW - Fracture mechanics KW - 2D filler KW - High-pressure hydrogen KW - Rapid gas decompression PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-648285 DO - https://doi.org/10.1016/j.ijhydene.2025.03.122 SN - 0360-3199 VL - 118 SP - 407 EP - 416 PB - Elsevier Ltd. AN - OPUS4-64828 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kittner, Maria A1 - Coesfeld, Bianca A1 - Schlau, Sven A1 - Werischak, Thomas A1 - Altmann, Korinna A1 - Kalbe, Ute T1 - Simultaneous sampling for microplastics and environmental contaminants from artificial turf: development of a new integrated microplastics eluate lysimeter N2 - To get a better understanding of potentially harmful contaminant emissions from soils or materials into the environment, politics demand practical and holistic sampling concepts for environmental samples such as leachates containing polycyclic aromatic hydrocarbons (PAH) or heavy metals, and hazardous particulate matter like microplastics (MP). Of particular concern are MP emissions from artificial turf sports pitches. So far, there has been only very limited data on MP mass emissions from artificial turf potentially posing a risk to the groundwater and no sampling device that allowed simultaneous sampling for dissolved and particulate contaminants. In this study, a novel integrative microplastics eluate lysimeter was developed to determine contaminant emissions from three artificial turf systems at different ageing states (fabric-new, artificially aged, real-time aged). For the accelerated ageing, all environmental simulation parameters were based on Central German conditions and simulated outdoor stress during the turf service lifespan of 15 years. MP masses from eluates were analysed using thermal extraction desorption-gas chromatography/mass spectrometry, PAH concentrations using gas chromatography/mass spectrometry and heavy metals using inductively coupled plasma-optical emission spectroscopy. Results showed that no PAH or heavy metal concentrations from the seepage water were above German legal limits for alternative granular construction materials considering soil and groundwater protection. Furthermore, it was found that only minimal MP emissions were released from new turf systems into the seepage water (< 1 mg/m2). Ageing of the artificial turf increased MP formation, especially from rubber infill and grass fibres, which are then carried into the seepage water. The highest total MP emissions over a simulated turf lifespan of 15 years were detected in two real-time aged turf systems ranging from 136.4–252.5 mg/m2. Considerably less total MP emissions were detected in accelerated aged artificial turf systems, one of which contained a synthetic rubber infill (5.4–8.0 mg/m2) and one without rubber infill (0.2–5.3 mg/m2). In summary, it was demonstrated that the newly developed MEL generated reliable and reproducible data and has thus proven itself as an integrated, straightforward and automated sampling device for simultaneous monitoring of particulate and dissolved pollutant emissions from simple soil matrices. KW - Lysimeter KW - Microplastics KW - Artificial turf KW - Thermal extraction desorption-gas chromatography/mass spectrometry KW - TED-GC/MS KW - Polycyclic aromatic hydrocarbons KW - PAH KW - Heavy metals KW - Soil samples PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-645301 DO - https://doi.org/10.1186/s12302-025-01235-1 SN - 2190-4715 VL - 37 IS - 1 SP - 1 EP - 15 PB - Springer Open AN - OPUS4-64530 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Campari, Alessandro A1 - Konert, Florian A1 - Razavi, Nima A1 - Sobol, Oded A1 - Alvaro, Antonio T1 - Hydrogen-assisted cracking: A deep learning approach for fractographic analysis N2 - Hydrogen handling equipment suffers from interaction with their operating environment, which degrades the mechanical properties and compromises component integrity. Hydrogen-assisted cracking is responsible for several industrial failures with potentially severe consequences. A thorough failure analysis can determine the failure mechanism, locate its origin, and identify possible root causes to avoid similar events in the future. Postmortem fractographic analysis can classify the fracture mode and determine whether the hydrogen-metal interaction contributed to the component’s breakdown. Experts in fracture classification identify characteristic marks and textural features by visual inspection to determine the failure mechanism. Although widely adopted, this process is time-consuming and influenced by subjective judgment and individual expertise. This study aims to automate fractographic analysis through advanced computer vision techniques. Different materials were tested in hydrogen atmospheres and inert environments, and their fracture surfaces were analyzed by scanning electron microscopy to create an extensive image dataset. A pre-trained Convolutional Neural Network was finetuned to accurately classify brittle and ductile fractures. In addition, Grad-CAM interpretability method was adopted to identify the image regions most influential in the model’s prediction and compare the saliency maps with expert annotations. This approach offered a reliable data-driven alternative to conventional fractographic analysis. KW - Failure analysis KW - Fractographic analysis KW - Hydrogen embrittlement KW - Material compatibility PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-646610 DO - https://doi.org/10.1016/j.commatsci.2025.114366 SN - 0927-0256 VL - 262 SP - 1 EP - 16 PB - Elsevier Science CY - Amsterdam [u.a.] AN - OPUS4-64661 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Nina A1 - Uhlig, Marvin A1 - Kromm, Arne A1 - Schröpfer, Dirk A1 - Höfer, Kevin A1 - Hensel, Jonas A1 - Kannengießer, Thomas T1 - Challenges in the evaluation of the weldability of old mild steels for future use N2 - For reasons of sustainability and cost efficiency, there is an increasing trend in the steel-processing industry to retrofit existing structures, avoiding costly shutdowns or dismantling. Although welding is a cost-effective joining method, it is rarely applied to old steels, whereas riveted or bolted connections are often uneconomical. Repair and refurbishment frequently require the replacement of damaged material or the creation of dissimilar old–new steel joints. Due to the varied manufacturing processes of historical steels, not all twentieth-century steels are inherently weldable, making an initial assessment of weldability essential. In this study, a historical non-deoxidized mild steel (produced by Siemens–Martin processing) originating from the construction of the Berlin Radio Tower (erected in 1926) was investigated using dilatometry to analyze its welding behavior. A database of welding CCT diagrams and HAZ simulations was established to support practice-oriented welding experiments, providing key insights into their weld-metallurgical behavior and weldability. Furthermore, initial welding trials were conducted, and the local residual stress states in dissimilar old–new steel joints were determined. These foundational investigations are critical for the development of innovative, load-adapted welding concepts for the repair and refurbishment of existing old-steel infrastructure in Germany. KW - Old mild steels KW - Repair welding KW - Weldability KW - Thermo-physical simulation KW - CCT diagrams PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-654784 DO - https://doi.org/10.1007/s40194-026-02366-6 SN - 1878-6669 SP - 1 EP - 14 PB - Springer nature AN - OPUS4-65478 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hübner, Martin A1 - Dittmann, Florian A1 - Kromm, Arne A1 - Varfolomeev, Igor A1 - Kannengiesser, Thomas T1 - Enhancement of the fatigue strength by application of a low transformation temperature (LTT) welding consumable N2 - Low transformation temperature (LTT) welding consumables offer a possibility to enhance fatigue strength in welded components without post-treatment. By lowering the martensite start temperature (MS), the volume expansion during transformation near ambient temperature reduces welding related tensile residual stresses in fatigue-critical areas. To evaluate this effect, longitudinal stiffeners were used, a LTT and conventional filler serve as welding consumable, also high frequency mechanical impact (HFMI) treatment was carried out. Three single-pass and six additional-pass sample series were investigated on residual stress and fatigue strength. The additional welds were applied in fatigue crack critical areas with different weld shapes, achieved by varying welding parameters. Mechanical tests on reference samples evaluated the properties of the diluted LTT welds. Although reduced toughness was observed, no fatigue cracks occurred in LTT single-pass weld roots. The fatigue strength at two million cycles increased from 81 MPa to 121 MPa compared to conventional welds, while HFMI reached 146 MPa. With an additional LTT weld pass the results varied from 138 MPa to 196 MPa, depending to the shape and residual stress state. The results show that LTT fillers effectively enhance fatigue performance, and that weld geometry and parameter selection are as critical as the chemical composition for maximizing the LTT effect. CY - Genua, Italy DA - 22.06.2025 KW - Low transformation temperature (LTT) KW - Martensite start temperature KW - Residual stress KW - Longitudenal stiffener KW - Fatigue strength PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-654520 DO - https://doi.org/10.1007/s40194-026-02356-8 SP - 1 EP - 14 PB - Springer Nature AN - OPUS4-65452 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kleba-Ehrhardt, Rafael A1 - Dávila, Josué A1 - Geissler, Johann A1 - Mohr, Gunther A1 - Schmidt, Johannes A1 - Heinze, Christoph A1 - Hilgenberg, Kai A1 - Gurlo, Aleksander A1 - Karl, David T1 - Influence of Haynes 282 powder oxidation on powder properties and component quality in laser powder bed fusion N2 - Reuse of powder in powder bed additive manufacturing is a common practice to enhance sustainability and reduce costs. However, the reusability of metal powder is limited by the oxidation of the powders. Even in a protective atmosphere, each build job leads to gradual oxidation of the powder, which has led to concerns about its impact on powder and part properties. Consequently, strict confidence intervals for oxygen content in nickel-based alloy feedstocks are enforced in the industry. Despite this, there is currently a lack of in-depth studies investigating the specific influence of oxygen on Haynes 282, a widely used nickel-based alloy. This study examines artificially aged Haynes 282 powder batches with oxygen content of 160 ppm, 330 ppm, 1050 ppm, and 1420 ppm. Detailed powder characterization was performed, including morphology, chemical composition, particle size, flowability, and packing behavior. Components were fabricated via PBF-LB/M to evaluate density and mechanical properties. The results showed that higher oxidation levels improved powder flowability and packing density. However, in manufactured parts, irregular melt tracks and increased surface roughness were observed, which could easily be removed by post-processing. No significant differences in density or mechanical properties at room temperature, such as tensile strength and elongation, were found. These findings indicate that H282 powder potentially remains suitable for reuse, even when the batches exhibit increased oxygen content, supporting discussions on revising the existing oxygen content confidence intervals for nickel-based alloys. The results highlight the potential for optimizing recycling strategies and reducing material waste in additive manufacturing processes. KW - Additive manufacturing KW - Powder bed fusion KW - Powder characterization KW - Powder oxidation KW - Powder recycling PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-654545 DO - https://doi.org/10.1016/j.addma.2025.105050 SN - 2214-8604 VL - 116 SP - 1 EP - 16 PB - Elsevier B.V. AN - OPUS4-65454 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Bär, J. A1 - Kanna, N.K. A1 - Duarte, Larissa A1 - Madia, Mauro T1 - Determination of the Kitagawa-Takahashi Diagram using DC Potential Drop Measurements N2 - The Kitagawa-Takahashi Diagram is an important tool for describing the fatigue limit of components containing defects. The models used for its description differ, particularly in the transition region corresponding to the short crack regime. Therefore, for a reliable statement about the fatigue limit in this area, an experimental validation of the models is necessary. However, the standardized staircase method requires a large number of samples and has a long test duration. In this work, a method is presented that allows a simpler and faster validation of the Kitagawa-Takahashi Diagram in the region of short cracks. Rectangular notches with a defined width and depth were manufactured in flat samples of a low-alloyed steel with two different heat treatments using an engraving laser. This method allows a rapid production of very sharp notches without plastic deformation and with only a slight thermal influence on the surrounding material. The samples prepared in this way were fatigued with block wise increasing loads until failure. Cracks are detected by means of a Direct Current Potential Drop method. The length of the loading block (number of cycles) is determined by the measured potential drop. This procedure enables a reliable and precise determination of the limit stress for the respective notch size with low experimental effort and time consumption. The tests have shown that in case of the normalized steel none of the models describes the determined values for the fatigue limit. For the hardened steel, the plot of the fatigue limit as a function of the Murakami parameter √area in combination with the El Haddad model allows a satisfactory description of the measured values. T2 - 5th International Symposium on Fatigue Design and Material Defects CY - Trento, Italy DA - 14.05.2025 KW - Kitagawa-Takahashi diagram KW - Damage tolerance KW - Fatigue KW - Potential drop KW - Fracture mechanics PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-655519 DO - https://doi.org/10.1016/j.prostr.2025.12.283 VL - 76 SP - 27 EP - 34 PB - Elsevier B.V. AN - OPUS4-65551 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dixneit, J. A1 - Gibmeier, J. A1 - Kromm, Arne A1 - Schubnell, J. A1 - Lang, F. A1 - Loebich, F. A1 - Carl, E.-R. A1 - Ya, W. T1 - Residual stress distribution of a large component manufactured by AM-DED-Arc from high-strength weld filler material X90 N2 - Currently, DED-Arc manufactured components are not covered by design guidelines, and design factors such as residual stress factors are not defined for such components. This hinders industrial use, especially for components with a remaining surface waviness required by industry. For the first time the stress state of a high-strength, low-alloy, large-scale DED-Arc component was characterised in the as-built state and after cutting off the component from the substrate plate. Complementary methods of residual stress analyses were applied to gain a holistic insight into the residual stress distributions of a thick-walled part. In the as-built state, direction-dependent and position-dependent tensile residual stresses were found for the component at the level of the yield strength of the part. The additive manufacturing strategy continuous spiral deposition has no significant influence on the residual stresses in bead threshold area compared to the residual stresses of the remaining component. For this case, bead threshold is no structural imperfection. By removing the part from the substrate plate, the residual stresses are significantly redistributed. Tensile residual stresses are then present at a moderate level. Compressive residual stresses were determined in the volume of the deposited material. The general consideration of ‘‘high’’ tensile residual stresses in such thick-walled components is rather conservative. Therefore, design guidelines should take the manufacturing condition into account. KW - AM-DED-Arc KW - Residual stress KW - High strength steel PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-655239 DO - https://doi.org/10.1177/03093247251406876 SN - 2041-3130 SP - 1 EP - 18 PB - SAGE AN - OPUS4-65523 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Gook, Sergej A1 - Biegler, Max A1 - Gumenyuk, Andrey A1 - Rethmeier, Michael T1 - Integration of hybrid laser-arc and narrow gap submerged arc welding for cost-effective joining of 80 mm thick S355ML steel plates N2 - This paper presents the results of developing a cost-effective, robust process for welding thick steel plates. Welding trials were performed on S355ML structural steel plates with a thickness of 80 mm. A specially designed U-shaped joint preparation with a 45 mm root face was proposed to enable thick welds to be welded using a combined technique. In the developed process, a hybrid laser arc weld (HLAW) is performed as the first pass. Subsequently, narrow-gap submerged arc welding (NG-SAW) is applied to the opposite side using a multi-layer technique. The weld cross-section is completed using a reliable overlap of both the HLAW and NG-SAW welds. This method achieves a 2.9-fold reduction in weld volume and filler material consumption, as well as shorter production times for thick-walled welds. Further advantages of the process combination include eliminating the need to form the root of the HLAW weld and the absence of a backing support. The applied process parameters ensure that the maximum heat input does not exceed 5 kJ/mm, leading to uniform hardness across the weld metal and heat-affected zone (HAZ). Impact toughness testing at −40 °C demonstrated excellent performance, with Charpy V-notch energies of 138 ± 45 J in the arc-dominated region and 65 ± 12 J in the critical laser-dominated zone of the HLAW weld. In addition, the NG-SAW weld exhibited an average Charpy V-notch energy of 274 ± 5 J, confirming excellent low-temperature toughness of the fill passes. Owing to its high process stability and practical applicability, the proposed welding approach shows high potential for integration into the fabrication of thick-walled offshore constructions. KW - Hybrid laser arc welding KW - Narrow gap submerged arc welding KW - Low carbon structural steel KW - Fusion zone size KW - Microstructure KW - Impact absorbed energy KW - Hardness PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-655627 DO - https://doi.org/10.1016/j.optlastec.2026.114796 SN - 0030-3992 VL - 197 SP - 1 EP - 12 PB - Elsevier Ltd. AN - OPUS4-65562 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ferrari, Bruno A1 - Fantin, Andrea A1 - Said, D. A1 - Fitch, A. N. A1 - Suárez Ocano, Patricia A1 - Mishurova, Tatiana A1 - Roveda, Ilaria A1 - Kromm, Arne A1 - Darvishi Kamachali, Reza A1 - Bruno, Giovanni A1 - Evans, Alexander A1 - Requena, G. A1 - Agudo Jácome, Leonardo A1 - Serrano Munoz, Itziar T1 - The impact of scanning strategy on cell structures in PBF-LB/M/IN718: an in situ synchrotron x-ray diffraction study N2 - In additive manufacturing, any change of the process parameters, such as scanning strategy, directly affects the cooling rates, heat accumulation, and overall thermal history of the build. Consequently, parts built with different process parameters tend to have different levels of crystallographic texture, residual stress, and dislocation density. These features can influence the properties of the material and their development during post-processing operations. In this study, IN718 prisms were built by laser powder bed fusion (PBF-LB/M) using two different scanning strategies (continuous 67° rotations around the build direction, ROT, and alternating 0°/67° scans, ALT) to provide two different as-built conditions. In situ time-resolved synchrotron diffraction was performed during a solution heat treatment at 1027 °C for 1 h. Ex situ scanning electron microscopy was used to support and complement the in situ observations. An approach to quantify the effect of elemental microsegregation at the cell walls is developed based on the deconvolution of asymmetric γ-nickel matrix peaks. Following this approach, the scanning strategies are shown to affect the as-built fraction of cell walls in the material, resulting in a difference of approximately 5 %, in weight fraction, between ROT and ALT (19 % vs. 24 %, respectively). This microsegregation was observed to be rapidly homogenized during the heating ramp, and no significant changes to the peak shape in the γ peaks occurred during the isothermal part of the heat treatment, regardless of the scanning strategy. KW - Additive manufacturing KW - Inconel 718 KW - Synchrotron x-ray diffraction KW - Heat treatment KW - Laser powder bed fusion KW - Cellular microstructure PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-650958 DO - https://doi.org/10.1016/j.jmrt.2025.11.214 SN - 2238-7854 VL - 41 SP - 593 EP - 608 PB - Elsevier B.V. AN - OPUS4-65095 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Czeskleba, Denis A1 - Rhode, Michael A1 - Wandtke, Karsten A1 - Irfan, Muhammad Dary A1 - Kannengiesser, Thomas T1 - Hydrogen diffusion in thick-walled S690 saw joints: part 1—experimental determination of microstructure-dependent diffusion coefficients N2 - High-strength low-alloyed steel S690 is widely used in heavy-duty applications, such as structural components, mobile cranes, and industrial plant construction, owing to their high strength and weldability. However, thick-plate submerged arc welding (SAW) can introduce elevated hydrogen levels and residual stresses that promote time-delayed hydrogen-assisted cold cracking (HACC). Accurate, microstructure-specific diffusion data are scarce, limiting predictive HACC assessments. This study presents an experimental determination of hydrogen diffusion coefficients (DH) in two S690 variants: thermomechanically rolled (S690MC) and quenched and tempered (S690Q). Multi-layer SAW welds were produced from 30 mm thick plate material at three heat input levels, and diffusion membranes were extracted from weld metal (WM), heat-affected zone (HAZ), and base material (BM). Hydrogen permeation tests, conducted in accordance with DIN En ISO 17081, yielded flux curves normalized in time from which DH was derived using the inflection-point method. At room temperature, DH values ranged from 6 × 10−5 mm2/s to 9 × 10−5 mm2/s across all regions and heat inputs, with no significant difference between S690MC and S690Q. Weld metal exhibited marginally lower DH, attributed to enhanced hydrogen trapping, while base material measurements showed greater variability. These microstructure-resolved diffusion coefficients add quantitative data for modern S690 SAW welds and provide internally consistent input parameters for the numerical simulations presented in part 2. The results support improved parameterization for subsequent assessments of HACC risk through the optimization of welding parameters. KW - Hydrogen assisted cracking KW - Submerged arc welding KW - Diffusion KW - Electrochemical permeation KW - Microstructure PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-655711 DO - https://doi.org/10.1007/s40194-026-02400-7 SN - 0043-2288 SP - 1 EP - 15 PB - Springer Science and Business Media LLC AN - OPUS4-65571 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Czeskleba, Denis A1 - Rhode, Michael A1 - Wandtke, Karsten A1 - Irfan, Muhammad Dary A1 - Kannengiesser, Thomas T1 - Hydrogen diffusion in thick-walled S690 SAW joints: part 2 – predictive modeling of heat input and microstructure influence N2 - High-strength low-alloy (HSLA) steels such as S690 are widely employed in thick-walled welded structures, where hydrogen-assisted cold cracking (HACC) remains a persistent concern. While microstructure-specific hydrogen diffusion coefficients (DH) for weld metal (WM), heat-affected zone (HAZ), and base material (BM) were experimentally established in Part 1 of this study, their quantitative influence on hydrogen accumulation and effusion has not yet been fully clarified. This work presents a transient, spatially resolved numerical model for simulating hydrogen transport in multi-pass submerged arc welds. The model integrates experimentally determined DH values with realistic thermal cycles and temperature-dependent boundary conditions. Developed in Python, the simulation tool is purpose-built for hydrogen diffusion in welded joints. It offers a focused, transparent alternative. It offers a focused, transparent alternative to general-purpose finite element platforms. Parametric analyses demonstrate that, although the diffusion coefficients vary by up to 50%, their impact on overall hydrogen retention is minor. In contrast, plate thickness, bead geometry, cooling time (t₈/₅), and interpass temperature exert a dominant influence on hydrogen distribution. Despite clear microstructural differences between the thermomechanically rolled (S690MC) and quenched and tempered (S690Q) variants, including opposite HAZ hardness responses (softening in S690MC, hardening in S690Q) in the (pen)ultimate weld bead, the simulations confirm that their diffusion behavior and hydrogen solubility are closely aligned. Consequently, differences in DH and solubility exert only a minor influence on hydrogen retention compared to thermal exposure and joint geometry. These findings support the interchangeable use of both steel grades in terms of HACC risk due to hydrogen diffusion kinetics under comparable welding conditions. KW - Hydrogen assisted cracking KW - Numerical simulation KW - Diffusion KW - Submerged arc welding PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-655721 DO - https://doi.org/10.1007/s40194-026-02395-1 SN - 0043-2288 SP - 1 EP - 16 PB - Springer Science and Business Media LLC AN - OPUS4-65572 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -