TY - JOUR A1 - Maximilian, Thuy A1 - Spyrantis, Alexander A1 - Böhning, Martin A1 - Niebergall, Ute A1 - Maaß, Robert T1 - Spatially resolved roughness exponent in polymer fracture N2 - The fracture surface of slow and continuous crack propagation during environmental stress cracking of a semicrystalline polyethylene exhibits isotropic roughness exponents at the local scale but resolved across the macroscopic fracture surface a clear position dependence is found. The spatially resolved roughness exponent admits values in the range between 0.1 and 0.4, demonstrating nontrivial exponents in the small length-scale regime. Instead, they vary across the fracture surface according to the stress-state distribution, which suggests that the exponents are intimately linked to the locally dominating dissipation processes during craze cracking. KW - Plasticity KW - Fracture KW - Material failure KW - Mechanical deformation PY - 2022 DO - https://doi.org/10.1103/PhysRevMaterials.6.L090601 VL - 6 IS - 9 SP - 1 EP - 7 PB - American Physical Society CY - USA, Maryland AN - OPUS4-55797 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wachtendorf, Volker T1 - Maßgeschneiderte künstliche Bewitterungstests zur Untersuchung der alterungsbedingten Freisetzung von Produkten in die Umwelt N2 - Genormte künstliche Bewitterungstests sind häufig nicht spezifisch für die Anwendungssituation oder das Material. Das macht die Entwicklung spezifischer Tests erforderlich. Für deren Entwicklung müssen Maximalparameter der Anwendungssituation bekannt sein, womit dann der künstliche Test formuliert wird und dessen Bedingungen werden dann solange optimiert, bis die Korrelation der Effekte von natürlichem und künstlichem Test ausreichend ist. Für Untersuchungen der Freisetzung kann der verbleibende Rest in der Probe und/oder die freigesetzte Menge in Luft, Boden, Wasser bestimmt werden. Im ersten Beispiel der Witterungswirkung wurde die Freisetzung von Kohlenstoff-Nanoröhrchen (CNT) aus Polymer-Kompositen untersucht (unter Verwendung von empfindlich-nachweisbarer radioaktiver 14C-Markierung für einzelne CNT-Partikel), in einem zweiten die Freisetzung von anorganischen und organischen Bestandteilen aus elastomeren Bestandteilen von Sportböden (Bahnen und Kunstrasen) in Wasser. T2 - SKZ-Tagung: Bewitterung van Kunststoffen CY - Würzburg, Germany DA - 06.07.2022 KW - Künstliche Bewitterung KW - UV KW - Degradation KW - Freisetzung KW - CNT KW - Carbo-Nanotubes KW - Composite KW - Nano-Partikel KW - 14C-Markierung KW - Sportböden KW - Kunstrasen KW - Grundwasser PY - 2022 AN - OPUS4-55219 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Tabaka, Weronika A1 - Timme, Sebastian A1 - Lauterbach, Tobias A1 - Medina, L. A1 - Berglund, L. A. A1 - Carosio, F. A1 - Duquesne, S. A1 - Schartel, Bernhard T1 - Bench-scale fire stability testing - Assessment of protective systems on carbon fibre reinforced polymer composites N2 - Fire resistance testing of components made of carbon fibre reinforced polymers (CFRP) usually demands intermediate-scale or full-scale testing. A bench-scale test is presented as a practicable and efficient method to assess how different fire protective systems improve the structural integrity of CFRPs during fire. The direct flame of a fully developed fire was applied to one side of the CFRP specimen, which was simultaneously loaded with compressive force. Three different approaches (film, non-woven, and coatings) were applied: paper with a thickness in the range of μm consisting of cellulose nanofibre (CNF)/clay nanocomposite, nonwoven mats with thickness in the range of cm and intumescent coatings with a thickness in the range of mm. The uncoated specimen failed after just 17 s. Protection by these systems provides fire stability, as they multiply the time to failure by as much as up to 43 times. The reduced heating rates of the protected specimens demonstrate the reduced heat penetration, indicating the coatings’ excellent heat shielding properties. Bench-scale fire stability testing is shown to be suitable tool to identify, compare and assess different approaches to fire protection. KW - Fire stability KW - Bench-scale fire resistance KW - Carbon fibre reinforced polymer KW - Protective coatings PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-532401 DO - https://doi.org/10.1016/j.polymertesting.2021.107340 SN - 0142-9418 SN - 1873-2348 VL - 102 SP - 7340 PB - Elsevier CY - Amsterdam AN - OPUS4-53240 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Jauregui Rozo, Maria A1 - Sunder, S. A1 - Tabaka, Weronika A1 - Klaffke, Benjamin A1 - Ruckdäschel, H. A1 - Schartel, Bernhard T1 - Unveiling aluminum diethyl phosphinate dual identity: Transfer from epoxy resins to glass fiber-reinforced composites N2 - This study examines the transfer of the flame-retardant aluminum diethyl phosphinate (AlPi) from epoxy resins to composites and the impact of AlPi on fire behavior and fire stability. Further, the effects of different particle sizes and the addition of zinc hydroxy stannate (ZHS) and inorganic silicate (InSi) are investigated. The research provides a detailed analysis of the fire behavior, fire stability, pyrolysis, flame-retardant modes of action, and flame retardancy index. Interestingly, the particle sizes did not significantly affect the flammability, fire behavior, or fire stability in the systems investigated. AlPi acts primarily in the gas phase, releasing phosphorus that yields flame inhibition. Adding glass fibers (GFs) to the epoxy resin boosts the flame retardancy in the condensed phase, reducing the heat release rate (HRR), total heat release (THR), and peak heat release rate (PHRR) by about 60%. This improvement is largely due to replacing fuel and forming a protective layer during burning. Despite the differences between thermoset and composite, the study demonstrates an effective transfer of flame-retardant properties from epoxy resins to fiber-reinforced composites, significantly enhancing the flame retardancy performance in both material systems. KW - Aluminum diethyl phosphinate KW - Epoxy resins KW - Fire behavior KW - Fire stability KW - Gas-phase active KW - Glass fiber-reinforced composites KW - Particle sizes PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-643013 DO - https://doi.org/10.1002/pc.29911 SN - 1548-0569 SN - 0272-8397 VL - 46 IS - 14 SP - 12981 EP - 12999 PB - Wiley AN - OPUS4-64301 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Tabaka, Weronika A1 - Meinel, Dietmar A1 - Schartel, Bernhard T1 - Sacrifice Few to Save Many: Fire Protective Interlayers in Carbon- Fiber-Reinforced Laminates N2 - The fire protection of carbon-fiber-reinforced polymer (CFRP) laminates often relies on flame-retardant coatings, but in some applications, their efficacy may diminish upon direct fire exposure due to rapid pyrolysis. This study introduces an innovative approach by integrating protective interlayers within the laminate structure to enhance the fire resistance. Various materials, including ceramic composite WHIPOX, titanium foil, poly(etherimide) (PEI) foil, basalt fibers, rubber mat, and hemp fibers, were selected as protective interlayers. These interlayers were strategically placed within the laminate layout to form a sacrificial barrier, safeguarding the integrity of the composite. Bench-scale fire resistance tests were conducted, where fire (180 kW/m2) was applied directly to the one side of the specimen by a burner while a compressive load was applied at the same time. Results indicate significant prolongation of time to failure for CFRP laminates with protective interlayers, which is up to 10 times longer. This innovative approach represents a potential advance in fire protection strategies for CFRP laminates, offering improved resilience against fire-induced structural failure. KW - Composites in fire KW - Fire resistance KW - Fire retardant interlayers KW - Laminate design KW - Carbon fibre reinforced PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-601943 DO - https://doi.org/10.1021/acsomega.4c01408 SN - 2470-1343 VL - 9 IS - 22 SP - 23703 EP - 23712 PB - ACS AN - OPUS4-60194 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Tabaka, Weronika T1 - Bench-scale fire stability testing - Protective layers in carbon fibre reinforced polymer laminates N2 - Fire resistance testing of components made of carbon fibre reinforced polymers (CFRP) composites usually demands intermediate-scale or full-scale testing. In this study, a bench-scale test is presented as a practicable and efficient method to assess the improvement in structural integrity of CFRP with different protective interlayers during fire. T2 - International Conference on Composite Materials (ICCM23) CY - Belfast, UK DA - 30.07.2023 KW - Fire resistance KW - Bench-scale testing KW - Carbon fibre reinforced polymer composite PY - 2023 AN - OPUS4-58099 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schartel, Bernhard T1 - Small but Great – Multifunctional Graphene in Rubber Nanocomposites N2 - A few layer/multilayer graphene (MLG) with a specific surface area of BET ≥ 250 m2/g is proposed as an efficient multifunctional nanofiller for rubbers. The preparation method, i.e., ultrasonically-assisted solution or latex premixing of master batches followed by conventional two-roll milling, strongly influences the dispersion in the elastomeric matrix and is fundamental for the final properties. When homogenously dispersed, single stacks of only approximately 10 graphene sheets, with an aspect ratio of ca. 35, work at low loadings, enabling the replacement of large amounts of carbon black (CB), an increase in efficiency, and a reduction in filler load. The appropriate preparation yielded nanocomposites in which just 3 phr are sufficient to significantly improve the rheological, curing, gas barrier properties, electrical and thermal conductivity, as well as mechanical properties of different rubbers, as shown for chlorine-Isobutylene-Isoprene rubber (CIIR), nitrile-butadiene rubber (NBR), natural rubber (NR), and styrene-butadiene rubber (SBR).[1-5] 3 phr of MLG tripled the Young’s modulus of CIIR, an effect equivalent to 20 phr of CB. The stronger interactions between MLG and NR or SBR also resulted in a reduction in the elongation at break by 20% and 50%, respectively, while the same parameter was hardly changed for CIIR/MLG and NBR/MLG. CIIR/MLG and NBR/MLG were stiffer but just as defomable than CIIR and NBR. The strong reinforcing effect of 3 phr MLG was confirmed by the increase of greater than 10 Shore A in hardness. MLG reduces gas permeability, increases thermal and electrical conductivities, and retards flammability. We investigated MLG also as a synergist for reducing the aluminium trihydrate loading in flame retardant hydrogenated acrylonitrile-butadiene (HNBR), polybutadiene chloroprene (BR/CR), and chlorosulfonated polyethylene rubber(CSM).[6-8] The higher the nanofiller concentration is, the greater the improvement in the properties. For instance, the permeability decreased by 30% at 3 phr of MLG, 50% at 5 phr and 60% at 10 phr, respectively. Moreover, the MLG nanocomposites improve stability of mechanical properties against the effects of weathering. In key experiments an increase in UV-absorption and a pronounced radical scavenging were proved as stabilizing mechanisms. In a nutshell, MLG is an efficient multifunctional nanofiller ready to be used for innovative rubber development. T2 - 34th PDDG Conference CY - Dubrovnik, Croatia DA - 11.06.2023 KW - Graphene KW - Nanocomposites KW - Reinforcement KW - Antioxydant KW - Flame retardant KW - Durability PY - 2023 AN - OPUS4-57693 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schartel, Bernhard T1 - Multifunctional Elastomer/Graphene Nanocomposites N2 - A few layer/multilayer graphene (MLG) with a specific surface area of BET=250 m2/g is proposed as an efficient multifunctional nanofiller for rubbers. The preparation method, i.e., ultrasonically-assisted solution mixing of master batches followed by two-roll milling, strongly influences the dispersion in the elastomeric matrix and is fundamental for the final properties. When homogenously dispersed, single stacks of only approximately 10 graphene sheets, with an aspect ratio of 34, work at low loadings, enabling the replacement of large amounts of carbon black (CB), an increase in efficiency, and a reduction in filler load. The appropriate preparation yielded nanocomposites in which just 3 phr are sufficient to significantly improve the rheological, curing, gas barrier properties, electrical and thermal conductivity, as well as mechanical properties of different rubbers, as shown for chlorine-Isobutylene-Isoprene rubber (CIIR), nitrile-butadiene rubber (NBR), natural rubber (NR), and styrene-butadiene rubber (SBR). 3 phr of MLG tripled the Young’s modulus of CIIR, an effect equivalent to 20 phr of CB. The stronger interactions between MLG and NR or SBR also resulted in a reduction in the elongation at break by 20% and 50%, respectively, while the same parameter was hardly changed for CIIR/MLG and NBR/MLG. CIIR/MLG and NBR/MLG were stiffer but just as defomable than CIIR and NBR. The strong reinforcing effect of 3 phr MLG was confirmed by the increase of greater than 10 Shore A in hardness. MLG reduces gas permeability, increases thermal and electrical conductivities, and retards flammability, the latter shown by the reduction in heat release rate in the cone calorimeter. We investigated MLG also as a synergist for reducing the aluminium trihydrate loading in flame retardant hydrogenated acrylonitrile-butadiene (HNBR), polybutadiene chloroprene (BR/CR), and chlorosulfonated polyethylene rubber(CSM). The higher the nanofiller concentration is, the greater the improvement in the properties. For instance, the permeability decreased by 30% at 3 phr of MLG, 50% at 5 phr and 60% at 10 phr, respectively. Moreover, the MLG nanocomposites improve stability of mechanical properties against the effects of weathering. In key experiments an increase in UV-absorption and a pronounced radical scavenging were proved as stabilizing mechanisms. In a nutshell, MLG is an efficient multifunctional nanofiller ready to be used for innovative rubber development. T2 - 19th European Polymer Congress, EPF 2022 CY - Prague, Czech Republic DA - 26.06.2022 KW - Graphene KW - Nanocomposite KW - Rubber KW - Elastomer PY - 2022 AN - OPUS4-55196 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Tabaka, Weronika A1 - Schartel, Bernhard T1 - Less is More: Optimised Fire Performance in Glass Fibre-reinforced Polybutylene Terephthalate Laminates with Concentrated Flame Retardant Top Layer N2 - To achieve optimum fire performance while maintaining mechanical integrity, flame retardants (FR) were strategically concentrated in the surface layer of a two-layer glass fibre-reinforced polybutylene terephthalate (PBT) laminate structure. Three potentially synergistic FR systems were selected to improve the fire performance of glass fibre-reinforced PBT: boehmite (AlOOH) with melamine polyzinc phosphate (MPZnP), aluminium diethyl phosphinates (AlPi) with melamine cyanurate (MC), and expandable graphite (EG) with melamine polyphosphate (MPP). Limited Oxygen Index (LOI) and UL-94 testing highlighted the influence of laminate architecture on flammability. The cone calorimeter results showed that increasing the FR concentration in the top layer significantly reduced both the peak heat release rate (PHRR) and the maximum average rate of heat emission (MARHE), with improvements depending on the specific FR system used. The laminate L-PBT/GF/AlOOH/MPZnP with a 2:2 thickness ratio showed outstanding performance, achieving a 45 % reduction in MARHE compared to composites with uniform FR distribution. This result showcases the superior thermal barrier properties and synergistic behaviour of AlOOH and MPZnP. The fire performance of laminates containing AlPi and MC was strongly influenced by the distribution and concentration of AlPi/MC. The EG/MPP system was found to be highly effective, forming a protective intumescent layer that significantly reduced both HRR and MARHE, demonstrating the effectiveness of strategically concentrating FR in the top layer. KW - Glass fibres KW - PBT KW - Flame retardants KW - Composites KW - Laminates KW - Fire behaviour KW - Flammability PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-626381 DO - https://doi.org/10.1016/j.jcomc.2025.100577 SN - 2666-6820 VL - 16 SP - 1 EP - 15 PB - Elsevier CY - Amsterdam AN - OPUS4-62638 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Rappsilber, Tim A1 - Yusfi, Nawar A1 - Krüger, Simone A1 - Hahn, S.-K. A1 - Fellinger, Tim-Patrick A1 - Krug von Nidda, Jonas A1 - Tschirschwitz, Rico T1 - Meta-analysis of heat release and smoke gas emission during thermal runaway of lithium-ion batteries N2 - Herein a meta-analysis of 76 experimental research papers from 2000 to 2021 is given about possible effects on the thermal runaway of lithium-ion battery cells. Data on the hazards of gas emissions and released heat are related to each other and differentiated by cell properties such as, cell geometry, cathode type or state of charge. Quantitative information on the total heat release in the range of 2.0–112.0 kJ Wh−1, the peak heat release rate in the range of 0.006–2.8 kW Wh−1and the smoke gas emission were extracted, normalized in terms of cell energy (Wh), combined in a data library and compared graphically. The total amount of gas emitted (3–48 mmol Wh−1) as well as the released amount of carbon monoxide (1–161 mg Wh−1) and hydrogen fluoride (2–197 mg Wh−1) were investigated as a function of the state of charge and cell geometry. The analysis reveals that the measured values are significantly influenced by the types of calorimeters and smoke gas analyzers used as well as by the type of thermal runaway trigger. This meta-analysis can serve as an important basis for any risk assessment of lithium-ion batteries. KW - Lithium-ion battery KW - Thermal runaway KW - Cathode active material KW - Heat release KW - Smoke gas emission PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-568071 DO - https://doi.org/10.1016/j.est.2022.106579 SN - 2352-152X VL - 60 SP - 1 EP - 15 PB - Elsevier CY - Amsterdam AN - OPUS4-56807 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Tabaka, Weronika T1 - Bench-scale fire stability testing of carbon fibre reinforced polymer laminates with protective layers N2 - Fire resistance testing of components made of carbon fibre reinforced polymers (CFRP) composites usually demands intermediate-scale or full-scale testing. In this study, a bench-scale test is presented as a practicable and efficient method to assess the improvement in structural integrity of CFRP with different protective interlayers during fire. Fire stability is one of the biggest issues of carbon fibre reinforced polymer (CFRP) composites, particularly when they are using in load bearing applications. As soon as the glass transition temperature of polymer matrix (100-200°C) is achieved, the composite loses its structural integrity, what leads to the distortion and failure. The principal fire stability test is based on simultaneous application of fire and mechanical load. Since the carbon fibres can transfer the tensile loads quite well, the compression load is chosen as a required mechanical load for a test. The fire tests were preceded by a static load test at room temperature to determine ultimate failure load. The specimen was loaded with a compression force until the failure load was reached, which was observed as a buckling. For the fire tests, 10% of compression failure load and direct flame of a fully developed fire (heat flux ≈ 180 kW m-2) were applied simultaneously to the specimen, while the time to failure was measured. The possibilities of bench-scale fire stability testing were presented by investigating new types of laminate structures, which exhibit promising flame retardancy and fireproof properties. The new approach of CFRP laminate differs with a protective concept. Every system consists of two different interlayers (titanium foil, thermoplastic foil PEI, ceramic layer WHIPOX, rubber tape Pyrostat, basalt fibres and kenaf fibres), where the one layer constitutes the fireproof protection, that delays the rise of temperature in the rest of laminate, and the second layer provides very good structural connection with carbon fibre layers, thus improves the mechanical integrity of CFRP composite in fire. The time to failure of CFRP composite was 17s. Protective systems significantly enhance the fire stability and increased time to failure by 3 to 10 times. Thicker specimens showed longer resistance time, however CFRP laminate with ceramic layer and titanium foil presented outstanding results and the best performance. The protection with Kenaf and basalt fibres offered a natural fibre solution with also good fire resistance performance Although bench-scale tests are limited with respect to assessing the performance of components and structures, they are valuable in the assessment of different materials concepts. Furthermore, the reduced effort of conducting bench-scale test (lower costs, time, personnel resources) makes it more practical and effective. T2 - 19th European meeting on Fire Retardant Polymeric Materials (FRPM23) CY - Dübendorf, Switzerland DA - 26.06.2023 KW - Fire resistance KW - Carbon fibre reinforced polymer KW - Bench-scale testing PY - 2023 AN - OPUS4-57880 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias A1 - Kömmling, Anja A1 - Böhning, Martin A1 - Silbernagl, Dorothee T1 - Comparison of ageing behavior of O-ring seals under hydrogen and air N2 - Elastomeric seals are essential components in the infrastructure which prevent leakage of gas and ensure proper function of technical devices and are therefore highly safety relevant. For proper function a remaining resilience and tolerance to pressure changes is required. The ageing of elastomers is an undesirable but inevitable process leading to a limited lifetime of rubber products such as seals. Independent of the application, as e.g. automotive, piping or container applications, a long lifetime or at least a timely exchange of a seal before occurrence of critical failure is desired. Hydrogen is a key element for the energy turnaround and therefore the compatibility of seals with hydrogen is essential. In addition to the effect of hydrogen uptake and release, which might also cause destructive effects such as rapid gas decompression, ageing at high temperature under hydrogen atmosphere is of interest too. Most of the existing work is addressing the performance of new materials and comprises only very limited investigations concerning long-term use and the behaviour of aged materials in contact with hydrogen. As ageing can lead to substantial changes of material properties, it must be evaluated whether these changes are beneficial or deteriorating for the component function. In this work we present and compare results of the characterization of three sealing materials (EPDM, HNBR, FKM) after ageing at high temperature under hydrogen and air. Despite the common assumption that ageing under hydrogen atmosphere should be less severe for the material in comparison to air ageing, this is not the case for every material. T2 - ASME PVP2025, Pressure Vessels & Piping Conference CY - Montreal, Quebec, Canada DA - 20.07.2025 KW - Aging KW - Seal KW - Compression set KW - Atomic force microscopy PY - 2025 SP - 1 EP - 7 AN - OPUS4-63889 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Zaghdoudi, M. A1 - Kömmling, Anja A1 - Böhning, Martin A1 - Jaunich, Matthias T1 - Ageing of elastomers in air and in hydrogen environment - A comparative study N2 - EPDM, HNBR and FKM materials were exposed at 150 ◦C to air under atmospheric pressure and to hydrogen at 50 bar for different ageing times. All measurements after hydrogen exposure were conducted on samples in degassed condition to assess irreversible effects resulting from that exposure and to compare them to those after ageing in air. Density, hardness, tensile properties, compression set, and hydrogen permeability of all samples were analysed. In both ageing environments, HNBR exhibited the most significant changes of material properties. However, for both EPDM and HNBR, considerably less severe ageing effects were observed under hydrogen in comparison to ageing in air. On the other hand, FKM showed about the same low level of deterioration in both ageing environments but exhibited poor resistance against damage due to rapid gas decompression in hydrogen environment that can lead to seal failure. The obtained results may serve as a guidance toward a better understanding for design and utilisation of elastomeric materials in future hydrogen infrastructure components. KW - Rapid gas decompression KW - Condensed matter physics KW - Hydrogen KW - Sustainability and the environment KW - Rubber sealing KW - Renewable energy PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-597417 DO - https://doi.org/10.1016/j.ijhydene.2024.03.053 SN - 0360-3199 SN - 1879-3487 VL - 63 SP - 207 EP - 216 PB - Elsevier CY - Oxford AN - OPUS4-59741 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Klippel, Andrea A1 - Hofmann‐Böllinghaus, Anja A1 - Piechnik, Kira A1 - Heydick, Lukas A1 - Wu, Hongyi A1 - Köhler, Florian A1 - Klaffke, Benjamin T1 - Experimental Analysis of Fire Behavior in Pine Forests and Agricultural Fields: Large‐Scale Tests Conducted Within the European TREEADS Project N2 - Two large‐scale experiments investigated fire spread mechanisms in vegetation ground fires in a pine forest and an agricultural field within the European TREEADS project. The tests, conducted in Saxony‐Anhalt and Brandenburg, targeted regions with dry, sandy soils and extensive pine stands and aim to improve suppression strategies and wildfire research. The forest experiment was conducted on a 16 × 22 m plot with line ignition using a gasoline‐diesel mix. Fire spread was documented with drone‐based video and infrared imaging. Ninety‐six thermocouples and two gas sensors were mounted on trees, and a mobile FTIR spectrometer enabled real‐time smoke analysis. A tilled and foam‐treated strip prevented uncontrolled spread. Under stable weather conditions (23°C, light wind, low soil moisture), a consistent temperature rise and distinct combustion phases were observed. Smoldering dominated in areas with mosses, grasses, and deadwood, with intermittent flaming, limited flame heights (< 0.5 m), and substantial smoke production. Peak temperatures exceeded 500°C, and CO concentrations reached 238 ppm, though wind turbulence complicated gas sampling. The second experiment on a cut agricultural field near Nauen involved burning approximately 700 m2 using a 20 m ignition line aligned with wind direction. Drone‐based infrared monitoring captured rapid spread on the stubble surface. The results underscore the variability and measurement challenges of outdoor fires and highlight the necessity of continued large‐scale experiments to support physical and numerical wildfire modeling. These findings provide essential empirical data for evaluating vegetation‐specific burning behavior, improving sensor deployment strategies, and refining validation approaches for next‐generation wildfire spread models under central European fuel and weather conditions, and supporting decision‐making in wildfire management. KW - Wildfire KW - Pine KW - Crop PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-654199 DO - https://doi.org/10.1002/fam.70045 SN - 0308-0501 SP - 1 EP - 11 PB - Wiley AN - OPUS4-65419 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hahn, Sarah‐K. A1 - Gnutzmann, Tanja A1 - Meinert, Marion A1 - Hofmann-Böllinghaus, Anja A1 - Oberhagemann, Dirk A1 - Krause, Ulrich T1 - Incipient Fires—Definition, Detection and Extinguishment by Laypersons N2 - The earlier a fire is noticed, the less developed it is and the easier it can be prevented respectively stopped, even by laypersons. Within the research project ‘TEBRAS’ the incipient phase of fires was investigated in detail. In the course of the project, it became apparent that the definition of what exactly the incipient phase of a fire encompasses is not definite and depends on the disciplines dealing with the subject ‘fire’. Based on the results of a literature review, an inquiry under experts and laypersons as well as practical fire tests a definition for the phenomenon of the incipient fire was developed which divides it into four phases. Driving key factors for each phase are identified considering the main parameters to detect and extinguish the fire. KW - Developing fires KW - Development of fires PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-649310 DO - https://doi.org/10.1002/fam.70025 SN - 0308-0501 VL - 50 IS - 1 SP - 3 EP - 10 PB - Wiley AN - OPUS4-64931 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wagner, Jan A1 - Häfner, P. A1 - Reimann, H.-A. A1 - Schartel, Bernhard T1 - Valorization of Natural Fibers in Flame Retarded Poly(lactic acid) N2 - Extensive research has explored natural fiber reinforced composites, typically focusing on a single fiber within a polymer matrix. Comprehensive comparisons across different natural fibers in the same polymer, which are critical for industrial material selection, remain limited. This work presents a systematic comparison of untreated hemp, flax, and sisal fibers incorporated at varying fiber lengths and loadings into flame retarded poly(lactic acid) (PLA). Fire behavior, thermal, and mechanical responses were investigated through thermogravimetry, UL 94, and cone calorimetry, alongside crystallinity, molecular weight (MW), and microstructural analysis. Fiber incorporation reduced the peak heat release rate (pHRR) by up to 30 % in 30 wt% hemp, attributed to protective layer formation, but increased flammability in UL 94. A phytic acid melamine salt combined with expandable graphite and 20 wt% hemp produced incomplete combustion at 50 kW/m², raising char residue from 4 to 24 wt% and halving pHRR. Petrella plots revealed that fiber addition alone lowered fire load and flashover propensity as effectively as phytic acid melamine; with hemp, phytic acid and expendable graphite, the flashover hazard and fire load were halved. MW was preserved while crystallinity and modulus increased with fiber content. Hemp delivered the most consistent reinforcement, while optimized processing enabled flax and sisal to improve stiffness. Performance gains were strongest when individual fibers were dispersed via optimized processing, preventing bundle fracture under load. Plasma modification of the fibers improved the maximum tensile strength in the composites. A practical guide is provided for valorizing natural fibers in PLA composites, demonstrating routes to bio-based, compostable materials with improved fire safety and mechanical performance suitable for industrial processing. KW - Poly(lactic acid) KW - Hemp KW - Sisal KW - Flax KW - Flame retardant KW - Phytic acid PY - 2026 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-653038 DO - https://doi.org/10.1016/j.mtcomm.2025.114575 SN - 2352-4928 VL - 50 SP - 1 EP - 41 PB - Elsevier Ltd. AN - OPUS4-65303 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Vega Puga, E. A1 - Wachtendorf, Volker A1 - Kömmling, Anja A1 - Brendelberger, S. A1 - Jaunich, Matthias A1 - Sattler, C. T1 - Lifetime prediction and degradation assessment of FKM and FFKM O-rings under high temperature thermo-oxidative ageing N2 - To support the development of solar reactor technologies for hydrogen production, this study investigates the thermo-oxidative degradation mechanisms of fluorinated elastomers and predicts their lifetimes at high temperatures (200–300 ◦C) consistent with the application requirements. An accelerated ageing programme is conducted with FKM and FFKM O-rings and flat samples for up to 21 days. Optical microscopy is used to analyse the exposed seals’ morphological changes, while IR microscopy is utilised to investigate the underlying chemical degradation mechanisms of both elastomers. Findings suggest that FKM’s degradation arises from dehydrofluorination of the polymer, followed by chain scission and backbone cleavage as a result of the oxidation of newly formed C=C double bonds. FFKM’s degradation is primarily associated with chain scission, but there is also indication that post-curing processes may occur during material ageing. Furthermore, hardness, equilibrium compression set (CS), continuous compression stress relaxation (CSR) and leakage rate tests are used to evaluate changes in the mechanical properties and sealing performance of the elastomers. Equilibrium CS data is extrapolated using time-temperature shifts (TTS) and used to derive an end-of-life criterion of 75 % equilibrium CS, which correlates to leakage rates higher than a predetermined threshold. Service lifetime predictions of FKM and FFKM O-rings at several temperatures are performed and a seal operating temperature of 200 ◦C is suggested, which ensures reasonable O-ring replacement intervals of more than half a year in the solar reactor for both considered materials. KW - Fluoroelastomer KW - Perfluoroelastomer KW - Thermo-oxidative ageing KW - Lifetime prediction KW - Compression set PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-630112 DO - https://doi.org/10.1016/j.polymertesting.2025.108820 SN - 1873-2348 VL - 147 SP - 1 EP - 17 PB - Elsevier BV CY - Amsterdam AN - OPUS4-63011 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias T1 - Comparison of Ageing Behavior of O-Ring Seals Under Hydrogen and Air N2 - Elastomeric seals are essential components in the infrastructure which prevent leakage of gas and ensure proper function of technical devices and are therefore highly safety relevant. For proper function a remaining resilience and tolerance to pressure changes is required. The ageing of elastomers is an undesirable but inevitable process leading to a limited lifetime of rubber products such as seals. Independent of the application, as e.g. automotive, piping or container applications, a long lifetime or at least a timely exchange of a seal before occurrence of critical failure is desired. Hydrogen is a key element for the energy turnaround and therefore the compatibility of seals with hydrogen is essential. In addition to the effect of hydrogen uptake and release, which might also cause destructive effects such as rapid gas decompression, ageing at high temperature under hydrogen atmosphere is of interest too. Most of the existing work is addressing the performance of new materials and comprises only very limited investigations concerning long-term use and the behaviour of aged materials in contact with hydrogen. As ageing can lead to substantial changes of material properties, it must be evaluated whether these changes are beneficial or deteriorating for the component function. In this work we present and compare results of the characterization of three sealing materials (EPDM, HNBR, FKM) after ageing at high temperature under hydrogen and air. Despite the common assumption that ageing under hydrogen atmosphere should be less severe for the material in comparison to air ageing, this is not the case for every material. T2 - ASME PVP2025, Pressure Vessels & Piping Conference CY - Montreal, Canada DA - 20.07.2025 KW - Aging KW - Seal KW - Compression set KW - Atomic force microscopy PY - 2025 AN - OPUS4-63888 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Jaunich, Matthias T1 - Elastomerdichtungen für Wasserstoffanwendungen - Vergleich des Alterungsverhaltens in Luft und Wasserstoff N2 - In diesem Beitrag soll ein Fokus auf das Alterungsverhalten von Elastomerdichtungen unter Wasserstoff gelegt werden. Hierfür wurden Untersuchungen bei einem mittleren Wasserstoffdruck über Alterungszeiten von bis zu 100 Tagen durchgeführt. Das Alterungsverhalten wird im Vergleich der Alterungseffekte unter thermooxidativen Bedingungen betrachtet und bewertet. Die Annahme, dass der Alterungseffekt unter Wasserstoff stets weniger ausgeprägt ist als an Luft bestätigt sich nicht durch die Ergebnisse. T2 - 4. O-Ring-Forum der Firma ISGATEC CY - Bad Schönborn, Germany DA - 15.05.2025 KW - Wasserstoff KW - Dichtung KW - Thermische Alterung KW - Elastomer PY - 2025 AN - OPUS4-63135 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Schilling, Markus A1 - Marschall, Niklas A1 - Niebergall, Ute A1 - Wachtendorf, Volker A1 - Böhning, Martin T1 - Unveiling Effects of Biodiesel and Diesel on Environmental Stress Cracking of PE-HD N2 - The behavior of high‐density polyethylene with respect to resistance against environmental stress cracking (ESC) is usually regarded as an inherent material property being specific for respective types of PE‐HD and tested using standardized methods, conditions, and also standard testing liquids (usually aqueous surfactant solutions). On the other hand, for practical applications the ESC behavior of those polymeric materials, commonly used for pipes or containers, in contact with other liquids (e.g., fuels) is often of relevant interest, but for a reasonable assessment, where consistent benchmark data for a direct comparison are often missing, it is essential to determine the actually prevailing failure mode and classify it related to crack propagation or other mechanisms. Using the well‐established Full Notch Creep Test, which favorably allows for a detailed microscopic fracture surface analysis after failure, the behavior of two typical PE‐HD types for container applications is investigated in biodiesel and diesel and compared to a standard surfactant solution. This enables a clear identification of characteristic features of the interaction of biodiesel and diesel as sorptive fuels in contact with the polymer, revealing the complex interplay of sorption and plasticization as well as ESC inducing effects on PE‐HD, which could be clearly shown for both fuels. KW - Biodiesel KW - Confocal laser scanning microscopy (LSM) KW - Diesel KW - Full notch creep test (FNCT) KW - Plasticization PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-650525 DO - https://doi.org/10.1002/pen.70239 SN - 0032-3888 SP - 1 EP - 16 PB - Wiley CY - Hoboken (NJ) AN - OPUS4-65052 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dudziak, Mateusz A1 - Dural, Esra A1 - Dey, R. A1 - Ullrich, M. S. A1 - Huth, Christian A1 - Thomson, C. A1 - Schartel, Bernhard T1 - Together We Can: Synergistic Flame Retardancy by Melamine Polyphosphate and Phosphorylated Microalgae in Polylactide Biocomposites N2 - A strategy for enhancing the sustainable flame retardancy of polylactide (PLA) composites by partially replacing melamine polyphosphate (MPP), a commercial flame retardant proposed for PLA, with wastewater polyphosphate-enriched microalgae (P-Algae) has been explored. The incorporation of P-Algae at a 1:1 ratio with MPP leads to a notable synergistic effect, surpassing the expected additive behavior of the individual components. Comprehensive characterization encompassing thermogravimetric analysis coupled with FTIR, pyrolysis combustion flow calorimeter (PCFC), cone calorimeter, oxygen index (LOI), UL-94 tests, and rheological measurements—demonstrates that the presence of this biomaterial can significantly enhance flame retardant performance. Replacing 50% of MPP with P-Algae in PLA resulted in a 17% reduction in peak heat release rate (pHRR) and maintained a V-0 rating in UL-94 testing. The use of P-Algae does not compromise the flame retardancy of PLA but rather contributes positively, offering a promising path toward more sustainable flame-retardant systems. By leveraging naturally derived biomass, this approach aligns with the growing demand for novel eco-friendly technologies in polymer engineering. Insights into an innovative renewable additive as a functional and effective component in flame-retardant biocomposites have been achieved. KW - Flame retardancy KW - Melamine polyphosphate KW - Phosphorus- enriched microalgae KW - Polylactide PLA KW - Synergism PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-640539 DO - https://doi.org/10.1002/pat.70350 SN - 1099-1581 SN - 1042-7147 VL - 36 IS - 9 SP - e70350 PB - John Wiley & Sons Ltd. AN - OPUS4-64053 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Klippel, A. A1 - Hofmann-Böllinghaus, Anja A1 - Piechnik, K. A1 - Gnutzmann, Tanja T1 - Development of toxicity assessment method for bus interior materials N2 - In recent years, fire safety requirements for bus interior materials have been increased and introduced into international regulations. Fire safety requirements for the burning rate, melting and dripping behaviour of interior materials already exist for many years. However, it remains unclear to what extent the release of smoke, combustion products and their toxicity should be limited. Therefore, a research and development project 82.0723 funded by BASt (Federal Highway Research Institute) was initiated to develop a simplified procedure for testing the toxicity and smoke development in case of fire of interior materials used in buses. The scope of the research included calculations to assess the toxicity of fire gases and the derivation of specifications for the formation of practicable limit values for smoke toxicity. Further investigations are needed to derive these limit values for smoke toxicity in order to be applicable for real fire scenarios in buses. T2 - Conference Fire in Vehicles FIVE CY - Stavanger, Norway DA - 24.04.2023 KW - Bus materials PY - 2023 SP - 80 EP - 90 AN - OPUS4-57627 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Manes, M. A1 - El Houssami, M. A1 - Campbell, R. A1 - Sauca, A. A1 - Rush, D. A1 - Hofmann-Böllinghaus, Anja A1 - Andersson, P. A1 - Wagner, P. A1 - Veeneklaas, J. A1 - van Hees, P. A1 - Guillaume, E. T1 - Closing Data Gaps and Paving the Way for Pan-European Fire Safety Efforts: Part I—Overview of Current Practices for Fire Statistics N2 - The analysis of the current state of fire statistics and data collection in Europe and other countries is needed to increase awareness of how fire incidents affect buildings and to support pan-European fire prevention and fire mitigation measures. The terminology and data collected regarding fire incidents in buildings in the EU Member States were mapped to obtain meaningful datasets to determine common terminology, collection methodology, and data interpretation system. An extensive literature review showed that fire data collection systems have been instrumental in informing firefighting strategies, evidence-based planning, prevention, and educational programmes. Differences and similarities between fire data collection systems were also investigated. The amount and quality of the information in fire statistical recording systems appear to be influenced by the complexity and structure with which the data are collected. The analysis also examined the existing fire statistics in the EU Member States and a few other countries. Finally, a detailed investigation of the number of fires, fire deaths, and injuries from 2009 to 2018 in several countries was examined based on data from a report by CTIF. The trends showed differences attributable to the existing fire statistical practices in terms of terminology and data collection, and interpretation. Part II proposes a common terminology for selected fire statistical variables. The results provide relevant information regarding fire safety at the European level and should be used to guide the development of more uniform fire statistics across Europe. KW - Fire statistics KW - European project PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-575711 DO - https://doi.org/10.1007/s10694-023-01415-6 SN - 1572-8099 SP - 1 EP - 44 PB - Springer CY - Heidelberg AN - OPUS4-57571 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - El Houssami, M. A1 - Försth, M. A1 - Fredriksson, H. A1 - Drean, V. A1 - Guillaume, E. A1 - Hofmann-Böllinghaus, Anja A1 - Sandinge, A. T1 - Fire safety of interior materials of buses N2 - This study provides an analysis on the fire safety of passengers and the fire protection of coaches and buses. A brief review of major bus fire incidents, an overview of current regulations in Europe, and their limitations are presented. The study finds that the current small-scale fire test methods described in UN ECE Reg No. 118 need to be replaced by test methods that can assess the reaction to fire of materials when exposed to ignition sources of varying sizes. To address these shortcomings, the study proposed an expert recommendation to update the material fire safety requirements and testing for buses. Additional measures are proposed, derived from objectives and strategies applied in other transport sectors, and can be tested through existing European and international standards, which are widely used by several industries. These measures aim to extend the time with tenable conditions for a safe evacuation in case of fire, reduce the degree of damage to buses, reduce the risk for fast and excessive thermal exposure on modern energy carriers needed for a more sustainable transport sector. KW - Fire KW - Bus interior materials KW - Rregulations PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-575700 DO - https://doi.org/10.1002/fam.3134 SN - 1099-1018 SP - 1 EP - 15 PB - Wiley CY - London AN - OPUS4-57570 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Piechnik, Kira A1 - Heydick, Lukas A1 - Hofmann-Böllinghaus, Anja A1 - Klippel, Andrea T1 - Comprehensive laboratory study on smoke gases during the thermal oxidative decomposition of forest and vegetation fuels N2 - AbstractThis study investigates the composition of smoke gases in forest and vegetation samples to draw conclusions about the actual smoke gas composition during wildfires. The focus is particularly on regions with extensive pine forests, like in Eastern Germany. The relevance of smoke gases is well illustrated by the example of wildfires in Québec, influencing air quality in New York, in 2023. By employing a modified DIN tube furnace, a bench‐scale test set‐up, the research emphasizes the examination of smoke composition from tree species and ground cover, prioritizing gases while disregarding particles. Key smoke gases are identified as CO, CO2, SO2, HCN, C3H4O (acrolein) and CH2O (formaldehyde) and their concentrations are compared with Acute Exposure Guideline Levels (AEGL) limits. Acknowledging the limitations of AEGL usage and the problem with direct quantitative comparison of toxicant concentrations (cf. ISO 29903‐1:2020), the study highlights variations in smoke composition across different samples. The results of the studies reveal a significant disparity in CO concentration between dry and fresh pine needles. Frequently, the AEGLs of key gases are exceeded significantly. The elemental analysis of the barks indicates distinct differences in composition, reflecting in the concentrations of smoke gases. The ratio of 1 mole of substance turnover to the identified key components will be used to determine input parameters for the subsequent numerical simulation. KW - Forest KW - Wildfire KW - Ignition PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-617744 DO - https://doi.org/10.1002/fam.3253 SP - 1 EP - 12 PB - Wiley online library AN - OPUS4-61774 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wu, Hongyi A1 - Buhk, Frederik A1 - Christiani, Ricardo A1 - Hofmann-Böllinghaus, Anja T1 - Influence of local vegetation on ignition and fire spread of vegetation fires-Experimental and numerical approach N2 - Within the framework of the European TREEADS project, Brandenburg and Saxony-Anhalt were designated as model regions. This designation facilitated the investigation of vegetation types, soil structure, and soil dryness. Brandenburg and Saxony-Anhalt are identified as the driest regions in Germany according to the annual mean soil moisture data. In these regions, 48% to 73% of the forests are composed of pine species. The soil profile is characterized by a relatively thin organic layer, measuring between 0.2 and 0.3 meters, underlain by sandy substrates. Consequently, surface and ground fires are more prevalent in these areas compared to other types of fires, such as crown fires. To investigate the influence of local vegetation, it goes through two aspects. One is laboratory study, the local vegetation samples were collected and tested for the thermal properties, such as activation energy, heat content and reaction kinetic of pyrolysis and dehydration. At the same time, small and medium scale combustion experiments were conducted to investigate the burning behavior. The other aspect is using the thermal properties as the input parameters for the development of numerical simulation in the computational fluid dynamics (CFD) tool. These models were then be validated with the combustion experiments, as a baseline for the further scaling up of the models, in order to investigate how the parameters influencing the fire spread in a large-scale case numerically. T2 - Interflam 2025, 16th International Fire Science and Engineering Conference CY - London, United Kingdom DA - 30.06.2025 KW - Wildfire PY - 2025 SP - 2221 EP - 2225 PB - Interscience CY - London AN - OPUS4-63932 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Müller, Simon T1 - FireSpread_MedEU N2 - Wildfires are becoming more frequent and severe under the influence of climate change, posing increasing risks to ecosystems, human health, and infrastructure. Accurate spatiotemporal data on wildfire propagation is essential for advancing fire behavior modeling, improving management strategies, and mitigating future impacts. However, existing datasets with both high spatial and temporal resolution are rare, costly, and time-consuming to produce. To address this gap, we present FireSpread_MedEU, a dataset comprising 313 consecutive burned area maps from 102 wildfire events across the Mediterranean and Europe between 2017 and 2023. Burned areas were derived from high-resolution Planet optical satellite imagery (~3 m spatial, mostly daily temporal resolution) using a semi-automated workflow, followed by manual refinement to ensure highest accuracy. Each dataset entry is enriched with detailed metadata and a subjective quality assessment. With its high level of spatiotemporal precision, FireSpread_MedEU provides essential data for the development and validation of machine learning models or wildfire simulation models. It opens new research opportunities in wildfire behavior analysis, risk assessment, and predictive modeling. KW - Wildfire KW - Spread KW - Machine Learning PY - 2025 DO - https://doi.org/10.5281/zenodo.16813435 PB - Zenodo CY - Geneva AN - OPUS4-64768 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Festag, Sebastian A1 - Esser, Jonas A1 - Maiworm, Björn A1 - Hofmann-Böllinghaus, Anja T1 - Herausforderungen des modernen Holzbaus: Erste statistische Erkenntnisse aus realen Gebäudebränden in Holzbauweise N2 - Hinsichtlich des Brandschutzes zeigt der durch die Bundesregierung geförderte Holzbau Herausforderungen gegenüber Massivbauweisen. Diese spiegeln sich in Erfahrungen von Feuerwehren wider, aber nun auch in statistischen Untersuchungen der Brandschadenstatistik der Vereinigung zur Förderung des deutschen Brandschutzes sowie der Arbeitsgemeinschaft der Leiterinnen und Leiter der Berufsfeuerwehren (AGBF) und des Deutschen Feuerwehrverbands (DFV). Im Zeitraum von 2013 bis 2017 wurden in der vfdb-Brandschadenstatistik Daten zu 5016 Alarmierungen bei Gebäudebränden in Deutschland systematisch mit einem einheitlichen Erfassungsbogen erfasst und seit 2016 „bemerkenswerte Brandeinsätze“ durch einen Evaluierungsbogen zu Maßnahmen des vorbeugenden Brand- und Gefahrenschutzes von AGBF/DFV. Grundlage des vorliegenden Beitrags sind die Auswertung und der Vergleich beider statistischer Datensätze hinsichtlich der Brände in Gebäuden in Holzbauweise. Es zeigt sich, dass der Holzbau mit brandschutztechnischen Herausforderungen verbunden ist. KW - Brandschutz KW - Brandstatistik PY - 2025 DO - https://doi.org/10.1002/bate.202400078 SN - 1437-0999 VL - 2025 IS - 102 SP - 1 EP - 8 PB - Wiley AN - OPUS4-63000 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Klippel, A. A1 - Hofmann-Böllinghaus, Anja A1 - Gnutzmann, Tanja A1 - Piechnik, K. T1 - Reaction-to-fire testing of bus interior materials: Assessing burning behaviour and smoke gas toxicity N2 - Although fire safety regulations for buses have been adapted in recent years regarding, for example, fire detection and engine fire suppression systems, the changes in regulations for bus interior materials are minimal. A comparison of fire safety regulations for interior materials in other transport sectors for trains, ships or aircraft reveals a much lower level of requirements for bus materials. Although repeated bus accidents as well as fire statistics show the danger a bus fire can pose to passengers. In particular, the combination of a fire incident and passengers with reduced mobility led to severe disasters in Germany and other European countries. To enhance the fire safety for passengers, the interior bus materials are crucial as the fire development in the bus cabin determines whether escape and rescue is possible. Against this background, bus interior materials were tested in different fire test scenarios. Measurement of a wide variety of parameters, for example, the mass loss, ignition time, smoke gas composition, heat release rate among others were carried out. Tested materials complied to the newest set of requirements. For this purpose, interior materials and their components had to be identified according to their chemical structure. Parts of the tests were funded by BASt (Federal Highway Research Institute) in the project 82.0723/2018. Experimental results show reaction-to-fire behaviour which lead to very limited times for escape and rescue in case of fire in a bus cabin. Based on the studies on fire behaviour and toxicity assessment, recommendations for improved fire safety regulations for interior materials could be made. KW - Burning behaviour KW - Bus interior materials KW - Cone calorimeter KW - DIN tube furnace KW - FTIR spectroscopy KW - Reference values KW - Smoke toxicity PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-576085 DO - https://doi.org/10.1002/fam.3108 SN - 1099-1018 VL - 47 IS - 5 SP - 665 EP - 680 PB - Wiley CY - New York, NY AN - OPUS4-57608 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Anderson, Johan A1 - Chiva, Roman A1 - Dumont, Fabien A1 - Lalu, Octavian A1 - Hofmann-Böllinghaus, Anja T1 - Assessment of fire performance of facades in a round robin using the European approach N2 - In recent years, an experimental round robin of full-scale façade tests was conducted using the proposed new European approach for assessing the fire performance of façades. The initial results were used to develop a calibration scheme and to propose assessment criteria aligned with appropriate safety levels. During the project, a need emerged to evaluate the stability of the fire source and the Consistency of heat exposure. This paper addresses these concerns by comparing the mass loss rates across a series of tests and analysing averaged temperature readings at various locations on the façade. The findings indicate that the method demonstrates high stability in terms of mass loss rates and provides consistent and appropriate heat exposure. T2 - Interflam 2025, 16th International Fire Science and Engineering Conference CY - London, UK DA - 30.06.2025 KW - Facade systems KW - Testing PY - 2025 VL - 2025 SP - 562 EP - 572 PB - Interscience CY - London AN - OPUS4-63998 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Anderson, J. A1 - Boström, L. A1 - Chiva, R. A1 - Guillaume, E. A1 - Colwell, S. A1 - Hofmann-Böllinghaus, Anja A1 - Toth, P. T1 - European approach to assess the fire performance of façades N2 - Several attempts have been made in the past to develop a European harmonized testing and assessment method for façades before the European commission decided to publish a call for tender on the topic. A project consortium from five countries (Sweden, UK, France, Germany and Hungary) applied to the call for tender and was contracted to develop a European approach to assess the fire performance of façades. 24 sub-contractors and 14 stakeholder entities were part of the project. The objective of the European project was to address a request from the Standing Committee of Construction (SCC) to provide EC Member States regulators with a means to regulate the fire performance of façade systems based on a European Approach agreed by SCC. The initial stages of this Project were focused on establishing a Register of the regulatory requirements in all Member States in relation to the fire Performance of façade systems, and to identify those Member States who have regulatory requirements for the fire performance façade systems which go beyond the current EN 13501 (reaction to fire and fire resistance) classification systems and to collate the details of these additional requirements. After having confirmed the regulatory needs a testing and classification methodology based on BS 8414 and DIN 4102-20 was developed to address the identified key performance and classification characteristics. This paper is a short overview of results the two-year development work, which Final Report published by the European Commission in 2018. KW - Facade KW - Regulation KW - Testing PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-530501 DO - https://doi.org/10.1002/fam.2878 SN - 1099-1018 VL - 45(5) IS - Special issue: Facade fire safety SP - 598 EP - 608 PB - Wiley CY - Oxford AN - OPUS4-53050 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Hofmann-Böllinghaus, Anja A1 - Klippel, Andrea T1 - Vehicle Fires: Significant Fire Hazard in Transportation Infrastructure N2 - Vehicle fires in transportation infrastructure such as depots, car parks, tunnels and stations are a recurring phenomenon, with recent years witnessing an alarming number of severe incidents, particularly in vehicle depots. These fires often result in the total loss of both vehicles and buildings, with striking similarities in their progression. Analysis of recent fire events, including a study conducted for the German insurer Provinzial, shows that fires in bus depots, military facilities and car parks tend to spread rapidly and destructively. While building regulations vary across sectors and countries, the fire safety standards for interior materials in road vehicles remain globally harmonized and are based on outdated regulations such as FMVSS 302, which offer only a minimal level of protection. In contrast, materials used in trains, ships, and aircrafts must comply with significantly stricter fire safety standards, which may explain the relatively lower incidence of fires in these sectors. Common fire protection systems in depots, such as sprinklers and vents, often fail to account for the specific characteristics of automotive vehicles, including their watertight design and the rapid development of hot gas layers that accelerate fire spread. Insurance companies have begun to acknowledge these challenges. Given the high flammability, heat release and smoke toxicity of materials commonly used in vehicles, combined with the growing share of combustible plastics over the past decades, this paper argues for a paradigm shift. Instead of relying solely on inhancing building protection, introducing significantly stricter fire safety requirements for vehicle materials could offer a more effective and sustainable approach to safeguarding transportation infrastructure. Ongoing experimental investigations are being conducted to evaluate the reaction to fire behavior of various bus interior materials. These studies focus on the emission of toxic gases during combustion, with particular attention to substances exceeding critical AEGL thresholds. Materials such as polyurethane foams and hard plastics have shown significant variation in their smoke gas profiles, highlighting potential health and safety risks in fire scenarios. The research aims to support the development of safer material choices and regulatory measures. Upon completion of tests with additional materials, all findings will be published to ensure transparent and comprehensive reporting. T2 - Interflam 2025, 16th International Fire Science and Engineering Conference CY - London, United Kingdom DA - 30.06.2025 KW - Vehicle fires KW - Transportation PY - 2025 AN - OPUS4-63922 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Geoerg, Paul A1 - Schumann, Jette A1 - Holl, Stefan A1 - Holl, Maik A1 - Hofmann-Böllinghaus, Anja T1 - The influence of individual impairments in crowd dynamics N2 - The importance of empirical relations to quantify the movement of pedestrians through a facility has increased during the last decades since performance-based design methods became more common. Bottlenecks are of special interest because of their importance for egress routes and as they result in a reduced capacity. The empirical relations as the density-dependent movement speed or flow rate were derived by studies under laboratory conditions, which were usually conducted with populations of homogeneous characteristics forbetter control of influencing variables. If individual characteristics of a crowd become more heterogeneous, individuals were forced to adapt their individual movement and control individual manoeuvring. These unintended interactions lead to a different shape of the fundamental empirical relations. Here, we present results from a movement study under well-controlled boundary conditions in which participants with and without different characteristics of disabilities participated. To consider the effect of different heterogeneities on the capacity of a facility, fundamental diagrams are generated using the Voronoi method. If participants with visible disabilities (such as using assistive devices) are part of a crowd, significant differences relating to the shape of the empirical Relations and the capacities are found. This indicates that the heterogeneity of a Population leads to an increased interpersonal interaction which results in influenced movement characteristics. KW - Engineering egress data KW - Heterogeneity KW - Human behaviour KW - Movement characteristics KW - Pedestrian dynamics PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-508943 DO - https://doi.org/10.1002/fam.2789 SN - 0308-0501 VL - 45 IS - 4 SP - 529 EP - 542 PB - Wiley Online Libary CY - New Jersey, USA AN - OPUS4-50894 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Piechnik, Kira A1 - Hofmann-Böllinghaus, Anja A1 - Klippel, Andrea T1 - Self‐ignition of forest soil samples demonstrated through hot storage tests N2 - AbstractThe increasing threat of forest fires on a global scale is not only a matter of concern due to the potential harm they may cause to both human and animal life but also due to their significant role in exacerbating climate change. In light of these circumstances, one might inquire as to whether forest soil can self‐ignite and, if so, under what conditions and at what temperatures this phenomenon may occur. This question is being addressed in the German pilot “Fire science of wildfires and safety measures” of the EU project TREEADS, and the first results are presented below. The importance of basic research into the self‐ignition of forest soil cannot be underestimated, as it provides crucial knowledge to prevent forest fires and protect human and animal health. Furthermore, mitigating the occurrence of forest fires can also play a role in reducing greenhouse gas emissions, contributing to global efforts to combat climate change. The procedure of the hot storage test is an effective means of determining whether a material can self‐ignite. During the investigation of six soil samples, it was found that five of them were indeed capable of self‐ignition. In addition to determining whether the material ignites, the modified hot storage test also analyzed the resulting smoke gases and measured their concentration. The research question of whether regional forest soil is capable of self‐ignition can be answered with yes based on these initial tests. Further experiments are needed to determine if self‐ignition causes forest fires. KW - FTIR KW - Hot storage KW - Ignition KW - Soil KW - Wildfire PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-594617 DO - https://doi.org/10.1002/fam.3198 SN - 1099-1018 VL - 48 IS - 4 SP - 495 EP - 507 PB - Wiley CY - New York, NY AN - OPUS4-59461 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Nandish, Ranjith A1 - Knaust, Christian A1 - Hofmann-Böllinghaus, Anja A1 - Gnutzmann, Tanja A1 - Zehfuß, Jochen T1 - Simulation of wood pyrolysis with component-based mechanism N2 - This paper presents a comprehensive fire simulation study that models the pyrolysis process of beech wood using kinetic parameters with the Fire Dynamics Simulator (FDS). The kinetic methodology is based on the application of these kinetic parameters to govern the underlying pyrolysis reactions. The primary objective was to numerically model the pyrolysis process for beech wood using both single-component (single-step, single reaction scheme) and multi-component (single-step, multi-reaction scheme) kinetic reaction schemes. The accuracy of the numerical model was validated by comparing FDS simulation results with experimental data obtained from thermogravimetric analysis (TGA) and cone calorimeter tests. This approach aids in identifying reliable kinetic reaction input parameters for modelling wood fires. A case study was included to demonstrate the implementation of the kinetic reaction schemes. Numerical results from the TGA simulations for the small-scale pure cellulose test using the single-component approach exhibit consistency with the experimental data. Furthermore, the results demonstrated that the multi-component approach more accurately replicates the shape of the experimental curve for beech wood compared to the single-component approach. However, discrepancies in the tail regions of the curves obtained from the FDS simulations showed the need for further improvement in the modelling approach, particularly regarding the exclusion of char oxidation reactions, which needs to be investigated further. KW - Simulation KW - Wood PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-639272 DO - https://doi.org/10.1007/s00231-025-03571-7 SN - 0947-7411 VL - 61 IS - 6 SP - 1 EP - 14 PB - Springer Science and Business Media LLC AN - OPUS4-63927 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Hofmann-Böllinghaus, Anja A1 - Klippel, Andrea A1 - Gnutzmann, Tanja A1 - Kaudelka, Sven A1 - Rabe, Frederik T1 - Influence of modern plastic furniture on the fire development in fires in homes: large-scale fire tests in living rooms N2 - About 80% of all fire fatalities in Germany occur because of fires in homes. It has been known for some time that modern materials (synonym for materials consisting mostly of synthetic polymers) tend to burn differently from older materials (synonym for materials consisting mostly of fibrous cellulosic substances) and it has been acknowledged that the amount of combustible plastics in homes has increased significantly over the last decades. To investigate the influence of modern furniture and ventilation conditions of fires in homes, a series of four large-scale tests in two Living rooms (LRs) with adjacent rooms (ARs) was performed by BAM and the Frankfurt fire service. Two LRs, one with older furniture and one with modern furniture, were tested twice each. Each test started with the ignition of a paper cushion on an upholstered chair. The influence of modern materials on the fire development was investigated, as well as the influence of the ventilation on the fire development. In all settings, an upholstered chair was the first burning item. Results of the test series show that fires in rooms with modern furniture develop faster than fires in rooms with older furniture. This is true for temperature development in the rooms as well as for smoke production. KW - Room fire KW - Furniture KW - Modern KW - Gas analysis KW - Smoke PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-527568 DO - https://doi.org/10.1002/fam.2934 VL - 45 IS - 1 SP - 155 EP - 166 PB - Wiley CY - London AN - OPUS4-52756 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Manes, M. A1 - Sauca, A. A1 - El Houssami, M. A1 - Andersson, P. A1 - McIntyre, C. A1 - Campbell, R. A1 - Rush, D. A1 - Hofmann-Böllinghaus, Anja A1 - Wagner, P. A1 - Leene, M. A1 - Oberhagemann, D. A1 - Jomaas, G. A1 - Grone, F. A1 - Guillaume, E. T1 - Closing Data Gaps and Paving the Way for Pan-European Fire Safety Efforts: Part II—Terminology of Fire Statistical Variables N2 - A well-defined terminology of fire-related variables is important for correct analyses and supporting knowledge-based decisions regarding the evaluation of building fires at the European level. After developing an overview of current practices for fire statistics in Part I, the terminology used and the data collected by the EU Member States and eight other countries regarding fire incidents, property damage and human losses were mapped to increase awareness of their practice and support a comprehensive assessment of several fire statistical datasets. A questionnaire was distributed to relevant authorities responsible for the collection, elaboration/analysis, and fire statistical data publications to define and select the essential variables for an appropriate fire assessment and fire incident description. Based on the results of the questionnaire able to identify the essential fire statistical variables and a detailed analysis of current definitions adopted in the fire statistics of the EU Member States and other countries, a common terminology is proposed to collect the necessary data in the EU Member States and obtain meaningful datasets based on standardised terms and definitions. The results will generate essential outputs to move towards harmonised fire statistics at the EU level and contribute to an appropriate analysis able to improve fire prevention and fire mitigation in building fires. KW - Fire statistics PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-575725 DO - https://doi.org/10.1007/s10694-023-01408-5 SN - 1572-8099 SP - 1 EP - 32 PB - Springer CY - Heidelberg AN - OPUS4-57572 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CHAP A1 - Hofmann-Böllinghaus, Anja ED - Vogdt, F. U. T1 - Brandschutz N2 - Grundlagen des vorbeugenden baulichen Brandschutzes KW - Brandprüfungen KW - Bauvorschriften PY - 2022 SN - 978-3-8348-2189-8 SP - 199 EP - 220 PB - Springer ET - 1 AN - OPUS4-54317 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR ED - Hofmann-Böllinghaus, Anja ED - Anderson, J. T1 - Special issue: Facade fire safety N2 - Façade fires are of growing concern worldwide. Severe facade fires in different parts of the world as well as activities in many countries regarding the testing of facades show the urgency of the fire safety challenges in façade fires. The need for knowledge and a wide Archive of work in this area has become evident after recent incidents which involved extensive facade fires. These include the tragic fires in Dubai and Grenfell Tower in 2017 in the United Kingdom. In many cases, the widespread live news coverage of the events and size of These fires has emphasized the need for progress in the understanding of the processes involved in these fires and put pressure upon the fire safety engineering community to find effective solutions. KW - Testing KW - Safety PY - 2021 UR - https://onlinelibrary.wiley.com/toc/10991018/2021/45/5 SN - 0308–0501 SN - 1099-1018 VL - 45 IS - 5 SP - 583 EP - 696 PB - Wiley CY - Oxford AN - OPUS4-53102 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Dudziak, Mateusz A1 - Riechers, Birte A1 - Maaß, Robert A1 - Michalchuk, Adam A1 - Schönhals, Andreas A1 - Szymoniak, Paulina T1 - Beyond conventional calorimetry: Unlocking thermal characterization with fast scanning techniques N2 - Fast scanning calorimetry (FSC) has emerged as a transformative technique in thermal analysis, enabling the investigation of rapid and kinetically driven thermal transitions that are inaccessible to conventional differential scanning calorimetry. This review highlights the capabilities enabled by FSC for studying a wide range of materials under extreme thermal conditions, including polymers, pharmaceuticals, metallic glasses, nanocomposites, and hydrogels. By employing ultrafast heating and cooling rates, FSC allows for the suppression of crystallization, resolution of weak transitions, and analysis of thermally labile or size-limited samples. The technique is particularly valuable for probing glass transitions, relaxation phenomena, and phase behavior in systems with complex morphologies or confined geometries. Case studies demonstrate the use of FSC in characterizing vitrification, physical aging, and interfacial dynamics, as well as its application in emerging fields such as additive manufacturing, supramolecular systems, and neuromorphic materials. Together, these examples underscore the role that FSC plays in advancing the understanding of structure-property relationships across diverse material classes. KW - Flash DSC KW - Calorimetry KW - Glass transition PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-647405 DO - https://doi.org/10.1016/j.tca.2025.180177 VL - 754 SP - 1 EP - 14 PB - Elsevier B.V. AN - OPUS4-64740 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Ciornii, Dmitri A1 - Hodoroaba, Vasile-Dan A1 - Wachtendorf, Volker A1 - Fengler, Petra A1 - Altmann, Korinna T1 - Interlaboratory Comparison Reveals State of the Art in Microplastic Detection and Quantification Methods N2 - In this study, we investigate the current accuracy of widely used microplastic (MP) detection methods through an interlaboratory comparison (ILC) involving ISO-approved techniques. The ILC was organized under the prestandardization platform of VAMAS (Versailles Project on Advanced Materials and Standards) and gathered a large number (84) of analytical laboratories across the globe. The aim of this ILC was (i) to test and to compare two thermo-analytical and three spectroscopical methods with respect to their suitability to identify and quantify microplastics in a water-soluble matrix and (ii) to test the suitability of the microplastic test materials to be used in ILCs. Two reference materials (RMs), polyethylene terephthalate (PET) and polyethylene (PE) as powders with rough size ranges between 10 and 200 μm, were used to press tablets for the ILC. The following parameters had to be assessed: polymer identity, mass fraction, particle number concentration, and particle size distribution. The reproducibility, SR, in thermo-analytical experiments ranged from 62%−117% (for PE) and 45.9%−62% (for PET). In spectroscopical experiments, the SR varied between 121% and 129% (for PE) and 64% and 70% (for PET). Tablet dissolution turned out to be a very challenging step and should be optimized. Based on the knowledge gained, development of guidance for improved tablet filtration is in progress. Further, in this study, we discuss the main sources of uncertainties that need to be considered and minimized for preparation of standardized protocols for future measurements with higher accuracy. KW - Microplastics KW - Interlaboratory comparison KW - PlasticsFatE KW - PET KW - PE KW - Reference materials KW - VAMAS KW - Thermo-analytical methods KW - Spectroscopical methods PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-630462 DO - https://doi.org/10.1021/acs.analchem.4c05403 SN - 1520-6882 VL - 97 SP - 8719 EP - 8728 PB - ACS Publications AN - OPUS4-63046 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Altmann, Korinna A1 - Wimmer, Lukas A1 - Alcolea-Rodriguez, Victor A1 - Waniek, Tassilo A1 - Wachtendorf, Volker A1 - Matzdorf, Kay A1 - Ciornii, Dmitri A1 - Fengler, Petra A1 - Milczewski, Frank A1 - Otazo-Aseguinolaza, Itziar A1 - Ferrer, Manuel A1 - Bañares, Miguel A. A1 - Portela, Raquel A1 - Dailey, Lea Ann T1 - Quality-by-design and current good practices for the production of test and reference materials for micro- and nano-plastic research N2 - Understanding the environmental and human health impacts of micro- and nanoplastic pollutants is currently a high priority, stimulating intensive methodological research work in the areas of sampling, sample preparation and detection as well as intensive monitoring and testing. It is challenging to identify and quantify microplastics in complex organic matrices and concepts for nanoplastic detection are still in their infancy. All analytical techniques employed in studying micro- and nanoplastics require suitable reference materials for validation measurements, with requirements as diverse as the analytical tools used, ranging from different polymer types, size distributions and shapes of the material to the concentrations employed in different experimental set ups (ng to g amounts). The aim of this manuscript is to outline current good practices for small-scale laboratory production and characterization of suitable test and reference materials. The focus is placed on top-downfragmentation methods as well as bottom-up precipitation methods. Examples using polyethylene, polypropylene, polystyrene and polyethylene terephthalate with size distribution classes of mainly 10–1000, 1–10 and <1 μm particles will be provided. Experiences and suggestions on how to produce well-characterized micro- and nano-plastics for internal research needs will ensure that studies using the materials have robust and informative outcomes. KW - Mmicroplastics KW - Nanoplastics KW - Reference materials KW - Standard validation method PY - 2025 DO - https://doi.org/10.1016/j.jhazmat.2025.139595 SN - 0304-3894 VL - 497 SP - 1 EP - 20 PB - Elsevier B.V. AN - OPUS4-63958 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Geburtig, Anja A1 - Wachtendorf, Volker A1 - Trubiroha, P. T1 - Simulationsdaten zur photooxidativen Beanspruchung an verschiedenen geografischen Freibewitterungs-Standorten N2 - Freibewitterungen weisen grundsätzlich eine hohe Variabilität der jeweiligen Intensität der Beanspruchungsparameter auf; sie sind nicht einfach wiederholbar. Um dennoch die Ergebnisse einer Beanspruchung vergleichen zu können, ist eine aussagekräftige Charakterisierung der Freibewitterung wichtig. Traditionell werden Daten bekannter Einflussgrößen wie Globalstrahlung, Temperatur oder Feuchtewerte herangezogen. Obwohl man weiß, dass diese Größen an den exponierten Oberflächen wechselwirken und kombiniert als Mikroklima Einfluss auf Degradationsprozesse nehmen, werden schon aus Praktikabilitätsgründen diese separat als klimatische Messgrößen angegeben. Die Aussagekraft dieser Daten ist mäßig. Ziel dieses Beitrags ist es, die Aussagekraft und damit Vergleichbarkeit zu erhöhen, indem diese Messdaten als Stundendaten zu Wirkintegralen vorverarbeitet und jahresweise akkumuliert werden. Betrachtet wird dafür der Prozess der Photooxidation, da dieser Alterungs-mechanismus bei allen Kunststoffen auftritt. Für eine einfache Modellierung wird die wirksame UV-Bestrahlung, gewichtet mit einer Arrhenius-abhängigen Ober¬flächen-temperatur (TOF), über den Beanspruchungszeitraum von hier je einem Jahr akkumuliert. Die Idee einer solchen Messgröße für photooxidative Ober¬flächen¬alterung wurde bereits vorgestellt [1]. Dort wurde ein Gerät vor¬geschlagen, mit dem dieser Wert für verschieden absorbierende Oberflächen für die Dauer einer Exposition akkumuliert wird, und ergänzend eine Abschätzung der Betauungs¬zeiten dieser Referenz-Oberflächen erfolgen könnte. Hier soll es um eine rechnerisch generierte Zusammenstellung dieser photo¬oxidativen 1-Jahres-Alterungswerte für verschiedene Standorte gehen. Ein Temperaturfaktor erfasst dabei den Einfluss der Strahlungserwärmung auf eine weiße, graue bzw. schwarze Referenzoberflächen, spiegelt also die Kopplung von solarer Strahlung und Temperatur wider [1]. Ermittelt wird er aus Stunden¬daten der Globalstrahlung und der Lufttemperatur. Die spektrale Wirkung wird aus Sonnenhöhenständen entsprechend der geografischen Breite mit Hilfe der FastRT-Oberfläche [2] als PiT·h-Wert abgeschätzt [3]. Anhand der errechneten Jahreswerte können die Schweregrade der photo¬oxidativen Beanspruchung an den verschiedenen Standorten unmittelbar verglichen werden. Die gezeigten Simulationsdaten für ein solches „elektronisches Referenzmaterial“ für photooxidative Degradation zeigen die prinzipielle Möglichkeit einer Kartografierung solcher Daten auf. T2 - 53. Jahrestagung der GUS CY - Stutensee-Blankenloch, Germany DA - 26.03.2025 KW - Polymer 3R, UV, Bestrahlung, Bewitterung PY - 2025 SN - 978-3-9826129-2-8 VL - 53 SP - 19 EP - 28 PB - Gesellschaft für Umweltsimulation e.V. CY - 76327 Pfinztal (Berghausen) AN - OPUS4-62902 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Geburtig, Anja A1 - Trubiroha, Peter A1 - Wachtendorf, Volker T1 - Significance of new data pairs for irradiance and (surface) temperature N2 - There is consent that UV irradiance and temperature at the place of photodegradation are the most important environmental parameters in weathering, along with humidity. This contribution shows how an improvement in the measurement data situation can improve the significance and comparability of outdoor exposures. Photooxidative ageing is calculated using sample polymers for which the corresponding modelling data (Exposure Response Functions, ERF) is available. The mean square deviations are estimated, which result from using different spectral irradiances and different spectral sensitivities, both of the sensors and the polymers. It will be shown here how the significance of the irradiance values increases with increasing approximation of the spectral sensitivities of the sensor and polymer. Also, the mean square deviations are estimated, which result from using different activation energies and surface temperatures. A selection of different variables to describe the weathering exposure is created. The potential of either individual values or data pairs is evaluated in terms of significance or correlation to the calculated photooxidative ageing. Recording hourly data also enables subsequent evaluations of individual test specimens, adapted to the respective colour or to determine activation energies. An accumulated value, calculated from PIT-radiometer irradiance and a suited surface temperature, can provide a comparison of different outdoor exposures over different locations or years. Thus, a characterisation of the weathering exposure would be related to a reference spectral sensitivity (much closer to a polymer than that of a common UV radiometer), one reference activation energy, and different surface temperature scenarios with, on the one hand, graded solar absorptions (white / grey / black) and, on the other hand, different thermal couplings (coated metal / thick plastic). This results in three values each for plastic samples and coated metals (light / grey / dark). It will never be possible to accurately predict the weathering tests for individual samples (with their specific sensitivities), but the proposed approaches can go a long way towards the comparability of outdoor weathering exposures. T2 - 10th European Weathering Symposium EWS CY - Graz, Austria DA - 11.09.2024 KW - Polymer 3R KW - Outdoor weathering PY - 2024 SN - 978-3-9826129-1-1 SP - 121 EP - 133 PB - Stober Medien GmbH CY - Eggenstein AN - OPUS4-61291 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Geburtig, Anja T1 - Significance of new data pairs for irradiance and (surface) temperature N2 - There is consent that UV irradiance and temperature at the place of photodegradation are the most important environmental parameters in weathering, along with humidity. This contribution shows how an improvement in the measurement data situation can improve the significance and comparability of outdoor exposures. Photooxidative ageing is calculated using sample polymers for which the corresponding modelling data (Exposure Response Functions, ERF) is available. The mean square deviations are estimated, which result from using different spectral irradiances and different spectral sensitivities, both of the sensors and the polymers. It will be shown here how the significance of the irradiance values increases with increasing approximation of the spectral sensitivities of the sensor and polymer. Also, the mean square deviations are estimated, which result from using different activation energies and surface temperatures. A selection of different variables to describe the weathering exposure is created. The potential of either individual values or data pairs is evaluated in terms of significance or correlation to the calculated photooxidative ageing. Recording hourly data also enables subsequent evaluations of individual test specimens, adapted to the respective colour or to determine activation energies. An accumulated value, calculated from PIT-radiometer irradiance and a suited surface temperature, can provide a comparison of different outdoor exposures over different locations or years. Thus, a characterisation of the weathering exposure would be related to a reference spectral sensitivity (much closer to a polymer than that of a common UV radiometer), one reference activation energy, and different surface temperature scenarios with, on the one hand, graded solar absorptions (white / grey / black) and, on the other hand, different thermal couplings (coated metal / thick plastic). This results in three values each for plastic samples and coated metals (light / grey / dark). It will never be possible to accurately predict the weathering tests for individual samples (with their specific sensitivities), but the proposed approaches can go a long way towards the comparability of outdoor weathering exposures. T2 - 10th European Weathering Symposium EWS CY - Graz, Austria DA - 11.09.2024 KW - Polymer 3R KW - Outdoor weathering PY - 2024 AN - OPUS4-61292 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Geburtig, Anja A1 - Wachtendorf, Volker A1 - Trubiroha, P. A1 - Giehl, A. A1 - Schönlein, A. A1 - Feil, F. T1 - Normenvorschlag zur Bewitterung transparenter oder transluzenter Kunststoffe N2 - Aufgrund des tieferen Eindringens der solaren Strahlung treten bei transparenten und bei transluzenten (durchscheinenden) Kunststoffen veränderte Bedingungen gegenüber opaken Proben auf. Dies kann zu speziellen Effekten und damit zu einem abweichenden Bewitterungsverhalten führen. Auch aus Mangel an geeigneten Normen werden diese Effekte häufig vernachlässigt. Deshalb initiiert der DIN-FNK auf ISO-Ebene ein entsprechendes Dokument. Die Norm ist in der Form eines Technical Reports geplant. In einem ersten Teil sollen die Besonderheiten transparenter oder transluzenter Kunststoffe erläutert werden, um den Nutzer für mögliche Probleme zu sensibilisieren. Im zweiten Teil werden Empfehlungen für Bestrahlung oder Bewitterung herausgearbeitet. In einem dritten Teil geht es dann um Besonderheiten bei der Messung von Eigenschaftsänderungen transparenter bzw. transluzenter Kunststoffe. In informativen Anhängen sollen verschiedene Beispiele die Thematik illustrieren. T2 - 51. Jahrestagung der GUS CY - Stutensee-Blankenloch, Germany DA - 29.03.2023 KW - Bewitterung KW - Polymer 3R KW - Bestrahlung KW - UV PY - 2023 SN - 978-3-9818507-8-9 SP - 39 EP - 46 PB - Gesellschaft für Umweltsimulation e.V. CY - Pfinztal (Berghausen) AN - OPUS4-57271 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Geburtig, Anja T1 - Simulationsdaten zur photooxidativen Beanspruchung an verschiedenen geografischen Freibewitterungs-Standorten N2 - Freibewitterungen weisen grundsätzlich eine hohe Variabilität der jeweiligen Intensität der Beanspruchungsparameter auf; sie sind nicht einfach wiederholbar. Um dennoch die Ergebnisse einer Beanspruchung vergleichen zu können, ist eine aussagekräftige Charakterisierung der Freibewitterung wichtig. Traditionell werden Daten bekannter Einflussgrößen wie Globalstrahlung, Temperatur oder Feuchtewerte herangezogen. Obwohl man weiß, dass diese Größen an den exponierten Oberflächen wechselwirken und kombiniert als Mikroklima Einfluss auf Degradationsprozesse nehmen, werden schon aus Praktikabilitätsgründen diese separat als klimatische Messgrößen angegeben. Die Aussagekraft dieser Daten ist mäßig. Ziel dieses Beitrags ist es, die Aussagekraft und damit Vergleichbarkeit zu erhöhen, indem diese Messdaten als Stundendaten zu Wirkintegralen vorverarbeitet und jahresweise akkumuliert werden. Betrachtet wird dafür der Prozess der Photooxidation, da dieser Alterungs-mechanismus bei allen Kunststoffen auftritt. Für eine einfache Modellierung wird die wirksame UV-Bestrahlung, gewichtet mit einer Arrhenius-abhängigen Ober¬flächen-temperatur (TOF), über den Beanspruchungszeitraum von hier je einem Jahr akkumuliert. Die Idee einer solchen Messgröße für photooxidative Ober¬flächen¬alterung wurde bereits vorgestellt [1]. Dort wurde ein Gerät vor¬geschlagen, mit dem dieser Wert für verschieden absorbierende Oberflächen für die Dauer einer Exposition akkumuliert wird, und ergänzend eine Abschätzung der Betauungs¬zeiten dieser Referenz-Oberflächen erfolgen könnte. Hier soll es um eine rechnerisch generierte Zusammenstellung dieser photo¬oxidativen 1-Jahres-Alterungswerte für verschiedene Standorte gehen. Ein Temperaturfaktor erfasst dabei den Einfluss der Strahlungserwärmung auf eine weiße, graue bzw. schwarze Referenzoberflächen, spiegelt also die Kopplung von solarer Strahlung und Temperatur wider [1]. Ermittelt wird er aus Stunden¬daten der Globalstrahlung und der Lufttemperatur. Die spektrale Wirkung wird aus Sonnenhöhenständen entsprechend der geografischen Breite mit Hilfe der FastRT-Oberfläche [2] als PiT·h-Wert abgeschätzt [3]. Anhand der errechneten Jahreswerte können die Schweregrade der photo¬oxidativen Beanspruchung an den verschiedenen Standorten unmittelbar verglichen werden. Die gezeigten Simulationsdaten für ein solches „elektronisches Referenzmaterial“ für photooxidative Degradation zeigen die prinzipielle Möglichkeit einer Kartografierung solcher Daten auf. T2 - 53. Jahrestagung der GUS CY - Stutensee, Germany DA - 26.3.2025 KW - Polymer 3R KW - UV KW - Bestrahlung KW - Bewitterung PY - 2025 AN - OPUS4-62903 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Geburtig, Anja T1 - Digitale Umweltsimulation am Beispiel der Photooxidation von Polymeren N2 - Die Umweltwirkungen auf ein Material werden als Überlapp der Funktionskurven von Materialempfindlichkeit und einwirkenden Umweltparametern betrachtet. Wenn entweder die Empfindlichkeit oder die Beanspruchungen Null sind, ergibt sich auch keine Umweltwirkung und bei beidseitig Werten größer Null das jeweilige Produkt der beiden. Die Akkumulation der nicht-reversiblen Effekte über die Zeit und allen Eigenschaftsänderungen entspricht der Alterung des Materials für den jeweiligen Expositionszeitraum. Die digitale Umweltsimulation gliedert sich hier in drei Teilaspekte. Ein erster, rein materialwissenschaftlicher Teil hat die Aufgabe, alle relevanten Materialempfindlichkeiten experimentell zu quantifizieren. Ein zweiter – unter Umständen numerischer Teil – hat die Aufgabe, das Bauteil und seine Einbaulage zu digitalisieren und aus den makroskopischen Umgebungsbedingungen die relevanten mikroklimatischen Umweltparameter für alle Oberflächen- oder Volumenelemente zu bestimmen. In einem dritten Teil werden die Einwirkungen über den betrachteten Zeitraum berechnet und kumuliert. Dieses Konzept, das auf den so genannten Expositions-Reaktions-Funktionen (ERF) basiert, wird an Beispielen der Photoxidation erläutert. Dieses Vorgehen wurde schon beim ViPQuali-Projekt als Numerische Umweltsimulation umgesetzt. Überprüft werden muss das Modell unbedingt an einer realitätsnahen Validierungsbeanspruchung. Hier werden die ermittelten ERFs mit über den kompletten Beanspruchungszeitraum geloggten Umweltparametern gekoppelt, um die berechnete mit der experimentell erfahrenen Alterungswirkung zu vergleichen. Nur so kann sichergestellt sein, dass alle für die Anwendungsumgebung relevanten Materialempfindlichkeiten einbezogen wurden. T2 - 52. Jahrestagung der GUS CY - Blankenloch, Germany DA - 26.03.2024 KW - Polymer 3R KW - UV KW - Bestrahlung KW - Bewitterung PY - 2024 AN - OPUS4-59831 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wachtendorf, Volker T1 - Gedanken, Tipps & Tricks zu künstlichen Bewitterungsprüfungen N2 - Die Fragestellung kann nur exemplarisch dargestellt werden, aber ist hoffentlich auch für langjährige Praktiker in den ausgewählten Punkten interessant. Es sollen für folgende Bereiche Beispiele gegeben werden: Probenvorbereitung, Testvorbereitung, Testdurchführung und Auswertung. T2 - 53. Jahrestagung der GUS 2025; Umwelteinflüsse erfassen, simulieren, bewerten. CY - Stutensee, Germany DA - 26.03.2025 KW - Künstliche Bewitterung KW - Umweltsimulation KW - Wechseltemperaturen KW - Prüfung KW - UV KW - Feuchte KW - Beregnung PY - 2025 AN - OPUS4-62862 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Wachtendorf, Volker A1 - Wägner, Yannick A1 - Geburtig, Anja T1 - Gedanken, Tipps & Tricks zu künstlichen Bewitterungsprüfungen N2 - Die Fragestellung kann nur exemplarisch dargestellt werden, aber ist hoffentlich auch für langjährige Praktiker in den ausgewählten Punkten interessant. Es sollen für folgende Bereiche Beispiele gegeben werden: Probenvorbereitung, Testvorbereitung, Testdurchführung und Auswertung. T2 - 53. Jahrestagung der GUS 2025 CY - Stutensee-Blankenloch bei Karlsruhe, Germany DA - 26.03.2025 KW - Wechseltemperaturen KW - Künstliche Bewitterung KW - Prüfung KW - UV KW - Feuchte KW - Beregnung PY - 2025 SN - 978-3-9826129-2-8 VL - 53 SP - 253 EP - 257 PB - Gesellschaft für Umweltsimulation e.V. CY - 76327 Pfinztal (Berghausen) AN - OPUS4-62861 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -