TY - CONF A1 - Cook, Jake Thomas T1 - Assessment of concrete bioreceptivity in algal biofilm green façade systems N2 - Content: Why Algal Biofilm Green Façade Systems?, Factors Influencing Bioreceptivity, Influence of pH and Microorganism Symbiosis, Pulse-Amplitude-Modulation (PAM) Fluorometry T2 - International Conference on Bio-Based Building Materials CY - Vienna, Austria DA - 21.06.2023 KW - Concrete KW - Façade KW - Bio-receptive KW - Extracellular polymeric substances KW - Fractional factorial PY - 2023 UR - https://www.rilem.net/agenda/5th-international-conference-on-bio-based-building-materials-1501 AN - OPUS4-58962 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Cook, Jake Thomas T1 - Assessment of concrete bioreceptivity in algal biofilm green façade systems N2 - Algal biofilm façades are an alternative to traditional green façades which can help to improve biodiversity and air quality within cities. They present a low maintenance approach in which subaerial algae are grown directly on concrete substrates. The intrinsic bioreceptivity of the substrate is a critical factor in successful facade colonisation. Existing research has identified several environmental and material properties which influence concrete bioreceptivity, however a consensus has yet to be made on which properties are most influential and how the interaction between properties may promote algal biofilm growth under specific conditions. T2 - International Conference on Bio-Based Building Materials CY - Vienna, Austria DA - 21.06.2023 KW - Concrete KW - Façade KW - Bio-receptive KW - Extracellular polymeric substances KW - Fractional factorial PY - 2023 UR - https://www.rilem.net/agenda/5th-international-conference-on-bio-based-building-materials-1501 AN - OPUS4-58976 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Cunningham, Patrick A1 - Wang, L. A1 - Kane, S. A1 - Kim, A. A1 - Jenkins, B. M. A1 - Miller, S. A. T1 - Lifecycle implications and mechanical properties of carbonated biomass ashes as carbon-storing supplementary cementitious materials N2 - Methods to sequester and store atmospheric CO2 are critical to combat climate change. Alkaline-rich bioashes are potential carbon fixing materials. This work investigates potential co-benefits from mineralizing carbon in biomass ashes and partially replacing high embodied greenhouse gas (GHG) Portland cement (PC) in cement-based materials with these ashes. Specifically, rice hull ash (RHA), wheat straw ash (WSA), and sugarcane bagasse ash (SBA) were treated to mineralize carbon, and their experimental carbon content was compared to modeled potential carbonation. To understand changes in the cement-based storage materials, mortars made with CO2-treated WSA and RHA were experimentally compared to PC-only mortars and mortars made with ashes without prior CO2 treatment. Life cycle assessment methodology was applied to understand potential reductions in GHG emissions. The modeled carbonation was ∼18 g-CO2/kg-RHA and ∼180 g-CO2/kg-WSA. Ashes oxidized at 500 °C had the largest measured carbon content (5.4 g-carbon/kg-RHA and 35.3 g-carbon/kg-WSA). This carbon appeared to be predominantly residual from the biomass. Isothermal calorimetry showed RHA-PC pastes had similar heat of hydration to PC-pastes, while WSA-PC pastes exhibited an early (at ∼1.5 min) endothermic dip. Mortars with 5 % and 15 % RHA replacement had 1–12 % higher compressive strength at 28 days than PC-only mortars, and milled WSA mortars with 5 % replacement had 3 % higher strength. A loss in strength was noted for the milled 15 % WSA, the CO2-treated 5 %, and the 15 % WSA mortars. Modeled reductions in GHG emissions from CO2-treated ashes were, however, marginal (<1 %) relative to the untreated ashes. KW - CO2 sequestration KW - CO2 storage KW - Biomass ash KW - Supplementary cementitious materials KW - Concrete PY - 2025 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-626959 DO - https://doi.org/10.1016/j.biombioe.2025.107772 SN - 1873-2909 VL - 197 SP - 1 EP - 13 PB - Elsevier CY - Amsterdam AN - OPUS4-62695 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Vogler, Nico A1 - Drabetzki, Philipp A1 - Lindemann, Mathias A1 - Kühne, Hans-Carsten T1 - Description of the concrete carbonation process with adjusted depth resolved thermogravimetric analysis N2 - The thermal gravimetric analysis (TG) is a common method for the examination of the carbonation progress of cement-based materials. Unfortunately, the thermal properties of some components complicate the evaluation of TG results. Various hydrate phases, like ettringite (AFt), C-S-H and AFm decompose almost simultaneously in the temperature range up to 200 °C. Additionally, physical bound water is released in the same temperature range. In the temperature range between 450 °C and 600 °C the decomposition of calcium hydroxide and amorphous or weakly bound carbonates takes place simultaneously. Carbonates, like calcite, from limestone powder or other additives may be already contained in the noncarbonated sample material. For this research an attempt was made to minimise the influence of these effects. Therefore, differential curves from DTG-results of non-carbonated areas and areas with various states of carbonation of the same sample material were calculated and evaluated. Concretes based on three different types of cement were produced and stored under accelerated carbonation conditions (1 % CO2 in air). The required sample material was obtained by cutting slices from various depth of previously CO2-treated specimen and subsequent grinding. During the sample preparation, a special attention was paid that no additional carbonation processes took place. As reference method for the determination of the carbonation depth the sprayed application of phenolphthalein solution was carried out. Microscopic analysis where examined to confirm the assumptions made previously. Furthermore, the observed effect of encapsulation of calcium hydroxide by carbonates caused by the accelerated carbonation conditions was examined more closely. KW - Microscopy KW - Accelerated carbonation KW - Carbonation behaviour KW - Concrete KW - Thermal Analysis PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-530571 DO - https://doi.org/10.1007/s10973-021-10966-1 VL - 147 IS - 11 SP - 1 EP - 14 PB - Springer AN - OPUS4-53057 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Deresse, N. E. A1 - Thiele, Marc A1 - Pirskawetz, Stephan A1 - Sarem, M. A1 - Francois, St. A1 - Verstrynge, E. T1 - Evaluation of Concrete Fatigue Damage with Elastic Wave-based Measurement Techniques N2 - The fatigue damage evolution and the fatigue life of quasi-brittle materials such as concrete are not yet completely understood. Accordingly to get better insights, researchers have recently been incorporating advanced measuring techniques in their fatigue experiments. In this research, acoustic emission techniques (AET), active ultrasonic, and deformation measurements are used to track the damage evolution of concrete samples subjected to fatigue loading. The samples are subjected to constant amplitude and stepwise fatigue loading in Brazilian splitting test set-ups. Initially, a good agreement is observed between the deformation and the ultrasonic measurements in capturing the crack propagation during Brazilian splitting tests. The three fatigue damage phases could be identified with all of the three techniques. The Phase II damage rates quantified by deformation measurements and AET in stepwise fatigue tests were used to predict the number of cycles to failure at various stress levels. The predictions were validated using the number of cycles to failure of the constant amplitude fatigue tests. T2 - 36th Conference of the European Working Group on Acoustic Emission CY - Potsdam, Germany DA - 18.09.2024 KW - Concrete KW - Acoustic emission KW - Ultrasonic testing KW - Fatigue PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-615677 DO - https://doi.org/10.58286/30228 SN - 1435-4934 VL - 29 IS - 10 SP - 1 EP - 10 PB - NDT.net AN - OPUS4-61567 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Krüger, Miriam E. A1 - Hilbig, Harald A1 - Stelzner, Ludwig A1 - Machner, Alisa T1 - Effect of the chemical composition of synthetic alkali-silica gels on their structure, swelling behavior and water uptake N2 - For alkali-silica reaction (ASR) gels, the relationship between swelling expansion, structure and chemical composition, particularly the effect of aluminum, remains unknown. This study investigates the structure, swelling expansion and associated water uptake of synthetic ASR gels with various Al/Si (0–0.1) and Ca/Si (0.1–0.4) ratios. The results show that aluminum incorporated into the gel structure reduces the overall swelling expansion and the leaching of silicate species during the swelling test. Moreover, they revealed that water in the Al-ASR gels is more tightly bound, reducing the overall water uptake compared to the Al-free ASR gels. Additionally, there is a linear correlation between the maximal swelling results and the ASR gel composition. However, no direct correlation emerged between the amount of water uptake and the free swelling of the ASR gels, which indicates that other factors, like the type of water bonding and pore size of the gels, are decisive for the swelling mechanism. KW - Concrete KW - Alkali-silica reaction (ASR) KW - Durability KW - 1H NMR relaxometry KW - 29Si NMR KW - 27Al NMR KW - FTIR KW - Al-ASR gel KW - Swelling test PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-624268 DO - https://doi.org/10.1016/j.cemconres.2024.107596 VL - 184 SP - 1 EP - 18 PB - Elsevier B.V. AN - OPUS4-62426 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Klimek, André A1 - Stelzner, Ludwig A1 - Hothan, Sascha A1 - Zehfuß, Jochen T1 - Influence of thermal strain on concrete spalling N2 - Understanding the susceptibility to spalling of concrete members in case of fire is important to evaluate the residual load-bearing capacity. The investigations of the spalling phenomenon of a concrete mixture using real scale members are necessary but expensive to carry out. Reducing the specimen size leads to an increase of boundary effects that can result in a reduced spalling or absence of spalling. In this study, fire tests were carried out on unrestrained, single-sided exposed, cuboid shaped specimens (0.6 m x 0.6 m x 0.29 m) as well as unrestrained and steel ring restrained cylindrical specimens (Ø = 0.47 m, h = 0.29 m), which induce different boundary conditions. These fire tests were carried out on two ordinary concrete mixtures. The two mixtures differ only in the type of aggregates (quartz gravel and basalt grit) and were used to investigate the influence of the thermal expansion of the aggregate on the spalling behaviour of the concrete. The results show a significant increase of the spalling depth due to the restrained thermal expansion achieved by the applied steel rings. Additionally, the type of aggregate has a direct influence on the spalling behaviour of a concrete mixture. The reduction of the boundary effects by the steel rings recreate the test conditions in the centre of a large concrete member. Thus, this type of specimen is suitable to determine the susceptibility to spalling of a material (screening-tests) as preliminary investigations to full scale fire tests. KW - Spalling KW - Concrete KW - Fire test KW - Restraint KW - Screening test PY - 2024 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-593350 DO - https://doi.org/10.1617/s11527-023-02274-x VL - 57 SP - 1 EP - 14 PB - Springer AN - OPUS4-59335 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Sigrüner, M. A1 - Hüsken, Götz A1 - Pirskawetz, Stephan A1 - Herz, J. A1 - Muscat, D. A1 - Strübbe, N. T1 - Pull-out behavior of polymer fibers in concrete N2 - The bond between polymer fibers and the surrounding cementitious matrix is essential for the development of concrete reinforcement. The single fiber pull-out test (SFPT) is the standard characterization technique for testing the bond strength. However, the different phases of debonding cannot be distinguished by the SFPT. This study investigates the debonding of different polymer fibers from the surrounding cementitious matrix with a modified SFPT and proposes methods to change the SFPT setup to generate more valuable information on the debonding mechanism. The SFPT was equipped with linear variable differential transformers (LVDT), digital image correlation (DIC) and acoustic emission (AE) analysis. The results demonstrate that the modified SFPT allows a better understanding of the different phases of debonding during fiber pull-out. Furthermore, bond strength values calculated by different methods reveal that the chemical bond of the investigated polymers is not different as reported by previous studies. Deformation measurements performed using LVDTs and DIC are suitable measuring techniques to characterize the debonding mechanism in SFPT. A correlation between recorded AE and debonding phases was not found. KW - Polymer Fibres KW - Concrete KW - Pull-Out Behaviour KW - Debonding Mechanism PY - 2023 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-582918 DO - https://doi.org/10.1002/pol.20230264 SN - 2642-4169 SP - 1 EP - 13 PB - Wiley Periodicals, LLC. AN - OPUS4-58291 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pohl, Christoph A1 - Smilauer, V. A1 - Unger, Jörg F. T1 - A three-phase transport model for high-temperature concrete simulations validated with X-ray CT data N2 - Concrete exposure to high temperatures induces thermo-hygral phenomena, causing water phase changes, buildup of pore pressure and vulnerability to spalling. In order to predict these phenomena under various conditions, a three-phase transport model is proposed. The model is validated on X-ray CT data up to 320 ◦C, showing good agreement of the temperature profiles and moisture changes. A dehydration description, traditionally derived from thermogravimetric analysis, was replaced by a formulation based on data from neutron radiography. In addition, treating porosity and dehydration evolution as independent processes, previous approaches do not fulfil the solid mass balance. As a consequence, a new formulation is proposed that introduces the porosity as an independent variable, ensuring the latter condition. KW - Concrete KW - Porous media KW - Spalling KW - Dehydration KW - Moisture transport KW - Heat transfer KW - Pore pressure KW - Porosity KW - Finite elements PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-532840 UR - https://doi.org/10.5281/zenodo.4890635 DO - https://doi.org/10.3390/ma14175047 SN - 1996-1944 VL - 14 IS - 17 SP - 1 EP - 21 PB - MDPI CY - Basel AN - OPUS4-53284 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Klimek, André A1 - Stelzner, Ludwig A1 - Hothan, Sascha A1 - Rogge, Andreas T1 - Fire induced concrete spalling in combination with size effects N2 - The size effect has its origin in fracture mechanics and describes the formation as well as propagation of cracks in brittle and solid materials in dependence of the specimen size. However, the size effect in concrete spalling describes the damage behaviour on a macroscopic scale for different sized specimens in case of fire. Concrete spalling is a very complex and yet not fully understood phenomenon. To reduce the effort of fire tests to analyse the spalling behaviour of concrete mixtures, this study investigates the susceptibility to spalling for six different concrete mixtures and three specimen sizes. The sizes were divided in full scale slabs (1.8 m x 1.2 m x 0.3 m), intermediate scale cuboids (0.6 m x 0.6 m x 0.3 m) and small scale cylinders (Ø0.15 m x 0.3 m). For this purpose, a novel test set-up was built to test six intermediate scale or twelve small scale specimens simultaneously to ensure a similar heating regime for every specimen. All specimens were fire exposed on one side and remained unrestrained. A size effect occurred for four of the six concrete mixtures. Compared to the full scale specimens the spalling was reduced significantly for all smaller specimen sizes. Additionally, spalling did not occur for the small scale specimens. The results show that the specimen size is an essential parameter to investigate the susceptibility to spalling of a concrete mixture. For future investigations the testing conditions must be adjusted for the intermediate scale specimens to recreate the conditions of the slabs. KW - Concrete KW - Spalling KW - Size effect KW - Fire test PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-559231 DO - https://doi.org/10.1617/s11527-022-02051-2 VL - 55 IS - 8 SP - 1 EP - 14 PB - Springer AN - OPUS4-55923 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pittrich, Tim A1 - Stelzner, Ludwig A1 - Weise, Frank T1 - Fire-induced spalling of normal strength concrete with different types of blended Portland cement N2 - The cement industry is looking to reduce its overall CO2 footprint. Greener manufacturing can be achieved by the introduction of more clinker-reduced cements. Concrete exposed to fire tends to show explosive spalling caused by thermomechanical and thermohydraulic processes. It is therefore essential to determine how concretes with clinker-reduced cements behave under fire exposure, especially for concretes containing calcined clays, as these are expected to be the supplementary cementitious material of the future. In this paper, normal strength concretes with four different cements (CEM I, CEM II/A-LL, CEM III/A and CEM II/B-Q) were examined for their fire-induced spalling behaviour. In addition, a mix with PP fibres was investigated for each concrete. The experiments were conducted on ring-restrained cylindrical specimens exposed to the hydrocarbon fire curve. The results showed that the cement type influences spalling behaviour. Samples with CEM I spalled the least, followed by CEM II/A-LL and CEM III/A. Finally, samples with CEM II/B-Q showed the most severe damage. It was found that the spalling behaviour of different concretes correlates with the moisture content before exposure to fire, meaning that higher moisture content leads to higher spalling susceptibility. The use of 2 kg/m³ PP fibres completely inhibited spalling regardless of the cement type used and therefore remains a successful avoidance strategy. T2 - Structures in Fire 2024 CY - Coimbra, Portugal DA - 19.06.2024 KW - Fire-induced concrete spalling KW - Concrete KW - Blended Portland cement KW - SCM KW - PP-fibres PY - 2024 SN - 978-989-35292-2-5 DO - https://doi.org/10.30779/cmm_SIF24 VL - 1st Edition SP - 461 EP - 471 AN - OPUS4-60809 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pimienta, Pierre A1 - McNamee, Robert A1 - Robert, Fabienne A1 - Boström, Lars A1 - Huang, Shan-Shan A1 - Mróz, Katarzyna A1 - Davie, Colin A1 - Mohaine, Siyimane A1 - Alonso, Maria Cruz A1 - Bodnarova, Lenka A1 - Bosnjak, Josipa A1 - Dal Pont, Stefano A1 - Dao, Vinh A1 - Dauti, Dorjan A1 - Dehn, Frank A1 - Felicetti, Roberto A1 - Hager, Izabela A1 - Hela, Rudolf A1 - Hozjan, Tomaz A1 - Juknat, Michael A1 - Jumppanen, Ulla-Maija A1 - Kirnbauer, Johannes A1 - Kolsek, Jerneja A1 - Korzen, Manfred A1 - Lakhani, Hitesh A1 - Lion, Maxime A1 - Lo Monte, Francesco A1 - Maluk, Cristian A1 - Meftah, Fekri A1 - Miah, Md Jihad A1 - Millard, Alain A1 - Mindeguia, Jean-Christophe A1 - Moreau, Bérénice A1 - Msaad, Yahia A1 - Ozawa, Mitsuo A1 - Pesavento, Francesco A1 - Pham, Duc Toan A1 - Pistol, Klaus A1 - Rickard, Ieuan A1 - Rodrigues, Joao Paulo Correia A1 - Roosefid, Mohsen A1 - Schneider, Martin A1 - Sharma, Umesh Kumar A1 - Sideris, Kosmas A1 - Stelzner, Ludwig A1 - Weber, Benedikt A1 - Weise, Frank T1 - Recommendation of RILEM TC 256-SPF on fire spalling assessment during standardised fire resistance tests: complementary guidance and requirements N2 - The recommendation is based on the co-authors’ work organized by the RILEM TC 256-SPF “Spalling of concrete due to fire: testing and modelling”. It aims to provide useful information, guidance and best practices in fire spalling assessment to laboratories that perform large-scale tests based on fire resistance test standards. It provides guidance on the spalling observation techniques during testing, as well as post-test spalling quantification/assessment methods. This document is intended to be used in conjunction with the fire resistance test standards, e.g. EN 1363-1 and ISO 834-1. KW - Concrete KW - Fire spalling KW - Large scale tests KW - Standardised fire resistance tests PY - 2024 DO - https://doi.org/10.1617/s11527-023-02248-z SN - 1871-6873 VL - 57 IS - 1 SP - 1 EP - 12 PB - Springer CY - Dordrecht AN - OPUS4-59288 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pimienta, Pierre A1 - McNamee, Robert A1 - Hager, Izabela A1 - Mróz, Katarzyna A1 - Boström, Lars A1 - Mohaine, Siyimane A1 - Huang, Shan-Shan A1 - Mindeguia, Jean-Christophe A1 - Robert, Fabienne A1 - Davie, Colin A1 - Felicetti, Roberto A1 - Miah, Md Jihad A1 - Lion, Maxime A1 - Lo Monte, Francesco A1 - Ozawa, Mitsuo A1 - Rickard, Ieuan A1 - Sideris, Kosmas A1 - Alonso, Maria Cruz A1 - Millard, Alain A1 - Jumppanen, Ulla-Maija A1 - Bodnarova, Lenka A1 - Bosnjak, Josipa A1 - Dal Pont, Stefano A1 - Dao, Vinh A1 - Dauti, Dorjan A1 - Dehn, Frank A1 - Hela, Rudolf A1 - Hozjan, Tomaz A1 - Juknat, Michael A1 - Kirnbauer, Johannes A1 - Kolsek, Jerneja A1 - Korzen, Manfred A1 - Lakhani, Hitesh A1 - Maluk, Cristian A1 - Meftah, Fekri A1 - Moreau, Bérénice A1 - Pesavento, Francesco A1 - Pham, Duc Toan A1 - Pistol, Klaus A1 - Correia Rodrigues, Joao Paulo A1 - Roosefid, Mohsen A1 - Schneider, Martin A1 - Sharma, Umesh Kumar A1 - Stelzner, Ludwig A1 - Weber, Benedikt A1 - Weise, Frank T1 - Recommendation of RILEM TC 256-SPF on the method of testing concrete spalling due to fire: material screening test N2 - The recommendation is based on the coauthors’ work organized by the RILEM TC 256-SPF ‘‘Spalling of concrete due to fire: testing and modelling’’. The Committee has defined two types of screening tests for characterization of concrete propensity to fire spalling: Material screening tests and Product screening tests. Definitions of both types of tests are given in the paper. The following recommendations apply to Material screening tests. The material screening tests described in these recommendations are a set of minimum requirements to test concrete spalling propensity (for example, the minimal specimen size). This document covers the aspects of concrete characterization, specimen geometries, storage conditions, test methods and measured parameters. KW - Concrete KW - Fire Spalling KW - Screening tests KW - High temperature PY - 2023 DO - https://doi.org/10.1617/s11527-023-02202-z VL - 56 IS - 9 SP - 1 EP - 12 PB - Springer Science and Business Media LLC AN - OPUS4-60635 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Thiele, Marc A1 - Pirskawetz, Stephan T1 - Analysis of damage evolution in concrete under fatigue loading by acoustic emission and ultrasonic testing N2 - The fatigue process of concrete under compressive cyclic loading is still not completely explored. The corresponding damage processes within the material structure are especially not entirely investigated. The application of acoustic measurement methods enables a better insight into the processes of the fatigue in concrete. Normal strength concrete was investigated under compressive cyclic loading with regard to the fatigue process by using acoustic methods in combination with other nondestructive measurement methods. Acoustic emission and ultrasonic signal measurements were applied together with measurements of strains, elastic modulus, and static strength. It was possible to determine the anisotropic character of the fatigue damage caused by uniaxial loading based on the ultrasonic measurements. Furthermore, it was observed that the fatigue damage seems to consist not exclusively of load parallel oriented crack structures. Rather, crack structures perpendicular to the load as well as local compacting are likely components of the fatigue damage. Additionally, the ultrasonic velocity appears to be a good indicator for fatigue damage beside the elastic modulus. It can be concluded that acoustic methods allow an observation of the fatigue process in concrete and a better understanding, especially in combination with further measurement methods. KW - Concrete KW - Fatigue KW - Damage evolution KW - Ultrasonic testing KW - Acoustic emission PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-541891 DO - https://doi.org/10.3390/ma15010341 SN - 1996-1944 VL - 15 IS - 1 SP - 341 EP - 355 PB - MDPI CY - Basel AN - OPUS4-54189 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -