TY - GEN A1 - Skrotzki, Birgit T1 - Brinell-Hardness (HBW 2.5/62.5) of Al-alloy EN AW-2618A after different aging times and temperatures N2 - The dataset contains data from Brinell hardness measurements of Al-alloy EN AW-2618A after aging for different times and temperatures. Aging was either load free or with applied tensile load (creep). KW - Aluminium alloy KW - EN AW-2618A KW - Brinell hardness KW - Aging KW - Creep PY - 2022 UR - https://doi.org/10.5281/zenodo.6787085 UR - https://doi.org/10.5281/zenodo.10396823 U6 - https://doi.org/10.5281/zenodo.6787084 PB - Zenodo CY - Geneva AN - OPUS4-55158 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - GEN A1 - Skrotzki, Birgit T1 - Radii of S-phase Al2CuMg in Al-alloy EN AW 2618A after different aging times at 190°C N2 - The dataset contains data from quantitative microstructural analysis of transmission electron microscopy (TEM) studies of the S-phase (Al2CuMg) radii in Al-alloy EN AW 2618A. The investigated material and the applied methods were described in detail in two publications. KW - Aluminium alloy KW - EN AW 2618A a KW - S-phase KW - Al2CuMg KW - Aging KW - Creep KW - Radii distribution KW - TEM PY - 2022 UR - https://doi.org/10.5281/zenodo.6659461 UR - https://doi.org/10.5281/zenodo.7625259 U6 - https://doi.org/10.5281/zenodo.6659460 PB - Zenodo CY - Geneva AN - OPUS4-55067 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER - TY - CONF A1 - Skrotzki, Birgit T1 - Aging processes in precipitation hardened aluminum alloys N2 - The mechanical strength of wrought high-strength aluminum alloys is essentially based on precipitation hardening, possibly in combination with prior forming, e. g. by stretching. Important parameters for achieving an optimum combination of hardness, strength, ductility, toughness, and further properties such as corrosion resistance are age-hardening temperature and time. During thermal (mechanical) treatment, nucleation and growth of precipitates takes place, leading to the desired degree of hardening. In aluminum alloys, precipitation sequences are usually passed through, i. e. a sequence of metastable precipitates is formed before the stable phase can precipitate. The optimum combination of properties is therefore based on a certain (optimum) microstructure, which can, however, change during the use of a component, since the microstructure is not stable. This happens in particular when the operating temperatures are close to the aging temperature and/or the operating times are sufficiently long. An external mechanical load may accelerate the processes. The presentation gives some examples for this. T2 - Materials Science and Engineering Congress MSE 2022 CY - Darmstadt, Germany DA - 27.9.2022 KW - Aluminium alloy KW - Precipitation hardening KW - Aging KW - Degradation PY - 2022 AN - OPUS4-55877 LA - eng AD - Bundesanstalt fuer Materialforschung und -pruefung (BAM), Berlin, Germany ER -