TY - JOUR A1 - Hilgenberg, Kai A1 - Daum, Werner A1 - Maierhofer, Christiane A1 - Altenburg, Simon A1 - Bruno, Giovanni A1 - Heckel, Thomas A1 - Skrotzki, Birgit A1 - Zerbst, Uwe A1 - Kranzmann, Axel A1 - Bettge, Dirk A1 - Sommer, Konstantin A1 - Seeger, Stefan A1 - Nitsche, Michael A1 - Günster, Jens A1 - Evans, Alexander T1 - Additive manufacturing at the BAM: We focus on Safety JF - Advanced Materials and Processes N2 - In Germany, the Federal Institute for Materials Research and Testing (BAM) is addressing challenges in the implementation of additive manufacturing on the industrial landscape for safety-critical applications. KW - Process development KW - Additive Manufacturing KW - In-situ Process Monitoring KW - Non-destructive Materials KW - Characterisation KW - Safety KW - Fatigue KW - Environment KW - Standardisation PY - 2019 UR - https://static.asminternational.org/amp/201910/22/ SN - 0882-7958 VL - 177 IS - 7 SP - 22 EP - 26 PB - ASM International CY - Materials Park, OH, USA AN - OPUS4-49780 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Pfennig, Anja A1 - Wolf, M. A1 - Kranzmann, Axel T1 - Corrosion and Corrosion Fatigue of Steels in Downhole CCS Environment—A Summary JF - Processes N2 - Static immersion tests of potential injection pipe steels 42CrMo4, X20Cr13, X46Cr13, X35CrMo4, and X5CrNiCuNb16-4 at T = 60°C and ambient pressure, as well as p = 100 bar were performed for 700–8000 h in a CO2-saturated synthetic aquifer environment similar to CCS sites in the Northern German Basin (NGB). Corrosion rates at 100 bar are generally lower than at ambient pressure. The main corrosion products are FeCO3 and FeOOH with surface and local corrosion phenomena directly related to the alloy composition and microstructure. The appropriate heat treatment enhances corrosion resistance. The lifetime reduction of X46Cr13, X5CrNiCuNb16-4, and duplex stainless steel X2CrNiMoN22-5-3 in a CCS environment is demonstrated in the in situ corrosion fatigue CF experiments (axial push-pull and rotation bending load, 60°C , brine: Stuttgart Aquifer and NGB, flowing CO2: 30 L/h, +/- applied potential). Insulating the test setup is necessary to gain reliable data. S-N plots, micrographic-, phase-, fractographic-, and surface analysis prove that the life expectancy of X2CrNiMoN22-5-3 in the axial cyclic load to failure is clearly related to the surface finish, applied stress amplitude, and stress mode. The horizontal grain attack within corrosion pit cavities, multiple fatigue cracks, and preferable deterioration of austenitic phase mainly cause fatigue failure. The CF life range increases significantly when a protective potential is applied. KW - Carbon capture and storage KW - Steel KW - High alloyed steel KW - Corrosion KW - Corrosion fatigue KW - CCS PY - 2021 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-523948 DO - https://doi.org/10.3390/pr9040594 VL - 9 IS - 4 SP - 594 PB - MDPI CY - Basel, Switzerland AN - OPUS4-52394 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Le, Quynh Hoa A1 - Bäßler, Ralph A1 - Knauer, S A1 - Jaeger, P A1 - Kratzig, Andreas A1 - Bettge, Dirk A1 - Kranzmann, Axel T1 - Droplet corrosion of CO2 transport pipeline steels in simulated oxyfuel flue gas JF - CORROSION N2 - The research focus of this study was set on the corrosion process of condensate as droplets on the surface of carbon steels (X52, X70) martensitic steel UNS S41500, and super austenite UNS N08031 in CO2 atmosphere with impurities at 278 K (to simulate the offshore transportation condition in a buried pipeline). The possibility of dew/droplet formation on the steel surface and wetting behavior of corresponding materials were evaluated by contact angle measurement in dense CO2 at 278 K. To observe the effect of impurities (SO2 and O2) on droplet corrosion process, exposure tests were carried out in the mixed atmosphere with a drop, 1 ‑ 10 µL in volume, of CO2 saturated ultra-pure water on steel surface. Comparable exposure tests were carried out with the same gas mixture and the same volume of water, as vapor, to observe the droplet formation and the corrosion process that follows. Effects of surface roughness on the droplet formation and its corrosion process were further studied and showed no significant role upon long time exposure. The results from droplet experiments were compared to those from the bulk electrolyte for the further recommendation on the quality control of gas stream along with the use of carbon steels as transport pipelines in CCS - Carbon Capture and Storage system. KW - CCUS, supercritical/dense phase CO2, carbon steels, martensitic steel, superaustenite steel, droplet corrosion PY - 2018 UR - http://corrosionjournal.com/doi/abs/10.5006/2927 DO - https://doi.org/10.5006/2927 SN - 0010-9312 SN - 1938-159X VL - 74 IS - 12 SP - 1406 EP - 1420 PB - NACE International CY - Houston, Texas, USA AN - OPUS4-46903 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Wollschläger, Nicole A1 - Nofz, Marianne A1 - Dörfel, Ilona A1 - Schulz, Wencke A1 - Sojref, Regine A1 - Kranzmann, Axel T1 - Exposition of sol-gel alumina-coated P92 steel to flue gas: Time-resolved microstructure evolution, defect tolerance, and repairing of the coating JF - Materials and Corrosion N2 - Technically relevant P92 steel (9% Cr) was coated with a micron-thick porous alumina layer prepared by sol-gel technique and treated with flue gas (60 CO2-30 H2O-2 O2-1 SO2-7 N2 (mole fraction in %)) at 650 ° to mimic an oxyfuelcombustion process. Local defects in the coating were marked using focused ion beam (FIB) technique and were inspected after exposition to hot flue gas atmosphere at 300, 800, and 1300 h, respectively. Local defects like agglomerated alumina sol particles tend to spall off from the coating uncovering the underlying dense chromia scale. Re-coating was found to restore the protection ability from oxidation when repeatedly treated with hot flue gas. Cracks and voids did not promote the local oxidation due to the formation of crystalline Mn/S/O species within and on top of the coating. The protective character of the steel-coating system is a result of (i) the fast formation of a dense chromia scale at the surface of sol-gel alumina-coated P92 steel bars in combination with (ii) the porous alumina coating acting as diffusion barrier, but also as diffusion partner in addition with (iii) fast Mn outward diffusion capturing the S species from flue gas. KW - Alumina coatings KW - Oxyfuel KW - Steel P92 KW - High temperature corrosion PY - 2018 DO - https://doi.org/10.1002/maco.201709712 SN - 1521-4176 SN - 0947-5117 SN - 0043-2822 VL - 69 IS - 4 SP - 492 EP - 502 PB - Wiley-VCH Verlag GmbH&Co. KGaA CY - Weinheim AN - OPUS4-45300 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Nützmann, Kathrin A1 - Wollschläger, Nicole A1 - Rockenhäuser, Christian A1 - Kranzmann, Axel A1 - Stephan-Scherb, Christiane T1 - Identification and 3D reconstruction of Cr5S6 precipitates along grain boundaries in Fe13Cr JF - JOM N2 - Metal sulfide grain boundary precipitates of a ferrous model alloy with 13 wt.% chromium formed at 650°C under a gas atmosphere containing 0.5% SO2 and 99.5% Ar were investigated after ageing for 3 h, 6 h, and 12 h. The precipitates formed along grain boundaries were identified as Cr5S6 using energy-dispersive x-ray spectroscopy in transmission electron microscopy and electron backscatter diffraction analysis. Serial focused ion beam slicing was conducted followed by three-dimensional reconstruction to determine the number, size, and penetration depth of the precipitates evolved at the different time steps. There was a linear increase in the number of precipitates with time, while their average size increased only for the initial aging time but became constant after 6 h. Based on these results, a model for grain boundary sulfidation of ferritic alloys is discussed. KW - Internal Sulfidation KW - Grain Boundary Corrosion KW - FIB Tomography PY - 2018 DO - https://doi.org/10.1007/s11837-018-2940-y SN - 1047-4838 SN - 1543-1851 VL - 70 IS - 8 SP - 1478 EP - 1483 PB - Springer Science + Business Media CY - New York, NY AN - OPUS4-45090 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Pfennig, Anja A1 - Kranzmann, Axel T1 - Impact of saline aquifer water on surface and shallow pit corrosion of martensitic stainless steels during exposure to CO2 environment (CCS) T2 - IOP Conference Series: Earth and Environmental Science N2 - Pipe steels suitable for carbon capture and storage technology (CCS) require resistance against the corrosive environment of a potential CCS-site, e.g. heat, pressure, salinity of the aquifer, CO2-partial pressure. Samples of different mild and high alloyed stainless injection-pipe steels partially heat treated: 42CrMo4, X20Cr13, X46Cr13, X35CrMo4 as well as X5CrNiCuNb16-4 were kept at T=60 °C and ambient pressure as well as p=100 bar for 700 h - 8000 h in a CO2-saturated synthetic aquifer environment similar to possible geological on-shore CCS-sites in the northern German Basin. Main corrosion products are FeCO3 and FeOOH. Corrosion rates obtained at 100 bar are generally much lower than those measured at ambient pressure. Highest surface corrosion rates are 0.8 mm/year for 42CrMo4 and lowest 0.01 mm/year for X5CrNiCuNb16-4 in the vapour phase at ambient pressure. At 100 bar the highest corrosion rates are 0.01 mm/year for 42CrMo4, X20Cr13 (liquid phase), X46Cr13 and less than 0.01 mm/year for X35CrMo4 and X5CrNiCuNb16-4 after 8000 h of exposure with no regard to atmosphere. Martensitic microstructure offers good corrosion resistance. T2 - 8th International Conference on Future Environment and Energy (ICFEE 2018) CY - Phuket, Thailand DA - 10.01.2018 KW - CCS KW - CO2 corrosion KW - Pipeline PY - 2018 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-465896 DO - https://doi.org/10.1088/1755-1315/150/1/012012 VL - 150 SP - 81 EP - 90 PB - IOP Publ. AN - OPUS4-46589 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Mosquera Feijoo, Maria A1 - Oder, Gabriele A1 - Saliwan Neumann, Romeo A1 - Buchheim, Michaela A1 - Kranzmann, Axel A1 - Olbricht, Jürgen T1 - Impact of Sample Geometry and Surface Finish on VM12‑SHC Ferritic–Martensitic Steel Under Cyclic Steam Atmosphere Operating Conditions JF - Oxidation of Metals N2 - The steam side oxidation of ferritic–martensitic VM12-SHC steel was investigated under thermo-cyclic conditions in water steam at 620/320 °C and 30 bar with a focus on assessing the influence of pre-oxidation time, specimen geometry and surface finish. The specimens were pre-oxidized under isothermal conditions in water steam at 620 °C and 30 bar for 500 h or 1500 h. After pre-oxidation treatment, all specimens were subjected up to 258 thermal cycles. Three different geometries—rectangular coupons, U-shaped ring segments and ring samples—were investigated to evaluate the influence of open/closed shape, and flat/curved surface on corrosion rate. At the same time, two types of surface finish were considered: “as received” and “ground.” The formation of a protective scale by pre-oxidation was investigated. EBSD and ESMA analyses revealed that the Cr-content of the alloy appeared to be insufficient for obtaining a protective oxide scale under studied conditions, at the same time the anayses confirmed that initial oxidation depends on presence of minor alloying elements as Si and Mn, strong oxide formers which can alter the kinetics and morphology of the corrosion reaction. Moreover, rectangular coupons with small wall thickness and flat surface exhibited the highest corrosion rate, while “ground” curved samples showed only local oxidation. This indicates that for same pre-oxidation time, oxidation kinetics is controlled by curvature. KW - Cyclic steam oxidation KW - 12%Cr steel KW - Specimen geometry KW - Surface treatments PY - 2022 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-551808 DO - https://doi.org/10.1007/s11085-022-10114-6 SN - 0030-770X SP - 1 EP - 18 PB - Springer AN - OPUS4-55180 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Koclega, Damian A1 - Radziszewska, A. A1 - Dymek, S. A1 - Morgiel, J. A1 - Maj, L. A1 - Kranzmann, Axel T1 - Improvement of Corrosion Resistance of 13CrMo4-5 Steel by Ni-Based Laser Cladding Coatings JF - Journal of Materials Engineering and Performance N2 - The 13CrMo4-5 ferritic steel is commonly used in power plants, due to its favorable mechanical properties. According to EN 10028-2, this steel can be used at temperatures up to 570°C because of its creep behavior. The inefficient corrosion resistance limits the application of this steel to lower temperatures depending on the gas temperature and slag formation. Therefore, the application of a highly resistant Ni-based coating is proposed to extend the corrosion resistance of elements made of ferritic steel. The corrosion test was performed in an environment containing a mixture of gases, like O2, COx, and SOx, and deposited ashes with elements, e.g., Na, Cl, Ca, Si, C, Fe, and Al. The exposure time was, respectively, 240 h, 1000 h and 4500 h at a temperature of 600°C. The oxide scale formed on the 13CrMo4-5 steel was significantly thicker than on the IN686 coating. The microstructure and chemical and phase compositions of the oxide scale were investigated using light optical microscopy together with scanning and transmission electron microscopy techniques. Energy dispersive x-ray analyses were performed when appropriate. KW - Aggressive environments KW - Corrosion resistance KW - High - temperature KW - Inconel 686 KW - Laser cladding PY - 2020 UR - https://nbn-resolving.org/urn:nbn:de:kobv:b43-514289 DO - https://doi.org/10.1007/s11665-020-04867-x SN - 1059-9495 VL - 29 IS - 6 SP - 3702 EP - 3713 PB - Springer AN - OPUS4-51428 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Blank, Robin A1 - Nitschke, Heike A1 - Saliwan Neumann, Romeo A1 - Kranzmann, Axel T1 - Materialographic Preparation of Salt JF - Praktische Metallographie N2 - Molten salt containing systems gain in importance for sustainable energy use and production. For research and development, interactions of molten salts with potential container materials are of major interest. This article introduces preparation procedures to display an intact metal and salt microstructure and their interface using light optical microscopy and scanning electron microscopy. The exemplary material combination is the ternary salt mixture NaCl-KCl-MgCl2 and the low alloyed steel 1.4901 (T92) with a maximum service temperature of 550 °C. These are potential elements/materials for use in latent heat thermal energy storages. KW - Molten salt KW - Corrosion KW - Steel KW - Aging KW - Dry preparation PY - 2021 DO - https://doi.org/10.1515/pm-2022-0058 VL - 59 IS - 10 SP - 628 EP - 640 PB - De Gruyter AN - OPUS4-56048 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Chandra, K. A1 - Dörfel, Ilona A1 - Wollschläger, N. A1 - Kranzmann, Axel T1 - Microstructural investigation using advanced TEM techniques of inner ocide layers formed on T92 steel in oxyfuel environment JF - Corrosion Science N2 - T92 steel was oxidized at 650 °C for 1000 h in dry and wet oxyfuel gases. The microstructure of inner oxide layer was investigated using scanning transmission electron microscopy and energy dispersive spectroscopy on thin lamellas of oxide cross-sections. The oxides were composed of fine equiaxed grains and separated into Fe-rich and Cr-rich regions. Fe-rich regions were wustite and iron sulphide while Cr-rich regions consisted of Fe-Cr spinel with different stoichiometries. Precipitates of (W,Mo)-rich oxides were formed within the oxide scale and beneath the oxide/alloy interface. Often iron sulphide and (W,Mo)-rich oxide were surrounded by Cr-rich spinel. KW - Steel KW - STEM KW - High temperature corrosion KW - Oxidation KW - Internal oxidation PY - 2019 DO - https://doi.org/10.1016/j.corsci.2018.12.008 SN - 0010-938X SN - 1879-0496 VL - 148 SP - 94 EP - 109 PB - Elsevier AN - OPUS4-47423 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Eh Hovsepian, P. A1 - Ehiasarian, A. P. A1 - Purandare, Y. P. A1 - Mayr, P. A1 - Abstoss, K. G. A1 - Mosquera Feijoo, Maria A1 - Schulz, Wencke A1 - Kranzmann, Axel A1 - Lasanta, M. I. A1 - Trujillo, J. P. T1 - Novel HIPIMS deposited nanostructured CrN/NbN coatings for environmental protection of steam turbine components JF - Journal of Alloys and Compounds N2 - To increase efficiency, modern steam plants are pushing their operational regime from super-critical (600 °C/300 bar) to ultra-super-critical (740/760 °C/350 bar) stretching existing turbine materials to their limits. The focus is on new generation functional materials and technologies which complement the inherent properties of existing materials. Current work proposes a novel High Power Impulse Magnetron Sputtering (HIPIMS) Deposition technology, for the first time, for deposition of a ceramic based CrN/NbN coating with a nanoscale multilayer structure (bi-layer thickness Δ = 1.9 nm) with superior adhesion (LC2 = 80 N) to protect low Chromium P92 steel widely used in steam power plants. Thermodynamic calculations predict the equilibrium phases and aggressive gaseous compounds generated by the interaction of steam with the coating. CrN/NbN coated P92 steel samples oxidised at 600 °C in a high pressure (50 bar) 100% steam atmosphere for up to 1000 h reveal the coating's superior oxidation resistance and protective mechanisms, especially against the detrimental effect of Hydrogen. High temperature (650 °C) Tensile Strength, Low Cycle Fatigue and Creep tests confirm that, unlike other state-of-the-art PVD technologies, HIPIMS is not detrimental to the mechanical properties of the substrate material. Water droplet erosion tests confirm no measurable weight loss after 2.4 X 10⁶ impacts. KW - Hipims KW - CrN/NbN KW - Nanoscale multilayers KW - Steam oxidation resistance KW - Water droplet erosion resistance PY - 2018 DO - https://doi.org/10.1016/j.jallcom.2018.02.312 SN - 0925-8388 SN - 1873-4669 VL - 746 SP - 583 EP - 593 PB - Elsevier AN - OPUS4-44800 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Stephan-Scherb, Christiane A1 - Nützmann, Kathrin A1 - Kranzmann, Axel A1 - Klaus, M. A1 - Genzel, C. T1 - Real time observation of high temperature oxidation and sulfidation of Fe-Cr model alloys JF - Materials and Corrosion N2 - Insights into early damage mechanisms during high-temperature gas corrosion provide important aspects for the prediction of the long-term stability of hightemperature materials exposed to a hot and corrosive environment. The current work presents a real time study concerning the combined oxidation and sulfidation of ferritic model alloys in a hot SO2 containing atmosphere using energy dispersive X-ray diffraction. The applied high temperature reactor allows the transmittance of high energetic X-rays in order to collect X-ray diffraction pattern of the sample surface in situ during the reaction with the reactive environment. The results revealed that the first phases crystallizing on iron with 2 wt% chromium and with 9 wt% chromium are oxides. The aging experiments at T = 650° C with 0.5% SO2 and 99.5% Ar were followed in situ and caused an external mixed oxide-sulfide layer on top of iron with 2 wt% chromium. On the higher alloyed material the external scale consists of iron oxides and the inner scale of mixed (Fe,Cr)-oxides and chromium-sulfides. The oxide content continuously increases parallel to an increase of the sulfide amount. Thus, the initially formed (Fe,Cr)-oxides do not have a protective character and support the transport of sulfur through the growing oxide scale. KW - High temperature corrosion KW - In situ diffraction KW - Sulfidation PY - 2018 DO - https://doi.org/10.1002/maco.201709892 SN - 0947-5117 VL - 69 IS - 6 SP - 678 EP - 689 PB - Wiley VCH Verlag AN - OPUS4-44776 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Nützmann, Kathrin A1 - Kranzmann, Axel A1 - Stephan-Scherb, Christiane T1 - The influence of chromium on early high temperature corrosion of ferritic alloys under SO₂ atmosphere JF - Materials at High Temperatures N2 - Comprehensive insights into the early stages of corrosion mechanisms provide fundamental knowledge to further understand and model long time material behaviour. The present work studies the early stages of combined oxidation and sulphidation of ferritic model alloys for time scales up to 250 h at 650 °C to observe the influence of chromium during the corrosion under SO2. Model alloys were used to focus on the reaction of the intended elements: Fe, Cr, S, and O. Pure iron simultaneously forms magnetite and iron sulphide in an early stage of corrosion, covered by a pure oxide layer after 100 h. Iron with 13 wt% Cr shows hematite and mixed Fe-Cr-oxides first, before sulphides nucleate in the inner corrosion zone. With increasing ageing time a magnetite layer is observed below the hematite layer. Quantitative phase fractions of all corrosion products observed were determined from cross section images. Characterization of the Fe13Cr corrosion scale by FIB revealed a highly porous structure in the inner corrosion zone where Cr-rich (Fe, Cr)-sulphides are present, and caused the scale to spall easily. KW - Early stages KW - Sulphidation KW - High temperature corrosion PY - 2018 DO - https://doi.org/10.1080/09603409.2018.1446705 SN - 0960-3409 VL - 36 IS - 6 SP - 558 EP - 568 PB - Taylor & Francis AN - OPUS4-44707 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - JOUR A1 - Nofz, Marianne A1 - Dörfel, Ilona A1 - Sojref, Regine A1 - Wollschläger, Nicole A1 - Mosquera Feijoo, Maria A1 - Schulz, Wencke A1 - Kranzmann, Axel T1 - Thin Sol-Gel Alumina Coating as Protection of a 9% Cr Steel Against Flue Gas Corrosion at 650 °C JF - Oxidation of Metals N2 - Samples of sol-gel alumina coated and uncoated P92 steel were exposed to flue gas at 650 °C for 300 h. As result of this treatment a 50 µm thick bi-layered oxide scale had formed on the surface of the uncoated sample. Below the scale a 40 µm thick inner oxidation zone was detected. In contrast, the porous, micron thick alumina coating enabled the formation of a chromium oxide scale with a thickness of some nanometers at the interface between steel substrate and coating. In this case high temperature corrosion of the steel was prevented so far. KW - Steel KW - Oxide coatings KW - High-temperature corrosion KW - TEM KW - SEM PY - 2018 DO - https://doi.org/10.1007/s11085-017-9799-0 SN - 0030-770X SN - 1573-4889 VL - 89 IS - 3-4 SP - 453 EP - 470 PB - Springer AN - OPUS4-44472 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -