TY - CONF A1 - Benseghier, Z. A1 - Philippe, P. A1 - Bonelli, S. A1 - Luu, L.-H. A1 - Cuéllar, Pablo T1 - Numerical modeling of erosion of cohesive granular material by a fluid flow N2 - The erosion phenomena is the main cause of the most serious incidents observed on earthen hydraulic structures such as dams and dikes. Thus, there is a real need to explore in depth and understand the mechanisms at work in such complex erosional processes for preventing similar risks. The aim of this study is to provide a micromechanical insight into the mechanisms taking place during the erosion of a cohesive granular material driven by a fluid flow, the objectives are summarized as follows: Perform numerical erosion tests. Parallelization of the code (Gpu). Extensive parametric analysis => rely micro parameters (eg. Cohesion) to macro parameters (eg. Soil erodibility, mechanical strengths). T2 - Ecole doctorale ED353, « Sciences Pour l'Ingénieur », Aix-Marseille Université (AMU) et Ecole Centrale de Marseille (ECM) CY - Marseille, France DA - 30.05.2018 KW - Erosion KW - Cohesive soils KW - LBM-DEM simulation PY - 2018 AN - OPUS4-46314 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Benseghier, Z. A1 - Cuéllar, Pablo A1 - Luu, L.-H. A1 - Delenne, J.-Y. A1 - Bonelli, S. A1 - Philippe, P. T1 - Use of DEM-LBM modeling to prove the relevance of free jet model for soil erosion by impinging jet N2 - The aim of this study is to provide a micromechanical insight into the mechanisms taking place during the erosion of a cohesive granular material driven by a fluid flow, the objectives are summarized as follows: Perform numerical erosion tests. Parallelization of the code (Gpu). Extensive parametric analysis => rely micro parameters (eg. Cohesion) to macro parameters (eg. Soil erodibility, mechanical strengths). T2 - 2nd YADE Workshop, IRSTEA, Aix-en-Provence CY - Aix-en-Provence, France DA - 26.04.2018 KW - DEM-LBM simulation KW - Erosion of cohesive soils KW - Jet erosion test PY - 2018 AN - OPUS4-46315 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Shamsuddoha, Md A1 - Hüsken, Götz A1 - Schmidt, Wolfram A1 - Kühne, Hans-Carsten A1 - Baeßler, Matthias ED - Alexander, M.G. ED - Beushausen, H. ED - Dehn, F. ED - Moyo, P. T1 - Workability and mechanical properties of ultrafine cement based grout for structural rehabilitation: A parametric study on the partial replacement with SCMs T2 - Proceedings of the International Conference on Concrete Repair, Rehabilitation and Retrofitting (ICCRRR 2018) N2 - Grouting is a universal repair and strengthening technique, which is constantly used for structural remediation of concrete components, trenches, mine subsidence, dam joints, restoration of masonry structures, and geological stabilizations. Having an extremely small particle size of only few microns, ultrafine cements are ideal for grouting applications due to their superior permeability and compressive strength properties of the hardened cement paste compared to that of the less-expensive, but coarser ordinary Portland cements. Supplementary cementitious materials (SCMs) are often used to replace ultrafine cement in order to modify certain properties and to reduce costs. The aim of this experimental study is to investigate the effect of three supplementary materials: microsilica (MS), fly ash (FA), and metakaolin (MK) on the workability, and mechanical properties of an ultrafine cement based grout with a constant water-binder ratio and constant superplasticizer content. Maximum percentages of replacement with ultrafine cement were 6% by volume of cement for MS and 16% for FA, and MK. In general, results suggest that the workability is improved by addition of FA, whereas is reduced, when modified with MS and MK. The compressive strength of grout after cement replacement remains comparable to that of pure cement grout. However, there is a tendency of the MS to positively affect the compressive strength opposite to FA, whereas flexural strength is positively affected by FA. Based on the results, it is evident that grouts with Hägerman cone flow more than 500 mm and compressive strength of more than 90 MPa after 28 days can be produced. T2 - International Conference on Concrete Repair, Rehabilitation and Retrofitting (ICCRRR 2018) CY - Cape Town, South Africa DA - 19.11.2018 KW - Grouting KW - Repair KW - Box-Behnken KW - Supplementary cementitious materials KW - Analysis of variance PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-464769 DO - https://doi.org/10.1051/matecconf/201819907006 SN - 2261-236X VL - 199 SP - 07006-1 EP - 07006-7 PB - MATEC Web of Conferences AN - OPUS4-46476 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Shamsuddoha, Md A1 - Hüsken, Götz A1 - Schmidt, Wolfram A1 - Kühne, Hans-Carsten A1 - Baeßler, Matthias T1 - Superplasticizer and shrinkage reducing admixture dosages for microfine cement in grout systems N2 - Grouts have numerous applications including crack repair as maintenance in construction industries. Microfine cements are intensively used for high strength mortar and grout products. They are ideal for injection grouting in structural repair. Such grouts should have suitable rheological properties to be injectable, especially those used in repair and rehabilitation. The use of superplasticizers (SP) in these products is thus becoming increasingly crucial to achieve favorable workability and viscosity properties. A difficulty in such grouts is the plastic shrinkage due to finer particles used. It is thus necessary to determine optimum SP and shrinkage reducing admixture (SRA) dosages for a microfine cement based grout. In this study, a saturation dosage was decided from two Polycarboxylate ether (PCE) based SPs in relation to neat cement using slump flow and rheological parameters. A range of grout mixtures was formulated containing micro silica (MS) and fly ash (FA), and tested for suitable rheological and mechanical parameters. Based on the results, a grout mixture with MS and FA was selected to determine optimum SRA content. According to the results, a SP dosage of 3% by weight of neat cement is sufficient to achieve saturation. The grout material including MS and FA can produce comparable properties to neat cement grout. MS is found to improve compressive strength within the range considered, whereas a higher FA content provides favourable rheological properties. Finally, a SRA dosage of 4%, which could reduce the shrinkage by about 43% after 28d days, is determined for the grout system. T2 - 2nd International Conference on Building Materials and Materials Engineering (ICBMM 2018) CY - University of Lisbon, Portugal DA - 26.09.2018 KW - Grout KW - Mix design KW - Shrinkage KW - Crack repair KW - Microfine cement PY - 2018 AN - OPUS4-46155 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Shamsuddoha, M. A1 - Hüsken, Götz A1 - Schmidt, Wolfram A1 - Kühne, Hans-Carsten A1 - Baeßler, Matthias T1 - Workability and mechanical properties of ultrafine cement based grout for structural rehabilitation: A parametric study on the partial replacement with SCMs N2 - Grouting is a universal repair and strengthening technique, which is constantly used for structural remediation of concrete components, trenches, mine subsidence, dam joints, restoration of masonry structures, and geological stabilizations. Having an extremely small particle size of only few microns, ultrafine cements are ideal for grouting applications due to their superior permeability and compressive strength properties of the hardened cement paste compared to that of the less-expensive, but coarser ordinary Portland cements. Supplementary cementitious materials (SCMs) are often used to replace ultrafine cement in order to modify certain properties and to reduce costs. The aim of this experimental study is to investigate the effect of three supplementary materials: microsilica (MS), fly ash (FA), and metakaolin (MK) on the workability, and mechanical properties of an ultrafine cement based grout with a constant water-binder ratio and constant superplasticizer content. Maximum percentages of replacement with ultrafine cement were 6% by volume of cement for MS and 16% for FA, and MK. In general, results suggest that the workability is improved by addition of FA, whereas is reduced, when modified with MS and MK. The compressive strength of grout after cement replacement remains comparable to that of pure cement grout. However, there is a tendency of the MS to positively affect the compressive strength opposite to FA, whereas flexural strength is positively affected by FA. Based on the results, it is evident that grouts with Hägerman cone flow more than 500 mm and compressive strength of more than 90 MPa after 28 days can be produced. T2 - International Conference on Concrete Repair, Rehabilitation and Retrofitting (ICCRRR 2018) CY - Cape Town, South Africa DA - 19.11.2018 KW - Analysis of variance KW - Box-Behnken KW - Grouting KW - Repair KW - Supplementary cementitious materials PY - 2018 AN - OPUS4-46712 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Shamsuddoha, Md A1 - Hüsken, Götz A1 - Schmidt, Wolfram A1 - Kühne, Hans-Carsten A1 - Baeßler, Matthias T1 - Ternary mix design of grout material for structural repair using statistical tools JF - Construction and Building Materials N2 - Repair is an indispensable part of the maintenance of structures over their lifetimes. Structural grouting is a widely used remediation technique for concrete components, trenches, mine subsidence, dam joints, restoration of masonry structures, and geological stabilizations. A structural grout system should be injectable in narrow spaces and hence include ingredients with finer particles. Ultrafine cements are ideal for these type of demanding grouts due to their superior properties compared to that of the less expensive, but coarser ordinary Portland cement (OPC). Supplementary cementitious materials (SCMs) are often used to replace OPC clinker based binder in order to modify certain properties and to reduce costs. The most commonly used SCMs are fly ash (FA), and ground granulated blast furnace slag (GGBS). For various special applications microsilica (MS), and metakaolin (MK) are also used. Identifying the optimum replacement contents of OPC by SCMs are a challenge during the design of such grouts. The aim of this experimental study is to investigate the effect of the selected SCMs (FA, MS and MK) on the slump flow, time of efflux, viscosity, shrinkage, and compressive and flexural strength of ultrafine cement based grouts with constant water-binder ratio and superplasticizer content. The test program was formulated using Box-Behnken design principles. Maximum percentages of replacement with ultrafine cement was 6% by volume of cement for MS and 16% for FA, and MK. The results suggest that most investigated grouts have the potential to be used for structural applications. The appropriate quadratic models are then formulated through statistical tools and presented as response surfaces. The trends indicate that fly ash improves the rheological properties, whereas microsilica and metakaolin positively affect shrinkage and mechanical properties to some extent. Based on the influence of SCMs and priorities among the properties, Decision Matrix Analysis (DMA) is carried out to select the most suitable ones among the SCMs. The analysis suggests that microsilica and fly ash are more suitable as SCMs than metakaolin without affecting the properties. KW - Grouting KW - Microsilica KW - Fly ash KW - Metakaolin KW - Workability KW - Viscosity KW - Strength KW - Mix design KW - Box-Behnken KW - Decision matrix analysis PY - 2018 DO - https://doi.org/10.1016/j.conbuildmat.2018.08.156 SN - 0950-0618 SN - 1879-0526 VL - 189 SP - 170 EP - 180 PB - Elsevier Ltd. AN - OPUS4-45922 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schneider, Ronald T1 - Risikoanalyse technischer Systeme: Aktivitäten an der BAM N2 - Die Risikoanalyse ist ein formales Verfahren zur Unterstützung von Entscheidungen unter Unsicherheit und Risiko. Es ermöglicht eine Optimierung von Maßnahmen zur Verhinderung unerwünschter Konsequenzen. Der Vortrag stellt die aktuellen Aktivitäten an der BAM in dem Feld Risikoanalyse technischer System vor. T2 - 4. Sitzung des Beirates „Infrastruktur“ der Bundesanstalt für Materialforschung und –prüfung (BAM) CY - Berlin, Germany DA - 19.04.2018 KW - Risiko KW - Risikoanalyse PY - 2018 AN - OPUS4-46436 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schneider, Ronald T1 - Bayes‘sche Analyse von Ingenieurmodellen N2 - Der Vortrag zeigt, dass Unsicherheiten in Ingenieurmodellen quantitativ mit Methoden der Wahrscheinlichkeitstheorie modelliert werden können. Zusätzlich können durch eine Bayes‘sche Analyse probabilistische Ingenieurmodelle konsistent anhand von Daten „gelernt“ werden. T2 - Workshop "Digitaler Zwilling" des BAM Koptenzzentrums „Modellierung und Simulation“ CY - Berlin, Germany DA - 04.06.2018 KW - Probabilitische Ingenieurmodelle KW - Bayes'sche Analyse PY - 2018 AN - OPUS4-46437 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Baeßler, Matthias A1 - Schneider, Ronald A1 - Hille, Falk A1 - Herrmann, Ralf A1 - Said, Samir T1 - Anwendung von kontinuierlichen sensor-basierten Monitoringverfahren zur Bewertung von Infrastrukturbauwerken N2 - Kontinuierliche Sensorbasierte Bauwerksmessungen leisten einen wichtigen Beitrag zur Sicherheit von Verkehrsbauwerken. Hierzu werden im Vorhaben AISTec Referenzbauwerke und Referenzverfahren untersucht. Der Vortrag stellt die Expertise des FB 7.2, Herangehensweisen und Projektziele vor´. T2 - Kick-Off AIStec CY - Weimar, Germany DA - 17.10.2018 KW - Zivile Sicherheit KW - Brücken KW - SHM PY - 2018 AN - OPUS4-46325 LA - deu AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -