TY - CONF A1 - Piechotta, Christian A1 - Köppen, Robert A1 - Becker, Roland A1 - Traub, Heike A1 - Ostermann, Markus T1 - Changes in polymer surface morphology and leaching of brominated flame retardants induced by different weathering scenarios N2 - In addition to previously reported results on the accelerated weathering of polystyrene samples (PS) containing 1 wt.% hexabromocyclododecane (HBCD), we present the first results of our investigations of polypropylene samples (PP) containing 0.1 wt.% BDE-209. All studied polymer samples were exposed to a defined weathering schedule in a climate chamber in accordance to regulation EN ISO 4892-3:2006. For the determination of BDE-209 in the collected raining water the samples were prepared in accordance to a validated protocol. Before the analyses each sample was spiked with isotopically labeled BDE-209. Subsequently the samples were extracted with isooctane. The obtained extracts were concentrated, and the resulting solutions were analyzed by GC/MS. Additionally, the total bromine content was monitored for the weathered and untreated samples using laser ablation inductively coupled plasma mass spectrometry (LA-ICP-MS) and X-ray fluorescence analysis (XRF) as a non-destructive and rapid method. In general, the resulting data from the accelerated weathering will be compared to those from the natural weathering experiments. Here, the surfaces of the test pieces were analyzed by LA-ICP-MS and XRF as well. Moreover, soil bed tests were conducted in a well characterized model soil. This soil (boulder-clay, sand with 12 % loam, particle size in total 0.2-4 mm) is filled in a free-draining basin inside of an air-conditioned cellar. In this manner, TOC, water capacity and humidity are recorded parameters. To induce a leaching process from the samples by the raining water, the target water content is calculated to 8%. The actual humidity is measured by a tensiometer, assuring the duration of the raining period. A defined humidity is a fundamental parameter for a biological activity in the soil. The test polymers were placed up to the half in the soil. Microbial activity of the soil is monitored by a reference polymer (polyurethane) and should induce the release of HBCD and BDE-209 out of the test materials. These released analytes will be captured by passive samplers (silicone tubes) placed in a distinct distance to the polymer samples in the soil. The soil bed experiments are complementary to the weathering experiments due to the biological activity in the soil. T2 - ANAKON 2019 CY - Münster, Germany DA - 25.03.2019 KW - BFR KW - LA-ICP-MS KW - XRF KW - Polymer PY - 2019 N1 - Folien in deutscher Sprache, Votrag, Titel und Abtract in englischer Sprache AN - OPUS4-49796 LA - mul AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Aristia, Gabriela T1 - Fenomena Korosi pada aplikasi panas bumi N2 - To accelerate the development of Indonesian geothermal energy, progress should be done in all aspects. Corrosion is an important part on the technological development to ensure the safety and longevity of a power plant. T2 - Fireside Chat der Indonesischen Botschaft CY - Berlin, Germany DA - 21.11.2019 KW - Corrosion KW - Korosi KW - Korrosion PY - 2019 AN - OPUS4-49735 LA - mul AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -