TY - JOUR A1 - Vollert, F. A1 - Thomas, Maximilian A1 - Kromm, Arne A1 - Gibmeier, J. T1 - Solidification Cracking Assessment of LTT Filler Materials by Means of Varestraint Testing and μCT N2 - Investigations of the weldability of metals often deal with hot cracking, as one of the most dreaded imperfections during weld fabrication. The hot cracking investigations presented in this paper were carried out as part of a study on the development of low transformation temperature (LTT) weld filler materials. These alloys allow to mitigate tensile residual stresses that usually arise during welding using conventional weld filler materials. By this means, higher fatigue strength and higher lifetimes of the weld can be achieved. However, LTT weld filler materials are for example, high-alloyed Cr/Ni steels that are susceptible to the formation of hot cracks. To assess hot cracking, we applied the standardized modified varestraint transvarestraint hot cracking test (MVT), which is well appropriate to evaluate different base or filler materials with regard to their hot cracking susceptibility. In order to consider the complete material volume for the assessment of hot cracking, we additionally applied microfocus X-ray computer tomography (μCT). It is shown that by a suitable selection of welding and MVT parameter the analysis of the complete 3D hot crack network can provide additional information with regard to the hot cracking model following Prokhorov. It is now possible to determine easy accessible substitute values (e.g., maximum crack depth) for the extent of the Brittleness Temperature Range (BTR) and the minimum critical strain Pmin. KW - LTT weld filler materials KW - μCT-analysis KW - Hot cracking KW - Varestraint test PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-509126 DO - https://doi.org/10.3390/ma13122726 VL - 13 IS - 12 SP - 2726 PB - MDPI AN - OPUS4-50912 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Fahrbach, M. A1 - Friedrich, Sebastian A1 - Cappella, Brunero A1 - Peiner, Erwin T1 - Calibrating a high-speed contact-resonance profilometer N2 - A European EMPIR project, which aims to use large-scale piezoresistive microprobes for contact resonance applications, a well-established measurement mode of atomic force microscopes (AFMs), is being funded. As the probes used in this project are much larger in size than typical AFM probes some of the simplifications and assumptions made for AFM probes are not applicable. This study presents a guide on how to systematically create a model that replicates the dynamic behavior of microprobes, including air damping, nonlinear sensitivities, and frequency dependencies. The model is then verified by analyzing a series of measurements. KW - Piezoresistive cantilever KW - AFM KW - contact resonance PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-509899 DO - https://doi.org/10.5194/jsss-9-179-2020 VL - 9 SP - 179 EP - 187 PB - Copernicus Publications AN - OPUS4-50989 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Florian, Camilo A1 - Wonneberger, R. A1 - Undisz, A. A1 - Kirner, Sabrina V. A1 - Wasmuth, Karsten A1 - Spaltmann, Dirk A1 - Krüger, Jörg A1 - Bonse, Jörn T1 - Chemical effects during the formation of various types of femtosecond laser-generated surface structures on titanium alloy N2 - In this contribution, chemical, structural, and mechanical alterations in various types of femtosecond laser-generated surface structures, i.e., laser-induced periodic surface structures (LIPSS, ripples), Grooves, and Spikes on titanium alloy, are characterized by various surface analytical techniques, including X-ray diffraction and glow-discharge optical emission spectroscopy. The formation of oxide layers of the different laser-based structures inherently influences the friction and wear performance as demonstrated in oil-lubricated reciprocating sliding tribological tests (RSTTs) along with subsequent elemental mapping by energy-dispersive X-ray analysis. It is revealed that the fs-laser scan processing (790 nm, 30 fs, 1 kHz) of near-wavelength-sized LIPSS leads to the formation of a graded oxide layer extending a few hundreds of nanometers into depth, consisting mainly of amorphous oxides. Other superficial fs-laser-generated structures such as periodic Grooves and irregular Spikes produced at higher fluences and effective number of pulses per unit area present even thicker graded oxide layers that are also suitable for friction reduction and wear resistance. Ultimately, these femtosecond laser-induced nanostructured surface layers efficiently prevent a direct metal-to-metal contact in the RSTT and may act as an anchor layer for specific wear-reducing additives contained in the used engine oil. KW - Laser-induced oxide layer KW - Laser-induced periodic surface strctures (LIPSS) KW - Femtosecond laser processing KW - Tribology KW - Surface processing PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-505660 DO - https://doi.org/10.1007/s00339-020-3434-7 SN - 0947-8396 SN - 1432-0630 VL - 126 IS - 4 SP - 266 PB - Springer Nature Switzerland AG AN - OPUS4-50566 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Reichelt, Manuel A1 - Cappella, Brunero T1 - Comparative analysis of error sources in the determination of wear volumes of oscillating ball-on-plane tests N2 - The accurate determination of wear volumes is a prerequisite for the study of numerous tribological phenomena. Wear volumes can be measured with different techniques or else be calculated starting from some quantities measured from the wear scar. Advantages and drawbacks of the measuring techniques are shown by means of wear scars and calottes resulting from ball-on-plane tests with 100Cr6 specimens. When measuring wear volumes, white light interferometry results to be one of the most suitable techniques. When wear volumes are calculated, errors result mainly from two sources: (1) the arbitrary choice of one or few line profiles for the determination of the width and of the planimetric wear, and (2) approximations in the calculation, which are even necessary when values of the wear volumes of the single tribological partners and not only the total volume are of interest. The effect of both error sources on the accuracy in the determination of wear volumes is characterized and elucidated by examples. It is found that errors due to approximations are negligible when compared to errors due to the arbitrary choice of one line profile. KW - Error sources analysis KW - White light interferometry KW - Statistical analysis KW - AFM KW - Wear KW - Oscillating ball-on-disc test PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-508407 DO - https://doi.org/10.3389/fmech.2020.00025 VL - 6 SP - Article 25 AN - OPUS4-50840 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schirdewahn, S. A1 - Spranger, Felix A1 - Hilgenberg, Kai A1 - Merklein, M. T1 - Localized Laser Dispersing of Titanium-Based Particles for Improving the Tribological Performance of Hot Stamping Tools N2 - Within the scope of this work, a new surface engineering technology named laser implantation has been investigated, in order to improve the tribological performance of hot stamping tools. This technique is based on manufacturing highly wear-resistant, separated, and elevated microfeatures by embedding hard ceramic particles into the tool surface via pulsed laser radiation. Hence, the topography and material properties of the tool are modified, which influences the thermal and tribological interactions at the blank-die interface. To verify these assumptions and to clarify the cause–effect relations, different titanium-based particles (TiB2, TiC, TiN) were laser-implanted and subsequently analyzed regarding to their geometrical shape and mechanical properties. Afterwards, quenching tests as well as tribological experiments were carried out by using titanium-diboride as the most promising implantation material for reducing the tribological load due to high hardness value of the generated implants. Compared to conventional tooling systems, the modified tool surfaces revealed a significantly higher wear resistance as well as reduced friction forces while offering the possibility to adjust the thermal interactions at the blank-die interface. Based on these results, a tailored tool surface modification can be pursued in future research work, in order to enhance the effectiveness of the hot stamping technology. KW - Hot stamping KW - Tribology KW - Surface modification KW - Localized laser dispersing PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-510981 DO - https://doi.org/10.3390/jmmp4030068 VL - 4 IS - 3 SP - 68 PB - MDPI AN - OPUS4-51098 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Friedrich, Sebastian A1 - Cappella, Brunero T1 - Application of contact-resonance AFM methods to polymer samples N2 - Contact-resonance AFM (CR-AFM) has been used in recent years for the measurement of mechanical properties. Compared with other techniques, CR-AFM has a much shorter acquisition time, compensating the incomplete theoretical understanding of the underlying physical phenomena. In the present paper, we propose a procedure, which allows to determine the elastic modulus of the sample as a parameter of the fit of the CR frequency as a function of the load. It is concluded that CR measurements are not appropriate for polymer samples. Major drawbacks are the bad resolution for moduli lower than ca. 10 GPa and the lack of a comprehensive physical model. KW - Atomic force microscopy KW - Contact resonance KW - Mechanical properties KW - Polymers KW - Wear PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-515621 DO - https://doi.org/10.3762/bjnano.11.154 VL - 11 SP - 1714 EP - 1727 AN - OPUS4-51562 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schirdewahn, S. A1 - Spranger, Felix A1 - Hilgenberg, Kai A1 - Merklein, M. T1 - Localized dispersing of TiB2 and TiN particles via pulsed laser radiation for improving the tribological performance of hot stamping tools N2 - The aim of this study is to increase the tribological performance of hot stamping tools by using a laser implantation process. This technique allows the fabrication of separated, elevated and dome-shaped microfeatures on the tool surface in consequence of a localized dispersing of ceramic particles via pulsed laser radiation. Hence, the topography and material properties of the tool are modified, which influences the tribological interactions at the blank-die interface. However, an appropriate selection of ceramic particles is an essential prerequisite, in order to obtain tailored and highly wear resistant surface features. In this regard, different titanium-based hard particles (TiB2 and TiN) were laser-implanted on hot working tool specimens and subsequently tested by means of a modified pin-on-disk test regarding to their wear and friction behavior. KW - Surface modification KW - Tribology KW - Laser implantation KW - Hot working tool steel KW - Hot stamping PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-514171 DO - https://doi.org/10.1016/j.procir.2020.09.069 VL - 94 SP - 901 EP - 904 PB - Elsevier B.V. AN - OPUS4-51417 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Yu, C.-H. A1 - Peng, R. L. A1 - Luzin, V. A1 - Sprengel, Maximilian A1 - Calmunger, M. A1 - Lundgren, J.-E. A1 - Brodin, H. A1 - Kromm, Arne A1 - Moverare, J. T1 - Thin-wall effects and anisotropic deformation mechanisms of an additively manufactured Ni-based superalloy N2 - Laser powder bed fusion (LPBF) of Ni-based superalloys shows great potential for high temperature applications, for example, as a burner repair application for gas turbines where the thin-walled structure is important. It motivates this work to investigate the evolution of microstructure and the anisotropic mechanical behavior when plate-like specimens are built with a thickness from 4 mm down to 1 mm. By performing texture analysis using neutron diffraction, a clear transition in fiber texture from <011> to <001> is indicated when the specimen becomes thinner. The residual stress shows no thickness dependence, and at the subsurface the residual stress reaches the same level as the yield strength. Due to the rough as-built surface, a roughness compensation method for mechanical properties of thin-walled structures is outlined and demonstrated. Tensile tests from room temperature up to 700 ◦C have been carried out. Anisotropic mechanical behavior is found at all temperatures, which is strongly related to the anisotropic texture evolution. Stronger texture evolution and grain rotations are discovered when the tensile loading is applied along the building direction. The mechanical behavior has been compared to a wrought material, where the high dislocation density and the subgrain structure of the LPBF material result in a higher yield strength. Combining the statistical texture analysis by neutron diffraction with mechanical testing, EBSD grain orientation mapping and the investigation of dislocation structures using transmission electron microscopy, this work illustrates the significance of texture for the thin-wall effect and anisotropic mechanical behavior of LPBF materials. KW - Hastelloy X KW - Hot tensile test KW - Crystallographic texture KW - Roughness KW - Residual stress KW - Dislocation density PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-518759 DO - https://doi.org/10.1016/j.addma.2020.101672 VL - 36 SP - 101672 PB - Elsevier B.V. AN - OPUS4-51875 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Heßmann, Jennifer A1 - Bachmann, Marcel A1 - Hilgenberg, Kai T1 - Numerical and experimental investigation of controlled weld pool displacement by electromagnetic forces for joining dissimilar materials N2 - In order to reduce CO2 emissions, an increasing interest in lightweight construction exists in the automotive industry, especially the multi-material-design approach. The main construction materials here are steels and aluminium alloys. Due to their different physical material properties and limited mutual solubility, these two materials cannot be joined thermally without difficulty. This paper presents a new joining approach for dissimilar materials. It uses electromagnetic displacement of a laser-generated melt pool to produce overlap joints between 1 mm steel (1.0330) and 2 mm aluminium alloy (EN AW 5754). Contactless induced Lorentz forces are generated by an alternating current (AC) magnet system. The controlled displacement of the aluminium alloy melt into the hole of the overlying steel sheet is investigated through numerical and experimental studies. The numerical results are compared with cross sections and thermocouple measurements. For the first time, it is possible to achieve a reproducible controlled melt pool displacement on thin sheets to produce overlap joints between dissimilar materials. KW - Displacement KW - Laser beam welding KW - Dissimilar materials KW - Joining technology KW - Electromagnetic field KW - Lorentz force KW - Numerical investigation PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-516640 DO - https://doi.org/10.3390/met10111447 VL - 10 IS - 11 SP - 1447 EP - 1462 PB - MDPI CY - Basel, Schweiz AN - OPUS4-51664 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Griesche, Axel A1 - Pfretzschner, B. A1 - Taparli, Ugur Alp A1 - Kardjilov, N. T1 - Time-Resolved Neutron Bragg-Edge Imaging: A Case Study by Observing Martensitic Phase Formation in Low Temperature Transformation (LTT) Steel during GTAW N2 - Polychromatic and wavelength-selective neutron transmission radiography were applied during bead-on-plate welding on 5 mm thick sheets on the face side of martensitic low transformation temperature (LTT) steel plates using gas tungsten arc welding (GTAW). The in situ visualization of austenitization upon welding and subsequent α’-martensite formation during cooling could be achieved with a temporal resolution of 2 s for monochromatic imaging using a single neutron wavelength and of 0.5 s for polychromatic imaging using the full spectrum of the beam (white beam). The spatial resolution achieved in the experiments was approximately 200 µm. The transmitted monochromatic neutron beam intensity at a wavelength of λ = 0.395 nm was significantly reduced during cooling below the martensitic start temperature Ms since the emerging martensitic phase has a ~10% higher attenuation coefficient than the austenitic phase. Neutron imaging was significantly influenced by coherent neutron scattering caused by the thermal motion of the crystal lattice (Debye–Waller factor), resulting in a reduction in the neutron transmission by approx. 15% for monochromatic and by approx. 4% for polychromatic imaging. KW - Austenite-to-martensite transformation KW - Neutron radiography KW - Bragg-edge imaging KW - Gas tungsten arc welding (GTAW) KW - Debye–Waller factor KW - Low transformation temperature (LTT) steel PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-538016 DO - https://doi.org/10.3390/app112210886 VL - 11 IS - 22 SP - 10886 PB - MDPI CY - Basel AN - OPUS4-53801 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -