TY - JOUR A1 - Zorn, R. A1 - Szymoniak, Paulina A1 - Kolmangadi, Mohamed Aejaz A1 - Wolf, M. A1 - Alentiev, D. A1 - Bermeshev, M. A1 - Böhning, Martin A1 - Schönhals, Andreas T1 - Low frequency vibrational density of state of highly permeable super glassy polynorbornenes – The Boson peak JF - Physical Chemistry Chemical Physics N2 - Inelastic incoherent neutron time-of flight scattering was employed to measure the low frequency density of states for a series of addition polynorbornenes with bulky side groups. The rigid main chain in combination with the bulky side groups give rise to a microporosity of these polymers in the solid state. The microporosity characterized by the BET surfaces area varies systematically in the considered series. Such materials have some possible application as active separation layer in gas separation membranes. All investigated materials show excess contributions to the Debye type density of states characteristic for glasses known as Boson peak. The maximum position of the Boson peak shifts to lower frequency values with increasing microporosity. Data for PIM-1 and Matrimid included for comparison are in good agreement to this dependency. This result supports the sound wave interpretation of the Boson peak. KW - Polynorbornes KW - Neutron Scattering PY - 2020 DO - https://doi.org/10.1039/d0cp03360j SN - 1463-9076 VL - 22 IS - 33 SP - 18381 EP - 18387 PB - Royal Chemical Society AN - OPUS4-51165 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schönhals, Andreas A1 - Zorn, R. A1 - Böhning, Martin T1 - Vibrational density of states and molecular mobility in a polymer with intrinsic microporosity PIM-1 as revealed by inelastic neutron scattering N2 - Polymers with intrinsic microporosity are promising candidates for the active separation layer in gas separation membranes. Here, by means of inelastic neutron scattering, the vibrational density of states (VDOS) and the molecular mobility were investigated for PIM-1, the prototypical polymer with intrinsic microporosity. The results are compared to data measured for a more conventional high-performance polyimide used in gas separation membranes (Matrimid). The measured data show the characteristic low frequency excess contribution to the VDOS above the Debye sound wave level, generally known as the Boson peak in glass-forming materials. In comparison to the Boson peak of Matrimid, that of PIM-1 is shifted to lower frequencies. This shift is discussed considering the microporous, sponge-like structure of PIM-1 as providing a higher compressibility at the molecular scale than for conventional polymers. Elastic fixed window scans were measured on a neutron backscattering spectrometer to have an overview about the molecular dynamics at a time scale of ca. 1 ns. The temperature dependence of the estimated mean squared displacement shows a step-like increase in the temperature range from 100 K to 250 K indicating the onset of some molecular mobility. The nature of this motional process was analyzed in detail by quasielastic neutron scattering combining Time-of-Flight and backscattering where the data are discussed with regard to both the q- and the temperature dependence. T2 - JCNS Workshop for Neutron Scattering CY - Tutzing at Munich, Germany DA - 07.10.2019 KW - Polymers of Intrinsic Microporosity KW - Neutron Scattering PY - 2019 AN - OPUS4-49271 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Schönhals, Andreas A1 - Zorn, R. A1 - Böhning, Martin T1 - Vibrational density of states and molecular mobility in a polymer with intrinsic microporosity PIM-1 as revealed by inelastic neutron scattering N2 - Polymers with intrinsic microporosity are promising candidates for the active separation layer in gas separation membranes. Here, by means of inelastic neutron scattering, the vibrational density of states (VDOS) and the molecular mobility were investigated for PIM-1, the prototypical polymer with intrinsic microporosity. The results are compared to data measured for a more conventional high-performance polyimide used in gas separation membranes (Matrimid). The measured data show the characteristic low frequency excess contribution to the VDOS above the Debye sound wave level, generally known as the Boson peak in glass-forming materials. In comparison to the Boson peak of Matrimid, that of PIM-1 is shifted to lower frequencies. This shift is discussed considering the microporous, sponge-like structure of PIM-1 as providing a higher compressibility at the molecular scale than for conventional polymers. Elastic fixed window scans were measured on a neutron backscattering spectrometer to have an overview about the molecular dynamics at a time scale of ca. 1 ns. The temperature dependence of the estimated mean squared displacement shows a step-like increase in the temperature range from 100 K to 250 K indicating the onset of some molecular mobility. The nature of this motional process was analyzed in detail by quasielastic neutron scattering combining Time-of-Flight and backscattering where the data are discussed with regard to both the q- and the temperature dependence. T2 - 7. European Conference on Neutron Scattering 2019 CY - Saint Petersburg, Russia DA - 30.06.2019 KW - Neutron Scattering KW - Polymer of intrinsic microporosity PY - 2019 AN - OPUS4-48421 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -