TY - JOUR A1 - Bachmann, Marcel A1 - Meng, Xiangmeng A1 - Artinov, Antoni A1 - Rethmeier, Michael T1 - Elucidation of the Bulging Effect by an Improved Ray-Tracing Algorithm in Deep Penetration Wire Feed Laser Beam Welding and its Influence on the Mixing Behavior N2 - Herein, an improved ray-tracing routine using a virtual mesh refinement approach is adopted in a 3D transientmultiphysics computational fluid Dynamics model for deep penetration wire feed laser beam welding. In a previous study, it was shown that the improved localization of the reflection points of the subrays within the keyhole leads to a more realistic development of the keyhole Depth being validated with experimental results. Another effect investigated in Detail herein is a drastic change in the flow behavior in the weld pool, which promotes the occurrence of a necking area in the solidification line and subsequent bulging under specific circumstances. This has a detrimental effect on the filler material element transport in the weld pool, leading to an inhomogeneous dilution of the added material. The numerical observations are backed up by experimentally obtained data, allowing to provide a clear physics-based explanation of the reduced mixing behavior of the filler wire in the melt pool. KW - Bulging effects KW - Numerical welding simulations KW - Ray-tracing methods KW - Wire feed laser beam welding PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-543322 DO - https://doi.org/10.1002/adem.202101299 SP - 1 EP - 9 PB - Wiley AN - OPUS4-54332 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bachmann, Marcel A1 - Meng, Xiangmeng A1 - Artinov, Antoni A1 - Rethmeier, Michael T1 - Evaluation of narrowed weld pool shapes and their effect on resulting potential defects during deep penetration laser beam welding N2 - This study presents mechanisms of the evolution of a narrowed region in the weld pool center during deep penetration laser beam welding. In numerous numerical studies presented in this study, it was also found that the local reduction of the weld pool size can cause detrimental effects on the melt flow behavior and the resulting properties of the welds. A particularly large influence of this effect was identified in three aspects. First, the local variation of the solidification sequence of the weld pool causes an increase in the hot-cracking susceptibility due to a locally delayed solidification. Second, it was proven that a change in the local length and width of the weld pool is associated with an adverse impact on the potential flow routes of the molten material that induces stronger local variations of its solidification. Thus, the element mixing, e.g., during the welding with filler materials, is blocked. This leads to a non-homogeneous chemical composition of the final weld and can cause undesired effects on the final material properties. Finally, another observed effect is related to the reduced ability of process pores to reach the top surface. As this type of porosity is usually produced around the keyhole tip, the change of the fluid flow regime above this area plays a significant role in determining the final path of the pores until the premature solidification in the middle of the weld pool captures them. This study summarizes mainly numerical results that were supported by selected experimental validation results. KW - Weld pool shape KW - Laser beam welding KW - Solidification KW - Porosity KW - Numerical process simulation PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-557759 DO - https://doi.org/10.2351/7.0000733 SN - 1042-346X VL - 34 IS - 4 SP - 1 EP - 7 PB - Laser Institute of America CY - Orlando, Fla. AN - OPUS4-55775 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Backes, A. T. A1 - Reinmuth-Selzle, K. A1 - Leifke, A. L. A1 - Ziegler, K. A1 - Krevert, C. S. A1 - Tscheuschner, Georg A1 - Lucas, K. A1 - Weller, Michael G. A1 - Berkemeier, T. A1 - Pöschl, U. A1 - Fröhlich-Nowoisky, J. T1 - Oligomerization and Nitration of the Grass Pollen Allergen Phl p 5 by Ozone, Nitrogen Dioxide, and Peroxynitrite: Reaction Products, Kinetics, and Health Effects N2 - The allergenic and inflammatory potential of proteins can be enhanced by chemical modification upon exposure to atmospheric or physiological oxidants. The molecular mechanisms and kinetics of such modifications, however, have not yet been fully resolved. We investigated the oligomerization and nitration of the grass pollen allergen Phl p 5 by ozone (O3), nitrogen dioxide (NO2), and peroxynitrite (ONOO–). Within several hours of exposure to atmospherically relevant concentration levels of O3 and NO2, up to 50% of Phl p 5 were converted into protein oligomers, likely by formation of dityrosine cross-links. Assuming that tyrosine residues are the preferential site of nitration, up to 10% of the 12 tyrosine residues per protein monomer were nitrated. For the reaction with peroxynitrite, the largest oligomer mass fractions (up to 50%) were found for equimolar concentrations of peroxynitrite over tyrosine residues. With excess peroxynitrite, the nitration degrees increased up to 40% whereas the oligomer mass fractions decreased to 20%. Our results suggest that protein oligomerization and nitration are competing processes, which is consistent with a two-step mechanism involving a reactive oxygen intermediate (ROI), as observed for other proteins. The modified proteins can promote pro-inflammatory cellular signaling that may contribute to chronic inflammation and allergies in response to air pollution. KW - Protein KW - Nitrotyrosine KW - Dityrosine KW - Allergy KW - Hay fever KW - Diesel exhaust KW - Combustion KW - Exhaust PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-529729 DO - https://doi.org/10.3390/ijms22147616 VL - 22 IS - 14 PB - MDPI CY - Basel AN - OPUS4-52972 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bacurau, V. P. A1 - Moreira, P. A. F. P. A1 - Bertoli, G. A1 - Andreoli, A. F. A1 - Mazzer, E. A1 - de Assis, F. F. A1 - Gargarella, P. A1 - Koga, G. A1 - Stumpf, G. C. A1 - Figueroa, S. J. A. A1 - Widom, M. A1 - Kaufman, M. A1 - Fantin, Andrea A1 - Cao, Y. A1 - Freitas, R. A1 - Miracle, D. A1 - Coury, F. G. T1 - Comprehensive analysis of ordering in CoCrNi and CrNi2 alloys N2 - Chemical Short-Range Order (CSRO) has attracted recent attention from many researchers, creating intense debates about its impact on material properties. The challenges lie in confirming and quantifying CSRO, as its detection proves exceptionally demanding, contributing to conflicting data in the literature regarding its true effects on mechanical properties. Our work uses highprecision calorimetric data to unambiguously prove the existence and, coupled with atomistic simulations, quantify the type of CSRO. This methodology allows us to propose a mechanism for its formation and destruction based on the heat evolution during thermal analysis and facilitates a precise identification of local ordering in CoCrNi alloys. Samples of CoCrNi (Co33Cr33Ni33) and CrNi2 (Cr33Ni66) alloys are fabricated in varying ordered states, extensively characterized via synchrotron X-ray diffraction, X-ray absorption spectroscopy, and transmission electron microscopy. Samples with considerably different ordered states are submitted to tensile tests with in-situ synchrotron X-ray diffraction. We demonstrate, despite inducing varied CSRO levels in CoCrNi, no significant alterations in overall mechanical behavior emerge. However, the CrNi2 alloy, which undergoes long-range ordering, experiences significant shifts in yield strength, ultimate tensile stress and ductility. KW - Mechanical properties KW - Short-range ordering KW - Calorimetry PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-611075 DO - https://doi.org/10.1038/s41467-024-52018-w VL - 15 IS - 1 SP - 1 EP - 11 PB - Springer Science and Business Media LLC AN - OPUS4-61107 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Baensch, Franziska A1 - Baer, Wolfram A1 - Wossidlo, Peter A1 - Habib, Abdel Karim T1 - Damage evolution detection in a pipeline segment under bending by means of acoustic emission N2 - A steel pipeline segment of 2.5 m length was subjected to quasi-static four-point bending load in three steps for studying the initial cracking and damage accumulation based on the Acoustic Emission (AE) technique and by the direct current potential drop (DCPD) technique. For the latter, a new post-test analysis method was established. AE is found more sensitive to crack initiation than DCPD. Formation of mesoscopic and macroscopic cracks as well as their closure and the resulting friction generate weighted peak frequencies below 400 kHz, whereas microscopic cracking produces AE with broad band spectra identifiable by weighted peak frequencies above 400 kHz. Critical states alike the maximum load level and the leak opening were accompanied by peak amplitudes above 85 dBAE. This rather fundamental study provides a data base for possibly developing advanced strategies of detection and alarm systems based on acoustic monitoring of pipelines, or at least, steel structures. KW - Crack KW - Accoustic emission KW - Frequency domain KW - Potential drop technique KW - Fracture PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-565171 DO - https://doi.org/10.1016/j.ijpvp.2022.104863 SN - 0308-0161 VL - 201 IS - 104863 SP - 1 EP - 9 PB - Elsevier Science CY - Amsterdam AN - OPUS4-56517 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Baer, Wolfram T1 - Chunky graphite in ferritic spheroidal graphite cast iron: Formation, prevention, characterization, impact on properties – An overview N2 - Ferritic spheroidal graphite cast iron (SGI) materials have a remarkable technical poten-tial and economic impact in modern industry. These features are closely related to the question of how the cast materials can be produced without structural defects and graphite degenerations such as for example chunky graphite. Although the chunky graphite degeneration superficially seems to be well known, its metallurgical background is still controversially discussed, appropriate field-tested non-destructive tools for its quantification in castings are lacking and the knowledge on its impact on material properties is fairly limited. Addressing this status, the article is providing a current overview on the subject. Existing theories on formation and growth mechanisms of chunky graphite are briefly reviewed. Furthermore, from a metallurgical point of view, causes for the appearance of chunky graphite as well as preventive measures are concisely summarized. Particular attention is paid to the morphology of chunky graphite and how it can be characterized by destructive and non-destructive techniques. Special emphasis was laid on providing a comprehensive overview on the impact of chunky graphite on strength, ductility, fatigue limit, fatigue crack growth rate as well as fracture tough-ness of ferritic SGI materials based on experimental data. Moreover, conclusions for the assessment of castings affected by chunky graphite are drawn. KW - Characterization KW - Ferritic spheroidal graphite cast iron KW - Chunky graphite KW - Properties KW - Formation KW - Prevention PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-499972 DO - https://doi.org/10.1007/s40962-019-00363-8 SN - 1939-5981 SN - 2163-3193 VL - 14 IS - 2 SP - 454 EP - 488 PB - Springer Verlag AN - OPUS4-49997 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Baer, Wolfram A1 - Wossidlo, Peter T1 - Validation of a low blow specimen technique for R-curve determination using a drop tower N2 - Fracture mechanics based component design requires appropriate fracture mechanics toughness data with respect to both, loading rate as well as test temperature. Taking high-rate loading into account such as with accidental scenarios, different standards such as ASTM E 1820 or BS 7448-3 provide some information on dynamic fracture mechanics testing. Nevertheless, the designations differ so that a validation of the own material specific test method used for dynamic R-curve determination is mandatory. In order to address this for ductile cast iron materials an experimental method for the reliable determination of dynamic J-integral crack resistance curves at -40 °C following the multiple specimen approach has been established and validated. The experimental concept offers some additional valuable features. Single values of dynamic crack initiation toughness can be determined using a single specimen technique based on crack sensors. Furthermore, an experimentally independent method is provided according to which CTOD δ5 R-curves can be established. The focus of the present paper is on the validation of the experimental low blow technique using a drop tower test system. A drop tower test system was developed and set up to perform low blow tests at temperatures down to -40 °C. The system allows for a variation of the impact mass and height and was optimized for testing of ductile cast iron at stress intensity rates from approximately 5∙10⁴ to 3∙10⁵ MPa√ms⁻¹. This range of loading rate is characteristic for instance with crash scenarios of heavy sectioned DCI casks for radioactive materials. In order to address characteristic challenges of impact tests (test duration of microseconds up to milliseconds, inertial effects, signal oscillations), an appropriate full bridge strain gage method for the measurement of force directly on the specimen as well as a non-contact measurement of load line displacement using an optical extensometer have been developed and validated. The low blow test requires either to prevent bouncing strikes of the hammer by using the stop block technique or to catch the hammer after its first strike. Both options are not part of the experimental concept and setup which have been realized here. The paper describes investigations which have been performed in order to make sure that bouncing strikes of the hammer do not cause additional crack extension in the specimen. This is necessary to ensure a unique relation between the work done and the achieved crack extension. The investigations covered the analysis of limit loads of the specimen with respect to the measured force. The measured stiffness of the specimen was assessed and signals of crack sensors were analyzed. Furthermore, an analysis of the mechanical behavior of the loading system and the specimen by optical observation was performed. Corresponding results are discussed in the paper. It had finally been proven that additional crack extension in the specimen due to bouncing strikes of the hammer is not to be expected under the given conditions of test setup, material and loading. It can be seen as a major experimental advantage that the striker does not have to be catched after the low blow test. T2 - XXIV Italian Group of Fracture Conference CY - Urbino, Italy DA - 01.03.2017 KW - Dynamic fracture mechanics KW - R-curve KW - Low blow KW - Ductile cast iron PY - 2017 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-437686 DO - https://doi.org/10.1016/j.prostr.2017.04.005 SN - 2452-3216 VL - 3 SP - 25 EP - 32 AN - OPUS4-43768 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Baeßler, Matthias A1 - Simon, Patrick T1 - Ballasted track on vibrating bridge decks: physical mechanisms, empirical findings, and a proposal for assessment N2 - This paper summarizes the key findings and physical mechanisms and provides information on open questions and the assessment of railway bridge superstructure vibrations. Bridges are classic disruption points on a railway track. If bridge superstructures are dynamically excited by train traffic, the vertical accelerations of the track must be considered. For a ballasted track, this can lead to the destabilization of the ballast track, as the bridge superstructure acts like a vibrating table. In this respect, the paper explains in more detail what is meant by destabilization, when this destabilization occurs and how various influencing parameters such as acceleration amplitude, the vibration sequence and frequency affect its occurrence. In the InBridge4EU project, gaps in knowledge such as the effect of single impulse loads are being investigated experimentally. A new test facility has been set up for this purpose, the initial results of which are presented here. An essential element in the assessment of this scenario is the stability of the track under high compression forces with simultaneous dynamic excitation of the superstructure. A new approach for the assessment of bridge vibrations with respect to lateral stability is presented. KW - Railway bridge dynamics KW - Bridge deck acceleration KW - Ballast destabilization KW - Lateral track stability KW - Track buckling PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-630972 DO - https://doi.org/10.1142/S0219455425400243 SN - 0219-4554 SN - 1793-6764 IS - 2540024 SP - 1 EP - 27 PB - World Scientific CY - Singapore AN - OPUS4-63097 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Baglo, K. A1 - Sauermoser, M. A1 - Lid, M. A1 - Paschke, T. A1 - Bin Afif, A. A1 - Lunzer, M. A1 - Bock, Robert A1 - Steinert, M. A1 - Flaten, A. A1 - Torgersen, J. T1 - Overcoming the transport limitations of photopolymer-derived architected carbon N2 - Photopolymer derived carbon grows in popularity, yet the range in available feature sizes is limited. Here we focus on expanding the field to low surface to volume ratio (SVR) structures. We describe a high temperature acrylic photopolymerizable precursor with FTIR and DSC and develop a thermal inert-gas treatment for producing architected carbon in the mm scale with SVR of 1.38 x10-3 μm-1. Based on TGA and MS, we distinguish two thermal regimes with activation energies of ~79 and 169 kJ mol-1, which we reason with mechanisms during the polymer’s morphologic conversion between 300 - 500 °C. The temperature range of the major dimensional shrinkage (300-440 °C, 50%) does not match the range of the largest alteration in elemental composition (440-600 °C, O/C 0.25-0.087%). The insights lead to an optimized thermal treatment with an initial ramp (2 °C min-1 to 350 °C), isothermal hold (14h), post hold ramp (0.5 °C min-1 to 440 °C) and final ramp (10 °C min-1 to 1000 °C). The resulting carbon structures are dimensionally stable, non-porous at the μm scale, and comprise an unprecedented variation in feature sizes (from mm to μm scale). The findings shall advance architected carbon to industrially relevant scales. KW - Carbon KW - Photopolymer KW - Transport limitations KW - Porous materials KW - Additive manufacturing PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-575038 DO - https://doi.org/10.1002/admt.202300092 SN - 2365-709X SP - 2300092 PB - Wiley-VCH GmbH AN - OPUS4-57503 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bakir, Nasim A1 - Artinov, Antoni A1 - Gumenyuk, Andrey A1 - Bachmann, Marcel A1 - Rethmeier, Michael T1 - Numerical simulation on the origin of solidification cracking in laser welded thick-walled structures N2 - One of the main factors affecting the use of lasers in the industry for welding thick structures is the process accompanying solidification cracks. These cracks mostly occurring along the welding direction in the welding center, and strongly affect the safety of the welded components. In the present study, to obtain a better understanding of the relation between the weld pool geometry, the stress distribution and the solidification cracking, a three-dimensional computational fluid dynamic (CFD) model was combined with a thermo-mechanical model. The CFD model was employed to analyze the flow of the molten metal in the weld pool during the laser beam welding process. The weld pool geometry estimated from the CFD model was used as a heat source in the thermal model to calculate the temperature field and the stress development and distributions. The CFD results showed a bulging region in the middle depth of the weld and two narrowing areas separating the bulging region from the top and bottom surface. The thermo-mechanical simulations showed a concentration of tension stresses, transversally and vertically, directly after the solidification during cooling in the region of the solidification cracking. T2 - 27TH INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS - METAL 2018 CY - Brno, Czech Republic DA - 23.05.2018 KW - Laser beam welding KW - Weld pool KW - Full penetration KW - Finite element method (FEM) KW - CFD model KW - Numerical simulation KW - Solidification cracking PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-450595 DO - https://doi.org/10.3390/met8060406 SN - 2075-4701 VL - 8 IS - 6 SP - 406, 1 EP - 15 PB - MDPI CY - Basel, Switzerland AN - OPUS4-45059 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -