TY - CONF A1 - Nehrig, Marko A1 - Scheidemann, Robert A1 - Wille, Frank A1 - Ballheimer, Viktor T1 - Investigation of the internal impact during a 9 m drop test of an accident-safe waste package N2 - The safety assessment of packages for the transport of radioactive material follows the IAEA regulations and guidance. The specified regulatory tests cover severe accidents and demonstrate the package containment system integrity. Special attention must be drawn to the behaviour of the content which could move inside the package due to unpreventable gaps caused by the loading procedure and the structure of the content. A possible internal impact of the content which occurs during the drop tests onto the lid system is investigated. The IAEA regulations SSR-6 and the Guidance SSG-26, revised recently, consider input from Germany and France related to the significance of internal gaps. In the context of a waste package design assessment, a model was equipped with a representative content to conduct a drop test with an internal impact. The weight and kinetic impact of this content covered all possible real contents. The objective of the test was to maximize the load onto the lid system and to prove the mechanical integrity by complying with the required leak tightness. The test was conducted conservatively at a package temperature lower than -40 °C at the BAM Test Site Technical Safety. This paper gives an overview of efforts to address internal gaps and their consequences, and the BAM efforts with the implementation of this topic into IAEA regulations and guidance material. The paper then focuses on the conduction of a drop test and investigation of internal component impact. T2 - ASME 2021 Pressure Vessels & Piping Conference (PVP2021) CY - Online meeting DA - 13.07.2021 KW - Internal gaps KW - Drop test KW - IAEA PY - 2021 SN - 978-0-7918-8535-2 DO - https://doi.org/10.1115/PVP2021-60996 SP - 1 EP - 6 PB - American Society of Mechanical Engineers (ASME) CY - New York, NY, USA AN - OPUS4-54742 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Nehrig, Marko T1 - Investigation of the internal impact during a 9 m drop test of an accident-safe waste package N2 - The safety assessment of packages for the transport of radioactive material follows the IAEA regulations and guidance. The specified regulatory tests cover severe accidents and demonstrate the package containment system integrity. Special attention must be drawn to the behaviour of the content which could move inside the package due to unpreventable gaps caused by the loading procedure and the structure of the content. A possible internal impact of the content which occurs during the drop tests onto the lid system is investigated. The IAEA regulations SSR-6 and the Guidance SSG-26, revised recently, consider input from Germany and France related to the significance of internal gaps. In the context of a waste package design assessment, a model was equipped with a representative content to conduct a drop test with an internal impact. The weight and kinetic impact of this content covered all possible real contents. The objective of the test was to maximize the load onto the lid system and to prove the mechanical integrity by complying with the required leak tightness. The test was conducted conservatively at a package temperature lower than -40 °C at the BAM Test Site Technical Safety. This paper gives an overview of efforts to address internal gaps and their consequences, and the BAM efforts with the implementation of this topic into IAEA regulations and guidance material. The paper then focuses on the conduction of a drop test and investigation of internal component impact. T2 - ASME 2021 Pressure Vessels & Piping Conference (PVP2021) CY - Online meeting DA - 13.07.2021 KW - Drop test KW - Internal gaps KW - IAEA PY - 2021 AN - OPUS4-54744 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weber, Mike A1 - Völzke, Holger A1 - Zencker, Uwe A1 - Herz, A. A1 - Kreienmeyer, M. T1 - Design of a Drop Test Target with Reproducible Properties for Konrad Prototype Testing N2 - Beginning in 1976 the former iron ore mine Konrad was geologically investigated concerning its suitability as a location for a German final repository for low and intermediate level waste. After a comprehensive licensing procedure it was approved and is now being prepared and equipped for the planned start of storage in 2027. At the end of the 1980s, the requirements for waste containers for storage in this repository were defined for the first time on the basis of an incident analysis of the on-site handling procedures, beginning with the unloading of the packages after the arrival at the site up to the final positioning in the underground storage galleries. A 5-meter drop onto the rock ground of the mine was identified as the covering case for high mechanical requirements (ABK II container class). In contrast to the 9-meter drop according to the IAEA Regulations for the Safe Transport of Radioactive Material, the 5-meter drop is performed onto a hard but not essentially unyielding target. The container is typically not protected by an impact limiter. The requirements for a potential test facility are described in the regulations for the Konrad repository. The mechanical strength of the target is defined as a concrete strength equivalent to the identified properties of the rock ground of the mine. Since 1991 BAM has consistently used precast reinforced concrete slabs as target for drop tests in the framework of licensing procedures as well as in research projects. While the original design fulfilled the requirement for the integrity of the concrete slab in most cases, it failed when drop tests onto an edge of a container were performed. A redesigned concrete slab developed in a research project and suggested as a reference target in 2009 has been successfully used in Konrad licensing procedures since then. The paper gives a brief overview of the historical development and it describes BAM’s efforts and approaches to continuously guarantee a concrete slab of defined quality and to provide a test setup for valid drop tests from the applicants and the authorities view. T2 - PATRAM 2022, 20th International Symposium on the Packaging and Transportation of Radioactive Materials CY - Juan-les-Pins, France DA - 11.06.2023 KW - Target KW - Drop test KW - Final repository Konrad PY - 2023 SP - 1 EP - 11 AN - OPUS4-58563 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weber, Mike T1 - Design of a Drop Test Target with Reproducible Properties for Konrad Prototype Testing N2 - Beginning in 1976 the former iron ore mine Konrad was geologically investigated concerning its suitability as a location for a German final repository for low and intermediate level waste. After a comprehensive licensing procedure it was approved and is now being prepared and equipped for the planned start of storage in 2027. At the end of the 1980s, the requirements for waste containers for storage in this repository were defined for the first time on the basis of an incident analysis of the on-site handling procedures, beginning with the unloading of the packages after the arrival at the site up to the final positioning in the underground storage galleries. A 5-meter drop onto the rock ground of the mine was identified as the covering case for high mechanical requirements (ABK II container class). In contrast to the 9-meter drop according to the IAEA Regulations for the Safe Transport of Radioactive Material, the 5-meter drop is performed onto a hard but not essentially unyielding target. The container is typically not protected by an impact limiter. The requirements for a potential test facility are described in the regulations for the Konrad repository. The mechanical strength of the target is defined as a concrete strength equivalent to the identified properties of the rock ground of the mine. Since 1991 BAM has consistently used precast reinforced concrete slabs as target for drop tests in the framework of licensing procedures as well as in research projects. While the original design fulfilled the requirement for the integrity of the concrete slab in most cases, it failed when drop tests onto an edge of a container were performed. A redesigned concrete slab developed in a research project and suggested as a reference target in 2009 has been successfully used in Konrad licensing procedures since then. The paper gives a brief overview of the historical development and it describes BAM’s efforts and approaches to continuously guarantee a concrete slab of defined quality and to provide a test setup for valid drop tests from the applicants and the authorities view. T2 - PATRAM 2022, 20th International Symposium on the Packaging and Transportation of Radioactive Materials CY - Juan-les-Pins, France DA - 11.06.2023 KW - Final repository Konrad KW - Drop test KW - Target PY - 2023 AN - OPUS4-58564 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weber, Mike T1 - Design of a Drop Test Target with Reproducible Properties for Konrad Prototype Testing N2 - Beginning in 1976 the former iron ore mine Konrad was geologically investigated concerning its suitability as a location for a German final repository for low and intermediate level waste. After a comprehensive licensing procedure it was approved and is now being prepared and equipped for the planned start of storage in 2027. At the end of the 1980s, the requirements for waste containers for storage in this repository were defined for the first time on the basis of an incident analysis of the on-site handling procedures, beginning with the unloading of the packages after the arrival at the site up to the final positioning in the underground storage galleries. A 5-meter drop onto the rock ground of the mine was identified as the covering case for high mechanical requirements (ABK II container class). In contrast to the 9-meter drop according to the IAEA Regulations for the Safe Transport of Radioactive Material, the 5-meter drop is performed onto a hard but not essentially unyielding target. The container is typically not protected by an impact limiter. The requirements for a potential test facility are described in the regulations for the Konrad repository. The mechanical strength of the target is defined as a concrete strength equivalent to the identified properties of the rock ground of the mine. Since 1991 BAM has consistently used precast reinforced concrete slabs as target for drop tests in the framework of licensing procedures as well as in research projects. While the original design fulfilled the requirement for the integrity of the concrete slab in most cases, it failed when drop tests onto an edge of a container were performed. A redesigned concrete slab developed in a research project and suggested as a reference target in 2009 has been successfully used in Konrad licensing procedures since then. The paper gives a brief overview of the historical development and it describes BAM’s efforts and approaches to continuously guarantee a concrete slab of defined quality and to provide a test setup for valid drop tests from the applicants and the authorities view. T2 - ASME 2023 Pressure Vessels & Piping Conference (PVP2023) CY - Atlanta, GA, USA DA - 16.07.2023 KW - Final repository Konrad KW - Drop test KW - Target PY - 2023 AN - OPUS4-58565 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weber, Mike T1 - Consequences of an Imperfectly Mounted Reinforcement Cage in a Cylindrical Concrete Container During Mechanical Specimen Tests N2 - In 2007 the license for the German Konrad repository for low and intermediate level radioactive waste was finally confirmed. Since then, the site is improved, prepared and equipped for the currently planned start of waste package emplacement in 2029. Bundesanstalt fuer Materialforschung und -pruefung is regularly contracted by the Bundesgesellschaft für Endlagerung as the responsible authority for waste product control, waste container design testing, and waste package acceptance. In this context BAM is mainly responsible for design testing of various container types including the evaluation of quality assurance measures for container manufacturing. In addition to general requirements concerning container design, the casks have to withstand specific mechanical load scenarios. Drop tests from different heights under consideration of the most damaging drop orientation and a stacking test are two examples for necessary safety demonstrations. If the containers are made from concrete the reinforcement has the function to absorb tensile forces the concrete is not able to withstand by its own. Because of manufacturing imperfections of cylindrical concrete containers manufactured already decades ago, the reinforcement cages are not always exactly, asymmetrically positioned when they were poured. This inspired BAM to perform various ABAQUS® finite-element (FE) simulations by using the example of a simplified cylindrical container design with generic dimensions. On the basis of the calculated tensile and compressive stress distributions suggestions are derived on how a cylindrical concrete container with an imperfectly placed reinforcement cage has to be oriented for a drop or stacking test to ensure the most damaging test scenario. T2 - RAMTRANS 2024 CY - London, United Kingdom DA - 14.05.2024 KW - Finite-element-analysis KW - Container design testing procedure KW - Reinforced concrete containers KW - Drop test KW - Stacking test KW - Imperfectly mounted reinforcement cage PY - 2024 AN - OPUS4-60120 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weber, Mike T1 - Consequences of an imperfectly mounted reinforcement cage in a generical cylindrical concrete container during mechanical specimen tests N2 - By highest court decision in 2007 the issued license for the Konrad repository (a former iron ore mine) for low and intermediate level radioactive waste was finally confirmed. Since then, the site is improved, prepared and equipped for the currently planned start of waste package emplacement by 2029. The Bundesanstalt fuer Materialforschung und -pruefung (BAM, Federal Institute for Materials Research and Testing) is regularly contracted by the Bundesgesellschaft für Endlagerung (BGE, Federal Company for Radioactive Waste Disposal) as the responsible authority for waste product control, waste container design testing, and waste package acceptance. In this context BAM is mainly responsible for design testing of various container types including the evaluation quality assurance measures for container manufacturing. In the written Konrad disposal requirements [1] [2], all acceptance criteria for potential final disposal containers are defined. In addition to general requirements concerning container design, materials, dimensions and others, specific mechanical load scenarios the casks have to withstand are derived from an analysis of the on-site handling and emplacement procedures. Drop tests from different heights under consideration of the most damaging drop orientation and a stacking test are two examples for safety demonstrations that have to be performed during the container design testing procedure to qualify the respective container type. The containers, whether cubic or cylindrical containers, can be made from different materials like ductile cast iron, reinforced concrete or as welded construction from steel plates and profiles. In case of concrete containers the reinforcement has the function to absorb tensile forces the concrete is not able to withstand by its own. Because of manufacturing imperfections of cylindrical concrete waste containers manufactured already decades ago, the reinforcement cages are not always exactly, axisymmetrically positioned when they were poured. This inspired BAM to perform various ABAQUS finite-element (FE) simulations [3] by using the example of a simplified cylindrical container design with generic dimensions and pure elastic material properties. As outcome the stress conditions in the container during the drop test impact under different drop positions and during the stacking test were investigated and are explained and illustrated in this contribution. Different reinforcement cage positions were calculated and compared. On the basis of the calculated tensile and compressive stress distributions suggestions are derived on how a cylindrical concrete container with an imperfectly placed reinforcement cage has to be oriented for a drop or stacking test to ensure the most damaging test scenario. T2 - ASME 2024 Pressure Vessels & Piping Conference CY - Bellevue, Washington, USA DA - 28.07.2024 KW - Container design testing procedure KW - Reinforced concrete containers KW - Drop test KW - Stacking test KW - Imperfectly mounted reinforcement cage KW - Finite-element-analysis PY - 2024 AN - OPUS4-62560 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Weber, Mike A1 - Völzke, Holger A1 - Nieslony, Gregor T1 - Consequences of an imperfectly mounted reinforcement cage in a generical cylindrical concrete container during mechanical specimen tests N2 - By highest court decision in 2007 the issued license for the Konrad repository (a former iron ore mine) for low and intermediate level radioactive waste was finally confirmed. Since then, the site is improved, prepared and equipped for the currently planned start of waste package emplacement by 2029. The Bundesanstalt fuer Materialforschung und -pruefung (BAM, Federal Institute for Materials Research and Testing) is regularly contracted by the Bundesgesellschaft für Endlagerung (BGE, Federal Company for Radioactive Waste Disposal) as the responsible authority for waste product control, waste container design testing, and waste package acceptance. In this context BAM is mainly responsible for design testing of various container types including the evaluation quality assurance measures for container manufacturing. In the written Konrad disposal requirements all acceptance criteria for potential final disposal containers are defined. In addition to general requirements concerning container design, materials, dimensions and others, specific mechanical load scenarios the casks have to withstand are derived from an analysis of the on-site handling and emplacement procedures. Drop tests from different heights under consideration of the most damaging drop orientation and a stacking test are two examples for safety demonstrations that have to be performed during the container design testing procedure to qualify the respective container type. The containers, whether cubic or cylindrical containers, can be made from different materials like ductile cast iron, reinforced concrete or as welded construction from steel plates and profiles. In case of concrete containers the reinforcement has the function to absorb tensile forces the concrete is not able to withstand by its own. Because of manufacturing imperfections of cylindrical concrete waste containers manufactured already decades ago, the reinforcement cages are not always exactly, axisymmetrically positioned when they were poured. This inspired BAM to perform various ABAQUS finite-element (FE) simulations by using the example of a simplified cylindrical container design with generic dimensions and pure elastic material properties. As outcome the stress conditions in the container during the drop test impact under different drop positions and during the stacking test were investigated and are explained and illustrated in this contribution. Different reinforcement cage positions were calculated and compared. On the basis of the calculated tensile and compressive stress distributions suggestions are derived on how a cylindrical concrete container with an imperfectly placed reinforcement cage has to be oriented for a drop or stacking test to ensure the most damaging test scenario. T2 - ASME 2024 Pressure Vessels & Piping Conference CY - Bellevue, Washington, USA DA - 28.07.2024 KW - Container design testing procedure KW - Reinforced concrete containers KW - Drop test KW - Stacking test KW - Imperfectly mounted reinforcement cage KW - Finite-element-analysis PY - 2024 SN - 978-0-7918-8851-3 DO - https://doi.org/10.1115/PVP2024-123797 VL - 5 SP - 1 EP - 8 PB - ASME CY - New York City, USA AN - OPUS4-62558 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gleim, Tobias T1 - Fracture Mechanical Investigations on a Welding Seam of a Thick-Walled Transport Package N2 - Untersuchung einer Schweißnaht mit verschiedenen Codes. Vergleiche von experimentellen und numerischen Ergebnissen T2 - Technical Exchange IRSN – BAM: Transport & Storage of Packages for Radioactive Material CY - Cadarache, France DA - 13.10.2022 KW - Drop test KW - Fracture initiation KW - Transport package PY - 2022 AN - OPUS4-56055 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Quercetti, Thomas A1 - Wille, Frank A1 - Neumann, Martin A1 - Linnemann, Konrad ED - Baraldi, P. ED - Di Maio, F. ED - Zio, E. T1 - Safety Evaluation of a Package for Radioactive Waste by Full-Scale Drop Testing N2 - As part of the evaluation of a package for the safe transport of radioactive waste the regulations of the IAEA International Atomic Energy Agency shall be fulfilled. The regulations define requirements for the package and specify mechanical and thermal test conditions. Different methods are allowed for the test performance to demonstrate compliance with the regulations. Next to calculational approaches and the use of models of an appropriate scale, the performance of full-scale testing with prototype packages respectively full-scale models is applied. The use of full-scale models has several advantages within the complete safety assessment procedure for a transport package approval. Scaling and corresponding similarity questions don’t have to be considered, additional material investigations can be limited and analyses to transfer test results to the original package design are reduced in number and complexity. Additionally, experience for future serial design procedures can be built up during manufacturing and assembling of the test model. BAM operates different drop and fire test facilities south of Berlin, Germany. BAM has started to perform a drop test campaign with a full-scale model of 120 metric tons weight for a transport package approval procedure. The paper describes experience with test preparation, drop performance and additional analyses. The measurement concept is explained and test goals regarding the package safety assessment and evaluation of safety margins are introduced. T2 - 30th European Safety and Reliability Conference and 15th Probabilistic Safety Assessment and Management Conference (ESREL2020 PSAM15) CY - Online meeting DA - 01.11.2020 KW - Slap-down KW - Transport safety KW - Package KW - Drop test KW - Similarity KW - FEA KW - Radioactive waste PY - 2020 UR - https://www.rpsonline.com.sg/proceedings/esrel2020/html/3809.xml SN - 987-981-14-8593-0 SP - Paper 3809,1 EP - 8 PB - Research Publishing Services CY - Singapore AN - OPUS4-50981 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gleim, Tobias A1 - Neumann, Martin A1 - Linnemann, Konrad A1 - Komann, Steffen A1 - Wille, Frank T1 - Fracture Mechanical Analyses of a Welding Seam of a Thick-Walled Transport Package N2 - Transport packages shall satisfy various safety criteria regarding mechanical, thermal and radiation phenomena. Typical requirements focusing mechanical aspects are usually drop tests in accordance with IAEA regulations. The drop tests are usually carried out experimentally and, as an additional measure, finite element analyses (FEA) are performed. A specific part of the investigations presented is the evaluation of the welding seam connecting cask shell and cask bottom. Experimental results and FEA are presented and compared. The evaluation of the welding seam performed includes a variety of aspects. In addition to the experimental and analytical stresses determined, different standards are used to investigate a possible crack initiation. Several destructive and non-destructive tests are performed for quality assurance in the manufacturing process as well as for different input parameters. The necessary monitoring and non-destructive measurement methods to define the boundary conditions of the standards are introduced. Taking into account all required parameters, the welding seam is examined and evaluated using the failure assessment diagrams (FAD) of the respective standards. It can be shown under the given boundary conditions that considering the experimental data, the welding seam is in the context of crack initiation below the enveloping curve in the acceptable region. More critical drop tests to be conducted are proposed and need to be investigated in future work. T2 - Pressure Vessels & Piping Conference® 2022 CY - Las Vegas, NV, USA DA - 17.07.2022 KW - Transport package KW - Drop test KW - Fracture initiation PY - 2022 SP - 1 EP - 9 AN - OPUS4-55375 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Gleim, Tobias A1 - Komann, Steffen T1 - Fracture Mechanical Analyses of a Welding Seam of a Thick-Walled Transport Package N2 - Transport packages shall satisfy various safety criteria regarding mechanical, thermal and radiation phenomena. Typical requirements focusing mechanical aspects are usually drop tests in accordance with IAEA regulations [1]. The drop tests are usually carried out experimentally and, as an additional measure, finite element analyses (FEA) are performed. A specific part of the investigations presented is the evaluation of the welding seam connecting cask shell and cask bottom. Experimental results and FEA are presented and compared. The evaluation of the welding seam performed includes a variety of aspects. In addition to the experimental and analytical stresses determined, different standards are used to investigate a possible crack initiation. Several destructive and non-destructive tests are performed for quality assurance in the manufacturing process as well as for different input parameters. The necessary monitoring and non-destructive measurement methods to define the boundary conditions of the standards are introduced. Taking into account all required parameters, the welding seam is examined and evaluated using the failure assessment diagrams (FAD) of the respective standards. It can be shown under the given boundary conditions that considering the experimental data, the welding seam is in the context of crack initiation below the enveloping curve in the acceptable region. More critical drop tests to be conducted are proposed and need to be investigated in future work. T2 - Pressure Vessels & Piping Conference® 2022 CY - Las Vegas, NV, USA DA - 17.07.2022 KW - Drop test KW - Fracture initiation KW - Transport package PY - 2022 AN - OPUS4-55374 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -