TY - CONF A1 - Rhode, Michael A1 - Nietzke, Jonathan A1 - Richter, Tim T1 - Hydrogen diffusion and desorption characteristics of a CoCrFeMnNi high entropy and a CoCrNi medium entropy alloy N2 - High-entropy alloys (HEAs) are innovative high-performance materials that have attracted more and more research attention. HEAs are characterized by a solid solution of typically five equiatomic metallic elements. In addition, medium-entropy alloys (MEA, with three elements) are of interest and become more and more important. Depending on the alloy concept, HEAs and MEAs show exceptional mechanical properties, especially high-strength and ductility combinations at both cryogenic and elevated temperatures combined with excellent corrosion resistance. Future structural HEA/MEA components can be exposed to potential applications with hydrogen containing environments like high-temperature water in pressurized nuclear reactors or aerospace structures. Other potential applications could be in materials for vessel walls in the field of cryogenic and high-pressure hydrogen storage. So far, the susceptibility of HEAs/MEAs to hydrogen assisted cracking (if any) and the hydrogen diffusion is not investigated in detail yet and can limit or extend possible applications of HEA/MEA as structural materials. In our work, we focused on the hydrogen absorption, diffusion, and distribution in a HEA (CoCrFeMnNi the original Cantor-alloy) and a MEA (CoCrNi). Cathodic hydrogen charging was carried out for the hydrogen ingress, and thermal desorption analysis (TDA) revealed complex hydrogen trapping in both alloy types up to 300 °C. The absorbed total hydrogen concentrations were > 100 ppm for the HEA and > 40 ppm for MEA. In addition, the assessment of the peak deconvolution is not trivial and must consider both experimental and microstructure influences. T2 - 4th International Conference on Metals and Hydrogen - Steely & Hydrogen 2022 CY - Ghent, Belgium DA - 11.10.2022 KW - Hydrogen KW - High-entropy alloy KW - Multiple principal element alloy KW - Thermal desorption analysis KW - Diffusion PY - 2022 SP - 1 EP - 11 CY - Ghent, Belgium AN - OPUS4-56076 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Development of a component test for assessment of delayed hydrogen assisted cracking susceptibility of thick walled submerged arc welded high strength offshore steels N2 - Offshore Wind Turbines (OWT) are a key factor in tomorrow's sustainable energy generation. The ever-increasing installation depth and weight of OWTs require suitable foundation concepts such as monopiles or tripods. Typically, mild steels such as S420ML are used with plate thicknesses of up to several hundred mm, resulting in high restraints in the welded joints. The large plate thickness requires high-efficiency welding processes such as submerged arc welding (SAW) with multiple wires. Due to the very high stiffness and plate thickness of the large-scale offshore structure, a susceptibility to time-delayed hydrogen assisted cracking (HAC) may occur. The evaluation of this crack susceptibility is very complex due to the component size and stiffness of real offshore structures. For this purpose, a near-component test geometry was developed to transfer the real stiffness conditions to laboratory (i.e. workshop) scale. The 350 kg mock-up studied consisted of heavy plates (thickness 50 mm, seam length 1,000 m) joined by a 22-pass submerged-arc weld. Additional stiffeners simulated the effect of high restraint or shrinkage restraint of the weld. Extreme scenarios of hydrogen absorption during welding were simulated by using flux in dry (HD < 5 ml/100g Fe) and wet (HD > 15 ml/100g Fe) conditions. Weld residual stresses were determined using a robotic X-ray diffractometer. Areas of critical tensile residual stress (at the level of the yield strength) were found in the weld metal and in the heat affected zone, suggesting that these weld sub-zones are the most critical in the case of hydrogen ingress. To identify possible delayed cracking, the welds were tested by phased array ultrasonic testing (PAUT) after welding, 6 h, 12 h, 24 h, and a maximum of 48 h. Summarized, no significant occurrence of HAC was detected, indicating the high crack resistance of the welded joint, i.e., a suitable combination of base material, welding consumable and parameters. T2 - MSE 2024: International Materials Science and Engineering Congress CY - Darmstadt, Germany DA - 24.09.2024 KW - Hydrogen KW - Offshore wind turbine KW - Component test KW - Submerged arc welding KW - Minimum waiting time PY - 2024 AN - OPUS4-61154 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schröder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Ausscheidungsverhalten und Eigenschaften der schweißbedingten Wärmeeinflusszonen hochfester Stähle in Abhängigkeit der Mikrolegierungsroute N2 - Für eine signifikante Festigkeitssteigerung von vergüteten, hochfesten Feinkornbaustählen mit einer Nominalstreckgrenze ≥ 690 MPa, ist die Zugabe von Mikrolegierungselementen, wie Nb und Ti, unerlässlich. Die Normvorgaben zur chemischen Zusammensetzung dieser Stähle (bspw. in DIN EN 10025-6) geben zur Erzielung der vorgeschriebenen Eigenschaften dabei oft nur Grenzgehalte für die Hersteller vor. Die Wirkung der Legierungselemente in der WEZ ist teilweise komplett konträr. Somit wird eine adäquate Vorhersage der Chargenabhängigkeit hinsichtlich der Schweißeignung und des Tragverhaltens der Schweißverbindung erschwert. Neben metallographischen Untersuchungen einzelner WEZ-Bereiche wurden unter Variation der chemischen Zusammensetzung, thermodynamische Phasenberechnungen mittels ThermoCalc durchgeführt. Hierdurch wird ein Verständnis zur Phasentransformation, Ausscheidungswachstum und -auflösung während des Schweißens in Abhängigkeit von Temperatur und Abkühlbedingungen geschaffen. T2 - 40. Vortrags- und Diskussionstagung Werkstoffprüfung 2022 CY - Dresden, Germany DA - 27.10.2022 KW - WEZ-Erweichung KW - Mikrolegierungseinflüsse KW - Thermodynamische Modellierung PY - 2022 SP - 1 EP - 6 AN - OPUS4-56168 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Assessment of in-service welding conditions for pressurized hydrogen pipelines via component test N2 - Hydrogen is the energy carrier of tomorrow. This requires a reliable transport infrastructure with the ability to carry large amounts of hydrogen e.g. for steel industry or chemical industry. The conversion of existing natural gas (NG) grids is an essential part of the worldwide hydrogen strategies, in addition to the construction of new pipelines. In this context, the transportation of hydrogen is fundamental different from NG as hydrogen can be absorbed into the pipeline material. Given the well-known effects of hydrogen embrittlement, the compatibility of the materials for the intended pipelines must be investigated (typically low alloy steels in a wide range of strengths and thicknesses). However, pipelines require frequent maintenance, repair or the need for installation for further outlets. In some cases, it is necessary to perform welding on or onto the pipelines while they are still in service, i.e. with active gas flow under high pressure, e.g. such as the well-known “hot tapping”, see Fig. 1a. This in-service welding causes challenges for hydrogen operations in terms of additional hydrogen absorption during welding and the material compatibility. The challenge can be roughly divided into the possible austenitization of the inner pipe material exposed to hydrogen, which can lead to sufficient hydrogen absorption, and the welding itself, which causes an increased temperature range. Both lead to a significant increase in hydrogen solubility and diffusivity of the respective materials compared to room temperature. In this context, knowledge about hot tapping on hydrogen pipelines is scarce due to the lack of operating experience. Fundamental experimental investigations are required to investigate the transferability from NG to hydrogen pipeline grids. For this reason, the present study introduces a specially designed mock-up / demonstrator concept for the realistic assessment of the welding processing conditions, see Fig. 1b. The mock-up was designed to enable in-situ temperature measurement during welding as well as ex-post extraction of samples for the quantification of the absorbed hydrogen concentration, see Fig. 1c. For safety measures, the necessary pressurized hydrogen volume was limited by the insertion of a solid cylinder ensuring a 1 cm hydrogen gas layer. Welding experiments on the pressurized mock-ups with the diameters DN50 and DN200 have shown that the austenitization temperature can be reached on the inner surface of the pipeline, especially on thinner-walled pipelines, using current welding practices. This corresponds to an increased hydrogen uptake in the welded area of several ppm T2 - 1st Conference on Hydrogen in Materials Science and Engineering (H2-MSE) CY - Siegburg, Germany DA - 11.02.2025 KW - Hydrogen KW - Pipeline KW - In-service welding KW - Component test PY - 2025 AN - OPUS4-62544 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Microalloying influence on precipitation behavior and mechanical properties of welded high strength structural steels N2 - Microalloying elements, such as Nb and Ti, are essential for the targeted mechanical strength of quenched and tempered, high-strength fine-grained structural steels with a nominal yield strength ≥ 690 MPa. Current specifications for chemical composition only provide upper limits for manufacturers. But even small deviations in the alloying route can have a drastic effect on the mechanical properties. Thus, an adequate prediction of the weldability and the integrity of the welded joint becomes difficult or even impossible due to the varying composition and, hence, the microstructures. Undesirable side effects are the possible softening of the heat-affected zone (HAZ) as well as the opposite effect of hardening. Against this background, different microalloying routes with varying Ti and Nb contents are systematically investigated for the first time on specially designed lab-cast alloys. The basis of each alloy route was the common S690QL in terms of both the chemical composition as well as the heat treatment. To investigate the weldability, three-layer welds were performed using metal active gas welding (MAG) and critical microstructural areas with high softening/hardening were identified. The scope was here on the identification of phase transformations during cooling and on the respective metallurgical precipitation behavior. Isothermal and non-isothermal phase calculations were performed using Thermo-Calc® and showed that the prediction of the non-equilibrium precipitation characteristics during welding is not trivial, especially for this relatively complex chemical composition. The mechanical properties of the welded joints were identified by both Charpy tests (toughness) and tensile tests (strain and strength). During the test, the local straining behavior of the welded joints, was identified using a digital image correlation (DIC) system, see Figure 1. Despite the generally good weldability of the materials, the results show a significant influence of the microalloying route as well as the welding heat input on the different precipitation kinetics. T2 - FEMS EUROMAT 2023 CY - Frankfurt a. M., Germany DA - 04.09.2023 KW - High-strength KW - Steel KW - Mechanical properties KW - Welding KW - Thoughness PY - 2023 AN - OPUS4-58221 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Determination of inner pipe surface temperatures during in-service welding on hydrogen pipelines by means of component-like mock up experiments N2 - Hydrogen is considered as one of the most important energy carriers in the future. The necessary large-scale transport over long distances requires a suitable pipeline infrastructure. Current plannings encompass a dual-way strategy of repurposing existing natural gas (NG) pipelines, supplemented by the construction of new hydrogen pipelines. In some cases, such as necessary grid extensions or installation of bypasses in case of repair work, techniques like “hot tapping” are applied. These techniques include so-called in-service welding on pressurized pipelines and are state-of-the-art for NG grids and oil pipelines. The existing NG pipeline grid consists of a wide range of materials with different strengths, diameters, and wall thicknesses. In this context, the material compatibility is crucial. The main difference between hydrogen and NG is that hydrogen can both penetrate the material and cause hydrogen embrittlement. In that connection, in-service welding encompasses elevated temperatures for a certain time during the typically multi-layer welding process. Locally even austenitization temperature can be reached or surpassed. Austenite has a higher hydrogen solubility at a significantly lower diffusion rate, which could lead to a critical hydrogen accumulation. Especially the inner pipe surface temperature is from utmost interest, as this interface is exposed to the pressurized hydrogen (up to 100 bar). However, direct measurement of the locally occurring temperatures is very challenging. For this reason, a component-like geometry was developed. The geometry consists of a pipeline segment with a metal sheet joined to the pipe segment, representing similar heat dissipation conditions as in the field. In addition, typical welding parameters were applied that are currently used in the NG grid. This allows the welding of realistic multi-layer fillet welds on the outer pipe wall with simultaneous temperature measurement using manifold thermocouples at defined positions: (1) adjacent to the weld seam on the outer pipe surface, (2) on the inner pipe surface and (3) on the welded metal sheet. To ensure realistic conditions, manual shielded metal arc welding (SMAW) and gas tungsten arc welding (GTAW) was investigated. The effects of different wall thicknesses and welding heat inputs on the temperature distribution and peak temperatures achieved on the inner pipe surface during welding vary depending on the chosen method. Peak temperatures above austenitization temperature up to 1078 °C have been measured on L245 pipes with wall thickness of 3.6 mm. For pipes made from higher strength materials, such as L485, with a wall thickness of 8 mm, peak temperatures between 607 °C and 755 °C were recorded. Temperature and austenitization directly affects hydrogen diffusivity and solubility, showing the importance of the findings. The temperature profile and cooling conditions influence the mechanical properties of the material as well. For this reason, metallurgical investigations are carried out to assess the hardness and microstructure of the welds. Hardening up to 248 HV10 was detected in the heat-affected zone (HAZ) of the top layer, which could lead to a locally increased susceptibility to hydrogen assisted cracking. Meanwhile, the minimum hardness found in the HAZ of the root layer was as low as 144 HV10, indicating a softening. The results of this study provide valuable insights into the suitability of existing materials and geometries for hydrogen transport. Secondly, the data collected will serve as a basis for planned numerical simulations to further improve knowledge and optimize welding processes to ensure the integrity and safety of hydrogen pipelines. T2 - IIW Intermediate Meeting, Com. II-A CY - Trollhättan, Sweden DA - 10.03.2025 KW - Testing KW - In-service welding KW - Hydrogen KW - Pipelines PY - 2025 AN - OPUS4-62690 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Influence of various microalloying strategies on the mechanical properties of weld seams in S690QL steel N2 - Microalloying elements such as niobium (Nb) and titanium (Ti) play a crucial role in achieving the desired mechanical properties of quenched and tempered high-strength fine-grained structural steels with a nominal yield strength of ≥ 690 MPa. Current specifications for the chemical composition only define upper limits for these elements, providing manufacturers with some flexibility. However, even minor deviations in alloying concepts can significantly influence the resulting mechanical properties. Consequently, accurately predicting weldability and the integrity of welded joints becomes challenging or even unfeasible due to variations in composition and the associated microstructural changes. Potential adverse effects include the softening of the heat-affected zone (HAZ) or, conversely, localized hardening phenomena. To address these challenges, various microalloying strategies with different Ti and Nb contents are being systematically investigated for the first time using specially designed laboratory-cast alloys. Each alloying approach is based on the commonly used S690QL steel grade while maintaining consistent chemical composition and heat treatment parameters. To evaluate the weldability, three-layer welds were produced using gas metal arc welding (GMAW), and critical microstructural regions, particularly those within the heat-affected zone (HAZ) exhibiting significant softening or hardening, were identified. The influence of the softened HAZ region on failure behavior was assessed through transverse tensile testing. Digital image correlation (DIC) was employed for in situ analysis of local strain distributions across different HAZ regions. In addition, Charpy tests were carried out on BM, WM and HAZ to determine the Charpy impact toughness. This was supported by metallographic analyses and thermodynamic simulation using ThermoCalc. T2 - IIW Intermediate Meeting, Com. II-A CY - Trollhättan, Sweden DA - 10.03.2025 KW - Welding KW - Microalloy elements KW - High strength steels KW - Mechanical properties PY - 2025 AN - OPUS4-62691 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Kaltrissprüfung für Offshore-Gründungen N2 - Die klassische Prüfung der verzögerten, wasserstoffunterstützten Kaltrissbildung von Schweißnähten umfasst mehr als 200 mögliche Prüfverfahren. Von diesen hat aber nur ein kleiner Teil praktische Bedeutung. Unabhängig davon, sind die Prüfverfahren typischerweise auf kleine Bauteilgeometrien beschränkt bzw. hinsichtlich ihrer Anwendungsfähigkeit für große Struktruren oder dickwandige, UP-geschweißte Komponenten wie Monopiles. Als Gründundgsstrukturen für Offshore-Windenergieanlagen können die Monopiles Größen bis zu 9 m Durchmesser, Längen bis zu 100 m, bei Gewichten bis zu 1.300 t erreichen. Hier ist eine Prüfung auf verzögerte Kaltrissbildung schwer durchführbar bzw. muss eine Wartezeit von bis zu 48 h eingehalten werden. Die voliegenende Präsentation gibt einen Überblick über an der BAM entwickelte Demonstratorgeometrien um eine praktikable Kaltrissprüfung auf Laborebene zu ermöglichen. Allerdings unter Beibehaltung der realen Steifigkeits- und Wärmeableitungsbedingungen, wie bei realen Großkomponenten. Zusätzlich wird ein Überblick über die Möglichkeiten von Wasserstoffdiffusionsmessungen zur Ermittlung von Diffusionskoeffizienten gegeben, die wiederum Anwendung in der numerischen Simulation der Wasserstoffdiffusion finden. T2 - Vortragsreihe des DVS e.V. - Bezirksverband Rostock CY - Rostock, Germany DA - 05.12.2024 KW - Schweißen KW - Rissbildung KW - Monopile KW - Kaltriss KW - Komponententest PY - 2024 AN - OPUS4-62033 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Fügetechnik in Wasserstofftechnologien: Prozesse und Perspektiven N2 - Der Vortrag gibt einen tiefen Überblick über die Bedeutung der Füge- und Schweißtechnik in Wasserstofftechnologien. Dazu gliedert sich der Vortrag in die Komplexe H2-Erzeugung, Speicherung, Transport, Anwendung auf und gibt jeweils repräsentative Industriebeispiele für den heutigen Anwendungsstand. Insbesondere werden hier Fertigungstechnologien für Brennstoffzellen vorgestellt, sowie Herausforderungen beim Reparaturschweißen von Wasserstoffpipelines. Zeitgleich wird in einem eigenen Kapitel die Bedeutung der additiven Fertigung ebenso erläutert, wie die aktuellen und umfassenden Tätigkeiten auf dem Gebiet der Normung zu H2-Technologien. T2 - Vortragsreihe der VDI-Ortsgruppe Magdeburg CY - Magdeburg, Germany DA - 23.10.2023 KW - Wasserstofftechnologien KW - Fügetechnik KW - Pipelines KW - Additive Fertigung KW - Normung PY - 2023 AN - OPUS4-58671 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Microstructure and local mechanical properties of friction stir welded dissimilar joints of CoCrFeMnNi and CoCrNi to austenitic steel AISI 304 N2 - Multiple principal element alloys (MPEA) represent a meanwhile widely investigated material class, which encompass high-entropy (HEA) and medium-entropy alloys (MEA). They are fundamentally different from conventional materials like Fe-Cr-Ni-based austenitic steels. However, the focus has been merely on the material synthesis. With the increase in available material quantities, the focus is now shifting to processing issues such as joining and welding. In this context, the weldability of MPEAs has received very little attention so far. In addition, MPEA/HEA/MEA are and will be expensive due to the alloying concept. From this point of view, also such materials will also have to be joined with other conventional materials like austenitic steels. In particular, there is a lack of experience with dissimilar metal welds (DMWs) and the corresponding mechanical properties. For this reason, the present study summarizes comprehensive experimental results on equiatomic CoCrFeMnNi (HEA) and CoCrNi (MEA), joined by solid-state friction stir welding (FSW) to an austenitic steel AISI 304. The mechanical properties were obtained by cross-weld tensile tests. For the first time (for these welding process and materials), the local strains in the different weld microstructures were measured in-situ by digital image correlation (DIC). A significant influence of the FSW process on both the resulting microstructure and the mechanical performance of the DWMs was identified. For example, the dynamic recrystallization plays a significant role in the performance of the welded joint. In addition, the FSW experiments proofed the weldability of both MPEAs when joined to austenitic steel AISI 304. This allows for further focused consideration of these highly innovative MPEAs. T2 - MSE 2024: International Materials Science and Engineering Congress CY - Darmstadt, Germany DA - 24.09.2024 KW - High-entropy alloy KW - Dissimilar metal weld KW - Microstructure characterization KW - Mechanical properties KW - Friction stir welding PY - 2024 AN - OPUS4-61157 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Update on "Call for interested people to contribute to series of comprehensive papers on welding and joining of components for sustainable energy systems" N2 - Based on the initial call in March 2024, an update time-frame is introduced on the working plan for a comprehensive review paper series on joining and welding technologies for the manufacturing of components and parts used in sustainable energy generation, conversion, and transport with focus on hydrogen and wind energy. T2 - 77th IIW Annual Assembly and International Conference, Meeting of Commission II-A CY - Ixia, Rhodes, Greece DA - 07.07.2024 KW - Review paper KW - Research study KW - Hydrogen KW - Joining KW - Welding PY - 2024 AN - OPUS4-60674 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Component test for simplified testing of hydrogen‐assisted delayed cold cracking of high‐strength, submerged arc‐welded offshore steel structures N2 - Offshore Wind Turbines (OWT) are a key factor in tomorrow's sustainable energy generation. The ever-increasing installation depth and weight of OWTs require suitable foundation concepts such as monopiles or tripods. Typically, mild steels such as S420ML are used with plate thicknesses of up to several hundred mm, resulting in high restraints in the welded joints. The large plate thickness requires high-efficiency welding processes such as submerged arc welding (SAW) with multiple wires. Due to the very high stiffness and plate thickness of the large-scale offshore structure, a susceptibility to time-delayed hydrogen assisted cracking (HAC) may occur. The evaluation of this crack susceptibility is very complex due to the component size and stiffness of real offshore structures. For this purpose, a near-component test geometry was developed to transfer the real stiffness conditions to laboratory (i.e. workshop) scale. The 350 kg mock-up studied consisted of heavy plates (thickness 50 mm, seam length 1,000 m) joined by a 22-pass submerged-arc weld. Additional stiffeners simulated the effect of high restraint or shrinkage restraint of the weld. Extreme scenarios of hydrogen absorption during welding were simulated by using flux in dry (HD < 5 ml/100g Fe) and wet (HD > 15 ml/100g Fe) conditions. Weld residual stresses were determined using a robotic X-ray diffractometer. Areas of critical tensile residual stress (at the level of the yield strength) were found in the weld metal and in the heat affected zone, suggesting that these weld sub-zones are the most critical in the case of hydrogen ingress. To identify possible delayed cracking, the welds were tested by phased array ultrasonic testing (PAUT) after welding, 6 h, 12 h, 24 h, and a maximum of 48 h. Summarized, no significant occurrence of HAC was detected, indicating the high crack resistance of the welded joint, i.e., a suitable combination of base material, welding consumable and parameters. T2 - MPA Seminar 2024 - Materials, Processes, Applications CY - Stuttgart, Germany DA - 08.10.2024 KW - Hydrogen KW - Offshore wind turbine KW - Component test KW - Submerged arc welding KW - Minimum waiting time PY - 2024 AN - OPUS4-61323 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Evaluation of the wear protection of modified NiMoCrSi alloy and machinability using ultrasonic-assisted milling N2 - The development of technologies for climate-neutral energy generation is an important contribution to reducing CO2 emissions, whereby the efficient use of material systems is a key factor. Wear-resistant coatings are required for highly efficient and economical steel components in energy, process and power plant engineering in order to withstand the high corrosive, tribological, thermal and mechanical loads. Considering price and supply risks as well as the increasing demands on corrosive resistance at high temperatures, conventional cobalt alloys are to be replaced by nickel alloys. In addition, there is a growing demand for defined surfaces of high quality or functional surfaces of these protective coatings. The milling required for this is often not economically feasible, especially for SMEs, due to high tool wear. A joint project of BAM and ISAF of TU Clausthal (Fosta P1550/IGF 21959 N) investigates the optimization of these challenging machining conditions by means of alloy modifications of the welding powder for plasma transferred arc cladding, without reducing the wear protection potential and using innovative ultrasonic assisted milling process for better machinability without reducing wear resistance. This article presents the results of investigations into the relationships between different alloy modifications (Ti, Al, Nb Mo and Hf with wX ≤ 0.01), the resulting microstructure and precipitation morphology, the machinability and the wear protection properties using a NiCrMoSiFeB alloy (trade name: Colmonoy 56 PTA). Tests using cast samples have already shown that the addition of Nb leads to a finer distribution of the hard phases and that this results in a reduction in cutting forces and tool wear during ultrasonic-assisted milling. The change in the microstructure morphology through the addition of Al, on the other hand, causes a significant increase in the cutting forces that occur. T2 - IIW Intermediate meeting of Commission II-A CY - Online meeting DA - 12.03.2024 KW - Ultrasonic assisted milling KW - Surface integrity PY - 2024 AN - OPUS4-61924 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Bericht zum Fortschritt des Projektes "Entwicklung von Wärmenachbehandlungskonzepten zur Vermeidung von Spannungsrelaxationsrissen" zur Sitzung des FA1 N2 - Dieses Dokument fasst den Projekfortschritt des BAM-Projektes "Entwicklung von Wärmenachbehandlungsstrategien zur Vermeidung von Spannungsrelaxationsrissen" im Rahmen des Fachausschusses 1 "Schweißmetallurgie" des DVS e.V. T2 - Sitzung des FA1 "Schweißmetallurgie" der Forschungsvereinigung Schweißen und verwandte Verfahren des DVS e.V. CY - Online meeting DA - 26.10.2021 KW - Spannungsrelaxationsrisse KW - Forschung KW - Schweißen KW - Wärmenachbehandlung PY - 2021 AN - OPUS4-53647 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - RPRT A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Fügetechnik für die neue Wasserstoffökonomie – Werkstoffe, Schweißtechnologien, Perspektiven – N2 - Die Studie gibt einen Überblick über die Aspekte der Fügetechnik und ihrer Bedeutung in Wasserstofftechnologien. Dazu werden die Grundlagen der Technologiefelder Wasserstofferzeugung, -speicherung, -transport und -nutzung vorgestellt und der Stand der Technik der fügetechnischen Fertigung von Komponenten in Wasserstofftechnologien zusammengefasst. Dabei werden nicht nur exklusiv Metalle betrachtet. Anhand repräsentativer Beispiele aus der Praxis, Forschung und Entwicklung wird die Bedeutung der Fügetechnik in Wasserstofftechnologien klar herausgestellt und mögliche Perspektiven für die Zukunft abgeleitet. Hier ist ersichtlich, dass Fügetechnologien wesentliche Bedeutung für die erfolgreiche Umsetzung von technischen Komponenten der Wasserstofftechnologien haben, von der Erzeugung bis zur Anwendung. Aus gesamtwirtschaftlicher Sicht umfassen die Schwerpunkte bzw. Trends der Fügetechnik dabei: die Erstellung neuer Infrastruktur für Wasserstoffspeicherung und -transport sowie die sichere Umnutzung der bestehenden Erdgasinfrastruktur. Bei der Wasserstoffanwendung wird die effiziente massentaugliche Produktion von Brennstoffzellen immer wichtiger. Es ist zudem klar ersichtlich, dass die additive Fertigung bereits jetzt ein hohes Potential für Komponenten von Wasserstofftechnologien besitzen und dieses wachsen wird. Aus den perspektivischen Anwendungen ergeben sich zudem Herausforderungen und Forschungsbedarfe für die notwendigen nationalen und internationalen Regelwerke und technischen Normen. Schwerpunktmäßig sind hierbei die bereits bestehenden Empfehlungen und kodifizierten Regeln vollständig zu adaptieren und in die Aus- und Weiterbildung von fügetechnischem Fachpersonal einzubetten. KW - Fügetechnik KW - Wasserstoff KW - Werkstoffe KW - Prozesse KW - Perspektiven PY - 2021 UR - https://www.dvs-media.eu/de/neuerscheinungen/4425/dvs-studie-zur-fuegetechnik-fuer-die-neue-wasserstoffoekonomie-werkstoffe-schweisstechnologien-perspektiven SN - 978-3-96144-157-0 SN - 978-3-96144-158-7 VL - 373 SP - 1 EP - 59 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-53498 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Schweißen im Wasserstoffanlagen- und Behälterbau - Eine Kurzübersicht N2 - Wasserstoff erfüllt die zentrale Rolle für die Umwandlung der bisherigen fossil-basierten Energieerzeugung und -nutzung auf eine dekarbonisierte, nachhaltige Form. Dazu muss der Wasserstoff erzeugt, gespeichert, transportiert werden, bevor er wieder der Nutzung zugeführt wird. Hierzu sind entlang der gesamtem Prozesskette Wasserstofftechnologien notwendig, die einen sicheren Betrieb erfordern. Hierbei kommt dem schweißtechnischen Anlagen- und Behälterbau wesentliche Bedeutung zu, insbesondere (aber nicht ausschließlich) für Speicherung und Transport des Wasserstoffes. Der vorliegende Beitrag gibt einen kurzen Überblick, wo und wie die konventionelle Schweißtechnik hierzu wichtige Beiträge leistet. Die additive Fertigung, also das „Drucken“ von Bauteilen wird dabei zunehmend wichtiger, entlang der gesamtem Prozesskette der Wasserstofftechnologien. Gleichwohl darf nicht unterschätzt werden, dass auch wesentlicher Bedarf an der Erweiterung und teilweiser Neufassung von bestehenden Regel- und Normenwerken besteht. T2 - 51. Sondertagung "Schweißen im Behälter- und Anlagenbau" CY - Munich, Germany DA - 28.02.2023 KW - Wasserstoff KW - Fügetechnik KW - Schweißen KW - Studie PY - 2023 AN - OPUS4-57076 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schroeder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Ausscheidungsverhalten und Eigenschaften der schweißbedingten Wärmeeinflusszonen hochfester Stähle in Abhängigkeit der Mikrolegierungsroute N2 - Für eine signifikante Festigkeitssteigerung von vergüteten, hochfesten Feinkornbaustäh-len mit einer Nominalstreckgrenze ≥ 690 MPa, ist die Zugabe von Mikrolegierungselementen, wie Nb und Ti, unerlässlich. Die Normvorgaben zur chemischen Zusammensetzung dieser Stähle (bspw. in DIN EN 10025-6) geben zur Erzielung der vorgeschriebenen Eigenschaften dabei oft nur Grenzgehalte für die Hersteller vor. Die Wirkung der Legierungselemente in der WEZ ist teilweise komplett konträr. Somit wird eine adäquate Vorhersage der Chargenabhängigkeit hinsichtlich der Schweißeignung und des Tragver-haltens der Schweißverbindung erschwert. Neben metallographischen Untersuchungen einzelner WEZ-Bereiche wurden unter Variation der chemischen Zusammensetzung, thermodynamische Phasenberech-nungen mittels ThermoCalc durchgeführt. Hierdurch wird ein Verständnis zur Phasentransformation, Aus-scheidungswachstum und -auflösung während des Schweißens in Abhängigkeit von Temperatur und Ab-kühlbedingungen geschaffen. T2 - Forschungsseminar BAM, BMDK CY - Magdeburg, Germany DA - 05.12.2022 KW - WEZ-Erweichung KW - Thermodynamische Simulation KW - Mikrolegierungseinfluss KW - Hochfester Feinkornbaustahl KW - Modifizierter Sprühlichtbogen PY - 2023 AN - OPUS4-56837 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kannengießer, Thomas A1 - Rhode, Michael T1 - Fügetechnik in Wasserstofftechnologien - Forschungsbedarf für die Branche N2 - Die Studie gibt einen kurzen Überblick über die jetzige Bedeutung der Fügetechnik in Wasserstofftechnologien und über zukünftige Forschungsbedarfe für die Branche in den einzelnen Technologiefeldern Wasserstofferzeu-gung, -speicherung, -transport und -nutzung. Fügetechnologien haben dabei wesentliche Bedeutung für die er-folgreiche Umsetzung von technischen Komponenten der Wasserstofftechnologien. Die Schwerpunkte bzw. For-schungsbedarfe ergeben sich bspw. durch die Erstellung neuer Infrastruktur für Wasserstoffspeicherung und -transport sowie durch Umnutzung der bestehenden Erdgasinfrastruktur. Bei der Wasserstofferzeugung und -anwendung wird z.B. die Entwicklung effiziente Massenproduktionsmethoden von Elektrolyseuren und Brennstoff-zellen einen wichtigen Meilenstein bilden und laserbasierte Fügetechnologien sind hier zum Teil schon etabliert. Die additive Fertigung nimmt dabei eine Querschnittsposition ein und besitzt hohes Anwendungspotential für die Zukunft z.B. für die Fertigung von Komponenten in Gasturbinen. Aus den technischen Fragestellungen und For-schungsbedarfen ergeben sich zudem Herausforderungen für die notwendige Neu- und Weiterentwicklung von technischen Regelwerken und Normen und den Eingang in die Aus- und Weiterbildung von fügetechnischem Fachpersonal. T2 - DVS Congress 2021 CY - Essen, Germany DA - 14.09.2021 KW - Wasserstoff KW - Fügetechnik KW - Forschung KW - Technologie PY - 2021 AN - OPUS4-53321 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Joining Processes in Hydrogen Technologies - Current need and future R&D activites, a review N2 - This study gives an overview on the important field of joining processes for component fabrication in hydrogen technologies. For that reason, the current need and future research and developement activites are highlighted for the different technological field of hydrogen generation, storage, transport and use. In addition, the emerging field of additive manufacturing is included. Finally, some remarks are given for necessary changes in the standardization and its challenges. T2 - 46th Seminar - Additive Manufacturing, Hydrogen, Energy, Integrity CY - Online meeting DA - 12.10.2021 KW - Hydrogen KW - Joining process KW - Welding KW - Review KW - Research and Development PY - 2021 AN - OPUS4-53554 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Nietzke, Jonathan A1 - Mente, Tobias A1 - Kannengießer, Thomas T1 - Diffusionsmessungen in UP-Mehrlagenschweißgut als effektives Tool gegen verzögerte Kaltrissbildung in Dickblechschweißungen N2 - Offshore-Windenergieanlagen bilden einen zentralen Bestandteil der zukünftigen Energieerzeugung. Hierzu notwendige Gründungs- und Turmstrukturen werden vorrangig aus UP-geschweißten Blechen aus hochfesten niedriglegierten Stählen mit Dicken bis zu 200 mm hergestellt. Die großen Blechdicken begünstigen hohe Schweißeigenspannungen und lange Diffusionswege für z. B. über den Schweißprozess eingebrachten Wasserstoff. Damit steigt das Risiko für eine wasserstoffunterstützte Kaltrissbildung (WKB) an. Zum sichereren Ausschluss von WKB in den geschweißten Komponenten wird in Abhängigkeit der Nahtgröße, Wärmeeinbringung und Stahlsorte eine Mindestwartezeit (MWZ) von bis zu 48 h empfohlen, bevor die zerstörungsfreie Prüfung durchgeführt wird. Es ist allerdings offen, ob die empfohlene MWZ zu konservativ ist. Einflüsse sind hier bspw. die schwierige Bewertung des Wasserstoffdiffusionsverhaltens im heterogenen UP-Mehrlagen-Schweißgut (SG) im Vergleich zum Grundwerkstoff (GW). Zudem sind nur sehr begrenzt H-Diffusionskoeffizienten für UP-Mehrlagen-SG als Grundlage zur Abschätzung des Zeitintervalls einer möglichen verzögerten Kaltrissbildung (somit MWZ) oder auch für Nachwärmprozeduren zur Wasserstoffreduktion (keine MWZ) verfügbar. Verlässliche H-Diffusionskoeffizienten sind daher ein adäquates Tool zur Bewertung des Risikos einer verzögerten WKB. Dieser Beitrag beschreibt Untersuchungen zur Charakterisierung der Wasserstoffdiffusionsverhalten in UP-Mehrlagen-SG eines 60 mm dicken Bleches einer Offshore-Stahlgüte. Dazu wurden Proben unterschiedlicher Dicke aus dem reinen Schweißgut extrahiert und über elektrochemische Permeation und Trägergasheißextraktion im Temperaturbereich bis 400 °C sehr interessante Ergebnisse zu den korrespondierenden Diffusionskoeffizienten erarbeitet. T2 - DVS Congress 2021 CY - Online meeting DA - 14.09.2021 KW - UP-Schweißen KW - Wasserstoff KW - Kaltriss KW - Permeation KW - Diffusion PY - 2021 SN - 978-3-96144-146-4 VL - 371 SP - 448 EP - 459 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-53369 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Joining processes for components in hydrogen technologies: Current need and future importance N2 - This presentation gives an overview on the importance of joining processes for component fabrication in hydrogen technologies. For that reason, the current need and future research and developement activites are highlighted for the three technological fields: hydrogen storage, transport and use (in terms of the emerging field of additive manufacturing). Finally, some remarks are given for necessary changes in the standardization. T2 - IIW Intermediate Meeting, Comm. II-A "Welding Metallurgy" CY - Online meeting DA - 17.03.2022 KW - Hydrogen KW - Welding KW - Research KW - Review KW - Additive manufacturing PY - 2022 AN - OPUS4-54488 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Kannengießer, Thomas T1 - Fügetechnik für die neue Wasserstoffökonomie N2 - Die Herausforderungen für die Fügetechnikbranche, die sich durch die neuen Wasserstoff-Technologiefelder „Erzeugung“, „Speicherung“, „Transport“ und „Nutzung“ ergeben, sind sehr vielfältig. Der DVS-Bericht 373 gibt dazu einen tieferen Einblick. Der hier vorliegende Kurzbericht stellt dazu ausgewählte Praxisbeispiele, zugehörige Herausforderungen und sich ergebende Chancen vor. Fügetechnologien haben dabei wesentliche Bedeutung für das erfolgreiche Umsetzen und Herstellen der benötigten technischen Komponenten, wie anhand der Themenkomplexe „Wasserstoff-Pipelines“ und „additive Fertigung“ betrachtet wird. Zudem ergeben sich Herausforderungen für die notwendigen Regelwerke und Normen, die nahezu vollständig angepasst oder geschaffen werden müssen. KW - Wasserstoff KW - Fügetechnik KW - Studie KW - Werkstoffe KW - Schweißen PY - 2022 UR - https://www.schweissenundschneiden.de/artikel/fuegetechnik-fuer-die-neue-wasserstoffoekonomie SN - 0036-7184 VL - 74 IS - 3 SP - 142 EP - 144 PB - DVS Media GmbH CY - Düsseldorf AN - OPUS4-54563 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Bericht zum Fortschritt des laufenden Projekts: "Entwicklung von Wärmenachbehandlungskonzepten zur Vermeidung von Spannungsrelaxationsrissen" N2 - Dieses Dokument fasst den Projekfortschritt des BAM-Projektes "Entwicklung von Wärmenachbehandlungsstrategien zur Vermeidung von Spannungsrelaxationsrissen" im Rahmen des Fachausschusses 1 "Schweißmetallurgie" des DVS e.V. für das Projektjahr 2021 zusammen und stellt die wichtigsten Ergebnisse in Kurzform vor. T2 - Sitzung des FA1 "Schweißmetallurgie" der Forschungsvereinigung Schweißen und verwandte Verfahren des DVS e.V. CY - Online meeting DA - 22.03.2022 KW - UP-Schweißen KW - Spannungsrelaxationsriss KW - Wärmenachbehandlung KW - Eigenspannungen KW - Schallemissionsanalyse PY - 2022 AN - OPUS4-54525 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kaiser, Sebastian T1 - Repair welding of pressurized in-service hydrogen pipelines: A review on current challenges and strategies N2 - As energy carrier of the future, green hydrogen can make a decisive contribution to a sustainable energy supply. In Europe concrete plans for a hydrogen pipeline grid already exist, as the so called “European Hydrogen backbone”. As building a completely new pipeline grid is economically not justifiable, a dual-way strategy of repurposing natural gas (NG) pipelines and newly built pipelines is intended. Long distance pipeline grids require regular maintenance and repairs. In that conection, for natural gas (NG) pipelines in-service welding is state of the art. Concepts such as hot-tapping (drilling into pressurized pipelines) and “stoppling” (sealing off pipeline sections after installing bypasses or pressure relieves) allow the repair of damaged pipeline sections or the installation of new branches without shutting the pipeline down. The EIGA 121/14 guideline already pointed out in 2014 that “a hydrogen hot-tap shall not be considered a routine procedure”. This shows that the determination of the transferability of these repair concepts to hydrogen pipelines is of utmost importance. Due to the degrading effects of hydrogen on mechanical proper-ties, commonly referred to as “hydrogen embrittlement” it is necessary to understand and investigate the occurring effects. In the special case of repair welding on in-service hydrogen pipelines an increased hydro-gen uptake due to a large heat input and microstructural changes in the material needs to be considered. For this reason, this paper gives an overview on existing weld repair concepts and its risks and limitations in terms of hydrogen absorption and possible embrittlement effects when transferred to hydrogen pipelines. The complexity lies in a large variety of materials (low alloyed steels), pipeline diameters and corresponding welded joints. The material compatibility of materials in used (repurposed NG-pipelines) and new condition must be investigated. Particularly for repurposed/used pipelines the effect of a pre-matured/corroded inner surface and sometimes insufficient documentation of the material “history” needs to be considered. An overview on ongoing and completed R&D-projects with respect to repair concepts for hydrogen pipelines and hydrogen effects on pipeline materials is given. T2 - 77th IIW Annual Assembly and International Conference, Meeting of Commission XI "Pressure Vessels and Piping" CY - Ixia, Rhodes, Greece DA - 07.07.2024 KW - Hydrogen KW - Repair welding KW - Pipelines KW - Study PY - 2024 AN - OPUS4-60673 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Fügetechnik in Wasserstofftechnologien Ein aktueller Überblick N2 - Der Vortrag gibt einen kurzen Überblick über die Bedeutung der Fügetechnik in Wasserstofftechnologien und über zukünftige Herausforderungen. Fügetechnologien, insbesondere die Schweißtechnik, haben dabei wesentliche Bedeutung für die Umsetzung von technischen Komponenten der Wasserstofftechnologien. Forschungsschwerpunkte ergeben sich insbesondere für die Erzeugung und den Transport des Wasserstoffs. T2 - Vortragsreihe des DVS Bezirksverbandes Mannheim-Ludwigshafen CY - Online meeting DA - 27.04.2023 KW - Wasserstoff KW - Schweißen KW - Studie PY - 2023 AN - OPUS4-57411 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Welding (and joining) technologies for the hydrogen economy - a short overview N2 - This study gives an overview on the important field of joining processes for component fabrication in hydrogen technologies. The current main issues and future perspectives are highlighted for the different technological field of hydrogen generation, storage, transport and use. In addition, the emerging field of additive manufacturing is included. Some remarks are given for standardization and regulations. T2 - Meeting of the European Welding Association (EWA), Executive Committee (EC) 1 CY - Frankfurt am Main, Germany DA - 22.03.2023 KW - Hydrogen KW - Welding KW - Research KW - Study PY - 2023 AN - OPUS4-57222 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Bewertung und Vermeidung von schweißverarbeitungsbedingten Rissen in hochfesten Baustählen N2 - Die vorliegende Präsentation fasst die Ergebnisse von drei laufenden bzw. beendeten AiF/IGF-Projekten zusammen, die über die Forschungsvereinigung Stahlanwendung FOSTA e.V. an der BAM bearbeitet wurden zum Thema: Bewertung und Vermeidung von schweißverarbeitungsbedingten Rissen in hochfesten Baustählen. T2 - FOSTA Tagung: Hochfester Stahl im Stahl und Anlagenbau CY - Essen, Germany DA - 16.05.2023 KW - Studie KW - Schweißen KW - Hochfester Stahl KW - Riss KW - Forschung PY - 2023 AN - OPUS4-57517 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Kromm, Arne A1 - Mente, Tobias A1 - Czeskleba, Denis A1 - Brackrock, Daniel A1 - Kannengießer, Thomas T1 - Bauteilversuch zur Bewertung der wasserstoffunterstützten Rissanfälligkeit geschweißter, dickwandiger Offshore-Gründungsstrukturen N2 - Offshore-Windenergieanlagen erfordern Gründungskonzepte aus unterpulver-(UP-)geschweißten Dickblechen (bspw. der Güte S420ML). Während der Schweißfertigung kann eine zeitverzögerte wasserstoffunterstützte Kaltrissbildung auftreten, deren Bewertung aufgrund der Bauteilgröße von Offshore-Strukturen sehr komplex ist. Deswegen wurde eine bauteilähnliche Geometrie (Mock-Up) entwickelt, um reale Steifigkeitsverhältnisse auf den Labormaßstab zu übertragen. Zusätzliche Versteifungen simulieren die Wirkung einer Einspannung bzw. Schrumpfbehinderung der Schweißnaht. Über die Verwendung von Schweißpulvern mit definierter Feuchte wurden zudem ein Extremszenario der Wasserstoffaufnahme simuliert. Entsprechend der vorgegebenen Mindestwartezeit für die ZfP von bis zu 48 h wurde die Schweißnaht zerstörungsfrei mit Phased-Array-Ultraschall-Prüfung (PAUT) geprüft und die Eigenspannungen über Röntgendiffraktometrie (XRD) bestimmt. Zusätzlich wurde die Wasserstoffverteilung in der Schweißverbindung numerisch simuliert. Außer zulässigen Defekten (wie Poren), wurde keine verzögerte Kaltrissbildung in den Mock-Ups festgestellt, was auf hohe Rissbeständigkeit hindeutet. T2 - Tagung Werkstoffprüfung 2023 CY - Berlin, Germany DA - 23.11.2023 KW - Kaltrissbildung KW - Wasserstoff KW - Offshore KW - Schweißen KW - Bauteiltest PY - 2023 DO - https://doi.org/10.48447/WP-2023-219 SP - 316 EP - 321 CY - Berlin AN - OPUS4-58908 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Bauteilversuch zur Bewertung der wasserstoffunterstützten Rissanfälligkeit geschweißter, dickwandiger Offshore Gründungsstrukturen N2 - Offshore-Windenergieanlagen erfordern Gründungskonzepte aus unterpulver-(UP-)geschweißten Dickblechen (bspw. der Güte S420ML). Während der Schweißfertigung kann eine zeitverzögerte wasserstoffunterstützte Kaltrissbildung auftreten, deren Bewertung aufgrund der Bauteilgröße von Offshore-Strukturen sehr komplex ist. Deswegen wurde eine bauteilähnliche Geometrie (Mock-Up) entwickelt, um reale Steifigkeitsverhältnisse auf den Labormaßstab zu übertragen. Zusätzliche Versteifungen simulieren die Wirkung einer Einspannung bzw. Schrumpfbehinderung der Schweißnaht. Über die Verwendung von Schweißpulvern mit definierter Feuchte wurden zudem ein Extremszenario der Wasserstoffaufnahme simuliert. Entsprechend der vorgegebenen Mindestwartezeit für die ZfP von bis zu 48 h wurde die Schweißnaht zerstörungsfrei mit Phased-Array-Ultraschall-Prüfung (PAUT) geprüft und die Eigenspannungen über Röntgendiffraktometrie (XRD) bestimmt. Zusätzlich wurde die Wasserstoffverteilung in der Schweißverbindung numerisch simuliert. Außer zulässigen Defekten (wie Poren), wurde keine verzögerte Kaltrissbildung in den Mock-Ups festgestellt, was auf hohe Rissbeständigkeit hindeutet. T2 - Tagung Werkstoffprüfung 2023 CY - Berlin, Germany DA - 23.11.2023 KW - Kaltrissbildung KW - Wasserstoff KW - Offshore KW - Bauteilversuch KW - Imperfektion PY - 2023 AN - OPUS4-58907 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael A1 - Masoud Nia, Niloufar A1 - Nietzke, Jonathen A1 - Kannengiesser, Thomas T1 - Ti and Nb microalloying of HSLA steels and its effect on hydrogen diffusion and trapping N2 - Fine-grain, high-strength, low-alloy (HSLA) structural steels with yield strengths > 600 MPa are now the state of the art in construction applications such as mobile cranes and civil engineering. HSLA grades derive their strength from a combination of specific heat treatment and the underlying chemical composition. In this context, Ti or Nb are essential to obtain a fine-grained microstructure as well as the necessary carbides or nitrides for precipitation strengthening. In this context, the specific effect of Ti or Nb-rich compounds on hydrogen trapping and diffusion is well known for special laboratory cast alloys, but unknown for realistic steel compositions. For this reason, a series of S690Q-based alloys were synthesized, close to a real steel composition, but with well controlled Ti or Nb additions in different amounts. Specimens were obtained from these alloys by electrochemical discharge machining (EDM). The specimens were tested using the well-established electrochemical permeation technique. From the experimental results, the hydrogen diffusion coefficients and the analytical subsurface hydrogen concentration were calculated. In addition, the hydrogen trapping behavior at elevated temperatures was interpreted by thermal desorption analysis (TDA) using different heating rates of hydrogen charged samples. The results showed that in contrast to metallurgically "pure" laboratory cast alloys, realistic chemical compositions were similar in their hydrogen trapping behavior, despite some small differences. All investigated steel grades exhibited shallow and reversible hydrogen trapping, regardless of their chemical composition. Of course, the experiments only allowed the calculation of effective diffusion coefficients and trapping energies, which represent an average of the entire microstructure. Nevertheless, HSLA steels are typically joined by arc welding, which includes the risk of delayed hydrogen assisted cracking. From the point of view of welding practice, however, a more or less identical hydrogen diffusion behavior means that no special "metallurgically specific", justifiable measures need to be considered, despite the well-established processes such as "soaking" or dehydrogenation heat treatment. T2 - MPAC 2025 CY - Stuttgart, Germany DA - 06.10.2025 KW - HACC KW - Hydrogen KW - HSLA PY - 2025 AN - OPUS4-64337 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schröder, Nina A1 - Rhode, Michael A1 - Kannengießer, Thomas A1 - Kromm, Arne A1 - Kadoke, Daniel A1 - Kruse, Julius T1 - Effect of Ti microalloying on the local strain behavior of cross-weld tensile samples determined by digital image correlation N2 - High-strength low-alloyed (HSLA) steels with yield strength / proof stress ≥ 600 MPa are the basis of modern light-weight steel constructions. Indeed, the economic and ecological benefits strongly depend on their processability in terms of welding. In this context, the use of highly productive welding processes and suitable welding consumables is of vital interest and requires a fundamental understanding of the microstructural changes in the HSLA steel and especially the heat-affected zone (HAZ) of the welded joint. Microalloying elements, such as Ti or Nb, are essential to achieve the desired mechanical properties. To analyse the weldability, three-layer welds were performed using gas metal arc welding (GMAW) and critical microstructures, such as areas of the HAZ that exhibit significant softening or hardening, were identified. The effect of the softened HAZ region on failure was evaluated using cross-weld tensile specimens. Digital image correlation (DIC) was used for in-situ monitoring of the development and accumulation of the local strains in different HAZ regions during tensile testing. Using a specially designed mirror system, the local strains of the microstructure zones on the top and bottom of the weld were recorded simultaneously. In addition, the analysis of the local deformation helps to understand the effects of the softened HAZ on the global strain, the reduction in area, the fracture position, and the overall fracture behavior. KW - High-strength structural steel KW - Microalloying influences KW - HAZ-softening KW - Digital Image Correlation KW - Constraint effect KW - Thermodynamic simulation PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-643558 DO - https://doi.org/10.1007/s40194-025-02185-1 SP - 1 EP - 17 PB - Springer Nature AN - OPUS4-64355 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - A decarbonized future requires pipelines for CO2? A brief overview on perspectives and challenges N2 - Despite the use of hydrogen, for example, in various industrial production processes, CO2 emissions are still unavoidable in the medium term. For example, cement, lime and glass production or waste recycling (waste-to-energy plants) will continue to emit CO2 due to the processing involved chemical reactions. Conversely, the chemical industry with its value chains needs CO2 / carbon as a primary raw material for all compounds that fall within the organic chemistry. In this connection, carbon capture utilization (CCU) will play a key role here. In addition to “natural” methods (via reforestation and the dilution of moors), carbon capture storage (CSS) is already playing a major role, for example by injecting it into old natural gas underground caverns. The resulting quantities of CO2 have to be transported on a large scale and similar to hydrogen pipelines, there are concrete plans for CO2 pipeline networks. For this reason, this presentation provides an introduction to the topic and briefly outlines the associated challenges. On the one hand, these lie in the qualification (testing and construction) and especially in the operation of the pipelines with regard to strict monitoring of the gas quality (e.g. carbonic acid corrosion) and in the avoidance of critical service conditions (sudden pressure fluctuations), which can lead to localized condensation. Among other things, this can lead to the lowering of the typically welded low-alloyed steel pipes below the ductile brittle transition temperature (DBTT) and thus can have an impact on pipeline integrity. T2 - 49th MPA Conference CY - Stuttgart, Germany DA - 06.10.2025 KW - CO2 KW - Pipeline KW - Welding KW - Testing PY - 2025 AN - OPUS4-64316 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Component test for simulation of in-service welding on hydrogen pipelines N2 - Hydrogen is set as the energy carrier of tomorrow and most countries will achieve large-scale hydrogen transport through the conversion of the natural gas (NG) grid and the construction of new pipelines. The interaction between hydrogen and the pipeline materials differs fundamentally from that of NG, as hydrogen is readily absorbed into the material. Considering the possible hydrogen embrittlement (HE), the compatibility of the pipeline materials (low-alloyed steels with a wide strength/thickness range) must be investigated. However, pipelines require intervention for maintenance, repair, or grid expansion with welding on/onto the pipelines while in service, i.e. the well-known "hot tapping" and "stoppling". The challenges compared to NG can be broadly divided into the possible austenitization of the inner pipe material exposed to hydrogen and the welding itself. Both result in a significant increase in hydrogen solubility and could potentially pose challenges in terms of HE. Emphasis is placed on the word "could" because knowledge of "hot tapping" on hydrogen pipelines is scarce due a lack of service experience. To this end, this study proposes a concept for a component-like demonstrator with the objectives: (1) safe feasibility of "hot tapping" on pressurized model hydrogen pipeline sections, (2) facilitate ex-post sample extraction for the purpose of quantifying the absorbed hydrogen concentrations, and (3) ensure in-situ temperature measurement during welding to monitor the pipeline surface temperature. For safety reasons in the event of an unintentional "burn-through", a solid cylinder was inserted in the demonstrator to restrict the hydrogen gas volume to a small, pressurized layer. Reference pipeline surface temperature measurements were ensured on comparable, unpressurized geometries. The investigated range of welding conditions was investigated for representative material/thickness combinations (DN60 to DN300), suggesting the feasibility of the demonstrator for the determination of reliable in-service welding conditions for both installed and new pipelines for hydrogen service. T2 - 49th MPA Conference CY - Stuttgart, Germany DA - 06.10.2025 KW - Hydrogen KW - Pipeline KW - In-service welding KW - Component test PY - 2025 AN - OPUS4-64317 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Ti and Nb influence on the HAZ microstructures of weld-simulated high-strength structural steel S690QL N2 - High-strength low-alloyed (HSLA) steels with yield strength / proof stress ≥ 600 MPa are the basis of modern light-weight steel constructions. Indeed, the economic and ecological benefits strongly depend on their processability in terms of welding. In this context, the use of highly productive welding processes, suitable welding consumables is of vital interest and requires a fundamental understanding of the microstructural changes in the HSLA steel and especially the heat-affected zone (HAZ) of the welded joint. Microalloying elements, such as Ti or Nb, are essential to achieve the desired mechanical properties. In this context, the underlying standards (such as EN 10025-6) only specify maximum values, resulting in different manufacturer customized microalloy concepts. Furthermore, even small deviations can have a drastic effect expressed by an excessive hardening or softening despite identical welding conditions and filler metal. The reason is the different thermal stability of the Ti and Nb-related precipitates (typically carbides or carbon nitrides). As a result, it is difficult (or even impossible) to adequately predict the weldability. Against this background, different microalloying routes with varying Ti and Nb contents for a S690QL reference grade were systematically investigated in terms of lab-cast alloys close to realistic chemical compositions. To investigate the influence of the welding heat input on the HAZ microstructure formation, physical simulations were carried with specified peak temperatures and cooling times (by a dilatometry). The focus was the identification of the occurring phase transformations during cooling and the final HAZ microstructure. In this context, a double welding cycle was simulated to further identify the behavior of the so-called intercritical HAZ (where softening is likely to occur) in case of the common multi-layer welding for thick plates. The results showed: (1) microalloying has significant influence on the formation of the individual HAZ dependent on (2) the thermal stability of the Ti or Nb-precipitates and (3) synergistic effects of further elements such as Mo and their effect on phase transformations in the HAZ. The results represent a microstructure-based validation of welding processing of such HSLA-steels e.g. in terms of preferred microalloy and weld heat input combinations. T2 - 49th MPA Conference CY - Stuttgart, Germany DA - 06.10.2025 KW - High-strength steel KW - Microalloy elements KW - Welding KW - Weld simulation KW - Microstructure PY - 2025 AN - OPUS4-64319 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Welding of high-entropy alloys - New material concept vs. old challenges N2 - HEAs represent a relatively new class of materials. The the alloy concept is fundamentally different from the most conventional materials and alloys that are used today. Recently, the focus of HEA designs is more application-based. For that purpose, the elements of interest are carefully selected and multiple phases as well as micro-structures are deliberately adjusted. Currently, only limited attention has been paid to weldability of HEA. This encompasses possible effects on metallurgy and its influence on the desired properties. It remains open if welding causes e.g. considerable number of intermetallic phases or segregations and their effect on weld joint properties. For that reason, the scope of this study is to summarize already available studies on welding of HEAs with respect to the HEA-type, the applied welding process and its influence on the weld joint properties. T2 - IIW Annual Assembly, Meeting of Commission II-A CY - Online meeting DA - 20.07.2020 KW - High-entropy alloy KW - Welding KW - Review PY - 2020 AN - OPUS4-51116 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Wasserstoffdiffusion und lokale Volta-Potentiale in Hoch- und Mittelentropie-Legierungen N2 - Hochentropie-Legierungen (HEAs) zeichnen sich durch einen Mischkristall-System aus mindestens fünf und Mittelentropie-Legierungen (MEAs) durch mindestens drei Hauptlegierungselemente aus, in äquiatomarer Zusammensetzung. Sie zeigen außergewöhnliche Anwendungseigenschaften, wie z.B. hohe Festigkeit, Duktilität oder Korrosionsbeständigkeit. Zukünftige HEA/MEA-Komponenten aufgrund ihrer Eigenschaften für wasserstoffhaltige Umgebungen (wie Behälter für kryogene oder Hochdruckspeicherung) von Interesse. Daher ist die Bewertung der Wasserstoffabsorption und die Diffusion in diesen Materialien von großer Bedeutung. Dazu wurden in unserer Studie eine CoCrFeMnNi-HEA und eine CoCrNi-MEA untersucht. Die Proben wurden elektrochemisch mit Wasserstoff beladen. Für die Ermittlung des Wasserstoffdiffusionsverhaltens wurde die thermische Desorptionsanalyse (TDA) mit unterschiedlichen Heizraten bis zu 0,250 K/s angewandt. Die nachfolgende Peakentfaltung der Signale führte zu Hochtemperatur-Desorptionsspitzen und Wasserstofftrapping auch über 280°C. Eine resultierende Gesamtwasserstoffkonzentration > 40 ppm wurde für den MEA ermittelt und > 100 ppm für den HEA. Dies deutet auf zwei wichtige Effekte hin: (1) verzögerte Wasserstoffdiffusion und (2) eine beträchtliche Menge an getrapptem Wasserstoff auch bei hoher Temperatur. Beide Effekte können hinsichtlich einer wasserstoffunterstützten Rissbildung kritisch werden, dies erfordert jedoch weitere Untersuchungen. Zusätzlich erfolgte die Bestimmung des lokalen Volta-Potentials mittels hochauflösender Kelvin-Sonden-Kraft-Mikroskopie (SKPFM). Die ermittelten Scans zeigen einen bestimmten Einfluss der Wasserstoffbeladung auf die Potentiale. T2 - Symposium on Materials and Joining Technology CY - Online meeting DA - 07.09.2020 KW - Wasserstoff KW - High-entropy alloy KW - Diffusion KW - Scanning kelvin probe force microscopy KW - Thermal desorption analysis PY - 2020 AN - OPUS4-51187 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Richter, Tim A1 - Schröpfer, Dirk A1 - Rhode, Michael A1 - Boerner, Andreas A1 - Saliwan Neumann, Romeo A1 - Schneider, M. A1 - Laplanche, G. T1 - Influence of machining on the surface integrity of high- and medium-entropy alloys N2 - High- and medium-entropy alloys (HEAs) are a quite new class of materials. They have a high potential for applications from low to high temperatures due to the excellent combination of their structural properties. Concerning their application as components; processing properties, such as machinability, have hardly been investigated so far. Hence, machinability analyses with a focus on the influence of the milling process and its basic parameters (cutting speed, feed per cutting edge) on the resulting surface integrity of specimens from an equiatomic high- (CoCrFeMnNi) and a medium- (CoCrNi) entropy alloy have been carried out. A highly innovative milling process with ultrasonic assistance (USAM) was compared to conventional milling processes. Recent studies have shown that USAM has a high potential to significantly reduce the mechanical load on the tool and workpiece surface during milling. In this study, the basic machining and ultrasonic parameters were systematically varied. After machining, the surface integrity of the alloys was analyzed in terms of topography, defects, subsurface damage, and residual stresses. It was observed that USAM reduces the cutting forces and increases the surface integrity in terms of lower tensile residual stresses and defect density near the surfaces for the CoCrFeMnNi alloy. It was shown that the cutting forces and the metallurgical influence in the sub surface region are reduced by increasing the cutting speed and reducing the feed rate per cutting edge. With the CoCrNi alloy, the tool revealed severe wear. As a result, for this alloy no influence of the parameters on the machinability could be determined. KW - High Entropy Alloy KW - Medium Entropy Alloys KW - Ultrasonic assited machining PY - 2022 DO - https://doi.org/10.1016/j.matchemphys.2021.125271 SN - 0254-0584 VL - 275 SP - 125271 PB - Elsevier B.V. AN - OPUS4-53606 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Mechanische Eigenschaften der Längschweißnaht einer X65-Pipeline in Druckwasserstoffatmosphäre N2 - Im folgenden Beitrag werden die Ergebnisse der mechanischen Eigenschaften unter 200 bar Druckwasserstoff des Werkstoffes 316L (1.4404) vorgestellt. Dazu wurden Hohlzugproben aus konventionellem, kaltgezogenem Material herausgearbeitet und per SLM-PBF additiv gefertigten Hohlzugproben gegenübergestellt. Die Proben wurden da-bei unter Druckwasserstoff einer SSRT-Prüfung mit einer Dehnrate von 1E-5/s unterzogen. Zusätzlich zum Werkstoffzustand wurde der Einfluss des Oberflächenzustandes charakterisiert: (1) additiv gefertigten Proben mit endkonturnaher Form „as-printed“ oh-ne zusätzliche Bohrung, (2) Bohren und (3) zusätzliches Honen. Die gemessene Degradation der mechanischen Eigenschaften unter Wasserstoff hing dabei in erster Linie von der Oberfläche ab und damit indirekt vom Werkstoffzustand „as-printed“ oder kaltgezogen ab. Während die Proben mit gebohrter und/oder gehonter Oberfläche eine RRA (Relative Reduction of Area) 78 % aufwiesen, zeigten die AM-Proben eine deutlich höhere RRA von 90 %. Ein möglicher Grund dafür sind während der Fertigung ausbildende Oxidschichten, die sich durch geringe Mengen an Restsauerstoff während des AM-Prozesses ausbilden. Zur abschließenden Charakterisierung sind weitere Untersuchungen erforderlich, insbesondere für ein größeres Parameterfeld an Prüftemperaturen (Oxideinwirkung) und Dehnraten (mechanische Beständigkeit der Oxidschicht ähnlich den Einflüssen auf „klassische“ Spannungsrisskorrosion). T2 - DGM Arbeitskreis Wasserstoff CY - Neu-Isenburg, Germany DA - 26.05.2025 KW - Pipeline KW - Wasserstoff KW - Hohlzugprobe PY - 2025 AN - OPUS4-63236 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Additive gefertigte 316L-Hohlzugproben unter Druckwasserstoff - Einfluss der Oberfläche und des Werkstoffzustandes N2 - Im folgenden Beitrag werden die Ergebnisse der mechanischen Eigenschaften unter 200 bar Druckwasserstoff des Werkstoffes 316L (1.4404) vorgestellt. Dazu wurden Hohlzugproben aus konventionellem, kaltgezogenem Material herausgearbeitet und per SLM-PBF additiv gefertigten Hohlzugproben gegenübergestellt. Die Proben wurden da-bei unter Druckwasserstoff einer SSRT-Prüfung mit einer Dehnrate von 1E-5/s unterzogen. Zusätzlich zum Werkstoffzustand wurde der Einfluss des Oberflächenzustandes charakterisiert: (1) additiv gefertigten Proben mit endkonturnaher Form „as-printed“ oh-ne zusätzliche Bohrung, (2) Bohren und (3) zusätzliches Honen. Die gemessene Degra-dation der mechanischen Eigenschaften unter Wasserstoff hing dabei in erster Linie von der Oberfläche ab und damit indirekt vom Werkstoffzustand „as-printed“ oder kaltgezogen ab. Während die Proben mit gebohrter und/oder gehonter Oberfläche eine RRA (Relative Reduction of Area) 78 % aufwiesen, zeigten die AM-Proben eine deutlich höhere RRA von 90 %. Ein möglicher Grund dafür sind während der Fertigung ausbildende Oxidschichten, die sich durch geringe Mengen an Restsauerstoff während des AM-Prozesses ausbilden. Zur abschließenden Charakterisierung sind weitere Untersuchungen erforderlich, insbesondere für ein größeres Parameterfeld an Prüftemperaturen (Oxideinwirkung) und Dehnraten (mechanische Beständigkeit der Oxidschicht ähnlich den Einflüssen auf „klassische“ Spannungsrisskorrosion). T2 - DGM Arbeitskreis Wasserstoff CY - Neu-Isenburg, Germany DA - 26.05.2025 KW - Wasserstoff KW - Additive Fertigung KW - Hohlzugprobe KW - Austentitischer Stahl PY - 2025 AN - OPUS4-63239 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rhode, Michael A1 - Richter, Tim A1 - Mayr, P. A1 - Nitsche, A. A1 - Mente, Tobias A1 - Böllinghaus, Thomas T1 - Hydrogen diffusion in creep-resistant 9% Cr P91 multi-layer weld metal N2 - Welded components of P91 9% Cr steel demand for careful welding fabrication with necessary post weld heat treatment (PWHT). Before the PWHT, a hydrogen removal heat treatment is necessary for avoidance of hydrogen assisted cracking (HAC). In this context, the microstructure and temperature-dependent hydrogen diffusion is important, and reliable diffusion coefficients of P91 weld metal are rare. For that reason, the diffusion behavior of P91 multi-layer weld metal was investigated for as-welded (AW) and PWHT condition by electrochemical permeation experiments at room temperature and carrier gas hot extraction (CGHE) from 100 to 400 °C. Hydrogen diffusion coefficients were calculated, and the corresponding hydrogen concentration was measured. It was ascertained that both heat treatment conditions show significant differences. At room temperature the AW condition showed significant hydrogen trapping expressed by to seven times lower diffusion coefficients. A preferred diffusion direction was found in perpendicular direction expressed by high permeability. The CGHE experiments revealed lower diffusion coefficients for the AW condition up to 400 °C. In this context, a hydrogen concentration of approximately 21 ml/100 g was still trapped at 100 °C. For that reason, a certain HAC susceptibility of as-welded P91 weld metal cannot be excluded, and hydrogen removal should be done before PWHT. KW - Creep resisting materials KW - Diffusion KW - Hydrogen KW - Weld metal KW - Post weld heat treatment KW - Microstructure PY - 2020 DO - https://doi.org/10.1007/s40194-019-00828-8 SN - 0043-2288 VL - 64 IS - 2 SP - 267 EP - 281 PB - Springer AN - OPUS4-50471 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Hollow specimens as simplified approach for testing metallic materials under high pressure hydrogen development and utilization N2 - The hydrogen economy requires large-scale storage and transportation options like long-distance transmission pipelines. The applied materials (typically steels) must be carefully tested under different conditions (pressure, temperature, impact of impurities, etc.) for their suitability and service with hydrogen. In combination with mechanical load, as occurs in every gas network, hydrogen can induce degradation of the mechanical properties and promote finally resulting in embrittlement, i.e., the formation of cracks. The conventional testing procedures consist of autoclaves in which samples are strained under pressurized hydrogen. The test apparatus requires large amounts of hydrogen and thus a high level of safety and costs. In very specific cases, these tests might be replaced by simplified electrochemical charging. However, these test alternatives raise several questions regarding the equivalency of both testing scenarios. In the early 1980’s the idea of a so-called hollow tensile sample raised and was reinitiated 2021 in ISO TC 164 by T. Ogata (NIMS, Japan) and further developed (e.g. by Fraunhofer IWM, Germany). The idea was: the sample itself represents the autoclave instead of charging a sample from outside. For that reason, a hole is drilled through the sample and the inner surface is pressurized by hydrogen gas during the mechanical testing. Indeed, this represents the main advantage as no expensive pressure-resistant autoclave equipment for large H-volumes is necessary, which significantly reduces the safety-related issues and thus the high costs. In the following, we show recent activities at BAM Berlin on adaption of the hollow-specimen technique for slow strain rate testing (SSRT). The current research activities are focussed on macroscopic influences like the sample geometry, minimum necessary dimensions, and microscopic influences e.g., on the surface by the processing method (drill hole quality and geometric precision) as well as the gas pressure effect (mechanical deformation of surface in different media). T2 - FEMS EUROMAT 2023 CY - Frankfurt a. M., Germany DA - 04.09.2023 KW - Hydrogen KW - Hollow tensile specimen KW - High-pressure KW - Mechanical properties KW - Testing PY - 2023 AN - OPUS4-58220 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Böllinghaus, Thomas A1 - Rhode, Michael A1 - Falkenreck, T. ED - Bender, B. ED - Göhlich, D. T1 - Korrosion und Korrosionsschutz N2 - Das Kapitel beginnt mit einer kurzen Einführung über die Korrosion (Wechselwirkung zwischen einem Metall, einer korrosiven Umgebung und der der jeweiligen Konstruktion). Im zweiten Abschnitt werden die wichtigsten Formen der wässrigen elektrochemischen Korrosion (Flächenkorrosion, galvanische, selektive und interkristalline Korrosion sowie Loch- und Spaltkorrosion) betrachtet. Darüber hinaus wird die elektrochemische Korrosion unter mechanischer Belastung betrachtet (Spannungsrisskorrosion, wasserstoffunterstützte Rissbildung, Korrosionsermüdung), sowie Sonderformen der Korrosion (Erosion, Fretting und mikrobiologisch induzierte Korrosion). Der dritte Abschnitt befasst sich mit der chemischen und Hochtemperaturkorrosion (Oxidation, Aufkohlung, Hochtemperatur-Wasserstoffangriff, Aufschwefelung, Nitrierung, Halogenierung). Zusätzlich enthält das Kapitel Maßnahmen zur Vermeidung der Korrosion. KW - Korrosion KW - Korrosionsschutz KW - Spannungsrisskorrosion KW - Wasserstoff KW - Loch- u. Spaltkorrosion PY - 2021 SN - 978-3-662-59710-1 DO - https://doi.org/10.1007/978-3-662-59711-8_34 VL - 1 SP - 691 EP - 725 PB - Springer-Verlag GmbH, ein Teil von Springer Nature CY - Berlin ET - 26 AN - OPUS4-52156 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Böllinghaus, Thomas A1 - Rhode, Michael A1 - Falkenreck, T. ED - Grote, K.-H. ED - Hefazi, H. T1 - 6. Corrosion and Corrosion Resistance N2 - The chapter starts with a brief introduction about corrosion, which is defined as the interdependency between a metal, a corrosive environment, and the respective component design. The second section introduces the most important forms of aqueous electrochemical corrosion (uniform corrosion, galvanic corrosion, selective and intergranular corrosion, and finally pitting and crevice corrosion in the case of passive layer forming metals). In addition, electrochemical corrosion under applied mechanical load is introduced (stress corrosion cracking, hydrogen-assisted cracking, corrosion fatigue), as well as special forms of corrosion (erosion, fretting, and microbiologically induced corrosion). The third section of this chapter introduces (mostly dry) chemical corrosion and high-temperature corrosion (oxidation, carburization, high-temperature hydrogen attack, sulfurization, nitriding, halogenation). As in the case of electrochemical corrosion, chemical corrosion can also be superimposed by mechanical loads. Finally, general facts on the testing of corrosion are introduced. KW - Corrosion KW - Corrosion testing KW - Handbook KW - Electrochemical corrosion KW - Chemical corrosion PY - 2021 SN - 978-3-030-47035-7 DO - https://doi.org/10.1007/978-3-030-47035-7_6 VL - 2021 SP - 185 EP - 213 PB - Springer Nature Switzerland AG CY - Cham (CH) ET - 2nd Edition AN - OPUS4-52423 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Der Weg zur Standardisierung der Hohlzugtechnik für die Nutzung mit gasförmigem Wasserstoff N2 - Dieser Kurzvortrag stellt selektierte Ergebnisse des Projektes "H2Hohlzug" im übergeordneten Projekt "TransHyDE" kurz vor. Insbesondere wird auf die Herausforderung eingegangen, wiederholbare Prüfbedingungen unter Druckwasserstoffbeanspruchung, einzuhalten. T2 - Herbstsitzung des DGM Arbeitskreises "Materialprüfung unter Wasserstoff" CY - Dortmund, Germany DA - 19.11.2024 KW - Hohlzugprobe KW - Wasserstoff KW - Materialprüfung KW - Standardisierung PY - 2024 AN - OPUS4-61718 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Additive manufacturing for components in hydrogen technologies N2 - With the introduction of a hydrogen-based energy and national economy, safety-relevant components for hydrogen technologies are becoming increasingly important. Characteristic of hydrogen technologies are, for example, harsh environmental conditions such as cryogenic or high-pressure storage, corrosion issues in fuel cells and electrolyzers, turbines, and many more. Additive manufacturing of components is becoming increasingly important and irreplaceable for the production of complex technical systems. Using the case studies of burners for gas turbines and electrodes and membranes for polymer (PEMFC) and solid oxide (SOFC) fuel cells, this article shows the potential of additive manufacturing of components. At the same time, however, the challenge of considering divergent mechanical properties depending on the direction of assembly in a "hydrogen-compatible" manner is also highlighted. Finally, the challenges posed by additive manufacturing and hydrogen for materials testing are highlighted under scenarios that are as realistic as possible. T2 - MPA-Workshop Hydrogen CY - Online meeting DA - 10.11.2022 KW - Additive manufacturing KW - Hydrogen KW - Technologies KW - Overview KW - Component PY - 2022 AN - OPUS4-56233 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Rhode, Michael T1 - Processing and application properties of multiple principal element alloys (MPEA) N2 - The presentation gives an overview of BAM's activities on processing influences and application properties of MPEAs in the form of joined and machined high and medium entropy alloys (CoCrFeMnNi and CoCrNi). In the case of welding, the focus is on defect-free welded joints with sufficient mechanical properties. In the case of machining, the focus is on the possible influence on the surface quality of the materials through adequate milling parameters. In addition, the hydrogen absorption and diffusion properties as well as the electrochemical corrosion behavior are fundamentally examined. T2 - FAU-Department Werkstoffwissenschaften, Seminar: Aktuelle Probleme der Werkstoffwissenschaften CY - Erlangen, Germany DA - 25.04.2024 KW - Welding KW - Application properties KW - Machining KW - High-entropy alloy KW - Hydrogen PY - 2024 AN - OPUS4-59975 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Drexler, A.-K. A1 - Konert, Florian A1 - Nietzke, Jonathan A1 - Hodžić, E. A1 - Pastore, S. A1 - Domitner, J. A1 - Rhode, Michael A1 - Sommitsch, C. A1 - Böllinghaus, Thomas T1 - Effect of Tensile Loading and Temperature on the Hydrogen Solubility of Steels at High Gas Pressure N2 - The hydrogen solubility in ferritic and martensitic steels is affected by hydrostatic stress, pressure, and temperature. In general, compressive stresses decrease but tensile stresses increase the hydrogen solubility. This important aspect must be considered when qualifying materials for high‐pressure hydrogen applications (e.g., for pipelines or tanks) by using autoclave systems. In this work, a pressure equivalent for compensating the effect of compressive stresses on the hydrogen solubility inside of closed autoclaves is proposed to achieve solubilities that are equivalent to those in pipelines and tanks subjected to tensile stresses. Moreover, it is shown that the temperature effect becomes critical at low temperatures (e.g., under cryogenic conditions for storing liquid hydrogen). Trapping of hydrogen in the microstructure can increase the hydrogen solubility with decreasing temperature, having a solubility minimum at about room temperature. To demonstrate this effect, the generalized law of the hydrogen solubility is parameterized for different steels using measured contents of gaseous hydrogen. The constant parameter sets are verified and critically discussed with respect to the high‐pressure hydrogen experiments. KW - Hydrogen KW - Solubility KW - Temperature KW - Tensile loading KW - Analytical calculation PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-586701 DO - https://doi.org/10.1002/srin.202300493 SN - 1611-3683 SP - 1 EP - 9 PB - Wiley AN - OPUS4-58670 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Drexler, A A1 - Konert, Florian A1 - Sobol, Oded A1 - Rhode, Michael A1 - Domitner, J A1 - Sommitsch, C A1 - Böllinghaus, Thomas T1 - Enhanced gaseous hydrogen solubility in ferritic and martensitic steels at low temperatures N2 - Metals that are exposed to high pressure hydrogen gas may undergo detrimental failure by embrittlement. Understanding the mechanisms and driving forces of hydrogen absorption on the surface of metals is crucial for avoiding hydrogen embrittlement. In this study, the effect of stress-enhanced gaseous hydrogen uptake in bulk metals is investigated in detail. For that purpose, a generalized form of Sievert's law is derived from thermodynamic potentials considering the effect of microstructural trapping sites and multiaxial stresses. This new equation is parametrized and verified using experimental data for carbon steels, which were charged under gaseous hydrogen atmosphere at pressures up to 1000 bar. The role of microstructural trapping sites on the parameter identification is critically discussed. KW - Hydrogen KW - Thermodynamic modelling KW - Pressure-dependent solubility KW - Steel KW - Trapping PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-559307 DO - https://doi.org/10.1016/j.ijhydene.2022.09.109 SN - 0360-3199 VL - 47 IS - 93 SP - 39639 EP - 39653 PB - Elsevier Ltd. AN - OPUS4-55930 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Konert, Florian A1 - Nietzke, Jonathan A1 - Grimault de Freitas, Tomás A1 - Rhode, Michael A1 - Sobol, Oded A1 - Böllinghaus, Thomas T1 - Investigation of resistance to gaseous hydrogen of a longitudinal weld seam in a X65 pipeline using the hollow specimen technique N2 - The constantly increasing demand for renewable energy sources leads to the necessity of transporting large amounts of hydrogen. Since pipelines enable a cost-effective way for the distribution of gaseous hydrogen, the interaction of hydrogen and the pipeline materials must be carefully investigated as hydrogen can cause a degradation of the mechanical properties under certain conditions. Especially welds, which are assumed to be more susceptible to the degradation enhanced by hydrogen, are of great interest. The aim of this study is to investigate the effect of gaseous hydrogen on the mechanical properties of an X65 pipeline, and the longitudinal submerged arc welding (SAW) welded joint. The tests are conducted using the hollow specimen technique on two types of specimens: one extracted from the base material (BM) and the other extracted as a cross-weld (CW) specimen consisting of BM and weld seam. The specimens are charged in situ under a pressure of 60 bar and tested using slow strain rate (SSR) tensile tests with a nominal strain rate of 10−5 s−1. The properties obtained of specimens tested in hydrogen atmosphere are compared to the properties of comparable specimen in inert argon atmosphere as a reference. The performed tests showed a decrease of the reduction of area (RA) from 72% in inert atmosphere to 52% in hydrogen atmosphere for the CW specimen and a decrease from 73% in inert atmosphere to 51% for the BM. Metallographic analyses showed the crack initiation between fine-grained heat-affected zone (FGHAZ) and BM for the specimens tested in hydrogen atmosphere as well as for the reference specimens. This leads to the conclusion that the location of the crack initiation does not change due to the presence of gaseous hydrogen. KW - Hydrogen KW - Hollow specimen technique KW - Pipeline KW - SSRT KW - Hydrogen embrittlement KW - Cross-weld specimen PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-624658 DO - https://doi.org/10.1007/s40194-025-01953-3 SN - 0043-2288 SN - 1878-6669 VL - 69 IS - 3 SP - 861 EP - 870 PB - Springer CY - Berlin AN - OPUS4-62465 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schaupp, Thomas A1 - Rhode, Michael A1 - Yahyaoui, Hamza A1 - Kannengießer, Thomas ED - Lippold, J. ED - Böllinghaus, Thomas ED - Norrish, J. ED - Scotti, A. T1 - Hydrogen-assisted cracking in GMA welding of high-strength structural steels using the modified spray arc process N2 - High-strength structural steels are used in machine, steel, and crane construction with yield strength up to 960 MPa. However, welding of these steels requires profound knowledge of three factors in terms of avoidance of hydrogen-assisted cracking (HAC): the interaction of microstructure, local stress/strain, and local hydrogen concentration. In addition to the three main factors, the used arc process is also important for the performance of the welded joint. In the past, the conventional transitional arc process (Conv. A) was mainly used for welding of high-strength steel grades. In the past decade, the so-called modified spray arc process (Mod. SA) has been increasingly used for welding production. This modified process enables reduced seam opening angles with increased deposition rates compared with the Conv. A. Economic benefits of using this arc type are a reduction of necessary weld beads and required filler material. In the present study, the susceptibility to HAC in the heat-affected zone (HAZ) of the high-strength structural steel S960QL was investigated with the externally loaded implant test. For that purpose, both Conv. A and Mod. SA were used with same heat input at different deposition rates. Both conducted test series showed same embrittlement index “EI” of 0.21 at diffusible hydrogen concentrations of 1.3 to 1.6 ml/100 g of arc weld metal. The fracture occurred in the HAZ or in the weld metal (WM). However, the test series withMod. SA showed a significant extension of the time to failure of several hours compared with tests carried out with Conv. A. KW - High-strength steel KW - GMA welding KW - Diffusible hydrogen KW - Implant test KW - Fractography PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-515330 DO - https://doi.org/10.1007/s40194-020-00978-0 SN - 1878-6669 SN - 0043-2288 VL - 64 IS - 12 SP - 1997 EP - 2009 PB - Springer CY - Berlin Heidelberg AN - OPUS4-51533 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -