TY - CONF A1 - Klein, Ulrich T1 - Messing unter Druck N2 - Schäden an verschiedenen Rohrverbindungs-Systemen im Sanitärbereich mit Bauteilen aus Messing. T2 - GfKORR Arbeitskreis Schadensanalyse CY - Frankfurt a.M., Germany DA - 17.10.2019 KW - Pressverbindung KW - Spannungsrisskorrosion KW - Messing KW - Schadensanalyse PY - 2019 AN - OPUS4-49335 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kauss, Norman A1 - Heyn, A. A1 - Halle, T. A1 - Rosemann, Paul T1 - Detection of sensitisation on aged lean duplex stainless steel with different electrochemical methods N2 - Ageing at 600 °C (from 0.1 h up to 20 h) leads to the formation of precipitations at the ferrite-ferrite (α/α) and ferrite-austenite (α/γ) grain boundaries of the lean duplex stainless steel (LDSS) X2CrNiN22-2. This leads to sensitisation due to chromium depletion and decreased pitting corrosion resistance proven by the results of various electrochemical methods (DL-EPR and determination of CPT, Epit). These results were compared with the KorroPad method, which uses an agar-based gel-electrolyte for the detection of stainless steel surfaces prone to pitting corrosion. However, the standard configuration of the KorroPad showed no differentiation for the various ageing conditions. Therefore, modified versions of the KorroPad with two, five and ten times higher NaCl and potassium ferrocyanide III (K3[Fe(CN)6]) concentrations were successfully used to visualise the behaviour detected by DL-EPR, Epit and CPT. Therefore, the KorroPad method can also detect a microstructure related reduction of pitting corrosion resistance, which can drastically reduce the experimental effort to generate sensitisation diagrams for stainless steels. KW - Lean duplex KW - Stainless steel KW - Sensitisation KW - Polarisation KW - Critical pitting temperature KW - Pitting corrosion KW - KorroPad KW - Ageing treatment PY - 2019 DO - https://doi.org/10.1016/j.electacta.2019.05.081 SN - 0013-4686 SN - 1873-3859 VL - 317 SP - 17 EP - 24 PB - Elsevier AN - OPUS4-48374 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kauss, Norman A1 - Heyn, A. A1 - Halle, T. A1 - Rosemann, P. T1 - Detektion von Sensibilisierung am nichtrostenden Lean-Duplex-Stahl 1.4062 mit verschiedenen elektrochemischen Methoden N2 - Vergleich von EPR, EKrit, CPT und KorroPad zur Ermittlung von Sensibilisierung an dem bei 600 °C gealterten Lean Duplex 1.4062. T2 - Korrosionsuntersuchung und -überwachung" und "Grundlagen und Simulation" CY - Dusseldorf, Germany DA - 21.11.2019 KW - Lean Duplex KW - Sensibilisierung KW - Lochkorrosion KW - EPR KW - KorroPad KW - Altern PY - 2019 AN - OPUS4-50180 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kauss, Norman A1 - Heyn, A. A1 - Halle, T. A1 - Rosemann, P. T1 - Detektion von Sensibilisierung am nichtrostenden Lean-Duplex-Stahl 1.4062 mit verschiedenen elektrochemischen Methoden N2 - Vorstellung von EPR, Ekrit, CPT und KorroPad zur Erfassung von Sensibilisierung am Lean Duplex 1.4062 an verschieden wärmebehandelten Zuständen. T2 - GfKORR-Arbeitskreis "Korrosion und Korrosionsschutz von Eisen und Stahl" CY - Duisburg, Germany DA - 12.12.2019 KW - Lean Duplex KW - Sensibilisierung KW - Lochkorrosion KW - EPR KW - KorroPad KW - Altern PY - 2019 AN - OPUS4-50182 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kamaraj, Abinaya A1 - Erning, Johann Wilhelm A1 - Reimann, S. A1 - Ahrens, A. T1 - Susceptibility of 304 stainless steel to crevice corrosion in electrochemically active fluids N2 - The susceptibility of AISI 304 stainless steel to crevice corrosion on the effect of contact with electrochemically active fluids was investigated using exposure and stepwise potentiostatic polarisation. Crevice materials made up of 304 SS and Polyether ether ketone (PEEK) forming two kinds of crevices including 304 SS-to-PEEK and 304 SS-to-304 SS were tested. T2 - NACE International Corrosion Conference 2019 CY - Nashville, TN, USA DA - 24.03.2019 KW - Steel KW - Crevice KW - Corrosion KW - ECA KW - Stainless PY - 2019 SP - Paper 12868 PB - NACE International CY - Houston AN - OPUS4-49286 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kamaraj, Abinaya A1 - Erning, Johann Wilhelm A1 - Reimann, S. A1 - Ahrens, A. T1 - Susceptibility of 304 stainless steel to crevice corrosion in electrochemically active fluids N2 - The susceptibility of AISI 304 stainless steel to crevice corrosion on the effect of contact with electrochemically active fluids was investigated using exposure and stepwise potentiostatic polarisation. Crevice materials made up of 304 SS and Polyether ether ketone (PEEK) forming two kinds of crevices including 304 SS-to-PEEK and 304 SS-to-304 SS were tested. T2 - Corrosion 2019 NACE CY - Nashville, TN, USA DA - 24.03.2019 KW - Desinfection KW - Crevice corrosion KW - ECA PY - 2019 AN - OPUS4-49284 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hlavacek, Petr A1 - Reinemann, Steffi A1 - Gluth, Gregor A1 - Ebell, Gino A1 - Mietz, Jürgen ED - Serdar, M. ED - Stirmer, N. ED - Provis, J. T1 - Behaviour of reinforced alkali-activated fly ash mortars under leaching conditions N2 - Corrosion of steel reinforcement in concrete is one of the major deterioration mechanisms limiting the service life of reinforced concrete structures. While for conventional (Portland cement-based) concretes a great amount of experience exists in this regard, the factors that determine the onset of reinforcement corrosion in alkali-activated materials are incompletely understood yet. One aspect of corrosion protection is leaching and the accompanying changes of the concrete pore solution. In the present study, alkali-activated fly ash mortars with embedded carbon steel rebars were exposed to de-ionised water for periods up to 330 days, and the electrochemical response of the steel (free corrosion potential, polarisation resistance), the alteration of the mortar (ohmic resistance, mechanical strength, pore size distribution) as well as the pore solution composition were monitored. Although substantial alkali leaching was observed, the pH of the pore solution remained at values sufficient to protect the embedded steel from depassivation. The mortar did not exhibit indications of significant deterioration. Thus, the present results suggest that leaching is not critical for protection of steel reinforcement in alkali-activated fly ash mortars and concretes. T2 - International Conference on Sustainable Materials, Systems and Structures (SMSS 2019) CY - Rovinj, Croatia DA - 20.03.2019 KW - Alkali-activated materials KW - Steel corrosion KW - Leaching PY - 2019 SN - 978-2-35158-223-7 VL - 1 SP - 118 EP - 124 PB - RILEM Publications CY - Paris AN - OPUS4-47585 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Hlavacek, Petr A1 - Ebell, Gino A1 - Gluth, Gregor A1 - Reinemann, Stefi A1 - Mietz, Jürgen A1 - Kühne, Hans-Carsten T1 - Betonstahlkorrosion in Geopolymerbetonen bei Angriff von Kohlenstoffdioxid und Chlorid N2 - Der kritische, Korrosion auslösende Chloridgehalt für die Beurteilung der Korrosions-beständigkeit von Betonstahl in Geopolymerbetonen ist von großer Bedeutung für die Dauerhaftigkeitsprognose für bewehrte Elemente aus solchen Materialien. Es sind kaum experimentelle Daten in der Fachliteratur vorhanden und die vorliegenden Werte unterscheiden sich zwischen den Studien erheblich. In diesem Projekt wurde der kritische, Korrosion auslösende Chloridgehalt für Betonstahl (BSt 500) in flugaschebasierten (Ca-armen) Geopolymermörtel für verschiedene Beaufschlagungskombinationen bestimmt: Chloridbeaufschlagung mit 1 M NaCl-Lösung; Auslaugen in entionisiertem Wasser und anschließende Chloridbeaufschlagung im 1 M NaCl-Lösung; Auslaugen in entionisiertem Wasser, Carbonatisierung in Luft bei 20 °C und natürlicher CO2 Konzentration und anschließende Chloridbeaufschlagung mit 1 M NaCl-Lösung. Für Referenz-Zwecke wurde zusätzlich der Korrosion auslösende Chloridgehalt für eine Portland-Zement Mischung bei Auslagerung in 1 M NaCl-Lösung bestimmt. KW - Korrosion KW - Geopolymer PY - 2019 SP - 1 EP - 83 AN - OPUS4-49752 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hlavacek, Petr A1 - Reinemann, Steffi A1 - Gluth, Gregor A1 - Ebell, Gino A1 - Mietz, Jürgen T1 - Behaviour of reinforced alkali-activated fly ash mortars under leaching conditions N2 - Corrosion of steel reinforcement in concrete is one of the major deterioration mechanisms limiting the service life of reinforced concrete structures. While for conventional (Portland cement-based) concretes a great amount of experience exists in this regard, the factors that determine the onset of reinforcement corrosion in alkali-activated materials are incompletely understood yet. One aspect of corrosion protection is leaching and the accompanying changes of the concrete pore solution. In the present study, alkali-activated fly ash mortars with embedded carbon steel rebars were exposed to de-ionised water for periods up to 330 days, and the electrochemical response of the steel (free corrosion potential, polarisation resistance), the alteration of the mortar (ohmic resistance, mechanical strength, pore size distribution) as well as the pore solu¬tion composition were monitored. Although substantial alkali leaching was observed, the pH of the pore solution remained at values sufficient to protect the embedded steel from depassivation. The mortar did not exhibit indications of significant deterioration. Thus, the present results suggest that leaching is not critical for pro¬tec¬tion of steel reinforcement in alkali-activated fly ash mortars and concretes. T2 - International Conference on Sustainable Materials, Systems and Structures (SMSS 2019) CY - Rovinj, Croatia DA - 20.03.2019 KW - Alkali-activated materials KW - Leaching KW - Steel corrosion PY - 2019 AN - OPUS4-47621 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Heise, Svenja A1 - Babutzka, Martin A1 - Burkert, Andreas T1 - Normentwurf für ein Prüfverfahren zur Bestimmung von Deckschichtwiderständen an Zinküberzügen mittels gelartiger Elektrolyte (WIPANO - GELELEK) N2 - Der Vortrag stellt das WIPANO-Vorhaben GELELEK vor. Zu Beginn wird die Problemstellung und Projektidee kurz erläutert. Anschließend wird ein Überblick über die Projektpartner, Projektziele und Arbeitsschritte gegeben, sowie die ausgewählten Probenbleche vorgestellt. Abschließend wurde noch eine Einladung zur Teilnahme am projektbegleitenden Ausschuss ausgesprochen. T2 - Sitzung des GAV-Forschungsbeirates CY - Iserlohn, Germany DA - 18.09.2019 KW - Deckschichtbildung KW - Gelartige Elektrolyte KW - Korrosion KW - Zinküberzüge PY - 2019 AN - OPUS4-49038 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Harnisch, J. A1 - Dauberschmidt, C. A1 - Ebell, Gino A1 - Mayer, T. T1 - The new DGZfP Specification B12 "Corrosion Monitoring of Reinforced Concrete Structures" N2 - The corrosion of steel in reinforced concrete structures is one of the main threats to their durability. Based on the scientific achievements of the past decades the knowledge about the deterioration mechanisms and possible repair strategies for corrosion induced damages have found their way into practice. It is common sense, that a detailed assessment of the structure is the foundation for a successful repair measure. In addition to the “traditional” singular on-site-procedures such as measurement of concrete cover, carbonation depth, half-cell potentials and chloride contents the monitoring of corrosion related parameters has gained in importance over the past few years. The advantages of a corrosion monitoring are obvious. In new buildings, structural elements which cannot be assessed after completion (e.g. tunnel segments), or members with electrically isolating coatings can be monitored by means of integrated sensors providing an insight into the development of crucial parameters such as electrochemical potentials, corrosion currents and the electrical resistivity of the concrete. A less known but very beneficial field of application is the use of corrosion monitoring as an integral part of a repair measure based on principles such as the cathodic protection of steel in concrete (CP) or increasing the electrical resistivity of the concrete (IR). By implementing a corrosion monitoring system, it is possible to survey the time dependent effect of the repair measure on the corrosion process which may lead to a confirmation of successful repair measure or to a modification of the repair strategy. As the principle of cathodic protection for steel in concrete is a recognized repair measure today, the number of applications increases steadily and thus increasing the relevance for corrosion monitoring. Nevertheless, no standards or guidelines concerning the corrosion monitoring are available in Germany today, making it difficult to implement corrosion monitoring in common practice. With this in mind an international task group formed to develop the specification B12 “Corrosion Monitoring of Reinforced and Prestressed Concrete Structures” published by the German Society for Non-Destructive Testing, DGZfP, spring 2018. This paper will present the new specification B12 by highlighting the basic measurement principles and illustrating the potentials of corrosion monitoring for new and existing concrete structures by means of case studies. T2 - SMAR 2019 CY - Potsdam, Germany DA - 27.08.2019 KW - Monitoring KW - Corrosion KW - Concrete structures PY - 2019 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-487980 SP - We.4.A.1, 1 PB - SMAR 2019 AN - OPUS4-48798 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Harnisch, J. A1 - Dauberschmidt, C. A1 - Ebell, Gino A1 - Meyer, T. T1 - The new DGZfP Specification B12 N2 - The corrosion of steel in reinforced concrete structures is one of the main threats to their durability. Based on the scientific achievements of the past decades the knowledge about the deterioration mechanisms and possible repair strategies for corrosion induced damages have found their way into practice. It is common sense, that a detailed assessment of the structure is the foundation for a successful repair measure. In addition to the “traditional” singular on-site-procedures such as measurement of concrete cover, carbonation depth, half-cell potentials and chloride contents the monitoring of corrosion related parameters has gained in importance over the past few years. The advantages of a corrosion monitoring are obvious. In new buildings, structural elements which cannot be assessed after completion (e.g. tunnel segments), or members with electrically isolating coatings can be monitored by means of integrated sensors providing an insight into the development of crucial parameters such as electrochemical potentials, corrosion currents and the electrical resistivity of the concrete. A less known but very beneficial field of application is the use of corrosion monitoring as an integral part of a repair measure based on principles such as the cathodic protection of steel in concrete (CP) or increasing the electrical resistivity of the concrete (IR). By implementing a corrosion monitoring system, it is possible to survey the time dependent effect of the repair measure on the corrosion process which may lead to a confirmation of successful repair measure or to a modification of the repair strategy. As the principle of cathodic protection for steel in concrete is a recognized repair measure today, the number of applications increases steadily and thus increasing the relevance for corrosion monitoring. Nevertheless, no standards or guidelines concerning the corrosion monitoring are available in Germany today, making it difficult to implement corrosion monitoring in common practice. With this in mind an international task group formed to develop the specification B12 “Corrosion Monitoring of Reinforced and Prestressed Concrete Structures” published by the German Society for Non-Destructive Testing, DGZfP, spring 2018. This paper will present the new specification B12 by highlighting the basic measurement principles and illustrating the potentials of corrosion monitoring for new and existing concrete structures by means of case studies. T2 - SMAR 2019 CY - Potsdam, Germany DA - 27.08.2019 KW - Corrosion KW - Monitoring PY - 2019 AN - OPUS4-48805 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Faes, W. A1 - Lecompte, S. A1 - van Bael, J. A1 - Salenbien, R. A1 - Bäßler, Ralph A1 - Bellemans, I. A1 - Cools, P. A1 - de Geyter, N. A1 - Morent, R. A1 - Verbeken, K. A1 - de Paepe, M. T1 - Corrosion behaviour of different steel types in artificial geothermal fluids N2 - Geothermal energy is an interesting alternative to polluting fossil energy sources. Therefore, in Belgium, two wells have been drilled for a deep geothermal power plant. However, the environment to which the installations are exposed is challenging. The geothermal brine has 165 g/l total dissolved solids (of which 90% are sodium and chlorine) and the production temperature can be up to 130 °C. To assess their suitability to be used in a geothermal power plant, the corrosivity of the artificial brine to three common construction materials was investigated with exposure and electrochemical tests. The metals under consideration are a low-alloyed carbon steel (S235JR), an austenitic stainless steel (UNS S31603) and a duplex stainless steel (UNS S31803). The carbon steel, that was found to corrode uniformly, could be considered as a constructional material if a sufficient wall thickness is chosen. The austenitic stainless steel and the duplex stainless steel demonstrate very low uniform corrosion rates. They are however susceptible to pitting and crevice corrosion. To guarantee safe operation of the geothermal power plant, the susceptibility of the alloys to stress corrosion cracking should be tested and in situ experiments should be performed. KW - Geothermal energy KW - Corrosion KW - Carbon dioxide KW - Carbon steel KW - Stainless steel PY - 2019 DO - https://doi.org/10.1016/j.geothermics.2019.05.018 SN - 0375-6505 VL - 82 IS - 11 SP - 182 EP - 189 PB - Elsevier Ltd. AN - OPUS4-48759 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Erning, Johann Wilhelm A1 - Gerhardy, K. T1 - Anschluss von Feuerlöschanlagen N2 - Die Ergebnisse des Diskurses zu den Möglichkeiten des Anschlusses von Feuerlöschanlagen an die öffentliche Trinkwasserverordnung werden zusammengefasst und beleuchtet. Grenzen der Anwendung werden beschrieben, Risiken dargestellt. KW - Absicherung KW - Trinkwasser KW - Feuerlöschen PY - 2019 SN - 1436-6134 VL - 2019 IS - 9 SP - 26 EP - 29 PB - wvgw Wirtschafts- und Verlagsgesellschaft Gas und Wasser mbH CY - Bonn AN - OPUS4-49277 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Erning, Johann Wilhelm T1 - Planung und Betrieb von Trinkwasserinstallationen: Was uns das Regelwerk sagt N2 - Die aktuellen Vorgaben aus gesetzlichen Regelungen und dem technischen Regelwerk für die Planung, Erstellung und den Betrieb einer Trinkwasserinstallation werden dargelegt. Beispiele für einzelne Punkte werden gegeben. T2 - Der sichere Einsatz von Werkstoffen aus Kupfer und Kupferlegierungen in der Trinkwasserinstallation CY - Iserlohn, Germany DA - 12.12.2019 KW - Werkstoffe KW - Trinkwasserinstalltion KW - Sicherer Betrieb KW - Wartung PY - 2019 AN - OPUS4-50184 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Erning, Johann Wilhelm T1 - Wie gehe ich bei einer Schadensuntersuchung vor? N2 - Die Vorgehensweise einer Schadensuntersuchung wird in Schritten erklärt und wichtige Einzelthemen diskutiert. T2 - Der sichere Einsatz von Werkstoffen aus Kupfer und Kupferlegierungen in der Trinkwasserinstallation CY - Iserlohn, Germany DA - 12.12.2019 KW - Schadensanalyse KW - Vorgehensweise PY - 2019 AN - OPUS4-50185 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Erning, Johann Wilhelm A1 - Kamaraj, Abinaya T1 - Susceptibility of 304 stainless steel to crevice corrosion in electrochemically active fluids N2 - The crevice corrosion behaviour of stainless steel 304 L n ECA fluids is investigated. Results are described, rules for operation are suggested T2 - Ceocor-Tagung 2019 CY - Copenhagen, Denmark DA - 21.05.2019 KW - Desinfection KW - Crevice corrosion KW - ECA PY - 2019 AN - OPUS4-49280 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Erning, Johann Wilhelm T1 - Observations of copper pitting corrosion in german tap waters N2 - In recent years, a new type of pitting corrosion is observed on half-had copper pipes. examples are given and possible reasons are discussed T2 - Eurocorr 2019 CY - Sevilla, Spain DA - 09.09.2019 KW - Water KW - Pitting KW - Corrosion KW - Copper KW - Drinking PY - 2019 AN - OPUS4-49281 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Erning, Johann Wilhelm A1 - Kamaraj, Abinaya T1 - Susceptibility of 304 stainless steel to crevice corrosion in electrochemically active fluids N2 - The susceptibility of AISI 304 stainless steel to crevice corrosion on the effect of contact with electrochemically active fluids was investigated using exposure and stepwise potentiostatic polarisation. Crevice materials made up of 304 SS and Polyether ether ketone (PEEK) forming two kinds of crevices including 304 SS-to-PEEK and 304 SS-to-304 SS were tested. T2 - Eurocorr 2019 CY - Sevilla, Spain DA - 09.09.2019 KW - ECA KW - Crevice KW - Corrosion KW - Stainless KW - Steel PY - 2019 AN - OPUS4-49282 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Erning, Johann Wilhelm T1 - A new type of copper pitting corrosion in german tap waters N2 - Half-hard copper pipes show pitting corosion under conditions until now seen as uncritical. Examples are discussed, possible causes described. T2 - MTECH 2019 CY - Porec, Croatia DA - 09.10.2019 KW - Drinking KW - Pitting KW - Corrosion KW - Copper KW - Water PY - 2019 AN - OPUS4-49283 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -