TY - JOUR A1 - Hensel, J. A1 - Kromm, Arne A1 - Nitschke-Pagel, T. A1 - Dixneit, Jonny A1 - Dilger, K. T1 - Capability of martensitic low transformation temperature welding consumables for increasing the fatigue strength of high strength steel joints N2 - The use of low transformation temperature (LTT) filler materials represents a smart approach for increasing the fatigue strength of welded high strength steel structures apart from the usual procedures of post weld treatment. The main mechanism is based on the effect of the low start temperature of martensite formation on the stress already present during welding. Thus, compressive residual stress formed due to constrained volume expansion in connection with phase transformation become highly effective. Furthermore, the weld metal has a high hardness that can delay the formation of fatigue cracks but also leads to low toughness. Fundamental investigations on the weldability of an LTT filler material are presented in this work, including the characterization of the weld microstructure, its hardness, phase transformation temperature and mechanical properties. Special attention was applied to avoid imperfections in order to ensure a high weld quality for subsequent fatigue testing. Fatigue tests were conducted on the welded joints of the base materials S355J2 and S960QL using conventional filler materials as a comparison to the LTT filler. Butt joints were used with a variation in the weld type (DY-weld and V-weld). In addition, a component-like specimen (longitudinal stiffener) was investigated where the LTT filler material was applied as an additional layer. The joints were characterized with respect to residual stress, its stability during cyclic loading and microstructure. The results show that the application of LTT consumables leads to a significant increase in fatigue strength when basic design guidelines are followed. This enables a benefit from the lightweight design potential of high-strength steel grades. KW - Low transformation temperature KW - Welding KW - Fatigue strength KW - Residual stress PY - 2020 DO - https://doi.org/10.3139/120.111562 VL - 62 IS - 9 SP - 891 EP - 899 PB - Carl Hanser Verlag AN - OPUS4-51180 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Combined effect of heating rate and restraint condition on stress relief cracking susceptibility during PWHT of thick-walled Cr-Mo-V steel submerged arc welded joints N2 - Contemporary steels creep-resistant steels like the 13CrMoV9-10 are used as thick plates e.g., for applications in hydrocrackers. The large plate thickness requires high efficiency welding processes like submerged arc welding (SAW) and a mandatory post weld heat treatment (PWHT). The PWHT-parameters stem from a combination of empirical knowledge and traditional experiments on free shrinking (FS) welds. In that connection, the formation of so-called stress-relief cracking (SRC) must be anticipated. The SRC susceptibility of a welded component is a complex combination and interaction of com-ponent specific, thermal, and metallurgical factors. Many of which have to date not been conclusively researched. For example, it is well known that SRCs develop during PWHT due to formation and growth of carbides on prior austenite grain boundaries, resulting in a significant hardness increase (secondary hardening) and toughness decrease. This leads to a high SRC susceptibility of the coarse grain heat-affected zone (CGHAZ) of the last weld bead during PWHT. This is intensified in case of high residual stresses from the component-specific, structurally induced stiffness. In combination with multi-layer welding this leads to a multiaxial stress distribution. Nonetheless, the combined effect of PWHT and high-residual stresses on the SRC formation is merely unknown. For that reason, this study presents the effect of different heating rates in conjunction with a certain component stiffness. For that reason, SAW joints of 13CrMoV9-10 steel were investigated under FS and defined external restraint condition. T2 - IIW Intermediate Meeting, Com. II-A CY - Incheon, Republic of Korea DA - 12.03.2024 KW - Stress relief cracking KW - Welding KW - Post weld heat treatment KW - Submerged arc welding KW - Cr-Mo-V steel KW - Creep-resisting steel PY - 2024 AN - OPUS4-59673 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Call for interested people to contribute to series of comprehensive papers on welding and joining of components for sustainable energy systems N2 - Joining and welding technologies are of high importance for the manufacturing of components and parts used in sustainable energy generation, conversion, and transport. In that connection, offshore and on-shore installed wind turbines are of high interest for the generation of electrical energy as well as photo-voltaic systems (solar cells). The electricity can be either directly transported or conversed via power-to-gas e.g., to hydrogen. In that scope, electrolyzer up to MW-range are of interest as well as the conver-sion back to electricity via fuel cells. In addition, hydrogen is a key element of the decarburization of in-dustries as well as the mobility sector encompassing sea, air and land transportation driven by hydrogen or its derivates. Well-known examples cover the direct reduction of iron ore to replace the conventional blast furnace process up to gas turbines or fuel cells for home-end use. All mentioned technologies re-quire reliable components, which are to a high extend dependent on joining and especially welding pro-cessing of materials. Especially, the (petro-) chemical industry has many years of experience with both materials used in hydrogen applications. The challenge is e.g., the transition to mass production of sys-tem components of electrolyzers/fuel cells and for distribution grids. At this point, the scalability of cur-rently applied joining processes often limits the economic efficiency, whereas especially laser welding or additive manufacturing will be of high interest. In that connection, it is very important to provide answers by joint research of universities, institutes, and industrial companies. Very often, solutions are already available and “just” have to be investigated and adapted for the new application, like repair welding of NG pipelines. For that reason, we want to set up a series of comprehensive papers with the aforementioned title. The idea is to get an in-depth but manageable overview of the importance of joining technologies in sustaina-ble energy generation, conversion, and transport encompassing current processes, limitations, and fur-ther perspectives. In that connection, the additive manufacturing is gaining more and more attention. If applicable, current challenges in the adaption or creation of new standards/regulations shall be addressed. T2 - IIW Intermediate Meeting, Com. II-A CY - Incheon, Republic of Korea DA - 12.03.2024 KW - Hydrogen KW - Welding KW - Comprehensive study KW - Component manufatcturing KW - Additive manufacturing PY - 2024 AN - OPUS4-59676 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Reliable hydrogen determination in metallic materials and their weld joints: Parameters and challenges N2 - In the course of tomorrow's hydrogen-based energy transition, the construction of the corresponding infrastructure will play a central role. The majority of materials used to date are typically welded for component fabrication. In that context, steels are widely applied and can be prone to hydrogen embrittlement. This includes the classical delayed cold cracking during welding processing as well as embrittlement phenomena during operation. For the evaluation of any hydrogen effect on, for example, the mechanical properties of a welded metallic material, the hydrogen content must be precisely determined. In the case of welds, for example, according to ISO 3690, this is the isothermal carrier gas hot extraction (CGHE). CGHE is based on accelerated hydrogen degassing due to thermal activation of hydrogen at elevated temperatures. In addition to the pure quantification of hydrogen, thermal desorption analysis (TDA) with varied heating rates can be used to determine and evaluate the bonding state at microstructural defects in the material. For both techniques, experimental and measurement influences have to be considered, which have a great effect on the result. For CGHE, for example, ISO 3690 suggests different sample geometries as well as minimum extraction times. The present study summarizes results and experiences of numerous investigations with different sample temperatures and geometries (ISO 3690 type B and cylindrical TDA samples) regarding: the influence of the sample surface (polished/welded), measurement accuracies depending on the sample volume as well as the insufficient monitoring of the effect of the PI controller on the extraction temperature. In particular, a deviating extraction temperature to the set temperature, can significantly falsify the measurement results. Based on the results, methods are shown to quickly reach the desired extraction temperature without having to physically interfere with the measurement equipment. This serves to substantially improve the reliability of hydrogen measurement through increased signal stability and accelerated hydrogen desorption. In general, an independent temperature measurement with dummy samples for the selected heating procedure is advisable to exclude possible unwanted temperature influences already before the measurement. In addition (and way more important), the methods described can be transferred directly to industrial applications. T2 - 47th MPA-Seminar CY - Stuttgart, Germany DA - 10.10.2023 KW - Hydrogen assisted cracking KW - Carrier gas hot extraction KW - Welding KW - ISO 3690 KW - Metals PY - 2023 AN - OPUS4-58677 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Erxleben, Kjell A1 - Kaiser, Sebastian A1 - Rhode, Michael A1 - Kannengiesser, Thomas A1 - Kromm, Arne T1 - In-service and repair welding of pressurized hydrogen pipelines–a review on current challenges and strategies N2 - Hydrogen is the energy carrier for a sustainable future without fossil fuels. As this requires a reliable transportation infrastructure, the conversion of existing natural gas (NG) grids is an essential part of the worldwide individual national hydrogen strategies, in addition to newly erected pipelines. In view of the known effect of hydrogen embrittlement, the compatibility of the materials already in use (typically low-alloy steels in a wide range of strengths and thicknesses) must be investigated. Initial comprehensive studies on the hydrogen compatibility of pipeline materials indicate that these materials can be used to a certain extent. Nevertheless, the material compatibility for hydrogen service is currently of great importance. However, pipelines require frequent maintenance and repair work. In some cases, it is necessary to carry out welding work on pipelines while they are under pressure, e.g., the well-known tapping of NG grids. This in-service welding brings additional challenges for hydrogen operations in terms of additional hydrogen absorption during welding and material compatibility. The challenge can be roughly divided into two parts: (1) the possible austenitization of the inner piping material exposed to hydrogen, which can lead to additional hydrogen absorption, and (2) the welding itself causes an increased temperature range. Both lead to a significantly increased hydrogen solubility in the respective materials compared to room temperature. In that connection, the knowledge on hot tapping on hydrogen pipelines is rare so far due to the missing service experiences. Fundamental experimental investigations are required to investigate the possible transferability of the state-of-the-art concepts from NG to hydrogen pipeline grids. This is necessary to ensure that no critical material degradation occurs due to the potentially increased hydrogen uptake. For this reason, the paper introduces the state of the art in pipeline hot tapping, encompassing current research projects and their individual solution strategies for the problems that may arise for future hydrogen service. Methods of material testing, their limitations, and possible solutions will be presented and discussed. KW - In-service KW - Welding KW - Hydrogen pipeline KW - Review PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-638847 DO - https://doi.org/10.1007/s40194-025-02127-x SN - 0043-2288 SP - 1 EP - 24 PB - Springer Science and Business Media LLC AN - OPUS4-63884 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Erxleben, Kjell T1 - Component test for the assessment of in-service welding on/onto pressurized hydrogen pipelines N2 - Hydrogen is seen as the energy carrier of the future. Therefore a reliable infrastructure to transport hydrogen in a large scale is needed. A so called European hydrogen backbone out of long distance transmission pipelines is planned by European countries to create a hydrogen transport infrastructure. Due to economic reasons this will be achieved by new build pipelines such as repurposed natural Gas (NG) pipelines, converted to hydrogen useage. A general suitability for hydrogen service of low alloyed pipeline steel, as it is used for NG service today, is given. But in case of necessary in-service welding procedures in terms of e.g. hot-tapping and stoppling, the risk of a critical hydrogen uptake into the pipe materials due to much higher temeperatures while welding and the possibility of hydrogen embrittlement (HE) needs to be closely investigated. The presentation gives an overview of the current H2-SuD project, investigating the feasability of in-service welding on future hydrogen pipelines. Therefore, component-like demonstrators were developed to test (I) the additional hydrogen uptake due to in-service welding under hydrogen pressure and (II) to measure the temperature field due to different welding parameters and demonstrator geometries, especially on the inner pipe wall surface. Collected data will be used to validate a numerical simulation of the thermal field and additionally the hydrogen diffusion in the pipeline material. T2 - Presentation at The University of Manchester CY - Manchester, United Kingdom DA - 12.09.2025 KW - In-service KW - Hydrogen KW - Pipeline KW - Welding PY - 2025 AN - OPUS4-64129 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Numerical simulation of weld heat input effect on microstructure and hydrogen diffusion in thick-walled S690 submerged arc welded joints N2 - High-strength, low-alloy (HLSA) steels such as S690 are an attractive option for heavy industries such as offshore wind turbines and peripheral equipment due to their combination of excellent mechanical properties and weldability. The construction of these thick-walled structures requires highly efficient welding processes such as submerged arc welding (SAW). However, SAW presents challenges related to delayed hydrogen assisted cold cracking (HACC). Despite its importance, the effect of different diffusion coefficients on the cold cracking susceptibility of different microstructures within SAW-welded S690 steels is not fully understood. For this reason, the present study focuses on comparing the cold cracking susceptibility of thermomechanically rolled (TM) or quenched and tempered (QL) variants of S690 steel. SAW was performed on specimens of both steel grades to produce weldments consisting of weld metal, heat-affected zone (HAZ), and base metal. Electrochemical hydrogen permeation tests (ISO 17081) were performed to determine the microstructure specific coefficients. Using the obtained coefficients, a numerical model was developed to identify the time- and microstructure-dependent local hydrogen diffusion and its influence on the distribution within the welds. The results showed that the TM grade exhibited slightly accelerated hydrogen diffusion compared to the QL grade, which is beneficial for hydrogen reduction and increases the HACC resistance. However, the further simulations with different ply sequences showed that the welding heat input (i.e. welding ply sequence) had a significantly higher effect on hydrogen accumulation. Specifically, increased welding heat input and increased thicknesses decrease hydrogen diffusivity. For this reason, microstructure-specific hydrogen diffusion played a minor role in thick-layer SAW joints compared to the need to control the welding parameters (layer sequence, individual layer thickness, welding heat input). T2 - FEMS Euromat 2025 - 18th European Congress and Exhibition on Advanced Materials and Processes CY - Granada, Spain DA - 15.09.2025 KW - Hydrogen assisted cracking KW - Welding KW - High strength steels KW - Numerical simulation KW - Electrochemical permeation PY - 2025 AN - OPUS4-64158 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wilhelm, Eugen A1 - Mente, Tobias A1 - Rhode, Michael T1 - Waiting time before NDT of welded offshore steel grades under consideration of delayed hydrogen-assisted cracking N2 - Offshore wind turbines (OWT) are a major goal of the energy strategy of Germany encompassing the increase of the installed wind power. OWT components are manufactured from welded steel plates with thicknesses up to 200 mm. The underlying standards and technical recommendations for construction of OWTs encompass specifications of so-called minimum waiting time (MWT) before non-destructive testing of the weld joints is allowed. Reason is the increased risk of time-delayed hydrogen assisted cold cracking as hydrogen diffusion is very slow due to the very thick plates. The strict consideration of those long MWT up to 48 h during the construction of OWTs leads to significant financial burden (like disproportionately high costs for installer ships as well as storage problems (onshore)). In this study, weld joints made of S355 ML were examined in comparison with the offshore steel grade S460 G2+M. The aim was to optimize, i.e., reduce, the MWT before NDT considering varied heat input, hydrogen concentration and using self-restraint weld tests. This would significantly reduce the manufacturing time and costs of OWT construction. To quantify the necessary delay time until hydrogen-assisted cold cracks appear, acoustic emission analysis was applied directly after welding for at least 48 h. KW - Hydrogen KW - Welding KW - Cracking KW - Offshore KW - Steel PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-524959 DO - https://doi.org/10.1007/s40194-020-01060-5 SN - 0043-2288 VL - 65 SP - 947 EP - 959 PB - Springer Nature AN - OPUS4-52495 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Richter, Tim T1 - Residual stresses in near-component specimens of a high and a medium entropy alloy due to tig and friction stir welding N2 - The new alloying concept of multi-element systems with defined entropy (HEA - High Entropy Alloy or MEA - Medium Entropy Alloy) is gaining increasing importance in materials research. Significantly improved properties or combinations of properties are shown by some HEA/MEA-systems, which have the potential to substitute conventional alloys such steels and are therefore promising for a wide range of applications, e.g., overcome of the trade-off between high strength and ductility. Thus, primarily the production and resulting microstructures of HEA as well as properties have been investigated so far. Furthermore, processing is a main issue to transfer HEA systems from the laboratory to real components, e.g., for highly stressed components. Since welding is the most important joining process for metals, it is crucial to investigate the influence of welding processing on these material properties to guarantee component integrity. Welding leads to residual stresses, which significantly affect the component integrity. Only a very few studies on the effect of welding on residual stresses in HEA and MEA weld joints are available so far. Hence, the focus of this study is the residual stress formation and distribution in a CoCrFeMnNi HEA and ternary CoCrNi MEA using two different welding processes: Tungsten Inert Gas (TIG) welding and soldi-state Friction Stir Welding (FSW). As a pathway for application of HEA in this investigation for the first time residual stress analyses in realistic near-component specimens were performed. The residual stresses were determined by X-ray diffraction (XRD) on the surfaces of top and root weld side. The results were correlated with the local welding microstructures. The results show that both FSW and TIG generate significant tensile residual stresses on the weld surfaces in and transverse to the welding direction. In the case of FSW of the CoCrFeMnNi HEA, the longitudinal residual stresses are in the range of the yield strength of approx. 300 MPa in the weld zone. T2 - OVGU-Kolloquium (BMDK des IWF) CY - Online meeting DA - 19.05.2022 KW - High Entropy Alloy KW - Welding KW - Residual stresses KW - Microstructure PY - 2022 AN - OPUS4-56671 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Joining technologies for hydrogen components: current need and future perspectives N2 - The study provides an overview of the aspects of joining and its importance in manufacturing of components for the more and more important field of hydrogen as key factor for the energy transition to a decarburized future. To this end, the fundamentals of the technology fields of hydrogen production, storage, transport, and application are presented and the state of the art of manufacturing of components for hydrogen technologies by joining is summarized. Based on representative examples from practice, research and development, the importance of joining technology in hydrogen technologies is clearly highlighted and perspectives for the future are derived. From a macroeconomic perspective, the focal points, or trends of joining technologies here include: the erection of new infrastructure for hydrogen storage and transport, and the safe conversion of existing natural gas infrastructure and its challenges for welded materials. In addition, we show the problems that are anticipated with in-service repair welding of hydrogen pipelines. In hydrogen applications, the efficient mass production of fuel cells and electrolysers is becoming increasingly important. For that reason, the importance of additive manufacturing is highlighted. Finally, the challenges for technical regulations and standardization by using hydrogen are shown. T2 - AJP 2023: 3rd International Conference on Advanced Joining Processes 2023 CY - Braga, Portugal DA - 19.10.2023 KW - Hydrogen KW - Infractstructure KW - Joining KW - Welding KW - Research PY - 2023 AN - OPUS4-58674 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Evaluation of local strain behavior of cross-weld tensile specimens of micro-alloyed high-strength steels by digital image correlation N2 - Microalloying elements such as Nb and Ti play a decisive function in achieving the desired mechanical strength of quenched and tempered, high-strength fine-grain structural steels with a nominal yield strength ≥ 690 MPa. The current specifications for the chemical composition only provide manufacturers with upper limits. However, even minor deviations in the alloy concept can have a significant impact on the mechanical properties. Consequently, accurate prediction of weldability and the integrity of welded joints becomes difficult or even impossible due to differences in composition and the resulting microstructures. Undesirable consequences include a possible softening of the heat-affected zone (HAZ) or, conversely, hardening effects. In view of these challenges, various microalloying strategies with different Ti and Nb contents are being systematically investigated for the first time using specially developed laboratory casting alloys. Each alloying route is based on the common S690QL, maintaining both the chemical composition and the heat treatment parameters. To analyse the weldability, three-layer welds were performed using gas metal arc welding (GMAW) and critical microstructures, such as areas of the heat-affected zone (HAZ) that exhibit significant softening or hardening, were identified. The effect of the softened HAZ region on failure was evaluated using transverse tensile specimens. Digital image correlation (DIC) is used to image changes in local strains in different HAZ regions in situ. Using a specially developed mirror system, the local strains of the microstructure zones on the top and bottom of the weld are recorded simultaneously. This makes it possible to analyse how the weld seam geometry (e.g., V-seam) influences the strain gradients. In addition, the analysis of the local deformation helps to understand the effects of the softened HAZ on the global strain, the fracture constriction, the fracture position, and the overall fracture behavior. T2 - IIW Intermediate Meeting, Com. II-A CY - Incheon, Republic of Korea DA - 12.03.2024 KW - Welding KW - High-strength steel KW - Alloy concept KW - Cross-weld tensile sample KW - Mechanical properties PY - 2024 AN - OPUS4-59675 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Joining technology for the new hydrogen economy: Current need and future perspectives N2 - This presentation gives an overview on the importance of joining processes for component fabrication in hydrogen technologies. For that reason, the current need and future research and developement activites are highlighted for the three technological fields: hydrogen storage, transport and use (in terms of the emerging field of additive manufacturing). Finally, some remarks are given for necessary changes in the standardization. T2 - Laser Colloquium Hydrogen 2024 CY - Aachen, Germany DA - 10.09.2024 KW - Hydrogen technologies KW - Joining KW - Welding KW - Challenges KW - Standardization PY - 2024 AN - OPUS4-61012 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Thickness and microstructure effect on hydrogen diffusion in creep-resistant 9 % Cr P92 steel and P91 weld metal N2 - Martensitic 9 %-Cr steels like P91 and P92 show susceptibility to delayed hydrogen assisted cracking depending on their microstructure. In that connection, effective hydrogen diffusion coefficients are used to assess the possible time-delay. The small number of available diffusion coefficients varies already at room temperature by several orders of magnitude (mostly regarded as result of present microstructure). Especially P91 weld metal diffusion coefficients are rare so far. For that reason, electrochemical permeation experiments had been conducted using P92 base metal and P91 weld metal (in as-welded and heat-treated condition) with different thicknesses. The diffusion coefficients are calculated by two methods (time-lag and inflection point method) were performed. The results show that, despite of microstructural effects, the sample thickness must be considered as it influences the calculated diffusion coefficients. Finally, the comparison of calculated and measured hydrogen concentrations (determined by carrier gas hot extraction) enables the identification of realistic diffusion coefficients. T2 - IIW Annual Assembly, Meeting of Commission IX-C CY - Online meeting DA - 15.07.2021 KW - Creep-resistant steel KW - Diffusion KW - Electrochemical permeation KW - Hydrogen KW - Welding PY - 2021 AN - OPUS4-53048 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Hydrogen embrittlement of steels N2 - Hydrogen assisted cracking of metals is a serious issue in the safety of components, espcially in case of welding. The current presentation gives an overview on specialized testing procedures at Department 9 including the quantitative determination of hydrogen. T2 - HYDROGENIUS BAM Joint Hydrogen Symposium CY - Online meeting DA - 06.07.2021 KW - Hydrogen KW - Embrittlement KW - Degradation KW - Carrier gas hot extraction KW - Welding PY - 2021 AN - OPUS4-53049 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Erxleben, Kjell T1 - Hydrogen determination in welded metallic materials: Necessity and challenges N2 - In the course of tomorrow's hydrogen-based energy transition, the construction of the corresponding infrastructure will play a central role. The majority of materials used to date are typically welded for component fabrication. In that context, steels are widely applied and can be prone to hydrogen embrittlement. For the evaluation of any hydrogen effect on, for example, the mechanical properties of a welded metallic material, the hydrogen content must be precisely determined. According to ISO 3690, carrier gas hot extraction (CGHE) can be used. In addition to the pure quantification of hydrogen, thermal desorption analysis (TDA) with varied heating rates can be used to determine and evaluate the bonding state at microstructural defects in the material. For both techniques, experimental and measurement influences have to be considered, which have a great effect on the result. For CGHE, for example, ISO 3690 suggests different sample geometries as well as minimum extraction times. The present study summarizes results and experiences of numerous investigations with different sample temperatures and geometries (ISO 3690 type B and cylindrical TDA samples) regarding: the influence of the sample surface (polished/welded), measurement accuracies depending on the sample volume. In particular, a deviating extraction temperature to the set temperature, can significantly falsify the measurement results. Based on the results, methods are shown to quickly reach the desired extraction temperature without having to physically interfere with the measurement equipment. This serves to substantially improve the reliability of hydrogen measurement through increased signal stability and accelerated hydrogen desorption. In general, an independent temperature measurement with dummy samples for the selected heating procedure is advisable to exclude possible unwanted temperature influences already before the measurement. In addition (and way more important), the methods described can be transferred directly to industrial applications. T2 - Eurocorr 2023 - The European Corrosion Congress CY - Brussels, Belgium DA - 27.08.2023 KW - Hydrogen KW - Carrier gas hot extraction KW - Welding KW - ISO 3690 KW - Measurement PY - 2023 AN - OPUS4-58305 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Standardization and examples for R & D activities on hydrogen technologies with respect to testing procedures in Germany N2 - This contribution briefly summarizes the standardization activities in accordance with the "Nationale Roadmap Wasserstofftechnologien" and presents selected results on the activities in Germany with scope on hydrogen transport in pipelines. The talk was given during a panel discussion to set-up a steering committee for standardization for hydrogen pipelines and welding , coordinated by the International Institute of Welding. T2 - IIW Annual Assembly, Meeting of Commission XI CY - Singapore DA - 19.07.2023 KW - Hydrogen KW - Welding KW - Pipelines KW - Standardization KW - Research PY - 2023 AN - OPUS4-57976 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Becker, Amadeus T1 - Adequate repair concepts for high-strength steel weld joints for offshore support structures considering design influences N2 - The sustainable and resource-efficient production of wind energy plants requires the use of modern high-strength fine-grain structural steels. This applies to both foundation and erection structures. During the assembly of steel structures, unacceptable defects can occasionally be found in the weld area. In most cases, the economical solution would be local thermal gouging of the affected areas and re-welding. Due to the high shrinkage restraint of the joint groove in the overall structure, the superposition of global and local welding-induced stresses may lead to crack formation and component failure, particularly in interaction with the degradation of the microstructure and mechanical properties of high-strength steels during the repair process [1]. Corresponding standards hardly provide any information on adequate repair concepts, and there is no uniform scientific data on which to base such concepts. In this study, several relevant findings are discussed based on examples of structural engineering focusing on mechanical-technological properties and residual stresses, e.g. [1]. Further experimental and numerical work as conducted by [2] and weld tests under defined restraint conditions in special weld test-setups [3] show that an optimization of the welding-induced stresses of high-strength structural steels is achievable by means of an adapted heat control. The present research involves systematic investigations of influences of shrinkage restraint, the number of repair cycles and heat control during repair welding of a recently available high-strength offshore steel S500MLO (EN 10225-1). A quantification of the shrinkage restraint of repair weld joints is achievable by means of restraint intensity concept [4], analogous to previous studies [5]. Using structural mechanics calculations, geometries of self-restrained specimens are identified representing different defined rigidity conditions of repair welds considering actual high-strength steel components. Welding experiments with DIC analyses (digital image correlation) of the occurring strains during welding and XRD analyses (X-ray diffraction) of the resulting residual stresses after welding and cooling show increasing transient loads and significantly elevated residual stress profiles in the weld area with increasing restraint intensity. Especially in the heat affected zone, tensile residual stresses of up to 80 % of the nominal yield strength occur when welding under increased restraint conditions. In relation to the presented existing results, this indicates that a safe repair welding is primarily achievable by means of appropriate repair concepts and heat control taking into account the high welding stresses and special microstructures of high-strength steels. Finally, the aim of this research is to derive recommendations for repair concepts appropriate to the stresses and materials involved providing a basis for standards and guidelines, especially for SMEs, in order to avoid damage and, in most cases, expensive reworking and to improve the full utilization of the potential of high-strength steels. T2 - 74th IIW Annual Assembly and International Conference, C II-A CY - Online meeting DA - 07.07.2021 KW - High-strength structural steels KW - Welding KW - Repair KW - Residual stresses KW - Restraint PY - 2021 AN - OPUS4-53320 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Mente, Tobias A1 - Kannengießer, Thomas A1 - Schaupp, Thomas A1 - Zavdoveev, Anatoly T1 - Challenges for testing hydrogen-assisted cold cracking in weld seams of high-strength steel grades N2 - Hydrogen can cause weld cold cracking even days after fabrication. In this respect, higher strength steels present a challenge to established cold crack testing. In general, the tolerable hydrogen concentration for crack prevention decreases with increasing material strength. In addition, advanced welding processes require changes in weld geometry and heat input. This directly influences the formation of crack-critical microstructures, e.g. in hardened areas of the heat-affected zone. The limits of use and application of modern cold cracking tests are evaluated by (1) the externally loaded Implant-test and (2) the self-restraint Tekken-test. In particular, external mechanical stresses, which cause additional mechanical loads on the components during welding, must be considered due to the component-specific stiffness of high-strength steels. Accompanying test methods for determining hydrogen concentration and diffusion in welds are presented, such as carrier gas hot extraction for determining hydrogen concentration (ISO 3690) or temperature-dependent diffusion coefficients. These values are of great importance for a holistic approach to the evaluation of the cold cracking sensitivity of high strength steels. KW - Hydrogen KW - Welding KW - Cold cracking test KW - High-strength steel PY - 2024 DO - https://doi.org/10.37434/tpwj2024.08.01 SN - 0957-798X VL - 2024 IS - 8 SP - 3 EP - 9 PB - International Association "Welding" CY - Kyiv, Ukraine AN - OPUS4-60946 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kaiser, Sebastian T1 - Evaluation of welding on in-service pressurized hydrogen pipelines by component testing N2 - Hydrogen transportation is fundamentally different from natural gas (NG) as it can be absorbed into the pipeline material. However, pipelines require frequent maintenance or repair, in some cases on or onto the pipelines while they are still under pressure. This in-service welding causes challenges for hydrogen operations. They can be roughly divided into: (1) possible austenitization of the inner pipe material exposed to hydrogen, and (2) welding itself with its temperature cycles. Both lead to a significant increase in hydrogen solubility/diffusivity of the materials. Fundamental investigations are required due to the missing service experience. The present study introduces a specially designed demonstrator concept for the assessment of the welding processing conditions. The mock-up was designed to enable temperature measurement during welding as well as ex-post extraction of samples for the quantification of the absorbed hydrogen. The necessary pressurized hydrogen volume was limited by the insertion of a solid cylinder. Welding experiments on the pressurized mock-ups (DN50 and DN200) have shown that the austenitization temperature is nearly reached on the inner surface of the pipeline. This corresponds to a significant hydrogen absorption of several ppm in the welded joint, especially for thin-walled pipelines. Nonetheless, a potential hydrogen assisted cracking was not identified. T2 - 24. Werkstofftechnisches Kolloquium CY - Chemnitz, Germany DA - 02.04.2025 KW - Pipeline KW - In-Service KW - Welding KW - Hydrogen PY - 2025 AN - OPUS4-62917 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kaiser, Sebastian A1 - Erxleben, Kjell A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Repair Welding of In-Service Hydrogen Pipelines - Concepts and Challenges N2 - Hydrogen is set as the energy carrier of tomorrow for a more sustainable fossil fuel free future. As this necessitates a reliable transport infrastructure, repurposing of the existing natural gas grid is planned. With regards to the well-known effect of hydrogen embrittlement, the compatibility of utilized materials must be investigated. First comprehensive studies on pipeline material hydrogen compatibility indicate that these materials can be applied to a certain extent. Nonetheless, the material compatibility is currently of high interest and focus of numerous research projects worldwide. However, pipelines require frequent maintenance and repair work. As part of these, in some cases it is necessary to do weldments onto pipelines while they are pressurized. This in-service welding introduces additional challenges for the material compatibility. Due to the resulting high temperatures, the metallurgical changes in the material and of course the presence of high-pressure hydrogen in the pipeline, additional investigations need to be conducted to ensure that no critical material degradation because of increased hydrogen absorption occurs and an overall material compatibility is given. For this reason, the present paper introduces in-service welding on pipelines. An overview of current research projects that deal with the application of in-service welding specifically on hydrogen pipelines and the emerging problems when applying these techniques on hydrogen pipelines is given. Methods of material testing, their limits and possible solutions are presented and discussed. T2 - 2024 15th International Pipeline Conference CY - Calgary, Alberta, Canada DA - 23.09.2024 KW - Hydrogen KW - Pipeline KW - Welding KW - In-Service PY - 2024 SN - 978-0-7918-8856-8 DO - https://doi.org/10.1115/IPC2024-133052 SP - 1 EP - 6 PB - The American Society of Mechanical Engineers (ASME) CY - New York AN - OPUS4-62262 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kromm, Arne T1 - Phase Transformation and Strain Evolution during Welding of Low Transformation Temperature Alloys N2 - In this work, the phase and strain formation in multipass welding of LTT gas metal arc welds were observed under realistic restraints by means of time resolved angular-dispersive synchrotron X-ray diffraction at the High Energy Materials Science beamline HEMS at PETRA III (DESY), Hamburg Germany. It was shown that the strain evolution during cooling correlates with the amount of martensite formed. Both, the strain of martensite and austenite are affected during phase transformation. Even though dilution processes limit the LTT effect in the root compared to the top layer, the strains are significantly reduced compared to the conventional weld metal. The observed effects are found for both Ni and Mn based LTT filler metals regardless of their respective Ms temperature. T2 - 2nd International Conference on Advanced Joining Processes AJP 2021 CY - Sintra, Portugal DA - 21.10.2021 KW - Welding KW - Residual Stress KW - In-situ diffraction KW - Synchrotron PY - 2021 AN - OPUS4-53609 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Richter, Tim A1 - Schröpfer, Dirk A1 - Manzoni, Anna Maria A1 - Schneider, M. A1 - Laplanche, G. T1 - Welding of high-entropy alloys and compositionally complex alloys - an overview N2 - High-entropy alloys (HEAs) and compositionally complex alloys (CCAs) represent new classes of materials containing five or more alloying elements (concentration of each element ranging from 5 to 35 at. %). In the present study, HEAs are defined as single-phase solid solutions; CCAs contain at least two phases. The alloy concept of HEAs/CCAs is fundamentally different from most conventional alloys and promises interesting properties for industrial applications (e.g., to overcome the strength-ductility trade-off). To date, little attention has been paid to the weldability of HEAs/CCAs encompassing effects on the welding metallurgy. It remains open whether welding of HEAs/CCAs may lead to the formation of brittle intermetallics and promote elemental segregation at crystalline defects. The effect on the weld joint properties (strength, corrosion resistance) must be investigated. The weld metal and heat-affected zone in conventional alloys are characterized by non-equilibrium microstructural evolutions that most probably occur in HEAs/CCAs. The corresponding weldability has not yet been studied in detail in the literature, and the existing information is not documented in a comprehensive way. Therefore, this study summarizes the most important results on the welding of HEAs/CCAs and their weld joint properties, classified by HEA/CCA type (focused on CoCrFeMnNi and AlxCoCrCuyFeNi system) and welding process. KW - High-entropy alloy KW - Compositionally complex alloy KW - Welding KW - Properties KW - Review PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-527068 DO - https://doi.org/10.1007/s40194-021-01110-6 SP - 1 EP - 15 PB - Springer Nature AN - OPUS4-52706 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Richter, Tim T1 - Local mechanical properties of TIG dissimilar metal welded high entropy alloy with austenitic steel AISI 304 N2 - High entropy alloys (HEA) are a new class of materials that have been investigated since the early 2000s and offer great potential to replace conventional alloys. However, since they sometimes have significant contents of expensive alloying elements such as Co or Ni, their use is only conceivable in highly stressed areas of components. For this purpose, the weldability with conventional alloys such as high-alloy austenitic steels must be investigated. In addition to the resulting microstructure, the mechanical properties are also fundamental for the usability of HEAs in DMWs. For this purpose, TIG welds of CoCrFeMnNi HEA (cold rolled and recrystallized state) with AISI 304 austenitic steel are investigated. These mechanical properties are analyzed in this work by means of tensile tests and local hardness measurement. The local strain behavior of the welded joints is also characterized by means of Digital Image Correlation (DIC). The results of the local hardness measurement show a clear influence of the initial condition of the HEA on the HAZ. Thus, the HEA in the cold-rolled condition shows a clear softening because of recrystallization processes in the HAZ. On the other hand, there is no influence on the hardness of the weld metal, which is approx. 200 HV0.1 in both cases. The tensile tests show a consistent failure of the weld in the weld metal. However, regardless of the HEA condition, strengths in the range of the recrystallized HEA (RM ~ 550–600 MPa) are achieved, although with significantly reduced fracture elongations. T2 - IIW Intermediate Meeting of Commission II-A CY - Garching, Germany DA - 06.03.2023 KW - High-entropy alloy KW - Welding KW - Dissimilar metal weld (DMW) joint KW - Mechanical properties KW - Digital image correlation PY - 2023 AN - OPUS4-57108 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröpfer, Dirk A1 - Kromm, Arne A1 - Lausch, Thomas A1 - Rhode, Michael A1 - Wimpory, R. C. A1 - Kannengießer, Thomas T1 - Influence of welding stresses on relief cracking during heat treatment of a creep-resistant 13CrMoV steel: Part III - Assessment of residual stresses from small-scale to real component welds N2 - For higher operational temperatures and pressures required in petrochemical plants, the modified 13CrMoV9-10 steel was developed providing high resistance against creep and compressed hydrogen. Extreme care during the welding procedure is necessary for this steel, attributed to low toughness, high strength in as-welded state, and increased susceptibility to stress relief cracking (SRC) during post-weld heat treatment (PWHT). Previous research of SRC in creep-resistant steels discussed mainly thermal and metallurgical factors. Few previous findings addressed the influences of welding procedure on crack formation during PWHT considering real-life manufacturing conditions. These investigations focus on effects of welding heat control on stresses during welding and subsequent PWHT operations close to realistic restraint and heat dissipation conditions using a special 3D testing facility, which was presented in parts I and II of this contribution. Part III addresses investigations on residual stress evolution affecting crack formation and discusses the transferability of results from large-scale testing to laboratory-scale. Experiments with test set-ups at different scales under diverse rigidity conditions and an assessment of the residual stresses of the weld-specimens using X-ray (surface near) and neutron diffraction analysis (bulk) were performed. This study aims to provide a way of investigating the SRC behaviour considering component-specific residual stresses via small-scale testing concepts instead of expensive weld mock-ups. KW - Welding KW - Creep-resistant steel KW - Residual stresses KW - Post-weld heat treatment KW - Stress relief cracking PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-524403 DO - https://doi.org/10.1007/s40194-021-01101-7 SN - 1878-6669 VL - 65 SP - 1671 EP - 1685 PB - Springer CY - Berlin AN - OPUS4-52440 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Mente, Tobias A1 - Kannengießer, Thomas T1 - Parameters and challenges for reliable hydrogen determination in welded joints by carrier gas hot extraction N2 - For the hydrogen-based energy economy of tomorrow, the construction of the necessary infrastructure will play a central role. Most materials used to date, such as welded steels, can be prone to hydrogen embrittlement under certain conditions. This includes the classic delayed cold cracking during welding as well as degradation phenomena during service of components in hydrogen-containing environment. For the evaluation of any hydrogen effect, for example, on the mechanical properties of a welded metallic material, the hydrogen content must be precisely determined. In the case of weld seams, the carrier gas hot extraction (CGHE) according to ISO 3690 is meanwhile state-of-the-art. CGHE is based on accelerated hydrogen degassing due to the thermal activation of hydrogen at elevated temperatures. In addition to the quantification of hydrogen, thermal desorption analysis (TDA) with varying heating rates can be used to determine and evaluate the hydrogen trapping at microstructural defects in the material. For both techniques, experimental and metrological influences must be considered, which have a major effect on the result. For example, ISO 3690 suggests different sample geometries and minimum extraction times for CGHE. This study summarizes the results and experiences of numerous investigations at the Federal Institute for Materials Research and Testing (BAM) with different sample temperatures and geometries (ISO 3690 type B and cylindrical TDA samples) regarding the influence of the sample surface (polished/welded), measurement accuracy depending on the sample volume and the insufficient monitoring of the effect of PI control on the extraction temperature. A deviating extraction temperature from the target temperature can significantly falsify the measurement results. Based on the results, methods are shown which allow the desired extraction temperature to be reached quickly without physically interfering with the measuring equipment. This serves to significantly improve the reliability of the hydrogen measurement through increased signal stability and accelerated hydrogen desorption. In general, an independent temperature measurement with dummy samples is recommended for the heating procedure of choice to exclude possible undesired temperature influences before the measurement. The methods described can be transferred directly to industrial applications KW - Welding KW - Hydrogen measurement KW - ISO 3690 KW - Carrier gas hot extraction PY - 2024 DO - https://doi.org/10.37434/tpwj2024.04.01 SN - 0957-798X VL - 4 SP - 3 EP - 10 PB - International Association Welding AN - OPUS4-60071 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schaupp, Thomas A1 - Ernst, W. A1 - Spindler, H. A1 - Kannengießer, Thomas T1 - Hydrogen-assisted cracking of GMA welded 960 MPa grade high-strength steels N2 - High-strength steels with yield strength of 960 MPa are susceptible to hydrogen-assisted cracking (HAC) during welding processing. In the present paper, the implant test is used to study HAC in a quenched and tempered steel S960QL and a high-strength steel produced by thermo-mechanical controlled process S960MC. Welding is performed using the gas metal arc welding process. Furthermore, diffusible hydrogen concentration (HD) in arc weld metal is determined. Based on the implant test results, lower critical stress (LCS) for complete fracture, critical implant stress for crack initiation, and embrittlement index (EI) are determined. At HD of 1.66 ml/100 g, LCS is 605 MPa and 817 MPa for S960QL and S960MC, respectively. EI is 0.30 and 0.46 for S960QL and S960MC, respectively. Fracture surfaces of S960QL show higher degradation with reduced deformation. Both, higher EI of S960MC and fractography show better resistance to HAC in the HAZ of S960MC compared to S960QL. KW - High-strength steel KW - Welding KW - Diffusible hydrogen KW - Hydrogen-assisted cracking KW - Heat-affected zone KW - Implant test PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-510307 DO - https://doi.org/10.1016/j.ijhydene.2020.05.077 SN - 0360-3199 VL - 45 IS - 38 SP - 20080 EP - 20093 PB - Elsevier Ltd CY - Amsterdam, NL AN - OPUS4-51030 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kromm, Arne A1 - Lausch, Thomas A1 - Schröpfer, Dirk A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Influence of welding stresses on relief cracking during heat treatment of a creep-resistant 13CrMoV steel: Part II - Mechanisms of stress relief cracking during post weld heat treatment N2 - Welding of 13CrMoV9-10 vanadium steel requires care due to an increased susceptibility to stress relief cracking during post weld heat treatment. Previous research into the crack formation in creep-resistant steels has focused on thermal and metallurgical factors; however, little knowledge has been gathered regarding the crack formation during post weld heat treatment considering real-life restraint conditions. This work is subdivided in two parts. Part I showed that an increasing heat input during submerged arc welding under restraint led to an increasing stress level in the joint prior to the post weld heat treatment. The magnitude of stress relief cracking observed in the heat-affected zone after the post weld heat treatment is affected by the heat input. In Part II of this work, the cracks and the associated microstructure which occurred under restraint were studied. The application of a Special acoustic emission analysis indicated that the cracks formed in a temperature range between 300 and 500 °C during the post weld heat treatment. The toughness in the heat-affected zone of the restrained welds was affected by the welding heat input. Microstructural analyses of all specimens revealed accelerated aging due to precipitation of carbides during post weld heat treatment under restraint. KW - Welding KW - Creep-resistant steel KW - Post weld heat treatment KW - Stress relief cracking PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-506283 DO - https://doi.org/10.1007/s40194-020-00881-8 SN - 1878-6669 VL - 64 SP - 819 EP - 829 PB - Springer CY - Berlin AN - OPUS4-50628 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Kromm, Arne A1 - Lausch, Thomas A1 - Schröpfer, Dirk A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Influence of welding stresses on relief cracking during heat treatment of a creep-resistant 13CrMoV steel: Part I - Effect of heat control on welding stresses and stress relief cracking N2 - The avoidance of failures during the fabrication or operation of petrochemical reactors made of creep-resistant, low-alloy steels as 13CrMoV9-10 requires still research despite over 60 years of international investigations in the field of stress relief cracking. The quality of modern base materials and filler metals leads to the fact that previously known crack causes, such as impurities of S or P, recede into the background. Rather, the causes are increasingly to be found in the fabrication process. Investigations on the influence of heat control on the stresses in welded components and thus on the stress relief cracking sensitivity under realistic manufacturing conditions are not yet available. This work is subdivided in two parts. Part 1 of this study focused on the effect of heat control during submerged arc welding on the stresses. For this purpose, a testing facility was applied, which allows to observe the forces and moments accumulating during welding or heat treatment in a component-like specimen under shrinkage restraint. The stress acting in the specimen increases with higher preheat/interpass temperatures and higher heat input. During the heat treatment, the stresses are relieved. Nevertheless, cracks are formed already during heating. The total crack length correlates with the heat input. KW - Welding KW - Creep-resistant steel KW - Post weld heat treatment KW - Stress relief cracking PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-506271 DO - https://doi.org/10.1007/s40194-020-00875-6 SN - 1878-6669 VL - 64 IS - 5 SP - 807 EP - 817 PB - Springer CY - Berlin AN - OPUS4-50627 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Thickness and microstructure effect on hydrogen diffusion in creep-resistant 9 % Cr P92 steel and P91 weld metal N2 - Martensitic 9 %-Cr steels like P91 and P92 show susceptibility to delayed hydrogen assisted cracking depending on their microstructure. In that connection, effective hydrogen diffusion coefficients are used to assess the possible time-delay. The small number of available diffusion coefficients varies already at room temperature by several orders of magnitude (mostly regarded as result of present microstructure). Especially P91 weld metal diffusion coefficients are rare so far. For that reason, electrochemical permeation experiments had been conducted using P92 base metal and P91 weld metal (in as-welded and heat-treated condition) with different thicknesses. The diffusion coefficients are calculated by two methods (time-lag and inflection point method) were performed. The results show that, despite of microstructural effects, the sample thickness must be considered as it influences the calculated diffusion coefficients. Finally, the comparison of calculated and measured hydrogen concentrations (determined by carrier gas hot extraction) enables the identification of realistic diffusion coefficients. T2 - IIW Intermediate Meeting, Comm. IX-C "Welding of creep and heat-resistant materials" CY - Online meeting DA - 08.03.2021 KW - Hydrogen KW - Welding KW - Diffusion KW - Creep-resistant steel KW - Electrochemical permeation PY - 2021 AN - OPUS4-52239 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - HEA Processing - SURDIA - Current R&D at BAM N2 - This presentation summarizes the latest results on the BAM-Themenfeld project SURDIA on processing of high-entropy alloys (HEAs) at BAM. At first, the influence of machining by ultrasonic-assisted milling on the surface integrity is presented. Second, the weld processing by Tungsten Inert Gas (TIG) welding is presented and the results of the Friction Stir Welding (FSW), which is conducted at BAM for the first time. T2 - DFG SSP 2006 - Subgroup meeting on the synthesis and processing of CCAs/HEAs CY - Online meeting DA - 08.10.2021 KW - High-entropy alloy KW - Ultrasonic-assisted milling KW - Welding KW - Processing KW - Surface integrity PY - 2021 AN - OPUS4-53497 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Richter, Tim A1 - Mente, Tobias A1 - Mayr, P. A1 - Nitsche, A. T1 - Thickness and microstructure effect on hydrogen diffusion in creep‑resistant 9% Cr P92 steel and P91 weld metal N2 - Martensitic 9% Cr steels like P91 and P92 show susceptibility to delayed hydrogen assisted cracking depending on their microstructure. In that connection, effective hydrogen diffusion coefficients are used to assess the possible time-delay. Limited data on room temperature diffusion coefficients reported in literature vary widely by several orders of magnitude (mostly attributed to variation in microstructure). Especially P91 weld metal diffusion coefficients are rare so far. For that reason, electrochemical permeation experiments had been conducted using P92 base metal and P91 weld metal (in as-welded and heat-treated condition) with different thicknesses. From the results obtained, diffusion coefficients were calculated using to different methods, time-lag, and inflection point. Results show that, despite microstructural effects, the sample thickness must be considered as it influences the calculated diffusion coefficients. Finally, the comparison of calculated and measured hydrogen concentrations (determined by carrier gas hot extraction) enables the identification of realistic diffusion coefficients. KW - Creep-resistant steel KW - Diffusion KW - Hydrogen assisted cracking KW - Welding KW - Electrochemical permeation PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-540645 DO - https://doi.org/10.1007/s40194-021-01218-9 SN - 0043-2288 SP - 1 EP - 16 PB - Springer Nature Switzerland AG AN - OPUS4-54064 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Nietzke, Jonathan A1 - Richter, Tim A1 - Mente, Tobias A1 - Mayr, P A1 - Nitsche, A T1 - Hydrogen effect on mechanical properties and cracking of creep‑resistant 9% Cr P92 steel and P91 weld metal N2 - Martensitic 9% Cr steels like P91 and P92 can show an increased susceptibility to delayed hydrogen-assisted cracking. The focus of this study was the microstructure and heat treatment efect on the mechanical properties of P92 base material and P91 multi-layer weld metal in both as-welded and post weld heat treated (PWHT) condition. Tensile tests with hydrogen free reference samples and electrochemically hydrogen charged samples were carried out; the mechanical properties were assessed and supported by detailed fractographic analysis. Finally, a hydrogen and microstructure-dependent fracture criterion is established. All investigated microstructures showed a hydrogen-infuenced degradation of the mechanical properties compared to the hydrogen-free reference samples. The as-welded martensitic P91 weld metal had the highest degree of degradation in the presence of hydrogen. The P91 PWHT weld metal and the P92 base material had comparable properties. From that point of view, a signifcantly increased risk for hydrogen-assisted cold cracking during welding fabrication of P91 weld joints must be considered before any heat treatment is conducted. T2 - IIW Annual Assembly, Meeting of Commission IX-C CY - Tokyo, Japan DA - 16.07.2022 KW - Creep-resisting materials KW - Welding KW - Hydrogen assisted cracking KW - Hydrogen embrittlement KW - Mechanical properties PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-564070 DO - https://doi.org/10.1007/s40194-022-01410-5 SN - 0043-2288 SP - 1 EP - 12 PB - Springer Nature CY - Basel (CH) AN - OPUS4-56407 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Richter, Tim A1 - Schröpfer, Dirk A1 - Rhode, Michael T1 - Residual stresses in a high- and a medium-entropy alloy due to TIG and friction stir welding N2 - The new alloying concept of multi-element systems with defined entropy (HEA—high-entropy alloy; MEA—medium-entropy alloy) is gaining increasing importance in materials research. Significantly improved properties or combinations of properties are shown by some HEA/MEA systems. Thus, primarily the production and resulting microstructures of HEA, as well as its properties, have been investigated so far. Furthermore, processing is a main issue in transferring HEA systems from the laboratory to real components. Since welding is the most important joining process for metals, it is crucial to investigate the influence of welding to guarantee component integrity. Welding leads to residual stresses, which significantly affect the component integrity. Hence, the focus of this study is the residual stress formation and distribution in a CoCrFeMnNi HEA and ternary CoCrNi MEA using two different welding processes: tungsten inert gas (TIG) welding and solid-state friction stir welding (FSW). As a pathway for the application of HEA in this investigation, for the first time, residual stress analyses in realistic near-component specimens were performed. The residual stresses were determined by X-ray diffraction (XRD) on the surfaces of top and root weld side. The results were correlated with the local welding microstructures. The results show that both FSW and TIG generate significant tensile residual stresses on the weld surfaces in, and transverse to, the welding direction. In the case of FSW of the CoCrFeMnNi HEA, the longitudinal residual stresses are in the range of the yield strength of approx. 260 MPa in the weld zone. KW - High entropy alloy KW - Welding KW - Residual stresses KW - Microstructure PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-567039 DO - https://doi.org/10.3390/jmmp6060147 SN - 2504-4494 VL - 6 IS - 6 SP - 1 EP - 11 PB - MDPI CY - Basel AN - OPUS4-56703 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröpfer, Dirk T1 - Influence of welding stresses on relaxation cracking during heat treatment of a creep-resistant 13CrMoV steel, Part III N2 - Efficiency and flexibility are currently a major concern in the design of modern power plants and chemical processing facilities. The high requirements for economic profitability and in particular climate change neutrality are driving this development. Consequently, plant equipment and chemical reactor components are designed for higher operating pressure and temperature. Creep-resistant CrMo steels had been used as constructional materials for decades but came to operational limitations, for example the resistance against so-called high-temperature hydrogen attack in petrochemical reactors. For that purpose, 20 years ago V-modified CrMo steels had been developed for use in the petrochemical industry due to their very good creep-strength and hydrogen pressure resistance at elevated temperatures enabling long service life of the respective components. For example, the 13CrMoV9-10 steel is applicable for process temperatures of up to 482 °C and hydrogen pressures of up to 34.5 MPa. Due to the large dimensions and wall thickness of the reactors (wall thickness up to 475 mm) and the special alloy concept, reliable weld manufacturing of the components is extremely challenging. First, low toughness and high strength of the weld joint in the as-welded condition are critical regarding weld cracking. High welding residual stresses are the result of the highly restrained shrinkage of the component welds. For this purpose, the entire component must be subjected to Post-Weld Heat Treatment (PWHT) after completion of the welding operation. The aim is to increase the toughness of the weld joints as well as to reduce the welding induced residual stresses. Before and during PWHT, extreme caution is required to prevent cracking. Unfortunately, V-modified CrMo steels possess an increased susceptibility to cracking during stress relaxation the so-called stress relief cracking (SRC). Available literature studies have largely focused on thermal and metallurgical factors. However, little attention has been paid on the influence of the welding procedure on crack formation during PWHT considering actual manufacturing conditions. For that reason, we investigated in our previous studies (part I and II), the influence of heat control on the mechanical properties by simulating actual manufacturing conditions prevailing during the construction of petrochemical reactors using a special 3D- acting testing facility. The focus of part I was put on the influence of the welding heat control on mechanical stresses and the effect on cracking during PWHT. Part II was mainly dedicated to the metallurgical causes of SRC during PWHT and the interaction with the occurring mechanical stresses. It could be shown that not only high welding-induced stresses due to increased weld heat input cause higher susceptibility for SRC formation. It was further intensified by an altered precipitation behaviour in presence of mechanical stresses that are caused by the component related restraint. The present part III shows how residual stresses, which are present in such welded components and significantly influence the crack formation, can be transferred to the laboratory scale. As a result, the effect on the residual stresses on the SRC behaviour can be evaluated on simplified small-scale specimens instead of expensive mock-ups. For this purpose, experiments with test set-ups at different scales and under different rigidity conditions were designed and carried out. T2 - IIW Annual Assembly, Meeting of Commission II-A CY - Online meeting DA - 20.07.2020 KW - Welding KW - Creep-resistant steel KW - Residual stresses KW - Post weld heat treatment KW - Stress relief cracking PY - 2020 AN - OPUS4-51587 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Influence of various microalloying strategies on the mechanical properties of weld seams in S690QL steel N2 - Microalloying elements such as niobium (Nb) and titanium (Ti) play a crucial role in achieving the desired mechanical properties of quenched and tempered high-strength fine-grained structural steels with a nominal yield strength of ≥ 690 MPa. Current specifications for the chemical composition only define upper limits for these elements, providing manufacturers with some flexibility. However, even minor deviations in alloying concepts can significantly influence the resulting mechanical properties. Consequently, accurately predicting weldability and the integrity of welded joints becomes challenging or even unfeasible due to variations in composition and the associated microstructural changes. Potential adverse effects include the softening of the heat-affected zone (HAZ) or, conversely, localized hardening phenomena. To address these challenges, various microalloying strategies with different Ti and Nb contents are being systematically investigated for the first time using specially designed laboratory-cast alloys. Each alloying approach is based on the commonly used S690QL steel grade while maintaining consistent chemical composition and heat treatment parameters. To evaluate the weldability, three-layer welds were produced using gas metal arc welding (GMAW), and critical microstructural regions, particularly those within the heat-affected zone (HAZ) exhibiting significant softening or hardening, were identified. The influence of the softened HAZ region on failure behavior was assessed through transverse tensile testing. Digital image correlation (DIC) was employed for in situ analysis of local strain distributions across different HAZ regions. In addition, Charpy tests were carried out on BM, WM and HAZ to determine the Charpy impact toughness. This was supported by metallographic analyses and thermodynamic simulation using ThermoCalc. T2 - IIW Intermediate Meeting, Com. II-A CY - Trollhättan, Sweden DA - 10.03.2025 KW - Welding KW - Microalloy elements KW - High strength steels KW - Mechanical properties PY - 2025 AN - OPUS4-62691 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Update on "Call for interested people to contribute to series of comprehensive papers on welding and joining of components for sustainable energy systems" N2 - Based on the initial call in March 2024, an update time-frame is introduced on the working plan for a comprehensive review paper series on joining and welding technologies for the manufacturing of components and parts used in sustainable energy generation, conversion, and transport with focus on hydrogen and wind energy. T2 - 77th IIW Annual Assembly and International Conference, Meeting of Commission II-A CY - Ixia, Rhodes, Greece DA - 07.07.2024 KW - Review paper KW - Research study KW - Hydrogen KW - Joining KW - Welding PY - 2024 AN - OPUS4-60674 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Erxleben, Kjell T1 - Challenges and difficulties in repair welding procedures on in-service hydrogen pipelines N2 - Hydrogen as an energy carrier plays a key role in tomorrow's energy transition. For effective use of hydro-gen as energy carrier the construction of the corresponding infrastructure is of utmost importance. In that context, large diameter long-distance transmission pipelines will form the so-called hydrogen backbone in the European Union with service pressures up to 100 bar (e.g., depending on national regulations). From an economically and ecologically point of view, a major goal is to repurpose the existing natural gas (NG) infra-structure to minimize the need to install new pipelines. To ensure the safety, reliability and integrity of this future hydrogen infrastructure repair welding or further welding of branch pipes etc. can be necessary at in-service conditions, meaning a permanent flow of pressurized hydrogen while executing the repair procedure. The reason is that a shut-down of large diameter pipelines is not easy or sometimes merely impossible. In fact, as long, as no oxygen enters the pipeline, there will neither be any combustion nor (in the worst-case scenario) explosion. The special techniques like hot tapping or stoppling are state-of-the-art for NG and oil pipeline grids. Currently, it is not finally clarified if repair welding procedures for NG pipelines can be trans-ferred to pure hydrogen pipelines. In opposite to NG, hydrogen can be way easier absorbed to the pipeline steels and diffuses through the material. If it accumulates in susceptible regions, i.e., in the welded joint or heat affected zone, hydrogen assisted embrittlement could occur and lead to loss of integrity or even cata-strophic failure of the pipeline. For example, requires the planned welding procedure a preheating and maintenance of the weld joint of up to 300°C for up to several hours at the outer. This temperature is way higher compared to the typical service temperature of max. 60°C at operational pressures of up to 100 bar. In accordance to API 941, these low-alloyed pipeline steels are subjected to short-term service loads, which they are not designed for. Another considerable fact is that if the weld seam is attached to the pipeline, the temperature especially for small wall thickness can be easily above the austenitization temperature. It is well known that austenite has a way higher hydrogen solubility compared e.g. to ferrite/bainite microstructure of the low-alloyed steel. Current studies indicate a remarkable increase of the hydrogen ingress dur-ing the austenitization from the inner pipe wall. It must be answered if a critical material degradation because of increased hydrogen uptake due to in-service welding procedures is likely to occur. T2 - MPA Seminar 2024 CY - Stuttgart, Germany DA - 08.10.2024 KW - In-service KW - Pipeline KW - Hydrogen KW - Welding KW - Repair PY - 2024 AN - OPUS4-61468 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Becker, Amadeus T1 - Consideration of design influences to provide adequate repair concepts for high-strength steel weld joints in offshore support structures N2 - The sustainable and resource-efficient production of offshore wind turbines requires the use of modern high-strength fine-grained structural steels (Martin and Schroeter, 2005). This applies to wind turbines in terms of increasing turbine sizes as well as to maintenance and installation vessels and equipment (Ummenhofer et al., 2013). Without the demanded high load-bearing capacities and boom lengths, the economic realization of these goals would be inconceivable. During the assembly of high-strength steel structures, unacceptable defects can occasionally be found in the weld area, although the welding process was executed in accordance with the specifications. In most cases, the economical solution would be local thermal gouging of the affected areas and re-welding. Corresponding standards hardly provide any information on adequate repair concepts, and there is no uniform scientific data on which to base such concepts. This applies particularly to the consideration and optimization of welding-induced stresses due to the high shrinkage hindrance of the gouging grooves and degradation of the adjacent microstructures by gouging and re-welding. The result, especially in the case of high-strength steel grades, are frequently recurring imperfections as well as a missing consideration of the additionally induced welding stresses in the design of the structure. In this context, at BAM component-relevant investigations focused on welding residual stress evolution and microstructural degradation during repair of weld joints due to local thermal gouging and re-welding are carried out within the scope of a FOSTA project (P1311, IGF 20162N). In this study, several relevant findings are discussed based on examples of structural engineering focusing on mechanical-technological properties and residual stresses, for instance found by (Schasse, 2017). Also experimental and numerical work as conducted by (Wongpanya, 2008) and weld tests under defined shrinkage restraint in special weld test-setups for research projects, e. g. FOSTA-P922 (Kannengiesser and Schroepfer, 2015) and P1011 (Kannengiesser and Schroepfer, 2017) have shown that an optimization of the welding-induced stresses of high-strength structural steels is specifically achievable by means of adapted heat control concepts (Schroepfer, 2017). The present research involves systematic investigations of influences of shrinkage restraint, the number of repair cycles and heat control during repair welding of the relatively new developed offshore-relevant high-strength steel S500MLO (EN 10225-1). For the quantification of the shrinkage restraint of weld joints, the concept of restraint intensity established by (Satho et al., 1973) was applied analogous to recent research, e. g. (Schwenk et al., 2008). By means of structural mechanics calculations, geometries of self-strained specimens were identified, that represent different defined rigidity conditions of repair welds of real components, cf. Fig. 1. It could be shown that with increasing weld joint restraint intensity significantly higher residual stresses in the weld metal and heat affected zone up to 80 % of the nominal yield strength occur, cf. Fig. 2. In relation to existing results, it has been shown that a safe repair of such welds can only be achieved by means of appropriate repair concepts and heat control taking the high welding stresses and special microstructures of high-strength steels into account. Finally, the aim of this research is to derive recommendations for repair concepts appropriate to the stresses and materials involved providing a basis for standards and guidelines, especially for SMEs, in order to avoid damage and, in most cases, expensive reworking and to improve the full utilization of the potential of high-strength steels. T2 - Wind Energy Science Conference 2021 CY - Online meeting DA - 25.05.2021 KW - High-strength structural steels KW - Welding KW - Repair KW - Residual stresses KW - Restraint PY - 2021 AN - OPUS4-53319 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Richter, Tim T1 - Characterization of Hydrogen Diffusion in a Thick-walled Submerged Arc Multi-Layer Weld Joint N2 - The energy production of the future will be dominated by CO2-emission free techniques like wind turbines and become essential in scope of the planned hydrogen economy. As onshore installation capacity is limited, the in-crease of the number of offshore wind turbines (OWT) is a major goal. In that connection, the OWTs continuously increase in size and weight and demand adequate foundations concepts like monopiles or tripods. These compo-nents are typically manufactured from welded mild steel plates with thickness up to 200 mm. The predominant welding technique is submerged arc welding (SAW) with up to five wires. In accordance with the standards, the occurrence of delayed hydrogen assisted cracking is anticipated by either a hydrogen removal heat treatment (HRHT) or a so-called minimum waiting time (MWT) before non-destructive testing (NDT) of the respective weld joint is allowed. The reason for the MWT is the necessary time for the hydrogen diffusion at ambient temperature due the high plate thickness. Both the effectiveness of a HRHT at elevated temperatures or the MWT at ambient temperature can be estimated by calculation of the diffusion time. This time depends on reliable hydrogen diffu-sion coefficients and these are rare in literature. For that reason, this study presents the hydrogen diffusion coef-ficients obtained from a multi-layer SAW joint of an offshore steel grade. Two different experimental techniques were used to identify the respective diffusion behavior: (1) hydrogen desorption experiments with a carrier gas hot extraction analyzer at elevated temperatures for the characterization of a HRHT and (2) the electrochemical permeation technique at ambient temperature for the characterization of an MWT. From both experiments, the respective diffusion coefficients were calculated. The obtained DCs are different from those reported in literature, i.e., the duration or applicability of a HRHT or MWT must be critically discussed. T2 - European Congress and Exhibition on Advanced Materials and Process - Euromat 2021 CY - Online meeting DA - 13.09.2021 KW - Welding KW - Offshore KW - Wind turbine KW - Hydrogen KW - Cracking PY - 2021 AN - OPUS4-53296 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schroeder, Nina T1 - Influence of microalloying on precipitation behavior and notched impact strength of welded high-strength structural steels N2 - This presentation summarizes the latest results on the microalloying influence on the preciptitation behavior on the mechanical properties of welded high-strength steel with a design yield strength of 690 MPa and above. For that reason, Charpy tests were performed for the pure weld metal and different heat-affected zones. Thermodynamic phase field modeling showed the usefulness of calculations in Thermocalc to predict the preciptiation behavior and (finally) to conclude the mechanistic behavior of the welded joint. T2 - IIW Intermediate meeting of Commission II-A CY - Garching, Germany DA - 06.03.2023 KW - Welding KW - High-strength steel KW - Phase field modeling KW - Preciptiates KW - Microstructure characterization PY - 2023 AN - OPUS4-57107 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Joining Processes in Hydrogen Technologies - Current need and future R&D activites, a review N2 - This study gives an overview on the important field of joining processes for component fabrication in hydrogen technologies. For that reason, the current need and future research and developement activites are highlighted for the different technological field of hydrogen generation, storage, transport and use. In addition, the emerging field of additive manufacturing is included. Finally, some remarks are given for necessary changes in the standardization and its challenges. T2 - 46th Seminar - Additive Manufacturing, Hydrogen, Energy, Integrity CY - Online meeting DA - 12.10.2021 KW - Hydrogen KW - Joining process KW - Welding KW - Review KW - Research and Development PY - 2021 AN - OPUS4-53554 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Joining processes for components in hydrogen technologies: Current need and future importance N2 - This presentation gives an overview on the importance of joining processes for component fabrication in hydrogen technologies. For that reason, the current need and future research and developement activites are highlighted for the three technological fields: hydrogen storage, transport and use (in terms of the emerging field of additive manufacturing). Finally, some remarks are given for necessary changes in the standardization. T2 - IIW Intermediate Meeting, Comm. II-A "Welding Metallurgy" CY - Online meeting DA - 17.03.2022 KW - Hydrogen KW - Welding KW - Research KW - Review KW - Additive manufacturing PY - 2022 AN - OPUS4-54488 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - A decarbonized future requires pipelines for CO2? A brief overview on perspectives and challenges N2 - Despite the use of hydrogen, for example, in various industrial production processes, CO2 emissions are still unavoidable in the medium term. For example, cement, lime and glass production or waste recycling (waste-to-energy plants) will continue to emit CO2 due to the processing involved chemical reactions. Conversely, the chemical industry with its value chains needs CO2 / carbon as a primary raw material for all compounds that fall within the organic chemistry. In this connection, carbon capture utilization (CCU) will play a key role here. In addition to “natural” methods (via reforestation and the dilution of moors), carbon capture storage (CSS) is already playing a major role, for example by injecting it into old natural gas underground caverns. The resulting quantities of CO2 have to be transported on a large scale and similar to hydrogen pipelines, there are concrete plans for CO2 pipeline networks. For this reason, this presentation provides an introduction to the topic and briefly outlines the associated challenges. On the one hand, these lie in the qualification (testing and construction) and especially in the operation of the pipelines with regard to strict monitoring of the gas quality (e.g. carbonic acid corrosion) and in the avoidance of critical service conditions (sudden pressure fluctuations), which can lead to localized condensation. Among other things, this can lead to the lowering of the typically welded low-alloyed steel pipes below the ductile brittle transition temperature (DBTT) and thus can have an impact on pipeline integrity. T2 - 49th MPA Conference CY - Stuttgart, Germany DA - 06.10.2025 KW - CO2 KW - Pipeline KW - Welding KW - Testing PY - 2025 AN - OPUS4-64316 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Ti and Nb influence on the HAZ microstructures of weld-simulated high-strength structural steel S690QL N2 - High-strength low-alloyed (HSLA) steels with yield strength / proof stress ≥ 600 MPa are the basis of modern light-weight steel constructions. Indeed, the economic and ecological benefits strongly depend on their processability in terms of welding. In this context, the use of highly productive welding processes, suitable welding consumables is of vital interest and requires a fundamental understanding of the microstructural changes in the HSLA steel and especially the heat-affected zone (HAZ) of the welded joint. Microalloying elements, such as Ti or Nb, are essential to achieve the desired mechanical properties. In this context, the underlying standards (such as EN 10025-6) only specify maximum values, resulting in different manufacturer customized microalloy concepts. Furthermore, even small deviations can have a drastic effect expressed by an excessive hardening or softening despite identical welding conditions and filler metal. The reason is the different thermal stability of the Ti and Nb-related precipitates (typically carbides or carbon nitrides). As a result, it is difficult (or even impossible) to adequately predict the weldability. Against this background, different microalloying routes with varying Ti and Nb contents for a S690QL reference grade were systematically investigated in terms of lab-cast alloys close to realistic chemical compositions. To investigate the influence of the welding heat input on the HAZ microstructure formation, physical simulations were carried with specified peak temperatures and cooling times (by a dilatometry). The focus was the identification of the occurring phase transformations during cooling and the final HAZ microstructure. In this context, a double welding cycle was simulated to further identify the behavior of the so-called intercritical HAZ (where softening is likely to occur) in case of the common multi-layer welding for thick plates. The results showed: (1) microalloying has significant influence on the formation of the individual HAZ dependent on (2) the thermal stability of the Ti or Nb-precipitates and (3) synergistic effects of further elements such as Mo and their effect on phase transformations in the HAZ. The results represent a microstructure-based validation of welding processing of such HSLA-steels e.g. in terms of preferred microalloy and weld heat input combinations. T2 - 49th MPA Conference CY - Stuttgart, Germany DA - 06.10.2025 KW - High-strength steel KW - Microalloy elements KW - Welding KW - Weld simulation KW - Microstructure PY - 2025 AN - OPUS4-64319 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Manzoni, Anna Maria T1 - Mechanical performance and integrity of tungsten inert gas (TIG) welded CoCrFeMnNi high entropy alloy with austenitic steel AISI 304 N2 - High entropy alloys (HEA) are a new class of materials that have been investigated since the early 2000s and offer great potential to replace conventional alloys. However, since they sometimes have significant contents of expensive alloying elements such as Co or Ni, their use is only conceivable in highly stressed areas of components. For this purpose, the weldability with conventional alloys such as high-alloy austenitic steels must be investigated. In addition to the resulting microstructure, the mechanical properties are also fundamental for the usability of HEAs in DMWs. For this purpose, TIG welds of CoCrFeMnNi HEA (cold rolled and recrystallized state) with AISI 304 austenitic steel are investigated. These mechanical properties are analyzed in this work by means of tensile tests and local hardness measurement. The local strain behavior of the welded joints is also characterized by means of Digital Image Correlation (DIC). The results of the local hardness measurement show a clear influence of the initial condition of the HEA on the HAZ. Thus, the HEA in the cold-rolled condition shows a clear softening because of recrystallization processes in the HAZ. On the other hand, there is no influence on the hardness of the weld metal, which is approx. 200 HV0.1 in both cases. The tensile tests show a consistent failure of the weld in the weld metal. However, regardless of the HEA condition, strengths in the range of the recrystallized HEA (RM ~ 550–600 MPa) are achieved, although with significantly reduced fracture elongations. T2 - International Conference on High-Entropy Materials (ICHEM 2023) CY - Knoxville, TN, USA DA - 18.06.2023 KW - Multi-principal element alloys KW - Welding KW - Mechanical properties KW - Dissimilar metal weld KW - Digital image correlation PY - 2023 AN - OPUS4-57713 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Welding of high-entropy alloys - New material concept vs. old challenges N2 - HEAs represent a relatively new class of materials. The the alloy concept is fundamentally different from the most conventional materials and alloys that are used today. Recently, the focus of HEA designs is more application-based. For that purpose, the elements of interest are carefully selected and multiple phases as well as micro-structures are deliberately adjusted. Currently, only limited attention has been paid to weldability of HEA. This encompasses possible effects on metallurgy and its influence on the desired properties. It remains open if welding causes e.g. considerable number of intermetallic phases or segregations and their effect on weld joint properties. For that reason, the scope of this study is to summarize already available studies on welding of HEAs with respect to the HEA-type, the applied welding process and its influence on the weld joint properties. T2 - IIW Annual Assembly, Meeting of Commission II-A CY - Online meeting DA - 20.07.2020 KW - High-entropy alloy KW - Welding KW - Review PY - 2020 AN - OPUS4-51116 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Manzoni, Anna Maria T1 - Reliable welding of high-entropy alloys N2 - The importance of high-entropy alloy (HEAs) in the field of materials research is increasing continuously and numerous studies have been published, recently. These are mainly focused on manufacturing of different alloy systems having excellent structural properties from low to high temperatures. Therefore, HEAs are of high potential for many applications in very demanding conditions. However, this is so far limited by poor knowledge and experience regarding economic and reliable component manufacturing. The processability of HEAs has hardly been investigated so far, indicated by the small number of publications worldwide: welding <30 and machining <5. Hence, this contribution provides an overview about the current state of the art on processing of HEAs. Fundamental principles are shown for safe weld joints while ensuring high component integrity. For safe welding, the combined consideration of complex interactions of material, construction and process is necessary. Recent studies on different HEAs showed the influence of heat input by means of different welding processes on the microstructure and respective properties. Based on intensive literature survey and on our initial study, the main research objectives of processing HEAs are presented. T2 - ICHEM 2020 - Third International Conference on High Entropy Materials CY - Berlin, Germany DA - 27.09.2020 KW - High Entropy Alloy KW - Welding KW - Welding processing influences PY - 2020 AN - OPUS4-51591 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Processing and application properties of multiple principal element alloys (MPEA) N2 - The presentation gives an overview of BAM's activities on processing influences and application properties of MPEAs in the form of joined and machined high and medium entropy alloys (CoCrFeMnNi and CoCrNi). In the case of welding, the focus is on defect-free welded joints with sufficient mechanical properties. In the case of machining, the focus is on the possible influence on the surface quality of the materials through adequate milling parameters. In addition, the hydrogen absorption and diffusion properties as well as the electrochemical corrosion behavior are fundamentally examined. T2 - FAU-Department Werkstoffwissenschaften, Seminar: Aktuelle Probleme der Werkstoffwissenschaften CY - Erlangen, Germany DA - 25.04.2024 KW - Welding KW - Application properties KW - Machining KW - High-entropy alloy KW - Hydrogen PY - 2024 AN - OPUS4-59975 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -