TY - JOUR A1 - Ringleb, F. A1 - Andree, Stefan A1 - Heidmann, B. A1 - Bonse, Jörn A1 - Eylers, K. A1 - Ernst, O. A1 - Boeck, T. A1 - Schmid, M. A1 - Krüger, Jörg T1 - Femtosecond laser-assisted fabrication of chalcopyrite micro-concentrator photovoltaics N2 - Micro-concentrator solar cells offer an attractive way to further enhance the efficiency of planar-cell technologies while saving absorber material. Here, two laser-based bottom-up processes for the fabrication of regular arrays of CuInSe2 and Cu(In,Ga)Se2 microabsorber islands are presented, namely one approach based on nucleation and one based on laser-induced forward transfer. Additionally, a procedure for processing these microabsorbers to functioning micro solar cells connected in parallel is demonstrated. The resulting cells show up to 2.9% efficiency and a significant efficiency enhancement under concentrated Illumination. KW - Chalcopyrite KW - Femtosecond laser patterning KW - Laser-induced forward transfer KW - Micro-concentrator solar cell KW - Photovoltaics PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-470026 DO - https://doi.org/10.3762/bjnano.9.281 SN - 2190-4286 VL - 9 SP - 3025 EP - 3038 PB - Beilstein-Institut zur Förderung der Chemischen Wissenschaften CY - Frankfurt, M. AN - OPUS4-47002 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Keller, Julia A1 - Moldenhauer, Daniel A1 - Byrne, L. A1 - Haase, H. A1 - Resch-Genger, Ute A1 - Koch, Matthias T1 - Complexes of the mycotoxins citrinin and ochratoxin A with aluminum ions and their spectroscopic properties N2 - The sensitive detection of the mycotoxin citrinin (CIT) utilizing ist fluorescence requires approaches to enhance the emission. In this respect, we studied the complexation of CIT and ochratoxin A (OTA) with Al3+ in methanol using absorption and fluorescence spectroscopy. In this context, an isocratic high performance liquid chromatography (HPLC) method using a polymer column and a fluorescence detector was also developed that enables the separation of the metal ion complexes from the free ligands and non-complexed Al3+. CIT and OTA showed distinct changes in their absorption and fluorescence properties upon Al3+-coordination, and the fluorescence of CIT was considerably enhanced. Analysis of the photometrically assessed titration of CIT and OTA with Al3+ using the Job plot method revealed 1:2 and 1:1 stoichiometries for the Al3+ complexes of CIT (Al:CIT) and OTA (Al:OTA), respectively. In the case of CIT, only one -diketone moiety participates in Al3+ coordination. These findings can be elegantly exploited for signal amplification and provide the base to reduce the limit of detection for CIT quantification by about an order of magnitude, as revealed by HPLC measurements using a fluorescence detector. KW - Complexation KW - Aluminum KW - Fluorescence KW - Job plot KW - HPLC-DAD/FLD PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-470502 DO - https://doi.org/10.3390/toxins10120538 SN - 2072-6651 VL - 10 IS - 12 SP - 538, 1 EP - 8 PB - MDPI CY - Basel AN - OPUS4-47050 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Brunner-Schwer, C. A1 - Kersting, R. A1 - Graf, B. A1 - Rethmeier, Michael T1 - Laser-plasma-cladding as a hybrid metal deposition-technology applying a SLM-produced copper plasma nozzle N2 - Laser-Metal-Deposition (LMD) and Plasma-Transferred-Arc (PTA) are well known Technologies which can be used for cladding purposes. The prime objective in combining LMD and PTA as a Hybrid Metal Deposition-Technology (HMD) is to achieve high Deposition rates at low thermal Impact. Possible applications are coatings for wear protection or repair welding for components made of steel. The two energy sources (laser and Plasma arc) build a Joint process Zone and are configurated to constitute a stable process at laser powers between 0.4-1 kW (defocused) and Plasma currents between 75-200 A. Stainless steel 316L serves as filler material. For this HMD process, a Plasma Cu-nozzle is designed and produced by powder bed based Selective Laser Melting. The potential of the HMD Technology is investigated and discussed considering existing process. This paper demonstrates how the interaction of the two energy sources effects the following application-relevant properties: Deposition rate, powder Efficiency and energy Input. T2 - LANE 2018 CY - Fürth, Germany DA - 3.09.2018 KW - Laser-metal-deposition KW - Plasma-transferred-arc KW - SLM printed plasma torch KW - Laser-plasma hybrid PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-470999 UR - 10.1016/j.procir.2018.08.020 DO - https://doi.org/10.1016/j.procir.2018.08.020 SN - 2212-8271 VL - CIRP 74 SP - 738 EP - 742 PB - Sciencedirect CY - Berlin AN - OPUS4-47099 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Emteborg, H. A1 - Florian, D. A1 - Choquette, S. A1 - Ellison, S. L. R. A1 - Fernandes-Whaley, M. A1 - Mackay, L. A1 - McCarron, P. A1 - Panne, Ulrich A1 - Sander, S. G. A1 - Kim, S.-K. A1 - Held, A. A1 - Linsinger, T. A1 - Trapmann, S. T1 - Cooperation in publicly funded reference material production N2 - The meeting was organised by the European Commission’s Joint Research Centre and held at the JRC-Geel site on 22–23 February 2018. It was a follow-up of a similar meeting held in 2009. The objective of the meeting was to exchange information about ongoing publicly funded reference material (RM) production, identify areas of interest for future specific RMs, including certified reference material (CRM) developments, investigate potential areas of collaboration, and to identify areas which may be of a lower importance in the future for a specific RM producer. The benefit of exchanging such information is to avoid duplication of efforts in RM production, make better use of public funds by potentially matching competencies, and to address problems that are common to publicly funded RM producers. T2 - Meeting regarding cooperation in publicly funded reference material production, European Commission's Joint Research Centre CY - Geel, Belgium DA - 22.02.2018 KW - Public funding KW - Reference materials PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-470206 DO - https://doi.org/10.1007/s00769-018-1349-1 SN - 0949-1775 SN - 1432-0517 VL - 23 IS - 6 SP - 371 EP - 377 PB - Springer CY - Berlin AN - OPUS4-47020 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schneider, Ronald T1 - Effect of repair models on risk based optimal inspection strategies for support structures of offshore wind turbines N2 - Owners or operators of offshore wind farms perform inspections to collect information on the condition of the wind turbine support structures and perform repairs if required. These activities are costly and should be optimized. Risk-based methods can be applied to identify inspection and repair strategies that ensure an optimal balance between the expected total service life cost of inspection and repair, and the achieved risk reduction. Such an optimization requires explicit modeling of repairs. In this paper, the impact of different repair models on the results of a risk-based optimization of inspection and repair strategies is quantified in a numerical example considering a jacket-type steel frame subject to high-cycle fatigue. The example showed that, in this specific application, there is no need for detailed modeling of the behavior of repaired welded connections. T2 - 5th International Conference on Smart Monitoring, Assessment and Rehabilitation of Civil Structures (SMAR 2019) CY - Potsdam, Germany DA - 27.08.2019 KW - Risk KW - Reliability KW - Inspection planning KW - Offshore wind turbines PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-488297 UR - https://www.smar2019.org/Portals/smar2019/bb/Th.2.A.4.pdf SP - Paper Th.2.A.4, 1 EP - 8 AN - OPUS4-48829 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zhang, Q. A1 - Zheng, M. A1 - Huang, Y. A1 - Kunte, Hans-Jörg A1 - Wang, X. A1 - Liu, Y. A1 - Zheng, C. T1 - Long term corrosion estimation of carbon steel, titanium and its alloy in backfill material of compacted bentonite for nuclear waste repository N2 - The container of high-level radioactive waste (HLRW) being in deep geological disposal, the backfill material is needed to serve as the second defense for HLRW and the highly compacted bentonite is generally selected. As the time goes, the underground water will infiltrate the backfill, causing the corrosion of materials for the building of containers in the formed electrolyte. Carbon steel, titanium and its alloy are the potential candidate materials for the fabrication of HLRW containers. The current investigation aims at assessing the safety of HLRW container in deep geological disposal for hundreds of thousands of years and facilitating the material selection for future Container fabrication by estimating their corrosion behavior in compacted bentonite with a series of moisture content at different temperatures through electrochemical methods including open circuit potential (OCP), electrochemical impedance spectroscopy (EIS) and potentiodynamic polarization curve (PC) measurements. The corrosion rates were estimated for a carbon steel, a pure titanium and a titanium alloy in compacted Gaomiaozi Bentonite infiltrated with simulated underground water in Beishan area of China over an expected disposal period up to 106 years respectively, showing that titanium and its alloy are more reliable materials for building HLRW containers than carbon steel. KW - Issues KW - Disposal KW - Performance KW - Moisture KW - Lifetime KW - Water KW - Model PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-492413 DO - https://doi.org/10.1038/s41598-019-39751-9 SN - 2045-2322 VL - 9 SP - 3195 PB - Nature Publishing Group AN - OPUS4-49241 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Brüngel, R. A1 - Rückert, J. A1 - Wohlleben, W. A1 - Babick, F. A1 - Ghanem, A. A1 - Gaillard, C. A1 - Mech, A. A1 - Rauscher, H. A1 - Hodoroaba, Vasile-Dan A1 - Weigel, S. A1 - Friedrich, C. M. T1 - NanoDefiner e-Tool: An Implemented Decision Support Framework for Nanomaterial Identification N2 - The European Commission’s recommendation on the definition of nanomaterial (2011/696/EU) established an applicable standard for material categorization. However, manufacturers face regulatory challenges during registration of their products. Reliable categorization is difficult and requires considerable expertise in existing measurement techniques (MTs). Additionally, organizational complexity is increased as different authorities’ registration processes require distinct reporting. The NanoDefine project tackled these obstacles by providing the NanoDefiner e-tool: A decision support expert system for nanomaterial identification in a regulatory context. It providesMT recommendations for categorization of specific materials using a tiered approach (screening/confirmatory), and was constructed with experts from academia and industry to be extensible, interoperable, and adaptable for forthcoming revisions of the nanomaterial definition. An implemented MT-driven material categorization scheme allows detailed description. Its guided workflow is suitable for a variety of user groups. Direct feedback and explanation enable transparent decisions. Expert knowledge is Held in a knowledge base for representation of MT performance criteria and physicochemical particle type properties. Continuous revision ensured data quality and validity. Recommendations were validated by independent case studies on industry-relevant particulate materials. Besides supporting material identification and registration, the free and open-source e-tool may serve as template for other expert systems within the nanoscience domain. KW - EC nanomaterial definition KW - Decision support KW - Expert system KW - Nanomaterial KW - Nanoparticles PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-492449 DO - https://doi.org/10.3390/ma12193247 VL - 12 IS - 19 SP - 3247 PB - MDPI CY - Basel, CH AN - OPUS4-49244 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Reimann, C. A1 - Kaufmann, Jan Ole A1 - Adams, L. C. A1 - Onthank, D. C. A1 - Thöne-Reineke, C. A1 - Robinson, S. P. A1 - Hamm, B. A1 - Botnar, R. M. A1 - Makowski, M. R. T1 - Dual-probe molecular MRI for the in vivo characterization of atherosclerosis in a mouse model: Simultaneous assessment of plaque inflammation and extracellular-matrix remodeling N2 - Molecular MRI is a promising in-vivo modality to detect and quantify morphological and molecular vessel-wall changes in atherosclerosis. The combination of different molecular biomarkers may improve the risk stratification of patients. This study aimed to investigate the feasibility of simultaneous visualization and quantification of plaque-burden and inflammatory activity by dual-probe molecular MRI in a mouse-model of progressive atherosclerosis and in response-to-therapy. Homozygous apolipoprotein E knockout mice (ApoE−/−) were fed a high-fat-diet (HFD) for up to four-months prior to MRI of the brachiocephalic-artery. To assess response-to-therapy, a statin was administered for the same duration. MR imaging was performed before and after administration of an elastin-specific gadolinium-based and a macrophage-specific iron-oxide-based probe. Following in-vivo MRI, samples were analyzed using histology, immunohistochemistry, inductively-coupled-mass-spectrometry and laser-inductively-coupled-mass-spectrometry. In atherosclerotic-plaques, intraplaque expression of elastic-fibers and inflammatory activity were not directly linked. While the elastin-specific probe demonstrated the highest accumulation in advanced atherosclerotic-plaques after four-months of HFD, the iron-oxide-based probe showed highest accumulation in early atherosclerotic-plaques after two-months of HFD. In-vivo measurements for the elastin and iron-oxide-probe were in good agreement with ex-vivo histopathology (Elastica-van-Giesson stain: y = 298.2 + 5.8, R2 = 0.83, p < 0.05; Perls‘ Prussian-blue-stain: y = 834.1 + 0.67, R2 = 0.88, p < 0.05). Contrast-to-noise-ratio (CNR) measurements of the elastin probe were in good agreement with ICP-MS (y = 0.11x-11.3, R² = 0.73, p < 0.05). Late stage atherosclerotic-plaques displayed the strongest increase in both CNR and gadolinium concentration (p < 0.05). The gadolinium probe did not affect the visualization of the iron-oxide-probe and vice versa. This study demonstrates the feasibility of simultaneous assessment of plaque-burden and inflammatory activity by dual-probe molecular MRI of progressive atherosclerosis. The in-vivo detection and quantification of different MR biomarkers in a single scan could be useful to improve characterization of atherosclerotic-lesions. KW - In-vivo KW - Molecular MRI PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-492514 DO - https://doi.org/10.1038/s41598-019-50100-8 VL - 9 IS - 1 SP - Article number: 13827 PB - Nature AN - OPUS4-49251 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Fletcher, D. C. A1 - Hunter, R. A1 - Xia, W. A1 - Smales, Glen Jacob A1 - Pauw, Brian Richard A1 - Blackburn, E. A1 - Kulak, A. A1 - Xin, H. A1 - Schnepp, Z. T1 - Scalable synthesis of dispersible iron carbide (Fe3C) nanoparticles by ‘nanocasting’ N2 - Metal carbides have shown great promise in a wide range of applications due to their unique catalytic, electrocatalytic and magnetic properties. However, the scalable production of dispersible metal carbide nanoparticles remains a challenge. Here, we report a simple and scalable route to dispersible iron carbide (Fe3C) nanoparticles. This uses MgO nanoparticles as a removable ‘cast’ to synthesize Fe3C nanoparticles from Prussian blue (KFeIII[FeII(CN)6]). Electron tomography demonstrates how nanoparticles of the MgO cast encase the Fe3C nanoparticles to prevent sintering and agglomeration during the high-temperature synthesis. The MgO cast is readily removed with ethylenediaminetetraacetic acid (EDTA) to generate Fe3C nanoparticles that can be used to produce a colloidal ferrofluid or dispersed on a support material. KW - Small-angle scattering KW - SAXS KW - Metal carbides KW - Nanoparticles KW - Nanocasting PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-486295 DO - https://doi.org/10.1039/C9TA06876G SN - 2050-7488 SN - 2050-7496 VL - 7 IS - 33 SP - 19506 EP - 19512 PB - Royal Society of Chemistry (RSC) AN - OPUS4-48629 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Geißler, Daniel A1 - Wegmann, Marc A1 - Jochum, T. A1 - Somma, V. A1 - Sowa, M. A1 - Scholz, J. A1 - Fröhlich, E. A1 - Hoffmann, Katrin A1 - Niehaus, J. A1 - Roggenbuck, D. A1 - Resch-Genger, Ute T1 - An automatable platform for genotoxicity testing of nanomaterials based on the fluorometric γ-H2AX assay reveals no genotoxicity of properly surface-shielded cadmium-based quantum dots N2 - The large number of nanomaterial-based applications emerging in the materials and life sciences and the foreseeable increasing use of these materials require methods that evaluate and characterize the toxic potential of these nanomaterials to keep safety risks to people and environment as low as possible. As nanomaterial toxicity is influenced by a variety of parameters like size, shape, chemical composition, and surface chemistry, high throughput screening (HTS) platforms are recommended for assessing cytotoxicity. Such platforms are not yet available for genotoxicity testing. Here, we present first results obtained for application-relevant nanomaterials using an automatable genotoxicity platform that relies on the quantification of the phosphorylated histone H2AX (γ-H2AX) for detecting DNA double strand breaks (DSBs) and the automated microscope system AKLIDES® for measuring integral fluorescence intensities at different excitation wavelengths. This platform is used to test the genotoxic potential of 30 nm-sized citrate-stabilized gold nanoparticles (Au-NPs) as well as micellar encapsulated iron oxide nanoparticles (FeOx-NPs) and different cadmium (Cd)-based semiconductor quantum dots (QDs), thereby also searching for positive and negative controls as reference materials. In addition, the influence of the QD shell composition on the genotoxic potential of these Cd-based QDs was studied, using CdSe cores as well as CdSe/CdS core/shell and CdSe/CdS/ZnS core/shell/shell QDs. Our results clearly revealed the genotoxicity of the Au-NPs and its absence in the FeOx-NPs. The genotoxicity of the Cd-QDs correlates with the shielding of their Cd-containing core, with the core/shell/shell architecture preventing genotoxicity risks. The fact that none of these nanomaterials showed cytotoxicity at the chosen particle concentrations in a conventional cell viability assay underlines the importance of genotoxicity studies to assess the hazardous potential of nanomaterials. KW - Nanomaterial KW - Genotoxicity testing KW - γ-H2AX assay KW - Quantum dot PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-486318 DO - https://doi.org/10.1039/C9NR01021A SN - 2040-3372 SN - 2040-3364 VL - 11 IS - 28 SP - 13458 EP - 13468 PB - The Royal Society of Chemistry AN - OPUS4-48631 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -