TY - CONF A1 - Leo, Reinhold T1 - Duplex stainless steels - Compatibility for high-pressure hydrogen applications N2 - Duplex Stainless Steels (DSS) are an essential component used in the construction of transportation pipelines because of their many distinctive qualities. The choice of DSS for a particular hydrogen application mainly depends on its susceptibility level to Hydrogen Assisted Cracking (HAC). Several mechanisms have been proposed to describe the occurring microscale processes behind HAC, and these include metastable phase transformation, Hydrogen Enhanced Localized Plasticity (HELP), and Hydrogen Enhanced Decohesion (HEDE). This contribution describes the path to ascertain if DSS is suitable for high-pressure gaseous hydrogen applications. The interplay between several critical factors that result in HAC was examined using high-pressure gaseous hydrogen charging, Electron Backscatter Diffraction (EBSD), tensile testing and hydrogen concentration measurements using Carrier Gas Hot Extraction (CGHE). T2 - Third German-African Green Hydrogen Forum 2025 CY - Bernburg (Saale), Germany DA - 23.09.2025 KW - Hydrogen Assisted Cracking KW - High Pressure Hydrogen KW - Duplex Stainless Steels KW - Hollow Specimen Technique PY - 2025 AN - OPUS4-64302 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Steiner, S. A1 - Heldt, J. A1 - Sobol, Oded A1 - Unger, Wolfgang A1 - Frömeling, T. T1 - Influence of oxygen vacancies on core-shell formation in solid solutions of (Na,Bi)TiO3 and SrTiO3 N2 - Solid solutions of (Na,Bi)TiO3 (NBT) and SrTiO3 (ST) are materials of interest for high-strain or high-energy density capacitor applications. Often, they exhibit chemical heterogeneity and develop core-shell structures during regular solid-state synthesis with an NBT-rich core. In this case, the NBT forms first so that the strontium needs to diffuse into the material to reach chemical homogeneity. Depending on the presence of core-shell structures, the electrical properties can vary drastically. In this work, we rationalize the effect of variations in oxygen vacancy concentration by Fe-acceptor and Nb-donor doping. It can be shown that a diffusion couple of strontium and oxygen is responsible for chemical homogenization and that the oxygen vacancy content can control the formation of a core-shell structure. KW - Lead-free ceramics KW - Bismuth titanates KW - Core-shell structures KW - Diffusion/diffusivity KW - Ferroelectricity/ferroelectric materials PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-525988 DO - https://doi.org/10.1111/jace.17845 SP - 1 EP - 10 PB - Wiley Periodicals LLC, John Wiley & Sons, Inc. AN - OPUS4-52598 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baer, Wolfram A1 - Breidung, Marc A1 - Wossidlo, Peter A1 - Wahl, Ken A1 - Gerwien, Peter A1 - Zerbst, Uwe A1 - Madia, Mauro A1 - Küppers, M. ED - Zimmermann, Martina T1 - Gezielte Werkstoffprüfung zur fail-safe-Bauteilauslegung am Beispiel eines Achsschenkels N2 - Bei der Auslegung von Achsschenkeln für Nutzfahrzeuge wird für den Überlastfall ein fail-safe-Kriterium (kontrolliertes Versagen) als Basisphilosophie angesetzt. Gefordert wird, dass sich der Achsschenkel auch unter Akzeptanz begrenzten Risswachstums hinreichend elastisch-plastisch verformen kann, ohne dass es zum Bruch kommt. Der Fahrer soll anschließend anhand der bleibenden Verformungen bemerken können, dass mit seinem Fahrzeug etwas nicht in Ordnung ist. Eine Voraussetzung für dieses Bauteilverhalten ist eine hinreichende Bruchzähigkeit des Werkstoffs. Diese, wie auch die Rissspitzenbeanspruchung, müssen ermittelt werden, um den bruchmechanischen Sicherheitsnachweis führen zu können. Zur Ermittlung der mechanisch-technologischen und bruchmechanischen Werkstoffeigenschaften wurde ein Prüfkonzept entwickelt, bei dem die Proben an der potenziell kritischen Stelle direkt aus den geschmiedeten Achsschenkeln entnommen werden. Die experimentelle Werkstoffcharakterisierung bildet dann die Beanspruchungsbedingungen beim Überlastereignis ab. Im Rahmen der Produktion stehen jedoch nur Kerbschlagarbeitswerte zur Verfügung und aufwändige bruchmechanische Versuche sollen vermieden werden. Deshalb wurde eine Korrelation zur Abschätzung der vorhandenen Bruchzähigkeit aus der Kerbschlagarbeit herangezogen. Es ergibt sich eine Ergebnismatrix, die die Einflussgrößen Versagenswahrscheinlichkeit, Temperatur und Bruchzähigkeit verknüpft. Abschließend wird ein erster Vergleich der abgeschätzten mit den experimentell ermittelten Bruchzähigkeitswerten gezogen. Dieser weist aus, dass die abgeschätzten Werte geringfügig konservativ sind. T2 - 40. Vortrags- und Diskussionstagung Werkstoffprüfung 2022 CY - Dresden, Germany DA - 27.10.2022 KW - Kerbschlagarbeit KW - Achsschenkel KW - Fail-safe KW - Bruchmechanische Auslegung KW - Korrelation PY - 2022 SP - 1 EP - 6 PB - DGM - Deutsche Gesellschaft für Materialkunde e.V. CY - Sankt Augustin AN - OPUS4-56152 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Holzwarth, M. A1 - Baer, Wolfram A1 - Mayer, U. A1 - Weihe, S. T1 - Untersuchung des Master Curve-Konzepts für ferritisches Gusseisen mit Kugelgraphit N2 - Das Master Curve (MC) Konzept nach ASTM E1921 wird momentan u.a. in der Kerntechnik für die bruchmechanische Sicherheitsbewertung ferritischer Stähle eingesetzt. Für ferritisches Gusseisen mit Kugelgraphit (GJS) fehlt jedoch eine Validierung dieser Methode und ggf. eine systematische Überprüfung möglicher Modifikationen grundlegender Ansätze des MC-Konzepts. Aus diesem Grund soll in einem kürzlich gestarteten BMUV-Verbundprojekt zwischen der MPA Stuttgart und der BAM Berlin die Anwendbarkeit des MC-Konzepts auf GJS bei dynamischer Beanspruchung untersucht werden. Ziel ist es, eine effektive und effiziente Methodik bereitzustellen, mit der mittels einer vergleichsweise kleinen Stichprobe bruchmechanischer Kleinproben eine Referenztemperatur T0 zur werkstoffspezifischen Temperaturjustierung der MC ermittelt werden kann. T2 - 55. Jahrestagung des DVM-Arbeitskreises "Bruchmechanik und Bauteilsicherheit" CY - Darmstadt, Germany DA - 14.02.2023 KW - Dynamische Beanspruchung KW - Bruchmechanik KW - Master Curve-Konzept KW - Gusseisen mit Kugelgraphit PY - 2023 DO - https://doi.org/10.48447/Br-2023-BB SP - 101 EP - 108 PB - DVM Berlin CY - Berlin AN - OPUS4-57024 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baer, Wolfram A1 - Holzwarth, Marcel A1 - Mayer, Uwe ED - Vormwald, Michael T1 - Untersuchung des Master Curve-Konzepts für ferritisches Gusseisen mit Kugelgraphit: Versuchswerkstoff und erste Ergebnisse an SE(B)140-Großproben N2 - In einem laufenden Kooperationsprojekt zwischen der BAM Berlin und der MPA Stuttgart wird das probabilistische Master Curve (MC) Konzept nach ASTM E1921 hinsichtlich seiner Übertragbarkeit auf ferritisches Gusseisen mit Kugelgraphit (DCI) untersucht. Zielsetzung ist die Bereitstellung einer Vorgehensweise zur Bestimmung und Bewertung der dynamischen Bruchzähigkeit von DCI im Übergangsbereich. In diesem Beitrag wird der Versuchswerkstoff der Festigkeitsklasse GJS-400 näher vorgestellt. Ferner werden erste Ergebnisse von zwei bruchmechanischen Versuchsserien an SE(B)140-Großproben bei Belastungsraten von ca. 6∙104 MPa√ms-1 bei -40 °C und -60 °C präsentiert. T2 - 56. Tagung des DVM-Arbeitskreises Bruchmechanik und Bauteilsicherheit CY - Kassel, Germany DA - 20.02.2024 KW - Dynamische Beanspruchung KW - Bruchmechanik KW - Master Curve-Konzept KW - Gusseisen mit Kugelgraphit PY - 2024 DO - https://doi.org/10.48447/BR-2024-BB SP - 49 EP - 58 PB - DVM-Verlag CY - Berlin AN - OPUS4-59518 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Holzwarth, Marcel A1 - Baer, Wolfram A1 - Mayer, Uwe A1 - Weihe, Stefan ED - Vormwald, Michael T1 - Untersuchung des Master Curve-Konzepts für ferritisches Gusseisen mit Kugelgraphit: Kritische Belastungsrate und erste Ergebnisse an C(T)-Proben N2 - Im laufenden Verbundprojekt MCGUSS untersuchen dieProjektpartner MPA Stuttgart und BAM Berlin das probabilistische Master Curve (MC) Konzept nach ASTM E1921 hinsichtlich seiner Übertragbarkeit auf ferritisches Gusseisen mit Kugelgraphit (DCI). Ziel des Projektes ist die Entwicklung einer Methode zur Bestimmung und Bewertung der dynamischen Bruchzähigkeit von DCI im Übergangsbereich. In diesem Beitrag werden die Eigenschaften des verwendeten Werkstoffs der Festigkeitsklasse GJS-400 vorgestellt und die sich daraus ergebenden Probenentnahmestellen näher erläutert. Weiterhin werden erste Ergebnisse der C(T)25-Versuchsserien vorgestellt, die bei Belastungsraten von ca. 5∙103 MPa√ms-1, 5∙104 MPa√ms-1 und 5∙105 MPa√ms-1 und einer Temperatur von -40 °C durchgeführt wurden. T2 - 56. Tagung des DVM-Arbeitskreises Bruchmechanik und Bauteilsicherheit CY - Kassel, Germany DA - 20.02.2024 KW - Dynamische Belastung KW - Master Curve KW - Gusseisen KW - C(T)-Proben PY - 2024 SP - 37 EP - 47 PB - DVM Verlag CY - Berlin AN - OPUS4-59519 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Holzwarth, M. A1 - Baer, Wolfram T1 - Untersuchung des Master Curve-Konzeptes für ferritisches Gusseisen mit Kugelgraphit N2 - Das Master Curve (MC) Konzept nach ASTM E1921 wird momentan u.a. in der Kerntechnik für die bruchmechanische Sicherheitsbewertung ferritischer Stähle eingesetzt. Für ferritisches Gusseisen mit Kugelgraphit (GJS) fehlt jedoch eine Validierung dieser Methode und ggf. eine systematische Überprüfung möglicher Modifikationen grundlegender Ansätze des MC-Konzepts. Aus diesem Grund soll in einem kürzlich gestarteten BMUV-Verbundprojekt zwischen der MPA Stuttgart und der BAM Berlin die Anwendbarkeit des MC-Konzepts auf GJS bei dynamischer Beanspruchung untersucht werden. Ziel ist es, eine effektive und effiziente Methodik bereitzustellen, mit der mittels einer vergleichsweise kleinen Stichprobe bruchmechanischer Kleinproben eine Referenztemperatur T0 zur werkstoffspezifischen Temperaturjustierung der MC ermittelt werden kann. T2 - 55. Jahrestagung des DVM-Arbeitskreises Bruchmechanik und Bauteilsicherheit CY - Darmstadt, Germany DA - 14.02.2023 KW - Bruchmechanik KW - Master Curve-Konzept KW - Dynamische Beanspruchung KW - Gusseisen mit Kugelgraphit PY - 2023 AN - OPUS4-57025 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baer, Wolfram T1 - Untersuchung des Master Curve-Konzepts für Ferritisches Gusseisen mit Kugelgraphit: Versuchswerkstoff und erste Ergebnisse von SE(B)140-Grossproben N2 - In einem laufenden Kooperationsprojekt zwischen der BAM Berlin und der MPA Stuttgart wird das probabilistische Master Curve (MC) Konzept nach ASTM E1921 hinsichtlich seiner Übertragbarkeit auf ferritisches Gusseisen mit Kugelgraphit (DCI) untersucht. Zielsetzung ist die Bereitstellung einer Vorgehensweise zur Bestim-mung und Bewertung der dynamischen Bruchzähigkeit von DCI im Übergangsbe-reich. In diesem Beitrag wird der Versuchswerkstoff der Festigkeitsklasse GJS-400 näher vorgestellt. Ferner werden erste Ergebnisse von zwei bruchmechanischen Versuchsserien an SE(B)140-Großproben bei Belastungsraten von ca. 6∙104 MPa√ms-1 bei -40 °C und 60 °C präsentiert. T2 - Jahrestagung des DVM-Arbeitskreises Bruchmechanik und Bauteilsicherheit CY - Kassel, Germany DA - 20.02.2024 KW - Bruchzähigkeit KW - Sprödbruch KW - Master Curve KW - Gusseisen mit Kugelgraphit KW - ASTM E1921 PY - 2024 AN - OPUS4-59860 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Mayer, Uwe T1 - Untersuchung des Master Curve-Konzeptes für ferritisches Gusseisen mit Kugelgraphit N2 - In dem Poster werden der Forschungsansatz, die Ziele, das Untersuchungsprogramm und die erwarteten Ergebnisse des BMUV-Forschungsvorhabens MCGUSS "Untersuchung des Master Curve-Konzeptes für ferritisches Gusseisen mit Kugelgraphit" vorgestellt. Mit Blick auf bruchmechanische Sicherheitsbewertungen in der Kerntechnik werden Stähle momentan mit dem deterministischen ASME-Referenzkurvenkonzept, ergänzt durch das probabilistische Master Curve-Konzept nach ASTM E1921, bewertet. Das Master Curve-Konzept wird bereits für die Bewertung von ferritischen Schmiedestahlbehältern verwendet. Bewertungsmethoden für ferritisches Gusseisen mit Kugelgraphit sind im Moment unvollständig. Normen wie die nationale BDG-Richtlinie P300 oder der internationale ASME-Code, Sect. III, Div. 3, WC-2330 decken Sprödbruch nicht ausreichend ab. Die Verwendung des Master Curve-Konzepts für ferritisches Gusseisen mit Kugelgraphit würde eine bruchmechanische Bewertung via einer KJc,d Verteilung erlauben und gleichzeitig Größeneffekte und einen Temperaturbereich von 100 K berücksichtigen. T2 - GRS-Projektstatusgespräch 2023 CY - Karlsruhe, Germany DA - 06.11.2023 KW - Dynamische Bruchzähigkeit KW - Sprödbruch KW - Gusseisen mit Kugelgraphit KW - Master Curve PY - 2023 AN - OPUS4-59060 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Mayer, Uwe T1 - Untersuchung des Master Curve-Konzeptes für ferritisches Gusseisen mit Kugelgraphit N2 - In dem Vortrag werden der Forschungsansatz, die Ziele, das Untersuchungsprogramm und die erwarteten Ergebnisse des BMUVForschungsvorhabens MCGUSS "Untersuchung des Master Curve-Konzeptes für ferritisches Gusseisen mit Kugelgraphit" vorgestellt. Mit Blick auf bruchmechanische Sicherheitsbewertungen in der Kerntechnik werden Stähle momentan mit dem deterministischen ASME Referenzkurvenkonzept, ergänzt durch das probabilistische Master Curve-Konzept nach ASTM E1921, bewertet. Das Master Curve-Konzept wird bereits für die Bewertung von ferritischen Schmiedestahlbehältern verwendet. Bewertungsmethoden für ferritisches Gusseisen mit Kugelgraphit sind im Moment unvollständig. Normen wie die nationale BDG-Richtlinie P300 oder der internationale ASME-Code, Sect. III, Div. 3, WC-2330 decken Sprödbruch nicht ausreichend ab. Die Verwendung des Master Curve-Konzepts für ferritisches Gusseisen mit Kugelgraphit würde eine bruchmechanische Bewertung via einer KJc,d Verteilung erlauben und gleichzeitig Größeneffekte und einen Temperaturbereich von 100 K berücksichtigen. T2 - GRS-Projektstatusgespräch 2023 CY - Karlsruhe, Germany DA - 06.11.2023 KW - Dynamische Bruchzähigkeit KW - Master Curve KW - Gusseisen mit Kugelgraphit KW - Sprödbruch PY - 2023 AN - OPUS4-59061 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Holzwarth, M. T1 - First results for the modification of the master curve concept for ferritic ductile cast iron N2 - Within the scope of fracture mechanics safety, ferritic ductile cast iron (DCI) does currently not have an established and validated method to determine and assess dynamic fracture toughness values in the ductile-to-brittle transition regime. For this reason, the applicability of the fracture mechanics Master Curve concept according to ASTM E1921 to DCI is being investigated in a joint research project between MPA Stuttgart and BAM Berlin. To investigate the applicability of the Master Curve concept for DCI, a DCI material of grade GJS-400 has been procured via a detailed manufacturing specification. From this material test specimens of various geometries and sizes (Tensile, Charpy-V, Pellini, SE(B)10, SE(B)25, SE(B)140, DC(T)9, C(T)25 and C(T)50) were produced. In total, about 500 test specimens will be tested to investigate and validate the Master Curve Concept as well as other assumptions (e.g. size effects, Weakest-Link, Weibull distribution) for DCI. While the whole project has not yet concluded, several work packages have yet been completed. Selected test results using C(T)25 specimens are presented. T2 - European Conference on Fracture 2024 CY - Zagreb, Croatia DA - 26.08.2024 KW - Dynamic fracture toughness KW - Ductile cast iron KW - Master curve PY - 2024 AN - OPUS4-61451 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Madia, Mauro A1 - Baer, Wolfram A1 - Wagener, Rainer A1 - Kiyak, Yusuf T1 - Betriebsfestigkeit und Bruchverhalten von bainitischen Schmiedestählen N2 - Die neue Generation von bainitischen Schmiedestählen bietet auf der einen Seite ein erhebliches Festigkeitspotenzial, das es im Sinne des Leichtbaus auch für zyklisch belastete Sicherheitsbauteile zu heben gilt. Auf der anderen Seite geht mit dieser Festigkeitssteigerung im Vergleich zu Vergütungsstählen ein Verlust an Duktilität und Zähigkeit einher. Am Beispiel des Demonstratorbauteils Achsschenkel ging das Forschungsvorhaben der Frage nach, wie ein Freigabeprozess zu gestalten ist, damit das Festigkeitspotenzial der neuen Stähle zuverlässig ausgenutzt werden kann. Als Ergebnis wird eine Vorgehensweise dargestellt, die den Eigenschaften der neuen Generation von Schmiedestählen Rechnung trägt, um den sicheren Betrieb der Komponenten zu gewährleisten. KW - Bainitischer Schmiedestahl KW - Bruchmechanik KW - Sicherheit KW - Betriebsfestigkeit KW - Bauteilauslegung PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-594296 SN - 2366-5106 SP - 50 EP - 54 PB - Industrieverband Massivumformung e. V CY - Hagen AN - OPUS4-59429 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baer, Wolfram A1 - Wossidlo, Peter ED - Zimmermann, M. T1 - Zur Frage der Verwendung von Untermaßprobenergebnissen des Kerbschlagbiegeversuchs - Eine ernüchternde Bilanz N2 - Der Kerbschlagbiegeversuch ist seit der ersten Hälfte des letzten Jahrhunderts standardisiert und seit langem als Prüfverfahren international genormt. Weltweit sind zu garantierende Werte der Kerbschlagenergie (KV) und Übergangstemperaturen (TÜ) in Produktnormen und Regelwerken festgelegt. Unter bestimmten Bedingungen besteht dabei die Option, statt Normalproben Untermaßproben zu prüfen. Im Rahmen einer Untersuchung der BAM wurde der aktuelle Status von Prüf- und Produktnormen sowie Regelwerken zur Bewertung der Bauteilintegrität hinsichtlich ihres Umgangs mit Untermaßprobenergebnissen erfasst. Zur Schaffung einer geeigneten aktuellen Datenbasis wurden an ISO-V-Proben der Dicken 2,5, 5,0, 7,5 und 10,0 mm aus vier aktuellen Baustählen KV2-T-Kurven ermittelt. Es wurden unterschiedliche Vorgehensweisen zur Kurvenanpassung und Festlegung von Übergangstemperaturen praktiziert. Ferner kamen verfügbare Ansätze zur Skalierung von Untermaßprobenergebnissen auf die Werte von Normalproben zur Anwendung. Das Ausmaß des Probendickeneffektes ist werkstoff- und temperaturabhängig. Im Bereich der Werkstoffprüfung ist akzeptiert, dass die Ergebnisse von Normal- und Untermaß-proben nicht ohne Weiteres ineinander überführt werden können. Der Stand der Produktnormung und der Regelwerke ist jedoch im besten Falle als unzureichend, vielfach jedoch schlicht als falsch zu bezeichnen. In einem weiten anwendungsrelevanten Temperaturbereich werden hier sogar deutlich nicht-konservative Skalierungsergebnisse geliefert. Die betroffenen Produkt-normenreihen und Regelwerke müssen überarbeitet werden. T2 - 40. Vortrags- und Diskussionstagung Werkstoffprüfung 2022: Werkstoffe und Bauteile auf dem Prüfstand, Prüftechnik – Kennwertermittlung – Schadensvermeidung CY - Dresden, Germany DA - 27.10.2022 KW - Kerbschlagbiegeversuch, Untermaßproben, Normalproben, Skalierung von Ergebnissen PY - 2022 SP - 1 EP - 6 PB - Deutsche Gesellschaft für Materialkunde (DGM) CY - Sankt Augustin AN - OPUS4-56155 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baer, Wolfram T1 - Zur Frage der Verwendung von Untermaßprobenergebnissen des Kerbschlagbiegeversuchs – eine ernüchternde Bilanz N2 - Der Kerbschlagbiegeversuch ist seit der ersten Hälfte des letzten Jahrhunderts standardisiert und seit langem als Prüfverfahren international genormt. Weltweit sind zu garantierende Werte der Kerbschlagenergie (KV) und Übergangstemperaturen (TÜ) in Produktnormen und Regelwerken festgelegt. Unter bestimmten Bedingungen besteht dabei die Option, statt Normalproben Untermaßproben zu prüfen. Im Rahmen einer Untersuchung der BAM wurde der aktuelle Status von Prüf- und Produktnormen sowie Regelwerken zur Bewertung der Bauteilintegrität hinsichtlich ihres Umgangs mit Untermaßprobenergebnissen erfasst. Zur Schaffung einer geeigneten aktuellen Datenbasis wurden an ISO-V-Proben der Dicken 2,5, 5,0, 7,5 und 10,0 mm aus vier aktuellen Baustählen KV2-T-Kurven ermittelt. Es wurden unterschiedliche Vorgehensweisen zur Kurvenanpassung und Festlegung von Übergangstemperaturen praktiziert. Ferner kamen verfügbare Ansätze zur Skalierung von Untermaßprobenergebnissen auf die Werte von Normalproben zur Anwendung. Das Ausmaß des Probendickeneffektes ist werkstoff- und temperaturabhängig. Im Bereich der Werkstoffprüfung ist akzeptiert, dass die Ergebnisse von Normal- und Untermaß-proben nicht ohne Weiteres ineinander überführt werden können. Der Stand der Produktnormung und der Regelwerke ist jedoch im besten Falle als unzureichend, vielfach jedoch schlicht als falsch zu bezeichnen. In einem weiten anwendungsrelevanten Temperaturbereich werden hier sogar deutlich nicht-konservative Skalierungsergebnisse geliefert. Die betroffenen Produkt-normenreihen und Regelwerke müssen überarbeitet werden. T2 - 40. Vortrags- und Diskussionstagung Werkstoffprüfung 2022 CY - Dresden, Germany DA - 27.10.2022 KW - Skalierung von Ergebnissen KW - Kerbschlagbiegeversuch KW - Untermaßproben KW - Normalproben PY - 2022 AN - OPUS4-56156 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wallin, Kim A1 - Baer, Wolfram T1 - Evaluation of Charpy-V transition curve fitting based on distribution-free statistical assessment N2 - A non-parametric, distribution-free, statistical assessment of 5 large Charpy transition curve data sets is used for the optimum fitting equations for smaller data sets. The assessment makes use of a combination of rank probability and binomial probability analysis of the data. The original non-parametric assessment method is improved by combining upper and lower bound binomial estimates, thus removing a bias that exists in the original method. The non-parametric assessment is not suitable as a standard method because it requires too many data points to give a reliable result. It is, however, ideal as a research tool to examine transition curve shape and scatter. Based on the assessment several recommendations for transition curve fitting can be made. KW - Mechanical Engineering KW - Mechanics of Materials KW - General Materials Science KW - Charpy Impact Test KW - Charpy Transition Curve PY - 2023 DO - https://doi.org/10.1016/j.ijpvp.2023.105079 SN - 0308-0161 VL - 206 SP - 1 EP - 13 PB - Elsevier B.V. AN - OPUS4-58635 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baer, Wolfram T1 - Chunky Graphite - Recognition, Quantification, and Impact on Properties of Spheroidal Graphite Cast Iron N2 - Since there is a continuously growing demand for complex, frequently heavy-sectioned spheroidal graphite cast iron (SGI) castings it is worth paying attention to the chunky graphite (CHG) degeneration which may occur under certain technological circumstances. Although a reference line for preventive actions in terms of general metallurgical and process measures could be drawn to avoid CHG in heavy-sectioned ferritic SGI castings, a broad majority of experts claim the avoidance of CHG in heavy sections cannot yet be rated a hundred percent process safe. A major reason may be seen in the fact that a universal, generally accepted explanation of CHG formation and growth has not yet been established, although several theories have been proposed. Nevertheless, metallurgical aspects are not in the focus of this paper. This paper is about the current state of methods to detect CHG in SGI on the laboratory and component scales. Capabilities and limits of different metallographic, fractographic and non-destructive computer tomographic methods to recognize and quantify CHG are discussed. With respect to the characteristic fili-gree three-dimensional string-like, multi-branched CHG structure, which is non-isometric and non-dispersed, serious implications on the possibility to quantitatively characterize the amount of CHG must be considered. In contrary to the metallurgical aspects, the knowledge about the impact of CHG on the materials and com-ponents properties is still surprisingly limited. Therefore, special emphasis of this paper is on the impact of CHG degeneration on the properties of ferritic SGI. Experimental results are reviewed to illustrate the effect of CHG on mechanical strength and ductility properties as well as fracture mechanics properties in terms of crack resistance and fracture toughness. The present situation is characterized by discussions and uncertainty about the acceptance or rejection of SGI components containing CHG. Addressing this, conclusions from the materials engineering point of view are drawn for quality control, a safe operational strategy in the foundry and component safety. T2 - InCeight Casting 2023 CY - Darmstadt, Germany DA - 06.03.2023 KW - Chunky graphite KW - Structure KW - Recognition KW - Quantification KW - Tensile properties KW - Fracture toughness KW - Ferritic spheroidal KW - Graphite cast iron PY - 2023 AN - OPUS4-57121 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baer, Wolfram T1 - Detection and understanding of the chunky graphite degeneration in ferritic spheroidal graphite cast iron materials with respect to fatigue N2 - CHG is very different compared to other graphite degenerations or defects; Filigree, multi-branched string-like, 3d interconnected structure; Morphology and volumetric amount of CHG cannot be accessed by stereological interpretation of 2d section data; Field-tested, technically established method to quantify CHG in components not available; Fatigue: CHG causes substantial reduction in fatigue limit and significant increase in crack growth rate; Therefore: Avoid or exclude CHG! T2 - 4th International Symposium on Fatigue Design and Material Defects CY - Online meeting DA - 26.05.2020 KW - Ductile cast iron KW - Chunky graphite degeneration KW - Fatigue KW - Correlation microstructure to properties PY - 2020 AN - OPUS4-54409 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baer, Wolfram A1 - Breidung, Marc A1 - Kiyak, Yusuf A1 - Zerbst, Uwe A1 - Madia, Mauro A1 - Küppers, M. T1 - Aspekte der analytischen bruchmechanischen Bauteilbewertung N2 - Am Beispiel eines abgesetzten zylindrischen Bauteils (Achsschenkel) werden Probleme der analytischen bruchmechanischen Bauteilbewertung diskutiert. Als Basis-philosophie wird ein Fail Safe-Kriterium (kontrolliertes Versagen) angesetzt. Die Forderung ist, dass sich der Achsschenkel, bevor er bricht, in einem Ausmaß plastisch verformen kann, bei dem der Fahrer bemerkt, dass mit seinem Fahrzeug etwas nicht in Ordnung ist. Um das zu gewährleisten, muss der Werkstoff einen bestimmten Riss-widerstand aufweisen. Dazu werden im hier vorgestellten ersten Teil des Projektes mittels FEM Rissspitzenbeanspruchungen in Abhängigkeit von der Auslenkung des Zylinders und angenommener Rissgrößen ermittelt. Diese finden als Zielgrößen in der weiteren Analyse Anwendung. Da eine einfach umzusetzende Lösung angestrebt wird, werden zusätzlich analytische Rechnungen an Ersatzgeometrien (halbunendliche Platte und Vollzylinder), aber mit den realen Spannungen am Bauteil durchgeführt. Es zeigt sich, dass die Ergebnisse wegen des Steifigkeitsunterschieds zwischen Bauteil und Ersatzgeometrie unvertretbar konservativ sind. Alternativ wird ein hybrides Konzept vorgestellt, für das die Modellparameter mittels FEM bestimmt werden. Es liefert sehr genaue Ergebnisse. Im Rahmen der analytischen Rechenvorschrift können die Lösungen auf andere Werkstoffe übertragen werden, ohne dass zusätzliche FEM-Analysen notwendig sind. T2 - 54. Tagung des DVM-Arbeitskreises Bruchmechanik und Bauteilsicherheit CY - Online meeting DA - 22.02.2022 KW - FEM KW - Bauteilbewertung KW - Fail-safe KW - Analytisches Modell PY - 2022 DO - https://doi.org/10.48447/Br-2022-BB VL - 254 SP - 1 EP - 11 PB - DVM CY - Berlin AN - OPUS4-54406 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baer, Wolfram A1 - Holzwarth, M. A1 - Mayer, U. T1 - Investigation of the Master Curve Concept for ferritic Ductile Cast Iron N2 - Based on state-of-the-art research and regulations, the application of the fracture mechanics master curve (MC) concept to ferritic ductile cast iron (DCI) is being investigated in a recently started German joint research project between BAM Berlin and MPA Stuttgart. This paper outlines the research approach and the planned investigations and provides first results. According to the IAEA guidelines SSG 26, the safety assessment of DCI containers for transport as well as interim and final storage of radioactive materials is based on the fracture mechanics criterion of general crack initiation exclusion. Within this context, the focus of the current research project is on the further development of brittle fracture safety assessment methods under dynamic loading conditions. Within fracture mechanics safety assessments for steels in nuclear technology, the probabilistic MC concept according to ASTM E1921 is currently used for quasi-static loading conditions as a supplement to the established deterministic ASME reference curve concept. The MC concept allows for an effective statistical consideration of the scatter of the material toughness in the transition regime. Furthermore, the MC can also be used for elevated loading rates as they occur in accident or crash scenarios. However, for DCI, a systematic review of potential modifications to the MC assumptions and procedure according to ASTM E1921 and an associated validation are still lacking. Therefore, a corresponding methodology shall be established to determine and assess dynamic fracture toughness values of DCI in the ductile-to-brittle transition regime, using samples extracted from a component. For the experimental program, a DCI material was produced as it is generally used for transport and storage containers. A basic mechanical-technological material characterization consisting of tensile, Charpy, and Pellini tests is planned. A comprehensive fracture mechanics test program was compiled covering dynamic testing of DC(T)9, C(T)25, C(T)50, SE(B)10, SE(B)25, and SE(B)140 specimens. Moreover, numerical analyses of different specimen geometries and test setups are planned to investigate the influences of stress triaxiality and loading rate. Throughout the experimental program, the microstructure-property relationship will be investigated based on quantitative metallographic and fractographic analyses. Finally, different MC assessment strategies will be considered, and modifications will be made if necessary. T2 - PATRAM22 Conference CY - Juans-les-Pins, France DA - 11.06.2023 KW - Master Curve KW - Ductile cast iron KW - Dynamic fracture toughness PY - 2023 SP - 1 EP - 9 PB - World Nuclear Transport Institute AN - OPUS4-57765 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baer, Wolfram A1 - Ohm, Katrin A1 - Holzwarth, Marcel A1 - Mayer, Uwe T1 - Master Curve-Auswertungen und fraktographische Analysen zum Bruchmechanismus – neue Ergebnisse zur Untersuchung des Master Curve Konzepts für ferritisches Gusseisen mit Kugelgraphit bei dynamischer Beanspruchung (Projekt MCGUSS) N2 - In diesem Beitrag werden erste Master Curve (MC)-Auswertungen und fraktographische Analysen zum Bruchmechanismus aus dem laufenden Kooperationsprojekt MCGUSS zwischen der BAM Berlin und der MPA Stuttgart diskutiert. Für zwei SE(B)140-Großprobenversuchsserien mit je 6-8 Versuchen bei -40 °C bzw. -60 °C und Belastungsraten von 5-8x10^4 MPa√m/s wurden Referenztemperaturen T0 bestimmt. Ergänzt wird dies für erste Versuchsreihen an SE(B)25-Kleinproben, die bei -60 °C und Belastungsraten von ca. 2x10^5 MPa√m/s geprüft wurden. An ausgewählten Bruchflächen dieser Versuche wurden detaillierte fraktographische REM-Analysen vorgenommen. Im Vordergrund stand die Charakterisierung des Bruchmechanismus in Abhängigkeit von den Einflussfaktoren Temperatur und Probengröße. In Richtung der Zähigkeitstieflage werden die Analysen komplettiert durch die Ergebnisse von zwei SE(B)140-Großprobenversuchen bei -100 °C bzw. -140 °C und Belastungsraten von ca. 5-8x10^4 MPa√m/s. T2 - 57. Tagung des DVM-Arbeitskreises Bruchmechanik und Bauteilsicherheit CY - Köln, Germany DA - 18.02.2025 KW - Dynamische Beanspruchung KW - Bruchmechanik KW - Master Curve-Konzept KW - Gusseisen mit Kugelgraphit PY - 2025 DO - https://doi.org/10.48447/BR-2025-467 SP - 113 EP - 122 PB - DVM-Verlag CY - Berlin AN - OPUS4-62554 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Holzwarth, Marcel A1 - Baer, Wolfram A1 - Mayer, Uwe A1 - Weihe, Stephan T1 - Investigation of the Master Curve Concept for Ferritic Ductile Cast iron N2 - Within fracture mechanics safety assessment for steels in nuclear technology, the probabilistic master curve (MC) concept according to ASTM E1921 is currently used for quasi-static loading conditions as a supplement to the established deterministic ASME reference curve concept. However, for ductile cast iron (DCI), a systematic review of potential modifications to the assumptions and the procedure according to ASTM E1921 and an associated validation are still lacking. For this reason, the application of the fracture mechanics MC concept to ferritic ductile cast iron is being investigated in a recently started joint research project between MPA Stuttgart and BAM Berlin. According to the IAEA guidelines SSG 26, the safety assessment of DCI containers for transport as well as storage of radioactive materials is based on the fracture mechanics criterion of general crack initiation exclusion. Within this context, the focus of the current research project is on the further development of brittle fracture safety assessment methods. Therefore, a methodology shall be established to determine and assess dynamic fracture toughness values of DCI in the ductile-to-brittle transition regime, using samples extracted from a component. For the experimental program, a DCI material will be produced as it is generally used for transport and storage containers. A basic mechanical-technological material characterization consisting of tensile, Charpy and Pellini tests is planned and a comprehensive fracture mechanics test program was compiled covering dynamic testing of DC(T)9, C(T)25, C(T)50, SE(B)10, SE(B)25, and SE(B)140 specimens. Numerical analyses of different specimen geometries and test setups are planned to investigate the influences of stress triaxiality and loading rate. Throughout the experimental program, the microstructure-property relationship will be investigated based on quantitative metallographic and fractographic analyses. Finally, different MC assessment strategies will be considered and modifications will be made if necessary. T2 - 21st International Symposium ASTM/ESIS Symposium on Fatigue and Fracture Mechanics CY - Washington, D.C., USA DA - 08.11.2023 KW - Dynamic Fracture Toughness KW - Cleavage fracture KW - Master Curve Concept KW - Ductile Cast Iron PY - 2023 AN - OPUS4-59063 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Holzwarth, Marcel T1 - Investigation of the Master Curve Concept for Ferritic Ductile Cast Iron N2 - Within fracture mechanics safety assessment for steels in nuclear technology, the probabilistic master curve (MC) concept according to ASTM E1921 is currently used for quasi-static loading conditions as a supplement to the established deterministic ASME reference curve concept. However, for ferritic ductile cast iron (DCI), a systematic review of potential modifications to the assumptions and the procedure according to ASTM E1921 and an associated validation are still lacking. For this reason, the application of the fracture mechanics MC concept to ferritic ductile cast iron is being investigated in a joint research project between MPA Stuttgart and BAM Berlin. According to IAEA SSG-26, the safety assessment of DCI containers for transport as well as storage of radioactive materials is based on the fracture mechanics criterion of general crack initiation exclusion. Within this context, the focus of the research project is on brittle fracture. The goal is the establishment of a methodology to determine and assess dynamic fracture toughness values of DCI in the ductile-to-brittle transition regime, using samples extracted from a component. The experimental program uses a DCI material of grade GJS-400, which is generally used for transport and storage containers of radioactive materials. Firstly, a basic mechanical-technological material characterization will be performed consisting of tensile, Charpy and Pellini tests. Following the material characterization, the loading rate relevant for brittle fracture will be determined using instrumented C(T)25-fracture tests at a temperature of -40°C. To be able to transfer the relevant loading rate to other specimen geometries or sizes, the time-dependent course of the Weibull stress is assessed via numerical analyses. With this information an extensive experimental program consisting of DC(T)9, C(T)25, C(T)50, SE(B)10, SE(B)25 and SE(B)140 specimens is performed. These experimental results will be further supported by numerical and fractographic analyses. The empirical experimental database developed for DCI materials will be used to assess the applicability of the MC concept for DCI materials under dynamic loading. At the current time manufacturing and precracking of test specimens is ongoing. The authors provide first results concerning the mechanical-technological material characterization, the relevant loading rate for brittle fracture determined via C(T)25 tests, and some early results of other specimen types. These experimental results are also supported by preliminary numerical and statistical analyses. T2 - Conference SMiRT27 CY - Yokohama, Japan DA - 04.03.2024 KW - Dynamic fracture toughness KW - Ductile cast iron KW - ASTM E1921 KW - Master curve KW - Brittle fracture PY - 2024 AN - OPUS4-59859 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Holzwarth, Marcel A1 - Mayer, Uwe A1 - Baer, Wolfram A1 - Weihe, Stefan T1 - Investigation of the Master Curve Concept for Ferritic Ductile Cast Iron N2 - Within fracture mechanics safety assessment for steels in nuclear technology, the probabilistic master curve (MC) concept according to ASTM E1921 is currently used for quasi-static loading conditions as a supplement to the established deterministic ASME reference curve concept. However, for ductile cast iron (DCI), a systematic review of potential modifications to the assumptions and the procedure according to ASTM E1921 and an associated validation are still lacking. For this reason, the application of the fracture mechanics MC concept to ferritic ductile cast iron is being investigated in a joint research project between MPA Stuttgart and BAM Berlin. According to Hojo et al. (2008) the MC concept is already in use for the brittle fracture safety assessment of ferritic forged steel containers, which would suggest an extension to ductile cast iron containers. In compliance with IAEA SSG-26, the safety assessment of DCI containers for transport as well as storage of radioactive materials is based on the fracture mechanics criterion of general exclusion of crack initiation. Within this context, the focus of the current research project is on the further development of brittle fracture safety assessment methods. Therefore, a methodology shall be established to determine and assess dynamic fracture toughness values of DCI in the ductile-to-brittle transition regime, using only a low number of small fracture mechanics test specimens extracted from a component. For the experimental program, a DCI material of grade GJS-400 (GGG-40) has been produced as it is generally used for transport and storage containers for nuclear material. A basic mechanical-technological material characterization consisting of tensile, Charpy, and Pellini tests has been planned and a comprehensive fracture mechanics test program was compiled covering dynamic testing of DC(T)9, C(T)25, C(T)50, SE(B)10, SE(B)25, and SE(B)140 specimens at various loading rates and temperatures. The specimen testing is divided between the project partners based on specimen geometry. MPA Stuttgart has been tasked with the testing of the C(T), DC(T) and Pellini specimens, while BAM Berlin was assigned the SE(B), Charpy and tensile tests. These tests allow for the determination of the loading rate relevant for brittle fracture via C(T)25 specimens and an assessment of size effects by transferring the relevant loading rate to other specimen geometries and sizes. Numerical analyses of different specimen geometries and test setups are planned to investigate the influence of stress triaxiality and loading rate. Furthermore, the time-dependent course of the Weibull stress is assessed via these numerical analyses. Throughout the experimental program, the microstructure-property relationship will also be investigated based on quantitative metallographic and fractographic analyses like scanning electron microscope images and metallographic sections. With the acquired experimental database fundamental assumptions of the MC concept, like the weakest link model and the Weibull distribution, will be assessed for the application to DCI. In the end, the applicability of the MC concept will be evaluated and if necessary, modifications to the MC concept for DCI will be proposed. This paper will present the preliminary results of the GJS400 material characterization and the related selection of test specimen extraction points. First results of the C(T)25 and SE(B)140 specimen testing will also be discussed supported by first metallographic analyses. T2 - SMiRT27 Conference CY - Yokohama, Japan DA - 03.03.2024 KW - Ductile Cast iron KW - Dynamic Fracture Toughness KW - Safety Assessment KW - Master Curve Concept PY - 2024 SP - 1 EP - 10 AN - OPUS4-59302 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baer, Wolfram ED - Bleicher, C. ED - Kaufmann, H. ED - Pittel, C. T1 - Chunky Graphite - Recognition, Quantification, and Impact on Properties of Spheroidal Graphite Cast Iron N2 - Since there is a continuously growing demand for complex, frequently heavy-sectioned spheroidal graphite cast iron (SGI) castings it is worth paying attention to the chunky graphite (CHG) degeneration which may occur under certain technological circumstances. Although a reference line for preventive actions in terms of general metallurgical and process measures could be drawn to avoid CHG in heavy-sectioned ferritic SGI castings, a broad majority of experts claim the avoidance of CHG in heavy sections cannot yet be rated a hundred percent process safe. A major reason may be seen in the fact that a universal, generally accepted explanation of CHG formation and growth has not yet been established, although several theories have been proposed. Nevertheless, metallurgical aspects are not in the focus of this paper. This paper is about the current state of methods to detect CHG in SGI on the laboratory and component scales. Capabilities and limits of different metallographic, fractographic and non-destructive computer tomographic methods to recognize and quantify CHG are discussed. With respect to the characteristic fili-gree three-dimensional string-like, multi-branched CHG structure, which is non-isometric and non-dispersed, serious implications on the possibility to quantitatively characterize the amount of CHG must be considered. In contrary to the metallurgical aspects, the knowledge about the impact of CHG on the materials and com-ponents properties is still surprisingly limited. Therefore, special emphasis of this paper is on the impact of CHG degeneration on the properties of ferritic SGI. Experimental results are reviewed to illustrate the effect of CHG on mechanical strength and ductility properties as well as fracture mechanics properties in terms of crack resistance and fracture toughness. The present situation is characterized by discussions and uncertainty about the acceptance or rejection of SGI components containing CHG. Addressing this, conclusions from the materials engineering point of view are drawn for quality control, a safe operational strategy in the foundry and component safety. T2 - InCeight Casting Conference 2023 CY - Darmstadt, Germany DA - 06.03.2023 KW - Fracture toughness KW - Chunky graphite KW - Structure KW - Recognition KW - Quantification KW - Ferritic spheroidal graphite cast iron KW - Tensile properties PY - 2023 SN - 978-3-8396-1892-9 SP - 1 EP - 11 PB - Fraunhofer Verlag AN - OPUS4-57120 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Baer, Wolfram A1 - Wossidlo, Peter A1 - Abbasi, Behboud T1 - On the question of how to analyze and apply Charpy pendulum impact test results correctly - Shortcomings in corresponding procedures and standards N2 - This paper is focused on the approximation of absorbed Charpy impact energy-temperature curves (KV-T) and the management of sub-size test piece results in Charpy pendulum impact tests. Both subjects are frequently underestimated but may have a strong impact on the assessment of product quality and structural integrity. The status of related test standards, product standards, structural integrity assessment procedures and corresponding research is reviewed. It is concluded that the state of regulation is partly insufficient and wrong. There is a wide gap between the state of knowledge in the field of materials testing and the requirements of product standards and structural integrity assessment procedures. The present paper aims at boosting and supporting the necessary discussion among the parties involved to raise the level of technical safety. Correspondingly, a large experimental database was created by Charpy impact testing of popular modern structural Steels with nominal yield strength from 235 MPa to 960 MPa. KV-T data were generated using test pieces with thicknesses between 2.5 mm and 10 mm. Different strategies for KV-T curve fitting, definition of transition temperatures, as well as upper and lower shelf energy levels were followed, and different scaling procedures were applied to the sub-size test piece results. The results show that proportional scaling of sub-size to full-size test piece results in terms of KV should be disallowed because it is a wrong approach. Regulations still incorporating such procedures should be revised as soon as possible. Existing nonproportional scaling and conversion procedures were applied. The results obtained illustrate that neither an overall nor consistent conservatism nor an adequate conservatism level can be achieved. In summary, the standardizing bodies should enforce the discussion to revise relevant test standards considering more precise specifications on Charpy data fitting. Furthermore, proposals are made for an improved management of sub-size test piece results. KW - Structural integrity assessment procedure KW - Charpy pendulum impact test KW - Sub-size test piece KW - Standard test piece KW - Curve fitting KW - Conversion of results KW - Absorbed energy KW - Transition temperature KW - Steel KW - Test standard KW - Product standard PY - 2022 DO - https://doi.org/10.1520/JTE20210781 SN - 0090-3973 VL - 50 IS - 4 SP - 2268 EP - 2293 PB - American Society for Testing and Materials (ASTM) CY - West Conshohocken, PA AN - OPUS4-55172 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Holzwarth, Marcel A1 - Baer, Wolfram A1 - Mayer, Uwe A1 - Weihe, Stefan T1 - On the Applicability of the Master Curve Concept for Ductile Cast Iron based on experimental and microstructural results N2 - Based on the state-of-the-art research and regulations, the application of the fracture mechanics master curve (MC) concept to ferritic ductile cast iron (DCI) is being investigated in a joint research project (MCGUSS) between BAM Berlin and MPA Stuttgart. The experimental program included a basic mechanical-technological material characterization consisting of tensile, Charpy and Pellini tests. To determine the relevant loading rate for brittle fracture, instrumented C(T)25 fracture tests were performed at different loading rates at a temperature of -40°C. The relevant loading rates are 5x10^3 MPa√ms-1 and 5x10^4 MPa√ms-1. A series of dynamic fracture tests consisting of DC(T)9, C(T)25 and C(T)50 specimens were performed at MPA. BAM performed corresponding test series with SE(B)10 (pre-cracked Charpy), SE(B)25 and SE(B)140 specimens to cover the influence of specimen geometry. In total about 400 tests were performed during this project. The experimental program is complemented by extensive fractographic and metallographic studies using scanning electron microscopy and cross sectioning, as well as characterizations of the chemical composition of the material and of the morphology and distribution of the graphite particles. KJcd values were evaluated for all C(T)25 specimens and some C(T)50 and DC(T)9 specimens. First Master Curve analyses suggest that modifications on the Master Curve setup will be neccessary for instance changing the coefficient from 0.019 to 0.045. This modification requires further validation and is only one of many possible modifications. The SE(B) specimen results clearly show an inverse size effect. This does not correlate with the weakest link effect attributed to steels which dictates lower fracture toughness values for larger specimens. Due to the presence of graphite particles in the DCI material, it is currently assumed that these particles play a significant role in the failure behavior of DCI materials and the following fracture mechanism is proposed: “Specimen size-dependent arrest of local brittle fracures before global brittle failure by weakest link”. T2 - 9th SEDS Workshop: Safety of Extended Dry Storage, 20.-22. Mai 2025 CY - Garching, Germany DA - 20.05.2025 KW - Statistics KW - Dynamic fracture toughness KW - Ductile cast iron KW - Master curve KW - Safety assessment PY - 2025 SP - 1 EP - 3 AN - OPUS4-63566 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Grimault de Freitas, Tomás A1 - de Araujo Abilio, André A1 - Konert, Florian A1 - Nietzke, Jonathan A1 - Krzysch, Zephanja A1 - Böllinghaus, Thomas A1 - Sobol, Oded T1 - Challenges with metallic materials for the transport and storage of hydrogen N2 - The hydrogen economy is one of the most important solutions to achieve climate neutrality in Europe. It involves the production, storage, transport and use of large quantities of hydrogen in existing and new infrastructures. Components along this supply chain, such as pipelines and storage tanks, are made of various metallic materials, with steel being the most common construction material. The rapid introduction of hydrogen therefore brings with it major challenges, in particular the need for comprehensive qualification of components and materials to ensure the sustainable and safe use of hydrogen technologies. This article provides an overview of the state of the art in the testing of materials and components as well as corresponding future trends and developments for a successful transition to a hydrogen economy. T2 - VGBE - Materials and Quality Assurance 2023 CY - Bergheim, Germany DA - 10.05.2023 KW - Hydrogen Embrittlement KW - Materials Testing KW - Component Testing KW - High-Pressure Gaseous Hydrogen KW - Hollow Specimen Technique PY - 2024 VL - 4 SP - 60 EP - 64 PB - VGBE Energy AN - OPUS4-60686 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Grimault de Freitas, Tomás T1 - Comprehensive Standardisation of the Hollow Specimen Technique for Tests in High-Pressure Hydrogen Gas N2 - The hollow specimen technique is a simple and economical method that has the potential to overcome the limitations and complement the current techniques for qualifying metallic materials under highpressure hydrogen gas. In this technique, an axial hole is manufactured in a tensile specimen, which is then filled with hydrogen gas, sealed, and placed in a standard testing machine. This method requires significantly lower amounts of hydrogen, resulting in fewer safety measures and does not require complex equipment or a specialised laboratory, unlike the conventional autoclave technique. Initial studies have demonstrated the feasibility of assessing hydrogen effects in metallic materials using the hollow specimen technique. This led to the establishment of the committee ISO/TC 164/SC 1/WG 9 to standardise the method, however, there are still open questions that currently prevent the technique from being standardised for hydrogen testing. These open questions are being addressed in the H2HohlZug project, which is presented in this contribution. T2 - Oxford - EPRI Hydrogen Embrittlement Workshop CY - Oxford, United Kingdom DA - 23.06.2024 KW - Hollow Specimen Technique KW - High-pressure Gaseous Hydrogen KW - Hydrogen Embrittlement KW - Tensile Testing PY - 2024 AN - OPUS4-60501 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Koerdt, Andrea T1 - The impact and potential of halophilic microorganisms on alternative fuels N2 - As more industrial interests focusing on using salt caverns and repurposed gas or petroleum reservoirs for alternative fuel storage, i.e. CO2/H2, the question raises whether microorganisms may impact the infrastructure, gas purity and storage condition over time. Environments with high salinity (> 1.5 Meq of NaCl) are resided by halophiles (salt-loving microorganisms). To compensate for the intensive osmotic stress, they have resorted to two main adaptation strategies: 1) production of compatible solutes and 2) accumulation of intracellular KCl. Microbial community analysis of several high salinity environments revealed a number of recurring genera, including Halomonas and Halanaerobium. However, the impact of halophiles on the overall integrity and stability of the storage facilities remain largely unknown. To evaluate the suitability and stability of saline storage facilities, several model halophilic microorganisms, such as members of Halomonas, will be selected as testing subjects. First, the impact of halophiles on the infrastructure will be determined using an integrative approach by combining a number of techniques, including electrochemistry, TOF-SIMS, SEM/FIB/EDS and FIB-TEM. Second, the abilities of halophiles to alter the fuel composition (i.e. increase/decrease the fractions of H2) will be monitored using gas chromatography by growing them under high pressure. As a result of climate change and the accompanying mandatory shift to renewable energy resources, microorganisms will continue to play an important role in the energy sector, both to their benefit and detriment. Thus, it is important to achieve a certain level of understanding regarding the activities and mechanisms of halophiles prior to large-scaled excursions. T2 - ISMOS-8 CY - Online meeting DA - 07.06.2021 KW - Microbiologically influenced corrosion KW - Hydrogen KW - Gas storage KW - Contamination PY - 2021 AN - OPUS4-52891 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Nietzke, Jonathan T1 - Evolution of tensile testing methodologies for hydrogen embrittlement in austenitic steels: a comparative study N2 - The energy transition towards hydrogen utilisation has increased the demand for reliable testing methods to evaluate the susceptibility of metallic materials to hydrogen degradation. However, traditional electrochemical pre-charging techniques have limitations in represent-ing realistic gaseous hydrogen exposure conditions. This study presents three comparative analyses of tensile testing methodologies, focusing on the differences between electrochem-ical pre-charging, gaseous pre-charging, and in-situ testing using hollow specimens for aus-tenitic steels AISI 304L and 316L type austenitic steels. Based on the results obtained, the first comparison reveals that electrochemically pre-charged and gaseously pre-charged specimens exhibit different behaviours regarding the impact on the mechanical properties. This effect can be retraced to the varying distribution of hydrogen throughout the specimens. Although comparable embrittlement was observed for similar hydrogen concentrations, the relationship appears to be non-systematic. The second comparison evaluates the performance of pre-charged hollow specimens (300°C, 100 bar, 21 days) in comparison to hollow specimens tested in-situ under 200 bar hydrogen during slow strain rate tensile tests (SSRT). While pre-charged specimens show a slight de-crease in elongation at fracture and a noticeable decrease in reduction of area (RA), in-situ tested specimens exhibit significantly more pronounced embrittlement. This is in accord-ance with the results of Michler et. al. In the third comparison, geometry effects between pre-charged conventional and pre-charged hollow specimens are explored. In this case, the hydrogen effect appears to be of the same order of magnitude for both specimen types, although some differences are ob-served. The study's findings underscore the importance of considering differences between test methods when assessing materials’ compatibility with hydrogen. It specifically emphasises the need for in-situ testing with gaseous hydrogen to better represent real conditions in ap-plications within the hydrogen sector. Furthermore, the study provides an initial compari-son between conventional and hollow specimens, demonstrating their capability to reveal hydrogen effects. However, additional research is essential to enhance the comparability of results yielded by these testing methods. T2 - European Conference on Fracture 2024 CY - Zagreb, Croatia DA - 26.08.2024 KW - Hollow Specimen Technique KW - Hydrogen KW - Austenitic Stainless Steel KW - Hydrogen Testing KW - AISI 316L PY - 2024 AN - OPUS4-60929 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Nietzke, Jonathan T1 - The relationship between surface condition and the influence of hydrogen on the mechanical properties of additively manufactured 316L N2 - The following contribution presents the analyses of additively manufactured (AM) 316L using hollow specimens at 200 bar hydrogen and a strain rate of 1E-5 s-1. The work includes a comparison of three types of hollow specimens: mechanically extracted from fully additively manufactured cylinders, near-net-shape additively manufactured specimens, i.e. as printed, and specimens made of conventional 316L. AM specimens were manufactured via powder bed fusion with laser beam of metals (PBF-LB/M). For the near-net-shape specimens the inner hole remained without any mechanical processing. The inner holes of the cylindric specimens were manufactured by drilling with subsequent honing. The susceptibility to hydrogen embrittlement was found to be strongly dependent on the surface being in contact with hydrogen. While specimens with a clean surface had a relative reduction of area (RRA) of around 78 %, those with an as-printed surface showed a significantly larger RRA of around 90 %. One possible reason for this are oxide layers formed due to small amounts of oxygen during the AM-process. Further research is required to determine if the lower effect on the mechanical properties is permanently for as printed parts or e.g. time dependent. Additionally, further work with variation in the nominal strain rate is required. T2 - IIW 77th Annual Assembly 2024 CY - Rhodes, Greece DA - 07.07.2024 KW - Austenitic steel 316L KW - Additive manufacturing KW - PBF-LB/M KW - Hydrogen degradation KW - Hydrogen embrittlement KW - Hollow specimen technique PY - 2024 AN - OPUS4-60618 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Nietzke, Jonathan T1 - Stainless Steels and Hydrogen Applications N2 - The contribution was presented at the Stainless Steel World Conference 2022. The presentation shows the influence of hydrogen on the mechanical properties of steel. Some test methods are shown and selected results are presented. T2 - Stainless Steel World Conference 2022 CY - Maastricht, Netherlands DA - 27.09.2022 KW - Gaseous hydrogen KW - Hydrogen Embrittlement KW - Hydrogen assisted cracking KW - SSRT PY - 2022 AN - OPUS4-55913 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Grimault de Freitas, Tomás T1 - Hollow Specimen Technique for Tests in High-Pressure Hydrogen Gas: The Path Towards Standardisation and the Case Study of a Pipeline Steel and its Weld N2 - The hollow specimen technique is a simple method that has the potential to make material qualification with gaseous pressurized hydrogen widely applicable for the hydrogen industry at low cost. The feasibility of this method has been demonstrated in several studies, leading to the establishment of an ISO committee for its standardization. Questions have emerged during this process, that currently prevent the method from being standardized for hydrogen testing. These questions relate to specimen geometry, specimen manufacturing and gas quality and are being systematically addressed in the TransHyDE-H2HohlZug project. The aim is to close the identified gaps towards the standardization of this method for hydrogen testing. This contribution presents the structure and milestones of the project, followed by the results regarding the influence of specimen production and its response to hydrogen effects. Depending on the production method, different roughness and residual stresses can be expected on the inner hole surface of the specimens. This is of importance since an increase in stress concentration sites have been found to be associated to a higher severity of hydrogen effects. This influence has been investigated after applying the following machining processes: a) drilled only; b) drilled and reamed; c) drilled and honed; d) electro-discharge machining (EDM) and honed; e) EDM and reamed. Roughness measurements using a profilometer, electron back-scatter diffraction (EBSD) analysis and microhardness tests have been performed previous to mechanical testing to infer on the effect of the different production methods on the surface of the inner hole. Next, the specimens were mechanically tested via slow strain rate tensile tests in a argon and in hydrogen, both at 150 bar and room temperature. Here, a strain-rate sensibility analysis was also performed to identify an optimal strain-rate for the mechanical tests. Based on the results an optimal production method is identified and proposed. T2 - ASTM Conference on Hydrogen Materials CY - La Rochelle, France DA - 03.06.2025 KW - Hydrogen KW - Hydrogen Embrittlement KW - Hollow Specimen Technique KW - High-Pressure Gaseous Hydrogen KW - Austenitic Stainless Steel KW - H2HohlZug KW - TransHyDE KW - Tensile Test KW - Pipeline Steel PY - 2025 AN - OPUS4-63329 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Sobol, Oded T1 - Challenges with metallic materials in hydrogen technologies N2 - The contribution was presented in the Joint European Summer School in Athens as part of several contributions from BAM in the field of hydrogen safety. These presentations are given in order to provide an overview about the activities of BAM as part of the competence center H2Safety@BAM T2 - JOINT EUROPEAN SUMMER SCHOOL (JESS) CY - Athens, Greece DA - 12.09.2022 KW - Gaseous hydrogen KW - Hydrogen Embrittlement KW - Hydrogen assisted cracking PY - 2022 AN - OPUS4-55822 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baer, Wolfram T1 - Gezielte Werkstoffprüfung zur fail-safe-Bauteilauslegung am Beispiel eines Achsschenkels N2 - Bei der Auslegung von Achsschenkeln für Nutzfahrzeuge wird für den Überlastfall ein fail-safe-Kriterium (kontrolliertes Versagen) als Basisphilosophie angesetzt. Gefordert wird, dass sich der Achsschenkel auch unter Akzeptanz begrenzten Risswachstums hinreichend elastisch-plastisch verformen kann, ohne dass es zum Bruch kommt. Der Fahrer soll anschließend anhand der bleibenden Verformungen bemerken können, dass mit seinem Fahrzeug etwas nicht in Ordnung ist. Eine Voraussetzung für dieses Bauteilverhalten ist eine hinreichende Bruchzähigkeit des Werkstoffs. Diese, wie auch die Rissspitzenbeanspruchung, müssen ermittelt wer-den, um den bruchmechanischen Sicherheitsnachweis führen zu können. Zur Ermittlung der mechanisch-technologischen und bruchmechanischen Werkstoffeigenschaften wurde ein Prüfkonzept entwickelt, bei dem die Proben an der potenziell kritischen Stelle direkt aus den geschmiedeten Achsschenkeln entnommen werden. Die experimentelle Werkstoffcharakterisierung bildet dann die Beanspruchungsbedingungen beim Überlastereignis ab. Im Rahmen der Produktion stehen jedoch nur Kerbschlagarbeitswerte zur Verfügung und aufwändige bruchmechanische Versuche sollen vermieden werden. Deshalb wurde eine Korrelation zur Abschätzung der vorhandenen Bruchzähigkeit aus der Kerbschlagarbeit herangezogen. Es ergibt sich eine Ergebnismatrix, die die Einflussgrößen Versagenswahrscheinlichkeit, Temperatur und Bruchzähigkeit verknüpft. Abschließend wird ein erster Vergleich der abgeschätzten mit den experimentell ermittelten Bruchzähigkeitswerten gezogen. Dieser weist aus, dass die abgeschätzten Werte geringfügig konservativ sind. T2 - 40. Vortrags- und Diskussionstagung Werkstoffprüfung 2022 CY - Dresden, Germany DA - 27.10.2022 KW - Korrelation KW - Achsschenkel KW - Fail-safe KW - Bruchmechanische Auslegung KW - Kerbschlagarbeit PY - 2022 AN - OPUS4-56153 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Bevilacqua, Tommaso A1 - Gumenyuk, Andrey A1 - Habibi, Niloufar A1 - Hartwig, Philipp A1 - Klawonn, Axel A1 - Lanser, Martin A1 - Rethmeier, Michael A1 - Scheunemann, Lisa A1 - Schröeder, Jöerg T1 - Large-scale thermo-mechanical simulation of laser beam welding using high-performance computing: A qualitative reproduction of experimental results N2 - Laser beam welding (LBW) is a non-contact joining technique that has gained significant importance in modern industrial manufacturing. One potential problem, however, is the formation of solidification cracks, which particularly affects alloys with a pronounced melting range. The aim of the present work is the development of computational methods and software tools to numerically simulate LBW. In order to obtain a sufficiently accurate solution, a large number of finite elements has to be used. Therefore, a highly parallel scalable solver framework, based on the software library PETSc, was used to solve this computationally challenging problem on a high-performance computing architecture. Finally, the experimental results and the numerical simulations are compared. They are found to be in good qualitative agreement, which confirms the validity of the numerical simulations and allows for a better interpretation of the experimentally observed strain distribution. KW - Laser beam welding KW - Termo-mechanical processes KW - Solidification cracking KW - High-performance computing KW - Domain decomposition methods PY - 2025 DO - https://doi.org/10.1016/j.rineng.2025.108827 SN - 2590-1230 SP - 1 EP - 33 PB - Elsevier B.V. AN - OPUS4-65290 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kröll, Mirco T1 - Harmonising Tribotests of Polymers in Hydrogen N2 - This talk harmonised methods to investigate friction and wear of commercial and experimental polymer compounds in hydrogen using several tribometers. T2 - Surface Ventures - Symposium on Hydrogen Tribology CY - Online meeting DA - 31.07.2025 KW - Hydrogen KW - Polymers KW - Tribometer KW - Wear KW - Coefficient of Friction KW - Interlaboratory comparison KW - Comparability KW - Harmonisation KW - Standardisation KW - Tribology KW - Oil-coupled compounds KW - FAIR data KW - Database KW - i-TRIBOMAT PY - 2025 AN - OPUS4-63838 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - Effect of temperature on the friction behaviour of rubber materials in hydrogen N2 - Safety and reliability are the major challenges to face for the development and acceptance of hydrogen technology. It is therefore crucial to study deeply material compatibility, in particular for tribological components that are directly in contact with hydrogen. Some of the most critical parts are sealing components that face high risk of damage due variation of pressure, temperature and mechanical stress. In this study, the friction and wear behaviour of several rubber materials was evaluated in hydrogen environment at ambient and low temperature. Tests were performed against 316L disks in a reciprocation motion. Results reveal that the hydrogen affects the friction and wear behaviour of most materials. The friction mechanism is dominated by deformation for most rubber materials at ambient temperature while sliding occurs at low temperature due to the increased hardness of the rubbers. T2 - Polytrib 2024 CY - Portorož, Slovenia DA - 03.10.2024 KW - Reciprocating sliding KW - Rubber materials KW - Hydrogen KW - Low temperature PY - 2024 AN - OPUS4-62019 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - Effect of high-pressure hydrogen environment on the physical and mechanical properties of elastomers N2 - This presentation deals with the exposure of HNBR rubbers to high pressure hydrogen (100 MPa) at 120 °C for 7 and 21 days under static conditions followed by characterization of their physical and mechanical properties.The core areas include swelling, rapid gas decompression, dynamic mechanical analysis (DMA), tensile strength and compression set properties. This study will assist in expanding the knowledge base of elastomer compatibility with hydrogen and therefore contribute significantly to the selection and development of polymer materials deploying hydrogen as a future energy carrier. T2 - EHEC European Hydrogen Energy Conferecne 2022 CY - Madrid, Spain DA - 18.05.2022 KW - Rubbers KW - Hydrogen KW - Characterization PY - 2022 AN - OPUS4-62084 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kröll, Mirco T1 - Harmonised tribological testing of polymers in hydrogen N2 - The focus of this work is to study the tribological performance of polymers in hydrogen atmosphere. Additionally, tests were carried out with up to three different tribometers at two institutions. The challenge to compare and harmonise equipment, procedures, and methods is an important part of the study. T2 - PolyTrib 2024 CY - Portoroz, Slovenia DA - 03.10.2024 KW - Hydrogen KW - Tribometer KW - Comparability KW - Harmonisation KW - Oil-coupled compounds PY - 2024 AN - OPUS4-61224 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Kröll, Mirco T1 - Tribological performance of polymer compounds in gaseous hydrogen N2 - In this study, friction and wear of conventional and alternative high performance polymer compounds, typically used for components of compressors, were investigated in gaseous hydrogen and nitrogen up to 80 bar of gas pressure. The compounds used were a commercial PEEK matrix with 10 wt.% each of PTFE, graphite, and short carbon fibres, a PPS matrix with 10 wt.% each of PTFE and graphite, and an experimental PA12 matrix with PTFE chemically coupled with an oleyl alcohol. Due to the cylindrical shape of the polymer samples, the contact area and pressure change if wear occurs. Therefore, experimental results of pre-screening tests have been used as input for FEM and an analytical model to determine the decreasing contact pressure over time. Afterwards, the outcome of the models was used to determine the duration of the experiments to reach typical contact pressures of seals in hydrogen compressors. T2 - ASMET TriboCorrosion International Conference 2025 CY - Vienna, Austria DA - 23.10.2025 KW - Hydrogen KW - Polymer KW - Tribometer KW - Comparability KW - Harmonisation KW - Oil-coupled compounds KW - Coefficient of Friction KW - Wear KW - FAIR data KW - Standardisation KW - Tribology KW - Database KW - i-TRIBOMAT PY - 2025 AN - OPUS4-64473 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Theiler, Geraldine A1 - Gradt, Thomas T1 - Comparison of the sliding behavior of several polymers in gaseous and liquid hydrogen N2 - The development of hydrogen technologies entails high safety requirements in distribution and dispensing infrastructure. Therefore, it is necessary to pursue research on material compatibility in hydrogen, especially for critical parts with tribological issues. The focus of this study is to evaluate the influence of hydrogen on a wider range of commercially available polymer materials. Thereby, the friction and wear behavior of different grades of TPE, POM, PA66, PA12, PPA, PEEK, PPS, PTFE, PAI, PI and PBI were investigated against a rotating steel disk (AISI 304). Filled and unfilled polymers from different suppliers were evaluated at room temperature in air, vacuum and hydrogen gas (H2) as well as in liquid hydrogen at - 253°C (LH2). The sliding behavior of the polymer materials is discussed by means of surface analyses, whereby special attention is paid to the formation of a transfer film. According to the results at ambient temperature, the effect of hydrogen environment on the tribological behavior of neat polymers may be related to lack of moisture, but also to saturated hydrocarbons in gaseous hydrogen. In liquid hydrogen, the best tribological performances were achieved with neat PA polymers as well as PPS and PI composites. KW - Polymers KW - Composites KW - Sliding wear KW - Hydrogen KW - Cryogenic temperature PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-597123 DO - https://doi.org/10.2474/trol.18.217 SN - 1881-2198 VL - 18 IS - 5 SP - 217 EP - 231 PB - Japanese Society of Tribologists AN - OPUS4-59712 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine A1 - Gradt, Thomas T1 - Comparison of the sliding behaviour of several polymers in hydrogen N2 - The work presented here deals with the friction and wear behaviour of polymer materials in hydrogen. Commercially available grades of PEEK, PA, PPA, PAI, PI and PBI were investigated at room temperature in air and hydrogen gas (H2) as well as in liquid hydrogen at -253°C (LH2). T2 - 7th World Tribology Congress, WTC 2022 CY - Lyon, France DA - 10.07.2022 KW - Friction KW - Wear KW - Polymers KW - Hydrogen KW - Cryogenic PY - 2021 SP - 1 AN - OPUS4-62089 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Theiler, Geraldine A1 - Gradt, Thomas T1 - Influence of counterface and environment on the tribological behaviour of polymer materials N2 - This paper focuses on the influence of the counterface materials on the sliding behaviour of polymer materials in hydrogen. Polyimide (PI), polyetheretherketone (PEEK) and Polytetrafluoroethylene (PTFE) materials were investigated against hardened 52100 martensitic bearing steel and 304 austenitic stainless steel with similar roughness (Ra = 0.2 μm). Results indicate that the friction and wear of PI and PEEK materials depend on the counterface material. This effect wasn’t observed for PTFE composites. While the tribological performance of polyimide is better against 52100 in hydrogen, improved sliding behaviour of PEEK materials is observed with 304 counterface, particularly at higher sliding speed. Surface analyses of the transfer film reveal that the influence of the counterface is primarily related to the chemical nature of the steel for PI and to the thermal conductivity of the disc for PEEK materials. KW - Friction KW - Wear KW - Polymers KW - Hydrogen Transfer Film PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-515483 DO - https://doi.org/10.1016/j.polymertesting.2020.106912 VL - 93 SP - 106912 PB - Elsevier Ltd. AN - OPUS4-51548 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - Influence of the counterface on the sliding behavior of polymer materials in hydrogen N2 - This presentation deals with the influence of the counterface materials on the sliding behaviour of some polymer materials in hydrogen. Polyimide (PI), polyetheretherketone (PEEK) and Polytetrafluoroethylene (PTFE) materials were investigated against hardened 52100 martensitic bearing steel and 304 austenitic stainless steel with similar roughness (Ra = 0.2 μm). Results indicate that the friction and wear of PI and PEEK materials depend on the counterface material. This effect wasn’t observed for PTFE composites. While the tribological performance of polyimide is better against 52100 in hydrogen, improved sliding behaviour of PEEK materials is observed with 304 counterface, particularly at higher sliding speed. Surface analyses of the transfer film reveal that the influence of the counterface is primarily related to the chemical nature of the steel for PI and to the thermal conductivity of the disc for PEEK materials. T2 - Hydrogenius & I2CNER Tribology Symposium CY - Online meeting DA - 29.01.2021 KW - Polymers KW - Hydrogen KW - Counterface KW - Friction KW - Wear PY - 2021 AN - OPUS4-52093 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - Polymer materials in hydrogen N2 - This presentation provides an overview of the applications and challenges related to polymer materials in hydrogen. The effects of hydrogen on polymers are described and test methods to evaluate the interactions between polymers and hydrogen are presented along with case studies. T2 - Masterstudiengang Wasserstofftechnologien DIU CY - Online meeting DA - 25.08.2023 KW - Hydrogen KW - Polymers PY - 2023 AN - OPUS4-61964 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - Tribology of polymeric materials in gaseous and liquid hydrogen N2 - This presentation gives an overview of the tribological behaviour of polymeric materials in gaseous and luquid hydrogen. T2 - HYDROGENIUS-BAM Joint Hydrogen Symposium CY - Online meeting DA - 06.07.2021 KW - Polymers KW - Hydrogen KW - Friction KW - Wear PY - 2021 AN - OPUS4-53701 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - Benchmarking of polymer materials for tribological applications in hydrogen N2 - The focus of this study is to evaluate of hydrogen on the friction and wear behavior of a wide range of polymer materials. Thereby, the tribological performance of filled and unfilled polymers from different suppliers were compared at room temperature in air and hydrogen gas (H2) as well as in liquid hydrogen at -253°C (LH2). T2 - 62. Tribologie-Fachtagung der Gesellschaft für Tribologie e. V. CY - Online meeting DA - 27.09.2021 KW - Polymers KW - Hydrogen KW - Friction KW - Wear PY - 2021 AN - OPUS4-53700 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Cano Murillo, Natalia T1 - Effect of high-pressure hydrogen environment on the physical and mechanical properties of different kinds of carbon black filled elastomers. N2 - As the transition towards the usage of renewable energy is getting urgent, the fluctuations of clean energy production require efficient storage alternatives. Hydrogen offers not only the possibility of energy storage but also, acts as an energy carrier. It is then important to study the effect of highly pressurized hydrogen atmosphere on the materials destinated for its storage and transport, in order to assure the reliable performance of the sealing materials containing hydrogen. In this study, a set of carbon black (CB) filled rubbers comprising hydrogenated acrylonitrile butadiene rubber (HNBR), acrylonitrile butadiene rubber (NBR) and ethylene propylene diene monomer rubber (EPDM) was tested under high pressure hydrogen atmosphere (1000 bar) and at different temperature conditions: 120°C for HNBR, room temperature and 85°C for NBR and EPDM. The influence of hydrogen on the materials properties was measured after 7 days of exposure under hydrogen and evaluated again after 48h. Density and volume change, as well as hardness, tensile tests, compression set, dynamic mechanical measurements and infrared spectroscopy evaluations were conducted to estimate the impact of high-pressure hydrogen on the rubber grades. Our study reveals, an effect on the physical and mechanical properties, possibly related to small changes in the matrix-filler interaction after the hydrogen exposure. All materials, however, show a trend to recover most of their properties 48h after hydrogen exposure. T2 - RubberCon 2023 CY - Edinburgh, Scotland DA - 09.05.2023 KW - Elastomers KW - Hydrogen exposure KW - Mechanical properties PY - 2023 AN - OPUS4-62007 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Theiler, Geraldine T1 - Comparison of the sliding behaviour of several polymers in hydrogen N2 - The work presented here deals with the friction and wear behaviour of polymer materials in hydrogen. Commercially available grades of PEEK, PA, PPA, PAI, PI and PBI were investigated at room temperature in air and hydrogen gas (H2) as well as in liquid hydrogen at - 253°C (LH2). T2 - 7th World Tribology Congress, WTC 2022 CY - Lyon, France DA - 10.07.2022 KW - Friction KW - Wear KW - Polymers KW - Hydrogen KW - Cryogenic PY - 2022 AN - OPUS4-62087 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -